A technology for concrete structures and construction methods, which is applied in basic structural engineering, underwater structures, artificial islands, etc., can solve problems such as affecting the normal use and durability of concrete structural engineering, troublesome leakage control, and lack of gripping force. , to achieve the effect of overcoming anti-leakage treatment, high construction efficiency and wide application range
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2019-08-20
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 1
Abstract
Description
Technical field
[0001] The invention relates to the technical field of concrete construction, in particular to a construction method for preventing leakage of a concrete structure joint. Background technique
[0002] The anti-leakage treatment of concrete structure joints is the basic link of engineering structure waterproofing. The incompatibility of the interface between the new and the old concrete and the improper handling of the cold joints are the main causes of water leakage in the joints of the concrete structure, and it is also one of the problems in the waterproofing of the concrete structure. The construction joints of concrete structures, post-pouring belts, joints of structural members, superimposed members, etc. all have problems dealing with the interface between new and old concrete.
[0003] The traditional anti-leakage treatment for joints of concrete structures mainly relies on the compactness and impermeability of the concrete itself. By improving the impermea...
Examples
Embodiment
[0036] Please refer to figure 1 , A construction method for preventing leakage of concrete structure joints, including the following steps:
[0037] S1. After chipping the old concrete joint interface and spraying water to keep it wet;
[0038] S2. After there is no clear water on the joint interface of the old concrete, spray permeable crystalline inorganic waterproof material on the joint interface of the old concrete;
[0039] S3. After the permeable crystalline inorganic waterproof material is solidified, rinse the joint interface of the old concrete with clean water, and remove the harmful substances replaced by the permeable crystalline inorganic waterproof material from the concrete;
[0040] S4. Set steel waterstop at the interface of the old concrete joint;
[0041] S5. Paint polymer emulsion on the interface of steel waterstop first, and then paint polymer cement-based waterproof coating;
[0042] S6. Spray a certain thickness of cement slurry mixture mixed with permeable crys...