Spacer, laminate of substrates, substrate production method, and method for producing substrate for magnetic disk

LAP714AUndetermined Publication Date: 2026-02-20HOYA CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
LAP714
Authority / Receiving Office
LA · LA
Patent Type
Applications
Current Assignee / Owner
Priority Date
2018-03-09
Filing Date
2019-03-11
Publication Date
2026-02-20

AI Technical Summary

Technical Problem

Existing methods for manufacturing magnetic disk substrates face challenges in maintaining substrate alignment during edge polishing, leading to positional deviations and variations in surface roughness due to spacer misalignment and pressure release, which complicates the process and reduces efficiency.

Method used

A sheet-like spacer with a smaller surface area than the substrate, made of resin with specific thickness and surface characteristics, is interposed between substrates to minimize positional deviation by limiting the thickness change upon pressure release, ensuring accurate edge polishing and maintaining substrate alignment.

Benefits of technology

The spacer effectively suppresses spacer and substrate displacement when pressure is released, reducing variations in surface roughness and polishing accuracy, thereby enhancing the efficiency and consistency of edge treatment processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
  • Figure 00000000_0002_ABST
    Figure 00000000_0002_ABST
  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The area of a spacer that is to be provided between the adjacent substrates in a laminate including a plurality of substrates to keep the adjacent 5 substrates apart from each other is smaller than those ofthe stacked substrates. When pressure is released to bring the laminate obtained by providing the spacers between the substrates from a pressed state in which 0.60 MPa of pressure is applied to the laminate in the stacking direction into a non-pressed state, an amount ofchange AW in thickness per spacer that is calculated from a 10 change in the thickness ofthe laminate due to the release of pressure is 30 pm or less.
Need to check novelty before this filing date? Find Prior Art

Description

Spacer, substrate stack, substrate manufacturing method, and magnetic disk substrate manufacturing method

[0001] The present invention relates to a spacer, a substrate stack, a substrate manufacturing method, and a magnetic disk substrate manufacturing method. The spacer is a sheet-like member that is interposed between adjacent substrates in a stack to separate the adjacent substrates when forming a stack of multiple substrates and performing edge processing on the multiple substrates.

[0002] Hard disk drives for data recording use magnetic disks in which a magnetic layer is provided on a disc-shaped non-magnetic glass plate for magnetic disks. When manufacturing a glass plate for magnetic disks, the main surfaces and edge faces (inner and outer edge faces) of the glass plate are ground or polished. To improve the efficiency of polishing the edge faces of the glass plates, a method is used in which a stack of multiple glass plates is formed by stacking them in the normal direction of their main surfaces, and the edge faces of the multiple glass plates are simultaneously polished with a polishing jig such as an abrasive brush. In the stack, spacers for edge polishing glass plates are provided between the glass plates to separate them and prevent the glass plates from coming into close contact with each other or from rubbing against each other and causing scratches on the main surfaces of the glass plates.

[0003] In polishing the edge faces of glass sheets, both the outer edge face and the inner edge face are polished. Therefore, when polishing a stack of glass sheets as described above, for example, the glass sheets are stacked on an outer edge face polishing jig, and the outer edge faces are polished under pressure, followed by polishing the inner edge faces. In this case, it is necessary to release the pressed glass stack and then disassemble the stack (separate the glass sheets) between the steps of polishing the outer edge faces and polishing the inner edge faces. A glass sheet stacking jig capable of polishing the outer edge faces and the inner edge faces without releasing the pressure on the glass stack and disassembling it is known (Patent Document 1).

[0004] The glass plate lamination jig has a shaft that is inserted into a circular hole in a glass plate for a magnetic recording medium, supports the inner end surface of the glass plate laminate, and aligns the glass plate for a magnetic recording medium. The shaft has clamp bolt fitting portions at both ends of the shaft that allow clamp bolts to be fitted thereto, and a shaft stopper portion around the shaft that supports the glass plate laminate.

[0005] JP 2013-73636 A

[0006] When using the glass plate lamination jig, the release of pressure and disassembly of the glass plate laminate are not necessary, improving production efficiency. However, the glass plate lamination jig has a complex configuration and is difficult to handle. Furthermore, polishing jigs such as polishing brushes must be configured to fit the glass plate lamination jig, resulting in low versatility when performing edge polishing. Furthermore, since the glass plate lamination jig is configured to accommodate a set number of stacked sheets of 100 or more, it is not possible to freely allocate the number of stacked sheets for inner edge polishing and outer edge polishing, taking into account the difference in polishing time between inner edge polishing and outer edge polishing, so as to increase glass plate production efficiency. In this respect, using the glass plate lamination jig for edge polishing can be inconvenient.

[0007] On the other hand, it is possible to release the pressure on the glass sheets in the stacking direction and replace the lamination jig to switch from polishing the outer edge surface to polishing the inner edge surface, or from polishing the inner edge surface to polishing the outer edge surface, without disassembling the glass sheet stack (separating the glass sheets). However, in this case, the pressure on the stack is released, which can cause the spacers between adjacent glass sheets to shift position due to their reshaping. This spacer shift can also cause misalignment between adjacent glass sheets. If the glass sheets are repressed while the stack is misaligned to perform edge polishing, the relative positions of the glass sheets with respect to the adjacent glass sheets change, resulting in variations in the amount of removal from the chamfered surfaces and sidewalls. Furthermore, spacer shifts can prevent proper polishing of the chamfered surfaces on the edge surfaces. For example, if the spacers between adjacent glass sheets shift toward the chamfered surfaces due to misalignment, the way the polishing brush impacts the area near the bottom of the recess between the chamfered surfaces changes, potentially resulting in inconsistent polishing. Since it is difficult to visually check whether or not there is misalignment, in order to obtain a laminate without misalignment, the laminate must be disassembled and the glass plates and spacers must be reassembled by arranging them in their predetermined positions, but disassembling and reassembling the laminate is a cumbersome task. When pressure is released from a laminate of glass plates in a compressed state, it is undesirable that the spacers may become misaligned due to deformation caused by the restoration of their shape, or that the glass plates may also become misaligned.

[0008] Therefore, the present invention aims to provide a spacer that is interposed between adjacent substrates in a stack of substrates such as glass plates to separate the adjacent substrates, and that can suppress misalignment of the spacer or even the substrates that occurs when pressure is released from the pressed stack, as well as a stack of substrates that includes this spacer, a method for manufacturing a substrate that performs edge polishing using a stack that includes this spacer, and a method for manufacturing a substrate for a magnetic disk.

[0009] One aspect of the present invention is a sheet-like spacer that is interposed between adjacent substrates in a stack of multiple substrates to separate the adjacent substrates when the stack is formed and edge processing of the multiple substrates is performed, wherein the area of ​​the spacer is smaller than that of the substrates, and when a pressure of 0.60 MPa is applied to the stack of multiple substrates in the stacking direction and the pressure is released to a non-pressure state, a thickness change ΔW per spacer calculated from the thickness of the stack that changes with the release of the pressure is 30 μm or less.

[0010] The spacer is preferably made of resin, and the contact angle of the spacer with pure water is preferably 50 degrees or less.

[0011] The spacer preferably has a surface roughness Ra of 0.2 μm or more. The spacer preferably has water resistance.

[0012] Another aspect of the present invention is a laminate including a plurality of substrates and the spacer between adjacent substrates of the plurality of substrates.

[0013] Yet another aspect of the present invention is a method for manufacturing a substrate, which includes processing a side surface of the laminate.

[0014] Yet another aspect of the present invention is a method for manufacturing a substrate, the method including processing a side surface of the laminate of the substrate, the processing of the side surface of the laminate including: a process for placing the laminate in a compressed state; a first side surface process for processing the side surface of the laminate in the compressed state; a process for releasing the laminate from the compressed state after the first end face process; an intermediate process for separating the laminate from the compressed state into two or more laminates, combining the laminate from the compressed state with other laminates in the stacking direction, or maintaining the laminate from the compressed state as is; a process for placing the laminate from the intermediate process into a compressed state after the intermediate process; and a second side surface process for further processing the side surface of the laminate in the compressed state after the intermediate process.

[0015] It is preferable that the laminate be brought into the pressed state by applying pressure to the substrates at both ends of the laminate in the stacking direction using a jig.

[0016] The substrate is preferably a glass plate.

[0017] Yet another aspect of the present invention is a method for manufacturing a magnetic disk substrate, comprising: a process for manufacturing a substrate that will become the magnetic disk substrate by a substrate manufacturing method that includes processing a side surface of the laminate; and a post-processing that performs at least a polishing process on the main surface of the substrate after processing the side surface of the laminate.

[0018] According to the above-mentioned spacer, substrate stack, substrate manufacturing method, and magnetic disk substrate manufacturing method, it is possible to suppress misalignment of the spacer or even the substrate that occurs when pressure is released from the stack in a pressed state.

[0019] 1A is a perspective view of an example of a glass plate produced in one embodiment, (b) is a diagram showing an example of a cross section of an end face of the glass plate shown in (a), and (c) is a diagram showing an example of a spacer used in one embodiment. It is a diagram explaining an example of a polishing process for polishing the side face of a stack of glass plates used in one embodiment. It is a diagram explaining the amount of change ΔW in the thickness of a spacer of one embodiment when pressure is released from a pressed state to an unpressured state. It is a diagram explaining the change in the shape of a stack of glass plates when a second end face is polished after a first end face is polished in one embodiment.

[0020] As described above, in a stack of glass plates in which spacers are sandwiched between the glass plates to separate and press the glass plates together, the pressure is released from the pressed state of the stack between the polishing of the inner edge surface and the polishing of the outer edge surface. This release of pressure can cause the glass plates and the spacers to become misaligned. It has been found that this misalignment depends on the characteristics of the spacers. In particular, it has been found that the greater the change in the thickness of the spacers when the pressure is released from the pressed state, the more frequently the misalignment occurs and the greater the amount of misalignment. Based on these findings, the present inventors have devised the following aspects.

[0021] A spacer is a sheet-like member that is interposed between adjacent substrates in a stack of multiple substrates to separate them when edge processing of the multiple substrates is performed. The spacer may have a shape similar to that of the substrate, e.g., a disk shape. Here, the area of ​​the spacer's surface in contact with the substrate is smaller than that of the substrate. In edge processing, for example, edge polishing, a stack of substrates is pressed in the stacking direction (thickness direction of the substrates), and a polishing solution containing cerium oxide or the like as an abrasive is supplied to the edge faces (outer or inner edge faces) of the substrates while the edge faces are polished with a polishing tool such as a polishing brush, polishing pad, or sponge. When a stack formed by sandwiching spacers between multiple substrates is pressed in the stacking direction with a pressure of 0.60 MPa and then released to a no-pressure state, the thickness change ΔW per spacer is 30 μm or less. The thickness change ΔW per spacer is calculated from the thickness of the stack that changes with the release of pressure.

[0022] When the above-mentioned change ΔW per spacer is 30 μm or less, defects after edge processing due to misalignment of the substrates or spacers (for example, in edge polishing, a partial increase in surface roughness or variations in the amount of material removed between substrates due to polishing) are reduced. The change ΔW is measured as a spacer characteristic, for example, as follows: First, 110 substrates, one spacer, and five substrates are stacked in this order from bottom to top, all in a dry state, to create a stack. The thickness of the stack when pressed (at a pressure of 0.60 MPa) is used as a reference, and the change in thickness of the stack when the pressure is released is measured, and this value is designated as change A. On the other hand, a stack similar to the above stack, except that it does not include spacers, is created, and the change in thickness of the stack before and after the pressure is released is measured in the same manner as above, and this value is designated as change B. From these values, the change ΔW is calculated using the following formula: (change ΔW) = (change A) - (change B). Here, the thickness of the stack increases when the pressure is released from the pressed state, as the spacers return to their original thickness. Here, depending on the material, it may take some time for the spacer thickness to return to its original state, so it is preferable that the change amount A and the change amount B are the amounts one minute after the pressure is released.

[0023] According to one embodiment, the change ΔW is preferably 20 μm or less, more preferably 10 μm or less. This prevents misalignment of the substrate or spacer when the pressure is released. On the other hand, a change ΔW close to zero, i.e., no change in spacer thickness at all, is undesirable because it may scratch the surface of the substrate. From this perspective, the change ΔW is preferably 0.05 μm or more, more preferably 0.1 μm or more. It is sufficient for the change ΔW to be 30 μm or less, and the average thickness W1 of one spacer in the unloaded state (initial state) is not particularly limited. Depending on the spacer material, it is possible to keep the change ΔW within the above range by reducing the average thickness W1 of the spacers. However, excessively thin spacers have low durability (easily damaged or torn), and are therefore undesirable from the standpoint of durability. The average thickness W1 of one spacer is, for example, 50 to 1500 μm. A smaller average thickness W1 is preferable because it increases the number of stacked spaces per unit length. From this viewpoint, W1 is preferably 1000 μm or less, more preferably 500 μm or less, and even more preferably 300 μm or less. On the other hand, if the average thickness W1 is too small, the sheet becomes more susceptible to breakage and the number of times it can be reused decreases. From this viewpoint, the average thickness W1 is preferably 100 μm or more.

[0024] The substrate described below is a glass plate. However, in addition to glass plates, the substrate also includes plates such as aluminum alloy substrates, silicon substrates, and titanium substrates. The substrate may have a disk shape with a hole in the center, but may also have shapes other than a disk shape, such as a circular shape without a hole in the center or a rectangular shape. The thickness of the substrate is not particularly limited, but from the viewpoint of increasing the number of stacked layers and improving processing efficiency, the thickness of the substrate is preferably 2 mm or less, more preferably 0.7 mm or less, and even more preferably 0.6 mm or less. Furthermore, the substrate is particularly suitable for the manufacture of glass substrates for magnetic disks, which require polishing of two edge surfaces, the inner edge and the outer edge, and for which a reduction in manufacturing cost is strictly required. The edge surface treatment performed on the substrate includes an edge surface polishing process in which the edge surface of the substrate and a polishing jig abutting the edge surface of the substrate are moved relatively at the contact portion to polish the edge surface, or an edge surface grinding process. In addition, edge surface processing includes not only edge surface polishing processing in which both the edge surface of the substrate and the polishing jig are moved at the contact portion, but also edge surface polishing processing in which only one of them is moved to polish. In this case, the area of ​​the spacer is smaller than that of the substrate so that the spacer does not protrude from the edge surface of the substrate. Furthermore, in edge surface processing, if the pressure applied to the stack in the stacking direction is released to an unpressured state between the first and second processing, edge surface processing includes processing of different edge surfaces of the substrate and processing of the same edge surface twice. The two processings include processing with different processing precision, such as grinding processing and polishing processing, or rough polishing processing and fine polishing processing.

[0025] FIG. 1( a) is a perspective view of an example of a glass plate whose edge is polished by sandwiching a spacer according to an embodiment. FIG. 1( b) is a view showing an example of a cross section of the edge of the glass substrate shown in FIG. 1( a). The glass plate 1 shown in FIG. 1( a) is a thin, disk-shaped glass plate having a circular hole in the center. The glass plate 1 can be used as a glass substrate for a magnetic disk. When the glass plate 1 is used as a glass substrate for a magnetic disk, the size of the glass substrate for a magnetic disk is not important, but the glass substrate for a magnetic disk has a nominal diameter of, for example, 2.5 inches or 3.5 inches. In the case of a glass substrate for a magnetic disk having a nominal diameter of 3.5 inches, for example, the outer diameter is 95 mm, the inner diameter of the circular hole is 25 mm, and the plate thickness is 0.3 to 2.0 mm. A magnetic disk is produced by forming a magnetic layer on the main surface of the glass plate 1.

[0026] The glass plate 1 includes a pair of main surfaces 11p, 12p, a side wall surface 11w formed on an edge surface, and chamfered surfaces 11c, 12c interposed between the side wall surface 11w and the main surfaces 11p, 12p. The side wall surface 11w includes the center position in the thickness direction of the glass plate 1. The inclination angle of the chamfered surfaces 11c, 12c with respect to the main surfaces 11p, 12p is not particularly limited and may be, for example, 45°. Furthermore, the boundary between the side wall surface 11w and the chamfered surfaces 11c, 12c is not limited to a shape having an edge as shown in the figure, and may be a smoothly continuous curved surface.

[0027] FIG. 1( c) is a diagram showing an example of a spacer used in one embodiment. The spacer 20 shown in FIG. 1( c) is a disk-shaped sheet-like member having a circular hole in the center. When forming a stack of disk-shaped glass plates 1 to polish the inner and outer end faces of the glass plates 1, the spacer 20 is interposed between adjacent glass plates in the stack to separate the adjacent glass plates 1. That is, the stack includes multiple glass plates 1 and a spacer 20 sandwiched between one of the glass plates 1 and another glass plate 1 to be stacked on the glass plate 1, separating the adjacent glass plates 1 from each other. In FIG. 1( c), the disk-shaped surface of the spacer 20 that contacts the glass plate 1 in the stack is referred to as the main surface.

[0028] The inner diameter of the disk-shaped hole in the spacer 20 is larger than the inner diameter of the disk-shaped hole in the disk-shaped glass plate 1, and the outer diameter of the disk-shaped spacer 20 is smaller than the outer diameter of the disk-shaped glass plate 1. That is, the area of ​​the main surface of the spacer 20, which is the portion that contacts the glass plate 1, is smaller than the area of ​​the main surface of the glass substrate 1. The inner diameter of the circular hole and the outer diameter of the disk-shaped spacer 20 are determined so that, when the spacer 20 is sandwiched between the glass plates 1, the inner and outer ends of the spacer 20 do not protrude beyond the positions of the chamfered surfaces 11c and 12c, specifically, the boundary between the chamfered surface 11c and the main surface 11p, and are a predetermined distance from the ends of the chamfered surfaces 11c and 12c. The predetermined distance is, for example, 5 μm to 5 mm. If the distances of the inner and outer ends of the spacer 20 from the chamfered surfaces 11c, 12c vary, the way a polishing tool such as a polishing brush contacts the chamfered surfaces 11c, 12c during edge polishing will vary between glass plates 1, resulting in variations in the degree of polishing of the chamfered surfaces 11c, 12c (surface roughness of the edge surfaces). For this reason, the inner diameter of the circular hole and the outer diameter of the disk shape of the spacer 20 are precisely set. Regarding this spacer 20, when a laminate formed by alternately stacking the spacers 20 and the glass substrates 1 is subjected to a pressure of 0.60 MPa in the stacking direction using a pressing tool, and then the pressure is released from a non-pressured state, the change in thickness ΔW per spacer 20 due to the release of pressure is 30 μm or less. According to one embodiment, the material of the spacer 20 is preferably resin, in order to prevent damage to the surface of the substrate. For example, the spacer 20 is preferably a sheet or film material made of resin such as nylon, acrylic, aramid, polyethylene (PE), polypropylene (PP), polyurethane (PU), or polyethylene terephthalate (PET), or a woven or nonwoven fabric made of fibers of these resins. The resin may contain additives such as fillers or inorganic materials. The spacer 20 may be made of a material other than resin, such as paper made from pulp fibers, or paper or synthetic paper made from both pulp fibers and resin fibers. The spacer 20 may also be made by laminating multiple sheets of the above-mentioned materials.

[0029] FIG. 2 illustrates an example of a polishing process in which the edge of a glass plate 1 is polished by polishing the side surface of a laminate 30. As shown in FIG. 2 , the laminate 30 has a spacer 20 interposed between adjacent glass plates 1 to separate the glass plates 1. At this time, pressure P is applied to the laminate 30 from both sides in the stacking direction (thickness direction of the glass plates 1) to press the laminate 30. The reason for pressing the laminate 30 is to prevent uneven polishing due to a difference in rotation between some glass plates 1 in the laminate 30 and adjacent glass plates 1 when the laminate 30 and the polishing jig are rotated relative to each other to polish the edge. In FIG. 2 , a polishing brush 32 is illustrated as the polishing jig. During polishing, the laminate 30 is pressed in the stacking direction, and polishing is performed with the polishing jig while supplying a polishing liquid to the edge (outer or inner edge) of the glass plate 1. In the edge polishing, for example, the polishing jig and the glass plate 1 are rotated so that the polishing jig and the edge surface (outer edge surface or inner edge surface) of the glass plate 1 move relative to each other.

[0030] FIG. 3 is a diagram illustrating a change in thickness ΔW of each spacer 20 when pressure is released from a compressed state to an uncompressed state in one embodiment of the spacer 20. In FIG. 3, the difference between W2 + ΔW and W1 is exaggerated for ease of understanding. However, the difference between W2 + ΔW and W1 may be small and approach zero. As shown by the hatched area in FIG. 3, the compressed spacer 20 is compressed to an average thickness W2 per spacer 20, which is thinner than the average thickness W1 per spacer 20 in the uncompressed state (initial state). If the spacer 20 is left in this state for, for example, three minutes or more and then the pressure is released, the spacer 20 thickens as it attempts to restore its original shape. This change in thickness is ΔW.

[0031] If the thickness change ΔW per spacer 20 is large, when the pressure on the laminate 30 is released between the polishing of the inner edge surface and the polishing of the outer edge surface to return to an unpressurized state, the spacers 20 provided between the adjacent glass plates 1 will be significantly misaligned due to restoration. This misalignment of the spacers 20 will further increase the likelihood of the glass plates 1 being misaligned relative to the adjacent glass plates 1. If the laminate of glass plates 1 is pressed again in a misaligned state to polish the edges, the relative position of the misaligned glass plate 1 with respect to the adjacent glass plates will change, resulting in variations in the amount of polishing allowance. Furthermore, if the position of the end (inner edge or outer edge) of the spacer 20 moves toward the chamfered surfaces 11c and 12c, the polishing of the chamfered surfaces 11c and 12c will vary between the glass plates 1. For this reason, as described above, the thickness change ΔW per spacer 20 is set to 30 μm or less.

[0032] The above-described polishing of the edge surface of the glass plate 1 is a part of the process for manufacturing the glass plate. The process for manufacturing the glass plate will be described below using a manufacturing method of a glass substrate for a magnetic disk as an example.

[0033] The raw glass plate that forms the glass plate 1 is a plate of a certain thickness produced, for example, by the float method or the down-draw method. Alternatively, the raw glass plate may be a plate obtained by press-molding a block of glass using a mold. The thickness of the raw glass plate is thicker than the target thickness of the final product, a magnetic disk glass substrate, by the amount of allowance to be removed by grinding and polishing, for example, by several μm to several hundred μm.

[0034] Next, the glass plate is shaped into a disk-shaped glass plate 1. For example, a scriber may be used to mechanically form a scribe line on the glass plate and then the glass plate is cleaved along the scribe line, or a laser beam may be used to modify a portion of the glass plate to facilitate cracking, and the glass plate may then be heated and cleaved. Next, the disk-shaped glass plate is shaped to form chamfered surfaces 11c and 12c on the cleaved surfaces. The chamfered surfaces 11c and 12c are formed using, for example, a grinding wheel. This produces the glass plate 1 having the shape shown in FIG. 1(b).

[0035] Next, the edge surface of the glass plate 1 is polished. In polishing the edge surface of the glass plate 1, as shown in FIG. 2 , a laminate 30, which is a laminate of multiple glass plates 1 and spacers 20 sandwiched between the glass plates 1, is pressed with pressure P applied in the stacking direction, and a polishing liquid is supplied to the side of the laminate 30 (the inner side surface formed by the inner end surfaces of the glass plates 1 or the outer side surface formed by the outer end surfaces of the glass plates 1), and the laminate is polished using a polishing jig, for example, a polishing brush 32. In polishing the inner side surface corresponding to the inner end surface of the glass plate 1 using the laminate 30, a fixing jig (not shown) is used to press the area near the outer side surface of the main surface of the glass plate 1 located on the upper or lower surface of the laminate 30. Thereafter, a polishing jig is inserted into the space of the laminate 30 corresponding to the circular hole in the glass plate 1, and the polishing jig is pressed against it from the inside to polish the inner side surface. When polishing the outer side surface corresponding to the outer end surface of the glass plate 1 using the laminate 30, a fixing jig (not shown) is inserted into a space in the laminate 30 corresponding to the circular hole in the glass plate 1, and the fixing jig (not shown) is used to press an area near the inner side surface of the main surface of the glass plate 1 located on the upper or lower surface of the laminate 30, thereby fixing the laminate 30. Thereafter, a polishing jig is pressed against the outer side surface of the laminate 30 from the outside, to polish the outer side surface.

[0036] Next, the main surfaces of the glass plate 1 after the edge polishing are ground and polished. In grinding the glass plate 1, a double-side grinding machine equipped with a planetary gear mechanism is used to grind the main surfaces of the glass plate 1. Specifically, both main surfaces of the glass plate 1 are ground while the outer edge of the glass plate 1 is held in a holding hole provided in a holding member of the double-side grinding machine. The double-side grinding machine has a pair of upper and lower surface plates (upper and lower surface plates) equipped with grinding members, and the glass plate 1 is sandwiched between the upper and lower surface plates. Then, by moving either the upper or lower surface plate, or both, and moving the glass plate 1 relative to each other while supplying coolant, both main surfaces of the glass plate 1 can be ground. For example, the grinding process can be performed by attaching a grinding member formed of a sheet of fixed abrasive grains in which diamonds are fixed with resin to the surface plate.

[0037] Next, the main surfaces of the ground glass plate 1 are subjected to a first polishing. Specifically, both main surfaces of the glass plate 1 are polished while the outer edge of the glass plate 1 is held in a holding hole provided in a polishing carrier of the double-side polishing machine. The purpose of the first polishing is to remove scratches and distortions remaining on the main surfaces after the grinding process or to adjust minute surface irregularities (microwaviness, roughness). In the first polishing, the glass plate 1 is polished while applying a polishing slurry using a double-side polishing machine having a configuration similar to that of the double-side polishing machine used in the above-mentioned fixed abrasive grinding process. In the first polishing, a polishing slurry containing free abrasive grains is used. The free abrasive grains used in the first polishing include abrasive grains such as cerium oxide or zirconia. In the double-side polishing machine, the glass plate 1 is sandwiched between a pair of upper and lower surface plates, similar to the double-side polishing machine. Overall disk-shaped flat polishing pads (e.g., resin polishers) are attached to the top surface of the lower surface plate and the bottom surface of the upper surface plate. Then, either the upper surface plate or the lower surface plate, or both, are moved to relatively move the glass plate 1 and each surface plate, thereby polishing both main surfaces of the glass plate 1. The size of the polishing abrasive grains is preferably within the range of 0.5 to 3 μm in average particle size (D50).

[0038] After the first polishing, the glass plate 1 may be chemically strengthened. In this case, a chemical strengthening liquid, such as a molten mixture of potassium nitrate and sodium sulfate, is used, and the glass plate 1 is immersed in the chemical strengthening liquid. This allows a compressive stress layer to be formed on the surface of the glass plate 1 by ion exchange. Chemical strengthening may be performed after the second polishing. Whether or not chemical strengthening is necessary may be appropriately selected taking into account the glass composition and other requirements.

[0039] Next, the glass plate 1 is subjected to a second polishing process. The second polishing process aims to mirror-polish the main surfaces. A double-sided polishing machine having the same configuration as the double-sided polishing machine used for the first polishing process is also used for the second polishing process. Specifically, the outer edge of the glass plate 1 is held in a holding hole provided in a polishing carrier of the double-sided polishing machine, and both main surfaces of the glass plate 1 are polished. The second polishing process differs from the first polishing process in terms of the type and particle size of the free abrasive grains and the hardness of the resin polisher. The hardness of the resin polisher is preferably lower than that of the first polishing process. For example, a polishing solution containing colloidal silica as free abrasive grains is supplied between the polishing pad of the double-sided polishing machine and the main surfaces of the glass plate 1 to polish the main surfaces of the glass plate 1. The size of the abrasive grains used for the second polishing process is preferably within the range of 5 to 50 nm in average particle size (D50). In addition to the first and second polishing processes, an additional polishing process may be performed, or polishing of both main surfaces may be completed in a single polishing process. The order of the above treatments may be changed as appropriate. After the second polishing, the glass plate 1 is washed. In this manner, the main surfaces of the glass plate 1 are polished to obtain a magnetic-disk glass substrate that satisfies the conditions required for a magnetic-disk glass substrate.

[0040] In this way, in polishing the edge surfaces in the manufacturing method of a glass plate, even when the pressure on the laminate 30 is released from a pressed state to an unpressured state, by setting the change in thickness ΔW per spacer 20 to 30 μm or less, the spacers 20 are less likely to shift in position, or even the glass plate 1 is less likely to shift in position. This reduces variations in polishing of the glass plate 1 within the laminate 30.

[0041] According to one embodiment, the contact angle of the spacer 20 with pure water is preferably 50 degrees or less. Since the main component of the polishing liquid is water, the surface of the spacer 20 is easily wetted by setting the contact angle with pure water to 50 degrees or less. The lower limit of the contact angle is not particularly limited, but is, for example, 0 degrees or more. By using such a hydrophilic spacer 20, an appropriate amount of water is retained between the glass plate 1 and the spacer 20 in the laminate 20 even in a pressed state, thereby increasing adhesion and reducing the likelihood of misalignment of the glass plate 1 or the spacer 20. Furthermore, scratches caused by contact with the spacer 20 are less likely to occur on the main surface of the glass plate 1. Furthermore, even when the laminate is formed in a dry state and then polished under pressure without wetting the laminate in advance, the water in the polishing liquid can quickly penetrate between the glass plate 1 and the spacer 20. This means that the laminate can be formed in a dry state, which facilitates handling of spacers that are particularly lightweight, have no tension, and have extremely low rigidity, thereby improving production efficiency. In particular, spacers that are lightweight, have no tension, and have extremely low rigidity tend to stick to various objects when wet, and tend to wrinkle when attached, making it difficult to form a laminate. The contact angle is measured by dropping 1 μl (microliter) of polishing liquid onto the surface of the spacer 20, and measuring the contact angle 10 seconds after dropping the polishing liquid using a contact angle measuring device. If the surface of the spacer 20 is dirty, clean it beforehand and measure it when it is completely dry.

[0042] Furthermore, according to one embodiment, the spacer 20 is preferably water-resistant so that it maintains its high strength even when wet with the polishing liquid. This improves durability by making the spacer 20 less susceptible to breakage even when the spacer 20 is incorporated into the laminate in a wet state. Furthermore, the spacer 20 can be reused, reducing production costs. Water resistance can be achieved, for example, by using a water-resistant material as the material for the spacer 20, or by providing a surface layer or surface treatment on the spacer surface that prevents water penetration. Furthermore, when the spacer 20 is made of fibers such as woven fabric or nonwoven fabric, it is possible to use, for example, water-resistant fibers or fibers with a water-resistant coating on the surface.

[0043] As described above, by polishing the side surfaces of the laminate 30 comprising a plurality of glass substrates 1 and spacers 20, the end surfaces of each glass plate 1 are polished, which increases the production efficiency of the glass plates 1 and also enables approximately uniform polishing between the glass plates 1.

[0044] According to one embodiment, the surface roughness Ra (arithmetic mean roughness, JIS B0601:2001) of the spacer 20 is preferably 0.2 μm or more. If the surface roughness Ra of the spacer 20 is less than 0.2 μm, the adhesion to the substrate, such as the glass plate 1, becomes too strong, making it difficult to peel the spacer 20 from the substrate, reducing workability and, in some cases, making it impossible to peel the spacer 20 from the substrate. On the other hand, if the surface roughness Ra exceeds 5.0 μm, scratches may be caused on the surface of the substrate. For this reason, the upper limit of the surface roughness Ra is preferably 5.0 μm. The surface roughness Ra of the main surfaces of the spacer 20 is measured using a stylus roughness meter.

[0045] According to one embodiment, the side surface treatment of the laminate 30 of glass plates 1 includes: a process of placing the laminate 30, which is obtained by alternately stacking the glass plates 1 and the spacers 20, in a compressed state; a first side surface treatment for treating the side surface of the laminate 30 in the compressed state; a process of releasing the laminate 30 from the compressed state after the first side surface treatment; an intermediate process of separating the laminate 30 from the compressed state into two or more laminates, bonding the laminate 30 from the compressed state to other laminates in the stacking direction, or maintaining the laminate 30 from the compressed state as is; a process of placing the laminate that has undergone the intermediate process in a compressed state after the intermediate process; and a second side surface treatment for further treating the side surface of the laminate in the compressed state after the intermediate process. In the process of placing the laminate 30 in the compressed state, pressure is applied to substrates, for example dummy substrates, at both ends of the laminate 30 in the stacking direction using a pressing jig to place the laminate 30 in the compressed state.

[0046] 4A is a diagram illustrating an example of a process for polishing the edge of a glass plate according to one embodiment. For example, a first edge polishing process (first side surface processing) is performed with the inner edge of the glass plate 1 as the first edge surface and the inner side surface of the laminate 30 as the first side surface. In a subsequent second edge polishing process (second side surface processing), the outer edge of the glass plate 1 is treated as the second edge surface and the outer side surface of the laminate 30 as the second side surface. In the second edge polishing process, edge polishing is performed on a bonded laminate 34 formed by bonding the laminate 30 to a laminate 33 of glass plates 1 that have been separately subjected to the first edge polishing process. Alternatively, the first edge polishing process (first side surface processing) is performed with the outer edge of the glass plate 1 as the first edge surface and the outer side surface of the laminate 30 as the first side surface. In a subsequent second edge polishing process (second side surface processing), the inner edge of the glass plate 1 is treated as the second edge surface and the inner side surface of the laminate 30 as the second side surface. In the second edge polishing treatment, edge polishing is performed on a bonded layer 34 obtained by bonding the laminate 30 and a laminate 33 of glass plates 1 that have been separately subjected to the first edge polishing treatment.

[0047] 4( b ) is a diagram illustrating an example of a process for polishing the edge of a glass plate according to another embodiment different from the embodiment shown in FIG. 4( a ). For example, a first edge polishing process (first side surface processing) is performed with the inner edge of the glass plate 1 as the first edge surface and the inner side surface of the laminate 30 as the first side surface. In a subsequent second edge polishing process (second side surface processing), the outer edge of the glass plate 1 is treated as the second edge surface and the outer side surface of the laminate 30 as the second side surface. In the second edge polishing process, the laminate 30 is separated into two or more separate laminates 36, and edge polishing is performed on one of the separate laminates 36. Alternatively, a first edge polishing process (first side surface processing) is performed with the outer edge of the glass plate 1 as the first edge surface and the outer side surface of the laminate 30 as the first side surface. In a subsequent second edge polishing process (second side surface processing), the inner edge of the glass plate 1 is treated as the second edge surface and the inner side surface of the laminate 30 as the second side surface. In the second end face polishing process, end face polishing is performed on one of the separated laminates 36 obtained when the laminate 30 is separated into two or more separated laminates 36. Note that in the example shown in Fig. 4(b), the thickness of the laminate 30 after the first end face polishing process is shown as the same thickness as the thickness of the bonded laminate 34 shown in Fig. 4(a), but the thickness of the laminate 30 may be different from the thickness of the bonded laminate 34.

[0048] In this way, by performing the second edge polishing process using the bonded laminate 34 or the separated laminate 36, even if the number of glass sheets 1 processed in the first edge polishing process differs significantly from the number of glass sheets 1 processed in the second edge polishing process, the waiting time for the laminate after the first edge polishing process until the second edge polishing process can be reduced, thereby improving the polishing efficiency of the glass sheets 1. In other words, the processing times for the first edge polishing process and the second edge polishing process can be made closer, preventing either polishing process from becoming a bottleneck. This improves the overall efficiency of the edge polishing process. For example, the perimeter of the outer side surface to be polished is longer than that of the inner side surface to be polished. Under the same polishing conditions, the total amount of polishing allowance required for polishing the outer side surface is larger than that for polishing the inner side surface, and therefore, polishing takes longer. Therefore, by simultaneously polishing a large amount of the outer edge surface of the glass sheet 1 using the bonded laminate 34 formed by bonding the laminates 30 and 33 whose inner side surfaces have been polished, the polishing efficiency of the glass sheet 1 can be improved. In addition, when an end surface polishing device is used that can separate the laminate into two laminates and polish the second side surfaces of the laminates at once, the second side surfaces of the two separated laminates 36 can be polished simultaneously, thereby improving the polishing efficiency of the glass plate 1.

[0049] In the examples shown in Figures 4(a) and 4(b), the laminate 30 after the first edge polishing process is bonded or separated and then subjected to the second edge polishing process. However, the laminate 30 may be maintained as is without being bonded or separated, and the second edge polishing process may be performed on the laminate 30. In the examples shown in Figures 4(a) and 4(b), the edge surfaces to be polished in the first edge polishing process and the second edge polishing process are different edge surfaces of the glass plate 1. However, the edge surfaces to be polished may be the same, for example, the inner edge surface or the outer edge surface. That is, in the first edge polishing process and the second edge polishing process, either the inner edge surface or the outer edge surface may be polished consecutively. In this case, the polishing accuracy may be different, such as rough polishing and fine polishing.

[0050] The glass plate 1 of the laminated body, which has been subjected to the first and second edge polishing processes shown in FIGS. 4( a) and 4(b), may be shipped from the processor that performed the first and second edge polishing processes to another processor, where post-processing, including grinding and polishing of the main surfaces of the glass plate 1, may be performed at the other processor. That is, the glass plate 1, i.e., the glass plate 1 after the edge polishing process, may be used as an intermediate product. This intermediate glass plate 1 is also referred to as a substrate in this specification. Furthermore, the glass plate 1 of the laminated body, which has been subjected to the first and second edge polishing processes, may be subjected to post-processing, including grinding and polishing of the main surfaces of the glass plate 1, at the same processor. According to one embodiment, the substrate manufacturing method includes a process for manufacturing a glass plate 1 (substrate) that will serve as a base for a magnetic disk substrate, using the substrate manufacturing method, which includes the first and second edge polishing processes of the laminate, and a post-processing step for performing at least a polishing process on the main surfaces of the glass plate 1 (substrate) after the second edge polishing process of the laminate.

[0051] (Experimental Example 1) To confirm the effect of the spacers 20 used in this manufacturing method of the glass plate 1, edge polishing was performed on glass plates 1 (outer diameter 95.05 mm, circular hole inner diameter 24.95 mm, thickness 0.7 mm, chamfered surfaces at the outer and inner ends each having a width of 150 μm in the main surface direction and an angle of 45°, and roundness of both the outer end (outer diameter) and the inner end (inner diameter) of 2 μm or less) stacked using the spacers 20. The target value for the removal allowance for edge polishing was 50 μm in diameter equivalent for both the outer and inner ends. Spacers of various materials and thicknesses were used to vary the thickness change ΔW per spacer. The edge polishing of the glass plate 1 was performed using a stack 30 consisting of 101 glass plates 1 and 100 spacers 20. Here, the two glass substrates 1 at both ends of the stack 30 were used as dummy substrates, and the 99 glass substrates 1 to be processed were the only ones left. The glass plate 1 and the spacers were prepared in a dry state, and were alternately stacked using a laminate forming device so that the spacers did not protrude from the main surface 11p of the glass plate 1 and the centers of the two were aligned. For edge polishing, the inner side surface of the laminate 30 in a pressed state (pressure P = 0.60 MPa) was polished with the stacking direction vertical. Then, with the stacking direction vertical, the pressure was released from the pressed state to return to an unpressurized state. To polish the outer side surface of the laminate 30, the laminate 30 was again pressed (pressure P = 0.60 MPa) and the outer side surface of the laminate 30 was polished. Note that no operations to correct the misalignment of the glass plate 1 or the spacers (e.g., disassembling and re-stacking the laminate) were performed before the pressurized state was restored. Furthermore, the contact angle of pure water with the spacers was 50 degrees or less, and the roughness Ra of the spacer surface was in the range of 0.2 to 5 μm.

[0052] By changing the laminate 30 from a pressed state to an unpressured state, misalignment of the spacers 20 and the glass plates 1 occurs along the main surface. This misalignment causes variations in the polishing results of the outer edge surfaces between the glass plates 1. Therefore, the roundness of the outer edge surfaces of all glass plates 1 after polishing was measured to confirm whether any glass plates 1 had significantly deteriorated roundness. Specifically, if even one glass plate with a roundness of 10 μm or more was found among 99 glass plates, it was deemed to have failed. Table 1 below shows the spacer material, spacer thickness (average thickness W1), the change in thickness ΔW per spacer, and the pass / fail result at that time. Sheet materials were used in Examples 1 to 8 and Comparative Examples 2 to 4, and a nonwoven fabric made of polyester resin fibers was used in Comparative Example 1.

[0053]

[0054] As can be seen from Table 1, by using spacers in which the thickness variation ΔW per spacer is 30 μm or less, misalignment of the spacers or glass plate 1 is unlikely to occur, thereby reducing variation in the polishing results of the outer edge surface. As shown in Examples 5, 6, and 8, even when the spacer thickness (average thickness W1) is greater than 200 μm, the variation ΔW is sometimes 30 μm or less, resulting in a pass / fail result. However, as shown in Examples 1, 2, 4, and 7 and Comparative Examples 2 to 4, even when the spacer thickness is 200 μm or less, the variation ΔW is sometimes 30 μm or less or exceeds 30 μm, resulting in variation in the pass / fail results. In other words, it can be seen that pass / fail cannot be determined based on spacer thickness alone.

[0055] (Experimental Example 2) Furthermore, spacers 20 were prepared with the same specifications as in Example 2, except that the surface roughness Ra of the spacers was varied. The same edge polishing (polishing of the inner side surface and the outer side surface of the laminate) as in Experimental Example 1 was performed, and the workability during separation (disassembly) of the laminate after edge polishing was evaluated. A known laminate separation device was used to separate the laminate. This device separates one glass plate 1 with a vacuum chuck, and then blows off the spacers 20 stuck to the glass plate 1 with an air blower. However, if the adhesive force between the glass plate 1 and the spacers 20 is too strong, the spacers 20 will not peel off properly, resulting in a separation error. The presence or absence of this separation error was evaluated. If a separation error occurred with even one spacer 20, it was deemed a "separation error."

[0056]

[0057] As can be seen from Table 2, by setting the surface roughness Ra of the spacer 20 to 0.2 μm or more, separation errors are eliminated and workability is improved.

[0058] The spacer, substrate stack, substrate manufacturing method, and magnetic disk substrate manufacturing method of the present invention have been described in detail above, but the spacer, substrate stack, substrate manufacturing method, and magnetic disk substrate manufacturing method of the present invention are not limited to the above embodiments and examples, and various improvements and modifications may be made within the scope of the present invention.

[0059] REFERENCE SIGNS LIST 1 glass plate 11p, 12p main surface 11w side wall surface 11c, 12c chamfered surface 20 spacer 30, 33 laminate 32 abrasive brush 34 bonded laminate 36 separated laminate

Claims

1. A sheet-like spacer that is placed between adjacent substrates in a stack to separate the adjacent substrates when forming a stack of multiple substrates and performing edge processing on the multiple substrates, wherein the area of ​​the spacer is smaller than that of the substrates, and when the stack formed by sandwiching the spacer between the multiple substrates is pressed from a pressed state of 0.60 MPa in the stacking direction to a non-pressured state, the amount of change in thickness per spacer, ΔW, calculated from the thickness of the stack that changes due to the release of the pressure, is 30 μm or less.

2. The spacer according to claim 1, wherein the spacer is made of resin.

3. A spacer according to claim 1 or 2, wherein the surface roughness Ra of said spacer is 0.2 μm or more.

4. A spacer according to any one of claims 1 to 3, wherein the spacer is water resistant.

5. A laminate comprising a plurality of substrates and a spacer according to any one of claims 1 to 4 between adjacent substrates of the plurality of substrates.

6. A method for manufacturing a substrate, comprising treating the side surface of the laminate according to claim 5.

7. A method for manufacturing a substrate including processing the side surfaces of a laminate of substrates as described in claim 5, wherein the processing of the side surfaces of the laminate includes: processing to put the laminate in a compressed state; a first side surface processing to process the side surfaces of the laminate in the compressed state; processing to release the laminate from the compressed state after the first side surface processing; an intermediate processing to either separate the laminate from which the compressed state has been released into two or more laminates, to combine the laminate from which the compressed state has been released with other laminates in the stacking direction, or to maintain the laminate from which the compressed state has been released as is; processing to put the laminate from which the intermediate processing has been performed into a compressed state after the intermediate processing; and a second side surface processing to further process the side surfaces of the laminate in the compressed state after the intermediate processing.

8. The method for manufacturing a substrate according to claim 6 or 7, wherein the substrate is a glass plate.

9. A method for manufacturing a magnetic disk substrate, comprising: a process for manufacturing a substrate that will become a magnetic disk substrate by the substrate manufacturing method according to any one of claims 6 to 8; and a post-processing step for performing at least a polishing process on the main surface of the substrate after the side surface of the laminate has been processed.