Metal powder laying device and laying method based on charge control
By using a charge control method and combining a charging roller and an electrode plate, precise placement of metal powder in selective laser melting technology was achieved, solving the problem of inaccurate powder distribution in a plane and improving powder placement accuracy and efficiency.
Patent Information
- Application Number
- CN202510996611.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-18
- Publication Date
- 2025-11-21
AI Technical Summary
Existing technologies struggle to achieve accurate distribution of metal powders in a plane, especially in selective laser melting technology, where powder particles are small and their precise placement in a two-dimensional plane is difficult to control.
A charge-controlled metal powder laying device is used to deliver charge to the organic photoconductor film using a charging roller. A laser forms an uncharged writing area, and an electrode plate provides charge repulsion to selectively adsorb metal powder onto the organic photoconductor film, achieving precise laying.
It achieves precise and efficient laying of metal powder in a two-dimensional plane, solves the problem of difficult powder positioning in traditional methods, and improves the powder laying accuracy and control capability.
Smart Images

Figure CN120984911A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of additive manufacturing technology, and in particular to a charge-controlled metal powder laying device and method. Background Technology
[0002] Selective Laser Melting (SLM) is a technology primarily used in metal additive manufacturing. Its basic principle involves laying a thin layer (approximately 30-100 micrometers) of metal powder, then selectively melting and rapidly solidifying a portion of it using a high-energy laser source. This process is repeated layer by layer to ultimately create a three-dimensional solid. This technology makes it easier to manufacture complex parts and has broad application prospects in aerospace, automotive, and other industries.
[0003] The development of multi-material additive manufacturing technology has enabled the selective distribution of materials in solids, achieving more complex functions. Currently, many solutions for multi-material 3D printing have been proposed in the fields of polymer additive manufacturing (FDM, DLP). For SLM technology, which is mainly geared towards metal additive manufacturing, multi-material distribution in the vertical forming direction can now be achieved, primarily by switching between multiple powder cylinders.
[0004] However, due to the small size of the powder particles, it is difficult to control their placement in a specific position. Therefore, how to achieve accurate material distribution in a plane is an urgent problem to be solved. Summary of the Invention
[0005] The purpose of this invention is to provide a charge-controlled metal powder laying device and method to address the problem of how to achieve accurate material distribution in a plane in the prior art.
[0006] In a first aspect, the present invention provides a charge-controlled metal powder laying apparatus, comprising a deposition plate, a moving stage, a powder drum, and a charging roller, wherein the moving stage is located above the deposition plate;
[0007] The powder drum is mounted on the movable platform. The powder drum includes an outer sleeve and an inner sleeve arranged coaxially. The outer sleeve is rotatably arranged around the inner sleeve. An organic photoconductor film is covered on the outer sleeve. The charging roller is used to deliver a first charge to the organic photoconductor film.
[0008] The inner sleeve has a first electrode plate inside, and the bottom of the inner sleeve is provided with a slot. The first electrode plate and the slot are both arranged along the length of the inner sleeve, and the first electrode plate is partially located in the slot.
[0009] It also includes a powder control system provided on the moving platform. The powder control system includes a powder tank 5 and a laser. The laser is used to form an uncharged writing black area on the organic photoconductor film. The powder tank 5 is used to deliver metal powder with a first charge to the writing black area.
[0010] The first electrode plate is used to repel the metal powder after being energized.
[0011] The charge-controlled metal powder laying device described in this application uses electrostatic control to selectively adsorb metal powder onto an organic photoconductor film, and utilizes charge repulsion to achieve precise and efficient laying of metal powder in a two-dimensional plane, solving the problem of difficult positioning of traditional metal powder.
[0012] Preferably, the powder hopper 5 is provided with a powder hopper inside, and a charging plate is provided at the bottom of the powder hopper. The charging plate is used to charge the metal powder in the powder hopper with a first charge.
[0013] The powder silo is also provided with a discharge port on one side of the bottom. A powder feeding shaft is rotatably installed at the discharge port. The powder feeding shaft is used to transport metal powder onto the organic photoconductor film.
[0014] Preferably, the device further includes a stirring paddle disposed at the discharge port, the stirring paddle being used to convey the metal powder to the powder feeding shaft.
[0015] Preferably, multiple powder control systems are arranged at intervals around the powder drum in a circumferential direction.
[0016] Preferably, the inner sleeve is fixedly connected to the movable platform, and a first bearing and a second bearing are sleeved on the inner sleeve, and the outer sleeve is connected to the outer ring of the first bearing and the second bearing.
[0017] Preferably, the inner sleeve includes a first cylinder and a second cylinder connected to each other, the diameter of the second cylinder is smaller than that of the first cylinder, the second cylinder is connected to the moving platform, the inner ring of the first bearing is sleeved on the first cylinder, and the inner ring of the second bearing is sleeved on the end of the second cylinder away from the first cylinder.
[0018] The outer sleeve includes a first annular body and a second annular body connected to each other. The diameter of the second annular body is smaller than that of the first annular body. The inner wall of the first annular body is connected to the outer ring of the first bearing, and the inner wall of the second annular body is connected to the outer ring of the second bearing.
[0019] The organic photoconductor film covers the first annular body.
[0020] Preferably, it further includes a gear set, which includes a driving gear and a driven gear that cooperate with each other, and the driven gear is fixedly mounted on the second annular body;
[0021] The gear set also includes a drive motor, which drives the driving gear, and the driving gear drives the outer sleeve to rotate through the driven gear.
[0022] In a second aspect, this application also discloses a charge-controlled metal powder deposition method, based on the metal powder deposition apparatus described in this application, comprising the following steps:
[0023] S1: Different metal powders are placed in different powder buckets 5;
[0024] S2: The charging roller is energized, and the outer sleeve is driven to rotate. The charging roller contacts the organic photoconductor film and charges the organic photoconductor film with a first charge.
[0025] S3: After the organic photoconductor film is charged, the laser is activated to write black on the surface of the organic photoconductor film to form the black area, and then the powder tank 5 is controlled to deliver metal powder with the first charge to the black area.
[0026] S4: After the powder drum moves to the powder spreading position, the first electrode plate is energized so that the first electrode plate repels the metal powder in the writing black area to the powder spreading position of the deposition plate.
[0027] S5: After the powder is spread, start the SLM equipment to continue the laser scanning work, and then repeat steps S1 to S5.
[0028] Preferably, in step S3:
[0029] The device includes multiple toner control systems, which are spaced circumferentially around the toner drum and sequentially activated according to the rotation direction of the organic photoconductor film to perform blackening and toner feeding on the organic photoconductor film.
[0030] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0031] This application discloses a charge-controlled metal powder laying device. A powder drum is mounted on a moving platform, which moves the powder drum on a deposition plate to lay powder at different locations on the deposition plate. The powder drum includes an outer sleeve and an inner sleeve coaxially arranged. The outer sleeve is covered with an organic photoconductor film. During use, a charging roller delivers a first charge to the organic photoconductor film. Then, a laser forms a non-charged writing area on the organic photoconductor film. A powder tank 5 then delivers metal powder with the first charge to the writing area. After the powder drum moves to the powder laying position, the first electrode plate is energized. The electrode plate provides a large amount of initial charge, which uses charge repulsion to repel the metal powder located at the bottom of the organic photoconductor film onto the deposition plate, thereby achieving precise placement of the metal powder. Furthermore, the outer sleeve rotates continuously during the process to place powder at different preset placement positions, achieving precise control of the placement position. The charge-controlled metal powder placement device described in this application uses electrostatic control to selectively adsorb metal powder onto the organic photoconductor film, and uses charge repulsion to achieve precise and efficient placement of metal powder in a two-dimensional plane, solving the problem of difficult positioning of traditional metal powder. Attached Figure Description
[0032] Figure 1 This is a structural diagram of this application.
[0033] Figure 2 yes Figure 1 Right view (deposition plate and first linear guide omitted).
[0034] Figure 3 This is a cross-sectional view of the powder drum and powder bucket 5.
[0035] Figure 4 This is a longitudinal sectional view of the powder drum and powder bucket 5.
[0036] Figure 5 This is a schematic diagram of the inner sleeve.
[0037] Figure 6 This is a schematic diagram of the outer sleeve.
[0038] Figure 7 This is a schematic diagram of powder bucket 5.
[0039] Figure 8 This is a cross-sectional view of powder bucket 5.
[0040] Figure 9 This is a schematic diagram of the structure of the first linear guide rail.
[0041] Figure 10 yes Figure 9 A magnified view of part A.
[0042] Figure 11This is a schematic diagram of the powder application in this application.
[0043] Marked in the image:
[0044] 1-Deposition plate,
[0045] 2-First linear guide rail,
[0046] 21-First slider, 22-First lead screw, 23-First optical axis, 24-First motor, 25-First frame,
[0047] 3-Mobile station,
[0048] 4- powder drum,
[0049] 41-Outer sleeve, 411-First annular body, 412-Second annular body,
[0050] 42-Inner sleeve, 420-Empty groove, 421-First cylinder body, 4211-First stepped portion, 422-Second cylinder body, 4221-Second stepped portion
[0051] 43-Organic photoconductor film,
[0052] 44 - First electrode plate,
[0053] 45 - First bearing,
[0054] 46 - Second bearing,
[0055] 47-End cap,
[0056] 5-Powder Bucket 5,
[0057] 51-Powder hopper, 52-Charging plate, 53-Powder feeding shaft, 54-Agitator, 55-Discharge port, 56-Arc-shaped baffle, 561-Opening 561
[0058] 6-Laser,
[0059] 7-Charging roller,
[0060] 8-Gear set,
[0061] 81-Drive gear,
[0062] 82-Driven gear,
[0063] 83 - Drive motor. Detailed Implementation
[0064] The present invention will now be described in further detail with reference to specific embodiments. However, this should not be construed as limiting the scope of the present invention to the following embodiments; all technologies implemented based on the content of the present invention fall within the scope of the present invention.
[0065] Unless otherwise specified, the use of terms such as "upper," "lower," "left," "right," "center," "inner," and "outer" to indicate orientation or positional relationships in the description of specific embodiments of the present invention is based on the orientation or positional relationships shown in the accompanying drawings, or the orientation or positional relationship in which the product / equipment / device is typically placed during use. These terms are merely for the purpose of facilitating the description of the present invention or simplifying the description in specific embodiments, enabling those skilled in the art to quickly understand the solution, and do not indicate or imply that a particular device / component / element must have a specific orientation, or be constructed and operated in a specific positional relationship. Therefore, they should not be construed as limitations on the present invention.
[0066] Furthermore, the use of terms such as "horizontal," "vertical," "suspended," "parallel," and "coaxial" does not imply that the corresponding device / component / element must be absolutely horizontal, vertical, suspended, parallel, or coaxial. Slight tilt or deviation is permissible, as long as it does not affect the normal function of the relevant component. For example, "horizontal" simply means that its direction is more horizontal relative to "vertical," not that the structure must be perfectly horizontal; a slight tilt is acceptable. "Coaxial" means that two components are arranged as coaxially as possible, allowing them to move coaxially or approximately coaxially when their relative positions change. Alternatively, it can be simplified to mean that the corresponding device / component / element, when arranged in "horizontal," "vertical," "suspended," "parallel," or "coaxial" directions, can have an error / deviation of ±10% relative to the corresponding direction, more preferably within ±8%, more preferably within ±6%, more preferably within ±5%, and more preferably within ±4%. For example, the deviation in the "coaxial" direction is controlled within 0.2mm to 1mm, preferably within 0.2mm to 0.5mm. As long as the corresponding device / component / element is within the error / deviation range, it can still achieve its function in the solution of the present invention.
[0067] Furthermore, the use of terms such as "first," "second," and "third" in terminology is merely for distinguishing descriptions of identical or similar components and should not be interpreted as emphasizing or implying the relative importance of a particular component.
[0068] Furthermore, in the description of the embodiments of the present invention, "several", "more than", and "a number of" represent at least two. The number can be any number, such as 2, 3, 4, 5, 6, 7, 8, or 9, and can even exceed nine.
[0069] Furthermore, in the description of the technical solution of this invention, unless otherwise explicitly specified / limited / restricted, the terms "set up," "install," "connect," "link," "provided with," "laid out," and "arranged" should be interpreted broadly. For example, they can refer to fixed connections, detachable connections, or integral connections; they can refer to common connection methods in the art, such as welding, riveting, bolting, and threaded connections. Such connections can be mechanical, electrical, or communication connections; they can be direct connections or indirect connections through an intermediate medium; and they can refer to the internal communication between two components.
[0070] Example 1
[0071] like Figures 1-10 As shown, a charge-controlled metal powder laying device includes a deposition plate 1, a moving stage 3, a powder drum 4, and a charging roller 7, with the moving stage 3 located above the deposition plate 1.
[0072] The powder drum 4 is mounted on the moving platform 3. The powder drum 4 includes an outer sleeve 41 and an inner sleeve 42 arranged coaxially. The outer sleeve 41 is rotatably arranged around the inner sleeve 42. An organic photoconductor film 43 is covered on the outer sleeve 41. The charging roller 7 is used to deliver the first charge to the organic photoconductor film 43.
[0073] The inner sleeve 42 has a first electrode plate 44 inside, and a slot 420 is provided at the bottom of the inner sleeve 42. The first electrode plate 44 and the slot 420 are both arranged along the length of the inner sleeve 42, and the first electrode plate 44 is partially located in the slot 420.
[0074] It also includes a powder control system mounted on the moving stage 3. The powder control system includes a powder tank 5 and a laser 6. The laser 6 is used to form an uncharged writing black area on the organic photoconductor film 43, and the powder tank 5 is used to deliver metal powder with a first charge to the writing black area.
[0075] The first electrode plate 44 is used to repel metal powder after energization.
[0076] This embodiment describes a charge-controlled metal powder laying device. A powder drum 4 is mounted on a moving stage 3. The moving stage 3 moves the powder drum 4 on a deposition plate 1 to lay powder at different positions on the deposition plate 1. The powder drum 4 includes an outer sleeve 41 and an inner sleeve 42 arranged coaxially. The outer sleeve 41 is covered with an organic photoconductor film 43. During use, a charging roller 7 delivers a first charge to the organic photoconductor film 43. Then, a laser 6 forms a non-charged writing area on the organic photoconductor film 43. A powder tank 5 then delivers metal powder with the first charge to the writing area. After the powder drum 4 moves to the powder laying position, the first electrode plate 44 is energized. When energized, the first electrode plate 44 uses charge repulsion to push the metal powder at the bottom of the organic photoconductor film 43 onto the deposition plate 1, thus achieving precise metal powder laying. Furthermore, the outer sleeve 41 rotates continuously during the process to lay powder at different preset positions, achieving precise control of the powder laying position. The charge-controlled metal powder laying device described in this embodiment uses electrostatic control to selectively adsorb metal powder onto the organic photoconductor film 43, and utilizes charge repulsion to achieve precise and efficient laying of metal powder in a two-dimensional plane, solving the problem of difficult positioning of traditional metal powder.
[0077] Among them, such as Figure 3 As shown, the empty slot 420 is located directly below the bottom of the inner sleeve 42. The first electrode plate 44 is energized, that is, the first electrode plate 44 provides a large amount of first charge. The first electrode plate 44 directly applies the charge repulsion force to the metal powder on the organic photoconductor film 43 through the empty slot 420, and repels all the first charged metal powder in this area onto the deposition plate 1.
[0078] In one of the alternative approaches, an organic photoconductor is a special type of semiconductor that is an insulator in the dark but becomes a conductor when exposed to a light source. The matrix material of the organic photoconductor is aluminum chlorophthalocyanine and polycarbonate. Aluminum chlorophthalocyanine is used to absorb light and generate charge carriers, while polycarbonate is used to transport charge.
[0079] In this application, the operation is carried out in a dark environment. First, the first charge is delivered to the organic photoconductor film 43 through the charging roller 7. Then, the laser 6 is activated to write black on the organic photoconductor film 43. Specifically, the position on the surface of the organic photoconductor film 43 where the metal powder is to be adhered is directionally scanned, that is, the position on the organic photoconductor film 43 to be written black is directionally scanned.
[0080] When the black area to be written on the organic photoconductor film 43 is illuminated by the laser 6, the black area to be written on the organic photoconductor film 43 becomes a conductor, and the first charge at the black area to be written flows away, forming an uncharged black area.
[0081] In an optional implementation, the first charge is either a positive charge or a negative charge.
[0082] In one or more implementations, such as Figure 4 As shown, the inner sleeve 42 is fixedly connected to the movable platform 3, and the first bearing 45 and the second bearing 46 are sleeved on the inner sleeve 42. The outer sleeve 41 is connected to the outer ring of the first bearing 45 and the second bearing 46.
[0083] The inner sleeve 42 is fixedly connected to the moving platform 3 so that the inner sleeve 42 moves together with the moving platform 3. Then, the first bearing 45 and the second bearing 46 are sleeved on the inner sleeve 42. The outer sleeve 41 is connected to the outer ring of the first bearing 45 and the second bearing 46, so that the outer sleeve 41 is rotatably installed on the inner sleeve 42, so that the outer sleeve 41 can move together with the inner sleeve 42 and can also rotate around the inner sleeve 42.
[0084] In optional implementations, such as Figure 5 As shown, the inner sleeve 42 includes a first cylinder 421 and a second cylinder 422 connected to each other. The diameter of the second cylinder 422 is smaller than that of the first cylinder 421. The second cylinder 422 is connected to the movable platform 3, as shown. Figure 4 The inner ring of the first bearing 45 is sleeved on the first cylinder 421, and the inner ring of the second bearing 46 is sleeved on the second cylinder 422.
[0085] like Figure 6 As shown, the outer sleeve 41 includes a first annular body 411 and a second annular body 412 connected to each other. The diameter of the second annular body 412 is smaller than that of the first annular body 411. The inner wall of the first annular body 411 is connected to the outer ring of the first bearing 45, and the inner wall of the second annular body 412 is connected to the outer ring of the second bearing 46. Figure 4 ,;
[0086] An organic photoconductor film 43 covers the first annular body 411.
[0087] Furthermore, such as Figure 5 As shown, the empty slot 420 is located directly below the bottom of the first cylinder 421, and the empty slot 420 is arranged along the length of the first cylinder 421.
[0088] like Figure 4 As shown, the first electrode plate 44 is arranged along the length of the first cylinder 421, and part of the first electrode plate 44 is located in the empty groove 420.
[0089] When the powder drum 4 moves to the preset powder spreading position, the first electrode plate 44 is energized, that is, the first electrode plate 44 provides a large amount of first charge. The first electrode plate 44 is used to repel the metal powder on the organic photoconductor film 43 in the corresponding area of the empty slot 420, and repel all the metal powder with the first charge in this area onto the deposition plate 1.
[0090] In an optional configuration, the end of the first cylinder 421 away from the second cylinder 422 has a first stepped portion 4211, and the first bearing 45 is sleeved on the first stepped portion 4211, such as... Figure 4 ;
[0091] The second cylinder 422 has a second stepped portion 4221 at one end near the first cylinder 421, and a second bearing 46 is sleeved on the second stepped portion 4221. The first cylinder 421 is connected to the second stepped portion 4221. Figure 4 .
[0092] Among the optional methods, such as Figure 4 As shown, it also includes an end cap 47, which is installed at the end of the first annular body 411 away from the second annular body 412 and seals the port of the first annular body 411.
[0093] In one or more implementations, such as Figure 1 , Figure 4 As shown, it also includes a gear set 8, which includes a driving gear 81 and a driven gear 82 that cooperate with each other. The driven gear 82 is fixedly mounted on the second ring body 412.
[0094] Gear set 8 also includes a drive motor 83, which drives the drive gear 81, and the drive gear 81 drives the outer sleeve 41 to rotate through the driven gear 82.
[0095] During operation, the drive motor 83 is started, which drives the drive gear 81. The drive gear 81 drives the outer sleeve 41 to rotate through the driven gear 82. At this time, metal powder is supplied to the outer sleeve 41 through the powder tank 5. Then, the powder drum 4 is moved to the predetermined powder spreading position by the moving table 3. During powder spreading, the drive motor 83 controls the rotation of the outer sleeve 41 so that the metal powder on the annular surface of the outer sleeve 41 can be spread out.
[0096] In one or more implementations, such as Figure 1 As shown, it also includes a first linear guide rail 2, which is located above the deposition plate 1. The moving stage 3 is mounted on the first linear guide rail 2 and can move along the length of the first linear guide rail 2.
[0097] The moving stage 3 moves along the length of the first linear guide rail 2, and the moving stage 3 drives the powder drum 4 to move on the deposition plate 1.
[0098] In optional implementations, such as Figure 9As shown, the first linear guide 2 includes a first slider 21, a first lead screw 22, a first optical axis 23 and a first motor 24. The first slider 21 has a first threaded hole in the middle, the first lead screw 22 passes through the first threaded hole, the first optical axis 23 passes through the first slider 21, and the first optical axis 23 is parallel to the first lead screw 22.
[0099] The first motor 24 is located at one end of the first lead screw 22, and the first motor 24 is used to drive the first lead screw 22 to rotate;
[0100] The moving stage 3 is fixedly connected to the first slider 21.
[0101] The first motor 24 drives the first lead screw 22 to rotate, thereby driving the first slider 21 to move. Since the moving table 3 is fixedly connected to the first slider 21, the moving table 3 is driven to move, which in turn drives the powder drum 4 and the powder bucket 5 to move.
[0102] In optional implementations, such as Figure 10 As shown, the first linear guide rail 2 also includes a first frame 25, a first lead screw 22 and a first optical axis 23 located inside the first frame 25, and the first lead screw 22 and the first optical axis 23 are arranged along the length of the first frame 25. The first motor 24 is installed at one end of the first frame 25.
[0103] The first slider 21 moves within the first frame 25 along the length direction of the first lead screw 22.
[0104] In one or more implementations, such as Figure 7 , Figure 8 As shown, the powder bin 5 is equipped with a powder hopper 51 inside, and a charging plate 52 is provided at the bottom of the powder hopper 51. The charging plate 52 is used to charge the metal powder in the powder hopper 51 with a first charge.
[0105] A discharge port 55 is provided on one side of the bottom of the powder silo 51. A powder feeding shaft 53 is rotatably installed at the discharge port 55. The powder feeding shaft 53 is used to transport metal powder onto the organic photoconductor film 43.
[0106] Before starting, metal powder is put into the powder hopper 51 of the powder bucket 5, and the charging plate 52 at the bottom of the powder hopper 51 is used to charge the metal powder in the powder hopper 51 with the first charge, so that the surface of the metal powder has the first charge.
[0107] Meanwhile, a discharge port 55 is provided on one side of the bottom of the powder hopper 51. A powder feeding shaft 53 is rotatably installed at the discharge port 55. When in use, the powder feeding shaft 53 rotates to adhere metal powder, and then the metal powder is transported to the organic photoconductor film 43.
[0108] The discharge port 55 is located on the side of the powder hopper 5 near the organic photoconductor film 43, and the powder feeding shaft 53 contacts the organic photoconductor film 43.
[0109] In this embodiment, the first electrode plate 44 applies a charge repulsion force to the metal powder on the organic photoconductor film 43, and repels all the first-charged metal powder in this region onto the deposition plate 1. The specific implementation is as follows:
[0110] like Figure 11 As shown, after the charging roller 7 transfers the first charge to the organic photoconductor film 43, the organic photoconductor film 43 is now carrying the first charge.
[0111] During operation, the charging roller 7 is first energized and the powder drum 4 is driven to rotate. After charging, the surface of the charging roller 7 carries a large amount of first charge, and after contacting the organic photoconductor film 43, the first charge is transferred to the surface of the organic photoconductor film 43.
[0112] Then, the laser 6 is used to write black areas onto the organic photoconductor film 43. Specifically, the laser 6 performs a directional scan of the surface of the organic photoconductor film 43 at the locations where metal powder is to be adhered, eliminating the first charge in the areas where the metal powder is to be adhered, thus forming corresponding black areas. Figure 11 ;
[0113] Then, the powder feeding shaft 53 is rotated, bringing it into contact with the locally charged organic photoconductor film 43. Under the influence of the electrostatic force, the metal powder carrying the first charge adheres to the writing area of the organic photoconductor film 43, such as... Figure 11 ;
[0114] It is important to note that the reason why the metal powder does not stick to other areas is that other areas carry a first charge, while the metal powder itself carries a first charge, so there is a mutual repulsion phenomenon. However, the black writing area is uncharged, so there is no repulsion phenomenon. The metal powder carrying the first charge will be adsorbed onto the black writing area of the organic photoconductor film 43.
[0115] In one or more implementations, such as Figure 1 As shown, multiple powder control systems are arranged at intervals around the powder drum in four directions.
[0116] Among them, there are no fewer than two powder control systems.
[0117] In this implementation, such as Figure 1 , Figure 11As shown, by setting up multiple powder control systems, each powder control system is activated sequentially according to the rotation direction of the organic photoconductor film 43 to perform blackening and powder feeding on the organic photoconductor film 43. For example, the laser 6 of the first powder control system is activated to perform the first blackening of the organic photoconductor film 43. Then, metal powder ① is provided to the first blackening area of the organic photoconductor film 43 through the powder tank 5 of the first powder control system. Then, the laser 6 of the second powder control system is activated to perform the second blackening of the organic photoconductor film 43. The second blackening area is staggered from the already blackened area. Then, metal powder ② is provided to the second blackening area of the organic photoconductor film 43 through the powder tank 5 of the second powder control system. And so on. This makes it easy to use electrostatic control to achieve the laying of various metal powders. Different metal powders have their corresponding blackening areas, which effectively avoids contamination between different materials and also achieves high and precise laying of metal powders.
[0118] The following example uses two toner control systems, namely two toner tanks 5 and two lasers 6. One toner tank 5 is named the first toner tank 5, and the other toner tank 5 is named the second toner tank 5. One laser 6 is named the first laser, and the other laser 6 is named the second laser.
[0119] The first powder bin 5 provides metal powder ①, and the second powder bin 5 provides metal powder ②;
[0120] After charging, when the powder drum 4 passes the first laser, the first laser performs the first writing on the organic photoconductor film 43, that is, it performs a directional scan on the surface of the powder drum 4 at the position where the metal powder ① is to be adhered. Then, the first powder container 5 provides the metal powder ① to the first writing area of the powder drum 4, such as... Figure 11 ;
[0121] After charging, when the toner drum 4 passes the second laser, the second laser performs a second writing operation on the organic photoconductor film 43, that is, it performs a directional scan on the surface of the toner drum 4 at the position where the metal powder ② is to be adhered. Then, the second toner cartridge 5 provides the metal powder ② to the second writing area of the toner drum 4, such as... Figure 11 ;
[0122] After the powder drum 4 reaches the powder spreading position, the first electrode plate 44 begins to provide a large amount of first charge at this position to repel the first charged metal powder on the powder drum 4 and repel it all onto the deposition plate 1, thus realizing a complete selective multi-material powder deposition process.
[0123] After the powder is spread, the SLM equipment will continue to perform laser scanning and other tasks.
[0124] In this application, it should be noted that the high precision of powder spreading depends primarily on the accurate blackening achieved by laser scanning. In existing powder spreading strategies using vibration or other methods, the precision of laser scanning is extremely high, easily reaching several micrometers. For the powder being spread, since the particle size of the powder has exceeded ten micrometers (generally 15μm to 53μm), this method of powder spreading can directly reach the limit of powder spreading precision (i.e., the size of the powder particle size). The powder spreading precision achieved by vibration and other methods is generally above 100μm.
[0125] Example 2
[0126] like Figure 8 As shown, based on Embodiment 1, the charge-controlled metal powder laying device described in this embodiment further includes a stirring paddle 54 provided at the discharge port 55, which is used to transport the metal powder to the powder feeding shaft 53.
[0127] The stirring paddle 54 is used to carry the metal powder out of the powder hopper 51. The stirring paddle 54 contacts the powder feeding shaft 53 so that the surface of the powder feeding shaft 53 is uniformly coated with metal powder.
[0128] In an optional configuration, the powder bucket 5 is fixedly connected to the moving platform 3, such as by bolts.
[0129] Among the optional methods, such as Figure 8 As shown, it also includes an arc-shaped baffle 56 disposed in the powder silo 51. The arc-shaped baffle 56 is disposed at the discharge port 55, and the arc-shaped baffle 56 forms a stirring chamber in the powder silo 51. The stirring paddle 54 and the powder feeding shaft 53 are located in the stirring chamber.
[0130] One side of the mixing chamber is connected to the discharge port 55, and the other side of the mixing chamber is provided with an opening 561, which is connected to the powder hopper 51, and the charging plate 52 is located outside the opening.
[0131] An arc-shaped baffle 56 is used to form a mixing chamber. The stirring paddle 54 and the powder delivery shaft 53 are located inside the mixing chamber. The metal powder passing through the charging plate 52 enters the mixing chamber through the opening 561, thereby preventing the metal powder above the powder hopper 51 that has not been charged with the first charge from contacting the powder delivery shaft 53. This ensures the powder delivery quality of the powder hopper 5 to the writing black area of the organic photoconductor film 43 and provides printing quality.
[0132] Example 3
[0133] like Figure 11 As shown, based on Embodiment 1 or Embodiment 2, the charge-controlled metal powder laying method described in this embodiment, and based on the metal powder laying device described in Embodiment 1 or Embodiment 2, includes the following steps:
[0134] S1: Put metal powder into powder bucket 5;
[0135] Metal powder is added into the powder hopper 51 of the powder hopper 5, and the charging plate 52 at the bottom of the powder hopper 51 is activated to charge the metal powder with the first charge.
[0136] S2: Power is applied to the charging roller 7, and the outer sleeve 41 is driven to rotate. The charging roller 7 comes into contact with the organic photoconductor film 43 and charges the organic photoconductor film 43 with the first charge.
[0137] S3: After the organic photoconductor film 43 is charged, the laser 6 is activated to write black on the surface of the organic photoconductor film 43 to form a black area. Then, the powder tank 5 is controlled to deliver metal powder with the first charge to the black area.
[0138] Among them, the bottom side of the powder silo 51 is also provided with a discharge port 55, a powder feeding shaft 53 is rotatably provided at the discharge port 55, and a stirring paddle 54 is also provided at the discharge port 55. By rotating the stirring paddle 54, powder is supplied to the powder feeding shaft 53 at the discharge port 55, so that the metal powder adheres to the surface of the powder feeding shaft 53.
[0139] The powder feeding shaft 53 contacts the organic photoconductor film 43 and, under the action of electric force, adheres the metal powder with the first charge to the writing black area of the organic photoconductor film 43.
[0140] S4: After the powder drum 4 moves to the powder spreading position, the first electrode plate 44 is energized so that the first electrode plate 44 repels the metal powder in the writing black area to the powder spreading position of the deposition plate 1.
[0141] S5: After the powder is spread, start the SLM equipment to continue the laser scanning work, and then repeat steps S1 to S5.
[0142] In step S3:
[0143] It includes multiple toner control systems, which are spaced around the toner drum in four directions. According to the rotation direction of the organic photoconductor film 43, each toner control system is activated in sequence to write black and feed toner onto the organic photoconductor film 43.
[0144] Example 4
[0145] Based on Examples 1 to 3, as follows Figure 11 As shown, the charge-controlled metal powder laying method described in this embodiment is a preferred method in actual operation. In this embodiment, the first charge is a negative charge, and the specific steps are as follows:
[0146] One: such as Figure 1 As shown, before starting, different metal powders are placed in the two powder containers 5 respectively;
[0147] Second: During operation, the charging roller 7 is first energized and the powder drum 4 is driven to rotate. After charging, the surface of the charging roller 7 carries a large amount of negative charge, and after contacting the powder drum 4, the negative charge is transferred to the surface of the organic photoconductor film 43 of the powder drum 4.
[0148] It is important to note that organic photoconductors are a special type of semiconductor that is an insulator in the dark but becomes a conductor when exposed to a light source.
[0149] Third: After charging, the powder drum 4 passes through the first laser 6. The first laser 6 writes black on the surface of the powder drum 4, that is, it performs directional scanning on the surface of the powder drum 4 at the position where the metal powder is to be adhered. According to the aforementioned principle, at this time, the corresponding position becomes a conductor, and the negative charge at that position disappears.
[0150] Fourth: At the same time, the stirring paddle 54 and charging plate 52 in the first powder bucket 5 start to work. The charging plate 52 is used to charge the metal powder in the powder bucket 5. Even if the surface of the metal powder has a certain amount of charge, the charge here is negative. The stirring paddle 54 is used to carry the metal powder out of the powder bucket 5 and contact the powder feeding shaft 53. After the powder feeding shaft 53 is coated with uniformly charged metal powder, it approaches the locally charged powder drum 4 and, under the action of the charge force, sticks the metal powder ① of the first powder bucket 5 to the black area.
[0151] It is important to note that the reason why the metal powder does not stick to other areas is that the other areas are negatively charged, while the metal powder itself is negatively charged, so there is a repulsion phenomenon. However, the black areas are uncharged, so there is no repulsion phenomenon.
[0152] 5. When passing the second laser 6, the powder drum 4 is written black again, that is, all other parts of the powder drum 4 are written black, and when passing the second powder bucket 5, the other parts of the powder drum 4 are coated with metal powder ②.
[0153] Sixth: After the powder drum 4 reaches the powder-laying position, the first electrode plate 44 begins to provide a large amount of negative charge at this point to repel the negatively charged metal powder on the powder drum 4 and repel it all onto the deposition plate 1, thus realizing a complete selective multi-material powder deposition process.
[0154] 7. After the powder is spread, the SLM equipment will continue to perform laser scanning and other tasks.
[0155] It should be noted that in the overall powder spreading process, the high precision of powder spreading depends primarily on the accurate blackening achieved by laser scanning. In existing powder spreading strategies using vibration or other methods, the precision of laser scanning is extremely high, easily reaching a few micrometers. For the powder being spread, since the particle size of the powder already exceeds ten micrometers (generally 15-53 micrometers), this method can directly reach the limit of powder spreading precision (i.e., the size of the powder particle size). The powder spreading precision achieved by vibration and other methods is generally above 100 micrometers.
[0156] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A charge-controlled metal powder laying device, characterized in that, It includes a deposition plate (1), a moving stage (3), a powder drum (4) and a charging roller (7), wherein the moving stage (3) is located above the deposition plate (1); The powder drum (4) is mounted on the moving platform (3). The powder drum (4) includes an outer sleeve (41) and an inner sleeve (42) arranged coaxially. The outer sleeve (41) is rotatably arranged around the inner sleeve (42). An organic photoconductor film (43) is covered on the outer sleeve (41). The charging roller (7) is used to deliver a first charge to the organic photoconductor film (43). The inner sleeve (42) has a first electrode plate (44) inside, and the bottom of the inner sleeve (42) is provided with a slot (420). The first electrode plate (44) and the slot (420) are both arranged along the length of the inner sleeve (42), and the first electrode plate (44) is partially located in the slot (420). It also includes a powder control system provided on the moving stage (3), the powder control system including a powder tank 5 (5) and a laser (6), the laser (6) being used to form an uncharged writing black area on the organic photoconductor film (43), and the powder tank 5 (5) being used to deliver metal powder with a first charge to the writing black area; The first electrode plate (44) is used to repel the metal powder after being energized.
2. The charge-controlled metal powder laying device according to claim 1, characterized in that, Multiple powder control systems are arranged at intervals around the powder drum (4) in a circumferential direction.
3. The charge-controlled metal powder laying device according to claim 1, characterized in that, The powder hopper 5 (5) is provided with a powder hopper (51) inside, and a charging plate (52) is provided at the bottom of the powder hopper (51); The powder silo (51) is also provided with a discharge port (55) on one side of the bottom, and a powder feeding shaft (53) is rotatably provided at the discharge port (55).
4. The charge-controlled metal powder laying device according to claim 3, characterized in that, It also includes a stirring paddle (54) provided at the discharge port (55).
5. The charge-controlled metal powder laying device according to claim 1, characterized in that, The inner sleeve (42) is fixedly connected to the moving platform (3), and a first bearing (45) and a second bearing (46) are sleeved on the inner sleeve (42). The outer sleeve (41) is connected to the outer ring of the first bearing (45) and the second bearing (46).
6. The charge-controlled metal powder laying device according to claim 5, characterized in that, The inner sleeve (42) includes a first cylinder (421) and a second cylinder (422) connected to each other. The diameter of the second cylinder (422) is smaller than that of the first cylinder (421). The second cylinder (422) is connected to the moving platform (3). The inner ring of the first bearing (45) is sleeved on the first cylinder (421), and the inner ring of the second bearing (46) is sleeved on the end of the second cylinder (422) away from the first cylinder (421). The outer sleeve (41) includes a first annular body (411) and a second annular body (412) connected to each other. The diameter of the second annular body (412) is smaller than that of the first annular body (411). The inner wall of the first annular body (411) is connected to the outer ring of the first bearing (45), and the inner wall of the second annular body (412) is connected to the outer ring of the second bearing (46). The organic photoconductor film (43) covers the first annular body (411).
7. A charge-controlled metal powder laying device according to claim 6, characterized in that, It also includes a gear set (8), which includes a driving gear (81) and a driven gear (82) that cooperate with each other, and the driven gear (82) is fixedly mounted on the second ring body (412); The gear set (8) also includes a drive motor (83), which drives the drive gear (81), and the drive gear (81) drives the outer sleeve (41) to rotate through the driven gear (82).
8. The charge-controlled metal powder laying device according to claim 1, characterized in that, It also includes a first linear guide rail (2), which is located above the deposition plate (1), and the moving stage (3) is mounted on the first linear guide rail (2), and the moving stage (3) is capable of moving along the length direction of the first linear guide rail (2).
9. A method for laying metal powder based on charge control, characterized in that, Based on the metal powder laying apparatus as described in any one of claims 1-8, the process includes the following steps: S1: Different metal powders are placed in different powder buckets 5 (5); S2: The charging roller (7) is energized, and the outer sleeve (41) is driven to rotate. The charging roller (7) contacts the organic photoconductor film (43) and charges the organic photoconductor film (43) with a first charge. S3: After the organic photoconductor film (43) is charged, the laser (6) is activated to write black on the surface of the organic photoconductor film (43) to form the writing black area, and then the powder tank 5 (5) is controlled to deliver metal powder with the first charge to the writing black area; S4: After the powder drum (4) moves to the powder spreading position, the first electrode plate (44) is energized so that the first electrode plate (44) repels the metal powder in the writing black area to the powder spreading position of the deposition plate (1). S5: After the powder is spread, start the SLM equipment to continue the laser scanning work, and then repeat steps S1 to S5.
10. A method for laying metal powder based on charge control according to claim 9, characterized in that, In step S3: The system includes multiple toner control systems, which are arranged circumferentially around the toner drum (4) and are activated sequentially according to the rotation direction of the organic photoconductor film (43) to write black and feed toner onto the organic photoconductor film (43).