Thermal barrier coating temperature and stress coupling test system and method
By co-doping Dy3+ and Cr3+ in the thermal barrier coating, and using 355nm and 532nm lasers to excite phosphorescence and fluorescence signals respectively, a spectroscopic optical path and data processing system were designed to realize real-time, in-situ, non-contact two-dimensional distribution measurement of temperature and stress in the thermal barrier coating. This solved the problem of spectral interference in the existing technology and improved the test accuracy.
Patent Information
- Application Number
- CN202610158528.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-02-04
- Publication Date
- 2026-04-24
AI Technical Summary
Existing technologies cannot achieve in-situ coordinated testing of temperature and stress in thermal barrier coatings, and spectroscopic measurement methods are easily affected by the coupling of temperature and stress, resulting in insufficient test accuracy.
A 355nm and 532nm laser was emitted using an excitation system. Combined with a phosphorescence/fluorescence spectroscopic optical path and acquisition system, phosphorescence and fluorescence signals were acquired through a YSZ coating co-doped with Dy3+ and Cr3+. Taking advantage of the fact that Dy3+ temperature measurement is not affected by stress and Cr3+ fluorescence signal is affected by temperature, a spectroscopic optical path and data processing system were designed to achieve decoupled measurement of temperature and stress.
It enables real-time, in-situ, non-contact two-dimensional distribution measurement of temperature and stress in thermal barrier coatings, solves the problem of spectral interference, and improves test accuracy.
Smart Images

Figure CN121916997A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of non-contact temperature and stress detection technology, specifically to a temperature and stress coupling testing system and method for thermal barrier coatings. Background Technology
[0002] With the continuous improvement of aero-engine performance, the required temperature of the turbine inlet gas is increasing, and the working environment of hot-end components is becoming increasingly harsh. Therefore, the necessity of using thermal barrier coatings for thermal protection of hot-end components has become increasingly prominent. A thermal barrier coating is a functional coating system used to protect the hot-end components of an aero-engine. The outermost layer is a ceramic layer, which, with its excellent thermal insulation properties, blocks the conduction of high temperatures to the substrate and is the core of achieving the thermal insulation function. However, the thermal expansion coefficients of ceramic and metal substrates differ significantly. Under high-temperature cycling, thermal stress can easily cause the ceramic layer to crack and detach. Therefore, an adhesive layer is usually added between the two. This layer can firmly bond the ceramic layer and the metal substrate, and its own properties can buffer the mismatch in thermal expansion coefficients, effectively alleviating thermal stress and ensuring the long-term stability and service life of the entire coating system in high-temperature environments.
[0003] In the high-temperature service environment of aero-engines, the high temperature environment can easily cause thermal barrier coatings to fail due to overheating. In addition, rapidly changing temperature boundaries and significant temperature gradients will cause large changes in thermal stress within the thermal barrier coating, ultimately leading to the failure and spalling of the thermal barrier coating. Therefore, realizing online coupled testing of thermal barrier coating temperature and stress is of great significance for the performance evaluation and life prediction of aero-engine thermal barrier coatings and hot-end components.
[0004] By analyzing the characteristics of existing non-contact testing solutions for temperature and stress, and considering the testing requirements for temperature and stress in thermal barrier coatings, the following drawbacks of existing solutions were identified: Main drawback: Existing solutions cannot achieve in-situ coordinated testing of temperature and stress in thermal barrier coatings. Existing solutions can only measure a single temperature or stress parameter and cannot simultaneously acquire temperature and stress information of the thermal barrier coating, especially failing to accurately measure the two-dimensional distribution of temperature and stress at specific locations within the thermal barrier coating.
[0005] Other drawbacks: Existing methods for measuring temperature or stress using spectroscopy, such as phosphorescence thermometry and PLPS, are susceptible to the coupling effect of temperature and stress on spectral information. For example, in phosphorescence thermometry, the operating wavelength of some phosphorescent ions, such as Eu3+, Tb3+, and Sm3+, is shifted by the stress in their environment. Similarly, in PLPS, the center wavelength of the characteristic peak of the tested ion is shifted not only by the stress in its environment but also by the increase in temperature, moving towards shorter wavelengths. Since the effects of temperature and stress on spectral characteristics are difficult to separate precisely, this directly affects the measurement accuracy, and currently there is no effective decoupling method.
[0006] To address the aforementioned issues, there is an urgent need for a temperature and stress coupling testing system and method for thermal barrier coatings, which can solve the problems associated with traditional methods. Summary of the Invention
[0007] The purpose of this invention is to provide a temperature and stress coupling testing system and method for thermal barrier coatings, which solves the problem of mutual interference between the temperature and stress coupling effects of thermal barrier coatings during testing, and solves the problem that the existing technology cannot perform real-time, in-situ, coordinated, and non-contact testing of the temperature and stress of thermal barrier coatings.
[0008] To achieve the above objectives, the technical solution adopted by the present invention is as follows: A temperature and stress coupling testing system for thermal barrier coatings includes an excitation light system, an excitation light transmission system, a phosphorescence / fluorescence spectrophotometer and acquisition system, and a data processing system. The excitation light system emits 355nm and 532nm lasers. The excitation light transmission system inputs the 355nm and 532nm lasers onto the thermal barrier coating of the sample. The phosphorescence / fluorescence spectrophotometer and acquisition system splits the light signal emitted by the thermal barrier coating into phosphorescence and fluorescence, and acquires the signals. The data processing system calculates the temperature field and stress field of the thermal barrier coating based on the acquired phosphorescence and fluorescence signals.
[0009] Furthermore, the excitation system includes a 355nm laser and a 532nm laser.
[0010] Furthermore, the excitation light transmission system includes a 355nm laser reflector, a first 532nm laser reflector, a second 532nm laser reflector, and a first dichroic mirror. The 355nm laser emits a 355nm laser beam, which is reflected by the 355nm laser reflector and then shines perpendicularly onto the surface of the first dichroic mirror. The 532nm laser emits a 532nm laser beam, which is reflected by the first 532nm laser reflector and then shines obliquely onto the thermal barrier coating. The 532nm laser beam is reflected at the same point as the 355nm laser beam reflected by the first dichroic mirror.
[0011] Furthermore, the angle between the 532nm laser irradiating the thermal barrier coating and the vertical direction is less than 30°.
[0012] Furthermore, the phosphorescence / fluorescence spectroscopic optical path and acquisition system includes a second dichroic mirror, a lens, a first filter, a reflector, a second filter, a first hyperspectral camera, and a second hyperspectral camera. The light signal excited by the thermal barrier coating enters the first filter through the first dichroic mirror, filtering out stray light below 400nm, and then enters the second dichroic mirror through the lens. Among them, the light of 440nm-520nm enters the first hyperspectral camera through the second dichroic mirror, and the light above 520nm is reflected by the second dichroic mirror to the reflector, and then reflected by the reflector to the second filter, filtering out light in the band below 600nm, and finally enters the second hyperspectral camera. The first hyperspectral camera acquires the phosphorescence signal of YSZ:Dy, and the second hyperspectral camera acquires the fluorescence signal of YSZ:Cr. The first and second hyperspectral cameras are connected to the data processing system for sending the acquired signals to the data processing system.
[0013] This invention also provides a method for testing the temperature and stress coupling of thermal barrier coatings, applied to the aforementioned temperature and stress coupling testing system for thermal barrier coatings, comprising: Step 1: Prepare a thermal barrier coating on the sample; Step 2: Place the sample inside the system and perform temperature-stress coupling tests based on the system.
[0014] Further, in step 1, a thermal barrier coating is prepared on the sample, specifically as follows: Dy 3+ With Cr 3+ YSZ:Dy,Cr is co-doped into a yttrium oxide-stabilized zirconia thermal barrier coating to form a YSZ:Dy,Cr coating. YSZ:Dy,Cr was sprayed onto the sample using atmospheric plasma spraying to prepare a thermal barrier coating for the sample.
[0015] Furthermore, in step 2, the sample is placed inside the system, and a temperature-stress coupling test is performed based on the system, specifically as follows: The sample is placed inside the system, and the system is calibrated and pretreated. After calibration, the system controls the simultaneous emission of 355nm and 532nm lasers, which illuminate the same position on the surface of the thermal barrier coating of the sample through the optical path. The phosphorescence signal of YSZ:Dy and the fluorescence signal of YSZ:Cr of the thermal barrier coating are collected by a hyperspectral camera. The working band intensity ratio matrix of YSZ:Dy and the wavelength shift matrix of the R1 characteristic peak of YSZ:Cr were calculated based on the phosphorescence signal of YSZ:Dy and the fluorescence signal of YSZ:Cr. The two matrices are converted into temperature field and stress field, respectively.
[0016] In summary, the present invention has at least one of the following beneficial technical effects: 1. This invention uses Dy 3+ With Cr 3+ Co-doped within the thermal barrier coating, the two-dimensional temperature and stress distribution of the thermal barrier coating is obtained based on the phosphorescence / fluorescence information of the two ions. Through high-precision decoupling of temperature and stress information, real-time in-situ non-contact testing of the two-dimensional temperature and stress distribution of the thermal barrier coating is achieved. Dy, an ion whose temperature measurement is unaffected by stress, is selected. 3+ As a thermometric ion, and its spectrum and Dy 3+ Cr in the non-overlapping region of the spectrum 3+ As a stress testing ion, it binds to Cr 3+ The correction of temperature interference to the R1 characteristic peak during stress testing solves the problem of mutual interference between the temperature and stress coupling effect of the thermal barrier coating on the test.
[0017] 2. This invention designs a system that accurately transmits 355nm and 532nm lasers to the surface of the coating to be tested, and collects the phosphorescence signal of YSZ:Dy and the fluorescence signal of YSZ:Cr respectively through two hyperspectral cameras, and finally outputs the temperature field and stress field of the thermal barrier coating, which solves the problem that the existing technology cannot perform real-time, in-situ, coordinated and non-contact testing of the temperature and stress of the thermal barrier coating. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the system of the present invention; Figure 2 This is a schematic flowchart of the method of the present invention; Figure 3 This is a schematic diagram of the thermal barrier coating structure. Reference numerals: 1. 355nm laser; 2. 532nm laser; 3. 355nm laser reflector; 4. First 532nm laser reflector; 5. Second 532nm laser reflector; 6. First dichroic mirror; 7. First filter; 8. Lens; 9. Second dichroic mirror; 10. First hyperspectral camera; 11. Reflector; 12. Second filter; 13. Second hyperspectral camera; 14. Computer. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention. Furthermore, the technical features involved in the various embodiments of this invention described below can be combined with each other as long as they do not conflict with each other.
[0020] like Figure 1As shown, this invention provides a temperature and stress coupling testing system for thermal barrier coatings, comprising: an excitation light system, an excitation light transmission system, a phosphorescence / fluorescence spectrophotometer and acquisition system, and a data processing system. The excitation light system is used to emit 355nm and 532nm lasers. The excitation light transmission system is used to input the 355nm and 532nm lasers onto the thermal barrier coating of the sample. The phosphorescence / fluorescence spectrophotometer and acquisition system is used to split the light signal emitted by the thermal barrier coating into phosphorescence and fluorescence, and to acquire the signals. The data processing system is used to calculate the temperature field and stress field of the thermal barrier coating based on the acquired phosphorescence and fluorescence signals.
[0021] The excitation system includes a 355nm laser 1 and a 532nm laser 2, in order to achieve the excitation of Dy in the thermal barrier coating. 3+ With Cr 3+ To achieve the best excitation effect, a 355nm laser (laser 1) and a 532nm laser (laser 2) were used to emit 355nm and 532nm lasers, respectively, to excite the two-element co-doped thermal barrier coating. The 355nm laser was used to excite Dy... 3+ It will not stimulate Cr 3+ 532nm laser is used to excite Cr 3+ It will not stimulate Dy 3+ .
[0022] The excitation light transmission system includes a 355nm laser reflector 3, a first 532nm laser reflector 4, a second 532nm laser reflector 5, and a first dichroic mirror 6. A beam splitter and a power meter can be additionally set according to specific needs. The two lasers output two circular Gaussian laser beams. After passing through the beam splitter (which can split the excitation beam into two optical paths with different intensities), part of the excitation light will be vertically reflected onto the surface of the power meter to monitor the fluctuation of the excitation light output energy. The other part of the excitation light passes directly through the beam splitter and then passes through the 355nm laser reflector 3 and the first 532nm laser reflector 4 respectively. A 355nm laser beam is reflected by a 355nm laser reflector 3 and then shines onto the surface of a first dichroic mirror 6 (which only allows wavelengths above 400nm to pass through and wavelengths below 400nm to be reflected). After reflection, the laser beam shines perpendicularly onto the surface. A 532nm laser beam is irradiated by a first 532nm laser reflector 4 and then by a second 532nm laser reflector 5. After reflection, the beam is obliquely incident on the thermal barrier coating (to ensure that the two laser beams are not blocked by optical elements, the 532nm laser beam is obliquely incident on the surface of the thermal barrier coating). The 532nm laser beam is incident on the same point as the 355nm laser beam reflected by the first dichroic mirror 6. The angle between the 532nm laser beam and the vertical direction when it irradiates the thermal barrier coating is as small as possible (±30°). A laser beam expander can be installed after the first 532nm laser reflector 4 according to specific needs. Adjusting its beam expansion ratio can change the size of the excitation beam on the coating surface.
[0023] To acquire the two-dimensional phosphorescence and fluorescence spectral information of the thermal barrier coating under test, the camera needs to be able to analyze the spectral information of each pixel. Therefore, a hyperspectral camera is used to acquire the light signal emitted by the thermal barrier coating. The hyperspectral camera performs spectral splitting on the light signal received by each pixel through gratings, filters, etc., and can analyze the 460nm and 494nm bands used for temperature measurement in the phosphorescence of YSZ:Dy and the R1 characteristic peak at 687nm used for stress measurement in the fluorescence signal of YSZ:Cr. In order to avoid the R1 characteristic peak of YSZ:Cr coinciding with the spectrum of YSZ:Dy when measuring stress shift, two hyperspectral cameras are used and a beam splitting path is designed. The phosphorescence / fluorescence spectrophotometric path and acquisition system includes a second dichroic mirror 9, a lens 8, a first filter 7, a reflector 11, a second filter 12, a first hyperspectral camera 10, and a second hyperspectral camera 13. The light signal excited by the thermal barrier coating passes through the first dichroic mirror and enters the first filter 7, filtering out stray light below 400nm. It then passes through the lens 8 and enters the second dichroic mirror 9. Light in the 440nm-520nm range (containing only the thermometric band) passes through the second dichroic mirror 9 and then into the first hyperspectral camera 10. Light above 520nm is filtered by the second dichroic mirror 9. The light is reflected onto mirror 11 and then onto the second filter 12, which filters out light below 600nm. The remaining light above 600nm (containing only the stress measurement band) finally enters the second hyperspectral camera 13. Through the design of the beam-splitting optical path, the first hyperspectral camera 10 collects the phosphorescence signal of YSZ:Dy, and the second hyperspectral camera 13 collects the fluorescence signal of YSZ:Cr. The first hyperspectral camera 10 and the second hyperspectral camera 13 are connected to the data processing system to send the collected signals. The camera shutter is triggered using an external trigger mode with a laser pulse signal.
[0024] The data processing system consists of a computer 14. The software system realizes the conversion between two-dimensional spectrum and temperature field and stress field based on the mapping relationship between light intensity ratio and temperature and R1 peak shift and stress, and finally obtains the two-dimensional temperature field and stress field of thermal barrier coating.
[0025] like Figure 2 As shown, the present invention also provides a method for testing the temperature and stress coupling of thermal barrier coatings, applied to the above-mentioned system, comprising: Step 1: Prepare a thermal barrier coating on the sample; Step 2: Place the sample inside the system and perform temperature-stress coupling tests based on the system.
[0026] In step 1, a thermal barrier coating is prepared on the sample, specifically as follows: Dy 3+ With Cr 3+ YSZ:Dy,Cr is co-doped into a yttrium oxide-stabilized zirconia thermal barrier coating to form a YSZ:Dy,Cr coating. YSZ:Dy,Cr was sprayed onto the sample using atmospheric plasma spraying to prepare a thermal barrier coating. The specific preparation process is as follows: 1. Clean the surface of the sample to be sprayed, and roughen the surface by means of sandblasting or other methods to improve the adhesion; 2. YSZ powder is fed into the plasma jet generated by the plasma gun. First, a bottom layer of pure YSZ coating is sprayed. Then, YSZ:Dy,Cr powder is fed into the jet to spray a middle layer of luminescent coating. Finally, YSZ powder is fed into the jet to spray a top layer of pure YSZ coating. 3. Inspect key coating properties, such as porosity and bonding strength, to ensure they meet usage requirements; The thermal barrier coating consists of three layers: a bottom layer of pure YSZ; a middle layer of YSZ:Dy,Cr co-doped layer, i.e., the luminescent layer; and a top layer of pure YSZ. The thicknesses δ1 and δ2 of the bottom and top layers of pure YSZ are controlled according to requirements to determine the location of YSZ:Dy,Cr within the thermal barrier coating, thus allowing selection of the target test location. Figure 3 The diagram shown is a schematic of the coating structure.
[0027] The testing principle of thermal barrier coatings will be explained next: This invention selects Dy 3+ As a temperature measuring element, the thermometric wavelengths are 460nm and 494nm. Phosphorescence in this wavelength range is generated by magnetic dipole transitions and is not affected by changes in stress state; that is, the temperature measurement is not affected by stress. Cr was selected as the appropriate element. 3+ As a stress testing ion, the test band is Cr. 3+ According to Wien's shift law, the R1 characteristic peak (center wavelength 687 nm) of the fluorescence spectrum shifts towards shorter wavelengths with increasing temperature. Therefore, interference correction techniques are needed to eliminate the influence of temperature on stress testing. The specific testing principle is as follows: 1. Temperature Testing Principle After being irradiated by a 355nm laser, the intensity ratio of the 460nm and 494nm bands in the phosphorescence spectrum emitted by Dy ions has a mapping relationship with temperature, as shown in formula (1): (1) In the formula, FIR Defined as light intensity ratio, I 1 and I 2 represents the light intensity at the 460nm and 494nm wavelengths, respectively; B It is a constant. This represents the energy difference between thermally coupled energy levels. This represents Boltzmann's constant. T Representing temperature, through multiple known... FIR and T At these points, a temperature measurement curve can be plotted, and thus... FIR and T The relationship between the curves is used to test the temperature at an unknown temperature. FIR By inputting the data into the temperature measurement curve, the temperature can be obtained, thus achieving the purpose of temperature measurement. 2. Stress Testing Principle When Cr ions are irradiated by a 532 nm laser, the center wavelength of the R1 characteristic peak in the emitted fluorescence spectrum will be affected by external stress, resulting in a blue shift or red shift. Specifically, a blue shift occurs under tensile stress, and a red shift occurs under compressive stress. The shifted wavelength Δ λ The relationship between stress and pressure is linear, as shown in equation (2): (2) In the formula, σ Stress, in MPa; Δ λ The offset of the center wavelength of the R1 characteristic peak from the center wavelength of the R1 characteristic peak of Cr ions under stress-free conditions is expressed in nm. π The constant is obtained by using multiple known methods under the condition that the coated samples are kept at the same temperature. σ and Δ λ By fitting the constant π to the point, a linear relationship can be obtained. Under a certain stress value of the coating, the Δ under that stress can be tested. λ The stress can be obtained from the fitted linear relationship, thus realizing stress measurement; 3. Principle of Temperature Interference Stress Measurement Correction Since the working peak of stress measurement is affected by temperature and shifts, it strongly interferes with the stress measurement results, so this interference must be corrected. The peak shift Δ of the R1 characteristic peak of Cr ions when only temperature is changed and no stress is applied. λ T With temperature change Δ TThere is a polynomial relationship between them, resulting in the modified relation shown in formula (3): (3) In the formula, Δ λ T The wavelength shifted from the R1 peak. α 1. α 2、...、α n Δ is a constant coefficient. T This represents the change in the temperature at which the Cr ions are located relative to the initial temperature before heating. Through multiple known Δ λ T Δ T A correction curve can be established from the points, and based on this curve, when the Cr ions are at a certain temperature, Δ T By substituting this value, we can obtain the R1 characteristic peak shift value Δ caused by the temperature effect of Cr ions. λ T .
[0028] In step 2, the sample is placed inside the system, and a temperature-stress coupling test is performed based on the system, specifically as follows: The sample is placed inside the system, and the system undergoes calibration pretreatment. Specifically, the calibration process is as follows: Before testing, it is necessary to first calibrate the "temperature-light intensity ratio" mapping relationship of YSZ:Dy and the "stress-R1 peak shift" mapping relationship of YSZ:Cr. 1. Temperature measurement calibration (1) Place the coating to be tested in the heating furnace and monitor the temperature using a standard thermocouple; (2) Turn on the heating furnace to heat the sample to be tested, and keep the temperature constant for a period of time every 50°C increase. Turn on the laser to emit a 355nm laser to excite the coating to be tested, and use a camera to take pictures of Dy. 3+ Two-dimensional phosphorescence spectrum, while simultaneously recording the standard thermocouple temperature as the actual temperature of the coating; (3) Use computer 14 to calculate Dy at each temperature 3+ The peak intensity ratio of 460nm and 494nm was obtained, and a series of scatter points were then substituted into formula (1) for fitting. After obtaining the constants B and ΔE, Dy was obtained. 3+ "Temperature-460nm / 494nm Peak Intensity Ratio" Mapping Curve; 2. Stress measurement calibration (1) Prepare a thermal barrier coating on the stripped substrate and place it on a stress loading stage; (2) First, tensile stress is applied, ranging from 0 to 100 MPa. The stress is maintained for every 5 MPa increase. The coating to be tested is excited by a 532 nm laser, and the Cr coating is photographed. 3+Two-dimensional fluorescence spectroscopy was performed; then, compressive stress was applied, ranging from -500 to 0 MPa (negative values represent compressive stress), with the stress maintained at 50 MPa increments. A 532 nm laser was then used to excite the coating under test, and images of the Cr coating were captured using a camera. 3+ Two-dimensional fluorescence spectroscopy; (3) Use computer 14 to calculate the shift of the R1 peak in the fluorescence spectrum captured under each stress, and the blue shift Δ λ Recorded as positive, Δ during redshift λ The result is denoted as negative. After obtaining a series of scattered points, the constant π is obtained by fitting the data into formula (2). 3. Calibration of the correction curve for temperature interference stress measurement (1) Prepare a thermal barrier coating on the stripped substrate, place it in a heating furnace, and monitor the temperature using a standard thermocouple; (2) Record the temperature of the coating before heating. T 1. From T The furnace was turned on to heat the sample to be tested from 1 to 1100°C, and the temperature was kept constant for a period of time in increments of 50°C. The laser was then turned on to emit a 532nm laser to excite the coating to be tested, and the Cr was photographed using a camera. 3+ Two-dimensional fluorescence spectroscopy was used, and the temperature of a standard thermocouple was recorded as the actual temperature of the coating. (3) Use computer 14 to calculate the R1 peak shift Δ in the fluorescence spectrum captured at each temperature. λ T And calculate the corresponding temperature and T Temperature difference Δ1 T After obtaining a series of scatter points, they are substituted into formula (3) to obtain constants α1, α2, ..., α3. n The correction curve can then be obtained.
[0029] After calibration, a temperature-stress coupling test of the thermal barrier coating is performed, which includes the following steps: 1. Trigger laser adjustment of the optical path and capture of phosphorescence and fluorescence: Use a computer to control the simultaneous emission of 355nm and 532nm lasers, and adjust the angles of the laser reflector and dichroic mirror so that both lasers irradiate the same position on the surface of the thermal barrier coating under test. Set the hyperspectral camera to external trigger mode, and use the laser pulse signal to control the shutter to expose during laser emission, and collect the two-dimensional YSZ:Dy phosphorescence and YSZ:Cr fluorescence signals of the coating; 2. Based on the two-dimensional YSZ:Dy phosphorescence and YSZ:Cr fluorescence signals obtained in the previous step, the computer 14 is used to obtain the light intensity ratio matrix of the YSZ:Dy working band and the wavelength shift matrix of the R1 characteristic peak of YSZ:Cr. Using the algorithm of the computer 14, the light intensities of the two peaks at 460nm and 494nm are compared at each pixel in the two-dimensional YSZ:Dy spectral image captured by the camera, and the wavelength difference Δ between the center wavelength of the R1 characteristic peak at each pixel in the two-dimensional YSZ:Cr spectral image and the center wavelength of the R1 characteristic peak under stress-free conditions (687nm) is calculated. λ (i.e., the wavelength shift of the R1 characteristic peak), and the intensity ratio matrix and the wavelength shift matrix of the R1 peak can be obtained respectively; 3. The two matrices are converted into temperature field and stress field respectively using computer 14; Temperature field: Based on the previously calibrated mapping relationship of "temperature-460nm / 494nm peak light intensity ratio" of YSZ:Dy, the light intensity ratio matrix calculated in the previous step is converted into a temperature matrix using the computer algorithm 14, thereby obtaining the temperature field of the thermal barrier coating to be tested. Stress field: First, based on the previously calibrated correction curve for temperature interference stress testing, the temperature change Δ of each pixel point relative to the initial temperature at the start of the calibration is calculated using the obtained temperature field. T The field is then substituted into the correction curve to obtain a corrected wavelength Δ. λ T The matrix, along with the calculated wavelength shift Δ of the R1 characteristic peak. λ Matrix subtraction is performed to correct for the temperature-induced shift of the R1 peak, resulting in the corrected matrix Δ. λ 'Matrix. Then, based on the previously calibrated linear function relationship of "stress-R1 characteristic peak shift wavelength" of YSZ:Cr, the computer 14 is used to calculate Δ λ The matrix is converted into a stress matrix to obtain the stress field of the thermal barrier coating under test.
[0030] Embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a completely hardware embodiment, a completely software embodiment, or an embodiment combining software and hardware aspects. Furthermore, the present invention may take the form of a computer program product embodied on one or more computer-usable storage media (including, but not limited to, disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.
[0031] This invention is described with reference to flowchart illustrations and / or block diagrams of methods, apparatus (systems), and computer program products according to embodiments of the invention. It will be understood that each block of the flowchart illustrations and / or block diagrams, and combinations of blocks in the flowchart illustrations and / or block diagrams, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, special-purpose computer, embedded processor, or other programmable data processing apparatus to produce a machine, such that the instructions, which execute via the processor of the computer or other programmable data processing apparatus, generate instructions for implementing the flowchart illustrations and / or block diagrams. Figure 1 One or more processes and / or boxes Figure 1 A device that provides the functions specified in one or more boxes.
[0032] These computer program instructions may also be stored in a computer-readable storage medium that can direct a computer or other programmable data processing device to function in a particular manner, such that the instructions stored in the computer-readable storage medium produce an article of manufacture including instruction means, which are implemented in a process Figure 1 One or more processes and / or boxes Figure 1 The function specified in one or more boxes.
[0033] These computer program instructions may also be loaded onto a computer or other programmable data processing equipment to cause a series of operational steps to be performed on the computer or other programmable equipment to produce a computer-implemented process, thereby providing instructions that execute on the computer or other programmable equipment for implementing the process. Figure 1 One or more processes and / or boxes Figure 1 The steps of the function specified in one or more boxes.
[0034] Contents not described in detail in this specification are prior art known to those skilled in the art. It is hereby indicated that the above description is intended to help those skilled in the art understand this invention, but does not limit the scope of protection of this invention. Any equivalent substitutions, modifications, improvements, or simplifications of the above descriptions that do not depart from the essential content of this invention fall within the scope of protection of this invention.
Claims
1. A temperature and stress coupling testing system for thermal barrier coatings, characterized in that, include: The system comprises an excitation light system, an excitation light transmission system, a phosphorescence / fluorescence spectrophotometer and acquisition system, and a data processing system. The excitation light system is used to emit 355nm and 532nm lasers. The excitation light transmission system is used to input the 355nm and 532nm lasers onto the thermal barrier coating of the sample. The phosphorescence / fluorescence spectrophotometer and acquisition system is used to split the light signal emitted by the thermal barrier coating into phosphorescence and fluorescence, and to acquire the signals. The data processing system is used to calculate the temperature field and stress field of the thermal barrier coating based on the acquired phosphorescence and fluorescence signals.
2. The temperature and stress coupling testing system for thermal barrier coatings according to claim 1, characterized in that, The excitation system includes a 355nm laser and a 532nm laser.
3. The temperature and stress coupling testing system for thermal barrier coatings according to claim 2, characterized in that, The excitation light transmission system includes a 355nm laser reflector, a first 532nm laser reflector, a second 532nm laser reflector, and a first dichroic mirror. The 355nm laser emits a 355nm laser beam, which is reflected by the 355nm laser reflector and then shines perpendicularly onto the surface of the first dichroic mirror. The 532nm laser emits a 532nm laser beam, which is reflected by the first 532nm laser reflector and then shines obliquely onto the thermal barrier coating. The 532nm laser beam is reflected at the same point as the 355nm laser beam reflected by the first dichroic mirror.
4. The temperature and stress coupling testing system for thermal barrier coatings according to claim 3, characterized in that, When the 532nm laser irradiates the thermal barrier coating, the angle between the laser and the vertical direction is less than 30°.
5. The temperature and stress coupling testing system for thermal barrier coatings according to claim 4, characterized in that, The phosphorescence / fluorescence spectroscopic optical path and acquisition system includes a second dichroic mirror, a lens, a first filter, a reflector, a second filter, a first hyperspectral camera, and a second hyperspectral camera. The light signal excited by the thermal barrier coating enters the first filter through the first dichroic mirror, filtering out stray light below 400nm. The light then enters the second dichroic mirror through the lens. Light in the 440nm-520nm range passes through the second dichroic mirror and then into the first hyperspectral camera. Light above 520nm is reflected by the second dichroic mirror onto the reflector, and then reflected by the reflector to the second filter, filtering out light below 600nm. Finally, the light enters the second hyperspectral camera. The first hyperspectral camera acquires the phosphorescence signal of YSZ:Dy, and the second hyperspectral camera acquires the fluorescence signal of YSZ:Cr. The first and second hyperspectral cameras are connected to the data processing system to send the acquired signals to the data processing system.
6. A method for testing the temperature and stress coupling of a thermal barrier coating, applied to the temperature and stress coupling testing system for thermal barrier coatings as described in any one of claims 1-5, characterized in that, include: Step 1: Prepare a thermal barrier coating on the sample; Step 2: Place the sample inside the system and perform temperature-stress coupling tests based on the system.
7. The method for testing the temperature and stress coupling of a thermal barrier coating according to claim 6, characterized in that, In step 1, a thermal barrier coating is prepared on the sample, specifically as follows: Dy 3+ With Cr 3+ YSZ:Dy,Cr is co-doped into a yttrium oxide-stabilized zirconia thermal barrier coating to form a YSZ:Dy,Cr coating. YSZ:Dy,Cr was sprayed onto the sample using atmospheric plasma spraying to prepare a thermal barrier coating for the sample.
8. The method for testing the temperature and stress coupling of a thermal barrier coating according to claim 7, characterized in that, In step 2, the sample is placed inside the system, and a temperature-stress coupling test is performed based on the system, specifically as follows: The sample is placed inside the system for calibration pretreatment. After calibration, the system controls the simultaneous emission of 355nm and 532nm lasers, which illuminate the same position on the surface of the thermal barrier coating of the sample through the optical path. The phosphorescence signal of YSZ:Dy and the fluorescence signal of YSZ:Cr of the thermal barrier coating are collected by a hyperspectral camera. The working band intensity ratio matrix of YSZ:Dy and the wavelength shift matrix of the R1 characteristic peak of YSZ:Cr were calculated based on the phosphorescence signal of YSZ:Dy and the fluorescence signal of YSZ:Cr. The two matrices are converted into temperature field and stress field, respectively.