Radiation-proof ultrathin p-type crystalline silicon cell and preparation method thereof
By integrating gallium doping and a composite back mirror structure, combined with a low-stress electrode system, the mechanical fragility and insufficient optical absorption of ultrathin crystalline silicon solar cells under space irradiation conditions were solved, resulting in improved battery performance with high efficiency and high stability.
Patent Information
- Application Number
- CN202610085474.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-01-22
- Publication Date
- 2026-04-24
AI Technical Summary
Existing technologies have failed to systematically solve the problems of mechanical fragility, insufficient optical absorption, and radiation resistance degradation in ultrathin crystalline silicon solar cells. In particular, under the high-energy particle irradiation environment in space, the boron-oxygen defects in traditional boron-doped solar cells lead to irreversible degradation of photoelectric conversion efficiency.
An integrated design employing a gallium-doped substrate, a composite back mirror structure, and a low-stress electrode system, combined with low-temperature processing, is used. This design includes a gallium-doped p-type single-crystal silicon substrate, a composite back mirror structure, and a flexible full-back electrode. Through selective emitters and stress-relieving trenches, a battery structure with low contact resistance and high optical path is formed.
It significantly improves the long-term stability and mechanical reliability of ultra-thin batteries under space irradiation environment, with a photoelectric conversion efficiency retention rate of over 83%, a mechanical fragmentation rate of less than 1.5%, and a doubling of optical absorption thickness, resulting in battery performance that comprehensively surpasses conventional products of the same thickness.
Smart Images

Figure CN121924837A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of photovoltaic device manufacturing technology, and relates to an ultra-thin p-type crystalline silicon cell resistant to radiation and its preparation method. Specifically, it relates to a p-type crystalline silicon cell with a thickness of 60-80 micrometers suitable for high-energy particle irradiation environments in space, which improves radiation resistance and mechanical reliability through gallium doping and low-stress composite structure, and its low-temperature preparation method. Background Technology
[0002] Thinning crystalline silicon photovoltaic cells (thickness ≤ 80 μm) is a key path to reducing the power-to-weight ratio (W / kg) and cost of space photovoltaic systems. However, thinning introduces a series of interconnected and severe challenges in terms of mechanics, optics, and radiation resistance. Mechanically, the stiffness of the thinner cells decreases due to a cubic relationship, making them prone to warping and breakage. Optically, insufficient absorption path length in the infrared band leads to current loss. Regarding radiation resistance, the boron-oxygen (BO) pair defects present in traditional boron (B)-doped cells can form severe carrier recombination centers under high-energy particle (e.g., electrons, protons) irradiation, resulting in irreversible degradation of photoelectric conversion efficiency. For ultra-thin cells, the reduced bulk thickness amplifies the recombination effect of radiation-induced defects, making the deterioration of radiation resistance a core bottleneck restricting their space applications.
[0003] Existing technologies typically employ isolated solutions, such as optimizing only the antireflective layer to improve initial efficiency, using thick gallium substrates to improve radiation resistance, or thinning the silicon wafer to reduce cost. None of these solutions systematically and collaboratively address the three mutually reinforcing problems of mechanical fragility, insufficient optical absorption, and radiation degradation at the architectural level of ultrathin batteries. In particular, current ultrathin battery technologies generally neglect radiation-sensitive material systems (such as boron doping) and the thermal stress introduced by high-temperature processes, resulting in unsatisfactory end-of-life (EOL) performance and reliability in space environments. Therefore, an integrated design and fabrication approach is urgently needed, incorporating systematic innovation in material selection, structural design, and process pathways to simultaneously achieve a balance between high efficiency, high mechanical yield, and high radiation resistance on ultrathin silicon wafers.
[0004] The information disclosed in this background section is intended only to enhance the understanding of the overall background of the present invention and should not be construed as an admission or in any way implying that the information constitutes prior art known to those skilled in the art. Summary of the Invention
[0005] To address the shortcomings of existing technologies, the present invention aims to provide a radiation-resistant ultrathin p-type crystalline silicon solar cell and its fabrication method. This cell, through an integrated design employing a gallium-doped substrate, a composite back mirror structure, and a low-stress electrode system, significantly improves long-term stability and mechanical reliability under space irradiation conditions while ensuring high conversion efficiency.
[0006] To achieve the above objectives, the present invention adopts the following technical solution: In a first aspect, the present invention provides a radiation-resistant ultrathin p-type crystalline silicon solar cell, comprising: p-type single-crystal silicon substrate with a thickness of 60~80 μm; A composite back mirror structure and a back metal electrode are sequentially disposed on the back side of a silicon substrate; A passivation and antireflection layer, a selective emitter, and a front metal electrode are sequentially disposed on the front side of a silicon substrate; in, The acceptor doping element of the p-type single-crystal silicon substrate is gallium (Ga), and its resistivity ranges from 1.0 to 3.0 Ω·cm.
[0007] The composite back mirror structure, from the inside out, includes: An ultrathin tunneling oxide layer with a thickness of 1.0~1.5 nm; The carrier selective transport layer consists of an intrinsic nanocrystalline silicon buffer layer directly deposited on an ultrathin tunneling oxide layer, and an in-situ phosphorus-doped polycrystalline silicon layer located above the buffer layer. The thickness of the buffer layer is 5–10 nm, and the thickness of the in-situ phosphorus-doped polycrystalline silicon layer is 15–30 nm, with a phosphorus atom concentration between 1 × 10⁻⁶. 19 cm -3 Up to 5×10 20 cm -3 Between them; the carrier-selective transport layer and the ultrathin tunneling oxide layer together form an electron-selective contact, which significantly reduces contact resistance and surface recombination; Wide bandgap dielectric light scattering layer, its material is magnesium-doped silicon nitride (SiN). x :Mg) or magnesium-doped silicon dioxide (SiO) x The silicon material has a refractive index of 2.0~2.4 and a thickness of 80~120 nm. Furthermore, the interface between this layer and the carrier selective transport layer is a light scattering interface with a randomly distributed array of nanoscale pits. The array of nanoscale pits randomly scatters long-wavelength light back into the silicon body, greatly enhancing the optical path. The selective emitter is composed of a stress-relieving trench that penetrates the front passivation antireflection layer and partially extends into the silicon substrate. The depth (D) of the trench and the thickness (T) of the silicon substrate satisfy the relationship: D = (8%~25%) × T, preferably 5~15 μm, and the width is 40~60 μm. A locally heavily doped region is formed on the inner surface of the trench, and the main gate portion of the front metal electrode fills the trench and forms an ohmic contact with the heavily doped region. Preferably, the dopant element in the heavily doped region is gallium, forming P ++ (Ga) heavily doped contact region.
[0008] The back metal electrode is a flexible full-back electrode that fully covers the wide bandgap dielectric light scattering layer. It is made of conductive composite material, in which thermoplastic polymer microspheres with a volume fraction of 5% to 15% and a particle size of 3 to 10 μm are uniformly dispersed. The front metal electrode uses a low-temperature conductive slurry with a curing peak temperature of no more than 380℃.
[0009] Preferably, the intrinsic nanocrystalline silicon buffer layer has a grain size of less than 15 nm, and its function is to adapt to the interface of the ultrathin tunneling oxide layer, release stress, and further passivate the interface state.
[0010] Preferably, the nanoscale pit array in the light scattering interface, with a pit depth of 50~100 nm, is induced at the interface after scanning the wide bandgap medium light scattering layer with a laser.
[0011] Preferably, in the flexible full-back electrode, the thermoplastic polymer microspheres are made of one of polyimide, polyamide, or acrylic resin.
[0012] In a second aspect, the present invention provides a method for preparing a radiation-resistant ultrathin p-type crystalline silicon solar cell as described in the first aspect, the method comprising the following steps: S1. Substrate Preparation and Texturing: Provide a gallium-doped p-type single-crystal silicon substrate with a resistivity of 1.0~3.0 Ω·cm and a thickness of 60~80 μm; use a potassium hydroxide (KOH) solution with a mass fraction of 0.5%~2% to anisotropically etch the substrate at 70~85℃ to form a random pyramid textured surface with a height of 0.8~1.5 μm on the front side of the substrate to optimize light capture, and form a nanoscale worm-like textured surface with a height of 300~800 nm on the back side of the substrate. The nanoscale worm-like textured surface increases light scattering and also provides a better adhesion interface for subsequent back film deposition. S2. Forming the front emitter: In a phosphorus-containing atmosphere, thermal diffusion is performed on the front side of the silicon substrate at 760~820 °C to form an n-type emitter with a sheet resistance of 90~110 Ω / □. + The emitter is then selectively wet-etched on the back side of the silicon substrate to remove the phosphosilicate glass and parasitic junctions formed during the diffusion process. S3. Deposition of functional thin films on the back side: On the back side of the silicon substrate, a silicon dioxide layer with a thickness of 1.0~1.5 nm is first grown as an ultrathin tunneling oxide layer using ultraviolet ozonochemical method at a temperature below 400℃; then, an intrinsic amorphous silicon layer with a thickness of 5~10 nm and an in-situ phosphorus-doped amorphous silicon layer with a thickness of 15~30 nm are deposited sequentially using plasma-enhanced chemical vapor deposition. S4. High-temperature annealing and crystallization: Under an inert gas protective atmosphere, the silicon wafer obtained in step S3 is annealed at 800~850 ℃ for 20~40 min, so that the intrinsic amorphous silicon layer and the phosphorus-doped amorphous silicon layer are simultaneously transformed into a polycrystalline silicon structure, forming a carrier selective transport layer and activating the phosphorus impurity. S5. Constructing the light scattering interface: A wide-bandgap dielectric light scattering layer is deposited on the carrier selective transport layer using plasma-enhanced chemical vapor deposition; subsequently, a pulsed laser with a wavelength of 515–532 nm is used at a speed of 0.8–1.2 J / cm². 2 The energy density was used to selectively scan the wide bandgap medium light scattering layer, inducing the formation of a random nano-pit array with a depth of 50~100 nm at the interface between it and the lower layer. S6. Deposit front passivation layer: On the front side of the silicon substrate, a silicon nitride layer with a thickness of 70~80 nm and a refractive index of 2.05~2.10 is deposited using plasma-enhanced chemical vapor deposition to serve as the front passivation and antireflection layer. S7. Preparation of selective emitter and stress relief trench: a) Grooving: Using a picosecond pulsed laser with a wavelength of 355 nm, the front passivation antireflection layer is ablated and removed along the preset main gate pattern position, and the silicon substrate is etched to form a trench with a depth of 5~15 μm and a width of 40~60 μm. b) Doping: A gallium-containing liquid dopant source is coated into the trench; a continuous wave or long-pulse laser with a wavelength of 780~1064 nm is used at a flux of 1.6~2.0 J / cm². 2 The energy density is scanned on the trench region coated with doped sources, causing the silicon material at the bottom of the trench to melt and recrystallize instantaneously, while simultaneously completing the doping and electroactivation of gallium atoms to form P. ++ (Ga) heavily doped contact region; S8. Forming local contacts on the back side: Using an infrared laser with a wavelength of 1064 nm, selectively ablate the wide bandgap dielectric light scattering layer and the carrier selective transport layer to expose the silicon region covered by an ultrathin tunneling oxide layer on the back side, forming a contact channel array with a linewidth of 15~25 μm. S9. Printing and Low-Temperature Co-curing Electrodes: A flexible conductive composite material is printed on the back side of the silicon substrate to form a fully covered back electrode; a low-temperature conductive paste is printed on the front side of the silicon substrate to form a front electrode pattern including a main grid and a fine grid, wherein the main grid is precisely aligned and covers the stress relief trench; finally, the printed battery is placed in a sintering furnace and held at a peak temperature of 360~380 ℃ for 60~150 s to allow the front and back electrodes to cure synchronously.
[0013] Preferably, in step S1, by controlling the concentration of the alkali solution and the corrosion time, the average aspect ratio (height / width) of the nanoscale worm-like texture on the back side is made greater than 1, so as to enhance the light trapping effect and film adhesion.
[0014] Preferably, in the doping process of step S7, the liquid doping source containing gallium is an organic solvent dilution of trimethylgallium or triethylgallium.
[0015] Preferably, in step S9, the flexible conductive composite material is prepared by mixing and dispersing silver-coated copper conductive filler, thermosetting resin and thermoplastic polymer microspheres.
[0016] Compared with existing technologies, this invention achieves a breakthrough in ultra-thin battery performance and has the following beneficial effects: Radiation resistance: This invention combines a gallium-doped substrate, a fully low-temperature process chain, and a composite back mirror passivation. Gallium doping fundamentally eliminates BO-type sensitive defect sources that cause radiation degradation; the low-temperature process (maximum temperature ≤850 °C) greatly suppresses the generation of thermally induced defects; the composite back mirror structure provides excellent surface passivation, minimizing the impact of radiation damage. The synergistic effect of these three factors enables the battery of this invention to withstand equivalent 1 MeV electrons and 1 × 10⁻⁶ ions of radiation. 15 cm -2 After standard space irradiation testing, the photoelectric conversion efficiency retention rate (EOL / BOL) can reach over 83%, which is more than 10 percentage points higher than that of traditional boron-doped PERC cells of the same thickness (typically below 75%), thus extending the on-orbit service life of satellites and other spacecraft.
[0017] Mechanical Reliability and Fabrication Yield: This invention employs a dual low-stress architecture consisting of stress-relief trenches and a flexible full-back electrode. The stress-relief trenches act as a mechanical fuse, effectively absorbing and dispersing concentrated stress generated during component lamination and subsequent encapsulation. The flexible full-back electrode provides overall buffering, suppressing crack initiation and propagation. Combined with rigorous control of thermal stress throughout the entire process, the total breakage rate of the 70 μm thick battery can be stably controlled below 1.5% on an industrial production line, and the warpage of the simulated laminated battery is less than 1.5 mm, meeting the rigid requirements for large-scale production of ultra-thin batteries.
[0018] Optical and electrical properties: The composite back mirror structure of this invention not only provides field-effect passivation, but also increases the back saturation current density. J oe ≤5 fA / cm 2 Its built-in laser-induced light scattering interface can reduce the internal reflectivity (R) of infrared photons with wavelengths above 1100 nm. int This increases the optical absorption capacity to over 95%, equivalent to more than doubling the optical absorption thickness of a 70 μm silicon wafer by more than 10 times, thereby increasing the short-circuit current density (J / L). sc It can exceed 40.5 mA / cm 2 Combined with the front P ++ (Ga) Selective contact results in low contact resistance and low open-circuit voltage (V) of the battery. oc The voltage reaches over 705 mV, the fill factor (FF) exceeds 82.0%, and the conversion efficiency (η) can reach over 24.0% with a thickness of 60-80 μm. The performance indicators comprehensively surpass those of conventional products of the same thickness.
[0019] Process compatibility and cost potential: The process is simplified and production capacity is increased by adopting electrode co-curing technology. The back electrode uses a low-cost conductive adhesive doped with polymer microspheres to partially replace the precious metal silver. Combined with the front ultra-fine grid line technology, material costs are reduced while ensuring performance. Attached Figure Description
[0020] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below.
[0021] Figure 1 This is a process flow diagram of the method for preparing an ultrathin p-type crystalline silicon solar cell according to an embodiment of the present invention. Detailed Implementation
[0022] To make the objectives, technical solutions, and advantages of this invention clearer, the embodiments of this invention will be described in detail below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this invention. All other embodiments obtained by those skilled in the art based on the embodiments of this invention without creative effort are within the scope of protection of this invention.
[0023] Example 1: Fabrication of a radiation-resistant ultrathin p-type crystalline silicon solar cell (gallium doping) This embodiment describes the preparation of a radiation-resistant ultrathin battery according to the preparation method of the second aspect of the present invention.
[0024] S1: A gallium-doped Czochralski single-crystal p-type silicon wafer with a thickness of 70±2 μm and a resistivity of 2.0 Ω·cm is selected. It is etched at 78℃ for 8 min in a mixed solution of 1.5wt% KOH and an appropriate amount of isopropanol to form a pyramid textured surface with an average height of about 2.5 μm on the front side of the silicon wafer and a nano-worm-like textured surface with an average height of about 500 nm on the back side. S2: A tube diffusion furnace is used with POCl3 as the phosphorus source to perform phosphorus diffusion on the front side of the silicon wafer at 790 ℃, forming an n-type silicon wafer with a sheet resistance of 100±5 Ω / □. + Emitter. Subsequently, a single-sided spraying device was used to rinse the back side with a dilute hydrofluoric acid solution (HF:H2O=1:20) to completely remove the phosphosilicate glass from the back side; S3: After cleaning, the silicon wafer is placed in a UV ozone cleaner for 15 minutes to grow a chemical SiO2 tunneling layer of approximately 1.2 nm thickness on the back side. It is then fed into a PECVD system to sequentially deposit a 7 nm thick intrinsic amorphous silicon (ia-Si:H) and a 23 nm thick in-situ phosphorus-doped amorphous silicon (na-Si:H). + -a-Si:H), where the flow ratio of phosphine to silane is set to 1.5%; S4: Place the silicon wafer in a rapid annealing furnace and anneal at 825 °C for 25 min in a pure N2 atmosphere to completely crystallize the amorphous silicon layer on the back side, forming a high-quality nanocrystalline silicon / doped polycrystalline silicon composite layer, i.e., a carrier selective transport layer, and obtain a high electrically activated phosphorus concentration. S5: On the crystallized back side, a 100 nm thick SiN layer with a refractive index of 2.2 is deposited using PECVD. x Mg thin film, then subjected to a laser with a wavelength of 532 nm and a pulse width of 200 ns, at a speed of 1.0 J / cm. 2 The laser energy density and 90% overlap rate are used to scan the surface of the thin film. The laser energy is absorbed by the thin film and conducted to the interface, inducing the formation of random nano-pits with a depth of about 60~90nm, which constitute the light scattering interface. S6: On the front side of the silicon wafer, PECVD is used to deposit silicon hydrogen nitride (SiN) with a thickness of 75 nm and a refractive index of 2.08. x :H) as a front passivation antireflection layer.
[0025] S7: Fabrication of selective emitter and stress relief trench: a) Laser grooving: Using a UV picosecond laser system with a wavelength of 355 nm and a pulse width of 10 ps, the laser is ablated along the center of the designed 1.2 mm spacing main grid line with a pulse energy of 40 μJ to precisely etch stress relief grooves with a depth of 10 μm and a width of 50 μm. b) Laser gallium doping: A 0.1 M trimethylgallium / ethanol solution was spin-coated into the trenches. After the solvent evaporated, an 808 nm continuous-wave semiconductor laser was used at a speed of 1.8 J / cm². 2 The energy density and scanning speed of 5 mm / s were used to scan the trench. The laser instantaneously melted the silicon layer at a depth of about 1-2 μm at the bottom of the trench, and gallium atoms were incorporated and activated during the subsequent rapid solidification, forming P-type silicon with a sheet resistance of less than 25 Ω / □. ++ (Ga) contact area; S8: Using an infrared fiber laser with a wavelength of 1064 nm, a local window is made on the back of the battery to ablate a dot matrix of contact holes with a diameter of 30 μm and a spacing of 1 mm, exposing the underlying tunneling oxide layer. Then, it is rinsed with 0.5% dilute HF solution for 30 s to remove laser residue. S9: Printed and Low-Temperature Co-Cure Electrode: a) Electrode preparation: A layer of flexible conductive adhesive is printed on the back side using a squeegee. The flexible conductive adhesive is composed of silver-coated copper powder, epoxy resin and 8 vol% 5 μm polyimide microspheres. A 300-mesh screen is used on the front side to print fine grids with a line width of 18 μm and a 50 μm wide main grid covering the trench. The paste is a low-temperature silver paste with a curing temperature of 365 ℃. b) Co-curing: The printed battery is placed in an infrared conveyor belt sintering furnace and held for 120 seconds in a temperature zone with a set peak temperature of 370 ℃, so that the front and back electrodes can be cured and ohmic contact formed simultaneously.
[0026] Example 2: An ultrathin battery based on boron doping (comparative example) This embodiment aims to illustrate the universality of the low-stress composite architecture of the present invention. Its preparation process is exactly the same as that of Example 1, with only the following two substitutions: The silicon substrate was replaced with a conventional boron-doped p-type silicon wafer of the same thickness (70 μm) and resistivity of 1.5 Ω·cm; In step S7b, the doping source is replaced with a trimethyl borate solution, and the laser doping energy is fine-tuned to 1.5 J / cm². 2 , forming P ++ (B) Contact area.
[0027] Comparative Example 1: Conventional Ultra-thin PERC Battery This comparative example uses the mainstream mass production process to prepare a 70 μm thick PERC cell.
[0028] S1: Using the same boron-doped silicon wafer as in Example 2, perform conventional double-sided pyramid texturing; S2: Perform phosphorus diffusion and backside cleaning as in Example 1; S3: 10 nm Al2O3 was deposited on the back side using atomic layer deposition (ALD), followed by 100 nm SiN deposition using PECVD. x ; S4: 80 nm SiN deposited on the front side using PECVD x As an antireflective coating; S5: Grooves are created on the back SiNx / Al2O3 film using a laser, with a linewidth of 30 μm; S6: Screen printing of silver paste on the front and aluminum paste on the back; S7: Rapid sintering is carried out in a chain sintering furnace at a peak temperature of 780 ℃ to form an aluminum back field (Al-BSF). Performance testing and comparative analysis: Initial performance tests, mechanical reliability tests, and simulated space irradiation aging tests were conducted on the battery samples (30 pieces each) prepared in Example 1, Example 2, and Comparative Example 1. The key results are summarized below: Table 1: Comparison of Initial Photoelectric Properties and Mechanical Characteristics Table 2: Radiation resistance stability test results (1 MeV electrons, cumulative charge 1×10⁻⁶) 15 e / cm 2 ) in conclusion: As shown in Table 1, the initial efficiency, open-circuit voltage, and short-circuit current of Examples 1 and 2 are significantly higher than those of Comparative Example 1. This is directly attributed to the dual advantages of the composite back mirror structure of the present invention: good back-side passivation (high V). oc ) and efficient long-wavelength light management (high J sc Meanwhile, the extremely low fragmentation rate and warpage of both structures demonstrate the effectiveness of the low-stress architecture.
[0029] Table 2 illustrates the core advantages of this invention. In Example 1, the efficiency retention rate of gallium-doped material after irradiation is as high as 83.7%, and its stability exceeds that of Example 2 (78.3%) and Comparative Example 1 (72.1%). This demonstrates that changing the substrate dopant from boron to gallium and combining it with the low-stress composite structure of this invention is a powerful technical means to improve the radiation resistance of ultrathin batteries.
[0030] The comparison between Examples 1 and 2 demonstrates that the composite back mirror + stress trench + flexible electrode architecture design of this invention is universal and applicable to substrates with different dopants. When gallium doping is used, this architecture can maximize its radiation resistance potential, making it suitable for extreme environments such as space. When boron doping is used, this architecture can also achieve terrestrial application performance far exceeding that of existing PERC technology while ensuring high yield. This reflects the powerful synergistic effect and market application flexibility of the technical solution of this invention.
[0031] In summary, this invention successfully addresses the industry challenge of balancing efficiency, yield, and radiation resistance in ultrathin crystalline silicon solar cells through systematic innovations in three areas: gallium doping, composite back mirrors and low-stress trenches, and low-temperature co-curing. In particular, integrating gallium doping technology into the low-stress architecture of ultrathin cells provides a clear and feasible technical route for developing next-generation high-performance, high-reliability space photovoltaic cells.
[0032] Those skilled in the art should understand that this invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to this invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the invention as claimed. The scope of protection of this invention is defined by the appended claims and their equivalents.
Claims
1. A radiation-resistant ultrathin p-type crystalline silicon solar cell, characterized in that, include: p-type single-crystal silicon substrate with a thickness of 60~80 μm; A composite back mirror structure and a back metal electrode are sequentially disposed on the back side of the silicon substrate; A front passivation antireflection layer, a selective emitter, and a front metal electrode are sequentially disposed on the front side of the silicon substrate; in, The acceptor doping element of the p-type single-crystal silicon substrate is gallium; The composite back mirror structure comprises, from the inside out: an ultrathin tunneling oxide layer, a carrier selective transport layer, and a wide bandgap dielectric light scattering layer. The interface between the wide bandgap dielectric light scattering layer and the carrier selective transport layer is a light scattering interface with randomly distributed nano-pits. The selective emitter is formed by a stress relief trench that penetrates the front passivation antireflection layer and extends partially into the silicon substrate. A locally heavily doped region is formed on the inner surface of the trench, and the main gate portion of the front metal electrode fills the trench and forms an ohmic contact with the heavily doped region.
2. The radiation-resistant ultrathin p-type crystalline silicon solar cell according to claim 1, characterized in that, The ultrathin tunneling oxide layer is a silicon dioxide layer with a thickness of 1.0~1.5 nm; The carrier selective transport layer comprises an intrinsic nanocrystalline silicon buffer layer directly deposited on the ultrathin tunneling oxide layer and an in-situ phosphorus-doped polycrystalline silicon layer located above the buffer layer; the thickness of the intrinsic nanocrystalline silicon buffer layer is 5~10 nm, the thickness of the in-situ phosphorus-doped polycrystalline silicon layer is 15~30 nm, and the phosphorus atom concentration is 1×10⁻⁶. 19 cm -3 Up to 5×10 20 cm -3 .
3. The radiation-resistant ultrathin p-type crystalline silicon solar cell according to claim 1, characterized in that, The wide bandgap dielectric light scattering layer is made of magnesium-doped silicon nitride or magnesium-doped silicon oxide, with a refractive index of 2.0~2.4 and a thickness of 80~120 nm; the depth of the nano-pits in the light scattering interface is 50 nm to 100 nm.
4. The radiation-resistant ultrathin p-type crystalline silicon solar cell according to claim 1, characterized in that, The depth D of the stress relief trench and the thickness T of the silicon substrate satisfy the following relationship: D = (8%~25%) × T, and the width of the trench is 40~60 μm.
5. The radiation-resistant ultrathin p-type crystalline silicon solar cell according to claim 1 or 4, characterized in that, The locally heavily doped region within the stress relief trench is doped with gallium, forming P ++ Contact area.
6. The radiation-resistant ultrathin p-type crystalline silicon solar cell according to claim 1, characterized in that, The back metal electrode is a fully covered, flexible, full-back electrode made of a conductive composite material, in which thermoplastic polymer microspheres with a volume fraction of 5% to 15% are uniformly dispersed; the curing peak temperature of the conductive slurry used for the front metal electrode is not higher than 380 ℃.
7. A method for preparing radiation-resistant ultrathin p-type crystalline silicon solar cells as described in any one of claims 1-6, characterized in that, Includes the following steps: S1. Provide a gallium-doped p-type single-crystal silicon substrate and perform double-sided texturing, so that a micron pyramid textured surface is formed on the front side and a nano-scale worm-like textured surface is formed on the back side. S2, forming n on the front side of the silicon substrate + Type of emitter, and remove the phosphosilicate glass on the back; S3. An ultrathin tunneling oxide layer, an intrinsic amorphous silicon layer, and an in-situ phosphorus-doped amorphous silicon layer are sequentially deposited on the back side of a silicon substrate. S4. The structure obtained in step S3 is subjected to high-temperature annealing to convert the amorphous silicon layer into polycrystalline silicon, forming the carrier selective transport layer. S5. Deposit a wide bandgap dielectric layer on the carrier selective transport layer and scan it with a laser to induce the formation of the light scattering interface at the interface. S6. Deposit a front passivation antireflection layer on the front side of the silicon substrate; S7. The stress relief trench is etched on the front side using a laser, and then a localized heavily doped region is formed in the trench using a gallium-doped source and laser scanning. S8. Laser windowing is performed on the back to create a local contact channel; S9. Electrodes are printed on the back and front sides respectively, and then co-cured at low temperature.
8. The preparation method according to claim 7, characterized in that, In step S1, a potassium hydroxide solution with a mass fraction of 0.5% to 2% is used for texturing. The height of the micron pyramid textured surface is 0.8 to 1.5 μm, and the height of the nanoscale worm-like textured surface is 300 to 800 nm.
9. The preparation method according to claim 7, characterized in that, In step S5, the wavelength of the laser is 515~532nm, and the scanning energy density is 0.8~1.2 J / cm². 2 .
10. The preparation method according to claim 7, characterized in that, Step S7 includes: S7a. Use a UV picosecond laser to etch the stress relief trenches with a depth of 5~15 μm and a width of 40~60 μm; S7b, A gallium-containing liquid dopant source is coated into the trench, and a laser with a wavelength of 780~1064 nm is used at a speed of 1.6~2.0 J / cm. 2 The energy density is scanned to achieve gallium doping and activation.