Center-intermittently patterned lithium metal electrode on a substrate
The roll-to-roll processing of lithium metal electrodes with intermittent patterning and controlled lamination addresses manufacturing challenges, resulting in a uniform and consistent lithium metal electrode structure for improved battery cell production.
Patent Information
- Application Number
- PCT/US2026/026503
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-05
- Filing Date
- 2026-05-04
- Publication Date
- 2026-11-12
AI Technical Summary
Conventional lithium metal electrode manufacturing methods face challenges such as lamination inconsistency, variation in lithium placement, unintended deposition, misalignment, and increased scrap due to intermittent lamination, which complicates downstream cell fabrication.
A method involving roll-to-roll processing that includes laminating lithium metal onto a polymer carrier film, forming intermittent openings, edge slitting, and controlled lamination onto a copper foil substrate to create a center-intermittently patterned lithium metal electrode, ensuring uniform lithium coverage and clean tab-region definition.
The process results in a more uniform, cleaner, and consistent lithium metal electrode structure suitable for downstream battery cell manufacturing, with improved thickness uniformity and reduced process variability, facilitating efficient tab formation and welding.
Smart Images

Figure US2026026503_12112026_PF_FP_ABST
Abstract
Description
CENTER-INTERMITTENTLY PATTERNED LITHIUM METAL ELECTRODE ON A SUBSTRATECROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims priority to U.S. Provisional Patent Application No.63 / 800.181, filed May 5, 2025. which is hereby incorporated by reference in its entirety.TECHNICAL FIELD
[0002] The present disclosure relates to lithium metal materials, and more particularly to a method for fabricating lithium metal electrodes.BACKGROUND
[0003] Lithium-ion batteries are a type of rechargeable battery that uses the reversible intercalation of lithium ions into electronically conducting solids to store energy. Lithium-ion batteries generally have better energy efficiency and a longer life cycle and calendar life than other types of rechargeable batteries. Lithium-ion batteries can be used in a wide range of electronics ranging from smaller devices to fully electric automobiles.SUMMARY
[0004] This summary is provided to introduce a selection of concepts in a simplified form that are further described below in the detailed description. This summary is not intended to identify key features or essential features of the claimed subject matter, nor is it intended to be used as an aid in determining the scope of the claimed subject matter.
[0005] According to an aspect of the present disclosure, a method is provided. The method comprises laminating a metal foil onto a substrate to form a supported web. Selected portions of the supported web are removed to form openings at predetermined intervals along a machine direction to form a patterned continuous web. The patterned continuous web is laminated onto acontinuous conductive substrate to form a patterned metal anode electrode comprising exposed regions of the continuous conductive substrate defined by the openings at predetermined intervals.
[0006] According to another aspect of the present disclosure, a patterned metal anode electrode is provided. The patterned metal anode electrode comprises a continuous conductive substrate and a continuous metal anode layer laminated onto the conductive substrate in a center-intermittent configuration. The continuous metal anode layer comprises a plurality of periodically spaced openings along a machine direction of the continuous conductive substrate, uniform longitudinal edges, and at least one exposed region of the continuous conductive substrate defined by the periodically spaced openings, wherein the at least one exposed region is configured to accommodate lead tab welding. As used herein, a continuous metal anode layer may include a patterned, mechanically continuous metal anode layer.
[0007] The foregoing general description of the illustrative embodiments and the following detailed description thereof are merely exemplary aspects of the teachings of this disclosure and are not restrictive.BRIEF DESCRIPTION OF FIGURES
[0008] Non-limiting and non-exhaustive examples are described with reference to the following figures.
[0009] FIG. 1 illustrates a flow diagram illustrating a sequence of a method for fabricating a metal anode electrode, according to aspects of the present disclosure;
[0010] FIG. 2 illustrates an overview of an example continuous web patterning process, according to aspects of the present disclosure;
[0011] FIG. 3 illustrates a detailed illustration of an example automated electrode punching process, showing the interaction between a punch tool and a lithium foil, according to aspects of the present disclosure;
[0012] FIG. 4 illustrates a top view of an example of a patterned web on a carrier film after center-intermittent punching, according to aspects of the present disclosure;
[0013] FIG. 5 illustrates a top view of an example of the slitting process used to trim edges of a center-intermittently patterned web, according to aspects of the present disclosure;
[0014] FIG. 6A illustrates combined top and side views of an example product produced through the electrode patterning and lamination process, according to aspects of the present disclosure;
[0015] FIG. 6B illustrates a side view of an example double laminated product produced through the electrode patterning and lamination process, according to aspects of the present disclosure;
[0016] FIG. 7 illustrates a top view of an example lithium metal electrode fabricated using a center-intermittent patterning (CIP) method, with an example of downstream customized notching, according to aspects of the present disclosure;
[0017] FIG. 8 illustrates a graph depicting example capacity retention data over fifty (50) cycles for a battery coin cell constructed with a lithium metal electrode fabricated via the CIP method, according to aspects of the present disclosure;
[0018] FIG. 9 illustrates a graph depicting an example cell voltage profile of the initial formation cycle for a battery coin cell constructed with a lithium metal electrode fabricated via the CIP method, according to aspects of the present disclosure;
[0019] FIG. 10 illustrates a plot depicting example Electrochemical Impedance Spectroscopy (EIS) results after 100 cycles for a battery coin cell constructed with a lithium metal electrode fabricated via the CIP method, according to aspects of the present disclosure;
[0020] FIG. 11 illustrates a plot depicting example tensile strength test results for two samples (one created using traditional lamination with no punching and one created using the CIP method), according to aspects of the present disclosure;
[0021] FIG. 12 illustrates a flow chart of a method for fabricating an anode electrode, according to aspects of the present disclosure; and
[0022] FIG. 13 illustrates a flow chart of another method for fabricating an anode electrode, according to aspects of the present disclosure.DETAILED DESCRIPTION
[0023] The following description sets forth exemplary aspects of the present disclosure. It should be recognized, however, that such description is not intended as a limitation on the scope of the present disclosure. Rather, the description also encompasses combinations and modifications to those exemplary aspects described herein.
[0024] In lithium metal electrode manufacturing, it is often desirable to laminate lithium metal onto a copper foil current collector while preserving a bare copper region for subsequent lead-tab formation or welding during downstream cell fabrication. In some conventional approaches, lithium metal is laminated onto copper foil in an intermittent manner so that lithium-free regions remain at locations corresponding to tab areas. Although such approaches can be used in production, intermittent lamination of discrete lithium sections may introduce manufacturing challenges, including lamination inconsistency, variation in lithium placement or amount from section to section, unintended lithium deposition in regions intended to remain bare, misalignment, increased scrap associated with misalignment or defective transfer, and the like.
[0025] Accordingly, improved processing methods are desired. In certain embodiments, the present disclosure addresses these issues by forming intermittent openings in a continuous lithium metal web prior to lamination onto a copper foil substrate, thereby allowing the lithium web to remain continuous while defining lithium-free regions corresponding to future tab locations. In this manner, the laminated structure can provide more uniform lithium coverage, cleaner tab-region definition, and reduced process variability. In some embodiments, the lithium metal may first be supported on a polymer carrier film (e.g., a polymer substrate), and the webmay further undergo edge slitting after formation of the intermittent openings so that clean edge regions are obtained before lamination onto the copper foil substrate.
[0026] In some embodiments, the present disclosure provides roll-to-roll methods and systems for fabricating a center-intermittently patterned (CIP) metal anode electrode on a conductive substrate, together with electrode products and intermediate structures produced thereby. In the disclosed process, a continuous metal foil, particularly a lithium metal foil is laminated onto a polymer substrate (e.g., a polymer carrier film) to form a supported web. The supported web is advanced through an in-line patterning station (e.g., a punching station or laser removal station) where selected center regions of the metal foil are removed at predetermined intervals along the machine direction, forming periodically spaced openings while maintaining the structural continuity of the remaining metal web. The patterned continuous web then passes through an edge-slitting station that removes peripheral buffer zones to produce a dimensionally controlled web with clean longitudinal edges. The patterned continuous metal web (e.g., lithium metal foil web with punched openings) is subsequently laminated onto a continuous conductive substrate (e.g., copper foil substrate) under controlled gap, pressure, and / or temperature conditions to produce a metal-on-substrate electrode having intentionally exposed bare-substrate regions at the locations of the punched openings. The disclosed electrode architecture is suitable for downstream tab formation, welding, customized notching, electrode punching, and incorporation into lithium metal battery cells employing liquid, semi-solid, or solid-state electrolytes. Also disclosed, is an intermediate pre-lamination product comprising a patterned continuous metal web on a carrier film, and a system for performing the roll-to-roll patterning process.
[0027] In some embodiments, the disclosed process may be understood as including lithium foil preparation followed by three in-line processing stages: intermittent patteming / punching to form openings in a continuous lithium web, edge slitting, and controlled lamination. These stageswork together to produce a lithium metal electrode structure that is cleaner, more uniform, and better suited for downstream cell manufacturing processes.
[0028] In the lithium foil preparation stage, lithium metal foil is prepared by laminating the lithium onto a substrate or carrier film (e.g., polymer substrate). The carrier film acts as a temporary mechanical support for lithium during later processing steps. In some embodiments, the carrier film may be a polymer film, such as polyethylene terephthalate (PET), although other suitable support materials may be used depending on stiffness, tension characteristics, dimensional stability, and compatibility with lithium processing. More specifically, the polymer carrier film may be a polyethylene terephthalate (PET) release film, a polypropylene (PP) release film, a polyimide (PI) release film, or a polyethylene (PE) release film, or any other type of polymer based film that remains readily detachable from lithium metal following high pressure processing. The carrier film (e.g., polymer substrate) is particularly useful because lithium metal is soft, reactive, and easily deformed. Without support, lithium foil may wrinkle, stretch, fold onto itself, or adhere to tooling surfaces during rapid roll-to-roll motion. By laminating the lithium onto a carrier film, the web can be transported with improved tension control and improved shape retention. The carrier film helps the lithium remain flat as it enters the punching zone, reduces the likelihood of uncontrolled deformation during punch engagement, and supports the lithium during high-speed indexed or synchronized motion. In this way, the carrier film is not merely a transport aid, but a structural support element that allows lithium to be processed in a more stable and controlled manner.
[0029] In the first stage, the supported lithium foil undergoes intermittent punching (e.g., patterning) while moving through the roll-to-roll process network. In this stage, selected center portions of the continuous lithium web are punched out at predetermined intervals along the machine direction so that the remaining lithium web retains continuity while defining future bare-copper regions after lamination. The punching mechanism may include a punch and die arrangement designed to minimize mechanical stress, tearing, or permanent deformation in thelithium. In some embodiments, the punch geometry may include rounded or radiused features to reduce stress concentration at cut boundaries. The roll-to-roll transport path may also be configured to maintain suitable web tension before, during, and after punching so that the laminated foil remains dimensionally stable. The punching operation may be controlled by a programmable logic controller, servo-driven index system, or other automated control architecture that synchronizes web advancement with punch timing and positional accuracy. In some embodiments, the punch perimeter, die opening, or other tooling surfaces that contact the supported web may include rounded comers, chamfered edges, radiused transitions, or combinations thereof to reduce marking, indentation, tearing, microcracking, or plastic deformation of the lithium metal during punching.
[0030] In the second stage, the punched laminated foil undergoes edge slitting. This slitting process removes edge irregularities that may have originated during the initial lithium-to-carrier lamination process or during upstream web handling. In practice, the edge regions of raw lithium laminated onto a plastic carrier may not always be sufficiently clean for direct downstream lamination. Such edges may contain contamination, deformation, unevenness, or nonuniform cut characteristics. By passing the punched laminated foil through a slitting station, unwanted edge regions can be removed so that the remaining patterned continuous web has a more uniform width and cleaner longitudinal edges. This slitting step also helps define a more precise final web geometry and prepares the patterned lithium web for more reliable lamination onto the copper foil substrate.
[0031] In the third stage, the patterned continuous lithium web is laminated onto a continuous copper foil substrate under controlled temperature and pressure conditions. In some embodiments, heated guide rollers, lamination rollers, press rollers, or other pressure-applying components may be used to bond the lithium web to the copper foil in a uniform manner. The controlled lamination conditions may help achieve consistent adhesion, consistent surface contact, and stable alignment between the patterned lithium web and the copper foil substrate.The resulting laminated structure includes a continuous copper foil substrate with a continuous lithium layer that is center-intermittently patterned along the machine direction so that intentionally exposed bare copper regions are present at predetermined locations (i.e., corresponding to the punched areas in the lithium metal). In some embodiments, the laminated lithium maintains a flush (e.g., smooth, planar, free from indentations or irregularities, flat, etc.) top surface relative to the copper foil for improved thickness uniformity. For example, the laminated lithium forms a smooth and uniform interface with the copper foil, such that the lithium layer is intimately bonded to the copper surface without surface irregularities, gaps, or discontinuities. This well-conformed contact between the lithium and copper foil may contribute to improved thickness uniformity across the electrode. For example, the electrode may exhibit a consistent and uniform thickness. In addition, the resulting patterned structure may include one or more bare copper regions configured to accommodate lead-tab welding or other downstream electrical connection requirements.
[0032] This architecture provides several practical advantages. The patterned openings can be formed in a repeatable manner while the lithium web remains continuous, the slitting step helps ensure that the lithium presented for lamination is clean and dimensionally controlled, and the controlled lamination process improves consistency of bonding between the lithium and the copper foil substrate. The overall process therefore provides a scalable roll-to-roll method for producing a center-intermittently patterned lithium metal electrode structure suitable for downstream electrode punching, tab formation, welding, cell-size shaping, or subsequent integration into battery manufacturing workflows.
[0033] Referring to FIG. 1, an exemplary diagram illustrating a sequence of a method 100 for fabricating a metal anode electrode is depicted. The method 100 may be performed via an inline process flow, in which blocks 102, 104, 106, and 108 may be performed in sequence.
[0034] In an embodiment, at block 102, the method 100 may perform metal foil preparation. For example, the process may begin by laminating a continuous lithium metal foil onto a carrierfilm. The carrier film may be a polymer film (e.g., polymer substrate) such as polyethylene terephthalate (PET), although other support materials may be used depending on stiffness, dimensional stability, tension behavior, and compatibility with lithium processing. The earner film functions as a temporary support layer that improves handling of the lithium metal during conveyance, indexing, punching, slitting, and downstream lamination. As noted above, because lithium metal is soft, highly deformable, and prone to wrinkling, stretching, folding, or adhering to tooling surfaces, the carrier film helps maintain flatness and positional control of the laminated structure during roll-to-roll processing. In this way, the carrier film serves not merely as a transport aid, but as a structural support element that allows the lithium metal foil to be processed with improved stability and reduced deformation.
[0035] At block 104, the method 100 performs electrode patterning. For example, the carrier film laminated with lithium metal foil is advanced in a controlled intermittent motion. Each forward motion may correspond to a predetermined length or fixed interval (e.g., 562 millimeters (mm), or approximately 562 mm + / - 0.5 mm) followed by a stop phase to perform precise patterning (e.g., punching). In an embodiment, patterning may include removing selected portions comprising at least portions of the lithium metal foil, and in some embodiments corresponding portions of the carrier film, to create openings in the lithium metal foil at the predetermined length or fixed interval. In an embodiment, the removal may be performed by a punching station. In another embodiment, the removal may be performed via laser removal (e.g., laser cutting or laser ablation). In some embodiments, the present disclosure enables precise patterning (e.g., punching) of center-intermittent openings in a continuous lithium metal foil laminated onto a carrier film prior to lamination of the remaining patterned continuous lithium web onto a conductive foil substrate (e.g., a copper foil substrate) in battery manufacturing.
[0036] At block 106, the method 100 performs edge slitting. For example, after the openings are formed in the supported web, one or more longitudinal edge portions of the patterned web may be removed to eliminate peripheral buffer zones, edge irregularities, contamination,deformation, burrs, or nonuniform edge regions. In some embodiments, the edge slitting may be performed using rotary knives, scissor-type slitters, blades, or other suitable slitting units positioned along opposite longitudinal edges of the moving patterned web. The edge-slitting operation may produce a patterned continuous web having a final uniform width and clean longitudinal edges before the patterned continuous web is laminated onto the continuous conductive substrate.
[0037] At block 108, the method 100 performs continuous lamination. . In some embodiments, the continuous lithium metal foil is positioned on top of a continuous copper foil substrate and subsequently pressed to form the continuous lamination. In some embodiments, the polymer substrate (e.g., polymer release film) on the lithium metal foil may be left adhered to the lithium metal foil for ease of transport, rolling, handling, and / or storage.
[0038] Referring to FIG. 2, FIG. 2 illustrates, in accordance with some embodiments, a system 200 to perform the overall continuous patterning process for forming intermittent openings in a continuous metal foil supported on a polymer substrate or carrier film. It should be noted that although different portions of the system 200 are illustrated in separate FIGs. 3-7, the system 200 may be a continuous process and that the embodiments illustrated in FIGs. 3-7 may be part of the overall system 200.
[0039] In traditional methods, lithium metal foil is continuously laminated onto the copper foil, such that that there are no regions where the copper foil is exposed without lithium metal foil coverage; this configuration is therefore described as “continuous.” In contrast, an “intermittent” configuration refers to a structure in which lithium foil and copper foil regions alternate along the length of the laminated structure at predetermined intervals and dimensions, resulting in a repeating copper-lithium-copper-lithium pattern along the length of the structure (i.e., length of the laminated foil). In some embodiments of the disclosed subject matter, the metal foil supported on the polymer substrate may be considered “continuous” because a supply roll 202 of the metal foil supported on the polymer substrate may be continuously fed in amachine direction 206. Said another way, the system 200 may fabricate or pattern multiple anode electrodes without pausing the system until the entire supply roll 202 is fed through the system 200.
[0040] In the illustrated arrangement, a supported web or laminated web 203 (also referred to herein simply as a “web”) is unwound from the supply roll 202. The web 203 may comprise the continuous metal foil supported on the polymer substrate or carrier film. The web 203 may be pre-formed by laminating the continuous metal foil onto the polymer substrate. The web 203 may be guided through a plurality of rollers 204 in a machine direction 206, advanced through a patterning station 208. and then a patterned web 205 is directed toward a rewinding roll 210 or downstream processing stations. In an embodiment, the system 200 may include a plurality of rollers 204 that provide tension control for the web 203.
[0041] The web 203 may be advanced in an indexed manner or in a synchronized continuous-motion manner, depending on the desired throughput and control architecture. Because the metal foil layer remains supported by the carrier film (e.g., polymer substrate) throughout this stage, the laminated metal foil layer may be transported with improved web tracking, reduced flutter, and improved positional accuracy during punch registration.
[0042] In an embodiment, the metal foil may be any metal used to form the anode electrode of a battery cell. In an embodiment, the metal foil may be lithium metal, although it should be noted that other types of metal may be deployed. Although examples described herein may refer to the metal foil as a lithium metal foil, other metallic foils may be similarly used and processed without departing from the scope of the disclosed subject matter.
[0043] In an embodiment, the earner film may be a polymer carrier film. For example, the polymer carrier film may be a release film made from polyethylene terephthalate (PET), polypropylene (PP), polyethylene (PE), polyimide (PI), or the like. In another embodiment, the polymer earner film may be a multilayer structure formed using polyethylene terephthalate (PET), polypropylene (PP), polyethylene (PE), polyimide (PI), or any combination thereof.
[0044] In some embodiments, the carrier film (i.e., polymer substrate) may have an overall width of about 160 mm to 240 mm. In an embodiment, the width may be approximately 180 mm to 220 mm. In some embodiments, the width may be approximately 200 mm.
[0045] In an embodiment, the metal foil laminated onto the carrier film may be approximately 80% of the width of the carrier film. For example, when the width of the carrier film is approximately 200 mm, the laminated metal foil thereon may initially occupy an active metal (e.g., lithium) width of about 160 mm prior to downstream edge slitting. The remaining lateral portions of the carrier film may serve as buffer zones that assist with transport through rollers 204, guides, and registration elements. Such buffer regions may also reduce edge-related damage and provide mechanically stable regions for web handling prior to slitting. The values described herein are illustrative and non-limiting, and other widths, buffer-zone dimensions, and web geometries may be used depending on product format and equipment design without departing from the scope of the disclosed subject matter.
[0046] At the patterning station 208, selected center portions (e.g., portions located at an approximate center between the lateral edges of the web 203) of the web 203 are removed to create a repeated center-intermittent opening pattern while maintaining the continuity of the remaining web 203. In some embodiments, removed portions 216 may have a generally rectangular shape and may have dimensions of about 40 mm by 60 mm. In other embodiments, the removed portions 216 may have a generally square shape. The openings may be formed at a fixed and repeatable interval along the machine direction 206. In an embodiment, the fixed or predetermined interval may be any desired length in the machine direction based on the desired size and / or dimensions of the final metal anode electrode that will be produced. In an example using the widths of the web 203 described above, the fixed interval may be approximately 562 mm.
[0047] Although a single patterning station 208 is illustrated in FIG. 2, it should be noted that a plurality of patterning stations 208 may be deployed. For example, multiple patterningstations 208 may be deployed in series such that multiple openings may be formed in the web 203 at the fixed interval.
[0048] In some embodiments, the web 203 may be advanced by indexed motion so that each patterning cycle occurs after a predetermined feed length has been reached. In other embodiments, patterning actuation may be synchronized with web position during continuous motion. In either case, the patterning process is configured such that the useful product is the remaining patterned web 205, not the removed portions 216. In some embodiments, the removed portions 216 may be collected in a collection tray 228 and recycled to form additional supply rolls 202 of the web 203, or may be disposed of.
[0049] In an embodiment, the patterning station 208 may be controlled by a programmable logic controller (PLC) 220. For example, the PLC 220 may be a customized application specific integrated controller (ASIC). In another example, the PLC 220 may be a general-purpose computer having a processor and a non-transitory computer readable medium, a computer program, and / or a computer program product storing instructions that are executed by the processor to perform the functions of the patterning station 208 described herein. In some embodiments, the non-transitory computer readable medium, a computer program, and / or a computer program product may be stored in memory of PLC 220.
[0050] In an embodiment, the PLC 220 may be communicatively coupled to a mechanical system 222 that drives the patterning station 208. For example, the mechanical system 222 may be a servo motor, a hydraulic system, or a pneumatic system for a punching station that punches the removed portions 216 out of portions of the web 203. In another embodiment, the mechanical system 222 may be a motor to control movement of a laser that is used to remove the removed portions 216 via laser cutting, laser ablation, or laser notching. In another embodiment, the mechanical system 222 may be a servo motor, a hydraulic system, or a pneumatic system for moving or controlling a rotary die cutting tool, a blade cutting, or any other tool that can be used to remove the removed portions 216.
[0051] In some embodiments where multiple patterning stations 208 are deployed, each of the patterning stations 208 may be the same type of patterning station or the patterning stations 208 may include different types of patterning stations 208. For example, all of the patterning stations 208 may be a punching station or some may be punching stations, while other patterning stations 208 may be laser cutters. In another example, all the patterning stations 208 may be punching stations, but the punching stations may have different sized dies. This may allow for different dimensioned or different sized anode electrodes to be formed within the same web.
[0052] FIG. 3 illustrates an example of the patterning station 208. In an embodiment, the patterning station 208 may be a punching station 300. In some embodiments, the punching station 300 includes an upper punch member 310 and a lower die member 312 positioned on opposite sides of the web 203 moving in the machine direction 206. During operation, the web 203 is advanced to a target position and held in position, while the upper punch member 310 moves down toward the lower die member 312 to shear out a selected portion of the web 203. The removed portion 216 may be collected, as described above.
[0053] In an embodiment, the selected portion of the web 203 may be located in a center region of the web 203. The removed portion 216 may then be discharged downward through a collection path. The patterned web 205, which includes a punched opening 250, continues downstream for further advancement and repeated punching cycles. The punching cycle, feed length, dwell interval, and discharge sequence may be coordinated by an automated control system including one or more PLCs 220 and one or more mechanical systems 222 (e.g.. servo motors, encoders, sensors, and / or registration elements) to reduce positional error and improve repeatability.
[0054] In some embodiments, the punch perimeter of the upper punch member 310, die opening of the lower die member 312, or other contact regions of the punching station 300 may include rounded corners, chamfered edges, radiused transitions, or combinations thereof. Such geometries may reduce concentrated stress at the cut boundary and thereby reduce marking,indentation, local tearing, microcracking, or plastic deformation in the continuous metal foil during the punching operation. This may be particularly advantageous where the metal foil is lithium foil as lithium foil is thin and mechanically delicate. The supporting carrier film may further assist in preserving the integrity of the remaining lithium web during punch engagement by stabilizing the layer of the lithium foil across the cutting region. Thus, the punching station 300 may be configured to form well-defined openings while minimizing mechanical damage to the useful patterned web 205 that continues downstream.
[0055] FIG. 4 illustrates a top view of an example of the patterned web 205 formed after the patterning station 208 (e.g.. the punching station 300 illustrated in FIG. 3). FIG. 4 illustrates a continuous metal foil 405 that is laminated on a polymer substrate 404. As noted above, the continuous metal foil 405 may comprise a lithium metal foil and the polymer substrate 404 or carrier film may be a polymer release film.
[0056] In the example illustrated in FIG. 4, the patterned web 205 may be described using a continuous lithium layer as the continuous metal foil 405. The continuous lithium metal layer may also be referred to by the reference numeral 405. In an embodiment, a width of the web 203 (illustrated in FIGs. 2 and 3) and the patterned web 205 may be measured along a dimension 414. In an embodiment, a width of the continuous metal foil 405 may be measured along a dimension 412. As discussed above, the polymer substrate 404 may have an overall width of about 160 mm to 240 mm. In an embodiment, the width of polymer substrate 404 may be approximately 180 mm to 220 mm. In an embodiment, the width of polymer substrate 40 may be approximately 200 mm.
[0057] In an embodiment, the continuous metal foil 405 may be approximately 80% of the width of the polymer substrate 404. For example, when the width of the polymer substrate 404 is approximately 200 mm, the continuous metal foil 405 thereon may initially occupy an active metal (e.g., lithium) width of about 160 mm prior to downstream edge slitting.
[0058] In the illustrated embodiment, the polymer substrate 404 supports the continuous lithium layer 405 in which discrete center openings 250 have been formed at selected intervals 410 along the machine direction 206. The openings 250 may be substantially rectangular or square having dimensions 416 and 418 (e.g., a length and width). In an embodiment, the openings 250 may have a dimension 416 of about 40 mm and a dimension 418 of about 60 mm, and may be repeated at intervals 410, such as about 500 mm - 600 mm, about 525 mm - 575 mm, about 550 mm - 570 mm, or approximately 562 mm + / - 5 mm. Thus, the remaining patterned web 205 remains continuous between successive openings 250, allowing the patterned structure to be transported as a single patterned web 205 for subsequent slitting and lamination rather than as separate transferred pieces. After punching, the removed portions 216 (illustrated in FIGs. 2 and 3) may be directed to a scrap or recycling stream, while the patterned web 205 proceeds as the useful intermediate product.
[0059] Following patterning, the patterned web 205 proceeds to an edge-slitting stage. FIG.5 illustrates a representative top view 500 of the slitting process used to trim the edges of the patterned web 205 (e.g., a center-intermittently patterned lithium metal laminate). It should be noted that FIG. 5 illustrates a portion of the overall system / process that is downstream from the patterning station 208. It should be noted that FIG. 5 has been simplified for ease of explanation and may include one or more additional components that are not shown (e.g., transport rollers, mechanisms to control / activate cutters / slitting units 502, and the like).
[0060] In some embodiments, the patterned web 205 initially includes the patterned metal region together with peripheral edge regions or buffer zones 420. To refine the web geometry and remove potentially defective or contaminated edge portions, one or more slitting units 502, such as rotary knives or scissor-type slitters, may be positioned along opposite longitudinal edges of the pattern web 205 while the patterned web 205 moves. These cutters or slitting units 502 may remove edge material along a line 506 and a line 507 in a controlled manner so that the resulting patterned web 205 has a uniform final width 508 and cleaner longitudinal edges. A uniform patterned metalweb 605 (illustrated in FIG. 6) may be formed after the slitting process, which can be laminated onto a continuous conductive foil substrate, as described below and illustrated in FIG. 6.
[0061] In some embodiments, the overall width (e.g., along the dimension 414) of the patterned web 205 prior to slitting may be about 200 mm, and approximately 20 mm may be removed from each side to result in a final overall laminate width (e.g., along the dimension 412) after slitting of about 160 mm. In other embodiments, the lithium-active width before slitting may be about 160 mm, and the final slit width may be selected as needed for downstream lamination or cell design. These values refer to different process stages and may vary depending on the equipment configuration and target product format. The slitting stage may remove edge burrs, handling defects, contaminated regions, or nonuniform edges introduced during upstream lamination or punching, and may thereby prepare the patterned continuous lithium web for more reliable lamination onto copper foil. The removed edge material may be vacuum collected, wound separately, or recycled.
[0062] After slitting, the patterned web 205 is laminated onto a continuous conductive foil substrate under controlled temperature and pressure conditions. The continuous conductive foil substrate may be any electrically conductive material suitable for use as a current collector. In an embodiment, the continuous conductive foil substrate may comprise copper foil, nickel foil, stainless steel foil, nickel-plated copper foil, and the like. In the examples described below, copper foil may be used as the continuous conductive foil substrate.
[0063] FIG. 6A illustrates combined top and side views of a representative intermediate product 600 produced through the punching, slitting, and lamination process. It should be noted that FIG. 6A illustrates a portion of the overall system / process that is downstream from the patterning station 208. It should be noted that FIG. 6A has been simplified for ease of explanation and may include one or more additional components that are not shown (e.g., transport rollers).
[0064] In the top view, a continuous copper foil substrate 604 extends continuously in the machine direction 206 and across the full product width. Laminated thereon is the continuous patterned metal web 605. In an embodiment, the continuous patterned metal web 605 may beremoved from the polymer substrate or carrier film 404 (or vice versa) after the slitting process described above. The continuous patterned metal web 605 includes center-intermittent openings 250 that define exposed regions 601 of bare copper at selected intervals along the machine direction 206.
[0065] In the side view, the continuous copper foil substrate 604 appears as a continuous lower layer, while the continuous patterned metal web 605 appears as an upper layer interrupted at the locations of the punched openings 250. These views illustrate that the final electrode structure is formed by laminating the remaining patterned continuous metal web 605 onto continuous copper foil substrate 604, rather than by separately placing removed punch-out portions onto the copper. The resulting product may provide improved thickness uniformity (e.g., thickness as measured from top to bottom in the side view), improved alignment, and repeatable bare-copper definition for downstream manufacturing operations.
[0066] In some embodiments, the lamination process may be performed under controlled temperature and pressure to ensure mechanical adhesion. For example, the PLC 220 may be communicatively coupled to a temperature control and / or pressure control means 606. In an embodiment, the temperature control and / or pressure control means 606 may be a single device or separate devices. For example, as separate devices, the temperature control means may include heating elements, and the pressure control means may include a guided roller that may apply pressure. The PLC 220 may control both the devices to set a desired temperature and a desired amount of pressure. In another example, the temperature control and / or pressure control means 606 may be a single device. For example, a heated guide roller may be deployed that provides both temperature control and pressure control.
[0067] The temperature control and / or pressure control means 606 may be used to establish intimate contact and adhesion between the patterned continuous metal web 605 and the continuous copper foil substrate 604. The lamination conditions may be selected to promote consistent bonding, good surface conformity, stable alignment, and reduced wrinkling or misregistration. Because the lithium layer remains as a continuous patterned web rather than separate transferredpieces or islands, the process may provide improved positional consistency and more reliable definition of the exposed regions 601 of bare copper corresponding to the previously formed openings 250.
[0068] In some embodiments, and as shown in a side view depicted in Figure 6B, the disclosed subject matter may comprise a double lamination structure 670 that includes a layer of continuous copper foil substrate 674 that is directly laminated with (e.g., sandwiched between) a top metal foil layer 675 on the substrate’s first / top surface and a bottom metal foil layer 676 on the substrate’s second / bottom surface. Notably, the top metal foil layer 675 includes a plurality of center-intermittent openings 680 that define exposed regions 671 (i.e., the top side of substrate 674) of bare copper at selected intervals along a machine direction (e.g., machine direction 206 shown in Figure 6A). Similarly, the bottom metal foil layer 676 includes center-intermittent openings 682 that define exposed regions 671 (i.e., the bottom side of substrate 674) of bare copper at selected intervals along the machine direction.
[0069] In some embodiments, each of these two metal foil layers 675, 676 of double lamination structure 670 may also be laminated with a polymer substrate (e.g., carrier release film) on a surface that is not in direct contact with the middle continuous copper foil substrate 674. For example, a double lamination structure 670 may be configured to have (e.g., proceeding from the top layer to bottom layer) a first polymer substrate layer (not shown), a first metal foil layer 675, the continuous copper foil substrate layer 674, a second metal foil layer 676, and a second polymer substrate layer (not shown).
[0070] FIG. 7 illustrates a representative metal (e.g., lithium) electrode 720 fabricated using the disclosed CIP method, together with an example of downstream customized notching. In some embodiments, the exposed region 601 intended for subsequent welding or electrical connection may be located at the left side, the right side, or the center of a portion 704 of the continuous patterned metal web 605 that is associated with the exposed region 601. For example, the portion 704 where the exposed region 601 is located relative to the portion 704 may depend on cell design and lead-tab requirements. Because the exposed region 601 is defined by the opening 250 formedin the continuous metal foil 405 before lamination, the size and location of the exposed region 601 may be controlled through the patterning station 208 of the CIP method. Thus, the patterning process may be used not only to define the lithium coverage pattern itself, but also to establish the position and dimensions of a downstream lead-tab welding region (e.g., the exposed regions 601).
[0071] In some embodiments, the patterned lithium-on-copper structure may also be further processed to form a customized notch adjacent to or associated with the exposed region 601 having various dimensions. For example, the metal electrode 720 may have an overall width 716 and an overall length 714. The portion 704 may have a length 712 and the same overall width 716. In an embodiment, the exposed region 601 may be custom notched to have a width 710 and a length 718.
[0072] Such a notch may be useful for downstream tab attachment, packaging, cell alignment, or other integration requirements. The notched configuration may be established after lamination while preserving the overall relationship between the patterned lithium layer (e.g., the continuous patterned metal web 605) and the continuous copper foil substrate 604. Accordingly, the disclosed process may provide not only a patterned lithium-on-copper electrode having intentional bare copper regions or exposed regions 601, but also a structure that can be further tailored by downstream cutting or notching operations without departing from the disclosed manufacturing concept. In some instances, the center-intermittently laminated sample is supplied to a customer, who subsequently performs a notching process to obtain electrodes of the desired dimensions. In the top view of Figure 7, the configuration of portion 704 includes visible lines on the lithium layer that indicate the predefined notching locations. After the notching operation, these markings guide the formation of precisely sized electrodes tailored to the customer’s specifications, as represented by the final structure 704.
[0073] FIGs. 8-10 illustrate representative electrochemical data obtained from a battery coin cell constructed using a lithium metal electrode fabricated via the disclosed CIP method. FIG. 8 depicts a graph 800 of capacity retention data over 50 cycles, FIG. 9 depicts a graph 900 of a cell voltage profile of the initial formation cycle, and FIG. 10 depicts a graph 1000 ElectrochemicalImpedance Spectroscopy (EIS) results after 100 cycles. These figures are provided to demonstrate that a cell may be successfully assembled and tested using a lithium anode prepared by the disclosed process. The electrochemical data may indicate that the disclosed patterned lithium-on-copper electrode architecture is compatible with practical cell fabrication and cycling, while still providing the manufacturing benefits associated with controlled patterning of the continuous lithium web prior to lamination.
[0074] FIG. 11 illustrates a graph 1100 that compares tensile strength data for two samples of lithium foil laminated to a copper substrate. One sample was created using traditional lamination with no punching as a reference. The other sample was created using the CIP method. These figures are provided to demonstrate that samples manufactured using the CIP method may not suffer from lack of adhesion via lamination. Notably, the results suggest that there may be no meaningful difference between the tensile strength of samples manufactured using the traditional method and the CIP method.
[0075] Referring to FIG. 12, a flowchart depicts a process 1200 for fabricating an anode electrode, according to aspects of the present disclosure. At block 1202, the process 1200 laminates a metal foil onto a substrate to form a supported web. For example, the metal foil may be a continuous roll of metal foil laminated onto the substrate to form the supported web. The metal foil may comprise any metal suitable for forming a metal anode layer for a battery cell. In an embodiment, the metal foil comprises a lithium foil.
[0076] At block 1204, the process 1200 removes selected portions of the supported web to form openings at predetermined intervals along a machine direction to form a patterned continuous web. In an embodiment, the patterning may be performed under the control of a PLC. The PLC may control a system to cut out removed portions to form the openings. The system may be a mechanical system such as a servo motor, a hydraulic system, or a pneumatic system for a punching station, to control movement of a laser, control a rotary die cutting tool, ablade cutting tool, or any other tool that can be used to remove portions of the supported web to form the openings.
[0077] At block 1206, the process 1200 laminates the patterned continuous web onto a continuous conductive substrate to form a patterned metal anode electrode comprising exposed regions of the continuous conductive substrate defined by the openings at predetermined intervals. In an embodiment, the substrate may be removed from the patterned continuous web such that the patterned metal foil is laminated onto the continuous conductive substrate.
[0078] In an embodiment, the continuous conductive substrate may be any type of conductive metal. For example, the continuous conductive substrate may be copper foil, nickel foil, stainless steel foil, or nickel-plated copper foil. In an embodiment, the continuous conductive substrate may be copper foil.
[0079] In some embodiments, the process 1200 may be repeated continuously until an end of the patterned continuous web is reached. For example, the supported web may be a large roll that is fed in a machine direction towards a machine (e.g„ a punching machine or a laser, as described above) that can perform the block 1204. The end of the roll is reached, the process 1200 may end.
[0080] Referring to FIG. 13. a flowchart depicts a process 1300 for fabricating an anode electrode, according to aspects of the present disclosure. At block 1302, the process 1300 laminates a metal foil onto a polymer substrate to form a supported web. For example, the metal foil may be a continuous roll of metal foil laminated onto the substrate to form the supported web. The metal foil may comprise any metal suitable for forming a metal anode layer for a battery cell. In an embodiment, the metal foil comprises a lithium foil.
[0081] At block 1304, the process 1300 removes selected portions of the supported web to form openings at predetermined intervals along a machine direction to form a patterned continuous web. In an embodiment, the patterning may be performed under the control of aPLC. The PLC may control a system to cut out removed portions to form the openings. The system may be a mechanical system such as a servo motor, a hydraulic system, or a pneumatic system for a punching station, to control movement of a laser, control a rotary die cutting tool, a blade cutting tool, or any other tool that can be used to remove portions of the supported web to form the openings.
[0082] At block 1306, the process 1300 slits one or more longitudinal edges of the patterned continuous web to remove peripheral buffer zones on both sides of the patterned continuous web, wherein the slitting is performed after the removing and before the laminating the patterned continuous web onto the continuous conductive substrate. In an embodiment, the block 1306 may be performed after block 1304 and before block 1308.
[0083] At block 1308, the process 1300 laminates the patterned continuous web onto a continuous conductive substrate to form a patterned metal anode electrode comprising exposed regions of the continuous conductive substrate defined by the openings at predetermined intervals. In an embodiment, the continuous conductive substrate may be any type of conductive metal. For example, the continuous conductive substrate may be copper foil, nickel foil, stainless steel foil, or nickel-plated copper foil. In an embodiment, the continuous conductive substrate may be copper foil.
[0084] At block 1310, the process 1300 separates the substrate from the patterned continuous web during the laminating onto the continuous conductive substrate. In other words, the substrate may be removed such that the patterned metal foil is laminated onto the continuous conductive substrate. In an embodiment, the block 1310 can be performed while the block 1308 is being performed. In other words, the block 1308 and the block 1310 can be performed at the same time or simultaneously.
[0085] In some embodiments, the process 1300 may be repeated continuously until an end of the patterned continuous web is reached. For example, the supported web may be a large roll that is fed in a machine direction towards a machine (e.g., a punching machine or a laser, asdescribed above) that can perform the block 1304. The end of the roll is reached, the process 1300 may end.
[0086] The disclosed process provides several practical advantages over conventional intermittent lamination approaches in which separate lithium pieces are individually transferred or placed onto a conductive substrate. By forming openings in a continuous lithium web prior to lamination, the useful patterned web remains mechanically continuous during handling and alignment, which may reduce misplacement, reduce variation in lithium amount from region to region, improve registration of the bare copper areas, and reduce scrap associated with defective transfer or misalignment. The subsequent edge-slitting stage may further improve dimensional control and cleanliness of the web prior to lamination. The controlled lamination stage may then produce a copper-supported patterned lithium electrode having repeatable bare copper regions, consistent bonding, and suitability for downstream tab formation, welding, customized notching, electrode punching, or incorporation into lithium metal batteries using liquid, semi-solid, or solid-state electrolytes.
[0087] Although particular embodiments, dimensions, process sequences, and example geometries have been described herein for purposes of illustration, the disclosed embodiments are not limited to the specific values, shapes, materials, or arrangements shown. The size, shape, spacing, and position of the punched openings may be varied; the carrier film and conductive substrate may be selected from a range of suitable materials; and the punching, slitting, and lamination equipment may be implemented using different control architectures and processing conditions. Accordingly, the disclosed embodiments are illustrative rather than limiting, and variations may be made without departing from the scope of the present disclosure as defined by the claims.
[0088] Furthermore, several implementations have been described. Nevertheless, it will be understood that various modifications may be made without departing from the spirit and scopeof the disclosure. Accordingly, other implementations are within the scope of the following claims.
Claims
CLAIMS1. A method, comprising:laminating a metal foil onto a polymer substrate to form a supported web;removing selected portions of the supported web to form openings at predetermined intervals along a machine direction to form a patterned continuous web; andlaminating the patterned continuous web onto a continuous conductive substrate to form a patterned metal anode electrode comprising exposed regions of the continuous conductive substrate defined by the openings at predetermined intervals.
2. The method of claim 1, wherein the supported web comprises a continuous roll that is advanced in the machine direction through a punching station.
3. The method of claim 1, further comprising:separating the polymer substrate from the patterned continuous web during the laminating onto the continuous conductive substrate.
4. The method of claim 1, wherein the metal foil comprises lithium metal.
5. The method of claim 1 , wherein the substrate comprises a polymer carrier film comprising at least one of: polyethylene terephthalate (PET), polypropylene (PP), polyethylene (PE), polyimide (PI), or a multilayer structure comprising a combination thereof.
6. The method of claim 1, wherein the continuous conductive substrate comprises at least one of: copper foil, nickel foil, stainless steel foil, or nickel-plated copper foil.
7. The method of claim 1, wherein the openings have a rectangular shape or a square shape sized to accommodate lead tab welding.
8. The method of claim 1, further comprising:slitting one or more longitudinal edges of the patterned continuous web to remove peripheral buffer zones on both sides of the patterned continuous web, wherein the slitting is performed after the removing and before the laminating the patterned continuous web onto the continuous conductive substrate, to form the patterned continuous web having a uniform width.
9. The method of claim 1, wherein the laminating the patterned continuous web onto the continuous conductive substrate is performed under a controlled pressure and a controlled temperature to ensure mechanical adhesion.
10. The method of claim 1, wherein the removing is performed via at least one of: mechanically punching, laser cutting, or laser ablation.
11. A patterned metal anode electrode, comprising:a continuous conductive substrate; anda continuous metal anode layer laminated onto the conductive substrate in a center-intermittent configuration, wherein the continuous metal anode layer comprises:periodically spaced openings along a machine direction of the continuous conductive substrate;uniform longitudinal edges; andat least one exposed region of the continuous conductive substrate defined by the periodically spaced openings, wherein the at least one exposed region is configured to accommodate lead tab welding.
12. The patterned metal anode electrode of claim 11, wherein the continuous metal anode layer comprises lithium metal.
13. The patterned metal anode electrode of claim 11, wherein the continuous conductive substrate comprises at least one of: copper foil, nickel foil, stainless steel foil, or nickel-plated copper foil.
14. The patterned metal anode electrode of claim 11 , wherein the at least one exposed region of the continuous conductive substrate is located at a left side, a right side, or a center of a portion of the continuous metal anode layer associated with the at least one exposed region.
15. The patterned metal anode electrode of claim 11, wherein the continuous metal anode layer comprises a flush top surface relative to the continuous conductive substrate for a uniform electrode thickness.
16. The patterned metal anode electrode of claim 11, wherein the periodically spaced openings are spaced at fixed intervals along the machine direction of the continuous metal anode layer.
17. The patterned metal anode electrode of claim 16, wherein the fixed intervals each comprise approximately 562 millimeters (mm).
18. The patterned metal anode electrode of claim 11, wherein the periodically spaced openings comprise a rectangular shape or a square shape.
19. The patterned metal anode electrode of claim 11, wherein the uniform longitudinal edges are formed via a slitting process.
20. The patterned metal anode electrode of claim 11, further comprising:a final width of approximately 160 millimeters (mm).