Model test stress test block and preparation and use method thereof
By developing a stress test block based on similar materials, the problems of stress testing accuracy and cost in model tests have been solved, realizing high-precision and low-cost stress monitoring, which is suitable for research on mining-induced pressure.
Patent Information
- Application Number
- CN201811556671.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-12-19
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2038-12-19
Smart Images

Figure CN109632158B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of similar material model test and in particular relates to a stress detection element and a preparation and use method thereof. Background Art
[0002] Similar material model test is an important test method for conducting research on mining pressure in mines. In the modeling stage, different similar material ratios are used to simulate the corresponding coal-bearing strata, and the model is laid layer by layer. During the simulated excavation process, the displacement, stress (strain) and support body working conditions of the model body are monitored in real time, and the characteristics of rock stratum movement and fracture and mining stress evolution are studied based on this. In recent years, with the gradual application of advanced testing technologies such as three-dimensional laser scanning, close-range photogrammetry, and digital speckle in model testing, the test accuracy and efficiency of indicators such as model surface deformation and displacement have been significantly improved. However, since the development of model testing, the development of model body stress monitoring technology has lagged behind, and has become a shortcoming restricting the refined development of model testing.
[0003] According to the different stress testing devices, the model body stress testing methods are mainly divided into pressure box, stress test block and other testing methods. The above-mentioned sensors are mostly packaged with metal or rubber materials on the outside. Since the deformation indicators such as elastic modulus of the packaging material are significantly different from those of the model material, the coupling degree of deformation transmission is poor, which reduces the accuracy of the test data; and the sensor can only measure stress in one direction. In recent years, with the development of fiber grating testing technology, the method of attaching fiber gratings to stress test blocks has gradually been applied to model tests, but this method involves debugging, demodulation, signal conversion, transmission and other links, and has high professional requirements on the test personnel. Especially when the model size is large, due to the large number of measuring points, the test cost is greatly increased. This method is difficult to be widely popularized in model tests. Summary of the invention
[0004] In view of the problems existing in this field, the purpose of the present invention is to propose a stress test block for model tests. Based on many years of experience in model testing and drawing on traditional stress testing methods, this research team has developed a stress test block based on a similar material matrix and optimized and improved a complete set of manufacturing processes. The manufacturing process of the stress test block includes processes such as blank production, chip lead, and moisture-proof packaging of the stress test block. The test results show that the mechanical properties of the block and the model material match and the deformation coordination is good; the stress test block has good moisture-proof insulation performance and long-term low zero drift value, and the long-term test performance is stable; the monitoring data can reflect the evolution of the internal stress of the model.
[0005] Another object of the present invention is to provide a method for preparing the model test stress test block.
[0006] Another object of the present invention is to provide a method for using the model test stress test block.
[0007] The technical solution for achieving the above-mentioned purpose of the present invention is:
[0008] A model test stress test block, comprising a blank, a moisture-proof coating, a strain gauge and a sand layer;
[0009] The blank is a block made of a material similar to the model material, and a strain gauge is attached to the outer surface of the block; the moisture-proof coating is attached to the outer surface of the block, between the block and the strain gauge, and the outer surface of the strain gauge;
[0010] The sand layer is attached to the outer surface of the moisture-proof coating.
[0011] Preferably, the strain gauge is bonded to the moisture-proof coating by α-cyanoacrylate ethyl adhesive. The α-cyanoacrylate ethyl adhesive can be commercially available 495 glue, or can be prepared by a method known in the art.
[0012] The block is a cuboid or a cube, and there are 1 to 3 strain gauges located on one face of the block. The angle between the long side of the strain gauge and one side of the face on which it is located is 0 degrees, 90 degrees or 45 degrees (the strain gauge is usually rectangular).
[0013] More preferably, the outer jacket material of the external wire is polytetrafluoroethylene (Teflon) material. The minimum nominal cross-section of the wire is 0.05 mm2.
[0014] A method for preparing a model test stress test block comprises the following steps:
[0015] 1) Pressing similar materials into a green body;
[0016] 2) Apply moisture-proof liquid on the blank and attach the strain gauge after it dries;
[0017] 3) Apply moisture-proof liquid again; apply standard sand before the last application of moisture-proof liquid dries.
[0018] The moisture-proof liquid is prepared by dissolving polyethylene particles in an organic solvent; the organic solvent is one or more of toluene, ethylbenzene, and xylene; preferably, the mass ratio of the polyethylene particles to the organic solvent is 1:(20-50).
[0019] Furthermore, the step 2) is to apply moisture-proof liquid on the blank and dry it at room temperature for 1.5 to 2 hours; continue to apply and dry, for a total of 4 to 6 times, and then paste the strain gauge.
[0020] Wherein, the step 3) is: brushing moisture-proof liquid on the block made in step 2), drying at room temperature for 1.5 to 2 hours, brushing and drying again, brushing 2 to 3 times in total, and dipping standard sand particles before the moisture-proof liquid applied last has dried.
[0021] The method for using the stress test block of the present invention comprises the following steps:
[0022] During the process of laying the similar material model, the stress test block is buried at a predetermined position inside the model, and the wire is led out and exposed outside the model;
[0023] After the similar material model is dried and cured, the model is subjected to a staged excavation test, and the stress test block tests the stress at different positions of the model in real time; during the model test, the stress test block is connected to an external test instrument through a wire, and the test data of the strain gauge is collected and stored in real time, thereby obtaining the deformation parameters of the block at different test stages;
[0024] When the block stress analysis is performed after the test, the dimensionless processing method is used to compare the strain values of the stress test block at different excavation stages with its initial strain value, and the ratio of the two is defined as the strain concentration coefficient at the measuring point; according to the corresponding relationship between the block strain and stress change, the stress change at the measuring point where each block is located is determined, and then the stress field change characteristics of the entire model body are obtained. Since the elastic modulus and other indicators of the same measuring point are constants, according to the classical analysis theory of generalized Hooke's law, the strain increment of each measuring point is positively correlated with the stress increment, so the strain concentration coefficient of each measuring point can reflect its stress concentration coefficient, and the stress change at the measuring point where each block is located is determined accordingly, and then the stress field change characteristics of the entire model body are obtained by inversion.
[0025] After the model test is completed, the stress test block is recovered and reused in subsequent model tests.
[0026] The beneficial effects of the present invention are:
[0027] (1) The present invention develops a stress test block based on similar materials according to the requirements of model test stress testing. One of its characteristics is that the stress test block uses the same material as the model layer, and the mechanical properties between the two are matched, the deformation compatibility is good, and the stress dynamics of the measuring point can be accurately captured; the second characteristic is that the packaging of the stress test block adopts the independently developed benzene-olefin composite moisture-proof liquid, the coating has good sealing performance, and the moisture-proof insulation of the block can adapt to the humid environment during the model laying and drying maintenance; the third characteristic is that the external patch adopts a cost-effective foil strain gauge, with high test accuracy (resolution 1με) and mature patch technology. Multiple measuring points can be arranged in the model according to the test needs, and the dynamic change characteristics of the model stress field can be inverted accordingly. In addition, the wire of the stress test block adopts wear-resistant and fold-resistant polytetrafluoroethylene (Teflon) material, and the outer diameter of the wire is small, which is convenient for reducing the "reinforcement effect" of the implanted wire.
[0028] (2) Based on the optimization research of the process links such as blank production, patch lead, and packaging sand wrapping, the stress test block developed by the present invention has little disturbance to the model stress field, good compatibility, reusability, and convenient preparation, and can monitor the stress distribution characteristics inside the model body during excavation. The beneficial effects of the stress test block have been verified in model tests such as mine stopes and tunnel support. According to the test needs, strain gauges of different specifications can be selected to monitor the stress in the three directions of transverse, longitudinal and tangential in real time. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 Prepare a flow chart for the stress test block.
[0030] Figure 2 This is a three-dimensional view of the stress test block.
[0031] Figure 3 Schematic diagram of the local structure of the stress test block.
[0032] Among them, 1: sand layer, 2: wire, 3: strain gauge, 4: moisture-proof coating, 5: similar material.
[0033] Figure 4 These are actual photos of the patch leads and moisture-proof process. The left picture shows the patch moisture-proof process; the right picture shows the sample after sand wrapping and packaging.
[0034] Figure 5 Photographs of the stress test block during zero drift testing.
[0035] Figure 6 This is the zero drift curve of the strain block during the zero drift test.
[0036] Figure 7 This is the layout diagram of the upper and lower rows of strain blocks for the mine model test.
[0037] Figure 8 shows the vertical and horizontal strain variation characteristics of the upper and lower measuring lines at different excavation stages.
[0038] FIG9 shows the final state of rock stratum fracture and fall, wherein FIG9(a) is an overview of rock stratum fracture, and FIG9(b) is a local fracture structure of the rock stratum.
[0039] Fig.10 This is the distribution characteristic diagram of the horizontal strain concentration coefficient of each strain block after large-scale rock collapse.
[0040] Fig.11 Photos of the excavation and recovery of the stress block. In the figure, (a) the stress block is exposed, (b) the stress block is recovered, and (c) the sample is recovered. DETAILED DESCRIPTION
[0041] The following specific embodiments are used to illustrate the present invention, but should not be construed as limiting the present invention.
[0042] In the embodiments, unless otherwise specified, the technical means used are conventional technical means in the art.
[0043] Test Example 1: Material Selection of Stress Test Block
[0044] The main body of the stress test is the stress test block (referred to as the stress block). After repeated optimization tests, its production process is divided into three stages: blank production, patch lead, and package sand wrapping. Blank production includes blank material selection, blank specification, blank molding and other links. Patch lead includes moisture-proof insulation, patch and other processes. The production process of the stress test block is as follows Figure 1 See the process photos for details. Figure 4 .
[0045] (1) Material selection
[0046] The mechanical properties of the stress test block and the model material should have good matching, so as to ensure that the stress test block and the model produce synchronous and coordinated deformation, and then reflect the stress change at the measuring point through the strain gauge reading on the surface of the block. To this end, the blank material uses a similar material ratio scheme with the same buried layer. Through years of similar material ratio experiments, the inventor's team has developed similar materials (referred to as SGC) with river sand, gypsum, and calcium carbonate as raw materials. The density of this type of similar material is 1800-1900kg / m3, the uniaxial compressive strength is 348-1100kPa, the elastic modulus is 0.11-0.725GPa, the Poisson's ratio is 0.028-0.404, and the cohesion is 0.13-0.33MPa. The model test application in recent years has shown that the SGC similar material basically meets the mechanical performance requirements of the coal mining model test. Due to space limitations, the mechanical indicators of some ratio schemes are listed here, see Table 1.
[0047] Table 1 Summary of mechanical parameters of SGC ratio scheme
[0048]
[0049] (2) Blank specifications and molding
[0050] The stress test block reflects the stress state of the point where the block is located, which is equivalent to the microelement in mechanical theory analysis. Therefore, the outer dimensions of the block should be much smaller than the minimum value of the three-dimensional dimensions of the model body, so as to minimize the interference of the block on the model stress field. The stress test block is intended to be implanted in the middle vertical section of the plane stress model of the stope and the plane strain model of the tunnel support. The thickness of the model body is 400mm and 300mm respectively. Drawing on the engineering experience that the excavation disturbance range of coal mine tunnels is 3 to 5 times the excavation span, the side length of the block should be less than 40mm and 30mm. Although the size of the block can be further reduced, considering the operability of similar material block making, demoulding, strain gauge size and subsequent strain gauge pasting processes, the blank specification is determined to be a rectangular block of 40mm×40mm×25mm, which is made by a mold.
[0051] (3) Selection of strain gauges and adhesives
[0052] At present, there are many types of strain gauges, including wire type, foil type, semiconductor type, thin film type and thick film type. According to the material and appearance characteristics of the blank, the cost performance of the five types of strain gauges in suitable working conditions and large-scale use in model tests is compared, and the metal foil strain gauge is selected. The characteristics of this type of strain gauge are stable performance and wide temperature range. In the field of force measurement and weighing sensors, 80% to 90% use metal foil strain gauges. The parameters of the foil strain gauge that match the blank size of the stress test block are shown in Table 2.
[0053] Table 2 Foil strain gauge parameters
[0054]
[0055] To ensure uniform bonding between the strain gauge base and the blank, an adhesive with low viscosity, fast curing and no irritating odor should be selected. By comparing the bonding mechanism and initial setting time of various adhesives such as 502, 495, and 914, it was determined to use 495 instant dry adhesive. The viscosity of the adhesive material is 20-60MPa·s, the initial setting time is 20 seconds, and the strain gauge patch takes an average of 10-15 seconds, so the initial setting time meets the patch operation requirements.
[0056] (4) Wire
[0057] Since the stress test block is placed in the model, the influence of the wire on the collapse and migration of the model body should be reduced as much as possible, and the natural rotation movement between the broken blocks of the model should not be interfered with, otherwise it will affect the accuracy of other test indicators. For this reason, there are strict requirements for the outer diameter, wear resistance, and folding resistance of the wire. Contradictory to this, since the stress test block is a single-point test, in order to obtain the distribution characteristics of the stress field inside the model, many measuring points are generally built in. When the number of wires is large, if the wire diameter is thick, it is easy to produce a "reinforcement effect", which interferes with the normal movement of the model block and even affects the structural characteristics of the overburden fracture. Therefore, under the premise of ensuring the transmission of wire signals, the outer diameter of the wire should be reduced as much as possible.
[0058] In the early stage of the test, enameled wire was used. Its advantage is that the outer diameter is very thin and there will be no "reinforcement effect" when implanted in the model body. Its disadvantage is that the toughness is poor. When the number of wires implanted in the model test is large, the lead wires are easy to bend and entangle. The paint color is single and the visual recognition is poor. In the early model test, it is difficult to comb the line, which increases the difficulty of troubleshooting the line fault.
[0059] After preliminary research, it was decided to use Teflon wire, which has been widely used in the electronics industry in recent years. Its jacket material is wear-resistant and fold-resistant polytetrafluoroethylene (Teflon). The minimum nominal cross-section of the wire is 0.05 mm2 and the outer diameter is 0.5 mm. This wire is implanted in the model body to minimize the "reinforcement effect" of the implanted wire. The wire parameters are shown in Table 3.
[0060] Table 3 Wire parameters of stress test block
[0061]
[0062] (5) Moisture-proof liquid
[0063] There are commercially available moisture-proofing liquids in the construction industry, but if used directly in stress test blocks, severe penetration will occur, causing the blocks to soften and disintegrate, affecting the working performance of the blocks.
[0064] The moisture-proof liquid of the present invention is prepared by dissolving polyethylene particles in an organic solvent; the organic solvent is toluene. The mass ratio of polyethylene particles to organic solvent is 1: (20-50). After the moisture-proof liquid is applied to the outer surface of the block, the organic solvent component in the moisture-proof liquid will volatilize, so the organic solvent will not penetrate into the blank. After the moisture-proof coating is dried, a moisture-proof and insulating polyethylene moisture-proof coating is formed on the outer surface of the block. According to experimental test experience, after the moisture-proof liquid is applied 4 to 6 times, the film thickness formed by the coating meets the moisture-proof requirements. Since the elastic modulus of the outer coating is between the strain gauge substrate and similar materials, the deformation of the block can be accurately transmitted to the strain gauge, ensuring good deformation coordination between the two, and realizing accurate measurement of strain at the measuring point.
[0065] Example 1
[0066] See also Figure 3 , a stress test block, comprising a blank, a strain gauge 3, a moisture-proof coating 4 and a sand layer 1;
[0067] The blank is a block made of a similar material 5 (SGC material), and a strain gauge 3 is attached to the block; the moisture-proof coating 4 covers the outside of the block, between the block and the strain gauge, and the outside of the strain gauge 3 respectively;
[0068] The blank is a rectangular parallelepiped, the strain gauge has 1 to 3 pieces, and the angle between the long side of the strain gauge and one side of the surface is 0 degrees, 90 degrees or 45 degrees (when in use, the plane where the strain gauge is located is perpendicular to the horizontal plane, and one side of the surface where it is located is the bottom side); specifically, in this embodiment, there are 2 pieces, and the angles with the bottom side are 0 degrees and 90 degrees respectively. The strain gauge is bonded to the moisture-proof coating by 495 instant adhesive; the sand layer is arranged on the outer surface of the moisture-proof coating.
[0069] The wire 2 connected to the strain gauge is a Teflon wire with a nominal cross section of 0.05 mm 2 , outer diameter is 0.5mm.
[0070] This embodiment further proposes a method for preparing the stress test block, comprising the steps of:
[0071] 1) Using a special mold to press similar materials into a green body, wherein the similar materials are composed of river sand as coarse aggregate, calcium carbonate as fine aggregate, and gypsum as adhesive;
[0072] 2) Apply moisture-proof liquid on the blank, let it dry at room temperature for 1.5 to 2 hours, then apply and dry again, a total of 4 to 6 times. After drying, paste the strain gauge;
[0073] The moisture-proof liquid is prepared by dissolving polyethylene particles in toluene; the mass ratio of the polyethylene particles to the toluene is 1:30.
[0074] 3) Apply moisture-proof liquid on the block prepared in step 2), dry at room temperature for 1.5 to 2 hours, apply and dry again, apply 2 to 3 times in total, and dip standard sand particles before the moisture-proof liquid applied for the last time dries.
[0075] Example 2
[0076] A stress test block comprises a blank, a strain gauge, a moisture-proof coating and a sand layer;
[0077] The blank is a block made of similar material (SGC material), and a strain gauge is attached to the block; the moisture-proof coating is arranged on the outside of the block, between the block and the strain gauge, and outside the strain gauge;
[0078] The blank is a cube, and the strain gauge has one piece, and the angle with the bottom edge is 0 degree. The strain gauge is bonded to the moisture-proof coating by 495 instant adhesive; and the sand layer is arranged on the outer surface of the moisture-proof coating.
[0079] The wire connected to the strain gauge is a Teflon wire with a nominal cross section of 0.05mm 2 , outer diameter is 0.5mm.
[0080] The preparation method of the stress test block is the same as that of Example 1.
[0081] Example 3
[0082] A stress test block comprises a blank, a strain gauge, a moisture-proof coating and a sand layer;
[0083] The blank is a block made of similar material (SGC material), and a strain gauge is attached to the block; the moisture-proof coating is arranged on the outside of the block, between the block and the strain gauge, and outside the strain gauge;
[0084] See also Figure 2 In this embodiment, the blank is a cube, and there are three strain gauges, with angles of 0 degrees, 45 degrees and 90 degrees to the bottom edge respectively. The strain gauge is bonded to the moisture-proof coating by 495 instant adhesive; and the sand layer is arranged on the outer surface of the moisture-proof coating.
[0085] The wire connected to the strain gauge is a Teflon wire with a nominal cross section of 0.05mm 2 , outer diameter is 0.5mm.
[0086] The preparation method of the stress test block is the same as that in Example 1.
[0087] Test Example 2: Moisture-proof insulation and zero drift test
[0088] As mentioned above, the stress block is buried in a similar material model. During the model laying and drying and curing stage, the block is surrounded by relatively moist similar materials that have not yet dried. Therefore, the stress block needs to have good moisture-proof insulation performance. In addition, due to the long test cycle of the model test, the stress block needs to maintain a low long-term zero drift value to ensure the accuracy of the test data. According to the above performance requirements, the stress block samples need to be tested for moisture-proof insulation and long-term zero drift.
[0089] (1) Moisture-proof insulation performance test
[0090] Refer to the "Determination Method of Density of Coal and Rock Blocks" to test the moisture resistance of the block. Test process: First, use a dry towel to clean the dust on the surface of the stress block, and weigh M0 on the balance; then place the stress block in a beaker of water and soak it for 24 hours. After taking out the stress block, wipe off the surface moisture, use a hot air blower to dry any remaining moisture on the surface, and weigh M1 on the balance again. If the difference between M1 and M0 is less than 0.5 grams, the moisture resistance is considered qualified, otherwise it means that water has penetrated into the test piece, and it is considered to be moisture-proof failure. After the moisture resistance test is passed, the resistance value of the stress block is tested synchronously, and the insulation performance test is carried out.
[0091] After testing, the moisture-proof performance and insulation performance of the stress test blocks of Examples 1-3 are qualified.
[0092] (2) Zero drift test
[0093] The sensitive element of the stress block is the strain gauge. According to the working characteristics of the strain gauge, when conducting resistance strain testing, due to external environmental changes such as time, temperature, and electromagnetic fields, the measured value will change, and the strain gauge will often have zero drift, referred to as zero drift.
[0094] According to the test plan of the stope model test, the test cycle is more than 48 hours. Considering the large temperature difference between day and night in summer and winter, the wiring method between the strain gauge and the strain meter has taken temperature compensation measures to eliminate the interference of the temperature difference between day and night on the test data; but due to the long test cycle, the stress block is bound to have zero drift, so it is necessary to test the zero drift characteristics of the stress block during the actual test, and compare the zero drift value with the test data of the stress block. Only when the zero drift value is much lower than the test data can the reliability of the test results be guaranteed, otherwise it will interfere with the overall test results.
[0095] The stress block zero drift test plan is to first lay a model of similar materials that are exactly the same as the formal test according to the field model test plan. The top of the model is a free surface. Since the weight of the model is much lower than the load applied by the top cylinder during the formal test, the stress block is approximately considered to be in a zero point state. Along the height direction of the model, 5 rows of stress blocks are buried from bottom to top in the model, totaling 42 blocks. Each stress block contains 1 vertical sheet and 1 horizontal sheet, totaling 84 strain gauges. Test scenarios such as Figure 5 shown.
[0096] Before the zero drift test, each stress block was connected to the strain gauge, and after the data of each channel was cleared, the timed automatic sampling mode was started, and the strain data timed sampling cycle was 10 seconds. The test lasted 48 hours and 17,280 sets of data were collected.
[0097] Due to space limitations, only the test data of the first and second rows of stress blocks (made in Example 1) are listed below. Figure 6As shown. The maximum zero drift value of each stress block for 48 hours is shown in Table 4. Statistics show that the maximum zero drift values of each vertical and horizontal strain gauge on the block are 7.8με and 8.5με respectively. In comparison, during the excavation test of the formal model, the strain value of each strain gauge varies from 115 to 240με. It can be seen that compared with the test values during the model excavation period, the strain block zero drift accounts for only 3.25%-6.78%, which has no significant effect on the test results.
[0098] Table 4 Statistics of zero drift of each stress block for 48 hours
[0099]
[0100]
[0101] Note: The meaning of the numbers in the table is: "1-1 vertical sheet" means the strain gauge of the first stress block in the first row for testing vertical stress; "1-1 horizontal sheet" means the strain gauge of the first stress block in the first row for testing horizontal stress. The same applies to other strain gauges.
[0102] The zero drift results of the stress test blocks prepared in Examples 2-3 were also qualified.
[0103] Application Examples
[0104] In order to verify the test effect of stress blocks in model tests, stress blocks were buried inside the model during model laying to monitor the stress distribution characteristics inside the model during excavation. The model uses the large mining height fully mechanized mining face in Jincheng Mining Area in my country as the engineering prototype. The purpose of the test is to study the mine pressure and rock movement characteristics of the large mining height fully mechanized mining face. The arrangement scheme of each stress block in the model is shown in Figure 7 The model is 1850mm high and 5000mm long.
[0105] At the beginning of the experimental plan, based on the key layer theory of rock layer control, it was determined that the fine sandstone with a thickness of 17.00m (upper) and 6.00m (lower) was sub-key layer 2 and sub-key layer 1 respectively. The breaking of sub-key layer 2 would cause a large-scale collapse of the overburden. To this end, a row of measuring lines was arranged in each corresponding layer in the model, focusing on the stress distribution characteristics of these two sub-key layers, such as Figure 7 As shown, subcritical layer 2 and subcritical layer 1 are framed by dotted lines in the figure. The stress blocks are made by using Example 1 (wherein, the material of the upper 1-9# stress blocks is selected from Class A SGC similar materials in Table 1, and the lower 10-18# stress blocks are selected from Class D SGC similar materials, that is, the same model materials as the layers where the strain blocks are located are respectively used), the spacing between adjacent blocks is 500mm, and a total of 18 blocks are buried. During the model excavation process, the stress test block is connected to the test instrument to collect and store the test data of the strain gauge in real time, and then the deformation parameters of the block at different test stages are obtained.
[0106] When analyzing the block stress data after the test, in order to facilitate data comparison and analysis, a dimensionless processing method was used to compare the strain values of the measuring points at different test stages with their initial strain values, and the ratio of the two was defined as the strain concentration coefficient at the measuring point. Since the elastic modulus and other indicators of the same measuring point are constants, according to the classical analysis theory of generalized Hooke's law, the strain increment and stress increment of each measuring point are positively correlated, so the strain concentration coefficient of each measuring point can reflect its stress concentration coefficient, and the stress change at the measuring point of each block is determined accordingly, and then the stress field change characteristics of the entire model body are obtained by inversion.
[0107] The vertical and horizontal strain characteristics of the upper and lower rows of survey lines at different excavation stages are shown in Figure 8. Figure 8 (a) vertical strain (upper row of survey lines); Figure 8 (b) vertical strain (lower row of survey lines); Figure 8 (c) horizontal strain (upper row of survey lines); Figure 8 (d) horizontal strain (lower row of survey lines). It can be seen from the figure that the vertical and horizontal strain concentration factors of the upper rock layer show an increasing trend as a whole during the excavation process. The three peak values of the vertical strain of the upper row of survey lines are particularly obvious. When it is close to the limit span and is about to break, the vertical strain peak coefficients of the survey lines increase to 3.93, 2.59 and 3.97 respectively, and the horizontal strain peaks increase to 3.52 and 7.12. The change trend of the lower row of survey lines is similar.
[0108] When the model was excavated to the 39th, 51st and 57th stages, the lower rock layer experienced initial and periodic pressure. At the 59th stage, the upper rock layer fell from bottom to top three times, and the final state of the rock layer breaking and falling is shown in Figure 9. According to the fracture structure morphology of each rock layer, the layers below 6.00m fine sandstone (not included) showed periodic cantilever fracture, and the maximum hanging top length before fracture was 45cm, which caused periodic pressure on the working face. The blocks above 6.00m fine sandstone were arranged closely after the fracture, and under the action of horizontal extrusion pressure, the blocks were hinged to form a force transmission structure.
[0109] After the upper rock layer collapsed on a large scale, the stress distribution characteristics of each stress block on the two measuring lines are as follows: Fig.10 As shown in the figure, the upper row of measuring lines are located near the overburden fracture line at the 3# and 7# measuring points, and their horizontal strain coefficients are as high as 9.10 and 28.06. The lower row of measuring lines is located near the fracture line at the 16# measuring point, and the coefficient reaches 7.20. Under the action of horizontal compression, the blocks are closely and orderly arranged, and the masonry beam structure is formed by hinge connection. According to the test results, the peak value of the horizontal compression force of the masonry beam structure appears near the front and rear fracture boundary lines of the overburden, especially the front boundary line, and the peak value is much higher than other measuring points in the same layer.
[0110] In order to verify the moisture resistance and reusability of the stress blocks, the excavation and recovery of the stress blocks were carried out simultaneously during the subsequent dismantling of the model, such as Fig.11As shown in the figure, the exposed stress block has a complete appearance, and after being coated with standard sand, the stress block can maintain a tight bond with the surrounding model body. The stress block can be completely recovered, and the recovered stress block has been used in subsequent model tests, showing good reusability.
[0111] The above embodiments are merely descriptions of specific implementation methods of the present invention, and are not intended to limit the scope of the present invention. Those skilled in the art may make various modifications and changes based on the prior art. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary engineering and technical personnel in the field shall fall within the protection scope determined by the claims of the present invention.
Claims
1. A method for preparing a model test stress test block, characterized in that: The following steps are involved: 1) Pressing similar materials into a green body; the similar materials are made of river sand, gypsum, and calcium carbonate, and the density of the similar materials is 1800-1900 kg / m 3 , uniaxial compressive strength 348 ~ 1100kPa, elastic modulus 0.11 ~ 0.725GPa, Poisson's ratio 0.028 ~ 0.404, cohesion 0.13 ~ 0.33MPa; 2) Apply moisture-proof liquid on the blank and dry it at room temperature for 1.5 to 2 hours; continue to apply and dry for 4 to 6 times, and then paste the strain gauge; the moisture-proof liquid is made of polyethylene particles dissolved in an organic solvent; the organic solvent is one or more of toluene, ethylbenzene, and xylene; the mass ratio of the polyethylene particles to the organic solvent is 1: (20 to 50); the strain gauge is a foil strain gauge; 3) Apply moisture-proof liquid on the block made in step 2), dry it at room temperature for 1.5 to 2 hours, apply it again and dry it, apply it 2 to 3 times in total, and dip the standard sand particles in the moisture-proof liquid applied for the last time before it dries.
2. The model test stress test block obtained by the preparation method of the model test stress test block according to claim 1 is characterized in that: It includes a blank, a moisture-proof coating, a strain gauge and a sand layer; The blank is a block made of a material similar to the model material, and a strain gauge is attached to the outer surface of the block; the moisture-proof coating is attached to the outer surface of the block, between the block and the strain gauge, and the outer surface of the strain gauge; The sand layer is attached to the outer surface of the moisture-proof coating.
3. The model test stress test block according to claim 2, characterized in that: The strain gauge is adhered to the outer surface of the moisture-proof coating by using ethyl α-cyanoacrylate adhesive.
4. The model test stress test block according to claim 2, characterized in that: The block is a cuboid, and there are 1 to 3 strain gauges located on one surface of the block. The angle between the long side of the strain gauge and one side of the surface on which it is located is 0 degrees, 90 degrees or 45 degrees.
5. The model test stress test block according to claim 2, characterized in that: The block is a cube, and there are 1 to 3 strain gauges located on one surface of the block. The angle between the long side of the strain gauge and one side of the surface where it is located is 0 degrees, 90 degrees or 45 degrees.
6. The model test stress test block according to claim 4 or 5, characterized in that: The outer jacket material of the external wire is polytetrafluoroethylene, and the minimum nominal cross-section of the wire is 0.05mm 2 .
7. The method for using the model test stress test block according to any one of claims 2 to 6, characterized in that: Includes operations: During the process of laying the similar material model, the stress test block is buried at a predetermined position inside the model, and the wire is led out and exposed outside the model; After the similar material model is dried and cured, the model is subjected to a staged excavation test, and the stress test block tests the stress at different positions of the model in real time; During the model test, the stress test block is connected to the test instrument through a wire to collect and store the test data of the strain gauge in real time, thereby obtaining the deformation parameters of the block at different test stages; When performing block stress analysis after the test, a dimensionless processing method was used to compare the strain values of the stress test block at different excavation stages with its initial strain values, and the ratio of the two was defined as the strain concentration coefficient at the measuring point; based on the corresponding relationship between block strain and stress change, the stress change at the measuring point where each block is located was determined, and then the stress field change characteristics of the entire model body were obtained.
8. The method of use according to claim 7, characterized in that: After the model test, the stress test block is recovered and reused in subsequent model tests.