Friction stir welding pressure control method and system and electronic equipment
By obtaining material parameters, monitoring spindle vibration and temperature, and dynamically adjusting welding pressure, the problems of low accuracy and poor stability of friction stir welding pressure control are solved, and the quality and production efficiency of high-precision welding are improved.
Patent Information
- Application Number
- CN202510984801.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-17
- Publication Date
- 2025-08-29
AI Technical Summary
The existing friction stir welding technology has problems such as low accuracy, poor stability, high cost and strict environmental requirements in welding pressure control, which is difficult to meet the needs of high-precision welding, resulting in unstable welding quality and production efficiency.
By obtaining the material parameters of the workpiece to be welded, using a laser-induced breakdown spectrometer to detect the components and calculate the reference pressure value; using a three-axis acceleration sensor to monitor the spindle vibration, the infrared thermal imager collects the temperature field distribution in real time; after welding is completed, the control parameters are optimized through ultrasonic flaw detection, forming a self-learning control loop, and dynamically adjusting the welding pressure.
It realizes precise control of welding pressure, improves welding quality and stability, reduces dependence on the environment, and improves production efficiency.
Smart Images

Figure CN120551546A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of welding pressure control, and in particular to a method, system and electronic equipment for controlling friction stir welding pressure. Background Art
[0002] As a solid-state welding technology, friction stir welding (FSW) offers advantages such as zero melting, smoke, and spatter, making it widely used in welding lightweight materials such as aluminum and magnesium alloys. With the continuous advancement of industrial technology, the requirements for welding quality are increasing across various industries, especially in high-precision fields such as aerospace, where the mechanical properties and dimensional accuracy of welded joints are directly related to product safety and reliability. However, current FSW technology faces technical bottlenecks in welding pressure control, which significantly limits its further development and application.
[0003] Currently, pressure control in friction stir welding is primarily achieved through the following methods. The first is a mechanical pressure control system, which utilizes mechanical structures such as springs or hydraulic cylinders to regulate and control pressure. This method has a relatively simple structure. The second is an electro-hydraulic servo control system, which uses electro-hydraulic servo valves and pressure sensors to achieve closed-loop pressure control, enabling high pressure regulation accuracy. The third is a pneumatic pressure control system, which utilizes pneumatic cylinders and pneumatic pressure regulating valves to regulate pressure, and has a relatively fast response speed. Furthermore, in traditional friction stir welding processes, spindle pressure is typically adjusted manually or semi-automatically to ensure constant pressure output during the welding process.
[0004] Existing mechanical pressure control systems suffer from low pressure regulation accuracy, making them incapable of meeting the demands of high-precision welding. While electro-hydraulic servo control systems offer high precision, they are complex, require high maintenance, and have demanding working environments. Pneumatic pressure control systems suffer from poor pressure stability and are significantly affected by the environment, making it difficult to ensure consistent welding quality. Manual or semi-automatic spindle pressure adjustment methods also struggle to precisely control spindle pressure during welding, resulting in unstable welding results for different materials or for the same material under varying stresses, impacting welding quality and production efficiency. Summary of the Invention
[0005] The purpose of this application is to overcome the above technical problems and provide a method, system, device and storage medium for controlling friction stir welding pressure. The friction stir welding pressure control method comprises the following steps: S1. Obtain the material parameters of the workpiece to be welded based on the material yield strength σ s And thermal expansion coefficient α, calculate the reference pressure value P through the preset algorithm base , establish an initial pressure control benchmark; S2. The spindle vibration acceleration is monitored in real time by a three-axis acceleration sensor. When any axial acceleration exceeds the set threshold, the pressure compensation algorithm ΔP=K·∫(a z )dt, where K is the material-related compensation coefficient; S3. Use an infrared thermal imager to collect the temperature distribution of the welding area in real time. When the temperature gradient exceeds the critical value, the welding pressure is dynamically corrected according to the thermal-mechanical coupling equation. S4. After welding is complete, ultrasonic testing is performed to obtain weld quality data. Based on the defect characteristics, the control parameters of S1-S3 are reversely optimized to form a self-learning control loop. Among them, the vibration compensation algorithm of step S2 and the thermal correction amount of step S3 are vector superimposed, the compensation coefficient K is dynamically adjusted according to the material parameters of step S1, and the optimization result of step S4 is directly written into the material database for subsequent welding parameter preset.
[0006] By adopting the above technical solution, the material parameters of the workpiece to be welded are obtained to calculate the reference pressure value, which can establish an initial pressure control reference to meet the welding requirements of different materials; the spindle vibration acceleration is monitored in real time and the pressure compensation algorithm is activated to cope with the influence of spindle vibration on welding pressure; the temperature field distribution of the welding area is collected in real time and the welding pressure is dynamically corrected according to the thermal-mechanical coupling equation, which can take into account the effect of temperature changes on welding pressure; after welding is completed, the weld quality data is obtained through flaw detection, and the control parameters are reversely optimized to form a self-learning control loop, and the optimization results are written into the material database, which can continuously improve the accuracy of welding pressure control and welding quality. At the same time, the vibration compensation algorithm is superimposed with the thermal correction vector and the compensation coefficient is adjusted according to the material parameters. It can comprehensively consider the influence of various factors on welding pressure and improve the control effect.
[0007] Preferably, the S1 includes: S1.1 Real-time detection of workpiece surface composition by laser-induced breakdown spectroscopy; S1.2 When the material composition deviation δ ≥ 5%, according to σ s =σ s 0·(1+0.2δ) modified yield strength; S1.3 Based on the modified σ s and thermal expansion coefficient α, through P base =K1·σ s (1+αΔT) Recalculate the reference pressure value.
[0008] By adopting the above technical solution and using laser-induced breakdown spectrometry to detect the surface composition of the workpiece in real time, material composition deviations can be discovered in a timely manner; when the material composition deviation reaches a certain level, the yield strength is corrected to more accurately reflect the actual characteristics of the material; the reference pressure value is recalculated based on the corrected yield strength and thermal expansion coefficient, and a more accurate initial pressure control reference is established, which improves the accuracy and adaptability of stir friction welding pressure control and helps to improve welding quality and stability.
[0009] Preferably, in S2: S2.1 Set the X / Y axis acceleration threshold a xy =3.5m / s², Z-axis threshold a z =5.2m / s²; S2.2 When the vibration frequency f∈[80Hz,120Hz], activate the second-order compensation term ΔP'=0.1·(df / dt)·P base ; S2.3 Total compensation ΔP total =ΔP+ΔP', where ΔP=K2·∫a z dt.
[0010] By adopting the above technical solution and setting the acceleration thresholds in the X / Y and Z axes, it is possible to accurately determine whether the spindle vibration exceeds the normal range and trigger pressure compensation in a timely manner; when the main frequency of vibration is within a specific range, the second-order compensation item is activated, and the influence of the change in vibration frequency on the welding pressure is taken into account, which can compensate the pressure more comprehensively; the total compensation amount is calculated and the first-order compensation is combined with the second-order compensation, which can more accurately and finely adjust the welding pressure according to the spindle vibration conditions, reduce the welding pressure fluctuations caused by vibration, and thus improve the welding quality and stability.
[0011] Preferably, the S3 specifically includes: S3.1 Establishing the thermal-mechanical coupling equation P thermal =K3·[∇T·(1+β·v)]², where β=0.02s / mm; S3.2 The value range of K3 is 0.002-0.005MPa / (℃²·mm²) calibrated by finite element model; S3.3 When the temperature gradient ∇T≥50℃ / mm is detected, the welding pressure P=P is updated in real time. base +P thermal .
[0012] By adopting the above technical solution, a thermal-mechanical coupling equation is established and the coefficient value range is calibrated, which can accurately quantify the relationship between welding pressure, temperature gradient and welding speed. When the temperature gradient reaches a critical value, the welding pressure is updated in real time. The welding pressure can be dynamically corrected according to the temperature field distribution in the welding area, effectively improving the accuracy and stability of pressure control during stir friction welding, thereby improving the quality and performance of the welded joint.
[0013] Preferably, the S4 includes: S4.1 When the porosity defect rate η_p ≥ 2%, reduce the critical temperature gradient by 10-15%; S4.2 When the crack defect rate η_c ≥ 1%, increase K2 by 20-30%; S4.3 Writing the optimized parameters into the distributed material database via blockchain.
[0014] By adopting the above technical solution, when the porosity defect rate reaches 2% or above, the critical value of the temperature gradient is lowered, which can better deal with the porosity defect problem and improve the welding quality; when the crack defect rate reaches 1% or above, the K2 value is increased, which helps to compensate for the pressure problem caused by cracks and improve the welding effect; using blockchain to write the optimization parameters into the distributed material database can achieve safe and reliable storage and sharing of data, making it easier to refer to these optimization parameters in subsequent welding, further improving welding quality and efficiency.
[0015] Preferably, it also includes: S5.1 Real-time detection of workpiece thickness change dh; S5.2 According to P_t(t) = P base [1 + γ (dh / dt)] adjusts the pressure, where γ = 0.05 s / mm; S5.3 When dh / dt ≥ 0.2 mm / s, simultaneously reduce the welding speed v to 80% of the original value.
[0016] By adopting the above technical solution, real-time detection of the thickness change of the workpiece can accurately grasp the workpiece condition. Adjusting the pressure according to the thickness change can make the welding pressure better adapt to the actual state of the workpiece, avoiding the impact of inappropriate welding pressure due to thickness change and affecting the welding quality; when the workpiece thickness change rate reaches a certain value, the welding speed is simultaneously reduced, which helps to further ensure the stability of the welding process and the welding quality.
[0017] Preferably, between S2 and S3, execute: S2a.1 Calculate the pressure nonuniformity μ=σ_p / μ_p using the strain gauge array; S2a.2 When μ≥0.3, re-plan the welding trajectory so that μ<0.25; S2a.3 Activate the path optimization module to generate a spiral progressive welding path.
[0018] By adopting the above technical solution, during the friction stir welding process, the material parameters of the workpiece to be welded are first obtained to calculate the reference pressure value, and then the spindle vibration acceleration is monitored by a three-axis accelerometer for pressure compensation. After that, the strain gauge array is used to calculate the pressure unevenness. When the pressure unevenness is greater than or equal to 0.3, the welding trajectory is replanned to make the pressure unevenness less than 0.25 and the path optimization module is activated to generate a spiral progressive welding path, which can solve the problem of uneven welding pressure distribution and improve the uniformity and stability of the welding pressure; then, the welding pressure is dynamically corrected according to the temperature field distribution of the welding area collected by the infrared thermal imager, and finally, the weld quality data is obtained by ultrasonic flaw detection to reversely optimize the control parameters, which can effectively ensure the precise control and stability of the friction stir welding pressure, improve welding quality and production efficiency, and at the same time, the optimized parameters are written into the material database for subsequent welding parameter presets, forming a self-learning control loop to further improve the welding effect.
[0019] A friction stir welding pressure control system, comprising: Material property analysis module, integrated with laser-induced breakdown spectrometer and material database, for real-time detection of workpiece surface composition and correction of yield strength σ s ; Multi-axis vibration sensing module, including a three-axis acceleration sensor and an FFT spectrum analysis unit, connected to the pressure compensation controller via the CAN bus; Thermomechanical coupling control module, equipped with an infrared thermal imager and a finite element calculation unit, and equipped with a real-time analytical algorithm for temperature gradient ∇T; Dynamic pressure actuator, including a piezoelectric actuator array driven by a servo motor, with a response accuracy of ±0.5MPa; The quality feedback optimization module integrates the ultrasonic flaw detector and the blockchain node, connecting to the distributed database through the IPFS protocol; Among them, each module achieves μs-level synchronization through time-sensitive networking (TSN), and the control instruction transmission delay is ≤1.5ms. The vibration sensing module and the thermal coupling module share a velocity coupling coefficient of β = 0.02s / mm; The pressure actuator receives the composite control signal from S2-S5 and satisfies P total =P base +ΔP total +P thermal The vector superposition relationship of The quality feedback module implements back-propagation optimization of the K1-K3 coefficients through smart contracts.
[0020] By adopting the above technical solutions, the material property analysis module can detect the surface composition of the workpiece in real time and correct the yield strength, providing a basis for accurately calculating the reference pressure; the multi-axis vibration sensing module uses a three-axis acceleration sensor and an FFT spectrum analysis unit, and cooperates with the CAN bus to connect the pressure compensation controller to effectively monitor the spindle vibration and perform pressure compensation; the thermal coupling control module is equipped with an infrared thermal imager and a finite element calculation unit, and is configured with a real-time temperature gradient analysis algorithm, which can dynamically correct the welding pressure according to the temperature field of the welding area; the dynamic pressure actuator includes a piezoelectric actuator array driven by a servo motor, with a response accuracy of ±0.5MPa, which can accurately perform pressure control; the quality feedback optimization module integrates an ultrasonic flaw detector and a blockchain node, connects to a distributed database through the IPFS protocol, and combines smart contracts to realize back propagation optimization of the K1-K3 coefficients, which can continuously improve the welding pressure control accuracy; each module realizes μs through a time-sensitive network Level synchronization, control command transmission delay ≤ 1.5ms, ensures efficient coordination of all parts of the system; the vibration sensing module and the thermal coupling module share the speed coupling coefficient, which facilitates unified coordination; the pressure actuator receives the composite control signal and satisfies the vector superposition relationship to achieve more comprehensive pressure control.
[0021] An electronic device comprises a memory, a processor and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of the above-mentioned friction stir welding pressure control method when executing the computer program.
[0022] By adopting the above technical solution, it is possible to calculate the reference pressure value based on the material parameters of the workpiece to be welded, use a three-axis accelerometer to monitor the spindle vibration acceleration for pressure compensation, use an infrared thermal imager to collect the temperature field distribution in the welding area and dynamically correct the welding pressure. After welding is completed, the control parameters are optimized through ultrasonic flaw detection to form a self-learning control loop. It is also possible to detect the surface composition of the workpiece to correct the yield strength, refine the vibration compensation algorithm, improve the thermal-mechanical coupling equation and the welding pressure update method, optimize the control parameters according to the weld defect rate, adjust the pressure and welding speed according to the change in workpiece thickness, plan the welding trajectory and generate a spiral progressive welding path, effectively solving the problems of low pressure control accuracy, poor stability, high cost and harsh environmental requirements in existing stir friction welding, and improve welding quality and production efficiency.
[0023] A computer-readable storage medium stores a computer program, and when the computer program is executed by a processor, the steps of the above-mentioned friction stir welding pressure control method are implemented.
[0024] By adopting the above technical solution, the reference pressure value can be calculated according to the material parameters of the workpiece to be welded, the pressure can be compensated and corrected by monitoring the spindle vibration acceleration and the temperature field distribution in the welding area, and the control parameters can be reversely optimized using the ultrasonic flaw detection results to form a self-learning control loop. The pressure can also be further accurately adjusted according to factors such as the workpiece composition deviation, vibration main frequency, temperature gradient, pore and crack defect rate, and workpiece thickness change. At the same time, the welding trajectory can be replanned to optimize the welding path, thereby effectively solving the problems of low precision, poor stability, high cost, and large environmental impact in the existing stir friction welding pressure control, improving the accuracy and stability of welding pressure control, ensuring the quality and performance of the welded joint, and improving welding quality and production efficiency.
[0025] In summary, this application has the following beneficial technical effects: 1. Obtain the material parameters of the workpiece to be welded and calculate the reference pressure value, establish the initial pressure control benchmark, and accurately adapt to the welding of different materials, solving the problem of traditional methods that are difficult to accurately control pressure and improving welding quality; 2. A three-axis accelerometer monitors the spindle's vibration acceleration and activates a pressure compensation algorithm. An infrared thermal imager is used to capture the temperature distribution in the welding zone and dynamically adjust the welding pressure. This approach addresses vibration and temperature changes during welding, ensuring stable welding pressure and preventing unstable welding results, thereby improving welding quality and production efficiency. 3. After welding is completed, the weld quality data is obtained through ultrasonic testing to reversely optimize the control parameters, forming a self-learning control loop. The optimization results are written into the material database for subsequent welding parameter presets, which can continuously improve the accuracy of welding pressure control and thus improve welding quality. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 Flowchart of the friction stir welding pressure control method in an embodiment of the present application.
[0026] Figure 2 This is a principle block diagram of the friction stir welding pressure control system in the embodiment of the present application. DETAILED DESCRIPTION
[0027] The technical solutions in the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings. The described embodiments are only possible technical implementations of the present invention, but are not limited thereto. Those skilled in the art can fully combine the embodiments of the present invention, and other embodiments obtained without creative work are also within the scope of protection of the present invention.
[0028] This application mainly adopts a scheme of obtaining parameters and combining multiple detections to dynamically control welding pressure, thereby achieving the effect of improving the control accuracy of stir friction welding pressure and the stability of welding quality. The following is a further detailed description of this application.
[0029] Example 1: Reference Figure 1 and Figure 2 The friction stir welding pressure control method provided in the embodiment of the present application includes the following steps: S1. Obtain the material parameters of the workpiece to be welded based on the material yield strength σ s And thermal expansion coefficient α, calculate the reference pressure value P through the preset algorithm base , establish an initial pressure control benchmark; S2. The spindle vibration acceleration is monitored in real time by a three-axis acceleration sensor. When any axial acceleration exceeds the set threshold, the pressure compensation algorithm ΔP=K·∫(a z )dt, where K is the material-related compensation coefficient; S3. Use an infrared thermal imager to collect the temperature distribution of the welding area in real time. When the temperature gradient exceeds the critical value, the welding pressure is dynamically corrected according to the thermal-mechanical coupling equation. S4. After welding is complete, ultrasonic testing is performed to obtain weld quality data. Based on the defect characteristics, the control parameters of S1-S3 are reversely optimized to form a self-learning control loop. Among them, the vibration compensation algorithm of step S2 and the thermal correction amount of step S3 are vector superimposed, the compensation coefficient K is dynamically adjusted according to the material parameters of step S1, and the optimization result of step S4 is directly written into the material database for subsequent welding parameter preset.
[0030] Specifically, S1 obtains the material parameters of the workpiece to be welded, based on the material yield strength σ s And thermal expansion coefficient α, calculate the reference pressure value P through the preset algorithm base In the step of establishing the initial pressure control benchmark, detection equipment and calculation methods are required.
[0031] Correspondingly, S1 includes the following: S1.1 can use laser-induced breakdown spectroscopy to detect the surface composition of the workpiece in real time; Specifically, laser-induced breakdown spectroscopy (LIBS) emits high-energy laser pulses onto the surface of a workpiece, instantly vaporizing the surface material and stimulating it to emit light. The material's composition is then determined by analyzing the spectrum. If LIBS is not available, chemical analysis can also be used.
[0032] S1.2 When the material composition deviation δ ≥ 5%, according to σ s = σ s The yield strength is corrected by 0·(1 + 0.2δ); correspondingly, the yield strength is reasonably corrected according to the change of material composition to more accurately calculate the reference pressure.
[0033] S1.3 Based on the modified σs and thermal expansion coefficient α, through P base = K1·σ s Recalculate the reference pressure value using (1 + αΔT), where K1 is a coefficient related to the welding process. This allows an accurate initial pressure control reference to be established based on the actual material properties.
[0034] Specifically, S2 monitors the spindle vibration acceleration in real time through a three-axis acceleration sensor. When any axial acceleration exceeds the set threshold, the pressure compensation algorithm ΔP = K·∫(a z )dt, where K is the material-related compensation factor. A triaxial accelerometer can measure acceleration in three mutually perpendicular directions and is typically installed at a suitable location on the spindle to accurately measure spindle vibration. For example, a piezoelectric triaxial accelerometer offers high sensitivity and fast response speed; a piezoresistive triaxial accelerometer is also available, offering lower cost.
[0035] Correspondingly, step S2 includes the following: S2.1 Set the X / Y axis acceleration threshold a xy = 3.5m / s², Z-axis threshold a z = 5.2m / s². When any axial acceleration exceeds this threshold, it indicates abnormal spindle vibration and requires pressure compensation. This step sets the X / Y axial acceleration thresholds to 3.5m / s² and the Z axial acceleration to 5.2m / s², values derived from experimental data on aluminum alloy welding processes. When the acceleration exceeds the threshold, it indicates that the spindle vibration energy has exceeded the critical value of plastic deformation of the material, potentially causing weld grain coarsening or abnormal hardness in the heat-affected zone. The higher Z-axis threshold (5.2m / s²) is because the axial pressure directly acts on the plastic flow layer, requiring greater tolerance for dynamic fluctuations.
[0036] S2.2 When the main vibration frequency f∈[80Hz, 120Hz], activate the second-order compensation term ΔP' = 0.1·(df / dt)·P base Because the first-order compensation alone may not be sufficient in this specific vibration frequency range, a second-order compensation term is added. The second-order compensation term ΔP'=0.1·(df / dt)·P is activated in the 80-120Hz frequency range. base This frequency range corresponds to the stick-slip vibration mode at the interface between the stirring head and the workpiece. Vibration in this frequency range significantly alters the heat input distribution, and simple integral compensation (ΔP) cannot eliminate the phase lag caused by the rate of change of frequency (df / dt). A second-order term coefficient of 0.1, calibrated through finite element simulation, effectively compensates for pressure fluctuations caused by frequency fluctuations, improving pressure control accuracy by 23%.
[0037] S2.3 Total compensation ΔP total= ΔP + ΔP', where ΔP = K2·∫a z dt, by integrating and calculating the compensation amount, we can more accurately deal with the influence of vibration on welding pressure. total =K2·∫a z dt+ΔP' is calculated using time-domain integration, with the integral time constant matching the material's stress relaxation characteristics. Integrating the Z-axis acceleration accumulates plastic deformation energy, avoiding transient vibration interference. The compensation coefficient K2 is dynamically adjusted based on the material database, and adaptive compensation is achieved in conjunction with the real-time welding speed v. In actual measurements, pressure fluctuations can be reduced from ±2.5 MPa to ±1.8 MPa.
[0038] Specifically, the S3 uses an infrared thermal imager to collect real-time temperature distribution in the weld zone. When the temperature gradient exceeds a critical value, the welding pressure is dynamically corrected based on the thermal-mechanical coupling equation. The infrared thermal imager receives infrared radiation from the object and converts it into a temperature image, thereby capturing the temperature distribution in the weld zone. It is typically installed in a location with a clear view of the weld zone. For example, a long-wave infrared thermal imager is suitable for low-temperature measurements; a medium-wave infrared thermal imager can also be used, offering higher accuracy.
[0039] The corresponding S3 includes the following: S3.1 Establish the thermal-mechanical coupling equation P thermal = K3·[∇T·(1 + β·v)]², where β = 0.02s / mm. This equation can be used to calculate the corrected pressure based on the temperature gradient and welding speed.
[0040] S3.2 uses a finite element model to calibrate the K3 value range to 0.002 - 0.005MPa / (℃²·mm²). The finite element model can simulate the thermal-mechanical coupling during the welding process and provide a basis for the K3 value.
[0041] S3.3 When the temperature gradient ∇T ≥ 50℃ / mm is detected, the welding pressure P = P is updated in real time. base + P thermal , ensuring that the welding pressure can adapt to temperature changes.
[0042] Specifically, after S4 welding is completed, ultrasonic testing is used to obtain weld quality data. Based on the defect characteristics, the control parameters for S1-S3 are reversely optimized, forming a self-learning control loop. Ultrasonic testing detects internal defects in welds by utilizing the principle that ultrasonic waves, when propagating through a material, generate reflected waves upon encountering defects. The ultrasonic flaw detector transmits ultrasonic waves into the weld, receives and analyzes the reflected waves, and generates weld quality data.
[0043] S4.1 When the porosity defect rate η_p ≥ 2%, reduce the temperature gradient threshold by 10-15%. This is because porosity may be related to excessively high temperatures during welding. Lowering the temperature gradient threshold can better control the temperature. S4.2 When the crack defect rate η_c ≥ 1%, increase K2 by 20-30%. Increasing the compensation coefficient can enhance the vibration compensation capability and reduce the occurrence of cracks.
[0044] S4.3 writes the optimized parameters into the distributed material database through blockchain. The characteristics of blockchain ensure the security and non-tamperability of data, and the distributed database facilitates data sharing and updating.
[0045] In addition, the method further comprises S5: S5.1 detects the thickness change dh of the workpiece in real time.
[0046] S5.2 According to P_t(t) = P base Adjust the pressure using the value [1 + γ (dh / dt)], where γ = 0.05s / mm. A displacement sensor can be used to detect changes in workpiece thickness. Install the sensor in a suitable location to measure the workpiece thickness in real time.
[0047] S5.3 When dh / dt≥0.2mm / s, the welding speed v is simultaneously reduced to 80% of the original value. This ensures that the welding pressure and welding speed match when the workpiece thickness varies greatly, thereby improving the welding quality.
[0048] Between the steps S2 monitoring vibration and S3 monitoring temperature, S2a is also executed: S2a.1 Calculate pressure nonuniformity using a strain gauge array: μ = σ_p / μ_p. The strain gauge array consists of multiple strain gauges attached near the weld. Pressure nonuniformity is calculated by measuring strain.
[0049] S2a.2 When μ≥0.3, replan the welding trajectory so that μ<0.25.
[0050] S2a.3 activates the path optimization module to generate a spiral progressive welding path, which can improve pressure distribution and enhance welding quality.
[0051] The implementation principle of this embodiment is as follows: This friction stir welding pressure control method forms a complete self-learning closed-loop control system through the coordinated control of multiple links, from initial material parameter acquisition and baseline pressure setting, to vibration and temperature monitoring and pressure adjustment during the welding process, and finally to post-weld quality inspection and parameter optimization. Each step is interconnected and mutually influential, enabling timely adjustment of welding pressure based on various changes during the welding process. This significantly improves the accuracy and stability of welding pressure control, effectively avoiding welding defects caused by improper pressure control, thereby improving welding quality and production efficiency, and offering a significant improvement over traditional pressure control methods.
[0052] Example 2: The difference between this embodiment and the above embodiment is that when detecting the composition of the workpiece material, if you do not want to use a laser-induced breakdown spectrometer, you can also use an energy spectrum analyzer. The energy spectrum analyzer determines the type and content of elements by emitting an electron beam to the sample and analyzing the energy and intensity of the generated X-rays. It can also detect the surface composition of the workpiece, but the operating principle and application scenarios are different from those of the laser-induced breakdown spectrometer. The energy spectrum analyzer is suitable for analyzing the composition of microscopic areas, while the laser-induced breakdown spectrometer is more suitable for rapid and large-scale composition detection.
[0053] The principle behind this embodiment is to use an energy spectrum analyzer (EDS) instead of a laser-induced breakdown spectrometer (LIBS) to detect workpiece material composition, broadening the range of available detection methods. Different detection equipment has different characteristics and advantages. The use of an EDS can meet user needs in specific situations while still enabling the acquisition of material parameters for baseline pressure calculation. This ensures the proper implementation of the friction stir welding pressure control method and improves its flexibility and applicability.
[0054] Example 3: The friction stir welding pressure control system provided in this embodiment includes a material property analysis module, a multi-axis vibration sensing module, a thermal coupling control module, a dynamic pressure actuator, and a quality feedback optimization module. These modules achieve μs-level synchronization via a time-sensitive network (TSN), with control command transmission latency of ≤1.5ms. This ensures the timeliness and accuracy of information transmission between modules and enables rapid response to various situations during the welding process.
[0055] Specifically, the material property analysis module integrates a laser-induced breakdown spectrometer and a material database to detect the surface composition of the workpiece in real time and correct the yield strength σ sAs previously described, the laser-induced breakdown spectrometer's function is to store the characteristic parameters of various materials in a material database, facilitating query and comparison. When changes in the workpiece's surface composition are detected, the module can modify the yield strength based on the database data and pre-set rules, providing accurate material parameters for subsequent pressure control.
[0056] Specifically, the multi-axis vibration sensing module includes a triaxial accelerometer and an FFT spectrum analysis unit, connected to the pressure compensation controller via the CAN bus. The triaxial accelerometer monitors spindle vibration in real time, while the FFT spectrum analysis unit performs spectrum analysis on the vibration signal to determine the frequency components. The CAN bus is used for data transmission, transmitting vibration data to the pressure compensation controller. The pressure compensation controller calculates the pressure compensation amount based on the vibration conditions, enabling real-time adjustment of the welding pressure.
[0057] Specifically, the thermomechanical coupling control module is equipped with an infrared thermal imager and a finite element calculation unit, along with a real-time analytical algorithm for the temperature gradient ∇T. The infrared thermal imager captures the temperature distribution in the weld zone, while the finite element calculation unit simulates the thermal-mechanical coupling, providing a basis for calibrating the parameters in the thermal-mechanical coupling equation. The real-time analytical algorithm rapidly calculates the temperature gradient. When the temperature gradient exceeds a critical value, the module dynamically adjusts the welding pressure according to the thermal-mechanical coupling equation.
[0058] Specifically, the dynamic pressure actuator comprises a piezoelectric actuator array driven by a servo motor, with a response accuracy of ±0.5 MPa. The servo motor provides power, driving the piezoelectric actuator array to vary pressure. Piezoelectric actuators offer fast response and high precision, enabling precise adjustment of welding pressure based on control signals, meeting the precise pressure control requirements during the welding process.
[0059] Specifically, the quality feedback optimization module integrates an ultrasonic flaw detector with a blockchain node, connecting to a distributed database via the IPFS protocol. The ultrasonic flaw detector inspects weld quality and captures defect data. The blockchain node ensures secure and tamper-proof data storage, while the IPFS protocol enables distributed data storage and sharing. The module uses this weld quality data to reversely optimize the control parameters of other modules, forming a self-learning loop and improving the control performance of the entire system.
[0060] The vibration sensing module and the thermal coupling module share a velocity coupling coefficient of β = 0.02s / mm, which ensures the consistency of the two modules when calculating the pressure adjustment amount. The pressure actuator receives the composite control signal from S2 - S5 to meet P total = P base + ΔP total + P thermalThe vector superposition relationship can comprehensively consider the impact of multiple factors such as vibration and temperature on welding pressure. The quality feedback module implements backpropagation optimization of the K1-K3 coefficients through smart contracts, further improving the system's adaptability.
[0061] The operating principle of this embodiment is as follows: This friction stir welding pressure control system achieves comprehensive, real-time, and precise control of welding pressure through the coordinated operation of various modules. From material property analysis to vibration and temperature monitoring during the welding process, and finally to pressure execution and quality feedback optimization, a complete closed-loop control system is formed. Synchronization and data transmission between modules via a high-speed network, sharing key parameters, enable the system to quickly and accurately respond to various changes during the welding process, improving the precision and stability of welding pressure control, thereby ensuring weld quality.
[0062] Example 4: The electronic device provided in the embodiment of the present application includes a memory, a processor, and a computer program stored in the memory and capable of running on the processor. When the processor executes the computer program, the steps of the stir friction welding pressure control method are implemented. The memory is used to store computer programs and related data. It can be different types of storage devices such as solid-state drives and mechanical hard drives. The processor is responsible for executing computer programs and processing and calculating data. When the electronic device is started and the relevant program is run, the processor will execute the steps of S1 obtaining parameters, S2 monitoring vibration, S3 monitoring temperature, S4 optimizing parameters, etc. in sequence according to the instructions in the program to achieve control of the stir friction welding pressure.
[0063] The principle behind this embodiment is that the electronic device provides an operating platform for the friction stir welding pressure control method. By storing the control method in memory as a computer program and executing it on a processor, an automated pressure control process is achieved. The electronic device boasts fast computing speed and strong processing capabilities, enabling rapid and accurate completion of various data processing and computational tasks. This ensures efficient implementation of the friction stir welding pressure control method and enhances the intelligent nature of the welding process.
[0064] Example 5: The computer-readable storage medium provided in the embodiments of the present application stores a computer program that, when executed by a processor, implements the steps of a friction stir welding pressure control method. The computer-readable storage medium may be a CD, a USB flash drive, a removable hard drive, or the like. When the processor reads the computer program from the storage medium, the program directs the processor to execute the friction stir welding pressure control method according to predetermined steps, including operations such as obtaining material parameters in step S1, performing pressure compensation in step S2, correcting pressure in step S3, and optimizing parameters in step S4.
[0065] The implementation principle of this embodiment is as follows: a computer-readable storage medium provides a storage medium for the program for the friction stir welding pressure control method. This facilitates the storage, transfer, and use of the program. Different computer devices can implement the same pressure control function by reading the program from the storage medium, improving the versatility and portability of the method, enabling the friction stir welding pressure control method to be more widely applied in various welding scenarios.
[0066] The above are all preferred embodiments of the present application and are not intended to limit the scope of protection of the present application. Therefore, any equivalent changes made based on the structure, shape, and principle of the present application should be included in the scope of protection of the present application.
Claims
1. A friction stir welding pressure control method, characterized in that: The following steps are involved: S1. Obtain the material parameters of the workpiece to be welded based on the material yield strength σ s And thermal expansion coefficient α, calculate the reference pressure value P through the preset algorithm base , establish an initial pressure control benchmark; S2. The spindle vibration acceleration is monitored in real time by a three-axis acceleration sensor. When any axial acceleration exceeds the set threshold, the pressure compensation algorithm ΔP=K·∫(a z )dt, where ΔP is the pressure compensation amount, which represents the dynamic pressure adjustment value caused by vibration, and K is the material-related compensation coefficient, the value of which is determined by the material yield strength σ s and thermal expansion coefficient α; S3. Use an infrared thermal imager to collect the temperature distribution of the welding area in real time. When the temperature gradient exceeds the critical value, the welding pressure is dynamically corrected according to the thermal-mechanical coupling equation. S4. After welding is complete, ultrasonic testing is performed to obtain weld quality data. Based on the defect characteristics, the control parameters of S1-S3 are reversely optimized to form a self-learning control loop. Among them, the vibration compensation algorithm of step S2 and the thermal correction amount of step S3 are vector superimposed, the compensation coefficient K is dynamically adjusted according to the material parameters of step S1, and the optimization result of step S4 is directly written into the material database for subsequent welding parameter preset.
2. The friction stir welding pressure control method according to claim 1, characterized in that: Said S1 comprises: S1.1 Real-time detection of workpiece surface composition by laser-induced breakdown spectroscopy; S1.2 When the material composition deviation δ ≥ 5%, according to σ s =σ s 0·(1+0.2δ) modified yield strength, σ s 0 is the nominal yield strength of the material, that is, the original yield strength value when no composition deviation occurs; S1.3 Based on the modified σ s and thermal expansion coefficient α, through P base =K1·σ s (1 + αΔT) recalculates the baseline pressure value. K1 is a coefficient related to the welding process, which can establish an accurate initial pressure control baseline based on the actual characteristics of the material. αΔT is a compensation term for thermal expansion effects, based on α being the material thermal expansion coefficient and ΔT being the difference between the actual temperature of the welding area and the room temperature.
3. The friction stir welding pressure control method according to claim 1, characterized in that: In S2: S2.1 Set the X / Y axis acceleration threshold a xy =3.5m / s², Z-axis threshold a z =5.2m / s²; S2.2 When the vibration frequency f∈[80Hz,120Hz], activate the second-order compensation term ΔP'=0.1·(df / dt)·P base ; S2.3 Total compensation ΔP total =ΔP+ΔP', where ΔP=K2·∫a z dt.
4. The friction stir welding pressure control method according to claim 1, characterized in that: The S3 specifically includes: S3.1 Establishing the thermal-mechanical coupling equation P thermal =K3·[∇T·(1+β·v)]², where P thermal is the thermal compensation pressure, K3 is the thermal-mechanical coupling coefficient, ∇T is the temperature gradient in the welding area, β is the velocity sensitivity coefficient, β=0.02s / mm; S3.2 The value range of K3 is 0.002-0.005MPa / (℃²·mm²) calibrated by finite element model; S3.3 When the temperature gradient ∇T≥50℃ / mm is detected, the welding pressure P=P is updated in real time. base +P thermal .
5. The friction stir welding pressure control method according to claim 1, characterized in that: The S4 includes: S4.1 When the porosity defect rate η_p ≥ 2%, reduce the critical temperature gradient by 10-15%; S4.2 When the crack defect rate η_c ≥ 1%, increase K2 by 20-30%; S4.3 Writing the optimized parameters into the distributed material database via blockchain.
6. The friction stir welding pressure control method according to claim 1, characterized in that: Also includes: S5.1 Real-time detection of workpiece thickness change dh; S5.2 According to P_t(t) = P base [1 + γ (dh / dt)] adjusts the pressure, where γ = 0.05 s / mm; S5.3 When dh / dt ≥ 0.2 mm / s, simultaneously reduce the welding speed v to 80% of the original value.
7. The friction stir welding pressure control method according to claim 1, characterized in that: Execute between S2 and S3: S2a.1 Calculate the pressure nonuniformity μ=σ_p / μ_p using the strain gauge array; S2a.2 When μ≥0.3, re-plan the welding trajectory so that μ<0.25; S2a.3 Activate the path optimization module to generate a spiral progressive welding path.
8. A friction stir welding pressure control system, characterized in that: include: Material property analysis module, integrated with laser-induced breakdown spectrometer and material database, for real-time detection of workpiece surface composition and correction of yield strength σ s ; Multi-axis vibration sensing module, including a three-axis acceleration sensor and an FFT spectrum analysis unit, connected to the pressure compensation controller via the CAN bus; Thermomechanical coupling control module, equipped with an infrared thermal imager and a finite element calculation unit, and equipped with a real-time analytical algorithm for temperature gradient ∇T; Dynamic pressure actuator, including a piezoelectric actuator array driven by a servo motor, with a response accuracy of ±0.5MPa; The quality feedback optimization module integrates the ultrasonic flaw detector and the blockchain node, connecting to the distributed database through the IPFS protocol; Among them, each module achieves μs-level synchronization through time-sensitive networking (TSN), and the control instruction transmission delay is ≤1.5ms. The vibration sensing module and the thermal coupling module share a velocity coupling coefficient of β = 0.02s / mm; The pressure actuator receives the composite control signal generated by the execution of steps S2-S5, which satisfies P total =P base +ΔP total +P thermal The vector superposition relationship of The quality feedback module implements back-propagation optimization of the K1-K3 coefficients through smart contracts.
9. An electronic device, characterized in that: The method comprises a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of the friction stir welding pressure control method according to any one of claims 1 to 7 when executing the computer program.
10. A computer-readable storage medium, characterized in that The computer-readable storage medium stores a computer program, and when the computer program is executed by a processor, the steps of the friction stir welding pressure control method according to any one of claims 1 to 7 are implemented.
Citation Information
Cited By
Forklift gantry welding deformation control and correction method
CN121787167A
Welding method and device for electronic device, electronic equipment and storage medium
CN122077160A
Electronic device soldering method, apparatus, electronic device, and storage medium
CN122077160B