Method for synergistically preparing recycled aggregate from urban updated garden waste and building waste

Through molecular-level deconstruction, nanocompolation, plasma sintering and gradient functional treatment, combined with intelligent monitoring and carbon footprint tracking, the resource waste and carbon emission problems in garden waste and construction waste treatment are solved, and high-performance recycled aggregates are prepared to achieve sustainable development.

CN120590085AInactive Publication Date: 2025-09-05安徽格林生态环境科技有限公司
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202510857969.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-07-24
Publication Date
2025-09-05
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

When dealing with garden waste and construction waste, the existing technology has problems of waste of resources, environmental pollution, unstable performance and high carbon emissions, making it difficult to meet high-standard engineering needs and sustainable development goals.

Method used

The preparation process of regenerated aggregates is optimized to achieve efficient resource utilization and low carbon emissions.

Benefits of technology

The performance of the prepared recycled aggregate has been significantly improved, meeting the requirements of high-standard engineering, reducing carbon footprint, reducing environmental pollution, and achieving a win-win situation of economic and environmental benefits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120590085A_ABST
    Figure CN120590085A_ABST
Patent Text Reader

Abstract

The invention discloses a method for synergistically preparing recycled aggregate from urban renewal garden waste and building waste, and relates to the field of treatment of garden waste and building waste. The method comprises the following steps: carrying out molecular-level deconstruction pretreatment on garden wastes, destroying cell walls by adopting dual-frequency ultrasound combined with biological enzymolysis, and treating the building wastes by combining high-pressure water jet with abrasive impact; performing nano-scale composite granulation, adding a nano-composite binder, and introducing CO2 to form a gel transition layer; by means of plasma-assisted sintering, particle diffusion is accelerated by means of radio-frequency plasma and an electric field; chemical vapor deposition is adopted, and a TiN-TiO2 gradient functional coating is formed; real-time monitoring and regulation are performed through a multi-mode sensor network and an intelligent algorithm, and process parameters are adjusted according to a product performance prediction result. The recycled aggregate disclosed by the invention is high in strength, good in heat preservation and strong in freezing resistance; negative carbon emission reduction is achieved in the production process, an intelligent system guarantees stable product quality, environmental protection and economic benefits are achieved, and urban update and solid waste treatment green transformation are promoted.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of garden waste and construction waste treatment, and in particular to a method for collaboratively preparing recycled aggregate from garden waste and construction waste in urban renewal. Background Art

[0002] With the acceleration of urbanization, the treatment of garden waste and construction waste has become a difficult problem in urban environmental governance. Most of the garden waste is only disposed of by landfill or incineration, which not only occupies a large amount of land resources, but also releases a large amount of greenhouse gases and harmful pollutants during the incineration process, causing serious damage to the ecological environment. The problem of construction waste is even more prominent, with an annual output of over 2 billion tons. Traditional treatment methods are mostly open-air stacking or simple crushing and backfilling, which leads to problems such as construction waste and dust pollution, and wastes a lot of potential resources. The existing single treatment technology has obvious limitations. The composting treatment cycle of garden waste is long, the efficiency is low, and it is easy to produce odorous gases; the recycled aggregates of construction waste are insufficient in strength and unevenly graded, making it difficult to meet high-standard engineering requirements.

[0003] In the field of solid waste resource utilization, traditional technologies have significant shortcomings in the coordinated treatment of garden waste and construction waste. Simple physical mixing methods do not fully consider the differences in the physical and chemical properties of the two, resulting in unstable performance of recycled products. The interfacial bonding between the biomass fibers in garden waste and the particles of construction waste is weak, which can easily cause cracking of the recycled aggregate; during high-temperature treatment, the low ignition point characteristics of garden waste may cause local overheating and destroy the mineral structure of the construction waste. In addition, the existing process lacks a systematic design for carbon emission reduction and energy recovery. The sintering process relies on fossil fuels and does not fully utilize the self-heating potential of garden waste, resulting in high carbon emissions per unit product, making it difficult to achieve sustainable development goals.

[0004] With the advancement of the "dual carbon" goals and the increasing demand for green urban development, traditional solid waste treatment models are no longer able to meet industry needs. While existing research has attempted to incorporate biomass into building materials, it has often focused on improving a single function and lacks comprehensive optimization of performance across the entire lifecycle. The application of intelligent technologies is limited to data monitoring, without enabling dynamic adaptive adjustment of process parameters. Developing a collaborative disposal technology that balances efficient resource utilization, environmental friendliness, and economic benefits, and overcomes current technical bottlenecks, has become a critical issue that urgently needs to be addressed in the process of urban renewal. Summary of the Invention

[0005] The present invention proposes a method for collaboratively preparing recycled aggregate from urban renewal garden waste and construction waste to solve the problems mentioned in the above-mentioned prior art.

[0006] To achieve the above objectives, the present invention adopts the following technical solution: a method for preparing recycled aggregate from urban renewal garden waste and construction waste, comprising: Molecular-level deconstruction pretreatment steps: Garden waste is treated with dual-frequency ultrasound combined with bio-enzymatic hydrolysis, using a composite enzyme solution prepared with cellulase and lignin peroxidase in appropriate proportions; construction waste is subjected to surface exfoliation using a high-pressure water jet combined with abrasive impact treatment, and X-ray diffraction is used to monitor crystal structure changes in real time; Nanoscale composite granulation steps: pre-treated garden waste and construction waste are mixed according to the mass ratio, and nano-composite binder is added; CO2 gas is introduced to form a gel transition layer on the surface of the material, and the formula is used. Control the uniformity of the gel layer, L is the average thickness of the gel layer, m gel is the gel mass, S total is the total specific surface area of ​​the material; Plasma assisted sintering steps: the mixed material is made into a green body and sent into the plasma sintering furnace, and the surface of the green body is bombarded by radio frequency plasma; Ar-H2 mixed gas is introduced, and the formula Auxiliary sintering, D is the actual diffusion coefficient, D0 is a constant, Q is the diffusion activation energy, R is the gas constant, T is the absolute temperature, E is the applied electric field strength, and E0 is the reference electric field; Gradient functionalization post-processing steps: using chemical vapor deposition technology to deposit a TiN-TiO2 gradient coating on the surface of the recycled aggregate, passing a mixed gas of TiCl4 and N2 to deposit a TiN hard layer; cutting into a mixed gas of TiCl4 and O2 to deposit a TiO2 photocatalytic layer, forming a gradient functional layer with specific performance; Intelligent monitoring and control steps: deploy Raman spectroscopy sensors, piezoresistive stress sensors, and infrared thermal imagers to monitor the molecular structure of materials, stress distribution of green bodies, and sintering temperature fields; use the convolutional neural network-long short-term memory network fusion model to analyze data. When product performance indicators deviate from the target value and exceed the threshold, the formula is used to Adjust process parameters, P adj is the adjusted process parameter, P0 is the original parameter, k is the adjustment coefficient, ΔX is the performance deviation value, X target is the target performance value.

[0007] Furthermore, it also includes: Synergistic optimization steps: adding carbon nanodots to the nanocomposite binder to form hydrogen bonds with the silicon-oxygen bonds in the water glass through the surface hydroxyl groups; introducing pulse current in the plasma sintering step, through the formula v diff =v0(1+αI) densification sintering degree, v diff is the actual diffusion rate, v0 is the diffusion rate when there is no current, α is the current influence coefficient, and I is the current density.

[0008] Furthermore, it also includes: Life cycle carbon management steps: establish a carbon footprint tracking system to record carbon emissions data from raw material collection and transportation, production and processing, product use to recycling; Calculate product carbon benefits, CF net is the net carbon footprint, CF i is the carbon emissions of each link, CF sequestration is the amount of carbon fixed.

[0009] Furthermore, the degree of bio-enzymatic hydrolysis of garden waste in the molecular deconstruction pretreatment step is calculated by the formula Control quantization, E d is the degree of enzymatic hydrolysis, W0 and W1 are the mass of the material before and after enzymatic hydrolysis, and C0 and C1 are the cellulose contents before and after enzymatic hydrolysis.

[0010] Furthermore, the gelation time of the nanocomposite binder in the nanoscale composite granulation step is calculated by the formula Regulation, t g is the gelation time, t0 is the reference time, K1, K2, K3 are constants, T is the temperature, P is the CO2 pressure, and S is the specific surface area of ​​the nanoparticles.

[0011] Furthermore, it also includes: Interface strengthening step: Before gradient functionalization post-treatment, the recycled aggregate is immersed in a mixed solution of silane coupling agent and dopamine; dopamine self-polymerizes to form a polydopamine layer, and after hydrolyzing the silane coupling agent, it reacts with the phenolic hydroxyl groups in the polydopamine layer and the hydroxyl groups on the aggregate surface to form a chemical bond connection.

[0012] Furthermore, in the plasma-assisted sintering step, the internal porosity of the recycled aggregate is controlled by adjusting the RF plasma power and electric field intensity, and the pore size distribution conforms to the log-normal distribution. , r is the pore size, μ is the logarithmic mean pore size, and σ is the logarithmic standard deviation.

[0013] Furthermore, it also includes: Intelligent grading steps for product performance: Use machine vision and artificial intelligence algorithms to detect the appearance and particle size distribution of recycled aggregates, and use online mechanical properties testing equipment to test the compressive strength of single particles; based on the test results, the recycled aggregates are divided into three grades.

[0014] Furthermore, it also includes: Efficient recovery steps of waste heat from production: Use organic Rankine cycle system to recover high temperature tail gas from plasma sintering furnace, and select R245fa as working fluid; Optimize system parameters, η ORC is the ORC system efficiency, W net is the net output work of the system, Q in For heat input.

[0015] Furthermore, it also includes: Raw material adaptability expansion steps: When the raw materials are mixed with plastic waste, a microwave irradiation treatment step is added to the molecular-level deconstruction pretreatment step; microwaves selectively heat the plastic to melt and volatilize, and use pyrolysis to generate free radicals to modify the surface of garden waste and construction waste.

[0016] Compared with the existing technology, the beneficial effects of the present invention are: In terms of product performance, the recycled aggregate produced by this invention surpasses traditional products in all indicators. Through gradient pretreatment and microstructural control, the aggregate's crushing index is significantly reduced, and its strength is significantly increased, meeting the requirements for preparing concrete above C40. Its thermal conductivity is significantly reduced, providing excellent insulation properties and broadening its application scenarios. Its functional gradient design combines lightweight and high strength, significantly improving its frost resistance and making it suitable for construction projects in extremely cold regions.

[0017] In terms of environmental benefits, this invention achieves significant energy conservation and emission reduction. Negative carbon sintering technology sequesters a significant amount of CO₂ per ton of product, significantly reducing the carbon footprint. The resource utilization of garden waste replaces some fossil fuel consumption, significantly reducing energy consumption per unit of product. Furthermore, pollution control throughout the entire process keeps dust emission concentrations well below national standards, effectively reducing environmental pollution.

[0018] The economic benefits are also significant. The intelligent compounding system and optimized production processes have reduced raw material and energy costs, significantly lowering overall production costs. Based on a 100,000-ton annual recycled aggregate production line, the annual cost savings are substantial. Furthermore, the product's improved performance enables its application in higher-end markets, increasing unit sales prices and further enhancing market competitiveness.

[0019] In terms of technological innovation, this invention establishes an integrated intelligent production system encompassing "detection-calculation-control." A machine learning model dynamically optimizes the mixing ratio, significantly reducing product performance fluctuations. A blockchain-based carbon footprint tracking system ensures data traceability throughout the entire lifecycle, providing a reliable basis for carbon trading. This technology offers a replicable solution for solid waste management in urban renewal, helping achieve the dual goals of "zero landfill" for construction waste and "full utilization" of garden waste, and driving the industry's transition toward a green, low-carbon future. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a schematic diagram of a method for collaboratively preparing recycled aggregate from urban renewal garden waste and construction waste, as proposed by the present invention; Figure 2 Schematic diagram of the interactive effect of electric field intensity and temperature on crushing index; Figure 3 Schematic diagram for comparison of multi-scale structural representation; Figure 4 This is a diagram comparing the carbon footprint of the life cycle; Figure 5 Schematic diagram of the prediction accuracy of the intelligent monitoring system Figure 6 Schematic diagram of the degradation efficiency of gradient functional coatings. DETAILED DESCRIPTION

[0021] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0022] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like to indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0023] In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the said features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined. In addition, the terms "installed", "connected" and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be a connection between the two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. The present invention will be further described in detail below with reference to the accompanying drawings.

[0024] Reference Figures 1 to 6 A method for preparing recycled aggregate from urban renewal garden waste and construction waste, comprising: Molecular deconstruction pretreatment step: Garden waste is treated with dual-frequency ultrasound (20kHz low frequency + 40kHz high frequency alternating action, power density 0.8-1.2W / cm 3) combined with biological enzymatic hydrolysis treatment, using cellulase (enzyme activity ≥ 6000U / g) and lignin peroxidase (enzyme activity ≥ 3500U / g) in a ratio of 2:1 to prepare a complex enzyme solution, and treat it at pH 4.8-5.2 and temperature 52-55℃ for 18-24 hours to destroy the hydrogen bonds between plant cell wall molecules, break the long cellulose chains into short chains with a degree of polymerization of 500-800, and degrade lignin into small molecular aromatic compounds, with the specific surface area increased to 12-15m 2 / g. Construction waste is subjected to surface exfoliation treatment using a high-pressure water jet (40-50 MPa) combined with abrasive impact (corundum particle size 0.1-0.3 mm). This removes a 50-100 μm thick layer of weathered material and impurities, exposing the fresh mineral surface. X-ray diffraction (XRD) is used to monitor crystal structure changes in real time to ensure that the main mineral phases (such as silicates and carbonates) are not destroyed.

[0025] Nanoscale composite granulation steps: Pre-treated garden waste and construction waste are mixed in a mass ratio of 1:3-1:5, and a nano-composite binder (prepared by nano-silicon dioxide (particle size 20-30nm), nano-calcium carbonate (particle size 80-100nm) and liquid water glass in a ratio of 1:1.5:3) is added, accounting for 3-5% of the total mass. The mixture is mixed in a planetary mixer at a stirring speed of 80-120r / min for 20-25 minutes. At the same time, CO2 gas (pressure 0.3-0.5MPa) is introduced to form a gel transition layer with a thickness of 50-80nm on the surface of the material with the water glass and nanoparticles. According to the formula (where L is the average thickness of the gel layer, m gel is the gel mass, S total is the total specific surface area of ​​the material) to control the uniformity of the gel layer.

[0026] Plasma assisted sintering steps: After the mixed material is made into a green body, it is sent into a plasma sintering furnace and first -3 -10 -2 In a Pa environment, a high-energy ion beam (energy 50-100eV) generated by radio frequency plasma (power 3-5kW, frequency 13.56MHz) is used to bombard the surface of the blank to etch away surface contaminants and activate surface atoms. The temperature is then raised to 1100-1200℃, and an Ar-H2 mixed gas (volume ratio 8:2) is introduced. Under the action of an electric field strength of 100-150V / cm, the active hydrogen atoms generated by the decomposition of H2 promote the diffusion and sintering between particles. According to the formula (Where D is the actual diffusion coefficient, D0 is a constant, Q is the diffusion activation energy, R is the gas constant, T is the absolute temperature, E is the external electric field intensity, and E0 is the reference electric field intensity) accelerates the sintering process and shortens the sintering time to 1 / 3 of the traditional method.

[0027] Gradient functionalization post-treatment steps: Using chemical vapor deposition (CVD) technology, a TiN-TiO2 gradient coating is deposited on the surface of the recycled aggregate. A TiCl4 and N2 gas mixture (volume ratio of 1:4) is introduced at 500-600°C to deposit a 0.2-0.3μm thick TiN hard layer. A TiCl4 and O2 gas mixture (volume ratio of 1:6) is then introduced at 650-750°C to deposit a 0.5-0.8μm thick TiO2 photocatalytic layer. This results in a gradient functional layer with a surface hardness of HV2000-2500 and a photocatalytic efficiency of ≥85% for methyl orange degradation in one hour under simulated sunlight.

[0028] Intelligent monitoring and control steps: Deploy a multimodal sensor network throughout the entire preparation process, including Raman spectroscopy sensors to monitor changes in the material's molecular structure in real time, piezoresistive stress sensors to monitor the stress distribution of the green body during forming, and infrared thermal imagers to monitor the sintering temperature field. A convolutional neural network-long short-term memory network (CNN-LSTM) fusion model is used to analyze sensor data. When the predicted product performance indicators (such as crushing index and water absorption rate) deviate from the target value by more than the threshold, the formula is used to calculate the target value. (where P adj is the adjusted process parameter, P0 is the original parameter, k is the adjustment coefficient, ΔX is the performance deviation value, X target The process parameters are automatically adjusted to the target performance value).

[0029] The present invention further comprises the following steps: Synergistic optimization steps: In the nanocomposite binder link, add carbon nanodots with a mass fraction of 0.5-1% and a particle size of 5-10nm. The surface of carbon nanodots is rich in hydroxyl groups, and water glass contains silicon-oxygen bonds, and the two can form hydrogen bonds. Hydrogen bonds are strong intermolecular forces, and numerous hydrogen bonds are interwoven to strengthen the binder network structure. By adding carbon nanodots during granulation, the binder can better wrap the bonded aggregate particles and enhance the bonding force between the particles. In the plasma sintering stage, a pulse frequency of 100-200Hz and a current density of 5-10A / cm 2 The pulse current passes through the recycled aggregate to generate Joule heat, which works synergistically with the plasma. The plasma contains high-energy particles and active groups, which increase the atomic activity on the particle surface. The Joule heat in turn increases the particle temperature and intensifies the atomic thermal motion. According to the formula v diff =v0(1+αI) to improve the sintering densification degree, v diffis the actual diffusion rate, v0 is the diffusion rate in the absence of current, α is the current influence coefficient, and I is the current density. Increasing current density increases the atomic diffusion rate by 2-3 times. Accelerated atomic diffusion promotes atomic fusion at the particle interface and improves sintering densification. The dense structure reduces internal porosity and defects, significantly enhancing mechanical properties such as aggregate strength and hardness, and improving durability. The synergistic optimization step improves the performance of recycled aggregates by strengthening the binder microstructure and regulating sintering atomic diffusion, resulting in superior performance in applications such as construction.

[0030] The present invention further comprises the following steps: Lifecycle carbon management steps: Establish a carbon footprint tracking system based on blockchain. Blockchain, with its decentralized, tamper-proof and traceable characteristics, ensures accurate recording of carbon footprint data. When collecting and transporting raw materials, vehicle sensors and smart devices collect and upload information such as transportation mileage and fuel consumption in real time. For example, in the transportation of garden waste, detailed records of routes, frequencies and fuel data are used to calculate carbon emissions. In the production and processing links, the energy consumption of equipment such as plasma sintering furnaces is monitored in real time, and smart electricity meters and gas meters upload energy usage data. Combined with process parameters, the carbon emissions of each process are calculated using an accounting model. During the product use and recycling stages, the product information management system interacts with the blockchain to record service life, maintenance and recycling information, and evaluate related carbon emissions and carbon reduction benefits. Through the formula Calculate carbon benefits. CF net is the net carbon footprint, CF i Carbon emissions in each link, including raw material collection and product use. sequestration This includes carbon sequestration from the carbonization of garden waste, which reduces atmospheric carbon, and carbon reduction from replacing natural aggregate with recycled aggregate, which avoids carbon emissions from natural aggregate mining and processing. Through precise tracking and calculation, we ensure that the net carbon footprint of each ton of recycled aggregate is ≤200kgCO2 equivalent, reducing the industry's environmental impact, enhancing the green competitiveness of our products, and helping the construction industry move towards low-carbon, sustainable development.

[0031] In the present invention, the degree of bio-enzymatic hydrolysis of garden waste in the molecular level deconstruction pretreatment step is calculated by the formula Quantify, the goal is to make E d In the formula, W0 and W1 are the mass of the material before and after enzymatic hydrolysis. Accurately weigh W0 before the start of enzymatic hydrolysis. During the enzymatic hydrolysis, some components decompose and the mass changes. After the end, W1 is obtained. Calculate the enzymatic hydrolysis ratio based on mass. C0 and C1 are the cellulose contents before and after enzymatic hydrolysis. Cellulose is the key component. C0 is measured by chemical method and C1 is measured after enzymatic hydrolysis. Reflects the degree of decomposition. The product of the two is E d, comprehensively showing the overall changes of enzymatic hydrolysis. In actual operation, the enzyme type, concentration, temperature, time and other conditions are constantly adjusted, and real-time monitoring is performed and E is calculated according to the formula d If E d If the value is less than 0.6, it may indicate low enzyme activity and a short reaction time, so the enzyme dosage can be increased or the reaction time can be extended. If it is greater than 0.8, it may indicate excessive enzymatic hydrolysis, requiring a lower enzyme concentration or a shorter reaction time. Through meticulous control, enzymatic hydrolysis of garden waste is optimized, providing high-quality raw materials for recycled aggregate production and improving process quality and efficiency.

[0032] In the present invention, the gelation time of the nanocomposite binder in the nanoscale composite granulation step is calculated by the formula Regulation. g is the gelation time, which is related to granulation and recycled aggregate performance; t0 is the reference time. K1, K2, and K3 are constants determined through extensive experimentation, reflecting the influence of temperature, CO2 pressure, and nanoparticle specific surface area, respectively. T is temperature, which affects molecular motion and reaction rate. High temperatures accelerate reactions and shorten gelation time, while low temperatures have the opposite effect. P is CO2 pressure, which changes the properties of the binder and affects the gelation rate. S is the specific surface area of ​​the nanoparticle; a larger temperature indicates higher activity and has a significant impact on gelation time. In actual operation, temperature control equipment is used to maintain 25°C, pressure regulation devices are maintained at 0.4 MPa, and nanoparticles with an appropriate specific surface area are selected. Based on calculated formulas and actual monitoring results, parameters are fine-tuned to achieve the ideal gelation time range, ensuring smooth granulation and improving the quality and performance of recycled aggregate.

[0033] The present invention further comprises the following steps: Interface strengthening step: Before gradient functionalization post-treatment, the recycled aggregate is immersed in a mixed solution of a silane coupling agent (KH560) and dopamine (concentration 0.5-1g / L). The silane coupling agent KH560 has a unique molecule, containing groups that react with both inorganic and organic materials. Dopamine self-polymerizes under weakly alkaline conditions (pH 8-9). The aggregate is treated in this solution for 30-45 minutes. During this treatment, dopamine self-polymerizes to form a 5-10nm thick polydopamine layer, which is rich in phenolic hydroxyl groups and highly reactive. Simultaneously, the silane coupling agent hydrolyzes, and the resulting active groups react with the phenolic hydroxyl groups in the polydopamine layer and the hydroxyl groups on the aggregate surface. Specifically, the hydrolysis of the silane coupling agent produces silanol groups (Si-OH), which condense with phenolic and hydroxyl groups to form Si-OC or Si-O-Si chemical bonds, transforming the bond from physical adsorption to a strong chemical connection, increasing the strength to 5-8MPa. Higher bonding strength prevents the coating from falling off, allowing it to fully exert its functions such as wear resistance, corrosion resistance, and photocatalysis, laying a solid foundation for the application of recycled aggregates in construction, environmental protection and other fields.

[0034] In the present invention, the pore structure is shaped by regulating the radio frequency plasma power and electric field strength in the plasma-assisted sintering step. Porosity is an important indicator of the performance of recycled aggregate and is controlled at 8-12%. If the porosity is too high, the aggregate strength is affected; if it is too low, the permeability is poor. The radio frequency plasma power affects the sintering energy input. High power promotes particle fusion and reduces porosity; low power leads to insufficient sintering and high porosity. The electric field strength guides ion migration and diffusion, optimizes particle arrangement, and helps to control porosity. The pore size distribution conforms to the log-normal distribution. By adjusting process parameters, we achieved a logarithmic mean pore size μ = 50 nm and a logarithmic standard deviation σ = 0.8. μ determines the average pore size and thus functions like aggregate filtration; σ reflects the degree of pore size dispersion. A suitable σ results in a concentrated pore size distribution, ensuring stable performance. In fluid transport applications, a well-defined pore size distribution ensures smooth fluid flow and maintains structural strength.

[0035] The present invention further comprises the following steps: Intelligent product performance grading steps: Machine vision and artificial intelligence algorithms are used to rapidly inspect the appearance of recycled aggregate. The machine vision system, equipped with a high-resolution camera and specialized image acquisition equipment, captures the color and shape of the recycled aggregate. Recycled aggregate from different sources and processing processes may exhibit color variations, which to some extent reflect composition and quality characteristics. For example, aggregate containing high levels of impurities may appear darker or more uneven in color. Image analysis algorithms are used to identify aggregate particle morphology, such as roundness and angularity. Regular particle shapes improve workability and strength in concrete preparation. The system also measures aggregate particle size distribution. Using specialized image processing techniques, aggregates of different particle sizes are separated and the percentage of particles in each size range is calculated. Well-graded aggregate grading ensures better packing and compaction in concrete, improving concrete performance. The compressive strength of individual particles is tested using online mechanical property testing equipment (with a loading rate set at 1 mm / min). Using a high-precision pressure sensor and a stable loading device, pressure is applied to individual particles of recycled aggregate at a constant loading rate of 1 mm / min, capturing pressure and displacement data in real time. As pressure gradually increases, aggregate particles will eventually break, and the maximum pressure value recorded is the compressive strength of a single particle. This parameter directly reflects the mechanical properties of the aggregate and is an important basis for assessing its quality. Based on the test results, recycled aggregate is classified into three grades. Grade I recycled aggregate has a crushing index of ≤10% and is suitable for concrete with strength grades of C40-C60. In projects such as high-rise buildings and bridges that require high concrete strength and durability, Grade I recycled aggregate can effectively ensure structural safety and stability. Grade II recycled aggregate has a crushing index between 10-15% and is suitable for concrete with strength grades of C20-C35. It can be used in general building structures and small components. Grade III recycled aggregate has a crushing index of 15-20% and is suitable for road bases. Road bases are subjected to repeated vehicle loads, and Grade III recycled aggregate meets the basic strength and stability requirements while ensuring the rational use of resources. Through intelligent product performance grading, the refined application of recycled aggregate is achieved, resource utilization efficiency is improved, and the sustainable development of recycled aggregate in the construction industry is promoted.

[0036] The present invention further comprises the following steps: Steps for efficient recovery of waste heat from production: Use the organic Rankine cycle (ORC) system to recover the high-temperature exhaust gas (temperature 400-500°C) discharged from the plasma sintering furnace, and select R245fa as the working fluid. R245fa has a low boiling point and can absorb heat and vaporize at a lower temperature. It also has stable chemical properties, ensuring stable operation of the system. The ORC system works based on the Rankine cycle. The high-temperature exhaust gas heats the liquid R245fa in the evaporator to vaporize it. The steam enters the turbine to expand and do work to drive the generator to generate electricity. After doing work, the steam is cooled and condensed into liquid in the condenser, and then pumped back to the evaporator to complete the cycle. In order to improve the efficiency of the system, the formula Optimize parameters. In actual operation, adjust the evaporator heat exchange area, turbine speed, condenser cooling medium flow, etc. to improve the system net output power W net , reasonably control the input heat Q in , improve system efficiency η ORC After optimization, waste heat power generation efficiency has reached 18-22%. The generated electricity is used to power factory lighting, small fans, water pumps, and other equipment, reducing power consumption and reliance on the external power grid. The efficient waste heat recovery process effectively utilizes high-temperature exhaust heat, lowering energy costs and carbon emissions. This aligns with the concept of sustainable development and contributes to a green and efficient production process.

[0037] The present invention further comprises the following steps: Raw material adaptability expansion steps: When the raw materials are mixed with plastic waste with a mass fraction of ≤5%, microwave irradiation treatment is added in the molecular-level deconstruction pretreatment stage. In the molecular-level deconstruction pretreatment stage, microwave irradiation with a frequency of 2.45GHz and a power density of 0.5-0.8W / cm³ is used. Microwaves, as electromagnetic waves of 300MHz-300GHz, can react with the polar molecules of plastics. The polar molecules of plastics oscillate at high speed and generate heat by friction under the microwave electric field, achieving selective heating and allowing the plastic to melt and volatilize quickly. In actual operation, the microwave irradiation time and power are precisely controlled. Set the irradiation time to 3-5 minutes. If the time is short, the plastic will be difficult to remove; if the time is long, it will affect the properties of other raw materials. The power density is maintained at 0.5-0.8W / cm 3 , ensuring that plastics are effectively processed without damaging other raw materials. Parameters are monitored and adjusted in real time during operation to ensure the effect. Free radicals generated by microwave irradiation pyrolysis are highly chemically active. Free radicals react with atoms or molecules on the surface of garden waste and construction waste to promote surface modification. For example, by adding to unsaturated bonds or initiating a series of reactions, the surface functional groups are changed, the roughness and active sites are increased, which is beneficial to enhance the bonding force between raw materials during subsequent preparation and improve the performance of recycled aggregates. The microwave irradiation treatment in the raw material adaptability expansion step not only removes plastic waste, but also modifies other raw materials without affecting the performance of recycled aggregates, expands the scope of application of raw materials, and improves the process's ability to handle complex raw materials, creating better conditions for the production and application of recycled aggregates.

[0038] The above are only preferred specific embodiments of the present invention, but the scope of protection of the present invention is not limited thereto. Any technician familiar with this technical field, within the technical scope disclosed by the present invention, who makes equivalent replacements or changes based on the technical solutions and inventive concepts of the present invention, should be covered by the scope of protection of the present invention.

Claims

1. A method for preparing recycled aggregate from urban renewal garden waste and construction waste, characterized in that: The following steps are involved: Molecular-level deconstruction pretreatment steps: Garden waste is treated with dual-frequency ultrasound combined with bio-enzymatic hydrolysis, using a composite enzyme solution prepared with cellulase and lignin peroxidase in appropriate proportions; construction waste is subjected to surface exfoliation using a high-pressure water jet combined with abrasive impact treatment, and X-ray diffraction is used to monitor crystal structure changes in real time; Nanoscale composite granulation steps: pre-treated garden waste and construction waste are mixed according to the mass ratio, and nano-composite binder is added; CO2 gas is introduced to form a gel transition layer on the surface of the material, and the formula is used. Control the uniformity of the gel layer, L is the average thickness of the gel layer, m gel is the gel mass, S total is the total specific surface area of ​​the material; Plasma assisted sintering steps: the mixed material is made into a green body and sent into the plasma sintering furnace, and the surface of the green body is bombarded by radio frequency plasma; Ar-H2 mixed gas is introduced, and the formula Auxiliary sintering, D is the actual diffusion coefficient, D0 is a constant, Q is the diffusion activation energy, R is the gas constant, T is the absolute temperature, E is the applied electric field strength, and E0 is the reference electric field; Gradient functionalization post-processing steps: using chemical vapor deposition technology to deposit a TiN-TiO2 gradient coating on the surface of the recycled aggregate, passing a mixed gas of TiCl4 and N2 to deposit a TiN hard layer; cutting into a mixed gas of TiCl4 and O2 to deposit a TiO2 photocatalytic layer, forming a gradient functional layer with specific performance; Intelligent monitoring and control steps: deploy Raman spectroscopy sensors, piezoresistive stress sensors, and infrared thermal imagers to monitor the molecular structure of materials, stress distribution of green bodies, and sintering temperature fields; use the convolutional neural network-long short-term memory network fusion model to analyze data. When product performance indicators deviate from the target value and exceed the threshold, the formula is used to Adjust process parameters, P adj is the adjusted process parameter, P0 is the original parameter, k is the adjustment coefficient, ΔX is the performance deviation value, X target is the target performance value.

2. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Synergistic optimization steps: Add carbon nanodots to the nanocomposite binder to form hydrogen bonds with the silicon-oxygen bonds in the water glass through the surface hydroxyl groups; The plasma sintering step introduces a pulse current, which is calculated by the formula v diff =v0(1+αI) densification sintering degree, v diff is the actual diffusion rate, v0 is the diffusion rate when there is no current, α is the current influence coefficient, and I is the current density.

3. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Lifecycle carbon management steps: Establish a carbon footprint tracking system to record carbon emissions data throughout the entire life cycle, from raw material collection and transportation, production and processing, product use to recycling; By formula Calculate product carbon benefits, CF net is the net carbon footprint, CF i is the carbon emissions of each link, CF sequestration is the amount of carbon fixed.

4. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: The degree of biodegradation of garden waste in the molecular deconstruction pretreatment step is determined by the formula Control quantization, E d is the degree of enzymatic hydrolysis, W0 and W1 are the mass of the material before and after enzymatic hydrolysis, and C0 and C1 are the cellulose contents before and after enzymatic hydrolysis.

5. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: The gelation time of the nanocomposite binder in the nanoscale composite granulation step is expressed by the formula Regulation, t g is the gelation time, t0 is the reference time, K1, K2, K3 are constants, T is the temperature, P is the CO2 pressure, and S is the specific surface area of ​​the nanoparticles.

6. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Interface strengthening step: before gradient functionalization post-treatment, the recycled aggregate is immersed in a mixed solution of silane coupling agent and dopamine; Dopamine self-polymerizes to form a polydopamine layer, and the silane coupling agent is hydrolyzed to react with the phenolic hydroxyl groups in the polydopamine layer and the hydroxyl groups on the surface of the aggregate to form a chemical bond connection.

7. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: In the plasma-assisted sintering step, the porosity of the recycled aggregate is controlled by adjusting the RF plasma power and electric field intensity, and the pore size distribution conforms to the log-normal distribution. , r is the pore size, μ is the logarithmic mean pore size, and σ is the logarithmic standard deviation.

8. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Intelligent grading steps for product performance: Use machine vision and artificial intelligence algorithms to detect the appearance and particle size distribution of recycled aggregates, and use online mechanical properties testing equipment to test the compressive strength of single particles; based on the test results, the recycled aggregates are divided into three grades.

9. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Efficient recovery steps of waste heat from production: Use organic Rankine cycle system to recover high temperature tail gas from plasma sintering furnace, and select R245fa as working fluid; Optimize system parameters, η ORC is the ORC system efficiency, W net is the net output work of the system, Q in For heat input.

10. The method for preparing recycled aggregate by synergistically using urban renewal garden waste and construction waste according to claim 1, characterized in that: Also includes: Raw material adaptability expansion steps: When the raw materials are mixed with plastic waste, a microwave irradiation treatment step is added to the molecular-level deconstruction pretreatment step; microwaves selectively heat the plastic to melt and volatilize, and use pyrolysis to generate free radicals to modify the surface of garden waste and construction waste.

Citation Information

Cited By

  • Oil sludge intelligent classification and cooperative processing data management system based on big data

    CN120952768A

  • An intelligent classification and collaborative processing data management system for oil sludge based on big data

    CN120952768B