Degradable plastic quality release and demolding residue traceability management method
By introducing a dual-channel ultraviolet optical detection method using fluorescent whitening agents and polyvinyl alcohol witness sheets into compostable plastic parts, the problem of real-time quantitative determination of external spraying and demolding residues on the surface of the parts has been solved, enabling stable release and traceability of the parts and improving production efficiency and compliance.
Patent Information
- Application Number
- CN202511606652.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-05
- Publication Date
- 2026-01-30
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the mass production of injection-molded or thermoformed parts that are compostable and in contact with food, it is difficult to achieve real-time, stable, and quantifiable determination of the residues left by external spraying on the surface of the parts, and to directly correspond to the migration and composting evaluation thresholds, which makes it difficult to guarantee production efficiency and compliance.
By adding the fluorescent whitening agent Eubi-type to the matrix as an inner channel tracer, and attaching a polyvinyl alcohol witness sheet to the edge of the cavity to form an outer channel, the intensity of the inner and outer channels is collected by dual-channel ultraviolet optical position acquisition, the ratio coefficient is calculated and the red-yellow-green threshold is set to generate a correction list, realizing automatic spraying volume, air cutting and mold temperature adjustment of the part, and generating cavity-level demolding events and binding them with two-dimensional barcodes.
It enables real-time, stable, and quantifiable determination of external spray residue on the surface of parts, forming consistent release and traceability across molds and production lines, taking into account the boundaries of food contact and compostability, reducing manual intervention and repeated adjustments, and improving production efficiency and compliance.
Smart Images

Figure CN121437016A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of quality release traceability technology, specifically to a method for quality release and mold release residue traceability management of biodegradable plastics. Background Technology
[0002] Compostable plastics (such as polylactic acid, polybutylene succinate and their blends) have been widely used in injection molding and thermoforming of food parts that come into direct or indirect contact with food, such as catering, ready-to-eat fresh food, and medical auxiliary packaging. These parts have narrow molding windows and are sensitive to crystallization and cooling. In production, they generally rely on a combination of internal lubricant / internal release additives and external release agents to ensure smooth ejection and surface quality.
[0003] Typical products include cup lids, takeout boxes, shallow trays, and medical device holders. These products have complex surface morphologies, significant curvature variations, and short thermal histories in thin-walled areas, resulting in uneven distribution and carrying height of the externally sprayed release agent on the surface. However, the actual residual amount of the externally sprayed release agent on the surface is invisible, offline sampling is lagging, and it is coupled with overall migration, specific migration, and disintegration and biodegradation: excessive residue may increase migration values and interfere with the composting process, while insufficient spraying can easily lead to whitening, patterning, rib breakage, and mold sticking, causing downtime and creating a dual contradiction between efficiency and compliance. Laboratory migration and composting evaluations often require a long period, making it difficult to promptly close the loop to process control, forcing production to rely solely on experience and post-production corrections. Existing online quality control relies heavily on indirect indicators such as experience windows, spray gun timing, or total weight, lacking real-time, quantitative, and batch-level evidence of residues on the surface of the parts.
[0004] Existing technologies attempt to detect coverage or film thickness using ultraviolet light by adding fluorescent indicators to release agents or mold coatings. However, these methods primarily observe the mold side or the coating itself, making it difficult to accurately correlate with migratable residues on the part surface. Furthermore, the inclusion of these indicators in the formulation may introduce additional migration and odor risks, hindering food contact and compostability compliance. On the other hand, compostable systems often contain fatty acid ester internal lubricants, which exhibit surface precipitation. This, combined with external spray residues, causes traditional single-channel optical readings to fluctuate due to light source attenuation, surface reflection, and distance variations, resulting in insufficient consistency in determinations across molds and curvatures.
[0005] Furthermore, production and supply chain traceability often remains at the batch or order level, making it difficult to correlate spray volume, online readings with cavities and mold batches one by one. When customers fail spot checks or file complaints, companies often have to expand the scope of isolation and re-inspection, unable to quickly define the boundaries of impact, leading to a significant increase in the costs of line stoppages, scrapping, and recalls.
[0006] Therefore, the current problem to be solved is: in the mass production scenario of compostable, food-contact injection-molded or thermoformed parts, how to obtain real-time, stable, quantifiable judgment results on the surface of the parts that are sprayed with the demolding residue, and how to directly correspond to the migration and composting evaluation thresholds, so as to form a traceable release basis at the cavity and mold granularity. Summary of the Invention
[0007] (a) Technical problems to be solved To address the shortcomings of existing technologies, this invention provides a method for quality release and mold release residue traceability management of biodegradable plastics. By collecting two intensity data points, calculating the ratio coefficient, and mapping it to surface residues, a red-yellow-green threshold and a correction list are generated. The part undergoes a black-box assessment, automatically issuing spray volume, air shear, and mold temperature commands. The method witnesses the removal of the molded part from the warm water and confirms the background temperature. Simultaneously, a cavity-level demolding event is generated and bound to a digitally linked two-dimensional barcode. Using a quantile reference and a convergence threshold, third-party compliant documents are archived in a document-like format, achieving consistent release and verifiable traceability across molds and production lines, while also considering food contact and compostability boundaries. This solves the technical problems described in the background art.
[0008] (II) Technical Solution To achieve the above objectives, the present invention provides the following technical solution: A method for quality release and mold release residue traceability management of biodegradable plastics includes incorporating fluorescent whitening agent Obi-type as an internal channel tracer into the matrix under the combination of matrix and internal mold release / lubrication; attaching polyvinyl alcohol witness sheets to the edge of the cavity and pre-setting riboflavin microarrays; setting dual-channel ultraviolet optical positions to form internal and external channels; Collect the intensity of the inner and outer channels, calculate the ratio coefficient and establish a mapping relationship with the residual surface density; set the three-color threshold and the corresponding correction rules for spray reduction, air shearing, and mold temperature adjustment based on the mapping. The part is detected by the black box to obtain the ratio coefficient, and spray volume, air shear, and mold temperature correction instructions are generated according to the three-color threshold. The cavity-level demolding event is generated, written into the event and product information sharing version 2.0, and bound to the digital link two-dimensional barcode. In mass production, the three-color thresholds are re-converged using quantile references to form update breakpoints; third-party compliance documents and cavity-level demolding events are centrally archived and bound as the basis for release and replication.
[0009] Furthermore, the matrix is selected from polylactic acid, polylactic acid and butylene glycol-adipic acid / terephthalic acid copolyester, and polybutylene succinate; the internal release / lubrication combination is composed of rice bran wax and glyceryl monostearate, both of which are fed from the same source as the matrix masterbatch, and the fluorescent whitening agent Obi-type is incorporated with the masterbatch.
[0010] Furthermore, the polyvinyl alcohol witness sheet is attached to the non-food contact edge of the cavity or the predetermined cutting area, and the surface is pre-formed with riboflavin microarrays; after the part is removed, the sample is collected at the black box detection position according to the predetermined path, and then the witness sheet is completely detached by warm water mist or short-range spray in the later stage.
[0011] Furthermore, after compensating for temperature, imaging delay, and incident angle, the ratio coefficient between the inner channel intensity and the outer channel intensity is calculated, and a monotonic mapping is established between the ratio coefficient and the residual surface density to form a three-color threshold distinguished by the breakpoint.
[0012] Furthermore, the correction rules are assigned according to priority: when the ratio coefficient is in the yellow zone and the spray volume has not touched the boundary, only the spray volume is adjusted; when it touches the boundary, the air cut is extended simultaneously; when entering the red zone, release is paused and the mold temperature or cooling time is adjusted.
[0013] Furthermore, the cavity-level demolding event includes the mold number, cavity number, internal correction strength, external correction strength, ratio coefficient, threshold judgment, spray volume setting, air shear and mold temperature command, witness sheet number, formula batch and compliance document number, and is written into the event and product information sharing version 2.0 and bound to a digital link two-dimensional barcode.
[0014] Furthermore, using the quantile reference of the shift ratio coefficient sequence as the field center, the three-color threshold is re-converged to generate an update breakpoint, and the version and source working condition are recorded on the online closed-loop curve page, and the rollback path is saved for cross-line review and copying. Third-party compliance documentation should include at least overall and specific migration reports in accordance with plastic food contact regulations, as well as interim reports on disintegration and biodegradation, and should be centrally archived and linked with cavity-level demolding events in a ticket folder.
[0015] Furthermore, economic reconciliation uses output, unit gross profit, machine time value, and cycle time savings as revenue items, and deducts spray volume cost, witness film cost, depreciation and maintenance cost; replication consistency is scored by percentile difference and weight, and replication is enabled after reaching a preset threshold.
[0016] (III) Beneficial Effects This invention provides a method for quality release and mold release residue traceability management of biodegradable plastics, which has the following beneficial effects: An optical brightener, Eubi-type, is introduced into the matrix and internal release lubrication assembly to form an inner channel. Polyvinyl alcohol witness sheets are attached to the edge of the cavity and pre-placed with riboflavin microarrays to form an outer channel, which is then used in conjunction with dual-channel ultraviolet optical imaging for synchronous acquisition. After the witness sheets are removed by warm water, no chemical residue is left on the parts, thus maintaining the boundary between compost and food contact.
[0017] A calibration array is established based on the amount of external spraying, mold temperature and formula. The strength of the internal and external channels is collected for each piece, the ratio coefficient is calculated and mapped with the residual surface density, and red, yellow and green thresholds and correction list are set to transform the external spraying residue from empirical judgment to quantitative criterion. The judgment caliber is consistent in different molds and curved surfaces.
[0018] The black box detection unit displays the strength of the inner channel, the strength of the outer channel, and the ratio coefficient per piece. It automatically generates instructions for spray volume, air cutting, and mold temperature correction based on red, yellow, and green thresholds. The subsequent stage verifies the separation of the polyvinyl alcohol witness sheet from warm water and confirms the background, forming a closed loop from detection to action to risk clearance, reducing manual intervention and repeated adjustments.
[0019] With cavity-level demolding events as the core, fields such as mold number, cavity number, ratio coefficient, threshold judgment, spray volume and air shear and mold temperature settings, witness sheet number and baseline confirmation, and compliance document number are written into the event and product information sharing version 2.0, and bound to the finished product digital link two-dimensional barcode to form a unified identification and verifiable traceability chain.
[0020] In mass production, the red, yellow, and green thresholds are re-converged using quantile references to generate update breakpoints. Threshold version management and rollback are implemented across molds and production lines. Combined with consistency scoring before replication and the binding of third-party compliance documents into a ticket-based archive, release, review, and replication follow the same criteria, providing a consistent foundation for large-scale replication and continuous improvement. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the process for quality release and mold release residue traceability management of biodegradable plastics according to the present invention. Detailed Implementation
[0022] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0023] Please see Figure 1 This invention provides a method for quality release and mold release residue traceability management of biodegradable plastics, including: Step 1: Establish input boundaries and observability: Add fluorescent whitening agent Eubi-type to polylactic acid or its copolymer system as an inner channel anchor; attach polyvinyl alcohol witness sheet to the edge of the cavity and pre-place riboflavin to form an outer channel; after part removal, set up dual-channel ultraviolet detection positions and fix the geometry; connect the key fields of the injection molding machine to the manufacturing execution system through the injection molding industry communication standard No. 77 as the starting point for calibration and traceability.
[0024] If the internal demolding / lubrication and internal channel tracer enter through different feeding paths, local enrichment is likely to occur after molding, leading to discrete internal strength readings and difficulty in reusing thresholds across molds. Rice bran wax and glyceryl monostearate are uniformly prepared into a masterbatch of the same material as the matrix, and fed into the same mixing hopper in the order of wax first and then ester. This allows the low-melting-point component to preferentially wet the surface of the matrix particles, and then be melt-blended under high shear to form a stable thin-layer coating. The fluorescent whitening agent Obi-type is incorporated into the same material masterbatch at a level of one part per million, so that it overlaps with the dispersion domain of the internal demolding / lubrication but does not participate in the chemical reaction.
[0025] At the feeding end, a dual-valve staggered feeding method is used. First, the rice bran wax masterbatch valve is opened for 30 counts, then the glycerol monostearate valve is opened, and finally the matrix valve is opened uniformly. This ensures that the two types of additives are first dispersed in a small volume and then mixed with the large volume matrix. The melting section adopts a higher shear level so that the masterbatch coating forms a continuous transition between particles.
[0026] This creates a homologous pathway where additives disperse first and the matrix then merges, reducing batch-to-batch fluctuations in internal channel readings. Simultaneously, the fluorescent whitening agent Obi-type enters along with the same masterbatch, undergoing the same thermal history, thus reducing the impact of subsequent temperature drift.
[0027] A sampling window is set at the end of the feeding process. Three handfuls of particles are randomly selected, and the waxy sheen is visually inspected for uniformity. Low-magnification microscopy confirms that no lumpy precipitation is observed. The sampling window is then closed, and batch handover is signed. Recording the uniform appearance, microscopic thin-layer examination, and handover signature as the visible final state before production helps to trace back to the same feeding source and visual evidence in any subsequent disputes.
[0028] Furthermore, the difference between the surface temperature of the workpiece during image acquisition and the image acquisition delay will change the luminescence intensity of the Euclid fluorescent whitening agent. It is necessary to normalize it using a unified reference surface to ensure that the subsequent threshold can be reused across work groups.
[0029] An exponential-logarithmic composite compensation relationship was established between the initial internal strength measured at the black box position and temperature and time delay. First, exponential compensation was applied to temperature drift, and then logarithmic stretching with a slow opening was applied to the effect of time delay, thereby obtaining the internal correction strength at a unified reference point. Furthermore, the internal intensity with different thermal histories and time delays is brought back to a unified reference, as follows:
[0030] Where: internal correction strength , is the strength used as a reference for the inner channel, and is non-negative; inner strength , is the direct reading from the camera in the black box position, and is non-negative; temperature The reference temperature is the surface temperature of the workpiece at the moment of image acquisition. , is the image acquisition reference temperature; image acquisition delay , is the time from mold ejection to image acquisition; reference delay For reference delay; temperature compensation coefficient The magnitude of decay of the exponential term. Between 0.01 and 0.1; Time compensation coefficient , used to determine the size of the opening for logarithmic terms. Between 0.01 and 0.3.
[0031] With this compensation, the coupling between the inner channel reading and process fluctuations is significantly weakened. When comparing different molds and curvatures, the inner channel becomes a stable self-calibration benchmark. In subsequent ratio determination, the inner channel plays the role of the denominator, which can effectively suppress the common drift caused by the light source and geometry.
[0032] Furthermore, a thermocouple probe and an image acquisition delay buzzer are fixed in the black box position to ensure that each piece is imaged within the set time window. After image acquisition, the internal correction intensity and temperature-delay bar are displayed on the screen. Recording of the piece is only allowed when the bar enters the green area; if it deviates, the image is automatically discarded and a prompt to re-acquire the image is given. Through the visible bar - allow / disable recording interface, the compensation conditions are ensured to be intuitively seen and executed by the operator, avoiding image drift caused by subjective human judgment.
[0033] External strength is significantly affected by the incident angle and surface curvature. Without angle compensation, external strength will fluctuate greatly with mold differences. Riboflavin microarrays are arranged on the test film to make it an overspray capture surface; during external channel imaging, a cosine power function is used to compensate for the incident angle to obtain the external corrected strength.
[0034] Furthermore, the attenuation caused by the incident angle and curvature is unified into a power-law framework, which facilitates cross-mold reuse, as detailed below:
[0035] Where: external correction strength , represents the external channel strength after angle correction, and is non-negative; external strength The fluorescence intensity of the witness film directly read by the camera is non-negative; the scaling factor , where is the gain coefficient of the optical system. Between 0.5 and 1.5; angle of incidence , where is the angle between the optical axis and the normal of the witness film; angle compensation power exponent , is the suppression index for the effect of curvature-angle. In 1 to 3.
[0036] After angle compensation, the sensitivity of the outer channel to image pose and curvature is reduced; combined with the inner channel compensation, the two are stabilized independently in geometric and thermal history.
[0037] Furthermore, after the witness film is attached, it is completely dissolved and detached by warm water mist or short-range spray in the rear section. Before detachment, the outer channel has completed image acquisition, and after detachment, the part no longer contains tracers. The water droplets generated by dissolution are uniformly introduced into the recycling tank and cleaned up according to shift handover.
[0038] When in use, the fixed sequence of capture-image acquisition-detachment ensures that the tracer does not enter the finished product; the witness sheet is used as a visible and removable temporary carrier, making the outer channel an independent physical surface, fundamentally avoiding the formulation disputes and migration risks caused by adding indicators to the release agent.
[0039] Using only the external correction intensity is insufficient for cross-line threshold reuse. However, using the internal correction intensity as the denominator to construct the ratio can cancel out the common drift of the optical system, thus transforming the problem into a single-parameter ratio determination. This is further mapped to the residual areal density for subsequent threshold setting. The ratio coefficient is defined by the ratio of the external correction intensity to the internal correction intensity. Then, a power function is used to establish the mapping relationship of residual areal density, ensuring a definite correspondence between optical readings and physical residue. Furthermore, the two readings are merged into a single stable index, facilitating threshold unification. Where:
[0040] Where: ratio coefficient , which is the dimensionless ratio of the two channels; external correction intensity Internal correction strength These are derived from the two formulas mentioned above, respectively.
[0041] When used, the ratio coefficient serves as a single parameter, providing direct coordinates for subsequent red-yellow-green threshold settings; at the same time, it weakens the differences in optical systems of different lines through the numerator and denominator structure.
[0042] Furthermore, a power function is used to characterize the monotonic correspondence between the ratio and the residue, which facilitates the labeling of the three-color thresholds in the form of curves on the same coordinate system, where:
[0043] Where: residual areal density The unit is micrograms per square decimeter, and it is non-negative; coefficient , is the dimensionless transformation coefficient. In the range of 1 to 100; index , representing the growth index from external intensity to residual intensity. Within the range of 0.5 to 2; offset , is the zero-point offset term. In the range of 0 to 10.
[0044] When used, this yields a plottable curve of ratio versus residue, providing a unified reference for threshold setting and shift recalibration in subsequent steps; the measurement conditions are clear, the algorithm configuration is feasible, and it is easy to replicate across different plant areas.
[0045] Step 2: Convert brightness into a quantitative value and form a release criterion: Establish a calibration array based on the amount of external spray, mold temperature and formula, collect the intensity of the internal and external channels for each piece, and complete the temperature and delay normalization and incident angle compensation; calculate the ratio coefficient and establish a mapping with the surface residue; set the red, yellow and green thresholds and the corresponding correction list for spray reduction, air shearing and mold temperature adjustment to form a unified standard.
[0046] If only a single operating condition is used for data collection, it is difficult to cover the interactions between external spraying, mold temperature, and formulation, as well as internal strength. External strength The fluctuations will manifest as non-convergence or multiple solutions in subsequent fitting, leading to a decrease in the ratio coefficient. The threshold is not transferable.
[0047] Among them, the minimum array starts with two levels of external spraying dosage × two levels of mold temperature × three formula groups, and internal strength is collected on a per-piece basis. External strength At the end of each operating condition, the chromatogram was obtained by wiping-liquid chromatography or weighing. The sampled values are used to form an optical-physical one-to-one mapping; subsequently, the corresponding temperature of each item is... With image acquisition delay Record them on the same line so that the difference between thermal history and beat can be eliminated during the calibration process.
[0048] In the black box position, fix the temperature probe and buzzer to the fixture bracket. After the buzzer sounds at the designated time, capture the image, and the screen will display the condition number and part number. - - - Records are kept; at the end of each working condition, the operator places the corresponding wiping cloth into a sample bag labeled with the same working condition number and returns it to the laboratory for registration. A fixed rhythm and standardized recording format ensure a closed loop of collection-sampling-backfilling, and internal strength... External strength It has cross-operating condition comparability, and subsequent calibration and ratio calculation are traceable with physical samples and serial numbers.
[0049] Five blank pieces were added at each of the array boundaries (highest mold temperature and lowest external spray) to observe when there was no witness piece residue. The baseline is set as an insurmountable zero-point constraint during modeling. This baseline locks the lower limit of the outer channel, preventing negative residuals or non-physical inflection points during fitting; the array covers the boundaries reachable in actual production, facilitating direct implementation after the threshold is set.
[0050] Internal strength With temperature With image acquisition delay The changes exhibit non-linear drift, and without correction, process differences will be incorrectly projected onto... Therefore, the internal strength needs to be considered. Mapping to a unified reference yields the internal correction strength. .
[0051] An exponential term is used to suppress temperature deviations, while a logarithmic term mitigates time delay differences. This results in a smooth and calculable normalization formula that neither excessively amplifies high-temperature fluctuations nor is overly sensitive to short time delays.
[0052] Where: internal correction strength As an internal channel reference, it is non-negative; internal strength Raw reading, non-negative; temperature 20 to 50 degrees Celsius; reference temperature 30 degrees Celsius; image acquisition delay 0 to 15 seconds; baseline delay 1 second; temperature compensation coefficient , 0.01 to 0.1; time compensation coefficient , 0.01 to 0.3.
[0053] Thus, the effects of different thermal histories and time delays can be converted to a unified benchmark in a controllable manner, so as to achieve different cycle times and mold temperatures. Comparable. Internal correction strength. It exhibits a single-peak stability region within the array range, reducing denominator jitter; This provides a basis for subsequent monotonicity and threshold transferability.
[0054] Furthermore, the temperature of the first and last pieces under each working condition was checked separately. With image acquisition delay If the data falls within the allowed recording range, and not within it, the entire segment of the data is marked as invalid and re-acquired. First and last component guardrails are used to prevent implicit deviations caused by mid-process drift, ensuring the strength of the internal correction. Statistical consistency.
[0055] As an overspray capture surface, the incident angle of the witness film The cosine attenuation caused by the curved surface position directly affects the external strength. If no compensation is provided, even if the external spray remains unchanged, Systematic deviations will also occur depending on the included angle.
[0056] The angle is suppressed by the cosine term in power form, while the proportionality constant is preserved. Used for calibrating the gain of optical systems, forming arrive Angle compensation is used to uniformly suppress the attenuation caused by angle and curvature, facilitating reuse across molds and surfaces.
[0057] Where: external correction strength As an outer channel reference, it is non-negative; outer strength The original reading is non-negative; the proportionality coefficient. , 0.5 to 1.5; angle of incidence 0 to 60 degrees; angle compensation power exponent , 1 to 3.
[0058] When in use, the external correction strength The correlation with positional changes weakens, and the comparability of the external channel in different cavity regions increases. After image acquisition, the witness film is completely dissolved and removed from the part by warm water mist or short-range spray in the later stage. The external channel of the part is then checked again in the black box position. The system displays a prompt that the witness film has been removed. Only after confirming that the external channel reading has returned to the background range can the part be packed.
[0059] The risk of tracer residue entering the finished product is eliminated by taking images, removing tracers, and confirming the background. The background confirmation is the visible final state, which is convenient for inspection.
[0060] Furthermore, it is necessary to combine the two calibration readings into a single stable index and correlate it with physical residual values. Establish monotonic correspondences to set release thresholds and corrective actions.
[0061] by Define the ratio coefficient Then, the ratio coefficient is fitted using a power function. With residual surface density The relationship is such that it avoids underfitting in the high residual region or overfitting in the low residual region of linear fitting, cancels out the common disturbances in the two readings, and forms a single transferable criterion, wherein:
[0062] Where: ratio coefficient Dimensionless, non-negative; external correction strength Internal correction strength These are derived from the two formulas mentioned above, respectively.
[0063] Ratio coefficient It exhibits a monotonically increasing trend across various operating conditions, providing clear coordinates for threshold segmentation. Furthermore, the ratio coefficient... Dimensionless readings converted to residual surface density For direct use of the three-color threshold, where:
[0064] Among them: residual areal density The unit is micrograms per square decimeter, and it is non-negative; power mapping coefficient. 1 to 100, used for dimensional matching; power exponent 0.5 to 2, control the growth curvature; offset , 0 to 10, corresponding to the background offset.
[0065] When used, the residual surface density is obtained through power mapping. and ratio coefficient The corresponding values remain monotonic and segmentable across the entire domain, making it easy to map the green-yellow-red thresholds onto the same curve. Subsequent readings only require the ratio coefficients. This can trigger either release or correction.
[0066] Step 3: Translate the criteria into production line actions and accumulate evidence: The part obtains the ratio coefficient through the black box position, and automatically generates and executes spray volume, air cutting and mold temperature commands according to the red, yellow and green thresholds; the witness sheet is removed with warm water in the later stage and the background of the outer channel is confirmed; the cavity-level demolding event is written into the event and product information sharing version 2.0, and bound to the finished product digital link two-dimensional barcode to realize part-level closed loop and batch traceability.
[0067] Directly compare the coefficients using a fixed threshold. It is determined that slight fluctuations in temperature difference and rhythm between shifts may cause false yellow or red signals, thus inducing unnecessary line stoppages; therefore, without changing the three-color threshold range, it is necessary to introduce a gentle absorption of the current thermal history and the previous state to give the target reference a buffering capacity.
[0068] Based on the internal correction strength produced in the previous step, External correction strength and ratio coefficient On the item-level page, the validity of the numerator and denominator is first displayed, and then the target ratio coefficient is generated by combining the ratio coefficient of the previous item with the current temperature deviation, which serves as a reference for correction. The three-color threshold is still organized with fixed breakpoints of green ≤ yellow ≤ red. The dynamic target is only used to mitigate minor disturbances and does not change the judgment boundary.
[0069] in:
[0070] Where: temperature difference weight Positive value; sign function ,return , or .
[0071] Target ratio coefficient This is a dimensionless reference for correcting this issue; the ratio coefficient of the previous issue. From the previous one Dimensionless; current ratio coefficient For this document The result is dimensionless; equilibrium coefficient A value between 0 and 1, used to weigh the previous item against the current item; temperature. Compared with reference temperature Definitions as before; temperature scale , is a parameter used for dimensional conversion of temperature difference, and is a positive value; temperature difference weight. , where is the weight of the temperature term, and is a positive value.
[0072] Therefore, by using an exponentially weighted approach to retain the previous information and using logarithmic terms to mitigate the temperature difference, we avoid excessive linear amplification. Item-level pages are displayed... , , At the same time, the target ratio coefficient is given. When the ratio coefficient Slightly crosses the boundary but the target ratio coefficient While still within the green zone, only limited correction instructions are generated to reduce unnecessary line stoppages, while not diluting the authority of the mandatory line stoppage in the red zone.
[0073] The component-level page presents the internal correction strength, external correction strength ratio coefficient, and target ratio coefficient in four blocks, with green / yellow / red bars marking the current interval. Operators only need to confirm that the correction command in the lower right corner of the page has been issued and the status light is green before the component can proceed to the subsequent warm water delamination stage; if the status light is gray, manual review is triggered. The use of bars and status lights transforms abstract parameters into an intuitive interface, reducing operational complexity; the unified page layout also facilitates cross-line support and audit evidence collection.
[0074] Adjusting the amount of external spray is the main lever for controlling the residue, but directly increasing or decreasing it according to the error ratio will cause the spray volume to fluctuate repeatedly at the green edge; it is necessary to use a smooth nonlinear function to map the error into an adjustment amount with a limited amplitude and cut it off within the physical boundary.
[0075] Furthermore, using the ratio coefficient Relative target ratio coefficient The deviation is used as input, and a hyperbolic tangent smoothing dead zone is used to generate spray volume increase / decrease commands. These commands are then superimposed with the spray volume boundary truncation operator to obtain the spray volume setting value for the next cycle. When the page is still in the green zone, the adjustment range is automatically suppressed, where:
[0076] Among them: injection volume correction amount The unit is the increase or decrease in mass per module, which can be positive or negative; gain , representing the maximum permissible adjustment range, a positive value; slope parameter. , controls the steepness of the response, positive value; other symbols are as above.
[0077] Therefore, by mapping the ratio deviation to a finite adjustment through a smooth nonlinear mapping, small fluctuations can be avoided from causing large movements.
[0078] Furthermore, when the ratio coefficient When it falls in the green zone and is close to the boundary, Still a small value; when approaching the red zone, Approaching the upper limit of the gain but not exceeding the physical ability, where:
[0079] Wherein: next cycle injection volume The unit is the mass per cycle; current spray volume. Same unit; lower boundary With upper boundary This refers to the physical allowable range given for the equipment and formulation; Truncation operator Defined as restricting the input to a closed interval. Operators within, .
[0080] To eliminate potential discrepancies in the definition of light intensity, a unified region integral operator is used to calculate the intensity of both internal and external channels. Specifically, for channel images... With Witness Area Background ring area ,definition:
[0081] And it stipulates:
[0082] Symbol: Pixel Intensity Camera grayscale; set size Number of pixels; region Determined by the template specified in the installation specifications. Its outer ring.
[0083] This ensures that the spray volume does not exceed the limit after correction, protecting the equipment and formula boundaries. The spray volume adjustment window on the page provides this information. The numerical values and boundary indicators are displayed; if the boundary is reached, the indicator turns yellow and is automatically checked in the correction action table to transfer to air shearing and mold temperature sharing.
[0084] Furthermore, the next cycle spray volume When the boundary is reached or multiple adjustments within a short period of time are ineffective, a single injection volume is insufficient to adjust the ratio coefficient. To bring back the green zone, we need to introduce air shear and mold temperature as secondary and tertiary levers, and maintain a stable rhythm by separating them from the witness sheet sequence, so as to avoid introducing new uncertainties due to workstation congestion.
[0085] Based on the ratio coefficient The current range and the next cycle injection volume The relative boundary position adopts a three-stage distribution of spray volume as the main factor, air cutting as the secondary factor, and mold temperature as the backup factor. Correspondingly, after the witness film is separated and the image is captured, it immediately enters the warm water mist in a predetermined sequence to ensure that the outer channel can return to the background after separation for sampling and confirmation.
[0086] When the ratio coefficient Located in the yellow zone and next cycle spray volume The boundary was not reached; only the spray volume command was issued. When the ratio coefficient Located in the yellow zone and next cycle spray volume Upon reaching the boundary, a command to extend the wind shear time is issued simultaneously, and the wind shear sharing is triggered by selecting the spray volume boundary on the page; When the ratio coefficient Upon entering the red zone, regardless of the spray volume in the next cycle... Regardless of the location, the system immediately issues a pause and release command, and writes the suggestion to increase the mold temperature or extend the cooling time into the correction action table, which is then reviewed and executed by the process engineer.
[0087] When in use, the three-stage distribution avoids single-lever overload and allows the corrective responsibilities to be carried out in an orderly manner across different workstations; at the same time, it keeps the time and position of the witness film detachment unchanged, ensuring smooth sampling and baseline confirmation.
[0088] For parts that have entered the warm water mist, a baseline inspection is performed in the black box position. The page should display a prompt bar indicating that the external channel is returning to the baseline. If the components do not return to the baseline, it is judged as an abnormality in the process. The system will automatically generate a yellow prompt to pause packing and investigate the cause. The process engineer will handle it according to the checklist for abnormality in the process, including water temperature verification, spray nozzle blockage inspection and witness film batch signature verification.
[0089] When in use, the risk of external channels is eliminated by following a fixed sequence of detachment, baseline confirmation, and packing, and a prompt bar is used as a visible final state to facilitate quality inspection and verification.
[0090] If only screenshots of the page are retained at the workshop level, it is difficult to provide irrefutable evidence in audits that cross factories or organizations; it is necessary to structure and record cavity-level demolding events in the database and generate signature summaries, which are then bound to supply chain identifiers to form a traceable chain of evidence.
[0091] Furthermore, the mold number, cavity number, , , , Threshold determination Fields such as air shear and mold temperature commands, witness sheet number, witness sheet detachment confirmation result, and compliance document number are packaged into a cavity-level demolding event. After calculating the signature digest, it is written into the event and product information sharing version 2.0, and the event identifier is bound to the batch field in the digitally linked 2D barcode during factory packaging. Among them:
[0092] Among them: signature digest , for fixed-length digests; one-way hash operator , is a one-way hash function, a one-way hash operator. For the standard implementation of the 256-family secure hash, its mapping is as follows ; symbol This is the join operator; the meanings of the remaining fields are as above, all representing the actual values of this item, join operator. This means byte concatenation connected by a fixed delimiter; it uses the Unified Character Encoding (UTF-8) and the delimiter is a vertical bar character (byte value). ).
[0093] This concretizes key fields into an irreversible summary, facilitating subsequent verification and tamper prevention. When clients or auditors scan the batch's QR code, they can compare the signature summary on the authorized page. To verify the authenticity and completeness of the cavity-level demolding event, we need to check whether the results are consistent with the on-site recalculation.
[0094] Before an event is written, the system verifies the integrity of the fields. After writing, a green bar indicating the event has been published appears on the page, and an event summary page is generated and archived along with the batch release data. If the writing fails, the system rolls back to the pending publication state and retains the unpublished cache, allowing process engineers to handle each item according to the event publication troubleshooting checklist. Furthermore, the data entry and signing process is visible and traceable, ensuring an uninterrupted chain of evidence from the workshop to the supply chain.
[0095] Step 4: Achieve multi-line replication and compliance closed loop: In batch production, the red, yellow, and green thresholds are re-converged using quantile references and managed in a versioned manner to ensure consistency across molds and production lines; third-party food contact and compostable documents are archived in a folder along with cavity-level demolding event tickets; a replication consistency scoring and economic reconciliation mechanism is set up to support release, review, and replication to operate under the same data baseline.
[0096] If the part-level judgment, sample inspection, regulatory report, and release record are not aligned, subsequent audits and recalls will not be able to quickly locate the release basis for a certain batch and a certain cavity, and the compliance report may deviate from the on-site threshold.
[0097] A fixed ticket-fold structure is established for each sampling batch in the order of sample-record-report-binding. The ticket-fold contains a three-color threshold curve page, an upper limit closed loop curve page, a sample list, witness sheet batch signature, swab sample pretreatment record, laboratory method file number, overall migration and specific migration report, compostable disintegration and biodegradation phase report and cavity-level demolding event summary page. A digital link two-dimensional barcode is printed on the ticket-fold cover so that any record can be retrieved with the same identifier.
[0098] Quality inspectors randomly select samples by part number from the black box, and seal them together with the witness film batch signature and the wiping solution bottle in the same bag. The bag is printed with a list of the batch number and cavity number for the shift. When the samples are handed over to the third-party laboratory, both parties sign the sample handover form for filing. After the laboratory sends back the report, the compliance administrator enters the report number into the ticket folder index page and binds and verifies it with the digital link of the same batch to the two-dimensional barcode.
[0099] When in use, all evidence related to the batch can be recalled through the same two-dimensional barcode, and any update to the project information will leave a trace, forming a verifiable path from item to evidence.
[0100] Once the third-party laboratory has completed the overall migration, specific migration, and compostable phase tests, the compliance administrator marks the regulatory anchor point as verified on the three-color threshold curve page and writes the signature summary and laboratory report number from the event summary page into the ticket index page.
[0101] When in use, the regulatory anchor point and the on-site threshold curve are displayed together in the ticket holder. Any subsequent regulatory review can be directly linked to the part-level judgment and cavity event of the shift, avoiding the risk of laboratory compliance but inconsistent on-site judgment.
[0102] The initial three-color thresholds are derived from the calibration array. During online production, there are shift temperature differences and new mold curvature differences. If re-convergence and generalization are not performed, it will cause the thresholds of different production lines to shift.
[0103] Furthermore, based on the ratio coefficient sequence collected during the shift, a reference ratio is extracted using the quantile operator, and this is used as a fulcrum to fine-tune the position of the green-yellow-red breakpoint. The quantile method only relies on sorting and does not introduce variance statistics, thus avoiding the influence of extreme values.
[0104] Wherein: reference ratio , serving as the central reference for reconvergence; quantile operator , defined as sorting the input sequence in ascending order and then taking the i-th... A function of elements; sample sequence , is the ratio coefficient collected during the shift; quantile level We take 0.5 or 0.65 as the robust center; sample size , which is the number of items handled during the shift, and is a positive integer.
[0105] Therefore, a stable median or upper quantile is extracted as the center of the field to avoid the influence of the long tail. A reference ratio is used. Centered on the new line, the three-color breakpoints are converged to the new line with a fixed offset to ensure consistent judgment criteria across molds; the converged breakpoints are generated on the three-color threshold curve page and labeled with the version number.
[0106] Furthermore, the reference ratio will be used. The report number is displayed alongside the regulatory report number in the ticket holder. A line graph is set on the online closed-loop curve page to compare the time, ratio coefficient time, and spray volume, checking for any jumps in the judgment before and after the breakpoint adjustment. If a jump occurs, the process engineer restores the previous breakpoint according to the breakpoint rollback list and records the reason. This achieves on-site adaptation without changing the regulatory anchor point, ensuring cross-line consistency while retaining the rollback path and avoiding blindly changing thresholds on-site.
[0107] Evaluating benefits based solely on verbal experience is insufficient to support project expansion. It is necessary to quantify output, gross profit, cycle time revenue, and consumable depreciation in the same function to generate an auditable economic reconciliation page.
[0108] The annual net profit is calculated by using the defect improvement function corresponding to output, unit gross profit, and the green zone as positive terms, the cycle time benefit brought by machine time value as the gain term, and the spray volume cost, witness film cost, depreciation and maintenance cost as deduction terms. The defect improvement function adopts a logarithmic form, decreasing marginally as the green breakpoint increases, which is consistent with engineering experience. Furthermore, by summarizing quality, cycle time, and cost into a single indicator, project initiation decisions can be made more conveniently, even in the absence of dimensions, where:
[0109] Of which: annual net income Money supply; output Annual output (number of pieces), positive; unit gross profit. The gross profit per item is positive. Defect Improvement Sensitivity The green breakpoints are mapped to coefficients representing the magnitude of improvement; positive values are obtained through regression analysis of the historical defect improvement-green breakpoint correspondence. , is the ratio coefficient of the upper green bound in the three-color threshold curve page, dimensionless; time value. The monetary value of machine time per hour is positive; the time saved by the beat rate is converted into time. The total duration accumulated from the online closed-loop curve is positive; injection volume cost Cost of witness film ,depreciation ,maintain This is an annual fee, not a negative one.
[0110] Therefore, the finance specialist uses this function to generate an economic reconciliation page, and the process meeting can adjust the green breakpoint. Or the value of the opportunity The sensitivity curves discuss the profit potential of different strategies; the page displays the net profit curve and parameter sensitivity entries, which can be archived directly.
[0111] Read the beat rate from the online closed-loop curve page to save time conversion. Read the spray volume cost from the material requisition form Cost of witness film Read depreciation from equipment ledger Read maintenance records After verification, the data is approved by both the finance specialist and the process engineer. When using the system, all inputs on the ledger page are supported by the source page, the process is verifiable, and the conclusions are reusable.
[0112] If a consistency metric is not set during multi-line replication, the threshold and judgment for the new line may deviate from the baseline, affecting brand image and auditing. A consistency score is defined based on a weighted sum of quantile differences. Three representative quantile levels are selected, and the quantiles obtained by the new line and the baseline under the same measurement conditions are compared one by one. The weights are determined by the process meeting; the lower the score, the higher the consistency. Replication is not allowed when the score exceeds the threshold.
[0113] Among them: consistency score Non-negative; weight ,satisfy And each term is non-negative; quantile level set The values are typically chosen as 0.2, 0.5, or 0.8. , The new line and the baseline were respectively subjected to the same imaging and sampling conditions. quantiles.
[0114] When used, robust quantile differences characterize cross-line differences, without relying on variance-based statistics. When consistency scoring... When the score is below the preset threshold, it is deemed open for replication, and the three-color threshold curve page and the online closed-loop curve page can be directly distributed to the new line for use; when the consistency score is... If the threshold is exceeded, the system generates a prompt that copying is rejected and recalibration is required, along with the time periods of the three workstations with the largest deviations, to facilitate on-site verification.
[0115] Before enabling replication, the compliance administrator adds a replication consistency page to the ticket folder index page and records the consistency score. Weight With quantile level set The signature digest is then linked to a digitally linked two-dimensional barcode for the new batch of products, creating a verifiable copy credential. In use, the scope of authorization no longer relies on verbal consent, but rather on quantitative scoring and verifiable credentials, ensuring that risks are controllable.
[0116] Those skilled in the art will recognize that the units and algorithm steps of the various examples described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are implemented in hardware or software depends on the specific application and design constraints of the technical solution. Those skilled in the art can use different methods to implement the described functions for each specific application, but such implementation should not be considered beyond the scope of this application.
[0117] Those skilled in the art will understand that, for the sake of convenience and brevity, the specific working processes of the systems, devices, and units described above can be referred to the corresponding processes in the foregoing method embodiments, and will not be repeated here.
[0118] In the several embodiments provided in this application, it should be understood that the disclosed systems, apparatuses, and methods can be implemented in other ways. For example, the apparatus embodiments described above are merely illustrative; for instance, the division of units is only a logical functional division, and in actual implementation, there may be other division methods. For example, multiple units or components may be combined or integrated into another system, or some features may be ignored or not executed. Furthermore, the coupling or direct coupling or communication connection shown or discussed may be through some interfaces; the indirect coupling or communication connection between apparatuses or units may be electrical, mechanical, or other forms.
[0119] The units described as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the units can be selected to achieve the purpose of this embodiment according to actual needs.
[0120] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.
Claims
1. A method for quality release and mold release residue traceability management of biodegradable plastics, characterized in that: Comprising, Under the base and internal demolding / lubricating combination, the fluorescent whitening agent OBI type is incorporated into the base as an internal channel tracer, the polyvinyl alcohol witness sheet is attached to the edge of the cavity, and the riboflavin micro dot array is pre-set; Set up double-channel ultraviolet light station, form internal channel and external channel; Collect the intensity of the internal channel and the external channel, calculate the ratio coefficient and establish the mapping relationship with the residual area density; According to the mapping, set three-color threshold and corresponding correction rules of reducing spray, delaying air cutting and adjusting mold temperature; The product obtains the ratio coefficient at the black box detection site, generates the spray amount, air cutting and mold temperature correction instructions according to the three-color threshold; Generate cavity level demolding events and write into event and product information sharing version 2.0 and bind digital link two-dimensional bar code; In batch production, the three-color threshold is re-converged with sub-quantile reference and updated breakpoints are formed; The third-party compliance file and the cavity level demolding event are centralized and uniformly archived and bound as the basis for release and replication.
2. The degradable plastic quality release and demolding residue traceability management method of claim 1, wherein: The base is selected from polylactic acid, polylactic acid and butanediol-hexanedioic acid / terephthalic acid copolyester, and polybutylene succinate; The internal demolding / lubricating combination is composed of rice bran wax and glycerol monostearate, which are homogeneously fed with the same material as the base, and the fluorescent whitening agent OBI type is incorporated with the master batch.
3. The degradable plastic quality release and demolding residue traceability management method of claim 2, wherein: The polyvinyl alcohol witness sheet is attached to the non-food contact edge or the predetermined cutting area of the cavity, and the surface is pre-set with a riboflavin micro dot array; After the product is taken, it is collected at the black box detection site along the designated path, and then the witness sheet is completely separated by warm water mist or short-range spraying in the later stage.
4. The degradable plastic quality release and demolding residue traceability management method of claim 3, wherein: After temperature, image taking delay and incident angle compensation, the ratio coefficient is calculated, and the ratio coefficient and the residual area density are monotonically mapped to form three-color thresholds divided by breakpoints.
5. The degradable plastic quality release and demolding residue traceability management method of claim 4, wherein: The correction rules are assigned according to priority: when the ratio coefficient is in the yellow zone and the spray amount does not reach the boundary, only adjust the spray amount; When the boundary is reached, the air cutting is simultaneously extended; When entering the red zone, the release is suspended and the mold temperature or cooling time is adjusted.
6. The degradable plastic quality release and demolding residue traceability management method of claim 1, wherein: The cavity level demolding event includes mold number, cavity number, internal correction intensity, external correction intensity, ratio coefficient, threshold judgment, spray amount setting, air cutting and mold temperature instruction, witness sheet number, formula batch and compliance file number, and is written into event and product information sharing version 2.0 and bound with digital link two-dimensional bar code.
7. The degradable plastic quality release and demolding residue traceability management method of claim 1, wherein: The sub-quantile reference of the on-duty ratio coefficient sequence is used as the field center to re-converge the three-color threshold to generate updated breakpoints, and the version and source working condition are recorded on the online closed loop curve page, and the rollback path is saved for cross-line review and replication; Third party compliance files include at least the overall migration and specific migration reports conducted under the plastic food contact regulations, as well as the disintegration and biodegradation phase reports, and are bound to the cavity level demolding events in the ticket folder.
8. The degradable plastic mass release and demolding residue traceability management method of claim 7, wherein: The economic reconciliation takes yield, unit gross profit, machine time value, and tact time saving length as the benefit items, and deducts the spray cost, witness piece cost, depreciation and maintenance cost; the copy consistency takes the quantile point difference and weight to calculate the score, and opens the copy after reaching the preset threshold.