Semiconductor device and forming method thereof

By employing alternating nanostructures and pseudo-nanostructures in multilayer stacks of semiconductor devices, combined with ALD and molecular inhibitor technologies, the problem of device density and performance consistency in vertically stacked transistors was solved, achieving precise gate electrode formation and improved device yield.

CN121487332APending Publication Date: 2026-02-06TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202511466218.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-02-05
Filing Date
2025-10-14
Publication Date
2026-02-06

AI Technical Summary

Technical Problem

As the minimum component size of semiconductor devices decreases, existing technologies struggle to effectively address the issues of device density and performance consistency. In particular, when forming vertically stacked transistors, the loading effect caused by the etch-back process affects the uniformity and consistency of device dimensions.

Method used

Alternating semiconductor nanostructures and pseudo-nanostructures are used to form multilayer stacks. Atomic layer deposition (ALD) is used to form gate dielectric and metal layers around the nanostructures, avoiding the etch-back process. Molecular inhibitors are used to control the deposition of the metal layers, forming vertically stacked lower and upper gate electrodes.

Benefits of technology

It achieves precise dimensional control of the lower and upper gate electrodes, avoids the load effect caused by the etch-back process, improves device performance and yield, and enhances device density and consistency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121487332A_ABST
    Figure CN121487332A_ABST
Patent Text Reader

Abstract

In an embodiment, a method includes forming a multilayer stack over a semiconductor substrate, the multilayer stack including alternating semiconductor nanostructures and dummy nanostructures; forming lower source / drain regions, wherein a lower semiconductor nanostructure of the semiconductor nanostructures extends between the lower source / drain regions; forming an upper source / drain region over the lower source / drain region; removing the dummy nanostructures to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; forming a first metal-containing layer around the upper semiconductor nanostructure and in the second opening; exposing a surface of the first metal-containing layer to a first molecular inhibitor to form a first passivation layer on the surface of the first metal-containing layer; and forming a lower gate electrode around the lower semiconductor nanostructure and in the first opening. The embodiment of the invention also relates to a semiconductor device and a forming method thereof.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of this disclosure relate to semiconductor devices and methods of forming the same. Background Technology

[0002] Semiconductor devices are used in a variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by sequentially depositing insulating or dielectric layers, conductive layers, and semiconductor layers on a semiconductor substrate, and by using photolithography to pattern the individual material layers to form circuit components and elements on the material layers.

[0003] The semiconductor industry continuously improves the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.) by constantly reducing the size of the smallest component, which allows more components to be integrated into a given area. However, as the size of the smallest component decreases, additional problems arise that need to be addressed. Summary of the Invention

[0004] One embodiment of this disclosure provides a method for forming a semiconductor device, comprising: forming a multilayer stack above a semiconductor substrate, the multilayer stack including alternating semiconductor nanostructures and pseudo-nanostructures; forming a lower source / drain region, wherein a lower semiconductor nanostructure of the semiconductor nanostructure extends between the lower source / drain regions; forming an upper source / drain region above the lower source / drain region, wherein an upper semiconductor nanostructure of the semiconductor nanostructure extends between the upper source / drain regions; removing the pseudo-nanostructure to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; forming a gate dielectric layer around the lower and upper semiconductor nanostructures; forming a first metal-containing layer around the upper semiconductor nanostructure and in the second opening; exposing the surface of the first metal-containing layer to a first molecular inhibitor to form a first passivation layer on the surface of the first metal-containing layer; and forming a lower gate electrode around the lower semiconductor nanostructure and in the first opening.

[0005] Another aspect of the embodiments of this disclosure provides a method for forming a semiconductor device, comprising: forming a multilayer stack over a semiconductor substrate, the multilayer stack including alternating semiconductor layers and dummy layers; patterning the multilayer stack to form fins, wherein the fins include alternating semiconductor nanostructures and dummy nanostructures, the semiconductor nanostructures being defined by the semiconductor layers and the dummy nanostructures being defined by the dummy layers; forming a lower source / drain region, wherein a lower semiconductor nanostructure of the semiconductor nanostructure extends between the lower source / drain regions; forming an upper source / drain region over the lower source / drain region, wherein an upper semiconductor nanostructure of the semiconductor nanostructure extends between the upper source / drain regions; removing the dummy nanostructures to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; forming a first metal-containing layer around the upper semiconductor nanostructures and in the second opening; forming a first passivation layer on the surface of the first metal-containing layer; and forming a lower gate stack around the lower semiconductor nanostructures and in the first opening.

[0006] In another aspect, embodiments of this disclosure provide a semiconductor device comprising: a plurality of first nanostructures extending between first source / drain regions; a plurality of second nanostructures located above the plurality of first nanostructures, the plurality of second nanostructures extending between second source / drain regions; an isolation structure located between the plurality of first nanostructures and the plurality of second nanostructures; a first gate stack located around the plurality of first nanostructures; and a second gate stack located above the first gate stack and disposed around the plurality of second nanostructures, wherein the second gate stack comprises: a first metal-containing layer located around the second nanostructures of the plurality of second nanostructures; a second metal-containing layer located above the first metal-containing layer and around the second nanostructures of the plurality of second nanostructures; and a first gate electrode layer located above the first metal-containing layer and the second metal-containing layer, wherein the sidewalls of the first metal-containing layer and the second metal-containing layer are adjacent to the sidewalls of the isolation structure. Attached Figure Description

[0007] When read in conjunction with the accompanying drawings, aspects of this disclosure are best understood from the following detailed description. It should be noted that, in accordance with standard industry practice, the various components are not drawn to scale. In fact, for clarity of discussion, the dimensions of the individual components may be arbitrarily increased or decreased.

[0008] Figure 1 An example schematic diagram of a stacked transistor (such as a complementary field-effect transistor (CFET)) according to some embodiments is shown in a three-dimensional view.

[0009] Figures 2 to 24B This is a view of an intermediate stage in the fabrication of a CFET according to some embodiments. Detailed Implementation

[0010] The following disclosure provides numerous different embodiments or examples for implementing various features of this disclosure. Specific examples of components and arrangements are described below to simplify this disclosure. Of course, these are merely examples and not intended to be limiting. For example, in the following description, forming a first component above or on a second component can include embodiments where the first and second components are in direct contact, and can also include embodiments where an additional component can be formed between the first and second components, such that the first and second components are not in direct contact. Furthermore, reference numerals and / or letters may be repeated in various examples. This repetition is for simplicity and clarity and does not in itself indicate a relationship between the various embodiments and / or configurations discussed.

[0011] Additionally, for ease of description, spatial relative terms such as “below,” “under,” “lower,” “above,” and “upper” may be used herein to describe the relationship between one element or component and another, as shown in the figures. Besides the orientations shown in the figures, spatial relative terms are intended to include different orientations of the device during use or operation. The device may be positioned in other ways (rotated 90 degrees or in other orientations), and the spatial relative descriptors used herein can be interpreted accordingly.

[0012] According to various embodiments, a semiconductor device including a CFET can be formed. The CFET includes a lower nanostructure FET and an upper nanostructure FET disposed above the lower nanostructure FET. Forming the semiconductor device may include forming an upper channel region of the upper nanostructure FET and a lower channel region of the lower nanostructure FET, the upper and lower channel regions being disposed above the fin. A gate dielectric layer is formed around the upper and lower channel regions and above the fin. A first metallized material layer may be formed around the upper channel region, such that the gate dielectric layer is disposed between the first metallized material layer and the upper channel region. The semiconductor device may be exposed to a first molecular inhibitor (e.g., aniline or aldehyde), such that the first molecular inhibitor selectively adheres to the surface of the first metallized material layer surrounding the upper channel region. A lower gate electrode is then formed above the gate dielectric layer and around the lower channel region using a conformal deposition process such as atomic layer deposition (ALD), wherein during the deposition process, the first molecular inhibitor acts as a protective layer to prevent material of the lower gate electrode from forming on the surface of the first metallized material layer. After the lower gate electrode is formed, the first molecular inhibitor and the first metal-containing material layer are removed using a suitable process. The semiconductor device can then be exposed to a second molecular inhibitor (e.g., aniline or aldehyde), allowing the second molecular inhibitor to selectively adhere to the top surface of the lower gate electrode. A second and third metal-containing material layer can be sequentially formed around the upper channel region, such that the gate dielectric layer is disposed between the second and third metal-containing material layers and the upper channel region. During the formation of the second and third metal-containing material layers, the second molecular inhibitor acts as a protective layer to prevent the second and third metal-containing material layers from forming on the top surface of the lower gate electrode. After the formation of the second and third metal-containing material layers, the second molecular inhibitor can be removed using a suitable process. Then, an upper gate electrode is formed above the lower gate electrode and around the gate dielectric layer, the second metal-containing material layer, the third metal-containing material layer, and the upper channel region using a conformal deposition process such as ALD.

[0013] Advantageous features of one or more embodiments disclosed herein allow for the formation of a lower gate electrode around a lower channel region and an upper gate electrode around an upper channel region, wherein the upper gate electrode is disposed above the lower gate electrode, without having to perform an etch-back process to remove the top portion of the lower gate electrode. As a result, the loading effects associated with the etch-back process, which could lead to variations in the component size of the lower gate electrode, can be avoided, resulting in improved uniformity and consistency of the dimensions of the lower and upper gate electrodes. This can lead to enhanced device performance and improved device yield. Furthermore, using atomic layer deposition (ALD) to form the lower and upper gate electrodes allows for the conformal deposition of the materials for the lower and upper gate electrodes, respectively, around the lower and upper channel regions of the nanostructured FET. As a result, precise dimensional control of the lower and upper gate electrodes can be achieved, which can allow for consistent device performance.

[0014] Figure 1 An example schematic diagram of a stacked transistor (such as a complementary field-effect transistor (CFET)) according to some embodiments is shown. Figure 1 This is a 3D view, in which some components of the CFET are omitted for clarity.

[0015] CFETs comprise multiple vertically stacked nanostructure FETs (e.g., nanowire FETs, nanosheet FETs, multi-bridge channel (MBC) FETs, nanoribbon FETs, gate-all-around (GAA) FETs, etc.). For example, a CFET may comprise a lower nanostructure FET of a first device type (e.g., n-type / p-type) and an upper nanostructure FET of a second device type opposite to the first device type (e.g., p-type / n-type). Specifically, a CFET may comprise a lower PMOS transistor and an upper NMOS transistor, or a CFET may comprise a lower NMOS transistor and an upper PMOS transistor. Each nanostructure FET comprises a semiconductor nanostructure 66 (including a lower semiconductor nanostructure 66L and an upper semiconductor nanostructure 66U), wherein the semiconductor nanostructure 66 serves as a channel region for the nanostructure FET. The semiconductor nanostructure 66 may be a nanosheet, nanowire, etc. The lower semiconductor nanostructure 66L is used for the lower nanostructure FET, and the upper semiconductor nanostructure 66U is used for the upper nanostructure FET. Channel isolation material ( Figure 1 It is not explicitly stated in the text, see Figure 22 It can be used to separate and electrically isolate the upper semiconductor nanostructure 66U from the lower semiconductor nanostructure 66L.

[0016] Gate dielectric 132 extends along the top, sidewalls, and bottom of semiconductor nanostructure 66. Gate electrode 134 (including lower gate electrode 134L and upper gate electrode 134U) is located above gate dielectric 132 and around semiconductor nanostructure 66. Source / drain regions 108 (including lower epitaxial source / drain region 108L and upper epitaxial source / drain region 108U) are located on opposite sides of gate dielectric 132 and gate electrode 134. Depending on the context, source / drain regions 108 may individually or collectively refer to a source or drain. Isolation components may be formed to separate desired source / drain regions 108 and / or desired gate electrode 134. For example, lower gate electrode 134L may optionally be separated from upper gate electrode 134U. Alternatively, lower gate electrode 134L may be coupled to upper gate electrode 134U. Additionally, the upper epitaxial source / drain region 108U can be connected through one or more dielectric layers ( Figure 1 It is not explicitly stated in the text, see Figure 22 This is separated from the lower epitaxial source / drain region 108L. The isolation components between the channel region, gate, and source / drain regions allow for vertical stacking of transistors, thereby improving device density. Due to the vertical stacking characteristics of CFETs, this schematic diagram can also be referred to as a stacked transistor or a folded transistor.

[0017] Figure 1 Reference cross sections used in subsequent figures are also shown. Cross section A-A' is parallel to the longitudinal axis of the semiconductor nanostructure 66 of the CFET and in the direction of current flow, for example, between the source / drain regions 108 of the CFET. Cross section B-B' is perpendicular to cross section A-A' and along the longitudinal axis of the gate electrode 134 of the CFET. These reference cross sections are referenced in subsequent figures for clarity.

[0018] Figures 2 to 24B This is a view of an intermediate stage in the fabrication of a CFET according to some embodiments. Figure 2 , Figure 3A and Figure 4 It is a 3D view, showing the relationship with Figure 1 A similar 3D view. Figure 5 , Figure 6 , Figure 7 , Figure 8 , Figure 9 , Figure 10A , Figure 11A , Figure 22 , Figure 23 and Figure 24A It shows along with Figure 1 A cross-sectional view of a cross section similar to the reference cross section A-A' in the diagram. Figure 3B , Figure 10B , Figure 11B , Figure 12 , Figure 13 , Figure 14 , Figure 15 , Figure 16 , Figure 17 , Figure 18 , Figure 19 , Figure 20 , Figure 21 and Figure 24B It shows along with Figure 1 A cross-sectional view of a cross section similar to the reference cross section B-B' in the diagram.

[0019] exist Figure 2 In this embodiment, a substrate 50 is provided. Substrate 50 can be a semiconductor substrate, such as a bulk semiconductor, a semiconductor-on-insulator (SOI) substrate, etc., and can be doped (e.g., with p-type or n-type dopants) or undoped. Substrate 50 can be a wafer, such as a silicon wafer. Typically, an SOI substrate is a layer of semiconductor material formed on an insulating layer. The insulating layer can be, for example, a buried oxide (BOX) layer, a silicon oxide layer, etc. The insulating layer is provided on a substrate (typically a silicon or glass substrate). Other substrates, such as multilayer or gradient substrates, can also be used. In some embodiments, the semiconductor material of substrate 50 can include silicon; germanium; compound semiconductors, including carbon-doped silicon, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including silicon germanium, gallium arsenide phosphide, aluminum indium arsenide, aluminum gallium arsenide, gallium indium arsenide, gallium indium phosphide, and / or gallium arsenide phosphide; or combinations thereof.

[0020] A multilayer stack 52 is formed over a substrate 50. The multilayer stack 52 includes alternating dummy layers 54 (including a first dummy layer 54A and a second dummy layer 54B) and semiconductor layers 56 (including a lower semiconductor layer 56L and an upper semiconductor layer 56U). A subset of the lower semiconductor layer 56L and the first dummy layer 54A is disposed below the second dummy layer 54B. Another subset of the upper semiconductor layer 56U and the first dummy layer 54A is disposed above the second dummy layer 54B. As described in more detail later, the dummy layers 54 will be removed, and the semiconductor layers 56 will be patterned to form the channel region of the CFET. Specifically, the lower semiconductor layer 56L will be patterned to form the channel region of the lower nanostructure FET of the CFET, and the upper semiconductor layer 56U will be patterned to form the channel region of the upper nanostructure FET of the CFET.

[0021] The multilayer stack 52 is shown as including a specific number of dummy layers 54 and a specific number of semiconductor layers 56. It should be understood that the multilayer stack 52 may include any number of dummy layers 54 and semiconductor layers 56. Each layer of the multilayer stack 52 may be grown by a process such as vapor phase epitaxy (VPE) or molecular beam epitaxy (MBE), or deposited by a process such as chemical vapor deposition (CVD) or atomic layer deposition (ALD).

[0022] The first dummy layer 54A and the second dummy layer 54B may be formed of a first semiconductor material. The first semiconductor material may be selected from candidate semiconductor materials of the substrate 50. In some embodiments, the dummy layer 54 (e.g., the first dummy layer 54A and the second dummy layer 54B) is formed of or includes silicon germanium, and the second dummy layer 54B may be formed of germanium or silicon germanium with a higher percentage of germanium atoms than the first dummy layer 545A. The first dummy layer 54A and the second dummy layer 54B have high etch selectivity to each other, such that the second dummy layer 54B can be removed at a faster rate than the first dummy layer 545A in subsequent processing. The semiconductor layer 56 (including a lower semiconductor layer 56L and an upper semiconductor layer 56U) is formed of a second semiconductor material different from the first semiconductor material. The second semiconductor material may be selected from candidate semiconductor materials of the substrate 50. In some embodiments, the semiconductor layer 56 is formed of silicon. Semiconductor layer 56 and dummy layer 54 have high etch selectivity to each other, which allows dummy layer 54 (e.g., first dummy layer 54A and second dummy layer 54B) to be removed in subsequent processes at a faster rate than semiconductor layer 56 (e.g., lower semiconductor layer 56L and upper semiconductor layer 56U).

[0023] exist Figure 3A and Figure 3B In this configuration, fins 62 are formed in the substrate 50, and nanostructures 64 and 66 (including a first pseudo-nanostructure 64A, a second pseudo-nanostructure 64B, a lower semiconductor nanostructure 66L, an intermediate semiconductor nanostructure 66M, and an upper semiconductor nanostructure 66U) are formed in the multilayer stack 52. In some embodiments, nanostructures 64, 66, and fins 62 can be formed in the multilayer stack 52 and the substrate 50, respectively, by etching trenches in the multilayer stack 52 and the substrate 50. The etching can be any acceptable etching process, such as reactive ion etching (RIE), neutral beam etching (NBE), or combinations thereof. The etching can be anisotropic. Nanostructures 64 and 66 are formed by etching a multilayer stack 52. A first pseudo-nanostructure 64A is defined from a first pseudo-layer 54A, a second pseudo-nanostructure 64B from a second pseudo-layer 54B, a lower semiconductor nanostructure 66L from some lower semiconductor layers 56L, an upper semiconductor nanostructure 66U from some upper semiconductor layers 56U, and an intermediate semiconductor nanostructure 66M from some lower semiconductor layers 56L and some upper semiconductor layers 56U. The first pseudo-nanostructure 64A and the second pseudo-nanostructure 64B can also be collectively referred to as pseudo-nanostructure 64. The lower semiconductor nanostructure 66L and the upper semiconductor nanostructure 66U can also be collectively referred to as semiconductor nanostructure 66.

[0024] As described in more detail below, one of the various nanostructures 64, 66 will be removed to form the channel region of the CFET. Specifically, the lower semiconductor nanostructure 66L will be used as the channel region of the lower nanostructure FET for the CFET. Furthermore, the upper semiconductor nanostructure 66U will be used as the channel region of the upper nanostructure FET for the CFET.

[0025] The intermediate semiconductor nanostructure 66M is a semiconductor nanostructure 66 located directly above / below (e.g., in contact with) the second pseudo-nanostructure 64B. Depending on the height of the subsequently formed source / drain regions, the intermediate semiconductor nanostructure 66M may or may not be adjacent to any source / drain regions and may or may not be used as a functional channel region for the CFET. Subsequently, the second pseudo-nanostructure 64B will be replaced by an isolation structure. The isolation structure and the intermediate semiconductor nanostructure 66M can define the boundaries between the lower nanostructure FET and the upper nanostructure FET.

[0026] The fins 62 and nanostructures 64, 66 can be patterned using any suitable method. For example, the fins 62 and nanostructures 64, 66 can be patterned using one or more photolithography processes, including dual-patterning or multi-patterning processes. Typically, dual-patterning or multi-patterning processes combine photolithography and self-alignment processes, allowing the creation of patterns with, for example, smaller pitches than that achievable using a single direct photolithography process. For example, in one embodiment, a sacrificial layer is formed over a substrate and patterned using a photolithography process. Spacers are formed alongside the patterned sacrificial layer using a self-alignment process. The sacrificial layer is then removed, and the remaining spacers can then be used to pattern the fins 62 and nanostructures 64, 66. In some embodiments, a mask (or other layer) may be retained on the nanostructures 64, 66.

[0027] Although each of the fins 62 and nanostructures 64, 66 is shown as having a constant width overall, in other embodiments, the fins 62 and / or nanostructures 64, 66 may have tapered sidewalls, such that the width of each of the fins 62 and / or nanostructures 64, 66 increases continuously in the direction toward the substrate 50. In such embodiments, each nanostructure 64, 66 may have a different width and be trapezoidal in shape.

[0028] Additionally, an isolation region 70 is formed above the substrate 50 and between adjacent semiconductor fins 62. The isolation region 70 may include a liner and a filler material located above the liner. Each of the liner and filler material may include a dielectric material, such as an oxide (e.g., silicon oxide), a nitride (e.g., silicon nitride), or a combination thereof. Forming the isolation region 70 may include depositing the dielectric material and performing a planarization process (such as a chemical mechanical polishing (CMP) process, a mechanical polishing process, etc.) to remove excess portions of the dielectric material, such as those located above the nanostructures 64, 66. The deposition process may include ALD, high-density plasma chemical vapor deposition (HDP-CVD), flowable chemical vapor deposition (FCVD), or a combination thereof. In some embodiments, the isolation region 70 comprises silicon oxide formed by an FCVD process and a subsequent annealing process. The dielectric material is then recessed to define the isolation region 70. The dielectric material may be recessed such that the upper portions of the semiconductor fins 62 and nanostructures 64, 66 extend higher than the isolation region 70.

[0029] The previously described process is merely one example of how the fins 62 and nanostructures 64, 66 can be formed. In some embodiments, the fins 62 and / or nanostructures 64, 66 can be formed using masking and epitaxial growth processes. For example, a dielectric layer can be formed over the top surface of the substrate 50, and trenches can be etched through the dielectric layer to expose the underlying substrate 50. Epitaxial structures can be epitaxially grown in the trenches, and the dielectric layer can be recessed such that the epitaxial structure protrudes from the dielectric layer to form the fins 62 and / or nanostructures 64, 66. The epitaxial structure can include the alternating semiconductor materials previously described, such as a first semiconductor material and a second semiconductor material. In some embodiments of epitaxial growth of the epitaxial structure, the material to be epitaxially grown can be doped in situ during growth, which avoids prior and / or subsequent implantation, but in-situ and implantation doping can be used together.

[0030] Additionally, suitable wells (not shown separately) can be formed in the semiconductor nanostructure 66. In other embodiments, suitable wells can be formed in the multilayer stack 52 prior to the formation of the fins 62 and nanostructures 64, 66. For example, n-type impurity implantation and / or p-type impurity implantation can be performed, or the semiconductor material can be doped in situ during growth. The n-type impurity can be at a concentration of 10. 17 atoms / cm 3 Up to 10 19 atoms / cm 3 Phosphorus, arsenic, antimony, etc., within the range. p-type impurities can be in the range of 10... 17 atoms / cm 3 Up to 10 19 atoms / cm 3The range includes boron, boron fluoride, indium, etc. The well in the lower semiconductor nanostructure 66L has a conductivity type opposite to that of the lower source / drain region, which will subsequently be formed adjacent to the lower semiconductor nanostructure 66L. The well in the upper semiconductor nanostructure 66U has a conductivity type opposite to that of the upper source / drain region, which will subsequently be formed adjacent to the upper semiconductor nanostructure 66U.

[0031] exist Figure 4 In this structure, a dummy dielectric layer 72 is formed on fins 62 and / or nanostructures 64, 66. The dummy dielectric layer 72 can be, for example, silicon oxide, silicon nitride, combinations thereof, etc., and can be deposited or thermally grown according to acceptable techniques. A dummy gate layer 74 is formed above the dummy dielectric layer 72, and a mask layer 76 is formed above the dummy gate layer 74. The dummy gate layer 74 can be deposited above the dummy dielectric layer 72 and then planarized, for example, by CMP. The mask layer 76 can be deposited above the dummy gate layer 74. The dummy gate layer 74 can be a conductive or non-conductive material and can be selected from the group consisting of amorphous silicon, polycrystalline silicon (polysilicon), polycrystalline silicon germanium (polycrystalline SiGe), metal nitrides, metal silicides, metal oxides, and metals. The dummy gate layer 74 can be deposited by physical vapor deposition (PVD), CVD, sputtering deposition, or other techniques for depositing the selected material. The dummy gate layer 74 can be formed from other materials that have high etch selectivity to insulating materials. The mask layer 76 may include, for example, silicon nitride, silicon oxynitride, etc. In the illustrated embodiment, the dummy dielectric layer 72 covers the isolation region 70 such that the dummy dielectric layer 72 extends between the dummy gate layer 74 and the isolation region 70. In another embodiment, the dummy dielectric layer 72 covers only the fins 62 and / or the nanostructures 64, 66.

[0032] exist Figure 5 In this process, the mask layer 76 can be patterned using acceptable photolithography and etching techniques to form a mask 86. The pattern of the mask 86 can then be transferred to the dummy gate layer 74 and the dummy dielectric layer 72 to form dummy gates 84 and dummy dielectrics 82, respectively. The dummy gates 84 cover the corresponding channel regions of the nanostructures 64, 66. The pattern of the mask 86 can be used to physically separate each dummy gate 84 from its adjacent counterparts. The dummy gates 84 may also have a longitudinal direction substantially perpendicular to the longitudinal direction of the corresponding fin 62. After patterning, the mask 86 can optionally be removed, such as by any acceptable etching technique.

[0033] exist Figure 6In this configuration, a gate spacer 90 is formed over nanostructures 64 and 66 and on the exposed sidewalls of mask 86 (if present), dummy gate 84, and dummy dielectric 82. The gate spacer 90 can be formed by conformally forming one or more dielectric materials and subsequently etching the dielectric material. Acceptable dielectric materials may include silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride, etc., which can be formed by deposition processes such as chemical vapor deposition (CVD), atomic layer deposition (ALD), etc. Other dielectric materials formed by any acceptable process may be used. Any acceptable etching process (such as dry etching, wet etching, etc., or combinations thereof) can be performed to pattern the dielectric material. The etching may be anisotropic. When etched, the dielectric material has portions remaining on the sidewalls of the dummy gate 84 (thus forming the gate spacer 90). In some embodiments, when etched, the dielectric material may also have portions remaining on the sidewalls of fins 62 and / or nanostructures 64 and 66.

[0034] Additionally, implantation can be performed for lightly doped source / drain (LDD) regions (not shown separately). LDD implantation can be performed before the formation of the gate spacer 90. Appropriate types of impurities can be implanted into the nanostructures 64, 66 to the desired depth. The LDD regions can have the same conductivity type as the source / drain regions, which will subsequently be formed adjacent to the semiconductor nanostructure 66. Furthermore, the LDD regions in the lower semiconductor nanostructure 66L can have a conductivity type opposite to that in the upper semiconductor nanostructure 66U. In some embodiments, the lower semiconductor nanostructure 66L has a p-type LDD region, and the upper semiconductor nanostructure 66U has an n-type LDD region. In some embodiments, the lower semiconductor nanostructure 66L has an n-type LDD region, and the upper semiconductor nanostructure 66U has a p-type LDD region. The n-type impurity can be any n-type impurity discussed previously, and the p-type impurity can be any p-type impurity discussed previously. The lightly doped source / drain regions can have a conductivity type of 10 17 atoms / cm 3 Up to 10 20 atoms / cm 3 The impurity concentration is within a certain range. Annealing can be used to repair implantation damage and reactivate implanted impurities. In some embodiments, the growth material of nanostructures 64, 66 can be in-situ doped during growth, which can avoid implantation, but in-situ doping and implantation doping can be used together.

[0035] It should be noted that previous disclosures typically described the processes for forming spacers and LDD regions. Other processes and sequences can be used. For example, fewer or additional spacers can be used, different step sequences can be employed, additional spacers can be formed and removed, etc.

[0036] Source / drain recesses 94 are formed in fins 62, nanostructures 64, 66, and substrate 50. Epitaxial source / drain regions are subsequently formed in the source / drain recesses 94. The source / drain recesses 94 may extend through nanostructures 64, 66 and into substrate 50. Fins 62 may be etched such that the bottom surface of the source / drain recesses 94 is positioned above, below, or flush with the top surface of isolation region 70. In the illustrated example, the top surface of isolation region 70 is positioned above the bottom surface of the source / drain recesses 94. The source / drain recesses 94 can be formed by etching fins 62, nanostructures 64, 66, and substrate 50 using anisotropic etching processes (such as RIE, NBE, etc.). During the etching process used to form the source / drain recesses 94, gate spacers 90 and dummy gates 84 mask portions of fins 62, nanostructures 64, 66, and substrate 50. Each layer of nanostructures 64, 66 and / or fins 62 can be etched using a single etching process or multiple etching processes. A timed etching process can be used to stop the etching of the source / drain trenches 94 after they have reached the desired depth.

[0037] exist Figure 7 In this process, the sidewalls of the first pseudo-nanostructure 64A, exposed through the source / drain trench 94, are recessed to form a sidewall trench 96A. Furthermore, the second pseudo-nanostructure 64B is removed to form an opening 96B between the lower semiconductor nanostructure 66L (collectively referred to as the lower semiconductor nanostructure 66L) and the upper semiconductor nanostructure 66U (collectively referred to as the upper semiconductor nanostructure 66U). The sidewall trench 96A is then filled with a spacer. The opening 96B is then filled with an isolation structure.

[0038] Sidewall recesses 96A can be formed by recessing the sidewalls of the first pseudo-nanostructure 64A using any acceptable etching process. The etching is selective for the first pseudo-nanostructure 64A (e.g., selectively etching the material of the first pseudo-nanostructure 64A at a faster rate than the material of the semiconductor nanostructure 66). The etching can be isotropic. Although the sidewalls of the first pseudo-nanostructure 64A appear straight after etching, the sidewalls can be concave or convex.

[0039] The opening 96B can be formed by removing the second pseudo-nanostructure 64B using any acceptable etching process. The etching is selective for the second pseudo-nanostructure 64B (e.g., selectively etching the material of the second pseudo-nanostructure 64B at a faster rate than the material of the semiconductor nanostructure 66). The etching can be isotropic. The pseudo-gate 84 can adhere to and support the upper semiconductor nanostructure 66U such that the upper semiconductor nanostructure 66U does not collapse after the opening 96B is formed.

[0040] In some embodiments, the same etching process is used to recess the sidewalls of the first pseudo-nanostructure 64A and remove the second pseudo-nanostructure 64B. For example, the second pseudo-nanostructure 64B can be completely removed without completely removing the first pseudo-nanostructure 64A, and the first pseudo-nanostructure 64A can be recessed without significantly recessing the semiconductor nanostructure 66. The etching process is selective among the materials of the first pseudo-nanostructure 64A, the second pseudo-nanostructure 64B, and the semiconductor nanostructure 66. Specifically, the etching process selectively etches the material of the first pseudo-nanostructure 64A at a faster rate than the material of the semiconductor nanostructure 66, and also selectively etches the material of the second pseudo-nanostructure 64B at a faster rate than the material of the first pseudo-nanostructure 64A. Therefore, the etching rate of the first pseudo-nanostructure 64A is less than the etching rate of the second pseudo-nanostructure 64B, and greater than the etching rate of the semiconductor nanostructure 66. In some embodiments, the second pseudo-nanostructure 64B is formed of germanium or silicon-germanium with a high percentage of germanium atoms, the first pseudo-nanostructure 64A is formed of silicon-germanium with a low percentage of germanium atoms, and the semiconductor nanostructure 66 is formed of germanium-free silicon. The etching process may include a dry etching process using chlorine gas, with or without plasma.

[0041] The intermediate semiconductor nanostructure 66M is exposed by an opening 96B. In some embodiments, an etching process thins the intermediate semiconductor nanostructure 66M. Therefore, the thickness of the intermediate semiconductor nanostructure 66M can be different from (e.g., less than) the thickness of the lower semiconductor nanostructure 66L and the upper semiconductor nanostructure 66U. In some embodiments, after the etching process, the intermediate semiconductor nanostructure 66M is 0% to 20% thinner than the lower semiconductor nanostructure 66L and the upper semiconductor nanostructure 66U.

[0042] exist Figure 8 In this configuration, an internal spacer 98 is formed in the sidewall recess 96A and on the sidewall of the remaining portion of the first pseudo-nanostructure 64A. As described in more detail later, a source / drain region will subsequently be formed in the source / drain recess 94, and the first pseudo-nanostructure 64A will be replaced with a corresponding gate structure. The internal spacer 98 serves as an isolation component between the subsequently formed source / drain region and the subsequently formed gate structure. Additionally, the internal spacer 98 can be used to prevent damage to the subsequently formed source / drain region by subsequent etching processes (such as etching processes used to form the gate structure). Furthermore, an isolation structure 100 is formed in the opening 96B and between the intermediate semiconductor nanostructure 66M. The isolation structure 100 and the intermediate semiconductor nanostructure 66M will define the boundaries between the lower nanostructure FET and the upper nanostructure FET.

[0043] The internal spacer 98 and the isolation structure 100 can be formed by conformally forming an insulating material in the source / drain recess 94, the sidewall recess 96A, and the opening 96B, and then subsequently etching the insulating material. The insulating material can be a carbon-containing dielectric material, such as silicon carbonitride, silicon oxycarbonate, silicon oxynitride, etc. Other low dielectric constant (low-k) materials with a k-value less than about 3.5 can be used. The insulating material can be formed by a deposition process (such as ALD, CVD, etc.). The etching of the insulating material can be anisotropic. For example, the etching process can be dry etching, such as RIE, NBE, etc. When etched, the insulating material has portions retained in the sidewall recess 96A (thus forming the internal spacer 98) and portions retained in the opening 96B (thus forming the isolation structure 100).

[0044] Although the outer walls of the internal spacers 98 and the isolation structure 100 are shown flush with the sidewalls of the semiconductor nanostructure 66, the outer walls of the internal spacers 998 and the isolation structure 110 may extend beyond or be recessed from the sidewalls of the semiconductor nanostructure 66. Therefore, the internal spacers 98 and the isolation structure 100 may partially fill, fully fill, or overfill the sidewall recesses 96A and openings 96B, respectively. Furthermore, although the sidewalls of the internal spacers 98 and the isolation structure 100 are shown as straight, these sidewalls may be concave or convex.

[0045] The isolation structures 100 have similar dimensions to the second pseudo-nanostructure 64B they replace. Therefore, the isolation structures 100 can have a large thickness, such as a greater thickness than the semiconductor nanostructure 66 and the first pseudo-nanostructure 64A, or the isolation structures 100 can have a small thickness, such as a smaller thickness than the semiconductor nanostructure 66 and the first pseudo-nanostructure 64A. In some embodiments, the isolation structures 100 are 60% to 90% thinner than the semiconductor nanostructure 66, and 40% to 90% thinner than the first pseudo-nanostructure 64A.

[0046] exist Figure 9In the source / drain region 94, a lower epitaxial source / drain region 108L and an upper epitaxial source / drain region 108U are formed. A first contact etch stop layer (CESL) 112 and / or a first interlayer dielectric (ILD) 114 may also be formed in the source / drain region 94. The first ILD 114 is located between the upper epitaxial source / drain region 108U and the lower epitaxial source / drain region 108L. The lower epitaxial source / drain region 108L is used for the lower nanostructure FET of the CFET, and the upper epitaxial source / drain region 108U is used for the upper nanostructure FET of the CFET. Therefore, the first ILD 114 serves as an isolation region to prevent short circuits between the lower nanostructure FET and the upper nanostructure FET. Furthermore, a second CESL 122 and / or a second ILD 124 may be formed on the upper epitaxial source / drain region 108U.

[0047] The lower epitaxial source / drain region 108L contacts the lower semiconductor nanostructure 66L but not the upper semiconductor nanostructure 66U. In some embodiments, the lower epitaxial source / drain region 108L applies stress to the corresponding channel region of the lower semiconductor nanostructure 66L to improve performance. The lower epitaxial source / drain region 108L is formed in a source / source recess 94 such that each stack of the lower semiconductor nanostructure 66L is disposed between corresponding adjacent pairs of lower epitaxial source / drain regions 108L. In some embodiments, an internal spacer 98 is used to separate the lower epitaxial source / drain region 108L from the first pseudo-nanostructure 64A, which will be replaced by a gate structure in a subsequent process.

[0048] The lower epitaxial source / drain region 108L is epitaxially grown in the lower portion of the source / drain recess 94. For example, the lower epitaxial source / drain region 108L can be grown laterally from the exposed sidewalls of the lower semiconductor nanostructure 66L and the bottom surface of the fin 62 / substrate 50 in the source / drain recess 94. During the epitaxy of the lower epitaxial source / drain region 108L, the intermediate semiconductor nanostructure 66M and / or the upper semiconductor nanostructure 66U can be masked to prevent undesirable epitaxial growth on the intermediate semiconductor nanostructure 66M and / or the upper semiconductor nanostructure 66U. After the lower epitaxial source / drain region 108L is grown, the mask on the intermediate semiconductor nanostructure 66M and / or the upper semiconductor nanostructure 66U can then be removed. The lower epitaxial source / drain region 108L has a conductivity type suitable for the device type of the lower nanostructure FET. In some embodiments, the lower epitaxial source / drain region 108L is an n-type source / drain region. For example, if the lower semiconductor nanostructure 66L is silicon, the lower epitaxial source / drain region 108L may include a material on which tensile strain is applied to the lower semiconductor nanostructure 66L, such as silicon, carbon-doped silicon, phosphorus-doped silicon, silicon phosphide, silicon arsenide, etc. In some embodiments, the lower epitaxial source / drain region 108L is a p-type source / drain region. For example, if the lower semiconductor nanostructure 66L is silicon-germanium, the lower epitaxial source / drain region 108L may include a material on which compressive strain is applied to the lower semiconductor nanostructure 66L, such as silicon-germanium, boron-doped silicon-germanium, boron-doped silicon, germanium, germanium-tin, etc. The lower epitaxial source / drain region 108L may have a surface protruding from the corresponding upper surface of the lower semiconductor nanostructure 66L, and may have a small facet.

[0049] The lower epitaxial source / drain region 108L can be implanted with dopant to form the source / drain region, similar to the previously discussed process for forming lightly doped source / drain regions, followed by annealing. The source / drain region can have a dopant content of 10... 19 atoms / cm 3 and 10 21 atoms / cm 3 The impurity concentration is within the range specified. The n-type and / or p-type impurities used for the source / drain regions can be any impurities previously discussed. In some embodiments, the lower epitaxial source / drain region 108L is in-situ doped during growth.

[0050] As a result of the epitaxial process used to form the lower epitaxial source / drain regions 108L, the upper surface of the lower epitaxial source / drain regions 108L has small planes that extend laterally outward beyond the sidewalls of the nanostructures 64, 66. In some embodiments, adjacent lower epitaxial source / drain regions 108L remain separated after the epitaxial process is completed. In other embodiments, these small planes cause adjacent lower epitaxial source / drain regions 108L of the same nanostructure FET to merge.

[0051] The first ILD 114 is formed above the lower epitaxial source / drain region 108L. The first ILD 114 can be formed of a dielectric material, which can be deposited by any suitable method, such as CVD, plasma-enhanced chemical vapor deposition (PECVD), or FCVD. The dielectric material can include phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), etc. Other dielectric materials formed by any acceptable process can be used.

[0052] The first CESL 112 can be formed between the first ILD 114 and the lower epitaxial source / drain region 108L. The first CESL 112 can be formed from a dielectric material that has high etch selectivity to the dielectric material of the first ILD 114, such as silicon nitride, silicon oxide, silicon oxynitride, etc., which can be formed by any suitable deposition process, such as CVD, ALD, etc.

[0053] The first CESL 12 and / or the first ILD 114 can be formed by depositing material for the first CESL 112 and material for the first ILD 114, followed by an etch-back process. In some embodiments, the first ILD 114 is initially etched, leaving the first CESL 112 unetched. An anisotropic etch process is then performed to remove portions of the first CESL 112 above the first ILD 114. After recessing, the sidewalls of the upper semiconductor nanostructure 66U are exposed.

[0054] The upper epitaxial source / drain region 108U contacts the upper semiconductor nanostructure 66U but not the lower semiconductor nanostructure 66L. In some embodiments, the upper epitaxial source / drain region 108U applies stress to the corresponding channel region of the upper semiconductor nanostructure 66U to improve performance. The upper epitaxial source / drain region 108U is formed in the source / source recess 94 such that each stack of the upper semiconductor nanostructure 66U is disposed between corresponding adjacent pairs of upper epitaxial source / drain regions 108U. In some embodiments, an internal spacer 98 is used to separate the upper epitaxial source / drain region 108U from the first pseudo-nanostructure 64A, which will be replaced by a gate structure in a subsequent process.

[0055] The upper epitaxial source / drain region 108U is epitaxially grown in the upper portion of the source / drain recess 94. For example, the upper epitaxial source / drain region 108U can be laterally grown from the exposed sidewalls of the upper semiconductor nanostructure 66U. The upper epitaxial source / drain region 108U has a conductivity type suitable for the device type of the upper nanostructure FET. The conductivity type of the upper epitaxial source / drain region 108U can be opposite to the conductivity type of the lower epitaxial source / drain region 108L. In other words, the upper epitaxial source / drain region 108U can be doped in the opposite way to the lower epitaxial source / drain region 108L. In some embodiments, the upper epitaxial source / drain region 108U is an n-type source / drain region. For example, if the upper semiconductor nanostructure 66U is silicon, the upper epitaxial source / drain region 108U may include a material on which tensile strain is applied to the upper semiconductor nanostructure 66U, such as silicon, carbon-doped silicon, phosphorus-doped silicon, silicon phosphide, silicon arsenide, etc. In some embodiments, the upper epitaxial source / drain region 108U is a p-type source / drain region. For example, if the upper semiconductor nanostructure 66U is silicon-germanium, the upper epitaxial source / drain region 108U may include a material on which compressive strain is applied to the upper semiconductor nanostructure 66U, such as silicon-germanium, boron-doped silicon-germanium, boron-doped silicon, germanium, germanium-tin, etc. The upper epitaxial source / drain region 108U may have a surface protruding from the corresponding upper surface of the upper semiconductor nanostructure 66U, and may have a small facet.

[0056] The upper epitaxial source / drain region 108U can be implanted with dopant to form the source / drain region, similar to the previously discussed process for forming lightly doped source / drain regions, followed by annealing. The source / drain region can have a dopant content of 10... 19 atoms / cm 3 and 10 21 atoms / cm 3The impurity concentration is within the range specified. The n-type and / or p-type impurities used for the source / drain regions can be any impurities previously discussed. In some embodiments, the upper epitaxial source / drain region 108U is in-situ doped during growth.

[0057] As a result of the epitaxial process used to form the upper epitaxial source / drain regions 108U, the upper surface of the upper epitaxial source / drain regions 108U has small planes that extend laterally outward beyond the sidewalls of the nanostructures 64, 66. In some embodiments, adjacent upper epitaxial source / drain regions 108U remain separated after the epitaxial process is completed. In other embodiments, these small planes cause adjacent upper epitaxial source / drain regions 108U of the same nanostructure FET to merge.

[0058] The second ILD 124 is deposited above the upper epitaxial source / drain region 108U. The second ILD 124 can be formed of a dielectric material, which can be deposited by any suitable method, such as CVD, plasma-enhanced chemical vapor deposition (PECVD), or FCVD. The dielectric material can include phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), etc. Other dielectric materials formed by any acceptable process can be used.

[0059] The second CESL 122 can be formed between the second ILD 124 and the upper epitaxial source / drain region 108U. The second CESL 122 can be formed from a dielectric material with high etch selectivity to the dielectric material of the second ILD 124, such as silicon nitride, silicon oxide, silicon oxynitride, etc., which can be formed by any suitable deposition process, such as CVD, ALD, etc.

[0060] The second CESR 122 and / or the second ILD 124 can be formed by depositing material for the second CESR 122 and material for the second ILD 124. A removal process is then performed to make the top surface of the second ILD 124 flush with the top surface of the gate spacer 90 and the mask 86 (if present) or dummy gate 84. In some embodiments, planarization processes such as chemical mechanical polishing (CMP), etch-back processes, or combinations thereof can be utilized. The planarization process may also remove the mask 86 on the dummy gate 84 and portions of the gate spacer 90 along the sidewalls of the mask 86. After the planarization process, the top surfaces of the second ILD 124, the gate spacer 90, and the mask 86 (if present) or dummy gate 84 are substantially coplanar (within process variations). Therefore, the top surface of the mask 86 (if present) or dummy gate 84 is exposed through the second ILD 124. In the illustrated embodiment, the mask 86 is retained after the removal process. In other embodiments, mask 86 is removed so that the top surface of dummy gate 84 is exposed through second ILD 124.

[0061] exist Figure 10A and Figure 10B In one or more etching steps, the dummy gate 84 is removed, forming a recess 67 between the gate spacers 90. A portion of the dummy dielectric 82 in the recess 67 is also removed. In some embodiments, the dummy gate 84 and dummy dielectric 82 are removed by an anisotropic dry etching process. For example, the etching process may include a dry etching process using a reactive gas that selectively etches the material of the dummy gate 84 at a faster rate than the materials of the second ILD 124, the isolation structure 100, the internal spacers 98, and the gate spacers 90. Each recess 67 between the gate spacers 90 exposes portions of the nanostructures 64, 66 and / or lies on top of portions of the nanostructures 64, 66, which serve as channel regions in the resulting device. The portions of the nanostructures 64, 66 serving as channel regions are disposed between adjacent pairs of lower epitaxial source / drain regions 108L or adjacent pairs of upper epitaxial source / drain regions 108U. During removal, the dummy dielectric 82 may serve as an etch stop layer when the dummy gate 84 is etched. Then, the dummy dielectric 82 can be removed after the dummy gate 84 is removed.

[0062] The remaining portion of the first pseudo-nanostructure 64A is then removed to extend the groove 67 and form openings in the region between the semiconductor nanostructures 66. The remaining portion of the first pseudo-nanostructure 64A can be removed by any acceptable etching process that selectively etches the material of the first pseudo-nanostructure 64A at a rate faster than that of the semiconductor nanostructure 66, the internal spacer 98, and the isolation structure 100. The etching can be isotropic. For example, when the first pseudo-nanostructure 64A is formed of silicon germanium, the semiconductor nanostructure 66 is formed of silicon, the internal spacer 98 is formed of silicon carbonitride, and the isolation structure 100 is formed of silicon carbonitride, the etching process can be a wet etching using tetramethylammonium hydroxide (TMAH), ammonium hydroxide (NH4OH), etc. In some embodiments, a trimming process (not shown separately) is performed to reduce the thickness of the exposed portions of the semiconductor nanostructure 66 and to extend the openings between the semiconductor nanostructures 66.

[0063] exist Figure 11A and Figure 11B In this configuration, gate dielectric 132 can be deposited in recesses 67, such as in openings between gate spacers 90 and between semiconductor nanostructures 66. Gate dielectric 132 can also be deposited on the top surface of the second ILD 124 and the gate spacers 90. Gate dielectric 132 may include one or more gate dielectric layers disposed around the lower semiconductor nanostructure 66L, the upper semiconductor nanostructure 66U, and the isolation structure 100. Specifically, gate dielectric 132 is disposed on the top surface of fin 62; the top surface, sidewalls, and bottom surface of semiconductor nanostructure 66; and the sidewalls of gate spacers 90. Gate dielectric 132 encloses all (e.g., four) sides of semiconductor nanostructure 66. Gate dielectric 132 can be formed of: oxides, such as silicon oxide or metal oxides; silicates, such as metal silicates; combinations thereof; multilayers thereof, etc. Additionally or optionally, the gate dielectric 132 may be formed of a high-k dielectric material (e.g., a dielectric material with a k value greater than about 7.0), such as metal oxides or silicates of hafnium, aluminum, zirconium, lanthanum, manganese, barium, titanium, lead, and combinations thereof. The dielectric material of the gate dielectric 132 may be formed by molecular beam deposition (MBD), ALD, PECVD, etc. Although a single-layer gate dielectric 132 is shown, the gate dielectric 132 may include any number of interface layers and any number of main layers. For example, the gate dielectric 132 may include an interface layer selectively formed on the surfaces of the lower semiconductor nanostructure 66L and the upper semiconductor nanostructure 66U, and an upper high-k dielectric layer located above the interface layer. The interface layer may not be formed on the surface of the isolation structure 100. Furthermore, depending on the material of the intermediate semiconductor nanostructure 66M, the interface layer may not be formed on the surface of the intermediate semiconductor nanostructure 66M.

[0064] exist Figure 12 In this process, conformal deposition processes such as CVD and ALD are used to deposit materials in groove 67. Figure 11A and Figure 11B A dielectric layer 160 is deposited over the structure shown. The dielectric layer 160 may include a material such as aluminum oxide. The dielectric layer 160 may be formed over the gate dielectric 132 and around the lower semiconductor nanostructure 66L, the upper semiconductor nanostructure 66U, and the isolation structure 100. The dielectric layer 160 may fill the openings between the semiconductor nanostructures 66 and the opening between the bottommost semiconductor nanostructure 66 and the fin 62. In an embodiment, the dielectric layer 160 is also formed over the isolation region 70.

[0065] exist Figure 13 In this process, a bottom anti-reflective coating (BARC) 162 is formed in a recess 67, above the top surface and sidewalls of a dielectric layer 160 in the recess 67. In some embodiments, any suitable process (such as spin coating, CVD, PECVD, etc.) is used to coat the substrate. Figure 12 A BARC layer 162 is formed over the structure shown. In an embodiment, the BARC layer 162 may fill the recess 67. After forming the BARC layer 162, a portion of the BARC layer 162 may be disposed over the top surface of the second ILD 124 and the gate spacer 90. After forming the BARC layer 162, a suitable etch-back process (e.g., a dry etching process or a wet etching process) may be performed to form a recess 69 formed between the gate spacers 90. For example, the etch-back process may remove the top portion of the BARC layer 162 located over the second ILD 124, the gate spacer 90, and the top surface of the dielectric layer 160. Furthermore, the etch-back process may extend the recess 69 and remove the portion of the BARC layer 162 adjacent to the sidewall of the dielectric layer 160. For example, the etch-back process may remove the portion of the BARC layer 162 adjacent to the sidewall of the portion of the dielectric layer 160 above the isolation structure 100. Furthermore, the etch-back process can remove the portion of the BARC layer 162 adjacent to the sidewall of the dielectric layer 160 disposed on the sidewall of the isolation structure 100. In this way, after performing the etch-back process, the top surface of the dielectric layer 160 in the groove 69, the sidewall of the portion of the dielectric layer 60 above the isolation structure 100, and the sidewall of the portion of the dielectric layer 16 disposed on the sidewall of the isolation structure 100 are exposed. In this embodiment, after performing the etch-back process, the portion of the dielectric layer 160 above the isolation structure 100 is located above the topmost surface of the BARC layer 162.

[0066] After performing the etch-back process, the remaining portion of BARC layer 162 is used as an etch mask to perform an etch process to remove exposed portions of the dielectric layer 160 disposed above the top surface of BARC layer 160. In embodiments, the etch process can be an isotropic etch process, such as thermal dry etching performed at elevated temperatures using a mixture of nitrogen and hydrogen. For example, the etch process can extend the groove 69 by removing portions of the dielectric layer 160 disposed above and between the topmost upper semiconductor nanostructures 66U to form openings between the upper semiconductor nanostructures 66U. In embodiments, after performing the etch process, the top surface of BARC layer 162 can be flush with the top surface of dielectric layer 160. In embodiments, after performing the etch process, the top surfaces of BARC layer 162 and dielectric layer 160 can be disposed above the bottom surface of isolation structure 100 and below the top surface of isolation structure 100.

[0067] exist Figure 14 In this embodiment, a suitable ashing process is used to remove the BARC layer 162 to extend the recess 69. In this embodiment, the ashing process may include exposing the BARC layer 162 to oxygen plasma, etc. After removing the BARC layer 162, a metal-containing layer 164 may be deposited over the structure and in the recess 69 (e.g., over the dielectric layer 160, gate dielectric 132, and semiconductor nanostructure 66). The metal-containing layer 164 may include titanium nitride, etc., conformally deposited using a suitable process (e.g., ALD, CVD, PVD, etc.). In this embodiment, the metal-containing layer 164 may be deposited over the gate dielectric 132 and around the upper semiconductor nanostructure 66U to fill the openings between the upper semiconductor nanostructures 66U. Furthermore, the metal-containing layer 164 may be formed on the top surface and sidewalls of the dielectric layer 160 and the gate spacer 90, and on the top surface of the second ILD 124.

[0068] exist Figure 15In this process, an etching process (e.g., a wet etching process using hydrogen peroxide (H2O2), ammonium hydroxide (NH4OH), hydrochloric acid (HCl), etc.) is performed to remove portions of the metal-containing layer 164 disposed on the sidewalls and top surface of the dielectric layer 160. In an embodiment, the etching process may also remove portions of the metal-containing layer 164 disposed on the top surface and sidewalls of the gate spacer 90 and on the top surface of the second ILD 124. After the etching process, the sidewalls and top surface of the dielectric layer 160 may be exposed to the recess 69. In an embodiment, after the etching process, portions of the metal-containing layer 164 may remain disposed around and between the upper semiconductor nanostructure 66U. Furthermore, after the etching process, portions of the metal-containing layer 164 may remain disposed on the sidewalls of the intermediate semiconductor nanostructure 66M and the isolation structure 100. In an embodiment, after the etching process, the bottom surface of the metal-containing layer 164 contacts the top surface of the dielectric layer 160.

[0069] After performing an etching process to remove the portion containing the metal layer 164, the dielectric layer 160 is removed by performing an etching process. Performing the etching process to remove the dielectric layer 160 may include using an acid or alkaline solution (including ammonium hydroxide (NH4OH), hydrochloric acid (HCl), etc.) as an etchant to perform an isotropic etching process, such as wet etching. The etching process may result in the formation of openings between the lower semiconductor nanostructures 66L in the recess 69 and between the bottommost lower semiconductor nanostructure 66L and the fin 62.

[0070] exist Figure 16 In the middle, will previously in Figure 15 The structure shown is exposed to molecular inhibitor 165. In embodiments, molecular inhibitor 165 may include aniline, aniline derivatives, aldehydes, etc. Molecular inhibitor 165 may be a small, low molecular weight organic compound that selectively adheres to and selectively passivates the surface of the metal-containing layer 164 in the groove 69. For example, molecular inhibitor 165 may be introduced in the form of a gas or liquid solution into the previously... Figure 15 In the process chamber with the structure shown, a molecular inhibitor 165 can form a thin passivation layer 166 on the surface of the metal-containing layer 164 (including the sidewalls, bottom surface, and top surface of the metal-containing layer 164). The passivation layer 166 can selectively prevent material deposition on the surface of the metal-containing layer 164 during subsequent deposition processes.

[0071] In embodiments, molecular inhibitor 165 may comprise aniline or aniline derivatives, such as 3,4-(methylenedioxy)aniline, aniline-2-sulfonic acid, N-(2-hydroxyethyl)aniline, 4-(trifluoromethyl)aniline, 4-(methylthio)aniline, 3-(methylthio)aniline, 3-(1-aminoethyl)aniline, 4-(octyloxy)aniline, 4-(piperidin-1-ylmethyl)aniline, p-toluidine, N-ethyl-4-fluoroaniline, 4-isopropylaniline, 4-nitroaniline, p-aminoaniline, 4-chloroaniline, or 4-iodoaniline. In embodiments, molecular inhibitor 165 may comprise aldehydes, such as acetaldehyde, acrolein, butyraldehyde, crotonaldehyde, formaldehyde, or propionaldehyde.

[0072] Figure 17 The formation of a lower gate electrode 134L is illustrated. The lower gate electrode 134L may include one or more gate electrode layers disposed above the gate dielectric 132 and around the lower semiconductor nanostructure 66L. The lower gate electrode 134L is disposed in the lower portion of the recess 69 between the gate spacers 90 and in the opening between the lower semiconductor nanostructure 66L, and between the bottommost lower semiconductor nanostructure 66L and the fin 62. In an embodiment, the top surface of the lower gate electrode 134L is located below the top surface of the isolation structure 100. The lower gate electrode 134L may be formed of a metallic material, such as tungsten, titanium, titanium nitride, tantalum, tantalum nitride, tantalum carbide, aluminum, ruthenium, cobalt, combinations thereof, multilayers thereof, etc. For example, in an embodiment, the lower semiconductor nanostructure 66L may form a channel region for a subsequently formed lower nanostructure FET. In embodiments where the subsequently formed lower nanostructure FET is a p-type device, the lower gate electrode 134L can be formed of a metallic material, such as ruthenium, titanium nitride, tungsten nitride, tantalum nitride, etc. Although a single-layer gate electrode is shown, the lower gate electrode 134L may include any number of work function conditioning layers, any number of barrier layers, any number of adhesive layers, and filler materials.

[0073] The lower gate electrode 134L is formed of a material suitable for the device type of a lower nanostructure FET. For example, the lower gate electrode 134L may include one or more work function regulating layers formed of a work function regulating metal suitable for the device type of a lower nanostructure FET. In some embodiments, the lower gate electrode 134L includes a p-type work function regulating layer, which may be formed of a p-type work function regulating metal, such as titanium nitride, tantalum nitride, combinations thereof, etc. Additionally or optionally, the lower gate electrode 134L may include a dipole inducing element suitable for the device type of a lower nanostructure FET. Acceptable dipole inducing elements include lanthanum, aluminum, scandium, ruthenium, zirconium, erbium, magnesium, strontium, and combinations thereof.

[0074] As an example of forming the lower gate electrode 134L, one or more gate electrode layers are formed above the gate dielectric 132 and around the lower semiconductor nanostructure 66L in the recess 69. For example, a suitable conformal deposition process (such as ALD) is used to form the lower gate electrode 134L in the lower portion of the recess 69 between the gate spacers 90 and in the opening between the lower semiconductor nanostructure 66L, and between the bottommost lower semiconductor nanostructure 66L and the fin 62. During the deposition process, a passivation layer 166 on the surface of the metal layer 164 (e.g., sidewalls, top surface, and bottom surface) can suppress material from forming one or more gate electrode layers on the surface of the metal layer 64 in the upper portion of the recess 69. The passivation layer 166 can act as a barrier during the deposition process and prevent precursor molecules from reaching the surface of the metal layer 164. As a result, one or more gate electrode layers are formed only in the lower portion of the recess 69, such that the top surface of the lower gate electrode 134L is lower than the top surface of the isolation structure 100. One or more gate electrode layers are not deposited on the surface of the metal-containing layer 164 in the upper portion of the groove 69, and the metal-containing layer 164 is disposed on the top surface of the lower gate electrode 134L after the lower gate electrode 134L is formed.

[0075] Advantages can be achieved by forming a metal-containing layer 164, which is disposed around and between the upper semiconductor nanostructure 66U, and on the sidewalls of the intermediate semiconductor nanostructure 66M and the isolation structure 100. Then, an etching process to remove the dielectric layer 160 is performed (as previously described). Figure 15 As described above, openings are formed between the lower semiconductor nanostructures 66L in the groove 69 and between the bottommost lower semiconductor nanostructure 66L and the fin 62. Then, by exposing the surface of the metal-containing layer 164 to a molecular inhibitor 165 (e.g., which may include aniline, aniline derivatives, aldehydes, etc.), a passivation layer 166 is selectively formed on the surface of the metal-containing layer 64 (including the sidewalls, bottom, and top surfaces of the metal-containing layer 164). The molecular inhibitor 165 may be a small, low-molecular-weight organic compound that selectively adheres to and selectively passivates the surface of the metal-containing layer 164 in the groove 69, without adhering to or passivating other surfaces, such as the semiconductor nanostructures 66 or the surface of the gate dielectric 132. Then, a lower gate electrode 134L is formed in the lower portion of the groove 69 between the gate spacers 90. A lower gate electrode 134L is formed above the gate dielectric 132 and around the lower semiconductor nanostructure 66L, such that the lower gate electrode 134L is disposed in the opening between the lower semiconductor nanostructures 66L and in the opening between the bottommost lower semiconductor nanostructure 66L and the fin 62. The lower gate electrode 134L is formed using a conformal deposition process such as ALD.

[0076] These advantages include allowing the lower gate electrode 134L to be formed in the lower portion of the recess 69 and around the lower semiconductor nanostructure 66L, while the passivation layer 166 suppresses material formation of the lower gate electrode 134L on the surface of the metal-containing layer 164 in the upper portion of the recess 69. As a result, material formation of the lower gate electrode 134L in the upper portion of the recess 69 (e.g., on the surface of the metal-containing layer 164 and / or the gate dielectric 132 around the upper semiconductor nanostructure 66U) can be avoided. This allows the upper gate electrode 134U to be subsequently formed in the upper portion of the recess 69 above the lower gate electrode 134L (and subsequently in…). Figures 20 to 22 As described in the text, the lower gate electrode 134 can be formed in the lower portion of the recess 69 without performing an initial etch-back process to remove any material from the upper portion of the recess 69 (e.g., on the surface of the metal layer 164 and / or gate dielectric 132 surrounding the upper semiconductor nanostructure 66U). As a result, the loading effects associated with the etch-back process that could lead to variations in the part size of the lower gate electrode 134L can be avoided, resulting in improved uniformity and consistency of the dimensions of the lower and upper gate electrodes (134L / 134U). This can lead to enhanced device performance and improved device yield. Furthermore, forming the lower gate electrode 134L in the lower portion of the recess 69 using atomic layer deposition (ALD) allows for conformal deposition of the material of the lower gate electrode 134L around the lower semiconductor nanostructure 66L. As a result, precise dimensional control of the lower gate electrode 134L can be achieved, which can allow for consistent device performance.

[0077] exist Figure 18 In this process, a suitable process is used to remove the passivation layer 166 from the surface containing the metal layer 164. For example, in an embodiment, a heat treatment process can be performed, wherein the process temperature during the heat treatment process can be in the range of 200°C to 400°C. The increased temperature of the heat treatment process can promote the decomposition of the molecules of the passivation layer 166. In an embodiment, an etching process can be performed to remove the passivation layer 166. Performing an etching process can include performing a dry etching process using free radicals (e.g., hydrogen free radicals, etc.) or plasma (e.g., hydrogen plasma, etc.). In an embodiment, a wet stripping process can be performed using a suitable solvent or chemical solution to dissolve and rinse away the passivation layer 166.

[0078] After removing the passivation layer 166, an etching process is performed to remove the metal-containing layer 164. In one embodiment, performing the etching process may include using hydrogen peroxide (H2O2) as an etchant to perform an isotropic etching process, such as wet etching. In other embodiments, the etching process may include exposing the surface of the metal-containing layer 164 to a solution comprising hydrogen peroxide (H2O2), ammonium hydroxide (NH4OH), and water. Performing the etching process may result in the formation of openings between the upper semiconductor nanostructures 66U in the recess 69 and between the bottom upper semiconductor nanostructure 66U and the intermediate semiconductor nanostructure 66M.

[0079] exist Figure 19 In the middle, the previous Figure 18 The structure shown is exposed to molecular inhibitor 167. In embodiments, molecular inhibitor 167 may include aniline, aniline derivatives, aldehydes, etc. Molecular inhibitor 167 may be a small, low molecular weight organic compound that selectively adheres to the surface (e.g., top surface) of the lower gate electrode 134L in the recess 69 and selectively passivates the surface of the lower gate electrode 134L in the recess 69. For example, molecular inhibitor 167 may be introduced in the form of a gas or liquid solution into the previously contained... Figure 18 In the process chamber with the structure shown, the molecular inhibitor 167 can form a thin passivation layer 168 on the surface (e.g., the top surface) of the lower gate electrode 134L. The passivation layer 168 can selectively prevent material deposition on the surface of the lower gate electrode 134L during subsequent deposition processes.

[0080] In embodiments, molecular inhibitor 167 may comprise aniline or aniline derivatives, such as 3,4-(methylenedioxy)aniline, aniline-2-sulfonic acid, N-(2-hydroxyethyl)aniline, 4-(trifluoromethyl)aniline, 4-(methylthio)aniline, 3-(methylthio)aniline, 3-(1-aminoethyl)aniline, 4-(octyloxy)aniline, 4-(piperidin-1-ylmethyl)aniline, p-toluidine, N-ethyl-4-fluoroaniline, 4-isopropylaniline, 4-nitroaniline, p-aminoaniline, 4-chloroaniline, or 4-iodoaniline. In embodiments, molecular inhibitor 167 may comprise aldehydes, such as acetaldehyde, acrolein, butyraldehyde, crotonaldehyde, formaldehyde, or propionaldehyde.

[0081] exist Figure 20In this embodiment, metal-containing layers 170 and 172 can be sequentially deposited over the gate dielectric 132 and the semiconductor nanostructure 66 in the recess 69. Metal-containing layer 170 may include materials such as titanium or aluminum, and is conformally deposited using a suitable deposition process (such as ALD). In this embodiment, metal-containing layer 170 can be deposited over the gate dielectric 132 and around the upper semiconductor nanostructure 66U. Metal-containing layer 170 can also be formed over the top surface of the intermediate semiconductor nanostructure 66M and on the sidewalls of the intermediate semiconductor nanostructure 66M. Furthermore, metal-containing layer 170 can also be formed on the sidewalls of the isolation structure 100. During the deposition process of forming metal-containing layer 170, a passivation layer 168 on the surface (e.g., the top surface) of the lower gate electrode 134L can suppress the formation of metal-containing layer 170 on the surface (e.g., the top surface) of the lower gate electrode 134L. The passivation layer 168 can act as a barrier during the deposition process and prevent precursor molecules from reaching the surface (e.g., the top surface) of the lower gate electrode 134L. As a result, a metal-containing layer 170 can be formed around the upper semiconductor nanostructure 66U, above the top surface of the intermediate semiconductor nanostructure 66M, on the sidewalls of the intermediate semiconductor nanostructure 66M, and on the sidewalls of the isolation structure 100. The metal-containing layer 170 is not deposited on the top surface of the lower gate electrode 134L, and after the metal-containing layer 70 is formed, the passivation layer 168 can be disposed between the bottom surface of the metal-containing layer 170 and the top surface of the lower gate electrode 134L.

[0082] The metal-containing layer 172 may include titanium nitride, etc., and is conformally deposited using a suitable deposition process (such as ALD). In an embodiment, the metal-containing layer 172 may be deposited over the metal-containing layer 170, the gate dielectric 132, and around the upper semiconductor nanostructure 66U to fill the openings between the upper semiconductor nanostructures 66U. The metal-containing layer 172 may also be formed over the top surface of the intermediate semiconductor nanostructure 66M and on the sidewalls of the intermediate semiconductor nanostructure 66M. Furthermore, the metal-containing layer 172 may also be formed on the sidewalls of the isolation structure 100. During the deposition process of forming the metal-containing layer 172, a passivation layer 168 on the surface (e.g., the top surface) of the lower gate electrode 134L may suppress the formation of the metal-containing layer 172 on the surface (e.g., the top surface) of the lower gate electrode 134L. The passivation layer 168 may act as a barrier during the deposition process and prevent precursor molecules from reaching the surface (e.g., the top surface) of the lower gate electrode 134L. As a result, the metal-containing layer 172 can be formed around the upper semiconductor nanostructure 66U, above the top surface of the intermediate semiconductor nanostructure 66M, on the sidewalls of the intermediate semiconductor nanostructure 66M, and on the sidewalls of the isolation structure 100. The metal-containing layer 172 is not deposited on the top surface of the lower gate electrode 134L, and after the metal-containing layer 172 is formed, the passivation layer 168 can be disposed between the bottom surface of the metal-containing layer 172 and the top surface of the lower gate electrode 134L.

[0083] exist Figure 21 In this process, a suitable process is used to remove the passivation layer 168 from the surface (e.g., the top surface) of the lower gate electrode 134L. For example, in an embodiment, a heat treatment process can be performed, wherein the process temperature during the heat treatment process can be in the range of 200°C to 400°C. The increased temperature of the heat treatment process can promote the decomposition of the molecules of the passivation layer 168. In an embodiment, an etching process can be performed to remove the passivation layer 168. Performing the etching process can include performing a dry etching process using free radicals (e.g., hydrogen free radicals, etc.) or plasma (e.g., hydrogen plasma, etc.). In an embodiment, a wet stripping process can be performed using a suitable solvent or chemical solution to dissolve and rinse away the passivation layer 168. After removing the passivation layer 168 from the surface (e.g., the top surface) of the lower gate electrode 134L, a space (which may have been previously occupied by the passivation layer 168) can be provided between the bottom surface containing the metal layers 170 and 172 and the top surface of the lower gate electrode 134L.

[0084] After removing the passivation layer 168, one or more gate electrode layers 174 are formed in the groove 69 above the lower gate electrode 134L, the metal-containing layer 170, the metal-containing layer 172, the gate dielectric 132, and the upper semiconductor nanostructure 66U. The one or more gate electrode layers 174 can fill the space between the bottom surfaces of the metal-containing layers 170 and 172 and the top surface of the lower gate electrode 134L. In this way, the one or more gate electrode layers 174 can contact the bottom surfaces of the metal-containing layers 170 and 172. In an embodiment, the one or more gate electrode layers 174 are disposed between the metal-containing layers 170 and 172 and the lower gate electrode 134L. In an embodiment, the bottom surface of the one or more gate electrode layers 174 can be higher than the bottom surface of the isolation structure, and the bottom surface of the one or more gate electrode layers 174 can be lower than the top surface of the isolation structure 100. In an embodiment, the bottom surfaces of metal-containing layers 170 and 172 may be higher than the bottom surface of the isolation structure, and the bottom surfaces of metal-containing layers 170 and 172 may be lower than the top surface of the isolation structure 100. In an embodiment, the sidewalls of metal-containing layers 170 and 172 are configured to be adjacent to the sidewalls of the isolation structure 100. In an embodiment, metal-containing layers 170, 172, and one or more gate electrode layers 174 form an upper gate electrode 134U, which is disposed above the gate dielectric 132 and around the upper semiconductor nanostructure 66U. The upper gate electrode 134U is disposed in the upper portion of the recess 69 between the gate spacers 90 and in the opening between the upper semiconductor nanostructures 66U. One or more gate electrode layers 174 may be formed of a metal-containing material, such as tungsten, titanium, titanium nitride, tantalum, tantalum nitride, tantalum carbide, aluminum, ruthenium, cobalt, combinations thereof, multilayers thereof, etc. For example, in one embodiment, the upper semiconductor nanostructure 66U can form the channel region for a subsequently formed upper nanostructure FET. In an embodiment where the subsequently formed upper nanostructure FET is an n-type device, one or more gate electrode layers 174 can be formed of a metallic material (such as titanium nitride). In one embodiment, the upper gate electrode 134U can include any number of power function conditioning layers, any number of barrier layers, any number of adhesive layers, and filler materials.

[0085] In some embodiments, the upper gate electrode 134U may include a dipole inducing element suitable for the device type of the upper nanostructure FET. Acceptable dipole inducing elements include lanthanum, aluminum, scandium, ruthenium, zirconium, erbium, magnesium, strontium, and combinations thereof. The dipole inducing element of the upper gate electrode 134U may differ from that of the lower gate electrode 134L. In some embodiments where the isolation layer is omitted, the upper nanostructure FET may be coupled to the lower nanostructure FET. In some embodiments, the lower gate electrode 134L may be physically and electrically coupled to the upper gate electrode 134U.

[0086] As an example of forming one or more gate electrode layers 174, one or more gate electrode layers 174 are formed in a recess 69 above the lower gate electrode 134L, the metal-containing layer 170, the metal-containing layer 172, the gate dielectric 132, and the upper semiconductor nanostructure 66U. For example, a suitable conformal deposition process (such as ALD) is used to form one or more gate electrode layers 174 in the upper portion of the recess 69 and above the lower gate electrode 134L. In the following figures, the metal-containing layer 170, the metal-containing layer 172, and one or more gate electrode layers 174 of the upper gate electrode 134U may not be shown separately, but may be collectively shown as the upper gate electrode 134U.

[0087] exist Figure 22 In this process, a removal process can be performed to remove excess portions of one or more gate electrode layers 174 and / or gate dielectric 132 located above the top surfaces of gate spacer 90 and second ILD 124. In some embodiments, planarization processes such as chemical mechanical polishing (CMP), etch-back processes, or combinations thereof can be utilized. When a planarization process is used, the top surfaces of gate spacer 90, second ILD 124, gate dielectric 132, and upper gate electrode 134U are coplanar (within process variations).

[0088] Gate dielectric 132 and gate electrode 134 (including lower gate electrode 134L and upper gate electrode 134U) form an alternative gate. Each corresponding pair of gate dielectric 132 and gate electrode 134 (including upper gate electrode 134U and / or lower gate electrode 134L) may be collectively referred to as a "gate structure" or "gate stack". Each gate structure extends along at least three sides (e.g., top surface, sidewalls, and bottom surface) of the channel region of the semiconductor nanostructure 66. The gate structure may also extend along the sidewalls and / or top surface of the semiconductor fin 62.

[0089] Advantages can be achieved by exposing the surface of the lower gate electrode 134L to a molecular inhibitor 167 (e.g., which may include aniline, aniline derivatives, aldehydes, etc.) to form a passivation layer 168 on the surface of the lower gate electrode 134L (including the top surface of the lower gate electrode 134). The molecular inhibitor 167 can be a small, low-molecular-weight organic compound that selectively adheres to the surface of the lower gate electrode 134L in the recess 69 (e.g., the top surface) and selectively passivates the surface of the lower gate electrode 134L in the recess 69 without adhering to or passivating other surfaces, such as the surface of the semiconductor nanostructure 66 or the gate dielectric 132. Metal-containing layers 170 and 172 can be sequentially deposited (e.g., using an ALD process) over the gate dielectric 132 and over the semiconductor nanostructure 66 in the upper portion of the recess 69 (e.g., around the upper semiconductor nanostructure 66U). A passivation layer 168 on the surface (e.g., top surface) of the lower gate electrode 134L can suppress the formation of metal-containing layers 170 and 172 on the surface (e.g., top surface) of the lower gate electrode 134L. The passivation layer 168 is removed from the surface (e.g., top surface) of the lower gate electrode 134L using a suitable process. After removing the passivation layer 168, one or more gate electrode layers 174 are formed in a recess 69 above the lower gate electrode 134L, metal-containing layers 170 and 172, gate dielectric 132, and upper semiconductor nanostructure 66U using a conformal deposition process such as ALD. The metal-containing layers 170, 172, and one or more gate electrode layers 174 form the upper gate electrode 134U in the upper portion of the recess 69, which is disposed above the gate dielectric 132 and around the upper semiconductor nanostructure 66U.

[0090] These advantages include allowing the upper gate electrode 134U to be formed in the upper portion of the recess 69 and around the upper semiconductor nanostructure 66U, while the passivation layer 168 suppresses the formation of material for the upper gate electrode 134U on the surface (e.g., the top surface) of the lower gate electrode 134L. This allows the use of conformal deposition processes such as ALD to deposit material for the upper gate electrode 134U (e.g., metal-containing layers 170 and 172) only around the upper semiconductor nanostructure 66U, without depositing material for the upper gate electrode 134U on the surface (e.g., the top surface) of the lower gate electrode 134L. Therefore, different and separate gate structures (e.g., the lower gate electrode 134L for the lower semiconductor nanostructure 66L and the upper gate electrode 134U for the upper semiconductor nanostructure 66U) can be formed without additional etch-back processes (e.g., removing portions of metal-containing layers 170 and 172 from the top surface of the lower gate electrode 134L). As a result, improved control over the dimensions of the lower gate electrode 134L and the upper gate electrode 134U can be achieved, and the risk of damaging the lower gate electrode 134L during the additional etch-back process is reduced. This can lead to enhanced overall device performance and improved device yield.

[0091] exist Figure 23 In the second ILD 124, a source / drain contact 144 is formed to electrically couple to the upper epitaxial source / drain region 108U and / or the lower epitaxial source / drain region 108L. As an example of forming the source / drain contact 144, an opening for the source / drain contact 144 is formed through the second ILD 124 and the second CESL 122. The opening can be formed using acceptable photolithography and etching techniques. In the illustrated embodiment, the opening is formed using a self-aligned contact (SAC) process. A liner (not shown separately) (such as a diffusion barrier layer, adhesive layer, etc.) and a conductive material are formed in the opening. The liner may include titanium, titanium nitride, tantalum, tantalum nitride, etc. The conductive material may be cobalt, tungsten, copper, copper alloy, silver, gold, aluminum, nickel, etc. A removal process can be performed to remove the material from the gate spacer 90, the second ILD 124 (see...). Figure 22 Excess material is removed from the top surface of the gate electrode 134U and the upper gate electrode 134U. The remaining liner and conductive material form the source / drain contacts 144 in the opening. In some embodiments, a planarization process is used, such as chemical mechanical polishing (CMP), etch-back process, or a combination thereof. After the planarization process, the gate spacer 90, the second ILD 124 (see Figure 22 The top surfaces of the upper gate electrode 134U and the source / drain contact 144 are substantially coplanar (within the process variation).

[0092] Optionally, a metal-semiconductor alloy region 142 is formed at the interface between the source / drain region 108 and the source / drain contact 144. The metal-semiconductor alloy region 142 can be a silicide region formed from metal silicides (e.g., titanium silicide, cobalt silicide, nickel silicide, etc.), a germanide region formed from metal germanides (e.g., titanium germanide, cobalt germanide, nickel germanide, etc.), or a silicon-germanide region formed from both metal silicides and metal germanides. The metal-semiconductor alloy region 142 can be formed before the material of the source / drain contact 144 by depositing metal in the opening for the source / drain contact 144 and then performing a thermal annealing process. The metal can be any metal capable of reacting with the semiconductor material of the source / drain region 108 (e.g., silicon, silicon-germanium, germanium, etc.) to form a low-resistance metal-semiconductor alloy, such as nickel, cobalt, titanium, tantalum, platinum, tungsten, other noble metals, other refractory metals, rare earth metals, or alloys thereof. Metals can be deposited using deposition processes such as ALD, CVD, PVD, etc. After a thermal annealing process, a cleaning process (such as wet cleaning) can be performed to remove any residual metal from openings in the source / drain contacts 144 (such as from the surface of the metal-semiconductor alloy region 142). The material for the source / drain contacts 144 can then be formed on the metal-semiconductor alloy region 142.

[0093] exist Figure 24A and Figure 24B In this configuration, the third ILD 154 is deposited over the gate spacer 90, the second ILD 124, the upper gate electrode 134U, and the source / drain contact 144. In some embodiments, the third ILD 154 is a flowable film formed by a flowable CVD method and subsequently cured. In some embodiments, the third ILD 154 is formed of a dielectric material, such as PSG, BSG, BPSG, USG, etc., which can be deposited by any suitable method, such as CVD, PECVD, etc.

[0094] In some embodiments, an etch stop layer (ESL) 152 is formed between the third ILD 154 and the gate spacer 90, the second ILD 124, the upper gate electrode 134U, and the source / drain contact 144. The ESL 152 may include a dielectric material that has high etch selectivity to the dielectric material of the third ILD 154, such as silicon nitride, silicon oxide, silicon oxynitride, etc.

[0095] A gate contact 156 and a source / drain via 158 are formed through the third ILD 154 to electrically couple to the upper gate electrode 134U and the source / drain contact 144, respectively. As an example of forming the gate contact 156 and the source / drain via 158, openings for the gate contact 156 and the source / drain via 158 are formed through the third ILD 154 and ESL 152. The openings can be formed using acceptable photolithography and etching techniques. A liner (not shown separately) (such as a diffusion barrier layer, adhesive layer, etc.) and a conductive material are formed within the openings. The liner may include titanium, titanium nitride, tantalum, tantalum nitride, etc. The conductive material may be cobalt, tungsten, copper, copper alloys, silver, gold, aluminum, nickel, etc. A planarization process (such as CMP) may be performed to remove excess material from the top surface of the third ILD 154. The remaining liner and conductive material form the gate contact 156 and the source / drain via 158 within the openings. The gate contact 156 and the source / drain via 158 can be formed in different processes or in the same process. Although shown as being formed in the same cross-section, it should be understood that each of the gate contact 156 and the source / drain via 158 can be formed in different cross-sections, which can prevent short circuits in the contacts.

[0096] The active devices shown are collectively referred to as the device layer. In some embodiments, contacts to the lower gate electrode 134L and the lower epitaxial source / drain region 108L can be fabricated on the back side of the device layer (e.g., the side opposite to the source / drain contact 144).

[0097] The embodiments of this disclosure have several advantageous features. The embodiments include forming a semiconductor device comprising a complementary field-effect transistor (CFET), wherein forming the semiconductor device may include forming an upper channel region of an upper nanostructure FET and a lower channel region of a lower nanostructure FET, the upper and lower channel regions being disposed above the fin. A gate dielectric layer is formed around the upper and lower channel regions and above the fin. A first metallized material layer may be formed around the upper channel region such that the gate dielectric layer is disposed between the first metallized material layer and the upper channel region. The semiconductor device may be exposed to a first molecular inhibitor (e.g., aniline or aldehyde, etc.) such that the first molecular inhibitor selectively adheres to the surface of the first metallized material layer surrounding the upper channel region. A lower gate electrode is then formed above the gate dielectric layer and around the lower channel region using a conformal deposition process such as atomic layer deposition (ALD), wherein during the deposition process, the first molecular inhibitor acts as a protective layer to prevent material of the lower gate electrode from forming on the surface of the first metallized material layer. After the lower gate electrode is formed, the first molecular inhibitor and the first metal-containing material layer are removed using a suitable process. The semiconductor device can then be exposed to a second molecular inhibitor (e.g., aniline or aldehyde), allowing the second molecular inhibitor to selectively adhere to the top surface of the lower gate electrode. A second and third metal-containing material layer can be sequentially formed around the upper channel region, such that the gate dielectric layer is disposed between the second and third metal-containing material layers and the upper channel region. During the formation of the second and third metal-containing material layers, the second molecular inhibitor acts as a protective layer to prevent the formation of the second and third metal-containing material layers on the top surface of the lower gate electrode. After the formation of the second and third metal-containing material layers, the second molecular inhibitor can be removed using a suitable process. Then, an upper gate electrode is formed above the lower gate electrode and around the gate dielectric layer, the second metal-containing material layer, the third metal-containing material layer, and the upper channel region using a conformal deposition process such as ALD.

[0098] One or more embodiments disclosed herein allow for the formation of a lower gate electrode around a lower channel region and an upper gate electrode around an upper channel region, wherein the upper gate electrode is disposed above the lower gate electrode, without having to perform an etch-back process to remove the top portion of the lower gate electrode. As a result, the loading effects associated with etch-back processes that could lead to variations in the component size of the lower gate electrode can be avoided, resulting in improved uniformity and consistency of the dimensions of the lower and upper gate electrodes. This can lead to enhanced device performance and improved device yield. Furthermore, using atomic layer deposition (ALD) to form the lower and upper gate electrodes allows for the conformal deposition of the materials for the lower and upper gate electrodes, respectively, around the lower and upper channel regions of the nanostructured FET. As a result, precise dimensional control of the lower and upper gate electrodes can be achieved, which can allow for consistent device performance.

[0099] According to an embodiment, a method includes: forming a multilayer stack over a semiconductor substrate, the multilayer stack including alternating semiconductor nanostructures and pseudo-nanostructures; forming a lower source / drain region, wherein lower semiconductor nanostructures of the semiconductor nanostructures extend between the lower source / drain regions; forming an upper source / drain region over the lower source / drain region, wherein upper semiconductor nanostructures of the semiconductor nanostructures extend between the upper source / drain regions; removing the pseudo-nanostructures to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; forming a gate dielectric layer around the lower and upper semiconductor nanostructures; forming a first metal-containing layer around the upper semiconductor nanostructures and in the second opening; exposing the surface of the first metal-containing layer to a first molecular inhibitor to form a first passivation layer on the surface of the first metal-containing layer; and forming a lower gate electrode around the lower semiconductor nanostructures and in the first opening. In an embodiment, the first molecular inhibitor includes aniline, an aniline derivative, or an aldehyde. In an embodiment, the material of the lower gate electrode includes ruthenium, titanium nitride, tungsten nitride, or tantalum nitride. In an embodiment, the first metal-containing layer includes titanium nitride. In an embodiment, forming the lower gate electrode around the lower semiconductor nanostructure and in the first opening includes performing an atomic layer deposition (ALD) process to conformally deposit the material of the lower gate electrode around the lower semiconductor nanostructure and in the first opening. In an embodiment, the method further includes removing a first passivation layer from the surface of the first metal-containing layer; and performing an etching process to remove the first metal-containing layer and form a third opening between the upper semiconductor nanostructures. In an embodiment, the method further includes exposing the top surface of the lower gate electrode to a second molecular inhibitor to form a second passivation layer on the top surface of the lower gate electrode; and forming a second metal-containing layer and a third metal-containing layer around the upper semiconductor nanostructure and in the third opening. In an embodiment, the method further includes removing the second passivation layer from the top surface of the lower gate electrode; and conformally depositing a gate electrode layer over the second metal-containing layer, the third metal-containing layer, and the lower gate electrode.

[0100] According to an embodiment, a method includes: forming a multilayer stack over a semiconductor substrate, the multilayer stack including alternating semiconductor layers and dummy layers; patterning the multilayer stack to form fins, wherein the fins include alternating semiconductor nanostructures and dummy nanostructures, the semiconductor nanostructures being defined by semiconductor layers and the dummy nanostructures being defined by dummy layers; forming a lower source / drain region, wherein a lower semiconductor nanostructure of the semiconductor nanostructure extends between the lower source / drain regions; forming an upper source / drain region over the lower source / drain region, wherein an upper semiconductor nanostructure of the semiconductor nanostructure extends between the upper source / drain regions; removing the dummy nanostructures to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; forming a first metal-containing layer around the upper semiconductor nanostructures and in the second opening; forming a first passivation layer on the surface of the first metal-containing layer; and forming a lower gate stack around the lower semiconductor nanostructures and in the first opening. In an embodiment, forming the first passivation layer includes exposing the surface of the first metal-containing layer to a first molecule inhibitor. In an embodiment, the first molecule inhibitor includes aniline, an aniline derivative, or an aldehyde. In an embodiment, the lower gate stack includes: a first gate dielectric layer surrounding the lower semiconductor nanostructure; and a first gate electrode layer above the first gate dielectric layer and within a first opening. In an embodiment, the material of the first gate electrode layer includes ruthenium, titanium nitride, tungsten nitride, or tantalum nitride. In an embodiment, the first metal-containing layer includes titanium nitride. In an embodiment, the method further includes removing a first passivation layer from the surface of the first metal-containing layer; performing an etching process to remove the first metal-containing layer and form a third opening between the upper semiconductor nanostructures; forming a second passivation layer on the top surface of the lower gate stack; and forming an upper gate stack around the upper semiconductor nanostructure and within the third opening.

[0101] According to an embodiment, the semiconductor device includes: a plurality of first nanostructures extending between first source / drain regions; a plurality of second nanostructures located above the plurality of first nanostructures and extending between second source / drain regions; an isolation structure located between the plurality of first nanostructures and the plurality of second nanostructures; a first gate stack located around the plurality of first nanostructures; and a second gate stack located above the first gate stack and disposed around the plurality of second nanostructures, wherein the second gate stack includes: a first metal-containing layer located around the second nanostructures of the plurality of second nanostructures; a second metal-containing layer located above the first metal-containing layer and around the second nanostructures of the plurality of second nanostructures; and a first gate electrode layer located above the first metal-containing layer and the second metal-containing layer, wherein the sidewalls of the first metal-containing layer and the second metal-containing layer are adjacent to the sidewalls of the isolation structure. According to an embodiment, the first metal-containing layer includes titanium aluminum, and the second metal-containing layer includes titanium nitride. In an embodiment, the first gate electrode layer includes titanium nitride, wherein the first gate electrode layer is disposed between the first gate stack and the first metal-containing layer. In one embodiment, the first gate stack includes a second gate electrode layer, wherein the second gate electrode layer includes ruthenium. In another embodiment, the semiconductor device further includes an isolation layer located between a corresponding second source / drain region of each first source / drain region and a corresponding second source / drain region of the second source / drain region.

[0102] The foregoing outlines features of several embodiments to enable those skilled in the art to better understand aspects of this disclosure. Those skilled in the art should understand that they can readily use this disclosure as a basis to design or modify other processes and structures for implementing the same purposes and / or achieving the same advantages as the embodiments described herein. Those skilled in the art should also recognize that such equivalent constructions do not depart from the spirit and scope of this disclosure, and that various changes, substitutions, and alterations can be made to them herein without departing from the spirit and scope of this disclosure.

Claims

1. A method for forming a semiconductor device, comprising: A multilayer stack is formed on a semiconductor substrate, the multilayer stack comprising alternating semiconductor nanostructures and pseudo-nanostructures; A lower source / drain region is formed, wherein the lower semiconductor nanostructure of the semiconductor nanostructure extends between the lower source / drain regions; An upper source / drain region is formed above the lower source / drain region, wherein the upper semiconductor nanostructure of the semiconductor nanostructure extends between the upper source / drain regions; The pseudo-nanostructure is removed to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; A gate dielectric layer is formed around the lower semiconductor nanostructure and the upper semiconductor nanostructure; A first metal-containing layer is formed around the upper semiconductor nanostructure and in the second opening; Exposing the surface of the first metal-containing layer to a first molecule inhibitor to form a first passivation layer on the surface of the first metal-containing layer; and A lower gate electrode is formed around the lower semiconductor nanostructure and in the first opening.

2. The method according to claim 1, wherein, The first molecular inhibitor includes aniline, aniline derivatives, or aldehydes.

3. The method according to claim 1, wherein, The material of the lower gate electrode includes ruthenium, titanium nitride, tungsten nitride, or tantalum nitride.

4. The method according to claim 1, wherein, The first metal-containing layer includes titanium nitride.

5. The method according to claim 1, wherein, Forming the lower gate electrode around the lower semiconductor nanostructure and in the first opening includes performing an atomic layer deposition (ALD) process to conformally deposit material of the lower gate electrode around the lower semiconductor nanostructure and in the first opening.

6. The method according to claim 1, further comprising: Remove the first passivation layer from the surface containing the first metal layer; as well as An etching process is performed to remove the first metal-containing layer and form a third opening between the upper semiconductor nanostructures.

7. The method according to claim 6, further comprising: The top surface of the lower gate electrode is exposed to a second molecular inhibitor to form a second passivation layer on the top surface of the lower gate electrode; as well as A second metal-containing layer and a third metal-containing layer are formed around the upper semiconductor nanostructure and in the third opening.

8. The method according to claim 7, further comprising: Remove the second passivation layer from the top surface of the lower gate electrode; as well as A gate electrode layer is conformally deposited above the second metal-containing layer, the third metal-containing layer, and the lower gate electrode.

9. A method for forming a semiconductor device, comprising: A multilayer stack is formed over a semiconductor substrate, the multilayer stack comprising alternating semiconductor layers and dummy layers; The multilayer stack is patterned to form a fin, wherein the fin comprises alternating semiconductor nanostructures and pseudo-nanostructures, the semiconductor nanostructures being defined by the semiconductor layers and the pseudo-nanostructures being defined by the pseudo layers; A lower source / drain region is formed, wherein the lower semiconductor nanostructure of the semiconductor nanostructure extends between the lower source / drain regions; An upper source / drain region is formed above the lower source / drain region, wherein the upper semiconductor nanostructure of the semiconductor nanostructure extends between the upper source / drain regions; The pseudo-nanostructure is removed to form a first opening between the lower semiconductor nanostructures and a second opening between the upper semiconductor nanostructures; A first metal-containing layer is formed around the upper semiconductor nanostructure and in the second opening; A first passivation layer is formed on the surface of the first metal-containing layer; and A lower gate stack is formed around the lower semiconductor nanostructure and in the first opening.

10. A semiconductor device, comprising: Multiple first nanostructures extend between first source / drain regions; Multiple second nanostructures are located above the multiple first nanostructures, and the multiple second nanostructures extend between the second source / drain regions; An isolation structure is located between the plurality of first nanostructures and the plurality of second nanostructures; A first gate stack is located around the plurality of first nanostructures; as well as A second gate stack is located above the first gate stack and disposed around the plurality of second nanostructures, wherein the second gate stack includes: A first metal-containing layer is located around the plurality of second nanostructures; A second metal-containing layer is located above the first metal-containing layer and around the second nanostructures of the plurality of second nanostructures; and A first gate electrode layer is located above the first metal-containing layer and the second metal-containing layer, wherein the sidewalls of the first metal-containing layer and the second metal-containing layer are adjacent to the sidewalls of the isolation structure.