Method for reducing the number of drawing flaw detection alarm points of alloy spring steel
Patent Information
- Application Number
- CN202610724844.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-05-25
- Publication Date
- 2026-08-28
AI Technical Summary
1.探伤效率低:现有热轧及精整工艺下,盘卷表面缺陷较多,导致探伤机频繁报警停机,操作人员需频繁介入打磨,严重影响生产效率
[0019] The system systematically solved the problem of compression damage during the packaging process, reducing the number of alarm points per roll with a flaw detection accuracy of 0.05mm from an average of 100+ to less than 30.
Smart Images

Figure CN122644393A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of alloy spring steel manufacturing and flaw detection technology, and in particular, it is a method for reducing the number of pull-out flaw detection alarm points of alloy spring steel. Background Technology
[0002] With the increasing demands for lightweighting and safety in the automotive industry, high-strength alloy spring steel of 2000MPa grade has been widely used. Due to the high alloy content of spring steel, there is a large amount of internal stress and structural stress after heat treatment. Surface defects can easily cause stress concentration in the product. When the material strength reaches a certain value, the stress concentration at the defect will exceed the upper limit that the material structure can withstand, resulting in problems such as spontaneous fracture and failure in fatigue testing. Especially in cold drawing and subsequent production and use, small defects on the material surface (such as hairline cracks, folds, inclusions, etc.) can cause severe stress concentration, leading to spontaneous fracture or fatigue fracture, endangering driving safety. Therefore, the high-end market has stringent requirements for the surface quality of alloy spring steel.
[0003] 0.05mm is an extremely high flaw detection precision required by domestic wire drawing factories. When a defect is detected during flaw detection, the machine will alarm and stop. Professionals will then grind the defect to remove it. If there are many surface defects, it will lead to more downtime, greatly affecting the customer's production efficiency. A large number of surface defects also indicates a higher risk to material quality, significantly impacting product quality stability.
[0004] In actual production, the squeezing damage caused when packaging spring steel coils is essentially due to friction between the coils. Under the pressure of the packaging machine, the coil is compressed from a loose state of 2.7m to a compact state of less than 1.7m. Therefore, during packaging, the coils will rub against each other and shift, resulting in abrasions at the point of maximum force. To improve squeezing damage, the most fundamental solution is to reduce the packaging pressure. However, low packaging pressure will cause the material to become loose and tilt during transportation. At the same time, too low pressure will cause the coil to be too long, exceeding the upper limit of the material rack when used by customers. Therefore, improvements are mainly made in terms of the surface condition of the material and the packaging pressure.
[0005] Therefore, in summary, the existing production process has the following problems: 1. Low flaw detection efficiency: Under the existing hot rolling and finishing processes, there are many surface defects in coils, which causes the flaw detection machine to frequently alarm and stop. Operators need to frequently intervene to grind, which seriously affects production efficiency.
[0006] 2. High quality risk: Manual polishing will always have some defects that are missed. Defects left over to subsequent processes can cause the finished springs to break, which seriously affects the stability of product quality. Therefore, the quality risk assessment and control of springs is more stringent.
[0007] 3. Difficulty in controlling defects in the finishing process: Although defects in the hot rolling process are easy to analyze and solve, “packaging crushing damage” and “scratches” generated during finishing, packaging and transportation have become the main bottlenecks affecting the pass rate of flaw detection.
[0008] 4. Packaging contradictions: Excessive packaging pressure can easily cause friction between the coils, resulting in squeezing damage; insufficient packaging pressure will cause the coils to become loose, easily tip over during transportation, and exceed the length limit, making them unsuitable for the customer's material rack.
[0009] Therefore, there is an urgent need for a systematic approach to improve the surface condition of materials from the source, and to significantly reduce the number of alarm points with a flaw detection accuracy of 0.05mm without affecting logistics and transportation. Summary of the Invention
[0010] The purpose of this invention is to solve the problems existing in the prior art by proposing a method for reducing the number of alarm points for pull-out flaw detection of alloy spring steel and a coil packaging process.
[0011] To achieve the above objectives, the present invention adopts the following technical solution: The present invention provides a method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel, comprising the following steps: The hot rolling process is controlled sequentially, the ring shape is optimized, the surface lubrication treatment is performed, and the packaging pressure is adjusted. The hot rolling process control includes increasing the wire drawing temperature and extending the residence time of the material in the high-temperature section to increase the thickness of the surface iron oxide scale and form a buffer layer during packaging and extrusion. The circular shape optimization includes adjusting the roller conveyor speed so that the roller conveyor speed is compatible with the circular shape naturally formed by the spinning on the roller; The surface lubrication treatment and packaging pressure adjustment include spraying lubricant on the surface of the coil before packaging and reducing the packaging set pressure to reduce the friction between the coil coils and reduce the length of the coil after packaging.
[0012] Through the synergistic effect of the above steps, the number of alarm points per roll of alloy spring steel with a flaw detection accuracy of 0.05mm can be controlled to less than 30.
[0013] As a further preferred option, hot rolling process control specifically includes: Increase the wire drawing temperature by 50°C and reduce the cooling water flow rate after the finishing mill on the rolling line; By increasing the air cooling time of the material on the Stellmore roller conveyor, the thickness of the surface iron oxide scale is increased from 0.008 mm to 0.014 mm, forming a uniform buffer isolation layer.
[0014] As a further preferred option, the circular shape optimization specifically includes: Continuously adjust the roller conveyor speed, observe the shape of the coil formed by the spinning and the uniformity of the coil overlap spacing, record the roller conveyor speed used for coils that tend to be round, produce at this roller conveyor speed, and record the matching coil specifications for direct use in subsequent production; avoid the coil formed by spinning being stretched and deformed during the movement, after the coil shape is flattened, the total length of the coil is reduced from 2.7m to 2.4m, in order to reduce the length of the coil spreading out on the C-hook, at this time the relative displacement of the head and tail of the packaged material under the pressure of the disc is greatly reduced.
[0015] As a further preferred option, the lubricant used in the surface lubrication treatment is a liquid polymer material, which is sprayed onto the surface of the coil to reduce the coefficient of sliding friction between the coils during the packaging and compression process.
[0016] As a further preferred option, the packaging pressure adjustment specifically includes: The baling pressure of the baler was reduced from 21 tons to 14 tons; While reducing the packaging pressure, the length of the coil after compaction should be controlled between 1.5m and 1.7m to prevent the coil from becoming loose or being crushed due to excessive pressure during transportation.
[0017] As a further preferred option, the alloy spring steel is 2000MPa grade high-strength alloy spring steel.
[0018] As a further preferred option, this method is adapted to a flaw detection accuracy requirement of 0.05 mm. Beneficial effects
[0019] The system systematically solved the problem of compression damage during the packaging process, reducing the number of alarm points per roll with a flaw detection accuracy of 0.05mm from an average of 100+ to less than 30.
[0020] While ensuring coil compactness (facilitating transportation), it significantly reduces surface damage and improves the production efficiency and yield of customers' drawing operations.
[0021] It requires minimal process modifications, has low costs, and is easy to implement on existing production lines. Attached Figure Description
[0022] Figure 1 To improve the previous flaw detection points; Figure 2 To improve the number of flaw detection points; Figure 3 To improve the thickness of the iron oxide scale to 0.008 mm; Figure 4 To improve the thickness of the iron oxide scale to 0.014 mm; Figure 5 To improve the previous ring shape; Figure 6 To improve the shape of the circle; Figure 7 The surface condition before lubrication treatment; Figure 8 This shows the surface condition after lubrication treatment; Figure 9 The final length is 1.6m under 21 tons of packaging pressure; Figure 10 With the aid of lubricant, the final length under a packaging pressure of 14 tons is 1.6m. Detailed Implementation
[0023] The technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments.
[0024] This patent provides a method to reduce the number of alarm points for 0.05mm flaw detection in alloy spring steel, helping to improve the stability of the performance of 2000MPa grade alloy spring steel. This patent improves the material coil shape by increasing the hot rolling temperature, thickening the iron oxide scale, reducing the roller speed, spraying lubricant on the surface, reducing the packaging pressure, and improving the packaging method. These steps suppress packaging crushing defects that occur during packaging. Through these steps, the number of material flaw detection alarm points can be reduced to below 30 points with a flaw detection accuracy of 0.05mm, reducing the impact of flaw detection alarms on coil production.
[0025] The present invention provides a method for reducing the number of pull-out flaw detection alarm points for alloy spring steel and a coil packaging process, comprising the following aspects: (1) Increase the spinning temperature and reduce the roller speed to maximize the contact time between the material and air at high temperature, and increase the iron oxide scale from 0.008 mm to 0.014 mm; Specifically, increasing the wire drawing temperature by 50°C and reducing the cooling water flow rate after the finishing mill on the rolling line increases the contact time between the material and air during hot rolling. At the same time, reducing the roller speed can also increase the residence time of the material on the Stellmore roller, thus increasing the contact time between the material and air. The ultimate goal is to increase the thickness of the surface iron oxide scale from 0.008mm to 0.014mm and improve the uniformity of the iron oxide scale, providing a buffer layer for packaging and extrusion.
[0026] (2) Reduce the speed of the roller conveyor to optimize the coiled coil, such as Figure 5As shown, the coil shape was previously inconsistent, and after the longitudinal stacking was transferred to the transverse C-shaped hook, it became relatively loose, with a length of about 2.7m. After optimizing the coil, the coil length was reduced from 2.7m to 2.4m, and the total length was reduced by 30cm, improving the material density. When the C-shaped hook was transferred to the baling machine, the coil suspended on the C-shaped hook began to shorten in length to less than 1.7m under the action of the baling machine's pressure plate. The head and tail of the coil are the two ends of the unfurled material, and the two ends converge towards the middle under the action of the pressure plate. Since the two ends are in direct contact with the pressure plate, they experience the greatest force and the most displacement, further reducing the length of the material's head and tail displacement during baling. Specifically, the key to reducing the speed of the roller conveyor is to stack the material and prevent the coil formed by the spinning from being pulled into an elliptical shape by the roller conveyor during the movement. Before the material falls onto the collecting drum, the more regular the circle is, the more regular the final coil will be. At the same time, the length of the coil after the coil is regularized is reduced from 2.7m to 2.4m, and the total length is reduced by 30cm. The density of the material is increased, which greatly reduces the length of the material head and tail displacement during packaging.
[0027] (3) After the material surface is coated with lubricant, the packing pressure is greatly reduced. The normal packing pressure is 21 tons and the material length is between 1.6m and 1.8m. After the lubricant is coated, the packing pressure is 14 tons and the material length is between 1.5m and 1.7m. Specifically, applying lubricant before packing reduces friction between the coils, making it easier for the coil to reach its final length of 1.7m under lower packing pressure. Because of the reduced friction, the material is more prone to displacement, and the friction between the coils is less than the material's surface hardness limit, thus avoiding the risk of crush damage during packing. Normally, a packing pressure of 21 tons is used for materials between 1.6m and 1.8m in length. After applying lubricant, the packing pressure is 14 tons, and the material length is between 1.5m and 1.7m.
[0028] The above description is only a preferred embodiment of the present invention, but the scope of protection of the present invention is not limited thereto. Any equivalent substitutions or modifications made by those skilled in the art within the scope of the technology disclosed in the present invention, based on the technical solution and inventive concept of the present invention, should be covered within the scope of protection of the present invention.
Claims
1. A method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel, characterized in that, Includes the following steps: The hot rolling process is controlled sequentially, the ring shape is optimized, the surface lubrication treatment is performed, and the packaging pressure is adjusted. The hot rolling process control includes increasing the wire drawing temperature and extending the residence time of the material in the high-temperature section to increase the thickness of the surface iron oxide scale and form a buffer layer during packaging and extrusion. The circular shape optimization includes adjusting the roller conveyor speed so that the conveyor speed is compatible with the circular shape naturally formed by the spinning on the roller conveyor. The surface lubrication treatment and packaging pressure adjustment include spraying lubricant on the surface of the coil before packaging and reducing the packaging set pressure to reduce the friction between the coil coils and reduce the length of the coil after packaging.
2. The method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1, characterized in that, The hot rolling process control specifically includes: Increase the wire drawing temperature by 50°C and reduce the cooling water flow rate after the finishing mill on the rolling line; By increasing the air cooling time of the material on the Stellmore roller conveyor, the thickness of the surface iron oxide scale is increased from 0.008 mm to 0.014 mm, forming a uniform buffer isolation layer.
3. The method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1, characterized in that, The circular optimization specifically includes: Continuously adjust the roller conveyor speed, observe the shape of the coil formed by the spinning and the uniformity of the coil overlap spacing, record the roller conveyor speed used for coils that tend to be round, produce at this roller conveyor speed, and record the matching coil specifications for direct use in subsequent production.
4. The method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1, characterized in that, The lubricant used in the surface lubrication treatment is a liquid polymer material, which is sprayed onto the surface of the coil to reduce the coefficient of sliding friction between the coils during the packaging and compression process.
5. A method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1 or 4, characterized in that, The packaging pressure adjustment specifically includes: The baling pressure of the baler was reduced from 21 tons to 14 tons; While reducing the packaging pressure, the length of the coil after compaction should be controlled between 1.5m and 1.7m to prevent the coil from becoming loose or being crushed due to excessive pressure during transportation.
6. The method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1, characterized in that, The alloy spring steel is a 2000MPa grade high-strength alloy spring steel.
7. The method for reducing the number of alarm points in pull-out flaw detection of alloy spring steel according to claim 1, characterized in that, This method is suitable for flaw detection accuracy requirements of 0.05mm.