Preparation method of high-sensitivity room-temperature flexible hydrogen sulfide gas sensor
By using laser direct writing to prepare LIG electrodes combined with WO3-SDS composite gas-sensitive layers, the problems of low sensitivity, poor flexibility, and complex fabrication of existing hydrogen sulfide gas sensors have been solved. This has resulted in a highly sensitive and flexible room temperature hydrogen sulfide gas sensor suitable for wearable devices and complex curved surface bonding.
Patent Information
- Application Number
- CN202610067105.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-01-19
- Publication Date
- 2026-04-14
AI Technical Summary
Existing hydrogen sulfide gas sensors suffer from problems such as high operating temperature, low sensitivity, slow response recovery, poor flexibility, complex manufacturing process, high cost, and limited applicability, making it difficult to meet the application requirements of wearable devices and complex curved surfaces.
A highly sensitive and flexible hydrogen sulfide gas sensor was fabricated by laser direct writing, combined with a WO3-SDS composite gas-sensitive layer, and through a PN heterojunction and a three-dimensional porous structure.
It achieves high-sensitivity detection at room temperature, with a 30% increase in sensitivity. It also boasts excellent flexibility, simple preparation, good long-term stability, suitability for wearable devices, low cost, and suitability for large-scale production.
Smart Images

Figure CN121856336A_ABST
Abstract
Description
Technical Field This invention belongs to the field of sensor technology, specifically relating to a method for preparing a highly sensitive room-temperature flexible hydrogen sulfide gas sensor, which is suitable for the accurate detection of low-concentration hydrogen sulfide gas at room temperature, and is particularly suitable for flexible electronics, wearable devices and other scenarios. Background Technology
[0001] Hydrogen sulfide is a highly toxic and flammable harmful gas widely found in industries such as chemical, mining, and wastewater treatment. It is also a biomarker for oral diseases, making its highly sensitive detection crucial for safe production and health monitoring. Traditional hydrogen sulfide gas sensors are mostly based on metal oxide materials, which suffer from high operating temperatures (200 to 400 °C), low sensitivity, and slow response recovery. While existing graphene-based sensors can operate at room temperature, their lack of flexibility and complex fabrication processes make them unsuitable for wearable applications and complex curved surface fitting.
[0002] CN104819976A discloses an electrochemiluminescence paper chip and its application in hydrogen sulfide detection. This method involves preparing hydrophobic and hydrophilic regions and hollow channels on filter paper using wax printing technology, screen printing a three-electrode system, and functionalizing the working electrode with 3D-GN-Au@Pd alloy nanoparticles. This method has advantages such as low cost, portability, high detection sensitivity, and low sample consumption. However, this method relies on modification with noble metal nanoparticles and graphene quantum dots, resulting in high raw material costs. Preparation requires complex steps such as autoclave heating and freeze-drying, leading to low batch production efficiency. Furthermore, the electrochemiluminescence signal is easily affected by environmental humidity, and the active sites on the electrodes are prone to failure after long-term use.
[0003] CN113049646A discloses a hydrogen sulfide sensor based on a Cu7S4-CuO hierarchical micron-flower sensitive material and its fabrication method. This method uses an Al2O3 ceramic tube with a ring-shaped gold electrode as a substrate, coated with Cu7S4-CuO micron-flower sensitive material, and incorporates a nickel-chromium alloy heating coil to form a side-heated structure. This method offers advantages such as high sensitivity (response value 156 at 50 ppm), low detection limit (as low as 50 ppb), good long-term stability, simple process, and suitability for mass production. However, this method uses a rigid ceramic tube substrate, lacking flexibility and wearability, relies on the heating coil for operation, resulting in high energy consumption, making it unusable in scenarios without an external power source, and the ceramic substrate is prone to cracking, limiting its environmental adaptability.
[0004] CN110108670B discloses a hydrogen sulfide sensor based on a thin-core optical fiber with a thin-film coating and its fabrication method. This method detects hydrogen sulfide concentration by coating a sensitive thin film on the surface of the thin-core optical fiber, and then combining it with a Faraday polarizer, an optical fiber circulator, and a spectrometer, utilizing spectral changes. This method has advantages such as simple structure, stable operation, fast response, high detection accuracy, small size, and light weight. However, this method relies on precise optical fiber fabrication processes, the thin-film coating is prone to wear and peeling, long-term stability is insufficient, and the optical fiber material has poor flexibility and high cost. Furthermore, the detection process is easily affected by ambient light interference, making it unsuitable for mass deployment under complex operating conditions.
[0005] Existing flexible gas sensors rely heavily on complex chemical modification or template methods, resulting in low raw material utilization, poor process repeatability, and high costs. LIG technology, through a single laser direct writing process, can fabricate three-dimensional porous graphene on polymer substrates, offering advantages such as ease of fabrication, excellent flexibility, and large specific surface area. Tungsten trioxide (WO3), a typical metal oxide gas-sensitive material, exhibits good selectivity for hydrogen sulfide, but its use alone suffers from poor dispersibility and insufficient response. Therefore, combining WO3 with LIG to leverage the advantages of both to fabricate a highly sensitive and flexible hydrogen sulfide gas sensor at room temperature is key to overcoming the current technological bottlenecks. Summary of the Invention: In view of the shortcomings of the prior art, the technical problem to be solved by the present invention is to provide a method for preparing a highly sensitive room temperature flexible hydrogen sulfide gas sensor. The method involves preparing a LIG flexible electrode by laser direct writing and combining it with a WO3-SDS composite gas-sensitive layer. The prepared flexible hydrogen sulfide gas sensor has the advantages of high sensitivity, simple preparation, long-term stability, and room temperature detection.
[0006] This invention is achieved using the following technical solution: Step 1: Fabrication of LIG interdigitated electrodes (1) Select a polyimide (PI) film with a thickness of 70-80μm, wipe the surface with anhydrous ethanol to remove impurities, and then let it air dry naturally; (2) Fix the dried PI film onto the glass slide with water-soluble tape to ensure that the film is flat and wrinkle-free; (3) A carbon dioxide laser with a wavelength of 10.6 μm is used, with a laser power of 8.2-10 W, a scanning speed of 50-80 mm / s, an image density of 400-600 PPI, and a focal length of 0-0.5 mm. The PI film is scanned along the preset interdigitated pattern in grating mode to induce the PI film to pyrolyze into a three-dimensional porous LIG, forming interdigitated electrodes (interdigitated width 0.3-1.0 mm, interdigitated spacing 0.3-0.8 mm). (4) Immerse the glass slide in clean water to dissolve the water-soluble adhesive tape, peel it off to obtain the flexible LIG interdigitated electrode, and dry it for later use.
[0007] Step 2: Preparation of WO3-SDS suspension (1) Weigh SDS and WO3 powder (WO3 particle size 1-5 μm) at a mass ratio of 1:50-1:70. (2) Add SDS to deionized water (1-1.5 g of deionized water for every 0.025 g of SDS), stir magnetically for 10-15 min until completely dissolved, and then disperse ultrasonically for 3-5 min; (3) Add the weighed WO3 powder, first ultrasonically disperse for 20-40 min, then disperse for 30-60 min using a high-speed disperser at a speed of 10000-20000 rad / min to obtain a uniform suspension with a WO3 mass concentration of 1.2-1.8 g / mL.
[0008] Step 3: Coating and molding of the gas-sensitive layer A precision pipette was used to quantitatively drop WO3-SDS suspension onto the surface of the LIG interdigitated electrode, with 0.1-0.2 mL of suspension dropped per square centimeter of electrode. Place the electrode after drop coating in a four-sided press, control the thickness of the gas-sensitive layer to be 120-180 μm, maintain the pressure at 10-20 psi, and let it stand for 5-10 min. The electrodes were dried in an oven at 60-80 ℃ for 1-2 h and then naturally cooled to room temperature to obtain a highly sensitive room temperature flexible hydrogen sulfide gas sensor.
[0009] Compared with the prior art, the beneficial effects of the present invention are as follows: High sensitivity at room temperature: By forming a PN heterojunction with WO3 and LIG, combined with the three-dimensional porous structure of LIG and SDS dispersion optimization, the sensor achieves a response of 24% to 20 ppb hydrogen sulfide at room temperature, with a theoretical detection limit of 744 ppt and an actual detection limit of 3 ppb, improving sensitivity by 30% compared to traditional sensors; Excellent flexibility: The LIG electrode based on 70-80 μm PI film has good flexibility and mechanical stability. The sensor capability is not significantly changed when the radius of curvature is 30 mm. It can fit complex curved surfaces and is suitable for wearable device scenarios. Simple preparation: The laser direct writing and drop-coating lamination process is integrated, requiring no complex equipment, with good process repeatability, suitable for large-scale production, and low cost per piece, less than 0.1 yuan; High stability: The gas-sensitive layer has a uniform structure, and the sensor has a long-term stability of more than seven months. The response and recovery times are 32 seconds and 78 seconds, respectively, which are better than the response time of 78 seconds and the recovery time of 90 seconds of flexible sensors on the market. Attached Figure Description
[0010] Figure 1 A schematic flowchart illustrating the fabrication method of a highly sensitive room-temperature flexible hydrogen sulfide gas sensor; Figure 2 This is a schematic diagram of the LIG electrode of the flexible hydrogen sulfide gas sensor in the experimental example of the present invention; Figure 3 This is a schematic diagram illustrating the flexibility of the flexible hydrogen sulfide gas sensor in the experimental examples of this invention. Figure 4 This is a response curve of the flexible hydrogen sulfide gas sensor in the experimental example of the present invention under 20 ppb hydrogen sulfide. Figure 5 This is a repeatability response curve of the flexible hydrogen sulfide gas sensor in the experimental example of the present invention under 20 ppb hydrogen sulfide. Figure 6 This is a continuity curve of the flexible hydrogen sulfide gas sensor in the experimental example of the present invention under 20-100 ppb hydrogen sulfide conditions; Figure 7 This is a graph showing the long-term stability of the flexible hydrogen sulfide gas sensor in the experimental example of this invention under 20 ppb hydrogen sulfide for seven months. Detailed Implementation
[0011] To make the objectives, technical solutions, and effects of this invention clearer and more explicit, the invention is further described in detail below. It should be understood that the specific embodiments described herein are for illustrative purposes only and are not intended to limit the scope of the invention. Unless otherwise specified, all technical methods used are common in this field.
[0012] This invention relates to a process method for a highly sensitive room-temperature flexible hydrogen sulfide gas sensor, the detailed steps of which are as follows: Figure 1 As shown, the steps of this method are: Step 1: Use software such as AutoCAD to draw the interdigitated electrodes; Step 2: Mass fabrication of LIG interdigitated electrodes on selected PI substrates using a CO2 laser. Step 3: Prepare SDS-WO3 solution; Step 4: Use a pipette to cast the suspension droplets obtained in step 3 onto the interdigitated electrodes.
[0013] Step 5: Use a four-sided press to press the suspension layer on the interdigitated electrodes, controlling the film thickness to 150 μm. Step 6: Place the sample in an 80°C drying oven for 10 minutes to complete the preparation of the hydrogen sulfide gas sensor.
[0014] In step 2, the thickness of the PI film is 75 μm.
[0015] In step 3, 0.025 g of sodium dodecyl sulfonate (SDS) is dissolved in 1 g of deionized water, and then 1.5 g of trioxide powder is added and the solution is sonicated for 30 minutes to obtain an SDS-WO3 solution.
[0016] Experimental Example Figure 2 This is a schematic diagram of the LIG electrode of the flexible hydrogen sulfide gas sensor in the experimental example of the present invention. Its line width is set to 0.5 mm, the width of the interdigitated electrode is set to 7.5 mm, and the length is set to 7.5 mm.
[0017] Figure 3 This is a schematic diagram demonstrating the flexibility of the flexible hydrogen sulfide gas sensor in the experimental examples of this invention. To fabricate a flexible laser-induced graphene interdigitated electrode based on a polyimide (PI) film, this study used water-soluble tape to fix the PI film onto a glass slide. After the LIG interdigitated electrode was fabricated on the PI film surface, the entire glass slide was immersed in water, causing the water-soluble tape on the back of the PI film to dissolve. This process did not damage the formed LIG interdigitated electrode. Through this method, the PI film could be easily peeled off the glass slide, thus obtaining a flexible interdigitated electrode with good mechanical properties.
[0018] Figure 4 This is a response curve of the flexible hydrogen sulfide gas sensor in the experimental example of this invention under 20 ppb hydrogen sulfide. Figure 4 It is known that when the sensor shows a response of -24% to 20 ppb of hydrogen sulfide gas, the time required to reach 90% of the final response, i.e., -21.6%, is recorded as the response time. This response time is 32 seconds, and the recovery time is 78 seconds.
[0019] Figure 5 This is a repeatability response curve of the flexible hydrogen sulfide gas sensor in the experimental example of this invention under 20 ppb hydrogen sulfide. Figure 5 It can be seen that in the five repeated experiments, the response of the sensor to 20 ppb hydrogen sulfide gas was almost completely consistent, and the time required for the sensor's resistance value to recover to close to the initial state after being removed from the hydrogen sulfide gas environment was 90%, showing high consistency and stability.
[0020] Figure 6The graph shows the continuous response curve of the flexible hydrogen sulfide gas sensor in the experimental example of this invention under 20-100 ppb hydrogen sulfide concentrations. The sensor was continuously placed in H2S gas environments with different concentrations (20 ppb, 40 ppb, 60 ppb, 80 ppb and 100 ppb). As the H2S gas concentration gradually increased, the absolute values of the sensor's response were 29%, 32%, 36%, 39% and 43%, respectively, which indicates that the sensor exhibits excellent dynamic response characteristics under room temperature conditions.
[0021] Figure 7 This is a long-term stability curve of the flexible hydrogen sulfide gas sensor in the experimental example of this invention under 20 ppb hydrogen sulfide for seven months. The results show that during the continuous testing for seven months, the sensor's response to 20 ppb hydrogen sulfide gas remained basically stable at around -24%. This demonstrates the sensor's excellent time stability.
[0022] It should be understood that the above embodiments are merely illustrative of specific implementations of the present invention and are not intended to limit the scope of the present invention. Those skilled in the art can make improvements or modifications based on the above description, and all such changes and modifications should fall within the protection scope of the appended claims.
[0023] Any aspects not covered in this invention are applicable to existing technologies.
[0024] Comparative Example 1: Using the preparation method described in claim 1, only the laser processing parameters in step 1 were changed: the laser power was set to 7 W (below the optimal range of 8.2-10 W), and the scanning speed was set to 90 mm / s (above the optimal range of 50-80 mm / s). All other parameters remained unchanged, and LIG interdigitated electrodes and sensors were prepared. Test results showed that due to insufficient laser power and excessively fast scanning speed, the PI film pyrolysis was incomplete, resulting in a sparse porous structure and poor conductivity in the generated LIG interdigitated electrodes. The resistance per unit length of the interdigitated electrodes reached hundreds of kilohms. The WO3-SDS gas-sensitive layer was not tightly bonded to the LIG electrode, and the sensor's response under 20 ppb hydrogen sulfide gas was only 8%, a decrease of 66.7% compared to the sensor prepared with the optimal parameters. The actual detection limit increased to 25 ppb, and after three repeated tests, the response fluctuated by more than 15%, failing to meet the detection requirements in terms of repeatability and stability.
[0025] Comparative Example 2: Using the preparation method described in claim 1, only the laser processing parameters in step 1 were changed: the laser power was set to 12 W (higher than the optimal range of 8.2-10 W), and the scanning speed was set to 40 mm / s (lower than the optimal range of 50-80 mm / s). All other parameters remained unchanged, and LIG interdigitated electrodes and sensors were prepared. Test results showed that excessively high laser power and excessively slow scanning speed led to localized overheating and excessive carbonization of the PI film, resulting in molten agglomeration on the surface of the LIG interdigitated electrodes. The interdigital spacing was filled with carbides, and some areas experienced short circuits. Obvious cracks were found after coating the gas-sensitive layer. The sensor showed no effective response to 20 ppb hydrogen sulfide at room temperature, with almost no change in resistance, completely losing its gas-sensing detection function.
[0026] Comparative Example 3: Using the preparation method described in claim 1, except for omitting the four-sided film pressing thickness control step in step 3, the WO3-SDS suspension was directly drop-coated onto the LIG electrode surface and then allowed to air dry (the gas-sensitive layer thickness was approximately 250 μm, exceeding the optimal range of 120-180 μm). All other parameters remained unchanged, and the sensor was prepared. Test results showed that the gas-sensitive layer thickness was too large and uneven, exhibiting obvious porosity and delamination, significantly increasing the hydrogen sulfide gas diffusion resistance. The sensor's response to 20 ppb hydrogen sulfide was 13%, a decrease of 45.8% compared to the sensor prepared with the optimal parameters. The response time was extended to 58 s, and the recovery time was extended to 110 s. Under bending conditions (bending radius 5 mm), the response further decreased to 7%, and irreversible resistance drift occurred, failing to meet reliability requirements for flexible applications.
Claims
1. A method for fabricating a highly sensitive room-temperature flexible hydrogen sulfide gas sensor, characterized in that, Includes the following steps: Step 1: Fabrication of laser-induced graphene interdigitated electrodes: A polyimide film is fixed on a glass slide, and LIG interdigitated electrodes are fabricated on the surface of the PI film using direct writing techniques such as carbon dioxide laser, ultraviolet light, and femtosecond laser. The carbon dioxide laser processing parameters are power 8.2-10 W, scanning speed 50-80 mm / s, and image density 400-600 PPI. Step 2: Preparation of WO3-SDS suspension: Dissolve sodium dodecyl sulfonate dispersant in deionized water, stir until dissolved, add tungsten trioxide powder, and then perform ultrasonic dispersion and high-speed dispersion treatment to obtain a uniform and stable WO3-SDS suspension; Step 3, Gas-sensitive layer coating and molding: The suspension from step (2) is drop-coated onto the surface of the LIG interdigitated electrode from step (1). The thickness of the gas-sensitive layer is controlled by a four-sided press, and then dried to obtain a highly sensitive room temperature flexible hydrogen sulfide gas sensor.
2. The method for preparing a highly sensitive room-temperature flexible hydrogen sulfide gas sensor according to claim 1, characterized in that, The PI film in step 1 has a thickness of 70-80 μm, a focal length of 0-0.5 mm for laser direct writing, and is processed in grating mode.
3. The method for preparing a highly sensitive room-temperature flexible hydrogen sulfide gas sensor according to claim 1, characterized in that, Before laser direct writing in step 1, the PI film needs to be cleaned with anhydrous ethanol and dried before laser processing.
4. The method for preparing a highly sensitive room-temperature flexible hydrogen sulfide gas sensor according to claim 1, characterized in that, The LIG interdigitated electrode prepared in step 1 has an interdigitated width of 0.3-1.0 mm, an interdigitated spacing of 0.3-0.8 mm, and an electrode thickness of 5-10 μm.
5. The method for preparing a highly sensitive room-temperature flexible hydrogen sulfide gas sensor according to claim 1, characterized in that, In step 2, the mass ratio of SDS to WO3 is 1:50-1:70, and the mass ratio of SDS to deionized water is 0.025 g:1-1.5 g; the ultrasonic dispersion time is 20-40 min, the high-speed dispersion speed is 10000-20000 rad / min, and the dispersion time is 30-60 min.
Citation Information
Patent Citations
Preparation of electrochemical luminescence paper chip and application of chip in hydrogen sulfide detection
CN104819976A
Fabrication method of hydrogen sulfide sensor based on coated thin-core optical fiber, and detection method of the sensor and hydrogen sulfide gas concentration.
CN110108670B
Hydrogen sulfide sensor based on Cu7S4-CuO hierarchical structure micron flower sensitive material and preparation method thereof
CN113049646A