Compressor blade tenon ultrasonic shot peening composite strengthening device and composite strengthening method

Through three-dimensional modeling and EDEM simulation, the structure of the shot peening chamber is optimized, combined with ball bearings and vibrating heads, to solve the problems of shot accumulation and poor uniformity in blade tenon shot peening, achieving uniform strengthening and stress distribution on the blade tenon surface, and improving Improve the performance of aero-engine blade parts.

CN118744403AActive Publication Date: 2024-10-08SHANGHAI FENGYUN AVIATION TECH CO LTD

Patent Information

Application Number
CN202410988301.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-10-08
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

During the shot peening process of compressor blade tenons, there are problems such as shot accumulation and poor uniformity of shot peening, resulting in uneven stress distribution in the strengthened area, making it difficult to improve the fatigue and corrosion resistance of the blade tenons.

Method used

Three-dimensional modeling software was used to establish the model of the blade tenon and ultrasonic shot peening device. Discrete element simulation was performed through EDEM software to optimize the shot peening chamber structure and parameters. Horizontal and vertical shot peening chambers were designed, combined with ball bearings and vibration. head to achieve uniform shot peening and secondary strengthening treatment of the blade tenon surface.

Benefits of technology

It improves the strength and stress distribution uniformity of the blade tenon surface, overcomes the problems of high roughness and projectile accumulation in traditional shot peening, and enhances the performance of aeroengine blade parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744403A_ABST
    Figure CN118744403A_ABST
Patent Text Reader

Abstract

The invention discloses an ultrasonic shot peening composite strengthening device and method for a blade tenon of a gas compressor, and the method comprises the steps: firstly building the blade tenon and the ultrasonic shot peening composite strengthening device through three-dimensional software, and then building a blade tenon ultrasonic shot peening discrete element simulation model based on EDEM software; analyzing the shot peening coverage rate condition of each area on the surface of the tenon after the blade tenon is subjected to shot peening strengthening by adopting the shot peening chamber in the ultrasonic shot peening strengthening device which is established for the first time, and optimally designing the shot peening chamber and shot peening parameters according to an analysis result until a simulation data result meets product requirements; then blade tenon ultrasonic shot peening composite strengthening chamber machining and blade tenon surface strengthening treatment are conducted; the shot blasting chamber comprises the transverse shot blasting chamber and the vertical shot blasting chamber, shot blasting is conducted on the surface of the stress contact area of the blade tenon through the transverse shot blasting chamber, then secondary strengthening treatment is conducted on the area where shot blasting is insufficient through the vertical shot blasting chamber, and the shot blasting uniformity of the blade tenon is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of metal surface shot peening strengthening, and in particular to an ultrasonic shot peening composite strengthening device and a composite strengthening method for compressor blade tenons. Background Art

[0002] Blades are key components of aircraft engines. During service, they are subjected to great pressure from the tenon groove of the compressor disc. The arc end face stress contact area is very prone to micro-wear failure, so it is very important to strengthen the surface of the blade tenon. The blade tenon is a complex and special-shaped structure with narrow corner area and semi-shielded and other characteristic structures. Due to the limitation of geometric dimensions, traditional surface strengthening processes such as shot peening and sand blasting are prone to cause problems such as shot accumulation, high roughness, and uneven surface strengthening, which in turn leads to uneven stress distribution in the strengthening area and easy deformation. Therefore, ensuring the uniformity of shot peening is the main difficulty in shot peening strengthening of blade tenons.

[0003] Ultrasonic shot peening is to repeatedly hit the surface of the tenon with high-speed projectiles, causing plastic deformation of the surface layer. Reasonable use of the introduction of residual compressive stress can improve the fatigue resistance and corrosion resistance of the tenon surface. However, there are also certain problems in the use of ultrasonic shot peening on blade tenons: it is difficult for the projectiles to directly impact the surface of the tenon shielding area during the shot peening process for blade tenons with complex special-shaped structures, resulting in projectile accumulation and poor shot peening uniformity during the shot peening process.

[0004] In order to solve the above technical problems, Chinese invention patent CN202211386840.7 discloses an ultrasonic shot peening strengthening device for the tenon of an aircraft engine compressor wheel, the device comprising a workbench; a compressor wheel clamping device arranged on the workbench, the compressor wheel clamping device being connected to a compressor wheel having a tenon, for adjusting the horizontal angle of the compressor wheel and controlling the rotation of the compressor wheel; a slide module fixed on the workbench, the slide module having a slider that can be adjusted vertically; a bracket mounted on the slider; and a shot peening chamber and an ultrasonic vibration device fixed on the bracket, the shot peening chamber having an opening on the upper side and a through hole on the lower side, the upper side opening of the shot peening chamber being adapted to the tenon of the compressor wheel, the ultrasonic vibration device having a vibration head, the vibration head partially extending into the through hole on the lower side of the shot peening chamber, and the vibration excitation of the projectile by the vibration head of the ultrasonic vibration device is realized by injecting a predetermined number of projectiles into the shot peening chamber.

[0005] Although the above patent document designs a special shot peening chamber for the tenon of the compressor impeller and uses ultrasonic shot peening technology to perform shot peening on the tenon, thereby improving the surface strength of the tenon, evenly distributing stress in the tenon area, and improving the fatigue strength performance of the compressor impeller of the aircraft engine, and solves the problem of uneven stress distribution in the strengthening area of ​​complex components after traditional shot peening, the device has a complex structure and high manufacturing cost, and it mainly performs shot peening on the tenon of the impeller, and is difficult to apply to other parts of the blade tenon, such as the obstructed parts such as the end face of the blade edge plate near the tenon.

[0006] Therefore, the problems of shot accumulation and poor shot peening uniformity in the current compressor blade tenon shot peening process have not been well solved. It is necessary to propose a new solution to improve the performance of the compressor blade tenon. Summary of the invention

[0007] The present application provides a compressor blade tenon ultrasonic shot peening composite strengthening device and a composite strengthening method, which are used to solve the problems of shot accumulation and poor shot peening uniformity in the existing compressor blade tenon during the shot peening strengthening process.

[0008] In order to achieve the above objectives, this application provides the following technical solutions:

[0009] In a first aspect, the present application provides a method for ultrasonic shot peening composite strengthening of a compressor blade tenon, comprising the following steps:

[0010] S1: Using 3D modeling software to build a 3D model according to the actual size of the blade tenon parts and the ultrasonic shot peening strengthening device, the ultrasonic shot peening strengthening device includes a shot peening chamber, a blade fixture, a ball bearing and a vibration head;

[0011] S2: importing the three-dimensional model established in step S1 into EDEM software, establishing a projectile model and a discrete element simulation model of ultrasonic shot peening strengthening of the blade tenon in the EDEM software, and performing ultrasonic shot peening simulation of the blade tenon using the simulation model to obtain a simulation result;

[0012] S3: using the simulation results obtained in step S2 to analyze the shot peening coverage of each area on the surface of the tenon after the blade tenon is shot peened by the shot peening chamber established for the first time, if the coverage is not up to standard, returning to step S1 to optimize the shot peening chamber, if it is up to standard, performing shot peening chamber processing and surface strengthening treatment;

[0013] S4: performing secondary strengthening treatment on the blade tenon which is unevenly shot peened in step S3;

[0014] Among them, the shot peening chamber includes a horizontal shot peening chamber and a vertical shot peening chamber. The vertical shot peening chamber is used to perform surface composite reinforcement on the blade tenon that is unevenly shot peened in the horizontal shot peening chamber; or, the horizontal shot peening chamber is used to perform surface composite reinforcement on the blade tenon that is unevenly shot peened in the vertical shot peening chamber.

[0015] In the above technical solution, in step S1, UG software is used to establish a three-dimensional model in 1:1 according to the actual size of the blade tenon part and the ultrasonic shot peening strengthening device, and the three-dimensional model is exported in a format that can be opened by EDEM software.

[0016] Furthermore, in step S2, when establishing the projectile model and the blade tenon ultrasonic shot peening discrete element simulation model, the model material properties, collision model and collision properties are set.

[0017] Furthermore, the performance parameters of the blade tenon, shot peening chamber, vibration head and projectile are written into the model material property module of the EDEM software. The performance parameters include material, Poisson's ratio, shear modulus, density and gravity.

[0018] Furthermore, the materials of the blade tenon, shot peening chamber and vibration head are all TC17.

[0019] Furthermore, the Poisson's ratio of the blade tenon, the shot peening chamber and the vibration head is 0.33.

[0020] Furthermore, the shear modulus of the blade tenon, shot peening chamber, and vibration head are all 4.397×10 4 GPa.

[0021] Furthermore, the density of the blade tenon, shot peening chamber and vibration head is 4.5g / cm 3 .

[0022] Furthermore, the material of the projectile is ZrO2, the Poisson's ratio is 0.3, and the shear modulus is 8.4×10 4 GPa, density 6.0g / cm 3 .

[0023] Furthermore, the gravity of the blade tenon, shot peening chamber, vibrating head and projectile is 9.8m / s 2 .

[0024] Furthermore, in the EDEM software, the collision model between the projectile and the blade tenon and the collision model between the projectile and the projectile are both the default models of the EDEM software.

[0025] Furthermore, the material of the projectile-blade tenon collision model is ZrO2-TC17, and the restitution coefficient of the projectile-blade tenon collision model is 0.6; the material of the projectile-projectile collision model is ZrO2-ZrO2, and the restitution coefficient of the projectile-projectile collision model is 0.8.

[0026] Furthermore, when the simulation model is used to perform ultrasonic shot peening simulation of the blade tenon in step S2, the discrete element simulation parameters of the ultrasonic shot peening strengthening of the blade tenon are set as follows: the shot material is zirconia, the shot diameter is 2.5 mm, the number of shots is 300, the amplitude of the vibration head is 0.06 mm, and the frequency is 20 kHz.

[0027] Furthermore, in step S3, the simulation results obtained in step S2 are used to analyze the collision conditions of each area on the surface of the projectile-blade tenon, the distribution of the projectile-blade tenon collision points is observed and counted, and the distribution results of the shot peening coverage rate of each area on the tenon surface are calculated; if the coverage rate does not meet the standard, return to step S1 and optimize the shot peening chamber structure through the simulation results.

[0028] Furthermore, the horizontal shot peening chamber is a cylindrical chamber, a mounting hole is provided on the side wall of the horizontal shot peening chamber, a ball bearing is arranged in the mounting hole, the blade clamp is installed in the ball bearing, the blade tenon part to be shot peened is clamped by the blade clamp, a vibration head is installed on a bottom wall of the horizontal shot peening chamber, and the installed blade tenon part and the vibration head are arranged relative to each other; the central axes of the blade tenon part, the blade clamp and the ball bearing are collinear; during the shot peening process, the blade tenon part is driven to rotate at a uniform speed along its own axis, and when the working surface of the tenon faces the vibration head, the tenon stops rotating for a preset time, and the discrete element simulation time of the blade tenon ultrasonic shot peening is set to 20s; the inner cavity size of the horizontal shot peening chamber is φ51mm×100mm.

[0029] Furthermore, the vertical shot peening chamber is a cylindrical chamber, a mounting hole is provided on a bottom wall of the vertical shot peening chamber, a ball bearing is arranged in the mounting hole, a blade clamp is installed in the ball bearing, a blade tenon part to be shot peened is clamped by the blade clamp, a vibration head is installed on the other bottom wall of the vertical shot peening chamber, and the installed blade tenon part and the vibration head are arranged at a relative interval; the central axis of the blade tenon part, the blade clamp, the ball bearing and the vertical shot peening chamber are collinear.

[0030] Furthermore, when the surface of the blade tenon that is unevenly shot peened in the horizontal shot peening chamber is compositely strengthened by the vertical shot peening chamber, the blade clamp drives the fixed blade tenon installed thereon into the vertical shot peening chamber so that the blade tenon is 50 mm away from the surface of the vibration head; the inner cavity size of the vertical shot peening chamber is φ51mm×100mm.

[0031] Furthermore, the materials of the blade tenon, the shot peening chamber and the vibration head are all titanium alloy, and the material of the projectile is zirconia ceramic material.

[0032] In the second aspect, the present application provides a compressor blade tenon ultrasonic shot peening composite strengthening device, including a shot peening chamber, a vibration head, a ball bearing and a blade clamp; the shot peening chamber includes a horizontal shot peening chamber and a vertical shot peening chamber, and the structure and size of the horizontal shot peening chamber as well as the structure and size of the vertical shot peening chamber are determined according to the above-mentioned compressor blade tenon ultrasonic shot peening composite strengthening method.

[0033] Compared with the prior art, this application has at least the following beneficial effects:

[0034] Based on further analysis and research on the existing technical problems, the present application recognizes that the current compressor blade tenon shot peening strengthening process has problems such as shot accumulation and poor shot peening uniformity. To this end, the present application provides a compressor blade tenon ultrasonic shot peening composite strengthening device and a composite strengthening method. The composite strengthening method first establishes a blade tenon and an ultrasonic shot peening strengthening device in a 1:1 ratio through three-dimensional software, and then establishes a blade tenon ultrasonic shot peening discrete element simulation model based on EDEM software, analyzes the shot peening coverage of each area on the tenon surface after the blade tenon is shot peened by the shot peening chamber established for the first time, and optimizes the design of the shot peening chamber and shot peening parameters according to the analysis results until the simulation data results meet the product requirements, and then the blade tenon ultrasonic Shot peening composite strengthening chamber processing and blade tenon surface strengthening treatment. The composite strengthening method provided in this application can accurately produce a shot peening chamber that meets production needs; in addition, the shot peening chamber in this application includes a horizontal shot peening chamber and a vertical shot peening chamber. The horizontal shot peening chamber can be used to uniformly shot peen the surface of the force contact area of ​​the blade tenon, and then the vertical shot peening chamber can be used to perform secondary strengthening treatment on the insufficiently shot peened area. The compressor blade tenon ultrasonic shot peening composite strengthening method provided in this application overcomes the problems of high blade surface roughness, shot accumulation, and poor shot peening uniformity during shot peening strengthening, improves the surface strength of the tenon, and evens out the stress distribution on the tenon surface, thereby achieving the purpose of improving the performance of aircraft engine blade parts. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.

[0036] The structures, proportions, sizes, etc. illustrated in this specification are only used to match the contents disclosed in the specification so as to facilitate understanding and reading by persons familiar with the technology. They are not used to limit the conditions under which the present invention can be implemented, and therefore have no substantial technical significance. Any structural modification, change in proportion or adjustment of size shall still fall within the scope of the technical contents disclosed in the present invention without affecting the effects and purposes that can be achieved by the present invention.

[0037] Figure 1 It is a flow chart of a compressor blade tenon ultrasonic shot peening composite strengthening method provided by the present application in an embodiment;

[0038] Figure 2 This is a software interface diagram showing the use of EDEM software to build a projectile model. The sphere in the figure is a schematic diagram of the projectile model built by the software;

[0039] Figure 3 A schematic diagram of a simulation effect of a blade tenon discrete element simulation model established using EDEM software in an embodiment, wherein the simulation model shows the effect of ultrasonic shot peening of the blade tenon in a horizontal shot peening chamber;

[0040] Figure 4 This is a schematic diagram of the structure of an ultrasonic shot peening composite strengthening device provided by the present application in an embodiment, wherein the shot peening chamber in the figure is a horizontal shot peening chamber;

[0041] Figure 5 (a) is a schematic diagram of the shot peening effect of a blade tenon in a YZ view obtained by using a compressor blade tenon ultrasonic shot peening composite strengthening method provided by the present application in an embodiment; (b) is a schematic diagram of the shot peening effect of a blade tenon in an XZ view obtained by using a compressor blade tenon ultrasonic shot peening composite strengthening method provided by the present application in an embodiment;

[0042] Figure 6 A schematic diagram of a blade tenon structure in a compressor blade tenon ultrasonic shot peening composite strengthening method provided by the present application in an embodiment;

[0043] Figure 7 This is a schematic structural diagram of an ultrasonic shot peening composite strengthening device provided by the present application in an embodiment, and the shot peening chamber in the figure is a vertical shot peening chamber.

[0044] Explanation of the reference numerals: 1. Horizontal shot peening chamber; 2. Blade tenon part; 21. Bottom surface of blade tenon; 22. Surface of force contact area of ​​blade tenon; 23. End surface of blade edge plate near tenon; 24. Working surface of blade tenon; 3. Vibrating head; 4. Ball bearing; 5. Blade clamp; 6. Vertical shot peening chamber. DETAILED DESCRIPTION

[0045] The inventors have realized in the production practice in this field that it is difficult for the projectiles to directly impact the surface of the shielded area of ​​the tenon during the current ultrasonic shot peening process, so the uniformity of the blade tenon shot peening is poor. In order to solve the problems existing in the prior art, the inventors have proposed this application in combination with the actual production and considering the production cost, so as to overcome the problems of projectile accumulation and poor uniformity of shot peening during the shot peening of the existing complex and special-shaped structural parts of the aero-engine. The present application provides a compressor blade tenon ultrasonic shot peening composite strengthening device and a composite strengthening method. The composite strengthening method mainly designs an ultrasonic shot peening strengthening combined chamber based on the shape, size and material properties of the tenon, combines discrete element simulation to analyze the shot peening coverage of the tenon surface, optimizes the design of the shot peening chamber structure according to the distribution, optimizes the ultrasonic shot peening strengthening combined chamber that meets the requirements, and then performs chamber processing, and uses the ultrasonic shot peening composite strengthening method to perform shot peening treatment on the tenon surface, solves the problems of projectile accumulation and uneven surface shot peening, thereby improving the surface strength of the tenon, uniformly distributing the stress in the tenon area, and achieving the purpose of improving the performance of aero-engine blade parts.

[0046] The present application is further described below in detail through specific embodiments in conjunction with the accompanying drawings.

[0047] Embodiment 1

[0048] This embodiment provides a method for ultrasonic shot peening composite strengthening of compressor blade tenons. Figure 1 The following is a detailed description of the steps of the ultrasonic shot peening composite strengthening method for the compressor blade tenon:

[0049] 1. Use UG software to establish a three-dimensional model according to the actual size of the blade tenon parts and the ultrasonic shot peening strengthening device. The ultrasonic shot peening strengthening device includes a shot peening chamber, a blade fixture, a ball bearing and a vibration head. The three-dimensional model is preferably established at a ratio of 1:1. Of course, in addition to UG software, other three-dimensional modeling software that can establish three-dimensional models can also be used, such as SolidWorks software.

[0050] 2. The three-dimensional models of the parts and the ultrasonic shot peening device established using UG software are exported in igs format files respectively. The exported files include at least the solid models of the shot peening chamber, blades, vibration head, ball bearing and blade fixture.

[0051] 3. Import the above igs format file into EDEM software and build a projectile model in EDEM software (such as Figure 2 ), establish a discrete element simulation model for ultrasonic shot peening of blade tenons, set the model material properties, collision model and collision properties, and finally establish Figure 3 The discrete element simulation model of the blade tenon is shown.

[0052] 4. Analyze the collision conditions of the projectile and blade tenon surface in various areas based on the simulation results, and observe and count the distribution of the projectile and blade tenon collision points. Figure 5 (a) and (b) are schematic diagrams of the shot peening effect of the blade tenon obtained by using the ultrasonic shot peening composite strengthening method for the compressor blade tenon provided in the present application in an embodiment.

[0053] 5. Based on the observed and statistical distribution of the projectile-blade tenon collision points, calculate the distribution results of the shot peening coverage rate of each area on the tenon surface.

[0054] 6. The distribution of the projectile-blade tenon collision point and the shot peening coverage distribution results of each area on the tenon surface are obtained from the above steps. According to the product requirements, it is determined whether it is necessary to optimize the structure of the blade tenon ultrasonic shot peening chamber, whether it is necessary to optimize the tenon rotation speed a (the unit of the tenon rotation speed a is: revolutions / minute), and whether it is necessary to optimize the tenon pause time b (the pause time b is the pause rotation time when the tenon working surface faces the vibration head, in minutes).

[0055] 7. If the simulation data results do not meet the product requirements, repeat the above steps 1 to 6, optimize the shot peening chamber structure through the simulation analysis results, and also optimize the shot peening parameters in the EDEM software (the shot peening parameters are at least the tenon speed a and the tenon pause time b) until the simulation data results meet the product requirements;

[0056] 8. If the simulation data results meet the product requirements, the ultrasonic shot peening composite strengthening test of the blade tenon is completed, and the control parameters of the surface strengthening treatment test and the processing plan of the strengthening chamber are determined.

[0057] In the above step 3, the performance parameters such as Poisson's ratio, shear modulus, density, etc. of the blade tenon, shot peening chamber, vibration head and projectile are written into the model material property module of the EDEM software. In one embodiment, the specific parameters are shown in Table 1 below:

[0058] Table 1 Material properties

[0059]

[0060] In this embodiment, the materials of the blades, shot peening chamber and vibration head are all titanium alloy, and the medium material of the projectile is zirconia ceramic material.

[0061] The default model used in the EDEM software is Hertz-Mindlin (no slip), which is accurate and efficient in force calculation. In the above step 3, the collision model assigned to the projectile-blade tenon in the EDEM software is Hertz-Mindlin (no slip), and the collision model assigned to the projectile-projectile is Hertz-Mindlin (no slip), and the projectile-blade tenon restitution coefficient, projectile-projectile restitution coefficient, static friction coefficient, and rolling friction coefficient are set. In one embodiment, the collision properties are shown in Table 2 below:

[0062] Table 2 Collision properties

[0063] Collision Objects Projectile-Blade Tenon Projectile-Projectile Material <![CDATA[ZrO2-TC17]]> <![CDATA[ZrO2-ZrO2]]> Coefficient of restitution 0.6 0.8

[0064] In the above step 3, the discrete element simulation parameters of the ultrasonic shot peening strengthening of the blade tenon are: the shot material is zirconium oxide (ZrO2), the shot diameter is 2.5mm, the number of shots is 300, the vibration head amplitude is 0.06mm, and the frequency is 20kHz.

[0065] After the establishment of the discrete element simulation model of ultrasonic shot peening strengthening of blade tenon, motion simulation is carried out. During the blade tenon shot peening process, the blade tenon rotates at a constant speed along its own axis. When the tenon working surface (which can be understood as the surface to be shot peened) rotates toward the vibration head, it stops rotating for a period of time and performs shot peening. The discrete element simulation time of ultrasonic shot peening of blade tenon is set to 20s. The collision of projectiles and various areas on the surface of blade tenon is analyzed by simulation calculation results. In order to facilitate the observation of the distribution of projectile-blade tenon collision points, the contact points are enlarged by 2 times. The structural dimensions of the shot peening chamber are optimized by simulation analysis results until the simulation analysis results meet the requirements. At this time, the structural dimensions of the shot peening chamber are the structural dimensions of the target shot peening chamber to be processed.

[0066] Therefore, the ultrasonic shot peening composite strengthening method for the compressor blade tenon provided in the present application first establishes the blade tenon and the ultrasonic shot peening strengthening device in a 1:1 ratio through UG software, and then establishes a discrete element simulation model of the blade tenon ultrasonic shot peening based on EDEM software, and analyzes the shot peening coverage of each area on the tenon surface after the blade tenon is shot peened by the shot peening chamber established for the first time, and optimizes the design of the shot peening chamber and shot peening parameters according to the analysis results until the simulation data results meet the product requirements, and then performs ultrasonic shot peening composite strengthening chamber processing of the blade tenon and surface strengthening treatment of the blade tenon. The composite strengthening method provided in the present application can be used In order to accurately produce a shot peening chamber that can meet production needs; in addition, the shot peening chamber in the present application includes a horizontal shot peening chamber and a vertical shot peening chamber. The horizontal shot peening chamber can be used to uniformly shot peen the surface of the force contact area of ​​the blade tenon, and then the vertical shot peening chamber can be used to perform secondary strengthening treatment on the insufficiently shot peened area. The ultrasonic shot peening composite strengthening method for the compressor blade tenon provided in the present application overcomes the problems of high blade surface roughness, shot accumulation, and poor shot peening uniformity during the shot peening strengthening process, improves the surface strength of the tenon, and evens out the stress distribution on the tenon surface, thereby achieving the purpose of improving the performance of aircraft engine blade parts.

[0067] Embodiment 2

[0068] The present embodiment provides an ultrasonic shot peening composite strengthening device, which includes a shot peening chamber, a vibration head, a ball bearing and a blade clamp, wherein the shot peening chamber includes a horizontal shot peening chamber and a vertical shot peening chamber, and the structure and size of the horizontal shot peening chamber and the vertical shot peening chamber are determined by the compressor blade tenon ultrasonic shot peening composite strengthening method provided in Example 1.

[0069] In this embodiment, the horizontal shot peening chamber is a cylindrical chamber, a mounting hole is provided on the side wall of the cylindrical chamber, a ball bearing is arranged in the mounting hole, a blade fixture is installed in the ball bearing, a blade tenon part to be shot peened is clamped by the blade fixture, a vibration head is installed on a bottom wall of the horizontal shot peening chamber, and the installed blade tenon part and the vibration head are arranged relative to each other, such as Figure 4 The central axes of the blade tenon parts, blade fixture and ball bearing are collinear. During the shot peening process, the blade tenon parts are driven to rotate at a uniform speed along their own axis. When the working surface of the tenon faces the vibration head, the tenon stops rotating for a while. The discrete element simulation time of the blade tenon ultrasonic shot peening is set to 20s.

[0070] In the present application, the blade tenon part 2 is inserted into the blade fixture 5, the blade fixture 5 is inserted into the ball bearing 4, and the roller bearing 4 is inserted into the horizontal shot peening chamber 1 to avoid the leakage of the projectile during the ultrasonic shot peening process. The axes of the blade tenon part 2, the blade fixture 5 and the ball bearing 4 are arranged on the same axis, which can ensure that the blade tenon part 2 can rotate at a constant speed along its own axis during the shot peening process.

[0071] In one embodiment, a discrete element simulation model of ultrasonic shot peening for blade tenons is established according to the parameters provided in the first embodiment, motion simulation is performed through the discrete element simulation model of ultrasonic shot peening for blade tenons, and the structure of the horizontal shot peening chamber is optimized through the simulation analysis results. Figure 5 Figure (a) in the figure corresponds to Figure 4 , 6 The shot peening effect on the surface of the blade tenon is analyzed. The blade tenon is facing the vibration head. The collision points on the surface 22 of the blade tenon force contact area are evenly distributed and dense, while the collision points on the bottom surface 21 of the blade tenon, the end surface 23 of the blade edge plate near the tenon, and the working surface 24 of the blade tenon are relatively sparse. Therefore, the structure of the horizontal shot peening chamber is further optimized, so that the collision points on the surface of the blade tenon force contact area are evenly distributed and dense, and the collision points on the bottom surface of the blade tenon and the end surface of the blade edge plate near the tenon are relatively sparse. Finally, the horizontal shot peening chamber is determined to be a cylindrical chamber with an inner cavity size of φ51mm×100mm.

[0072] In the horizontal shot peening chamber of the present application, the collision points on the bottom surface of the blade tenon and the end surface of the blade edge plate near the tenon are relatively sparsely distributed. Therefore, the present application performs secondary shot peening strengthening treatment on the bottom surface of the blade tenon and the end surface of the blade edge plate near the tenon by setting up a vertical shot peening chamber.

[0073] In this embodiment, the vertical shot peening chamber is a cylindrical chamber, a mounting hole is opened on a bottom wall of the cylindrical chamber, a ball bearing is arranged in the mounting hole, the blade clamp is installed in the ball bearing, the blade tenon part to be shot peened is clamped by the blade clamp, and a vibration head is installed on the other bottom wall of the vertical shot peening chamber, and the installed blade tenon part and the vibration head are arranged relative to each other.

[0074] Specifically, the vertical shot peening chamber structure is as follows Figure 7 As shown, the blade tenon part 2 is inserted into the blade fixture 5, the blade fixture 5 is inserted into the ball bearing 4, and the roller bearing 4 is inserted into the vertical shot peening chamber 6 to avoid leakage of the projectile during the ultrasonic shot peening process. The central axes of the blade tenon part 2, the blade fixture 5 and the ball bearing 4 are located on the same straight line. Furthermore, during the secondary shot peening process, the blade tenon part 2 is fixed, and the blade fixture 5 drives the blade tenon part 2 to penetrate into the vertical shot peening chamber 6, so that the blade tenon part 2 is at a position 50 mm away from the surface of the vibration head 3.

[0075] In one embodiment, a discrete element simulation model of ultrasonic shot peening strengthening of the blade tenon is established according to the parameters provided in Example 1, motion simulation is performed through the discrete element simulation model of ultrasonic shot peening strengthening of the blade tenon, and the structure of the vertical shot peening chamber is optimized through the simulation analysis results. Finally, it is determined that the vertical shot peening chamber is a cylindrical chamber with an inner cavity size of φ51mm×100mm.

[0076] The blade clamp in the present application can use conventional clamps in the art, as long as it can meet the use requirements of the present application.

[0077] Therefore, the ultrasonic shot peening composite strengthening method for the compressor blade tenon provided in the present application is a method of continuous simulation and optimization. A discrete element simulation model of the blade tenon ultrasonic shot peening is established based on EDEM software, and the shot peening coverage of each area on the tenon surface after the blade tenon is shot peened in a horizontal shot peening chamber or a vertical shot peening chamber is analyzed. The horizontal shot peening chamber and shot peening parameters are optimized and designed according to the analysis results, or the vertical shot peening chamber and shot peening parameters are optimized and designed according to the analysis results. The horizontal shot peening chamber and the vertical shot peening chamber are used in combination to perform secondary strengthening treatment on the insufficiently shot peened areas. That is, the present application adjusts the simulation conditions through feedback from the simulation results, and finally obtains the structural dimensions of the target product that can meet the design requirements.

[0078] When the present application counts the distribution of the projectile-blade tenon collision points and calculates the distribution of the shot peening coverage rate of each area on the tenon surface, if it is analyzed from the shot peening effect on the blade tenon surface that the collision points on the surface 22 of the blade tenon facing the vibration head, that is, the blade tenon force contact area, are evenly and densely distributed, and the collision points on the blade tenon bottom surface 21, the blade edge plate near the tenon end surface 23 and the blade tenon working surface 24 are relatively sparsely distributed, then it is considered that the simulation data results do not meet the product requirements, and the horizontal shot peening chamber will be further optimized.

[0079] In summary, the ultrasonic shot peening composite strengthening method for the compressor blade tenon provided in the present application can design an ultrasonic shot peening strengthening combined chamber according to the structural dimensions and material properties of the blade tenon, combine discrete element simulation to analyze the shot peening coverage rate of the tenon surface, and use ultrasonic shot peening composite strengthening technology to perform shot peening strengthening treatment on the shielding structure of the blade tenon working surface. The chamber structure and shot peening parameters are optimized and designed, overcoming the problems of high roughness, shot accumulation, and poor shot peening uniformity in the shot peening strengthening process of existing complex and special-shaped structural parts of aircraft engines, so as to improve the surface strength of the tenon and evenly distribute the stress on the tenon surface, thereby achieving the purpose of improving the performance of aircraft engine blade parts.

[0080] The technical features of the above embodiments may be arbitrarily combined (as long as there is no contradiction in the combination of these technical features). To make the description concise, not all possible combinations of the technical features in the above embodiments are described; these embodiments that are not explicitly written should also be considered to be within the scope of this specification.

[0081] The above is a relatively specific and detailed description of the present application through general description and specific embodiments. It should be understood that, based on the technical concept of the present application, several conventional adjustments or further innovations can be made to these specific embodiments; however, as long as they do not deviate from the technical concept of the present application, the technical solutions obtained by these conventional adjustments or further innovations also fall within the scope of protection of the claims of the present application.

Claims

1. A method for ultrasonic shot peening composite strengthening of compressor blade tenons, characterized in that: The steps include: S1: Using 3D modeling software to build a 3D model according to the actual size of the blade tenon parts and the ultrasonic shot peening strengthening device, the ultrasonic shot peening strengthening device includes a shot peening chamber, a blade fixture, a ball bearing and a vibration head; S2: importing the three-dimensional model established in step S1 into EDEM software, establishing a projectile model and a discrete element simulation model of ultrasonic shot peening strengthening of the blade tenon in the EDEM software, and performing ultrasonic shot peening simulation of the blade tenon using the simulation model to obtain a simulation result; S3: using the simulation results obtained in step S2 to analyze the shot peening coverage of each area on the surface of the tenon after the blade tenon is shot peened by the shot peening chamber established for the first time, if the coverage is not up to standard, returning to step S1 to optimize the shot peening chamber, if it is up to standard, performing shot peening chamber processing and surface strengthening treatment; S4: performing secondary strengthening treatment on the blade tenon which is unevenly shot peened in step S3; Among them, the shot peening chamber includes a horizontal shot peening chamber and a vertical shot peening chamber, the vertical shot peening chamber is used to perform surface composite reinforcement on the blade tenon that is unevenly shot peened in the horizontal shot peening chamber; or, the horizontal shot peening chamber is used to perform surface composite reinforcement on the blade tenon that is unevenly shot peened in the vertical shot peening chamber.

2. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1 is characterized in that: In step S1, UG software is used to establish a 3D model in accordance with the actual size of the blade tenon part and the ultrasonic shot peening strengthening device at a ratio of 1:1, and the 3D model is exported in a format that can be opened by EDEM software.

3. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1, characterized in that: In step S2, when establishing the projectile model and the blade tenon ultrasonic shot peening discrete element simulation model, the model material properties, collision model and collision properties are set.

4. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 3 is characterized in that: In the model material property module of the EDEM software, write the performance parameters of the blade tenon, shot peening chamber, vibration head and projectile, the performance parameters including material, Poisson's ratio, shear modulus, density and gravity; The blade tenon, shot peening chamber and vibration head are all made of TC17; The Poisson's ratio of the blade tenon, shot peening chamber and vibration head is 0.33; The shear modulus of the blade tenon, shot peening chamber and vibration head are all 4.397×10 4 GPa; The density of the blade tenon, shot peening chamber and vibration head is 4.5g / cm 3 ; The material of the projectile is ZrO2, the Poisson's ratio is 0.3, and the shear modulus is 8.4×10 4 GPa, density 6.0g / cm 3 ; The gravity of the blade tenon, shot peening chamber, vibrating head and projectile is 9.8m / s 2 .

5. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 3 is characterized in that: In EDEM software, the collision model between projectile and blade tenon and the collision model between projectile and projectile are both the default models of EDEM software; The material of the collision model between projectile and blade tenon is ZrO2-TC17, and the coefficient of restitution of the collision model between projectile and blade tenon is 0.6; the material of the collision model between projectile and projectile is ZrO2-ZrO2, and the coefficient of restitution of the collision model between projectile and projectile is 0.8; When the simulation model is used to simulate the ultrasonic shot peening of the blade tenon in step S2, the discrete element simulation parameters of the ultrasonic shot peening strengthening of the blade tenon are set as follows: the shot material is zirconia, the shot diameter is 2.5 mm, the number of shots is 300, the amplitude of the vibration head is 0.06 mm, and the frequency is 20 kHz.

6. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1, characterized in that: In step S3, the simulation results obtained in step S2 are used to analyze the collision conditions of each area on the surface of the projectile-blade tenon, the distribution of the projectile-blade tenon collision points is observed and counted, and the distribution results of the shot peening coverage rate of each area on the tenon surface are calculated; if the coverage rate does not meet the standard, return to step S1 and optimize the shot peening chamber structure through the simulation results.

7. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1, characterized in that: The horizontal shot peening chamber is a cylindrical chamber, a mounting hole is provided on the side wall of the horizontal shot peening chamber, a ball bearing is arranged in the mounting hole, the blade fixture is installed in the ball bearing, the blade tenon part to be shot peened is clamped by the blade fixture, a vibration head is installed on a bottom wall of the horizontal shot peening chamber, and the installed blade tenon part and the vibration head are arranged relatively spaced apart; the central axes of the blade tenon part, the blade fixture and the ball bearing are collinear; during the shot peening process, the blade tenon part is driven to rotate at a uniform speed along its own axis, and when the working surface of the tenon faces the vibration head, the tenon stops rotating for a preset time, and the discrete element simulation time of the blade tenon ultrasonic shot peening is set to 20s; The inner cavity size of the horizontal shot peening chamber is φ51mm×100mm.

8. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1, characterized in that: The vertical shot peening chamber is a cylindrical chamber, a mounting hole is provided on a bottom wall of the vertical shot peening chamber, a ball bearing is arranged in the mounting hole, the blade clamp is installed in the ball bearing, the blade tenon part to be shot peened is clamped by the blade clamp, a vibration head is installed on the other bottom wall of the vertical shot peening chamber, and the installed blade tenon part and the vibration head are arranged relatively spaced apart; the central axes of the blade tenon part, the blade clamp, the ball bearing and the vertical shot peening chamber are collinear; When the surface of the blade tenon which is unevenly shot-peened in the horizontal shot-peening chamber is compositely strengthened by the vertical shot-peening chamber, the blade fixture drives the fixed blade tenon mounted thereon to penetrate into the vertical shot-peening chamber so that the blade tenon is at a position 50 mm away from the surface of the vibration head; The inner cavity size of the vertical shot peening chamber is φ51mm×100mm.

9. The method for ultrasonic shot peening composite strengthening of compressor blade tenons according to claim 1, characterized in that: The blade tenon, shot peening chamber and vibration head are all made of titanium alloy, and the shot is made of zirconium oxide ceramic material.

10. A compressor blade tenon ultrasonic shot peening composite strengthening device, characterized in that: It includes a shot peening chamber, a vibration head, a ball bearing and a blade clamp; the shot peening chamber includes a horizontal shot peening chamber and a vertical shot peening chamber, and the structure and size of the horizontal shot peening chamber and the structure and size of the vertical shot peening chamber are determined according to the compressor blade tenon ultrasonic shot peening composite strengthening method according to claim 1.

Citation Information

Patent Citations

  • Planar array type ultrasonic shot-peening reinforcing device and method

    CN107488780A

  • Ultrasonic shotblast strengthening equipment

    CN107574293A

  • Ultrasonic kinetic energy shot peening device

    CN109097544A

  • Spiral bevel gear shot peening strengthening coverage rate prediction method

    CN115758811A

  • Thin-wall blade shot peening strengthening process parameter determination method based on damage control

    CN118153382A

Cited By

  • Parameter optimization method for ultrasonic vibration grinding reinforcement of surface of gas turbine blade tenon material

    CN120180820A