Formaldehyde detection device and detection method
By using coated aminated graphene oxide and potassium periodate detection sheets in the formaldehyde detection device, the problem of long time and high cost of formaldehyde detection in the existing technology is solved, and a simple, accurate and low-cost detection is provided. method.
Patent Information
- Application Number
- CN201710672843.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2017-08-08
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2037-08-08
AI Technical Summary
In the existing technology, the detection method of formaldehyde in indoor environments and workplaces requires professionals and equipment, is time-consuming and expensive, and is not suitable for ordinary households.
A formaldehyde detection device including a standard container and a detection piece is designed. The detection piece is coated with a composite of aminated graphene oxide and potassium periodate. After the standard container is sealed in the environment to be tested for 24 hours, the determination is based on the color card. Formaldehyde concentration.
It realizes simple, fast and low-cost formaldehyde concentration detection, is suitable for ordinary families, and improves the accuracy of detection results.
Smart Images

Figure CN107328768B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a gas detection device and a detection method, and in particular to a formaldehyde detection device and a detection method. Background Art
[0002] Formaldehyde was identified as a Class 1 carcinogen in 2006. Long-term exposure to formaldehyde inhalation of 12 mg / m 3 It can cause drowsiness, weakness, headache, finger tremor, and decreased vision. Long-term inhalation of 20-70 mg / m 3 It can cause loss of appetite, weight loss, weakness, headache, and insomnia. The formaldehyde content in residential buildings should be lower than 0.12 mg / m 3 , so it is very meaningful to monitor the formaldehyde content in the environment.
[0003] The formaldehyde concentration test in indoor environment and workplace air mostly adopts air sampling method, that is, using sampling pump to extract a certain volume of air sample through formaldehyde absorption bottle, and then using chemical colorimetry for analysis. This method requires professionals and professional equipment for analysis and testing, and it is time-consuming and expensive, so it is not suitable for ordinary people's families. Summary of the invention
[0004] Based on this, it is necessary to provide a formaldehyde detection device and a detection method for simply and quickly testing whether the formaldehyde concentration exceeds the standard.
[0005] A formaldehyde detection device is used to detect whether the concentration of formaldehyde exceeds a standard. The formaldehyde detection device comprises a standard container and a detection sheet.
[0006] The standard container volume includes a bottom box and a lid.
[0007] The bottom box is provided with a sealing groove, and the cover is provided with a sealing strip used in conjunction with the sealing groove.
[0008] The sealing strip material is one of silica gel and rubber.
[0009] The cover is provided with an insertion hole for placing the detection sheet.
[0010] The detection sheet is a substrate coated with an amino-modified graphene oxide and potassium periodate composite material.
[0011] In one embodiment, a method for preparing a composite material of aminated graphene oxide and potassium periodate comprises the following steps:
[0012] Add graphite oxide and potassium periodate to deionized water at 80-100° C., mix and disperse by ultrasonication to obtain a graphene oxide-potassium periodate suspension, then add ammonia water with a mass concentration of 30%, and place in an ice bath for stirring and cooling, wherein the mass ratio of the graphite oxide to potassium periodate is 100:6-20, and the solid-liquid ratio of the graphite oxide to the ammonia water is 1 g:30 ml;
[0013] The composite material mixture is filtered, and the obtained amino-modified graphene oxide and potassium periodate slurry is coated on the substrate through a coater, and then the coated substrate is placed in a vacuum drying oven for drying to obtain the detection sheet, which is then sealed and stored for later use;
[0014] In one embodiment, the ultrasonic dispersion time is 30 minutes to 120 minutes.
[0015] In one embodiment, the vacuum drying temperature is 60-80°C.
[0016] In one embodiment, the vacuum drying time is 24 hours to 48 hours.
[0017] A formaldehyde detection method using the above formaldehyde detection device comprises the following steps:
[0018] Place the bottom box of the standard container in the test environment for 24 hours;
[0019] Add a lid to the bottom box, insert the test piece, and seal it for 24 hours;
[0020] According to the color chart, compare the color changes of the test piece to determine the concentration of formaldehyde.
[0021] The invention has the following beneficial effects: the detection device is easy to manufacture, and the raw materials are cheap and easily available, so the manufacturing cost is low. The detection method is simple and clear, and multi-point detection can be used to increase the accuracy of the detection result. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the structure of a detection device according to one embodiment.
[0023] Figure 2 A schematic diagram of a detection sheet according to an embodiment. DETAILED DESCRIPTION
[0024] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific implementation disclosed below.
[0025] like Figure 1 As shown, the standard container includes a base box 100 and a cover 200. The base box has a sealing groove 110, which is used in conjunction with a sealing strip 210 of the cover to complete the seal. The cover has a plug hole 220 for placing a detection sheet 300 and covering the plug hole 220. The detection sheet also includes a substrate 310 and a handheld stick 320.
[0026] like Figure 2 As shown, an amino-modified graphene oxide and potassium periodate composite material 330 is coated on a substrate for detecting formaldehyde.
[0027] A formaldehyde detection device is used to detect whether the concentration of formaldehyde exceeds the standard, and the formaldehyde detection device includes a standard container and a detection sheet. The standard container has a volume of 20L and includes a bottom box and a cover.
[0028] The bottom box is provided with a sealing groove, and the cover is provided with a sealing strip used in conjunction with the sealing groove.
[0029] The sealing strip material is silicone.
[0030] The cover is provided with an insertion hole for placing the detection sheet.
[0031] The detection sheet is a composite material of amino-modified graphene oxide and potassium periodate coated on a substrate, wherein the size of the substrate is 20mm*10mm*2mm, the mass ratio of amino-modified graphene oxide to potassium periodate is 100:5-20, and the coating thickness is 10-50 μm. The coating method adopts transfer coating.
[0032] In one embodiment, a method for preparing a composite material of aminated graphene oxide and potassium periodate comprises the following steps:
[0033] Add graphite oxide and potassium periodate to deionized water at 80-100° C., mix and disperse by ultrasonication to obtain a graphene oxide-potassium periodate suspension, then add ammonia water with a mass concentration of 30%, and place in an ice bath for stirring and cooling, wherein the mass ratio of the graphite oxide to potassium periodate is 100:6-20, and the solid-liquid ratio of the graphite oxide to the ammonia water is 1 g:30 ml;
[0034] The composite material mixture is filtered, and the obtained amino-modified graphene oxide and potassium periodate slurry is coated on the substrate through a coater, and then the coated substrate is placed in a vacuum drying oven for drying to obtain the detection sheet, which is then sealed and stored for later use;
[0035] In one embodiment, the ultrasonic dispersion time is 30 minutes to 120 minutes.
[0036] In one embodiment, the vacuum drying temperature is 60-80°C.
[0037] In one embodiment, the vacuum drying time is 24 hours to 48 hours.
[0038] A formaldehyde detection method using the above formaldehyde detection device comprises the following steps:
[0039] Place the bottom box of the standard container in the test environment for 24 hours;
[0040] Add a lid to the bottom box, insert the test piece, and seal it for 24 hours;
[0041] According to the color chart, compare the color changes of the test piece to determine the concentration of formaldehyde.
[0042] During the specific test, the prevention of formaldehyde capture in the formaldehyde detection device shall refer to the provisions of GB50325-2006 "Code for Indoor Environmental Pollution Control of Civil Construction Engineering", which is as follows: During the acceptance of civil construction projects, the indoor environmental pollutant concentration detection points shall be set according to the room area:
[0043] 1. Room area <50m 2 When , set 1 detection point;
[0044] 2. When the room area is 50~100m 2 When , set 2 detection points;
[0045] 3. Room area>100m 2 When testing, set up 3-5 detection points.
[0046] When there are two or more detection points in a room, the average value of the detection results at each point should be taken as the detection value of the room.
[0047] During the acceptance of civil construction projects, on-site testing points for environmental pollutant concentrations should be no less than 0.5m from the interior wall and 0.8-1.5m from the floor; the testing points should be evenly distributed, avoiding ventilation ducts and vents.
[0048] The following is further described in conjunction with specific embodiments. Example 1
[0049] The formaldehyde detection device is used to detect whether the concentration of formaldehyde exceeds the standard. The formaldehyde detection device includes a standard container and a detection piece.
[0050] The standard container has a capacity of 20L, including a bottom box and a lid.
[0051] The bottom box is provided with a sealing groove, and the cover is provided with a sealing strip used in conjunction with the sealing groove.
[0052] The sealing strip material is silicone.
[0053] The cover is provided with an insertion hole for placing the detection sheet.
[0054] The detection sheet is a composite material of amino-modified graphene oxide and potassium periodate coated on a substrate, wherein the size of the substrate is 20mm*10mm*2mm, the mass ratio of amino-modified graphene oxide to potassium periodate is 100:10, and the coating thickness is 20 μm. The coating method adopts transfer coating.
[0055] The preparation method of the composite material of aminated graphene oxide and potassium periodate comprises the following steps:
[0056] Add graphite oxide and potassium periodate to deionized water at 80°C and mix them, then disperse them by ultrasonication to obtain a graphene oxide-potassium periodate suspension, then add ammonia water with a mass concentration of 30%, and place them in an ice bath for stirring and cooling, wherein the mass ratio of the graphite oxide to potassium periodate is 100:10, and the solid-liquid ratio of the graphite oxide to the ammonia water is 1g:30ml;
[0057] The composite material mixture is filtered, and the obtained amino-modified graphene oxide and potassium periodate slurry is coated on the substrate through a coater, and then the coated substrate is placed in a vacuum drying oven for drying to obtain the detection sheet, which is then sealed and stored for later use;
[0058] The ultrasonic dispersion time is 60 minutes.
[0059] The vacuum drying temperature is 80°C.
[0060] The vacuum drying time is 38 hours.
[0061] A formaldehyde detection method using the above formaldehyde detection device comprises the following steps:
[0062] Place the bottom box of the standard container in the test environment for 24 hours;
[0063] Add a lid to the bottom box, insert the test piece, and seal it for 24 hours;
[0064] According to the color chart, compare the color change of the test piece to determine the concentration of formaldehyde;
[0065] Select a room with an area of 80 m 2 Houses, with 2 testing points;
[0066] Take the average value of the test results at each point as the test value of the room.
[0067] During the acceptance of civil construction projects, the on-site detection points for environmental pollutant concentrations shall be 1m away from the inner wall and 1.5m above the floor; the detection points shall be evenly distributed, avoiding ventilation ducts and vents.
[0068] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A formaldehyde detection device, used to detect whether the concentration of formaldehyde exceeds the standard, the formaldehyde detection device comprises a standard container and a detection sheet; It comprises a bottom box and a cover, wherein the bottom box has a sealing groove, and the cover has a sealing strip used in conjunction with the sealing groove; the sealing strip is made of one of silica gel and rubber; the cover has a plug hole for placing the detection sheet, and the detection sheet is a composite material of amino-modified graphene oxide and potassium periodate coated on a substrate; The preparation method of the composite material of aminated graphene oxide and potassium periodate comprises the following steps: Step 1: Add graphite oxide and potassium periodate to deionized water at 80-100°C and mix them by ultrasonic dispersion to obtain a graphene oxide-potassium periodate suspension. Then add ammonia water with a mass concentration of 30% and place it in an ice bath for stirring and cooling. in, The mass ratio of the graphite oxide to potassium periodate is 100:6 to 100:20, and the solid-liquid ratio of the graphite oxide to the ammonia water is 1g:30ml; Step 2: Filter the composite material mixture, apply the obtained amino-modified graphene oxide and potassium periodate slurry onto the substrate through a coater, and then place the coated substrate in a vacuum drying oven for drying to obtain the detection sheet, which is then sealed and stored for later use; The ultrasonic dispersion time is 30 minutes to 120 minutes; The vacuum drying temperature is 60-80°C; The vacuum drying time is 24 to 48 hours.
2. According to claim 1, a formaldehyde detection method using the above formaldehyde detection device, The following steps are involved: Step 1: Place the base box of the standard container in the test environment for 24 hours; Step 2: Add a lid to the bottom box, insert the test piece, and seal for 24 hours; Step 3: Compare the color change of the test piece according to the colorimetric card and read the formaldehyde concentration.
Citation Information
Patent Citations
Formaldehyde detection device, making method and formaldehyde detection method thereof