How to Analyze Plastics or Rubber

A non-destructive near-infrared analysis method using regression coefficients from PLS regression analysis effectively assesses plastic deterioration by measuring absorbance and differential processing, addressing the limitations of existing destructive mechanical tests and near-infrared techniques.

JP7573849B2Active Publication Date: 2024-10-28NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE & TECHNOLOGY
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020110070
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-26
Publication Date
2024-10-28
Estimated Expiration
2040-06-26

AI Technical Summary

Technical Problem

Existing methods for analyzing the deterioration of plastics like polypropylene, such as mechanical tests, are destructive and cannot accurately assess properties like elongation at break, while existing near-infrared techniques only measure oxide formation without providing a comprehensive analysis of material state.

Method used

A non-destructive analysis method using near-infrared light that involves measuring absorbance, performing second-order differential processing on the spectrum data, and calculating regression coefficients through PLS regression analysis to estimate properties like elongation at break.

Benefits of technology

Accurately estimates the state of plastic properties like elongation at break by analyzing near-infrared spectra, providing a reliable and non-destructive assessment of material deterioration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573849000007
    Figure 0007573849000007
  • Figure 0007573849000008
    Figure 0007573849000008
  • Figure 0007573849000009
    Figure 0007573849000009
Patent Text Reader

Abstract

To provide a plastic material or rubber material analytical method, by which property degradations such as elongation at break caused by degraded plastic materials or rubber materials can be nondestructively analyzed.SOLUTION: Disclosed is a method for analyzing desired properties of a plastic or rubber using a near-infrared ray, that is an analytical method including: (i) a step of measuring an absorbance for a near-infrared area of the plastic or rubber; (ii) a step of obtaining compensated spectral data by secondarily differentiating near-infrared spectral data obtained by measuring the absorbance; and (iii) a step of calculating a value obtained by multiplying and adding a second differentiated value of the absorbance in each wave length of the compensated spectral data by each regression coefficient obtained from PLS regression analysis, wherein the obtained value shows an estimated value of the desired properties of the plastic or rubber.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for analyzing desired properties of plastics or rubber by near-infrared light, and more particularly to a method for irradiating plastics or rubber with near-infrared light and estimating the state of the desired properties of the plastic or rubber material based on the measured results. [Background technology]

[0002] A plastic material called polypropylene is used in automobile bumpers, electrical wiring covers, and building materials such as electric cables and optical fibers. It is known that plastics such as polypropylene deteriorate when exposed to sunlight or high temperatures for long periods of time, resulting in a decrease in strength and bending properties. Therefore, there is a need for a method to diagnose the progression of deterioration of these materials and enable appropriate management.

[0003] Conventionally, the deterioration of plastic products has been measured by mechanical testing, which measures the force applied when the test object is tensile deformed. Because this method deforms and destroys the test object, no technology has been established to diagnose the deterioration of plastics that are already incorporated into automobiles and building materials and are actually used.

[0004] Patent Document 1 discloses a technique for detecting the generation of oxides due to the deterioration of plastics using near-infrared light to determine the degree of deterioration. However, this technique estimates the amount of oxides generated by the deterioration of plastics, and is not suitable for analyzing the actual state of deterioration, such as breaking elongation. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2001-208684 A Summary of the Invention [Problem to be solved by the invention]

[0006] An object of the present invention is to provide a method for analyzing plastic or rubber materials that can non-destructively analyze the decrease in properties such as breaking elongation due to deterioration of plastic or rubber materials. [Means for solving the problem]

[0007] The near-infrared light absorption characteristics of plastics such as polypropylene change as degradation progresses. The present inventors focused on this characteristic and came up with the idea of ​​estimating the state of plastics or rubber from the change in the shape of the near-infrared spectrum. Specifically, they investigated the existence of a regression coefficient in which the value obtained by multiplying the absorbance at each wavelength of the near-infrared spectrum by a coefficient and adding them up indicates the state of a specific property of the plastic or rubber. If such a regression coefficient can be obtained, the state of a specific property of the plastic or rubber can be estimated simply by obtaining near-infrared spectrum data of the plastic or rubber. However, it is difficult to calculate the regression coefficient from a huge amount of numerical data such as a spectrum. Therefore, the present inventors came up with the idea of ​​calculating the regression coefficient by machine learning and succeeded. When the breaking elongation of polypropylene was estimated using the calculated regression coefficient, a high correlation coefficient was obtained between the breaking elongation and the actual mechanical test. The present invention was completed based on the above findings and includes the following aspects: That is, one aspect of the present invention is [1] A method for analyzing a desired property of a plastic or rubber using near-infrared light, comprising: (i) measuring the absorbance of the plastic or rubber in the near infrared region; (ii) performing second-order differential processing on the near-infrared spectrum data obtained by measuring the absorbance in the step (i) to obtain corrected spectrum data; (iii) multiplying the second derivatives of absorbance at each wavelength of the corrected spectrum data obtained in the step (ii) by the regression coefficients obtained by the PLS regression analysis, and then calculating the sum of the multiplied values; wherein the value obtained by step (iii) provides an estimate of a desired property of said plastic or rubber. Here, in one embodiment of the analysis method of the present invention, [2] The analysis method according to [1] above, The step (iii) is characterized in that the step (iii) is a step of calculating a value according to the following formula:

number

[10] The method for calculating a regression coefficient according to the above [9], further comprising the following steps (a) to (c): (a) measuring the absorbance in the near infrared region of a plurality of plastics or rubbers in different states with respect to a desired property; (b) performing second-order differential processing on the near-infrared spectrum data obtained by measuring the absorbance in the step (a) to obtain corrected spectrum data; (c) measuring actual values ​​of the desired property for each of a plurality of plastics or rubbers in different states; Effect of the Invention

[0008] According to the analytical method of the present invention, it is possible to accurately estimate the state of desired properties, such as the breaking strength of plastics or rubber, simply by measuring the near-infrared spectrum. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a flow chart of one embodiment of the analytical method of the present invention. [Diagram 2] FIG. 2 is a graph showing the near-infrared spectrum of degraded polypropylene. [Diagram 3] FIG. 3 is a graph showing the near-infrared absorption spectrum of polypropylene, the baseline of which has been corrected by second derivative processing. [Figure 4] FIG. 4 is a graph showing the standard deviation of predicted values ​​for each number of principal components in the PLS regression analysis using the near-infrared spectrum of polypropylene. [Diagram 5] FIG. 5 is a graph showing the regression coefficients calculated by the PLS regression analysis. [Figure 6] FIG. 6 is a graph showing the relationship between the breaking elongation of degraded polypropylene and the breaking elongation predicted by PLS regression analysis. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] In one aspect, the present invention provides a method for analyzing a desired property of a plastic or rubber using near infrared light, the method comprising the steps of: (i) measuring the absorbance in the near infrared region of the plastic or rubber (ii) a step of obtaining corrected spectral data by subjecting the near-infrared spectral data obtained by measuring the absorbance in the step (i) to second-order differential processing. (iii) multiplying the second derivative values ​​of absorbance at each wavelength of the corrected spectrum data obtained in the step (ii) by the regression coefficients obtained by the PLS regression analysis and calculating the sum of the multiplied values. The value obtained by the step (iii) represents an estimated value of the desired property of the plastic or rubber. Thus, the analytical method of the present invention makes it possible to non-destructively analyze the decrease in a desired property, such as elongation at break, due to deterioration of a plastic or rubber material.

[0011] In the present invention, the "plastic or rubber" capable of analyzing the desired properties is not limited as long as it absorbs near-infrared light and can be measured. Examples of such plastics include, but are not limited to, polypropylene, polyethylene, polystyrene, polyurethane, polylactic acid, nylon, polycarbonate, polyvinyl chloride, ABS resin, polyester, and acrylic resin, and rubber includes synthetic rubber and natural rubber.

[0012] "Desired properties" include elongation at break, tensile strength, yield stress, maximum stress, stress at break, strain at break, modulus of elasticity, elastic modulus, upper yield point, lower yield point. In a preferred embodiment, the desired property is elongation at break.

[0013] As described above, the analytical method of the present invention includes "(i) the step of measuring the absorbance of plastic or rubber in the near infrared region." Here, the near-infrared region for measuring absorbance can be selected based on the wavelength absorbed by the plastic or rubber component. For example, when the plastic is polypropylene, the wavelength region can be 1200 to 2500 nm, and for other plastics or rubbers, a person skilled in the art can appropriately select the near-infrared region based on the wavelength absorbed according to the target plastic or rubber. The near-infrared region to be measured is preferably in the range of wavelengths of near-infrared light in which the functional groups of the target plastic or rubber show optical absorption, so that the desired properties of the plastic or rubber can be analyzed with high accuracy. For example, when the plastic is polypropylene, the wavelength region of 1600 to 1900 nm is more preferable. The absorbance is measured for all wavelengths included in a specific near-infrared region. For example, when measuring the absorbance in the wavelength region of 1600 to 2000 nm, the absorbance is measured at 1 nm intervals (i.e., 1600 nm, 1601 nm, 1602 nm, . . . 1999 nm, 2000 nm). The interval between the wavelengths to be measured is preferably short, and is preferably the lower limit of the measurement interval of the measuring device. The interval between the wavelengths to measure the absorbance is preferably 1 nm, but is not limited to this, and may be, for example, 2 nm. By measuring the absorbance at regular wavelength intervals, near-infrared spectrum data in a specific near-infrared region can be obtained for the target plastic or rubber. For the measurement of absorbance, a commercially available near-infrared spectrometer such as the near-infrared spectrophotometer NIRSCAN-MKII manufactured by Systems Engineering Corporation can be used.

[0014] After obtaining near-infrared spectral data in step (i), "(ii) a step of obtaining corrected spectral data by subjecting the near-infrared spectral data obtained by measuring the absorbance in step (i) to second-order differential processing" is carried out. After measuring the absorbance in a specific near infrared region, the obtained spectral data is subjected to second derivative processing to perform baseline correction, which allows correction of the height of the absorption peak resulting from the crystalline or amorphous structure of the plastic or rubber, which may differ significantly from the actual value.

[0015] After obtaining the corrected spectral data in step (ii), "(iii) a step of multiplying the second derivative values ​​of the absorbance at each wavelength of the corrected spectral data obtained in step (ii) by the regression coefficients obtained by the PLS regression analysis and adding them up" is performed. The values ​​obtained by this process provide an estimate of the desired properties of the plastic or rubber.

[0016] Here, PLS regression analysis is a linear regression method that combines multiple regression analysis and principal component analysis (Wold S, Sjostrom M, Eriksson L, Chemom. Intell. Lab. Syst.: 58, 109-130 (2001)), and solves the problem of multicollinearity. PLS regression analysis is a method that creates principal components that maximize the covariance between the objective variable and the principal components by linearly combining the explanatory variables, and uses the principal components to estimate the objective variable. The "regression coefficient obtained by PLS regression analysis" refers to an optimal regression coefficient selected according to the type of plastic or rubber for which the state of the desired property is to be predicted and the desired property. For example, if the plastic is polypropylene and the desired property is breaking elongation, a regression coefficient capable of predicting the breaking elongation of polypropylene is used. The regression coefficient can be a coefficient previously determined for each target plastic or rubber.

[0017] Here, "the second derivative value of the absorbance at each wavelength of the corrected spectrum data is multiplied by the regression coefficient obtained by PLS regression analysis and the sum is calculated" can be specifically calculated using the following formula.

number

[0018] In one embodiment, the regression coefficients in the above step (iii) can be regression coefficients obtained by PLS regression analysis in which (a) the second derivative value of absorbance in the near-infrared region is used as an explanatory variable for a plurality of plastics or rubbers in different states with respect to a desired property, and (b) the actual measured value of the desired property is used as a response variable. "Multiple plastics or rubbers in different states with respect to the desired property" refers to multiple plastics or rubbers having the same composition but different desired properties. For example, if the desired property is breaking elongation, it refers to multiple plastics or rubbers having the same composition but different breaking elongation. These multiple plastics or rubbers are used to provide explanatory variables and response variables used in PLS regression analysis to obtain regression coefficients. Specifically, the absorbance at each wavelength of near-infrared spectrum data obtained from these multiple plastics or rubbers is used as an explanatory variable, and the actual measured value of the desired property is used as the response variable. As described above, the method of preparation of "multiple plastics or rubbers in different states with respect to the desired property" is not limited as long as it can provide explanatory variables and target variables used in PLS regression analysis. In a preferred embodiment, the "multiple plastics or rubbers in different states with respect to the desired property" can be prepared by aging treatment. The aging treatment is not limited as long as it can deteriorate the desired property, and known methods (heat treatment, light treatment, moisture absorption treatment) can be adopted. For example, when the desired property is elongation at break, it can be performed by heat treatment for a certain period of time. When preparing multiple plastics or rubbers in different states with respect to the desired property, it is preferable to use the same aging treatment method for each plastic or rubber (i.e., preparing multiple plastics in different states with respect to the desired property by heat treatment only). The number of "multiple plastics or rubbers in different states with respect to the desired property" to be prepared is not limited as long as the regression coefficient that can accurately predict the desired property can be obtained when the regression coefficient is obtained by PLS regression analysis using the multiple plastics or rubbers. The number can be, for example, 10 or more, 20 or more, or 50 or more, but is not limited thereto.

[0019] Furthermore, the "regression coefficients obtained by PLS regression analysis" can be obtained, for example, by the following steps (a) to (d): (a) measuring the absorbance in the near infrared region of a plurality of plastics or rubbers in different states with respect to the desired property; (b) performing second-order differential processing on the near-infrared spectrum data obtained by measuring the absorbance in the step (a) to obtain corrected spectrum data; (c) measuring actual values ​​of the desired property for each of a plurality of plastics or rubbers in different states; (d) performing a PLS regression analysis by machine learning using the corrected spectrum data obtained in the step (b) and the actual measurement data of the properties obtained in the step (c) to obtain the regression coefficients.

[0020] The method for measuring absorbance in step (a) and the method for obtaining corrected spectral data in step (b) can be performed in the same manner as in steps (i) and (ii) above. In step (c), the method for measuring the actual value of the desired property of the plastic or rubber is not limited, and a suitable known method can be adopted depending on the target plastic or rubber and the desired property. For example, when it is desired to measure the breaking elongation as the desired property, it can be measured using a commercially available tensile tester. A technique for performing PLS regression analysis by machine learning using the corrected spectrum data obtained in the above step (a) and the actual measurement data of the desired properties obtained in the above step (b) is known, and can be performed using a commercially available program (e.g., The Unscrambler manufactured by CAMO Analytic). The number of principal components used in the PLS regression analysis may be selected from the combination with the lowest standard deviation in cross-validation. A known program (for example, The Unscrambler by CAMO Analytic) may be used for cross-validation.

[0021] The present invention will be described in more detail below with reference to specific examples, etc. However, the present invention is not limited to the following examples in any way. EXAMPLES

[0022] In the following examples, near-infrared spectra of polypropylene films (total of 22 specimens) were measured, of which 15 specimens were used as learning data and 7 specimens were used as test data. PLS regression analysis was performed on the spectra of the learning data, and a regression model capable of predicting the breaking elongation from the spectral data was constructed. Using the obtained regression model, the breaking elongation of each of the seven test data specimens was predicted from the spectral data.

[0023] (1. Sample creation) Polypropylene (PP) samples were prepared using a T-die extruder attached to a melt compounder. PP pellets were melt compounded at a rotation speed of 200 rpm and a temperature of 180°C, and then further compounded in the T-die at a rotation speed of 45 rpm and a temperature of 180°C. The compounded PP was injection molded from a 0.4 mm lip land at 80°C and a speed of 1 m / min. The injected PP sheet was wound up on a roll stack at 80°C and a speed of 1 m / min. Dumbbell pieces were cut out of the PP sheet according to JIS K 6251.

[0024] (2. Deterioration Treatment) The PP dumbbell pieces were aged in an oven at 130°C for 32 days. During the aging period, the dumbbell pieces that had reached the specified number of days (after aging for 1, 2, 3, 4, 7, 9, 10, 11, 14, 15, 17, 18, 21, 22, 23, 24, 25, 28, 29, 30, 31, or 32 days) were taken out and subjected to near-infrared spectroscopy and tensile testing.

[0025] (3. Measurement of breaking elongation) The breaking elongation (%) of each PP sample that had been aged for a specified number of days was measured using a Shimadzu tensile tester. The sample was stretched at a speed of 10 mm / min at room temperature of 25°C, and the breaking elongation was measured. The learning data of the breaking elongation of each PP sample obtained was used as the objective variable for the PLS regression analysis described below in 6. (See Table 1 below). [Table 1]

[0026] (4. Near-infrared spectrum measurement) Using a near-infrared spectrometer manufactured by System Engineering Co., Ltd., the spectra of 22 PP samples that had been subjected to aging treatment were measured in the wavelength range of 1600 to 2000 nm, with an accumulation count of 64. The obtained spectral data of the 22 samples is shown in Figure 2.

[0027] (5. Analysis of Near-Infrared Spectra) The measured near-infrared spectrum (Figure 2) shows a strong baseline shift due to light scattering. In addition, the absorption peaks resulting from the PP crystal and amorphous structures overlap, causing the peak heights to differ significantly from the actual values. For this reason, second-order derivative processing was performed to remove baseline fluctuations and peak overlaps. Figure 3 shows the baseline-corrected spectrum after second-order derivative processing. Of the corrected spectral data obtained, the learning data was used as the explanatory variables for the PLS regression analysis described below in 6.

[0028] (6. PLS regression analysis) PLS regression analysis was applied to the near-infrared spectrum of the training data that had been subjected to second-order differentiation, and a training model (regression coefficient) for estimating the breaking elongation of PP was calculated. The Unscrambler manufactured by CAMO Analytic was used for the PLS regression analysis. Specifically, the 1600-2000 nm spectral data of the training data specimen, corrected for every 1 nm (1-32 days of aging treatment), was used as the explanatory variable, and the breaking elongation rate of the training data specimen (1-32 days of aging treatment) was used as the objective variable. In addition, the results of the cross-validation method showed that the model with the smallest prediction error (standard deviation of predicted value) was the one that performed PLS regression analysis using the scores of the first and second principal components (Figure 4).

[0029] The regression coefficients calculated by PLS analysis using the scores of the first and second principal components (Figure 5) showed that the regression coefficients had large negative values ​​at the wavelength position where the absorption peak (1706 nm) due to the crystalline structure appeared. On the other hand, the regression coefficients had large positive values ​​at the wavelength position where the absorption peak (1691 nm) due to the amorphous structure appeared. This demonstrated that the learning model obtained was able to estimate the breaking elongation based on information about the quantitative change between crystalline and amorphous PP.

[0030] (7. Calculation of breaking elongation using regression coefficients) As described above, by using the near-infrared spectrum data and breaking elongation of the learning data, we were able to obtain a regression coefficient that can predict the breaking elongation. Specifically, the breaking elongation of polypropylene can be predicted by using the following formula. The regression coefficients can be the values ​​shown in Figure 5.

number

Claims

1. 1. A method for analyzing the loss of a desired property due to degradation of a plastic or rubber using near infrared light, comprising the steps of: (i) measuring the absorbance of the plastic or rubber in the near infrared region; (ii) performing second-order differential processing on the near-infrared spectrum data obtained by measuring the absorbance in the step (i) to obtain corrected spectrum data; (iii) calculating a value obtained by multiplying each of the second derivative values ​​of absorbance at each wavelength of the corrected spectrum data obtained in the step (ii) by a regression coefficient obtained by the PLS regression analysis, and then adding up the multiplied values, the regression coefficients are values ​​obtained using absorbance in the near infrared region of a plurality of plastics or rubbers produced by a deterioration treatment and in different states with respect to the desired property, The analytical method of claim 1, wherein the value obtained by step (iii) provides an estimate of a desired property of the plastic or rubber.

2. The method of claim 1 , The analysis method, wherein the step (iii) is a step of calculating a value according to the following formula: [0010] (where x is the second derivative of absorbance for each wavelength in the corrected spectral data, b is the regression coefficient corresponding to each second derivative, y represents an estimate of the desired property, and n is the total number of wavelengths having second derivatives.)

3. The analysis method according to claim 1 or 2, the regression coefficient in the step (iii) is a regression coefficient obtained by a PLS regression analysis in which (a) the second derivative value of absorbance in the near-infrared region is used as an explanatory variable, and (b) the actual measured value of the desired property is used as a response variable, for a plurality of plastics or rubbers in different states with respect to the desired property.

4. The analysis method according to claim 1 or 2, The regression coefficients are obtained by the following steps (a) to (d): (a) measuring the absorbance in the near infrared region of a plurality of plastics or rubbers in different states with respect to the desired property; (b) performing second-order differential processing on the near-infrared spectrum data obtained by measuring the absorbance in the step (a) to obtain corrected spectrum data; (c) measuring actual values ​​of the desired property for each of a plurality of plastics or rubbers in different states; (d) performing a PLS regression analysis by machine learning using the corrected spectrum data obtained in the step (b) and the actual measurement data of the desired property obtained in the step (c) to obtain the regression coefficients.

5. The analysis method according to any one of claims 1 to 4, The method of analysis, wherein the desired property of the plastic or rubber is elongation at break.

6. The analysis method according to any one of claims 1 to 5, The method of analysis, wherein the plastic or rubber is polypropylene.

7. The method of claim 6, further comprising: The analytical method, wherein the near infrared region is a wavelength region of 1600 to 2000 nm.

Citation Information

Patent Citations

  • Method for separating defective product of polymer compound

    JP2000159897A

  • Determining apparatus and method for plastics and classifying apparatus and method therefor

    JP2001208684A

  • Method for distinguishing grade of high-molecular material

    JP2002090299A

  • Analytical curve transplantation method

    JP2005233882A

  • Inspection system, inspection method, and method for manufacturing inspection system

    JP2019086499A