Protection components

A layered insulating resin structure with conductive metal thin layers and a bridge pattern addresses the inconsistency in resistance and disconnection time of existing protection elements, providing a reliable overcurrent blocking solution.

CN110828255BActive Publication Date: 2024-12-03TE CONNECTIVITY JAPAN GK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201910733866.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-08-08
Filing Date
2019-08-08
Publication Date
2024-12-03
Estimated Expiration
2039-08-08

AI Technical Summary

Technical Problem

Existing protection elements, such as polymer PTC elements, suffer from variations in resistance value and disconnection time due to thickness variations in the fuse layer formed by electroplating, which can lead to inconsistent performance when blocking overcurrents.

Method used

A protection element with a layered insulating resin structure featuring conductive metal thin layers on both main surfaces, connected via a conductive connection through a through-opening, and a bridge pattern that ensures consistent resistance and disconnection time by controlling the thickness and arrangement of the metal layers.

Benefits of technology

The solution provides a protection element with minimal variation in resistance value and disconnection time, ensuring reliable and consistent overcurrent blocking capabilities.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110828255B_ABST
    Figure CN110828255B_ABST
Patent Text Reader

Abstract

The present invention provides a protection element with a small change in resistance value and disconnection time of a fuse layer. The protection element of the present invention comprises a layered element formed of an insulating resin and a conductive metal thin layer arranged on at least one of the two main surfaces of the layered element, wherein at least one of the conductive metal thin layers has a fuse pattern.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a protection element for protecting an electrical device, and more particularly to a protection element or circuit included in the electrical device. Background Art

[0002] PTC elements, temperature fuse elements, current fuse elements, etc. are used as protection elements that block the flow of current when an overcurrent flows through an electrical device. Among them, when used in a cylindrical secondary battery, a polymer PTC element helps to effectively utilize the space inside the battery because the polymer PTC element can be arranged on the sealing plate of the secondary battery by being accommodated in the sealing plate of the secondary battery.

[0003] Although the above-mentioned polymer PTC element is reversible, problems may occur depending on the application. For example, when the PTC element is used in a plurality of cylindrical lithium-ion secondary battery cells used in parallel, the battery cell may continue to generate heat unless the short-circuit unit using the PTC element is removed. The PTC element is also disadvantageous when a large current is continuously energized because the PTC element has a relatively small rated capacity.

[0004] As a protection element that takes these problems into consideration, a protection element is known that includes an insulating layered element having at least one through-opening, a conductive metal thin layer located on each main surface of the layered element, and a fuse layer located on a side surface defining at least one of the through-openings and electrically connected to the conductive metal thin layer (Patent Document 1). With this protection element, even if the overcurrent does not significantly exceed the rated amount, for example, even if the overcurrent is approximately twice the rated amount, the overcurrent can be quickly and reliably blocked while allowing a large current to flow.

[0005] [Prior art literature]

[0006] [Patent Document]

[0007] Patent Document 1: WO2014 / 034833 Summary of the invention

[0008] [Problems to be Solved by the Invention]

[0009] The protection element described in Patent Document 1 has a fuse layer formed on the side surface of the through opening by electroplating (particularly electrolytic plating). The fuse layer has a predetermined cross-sectional area to obtain a predetermined fuse function. This cross-sectional area can be adjusted according to the thickness of the fuse layer; however, when the fuse layer is formed by electroplating on the side surface of the through opening, a thickness variation of about ±20% may occur. In other words, the resistance value, disconnection time, etc. of the protection element may vary.

[0010] An object of the present invention is to provide a protection element having a small change in the resistance value of a fuse layer and a disconnection time.

[0011] [Methods of solving the problem]

[0012] The present disclosure includes the following aspects.

[0013] According to one aspect of the present invention, there is provided a protection element, comprising: a layered element formed of an insulating resin; and a conductive metal thin layer disposed on at least one of two main surfaces of the layered element. At least one of the conductive metal thin layers has a fuse pattern.

[0014] In an exemplary embodiment according to the present invention, the layered element has at least one through-opening, the conductive metal thin layers are arranged on both main surfaces of the layered element, and the conductive metal thin layers arranged on the two main surfaces of the layered element are electrically connected via a conductive connection passing through the through-opening.

[0015] In an exemplary embodiment according to the present invention, the laminar element is a ring with a through opening in the center.

[0016] In an exemplary embodiment according to the present invention, the conductive metal thin layer arranged on a main surface of the annular layered element includes a first annular metal thin layer located on the outer edge side of the annular layered element, a second annular metal thin layer located on the inner edge side of the annular layered element, and a bridging portion for electrically connecting the first annular metal thin layer and the second annular metal thin layer.

[0017] In an exemplary embodiment according to the invention, there is a bridge.

[0018] In an exemplary embodiment according to the invention, there are two to eight bridges relative to the center of the ring.

[0019] In an exemplary embodiment according to the present invention, the distance between the first annular metal thin layer and the second annular metal thin layer is 0.1 mm to 5.0 mm.

[0020] In an exemplary embodiment according to the present invention, the width of the first annular metal thin layer is greater than the width of the second annular metal thin layer.

[0021] In an exemplary embodiment according to the present invention, the conductive metal thin layer includes nickel foil or copper foil.

[0022] In an exemplary embodiment according to the present invention, the protection element further includes an insulating layer on the conductive metal thin layer having the fuse pattern, and the insulating layer at least covers the fuse pattern.

[0023] According to another aspect of the present invention, an electrical device is provided, comprising the protection element as described above.

[0024] According to yet another aspect of the present invention, a sealing body is provided, wherein the sealing body comprises the protection element as described above.

[0025] According to yet another aspect of the present invention, there is provided a secondary battery cell including the protection element as described above.

[0026] [Effects of the invention]

[0027] According to the present disclosure, a protection element having a small variation in the resistance value and disconnection time of a fuse layer is provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 schematically illustrates a protection element according to an embodiment of the present invention; and

[0029] Figure 2 Schematically shows Figure 1 A cross-sectional view of the protection element shown along line xx.

[0030] [reference numerals list]

[0031] 1: Protection element

[0032] 2: Layered components

[0033] 3, 4: Conductive metal thin layer

[0034] 5: Conductive connection

[0035] 6: Bridge

[0036] 7: The first annular metal layer

[0037] 8: Second annular metal layer

[0038] 9: Through opening DETAILED DESCRIPTION

[0039] The protection element of the present disclosure will be described in detail with reference to the accompanying drawings.

[0040] like Figure 1 and Figure 2As shown, a protection element 1 according to an embodiment of the present disclosure includes an annular layered element 2 formed of an insulating resin, conductive metal thin layers 3 and 4 arranged on two main surfaces of the layered element 2, and a conductive connecting portion 5, which is arranged on the inner wall surface of the through opening and electrically connects the conductive metal thin layers 3 and 4. The conductive metal thin layer 3 on one main surface of the layered element 2 has a bridge portion 6, which is a fuse pattern. The conductive metal thin layer 3 includes a first annular metal thin layer 7 located on the outer edge side of the annular layered element 2, a second annular metal thin layer 8 located at the inner edge of the annular layered element 2, and a bridge portion 6 electrically connecting the first annular metal thin layer 7 and the second annular metal thin layer 8. The layered element 2, the first annular metal thin layer 7 and the second annular metal thin layer 8 are arranged in a concentric manner. In the protection element 1, the current flows in the order of the first annular metal thin layer 7, the bridge portion 6, the second annular metal thin layer 8, the conductive connecting portion 5 and the conductive metal thin layer 4 (or vice versa). When an excessive current flows through such a protection element 1 , the bridge portion 6 as a fuse pattern is melted to block the current.

[0041] According to the present embodiment, the layer element 2 is a ring having a through opening 9 at the center. The through opening 9 penetrates the layer element 2 along the thickness direction of the layer element and has a circular planar shape (ie, a cross-sectional shape perpendicular to the thickness direction).

[0042] In addition, it should be noted that in the present disclosure, the shape of the layered element, the presence or absence of through openings, and the shape of the through openings are not limited to the present embodiment.

[0043] For example, the form of the laminar element is not particularly limited, as long as the thickness dimension is smaller than the other dimensions, and preferably substantially smaller (e.g., a sheet-like form). The plane shape of the laminar element or the cross-sectional shape of the laminar element perpendicular to the thickness direction of the laminar element preferably has a shape of geometric linear symmetry and / or point symmetry, such as a circular shape, a square shape, a rectangular shape, a rhombus shape, an annular shape (particularly a circular annular shape or a so-called annular shape), etc. In addition, the laminar element may be a plate-like member without a through opening.

[0044] Through openings may or may not be present. If through openings are present, there may be one or two or more through openings, for example, two to eight through openings. If there are multiple through openings, the through openings are preferably arranged equally relative to the center. By arranging them uniformly, the length of the current path flowing through the conductive metal thin layer can be made shorter, and the resistance in the conductive metal thin layer can be made smaller.

[0045] The planar shape of the through opening may be circular, square, diamond, rectangular or elliptical.

[0046] The thickness of the layered element 2 is not particularly limited, but can be, for example, 0.03mm to 10mm, preferably 0.05mm to 5.0mm, more preferably 0.1mm to 2.0mm, even more preferably 0.1mm to 1.0mm, and particularly preferably 0.2mm to 0.5mm. By setting the thickness of the layered element to 10mm or less, the protective element is advantageously miniaturized. Reducing the thickness of the layered element advantageously makes the layered element more compact, for example, when the protective element is used in a battery, the volume of the battery cell can be made larger. By setting the thickness of the layered element to not less than 0.03mm, the resistance voltage between the two main surfaces of the layered element can be fully ensured. By making the layered element thicker, a higher pressure resistance is achieved, thereby allowing the layered element to be used at a higher voltage.

[0047] The insulating resin constituting the laminar element 2 is not particularly limited, as long as the insulating resin is an electrical insulating resin. Exemplary insulating resins include resins such as polyethylene, polypropylene, polycarbonate, fluororesin, acrylonitrile-butadiene-styrene (ABS) resin, polycarbonate-ABS alloy resin, polybutylene terephthalate (PBT) resin, and elastomers. This insulating resin has the same flexibility as the polymer used for the polymer PTC element, so the protection element of the present invention can be preferably incorporated into various electrical devices, for example, incorporated into the sealing plate of the secondary battery cell, rather than incorporated into the polymer PTC element. Particularly preferably, the insulating resin can be polyethylene or polyvinylidene fluoride.

[0048] According to the present embodiment, the conductive metal thin layers 3 , 4 are respectively arranged on the two main surfaces of the layered element 2 .

[0049] The conductive metal thin layer is not particularly limited and the conductive metal thin layer may be constructed of a metal such as nickel, copper, aluminum, gold, etc., as long as it is a conductive metal thin layer. Such a conductive metal thin layer may be a single layer or may be formed of a plurality of metal thin layers. The conductive metal thin layer may preferably be a nickel foil or a laminate of nickel and copper (nickel-copper foil). When the copper foil is a nickel-copper foil, the copper foil is preferably located on the insulating resin side.

[0050] The thickness of the conductive metal thin layer is not particularly limited, but may be, for example, 0.1 μm to 300 μm, preferably 1.0 μm to 100 μm, and more preferably 5.0 μm to 50 μm. By making the thickness of the conductive metal thin layer larger, the resistance of the conductive metal thin layer can be made smaller. On the other hand, by making the thickness of the conductive metal thin layer smaller, the thickness of the protective element can be made smaller, which is advantageous in terms of miniaturization.

[0051] The laminar element in which the conductive metal thin layer is located on each main surface can be manufactured by simultaneously extruding the insulating resin forming the laminar element together with the metal sheet (or metal foil) constituting the metal thin layer, thereby obtaining an extrudate in which the insulating resin is sandwiched between the conductive metal thin layers. On the other hand, the laminar element can be manufactured by obtaining a laminar product of the insulating resin (for example, by extrusion), sandwiching the laminar product between the conductive metal thin layers, and hot-pressing the laminar product and the conductive metal thin layers together to obtain a press-fit body. In yet another aspect, the laminar element can be manufactured by forming a plating layer on the laminar element.

[0052] In the present embodiment, the conductive metal thin layer 3 comprises a first annular metal thin layer 7 located on the outer edge side of the annular layer element 2, a second annular metal thin layer 8 located on the inner edge side of the annular layer element 2, and a bridge portion 6 electrically connecting the first annular metal thin layer 7 and the second annular metal thin layer 8. The first annular metal thin layer 7 and the second annular metal thin layer 8 are arranged concentrically along the layer element 2. On one main surface of the layer element, the first annular metal thin layer 7 occupies an area of ​​a predetermined distance inward from the outer edge, and the second annular metal thin layer 8 occupies an area of ​​a predetermined distance outward from the inner edge. The first annular metal thin layer 7 and the second annular metal thin layer 8 are not in direct contact, and the four bridge portions 6 are electrically connected by cross-linking the first annular metal thin layer 7 and the second annular metal thin layer 8. The bridge portion 6 corresponds to a fuse pattern, and when an overcurrent flows through the protection element, the fuse pattern is blown to block the current.

[0053] Note that in the protection element according to the present disclosure, a "fuse pattern" refers to a pattern configured to be cut off in response to an excessive current or abnormal heat generation. Therefore, the shape is not particularly limited as long as the shape performs the function.

[0054] In this embodiment, the width of the first annular metal thin layer 7 is greater than the width of the second annular metal thin layer 8. By making the width of the first annular metal thin layer 7 greater, it is easy to fix the protection element 1 when attaching the protection element 1 to other components. In addition, by fixing the outer side of the protection element, the influence of pressure on the bridge portion can be reduced.

[0055] The width of the first annular metal thin layer 7 is not particularly limited, but can be, for example, 1.0 mm to 20 mm, preferably 2.0 mm to 15 mm, and more preferably 5.0 mm to 10 mm. By increasing the width of the first annular metal thin layer 7, when the protection element 1 is electrically connected to other electrical elements at the first annular metal thin layer 7, the contact area can be increased, thereby making it easy to make the connection and reducing the resistance at the connection point.

[0056] The width of the second annular metal thin layer 8 is not particularly limited, but may be, for example, 0.1 mm to 18 mm, preferably 0.5 mm to 10 mm, and more preferably 1.0 mm to 8.0 mm.

[0057] The distance between the first annular metal thin layer and the second annular metal thin layer is not particularly limited as long as the insulation distance can be ensured. For example, the distance can be, for example, 0.1 mm to 5.0 mm, preferably 0.5 mm to 3.0 mm. By increasing the distance between the first annular metal thin layer and the second annular metal thin layer, the insulation between the first annular metal thin layer and the second annular metal thin layer can be made more reliable. In addition, the bridge portion 6 can be more reliably prevented from being connected after fusing. By reducing the distance between the first annular metal thin layer and the second annular metal thin layer, the length of the bridge portion can be reduced, thereby reducing the resistance of the bridge portion.

[0058] The length of the bridge portion 6 (the length from the position in contact with the first annular metal thin layer to the position in contact with the second annular metal thin layer) is substantially equal to the distance between the first annular metal thin layer and the second annular metal thin layer. That is, the length of the bridge portion 6 is not particularly limited, but may be, for example, 0.1 mm to 5.0 mm, and preferably 0.5 mm to 3.0 mm.

[0059] The width of the bridge portion 6 is not particularly limited, but may be, for example, 0.1 mm to 5.0 mm, preferably 0.5 mm to 3.0 mm.

[0060] Note that, in the present embodiment, the number of bridge portions 6 is four, but the number is not particularly limited.

[0061] In one aspect, there is one bridge. Since there is only one bridge, the bridge can be blown faster and more reliably when the protection element is operated. In addition, after the bridge is blown, the insulation distance at the fuse part can be more reliably ensured.

[0062] In another aspect, the number of bridges may be two or more, for example, 2 to 8, more preferably 3 to 6. By increasing the number of bridges to be greater than the number of bridges, for example, making the number of bridges greater than two or more, in addition to being able to suppress arcing, the rated current can be made larger. In addition, by making the number of bridges greater, the mechanical strength of the protection element can be increased.

[0063] When there are multiple bridges, the bridges are arranged at equal angles relative to the center of the ring. By placing the bridges at equal angles relative to the center of the ring, the length of the current path through the conductive metal thin layer can be shortened and the resistance in the conductive metal thin layer can be made smaller.

[0064] In the protection element of the present disclosure, at least a portion of the metal thin layer having the above-mentioned fuse pattern may have an insulating layer.

[0065] In one aspect, an insulating layer is provided to cover the fuse pattern (the bridge portion in the above embodiment). By covering the fuse pattern with the insulating layer, scattering of metal at the time of blowing can be prevented.

[0066] In one aspect, the insulating layer is an annular ring concentric with the laminar element 2 and is arranged to cover the outside of the bridge (i.e., fuse pattern) from the inner edge of the annular ring of the laminar element. Preferably, the distance between the outer edge of the insulating layer and the edge of the bridge (the edge on the outer edge side of the annular ring) can be 0.1 mm to 2.0 mm.

[0067] The insulating layer is provided so that a portion of the metal thin layer is exposed. In the exposed portion of the metal thin layer, the protection element of the present disclosure can be connected to other electrical elements.

[0068] In a preferred aspect, the insulating layer is an annular ring concentric with the layered element 2, which is arranged to cover the inner edge of the circular ring of the layered element to the outside or even farther than the bridging portion (i.e., the fuse pattern), and the annular metal thin layer is arranged to be exposed in an area at a predetermined distance from the outer edge.

[0069] The thickness of the insulating layer is not particularly limited, but may be, for example, 1 μm to 50 μm, preferably 5 μm to 15 μm.

[0070] Although the insulating resin is not particularly limited as long as the insulating resin is an electrically insulating resin, a resin having high heat resistance (eg, solder resist) is preferable.

[0071] The protection element 1 is located on the side surface defining the through opening 9, which has a conductive connection 5 electrically connecting the conductive metal thin layers 3 and 4 located on the two side main surfaces of the layered element 2. In other words, the conductive metal thin layers 3 and 4 are electrically connected through the conductive connection 5 passing through the through opening 9.

[0072] The conductive connection part 5 is preferably a conductive layer. The conductive connection part 5 may be a single layer, or may be composed of two or more layers (for example, two layers, three layers, or four layers).

[0073] Although the material constituting the conductive connection portion 5 is not particularly limited as long as the material is conductive, the material may be, for example, a metal such as nickel, copper, aluminum, gold, or the like.

[0074] The conductive connection 5 is preferably formed by electroplating.

[0075] The thickness of the conductive connection part 5 is not particularly limited as long as the conductive connection part 5 is not blown earlier than the bridge part. The thickness of the conductive connection part 5 can be, for example, 1.0 μm to 500 μm, preferably 5.0 μm to 300 μm, and more preferably 10 μm to 200 μm. By setting the thickness of the conductive connection part 5 to not less than 1.0 μm, the resistance of the conductive connection part 5 can be reduced. In addition, by setting the thickness of the conductive connection part 5 to not more than 500 μm, it is easy to form the conductive connection part 5. In particular, when the conductive connection part 5 is formed by electroplating, by setting the thickness of the conductive connection part 5 to 20 μm or less, the conductive connection part 5 can be more easily formed.

[0076] In one aspect, the protection element of the present invention can be obtained by forming a conductive metal thin layer on a major surface of a layered element and then removing a portion of the conductive metal thin layer to form a fuse pattern.

[0077] In a preferred aspect, the protection element of the present disclosure comprises the following steps:

[0078] forming a through opening in the laminar element;

[0079] applying a thin layer of conductive metal to both major surfaces of the layered element;

[0080] forming a fuse pattern by etching at least one conductive metal thin layer; and

[0081] A conductive connection is formed in the through opening to electrically connect the conductive metal thin layers on the two main surfaces.

[0082] Since the protection element of the present disclosure has a conductive metal thin layer located on the main surface of the layered element and having a fuse pattern, the thickness of such a fuse pattern can be easily adjusted. In particular, a metal foil prepared separately from the layered element is placed on the layered element, and then the fuse pattern is formed, thereby facilitating the control of the thickness of the fuse pattern. Therefore, changes in the resistance value, disconnection time, etc. of the protection element of the present disclosure are suppressed.

[0083] [Example]

[0084] Made Figure 1 and Figure 2 The protection element according to the present disclosure shown in FIG. 1 is symmetrically provided with two bridge portions 6. Specifically, the protection element is manufactured as described below.

[0085] First, a sheet was prepared with an insulating resin used as a layered member sandwiched between two conductive metal thin layers. A thin Ni layer with a thickness of 25 μm was used as the conductive metal thin layer, and polyethylene with a thickness of 400 μm was used as the layered member.

[0086] Next, a through opening having a diameter of 6.0 mm was formed in the sheet. Subsequently, a resist was formed, a portion of one conductive metal thin layer (the portion to be removed by subsequent etching) was then exposed, the other portion was covered, after which the exposed portion of the conductive metal thin layer was removed by etching to form a slit. The width of the slit (i.e., the distance between the first annular metal thin layer and the second annular metal thin layer) was 0.4 mm. In addition, the width of the second annular metal thin layer was 0.8 mm, and the width of the bridge portion was 0.6 mm.

[0087] The resist is then removed, and an electroless copper plating layer is formed on the entire sheet by electroless plating. Then, all portions other than the through openings are masked, and an electrolytic copper plating layer is formed on the electroless copper plating layer of the through openings by electrolytic plating.

[0088] The mask is then removed, and the chemical copper plating layer exposed on the main surface of the sheet is removed by etching. The entire sheet is then plated with nickel. Through this electroplating process, a nickel plating layer is formed on the entire sheet except for the portion where the insulating resin is exposed.

[0089] Finally, the sample was punched into a disk shape having a diameter of 14.6 mm, which was concentric with the through opening, to obtain a protective element according to the present disclosure.

[0090] (Comparison example)

[0091] As a comparative example, a protection element of a comparative example was manufactured by forming a fuse layer by plating on the side surface of the through opening without a slit.

[0092] (evaluate)

[0093] Resistance Value

[0094] For the protection element of the present disclosure, the resistance value between the first annular metal thin layer and the conductive metal thin layer on the main surface facing the first annular metal thin layer was measured, and for the protection element of the comparative example, the resistance value between the conductive metal thin layers at the positions corresponding to the above positions was measured. The measurement was performed on 28 samples of the protection element of the present disclosure and 59 samples of the protection element of the comparative example.

[0095] The measurement results show that the average value of the resistance value of the example is approximately the same as the average value of the resistance value of the comparative example. On the other hand, the percentage of the standard deviation of each average value (standard deviation / average value) is 5.5%, while that of the comparative sample is 12.0%. That is, it is confirmed that the resistance value of the protection element of the present disclosure has very little change.

[0096] Disconnection time

[0097] For the examples and comparative examples, the disconnection time was measured using 5 samples each. The test was conducted with applied currents of 80A and 60A.

[0098] As a result of the measurement, it was found that the ratio of the standard deviation of the example sample to the average value was 7.8% at 80 A and 4.5% at 60 A. On the other hand, the ratio of the standard deviation of the comparative sample to the average value was 17.1% at 80 A and 33.9% at 60 A. That is, it was confirmed that the disconnection time of the protection element of the present disclosure had very little variation.

[0099] [Industrial Applicability]

[0100] The protection element of the present invention can be used as a protection element that blocks the flow of current when an excessive current flows in an electric device such as a secondary battery.

Claims

1. A protection element, include: a laminar member formed of an insulating resin; and a conductive metal thin layer, the conductive metal thin layer being arranged on at least one of the two main surfaces of the layered element, wherein at least one of the conductive metal thin layers has a fuse pattern, The laminar element is a circular ring with a through opening in the center, The conductive metal thin layer disposed on one main surface of the annular layered element includes a first annular metal thin layer located on the outer edge side of the annular layered element, a second annular metal thin layer located on the inner edge side of the annular layered element, and a fuse pattern for electrically connecting the first annular metal thin layer and the second annular metal thin layer, having 2 to 8 fuse patterns arranged equiangularly with respect to the center of the ring, The annular metal thin layer and the fuse pattern are formed integrally, and The protection element further includes an insulating layer on the conductive metal thin layer having the fuse pattern, the insulating layer covering at least the fuse pattern.

2. The protection element according to claim 1, in, The laminar element has at least one through opening; The conductive metal thin layer is disposed on both major surfaces of the layered element; and The conductive metal thin layers provided on both main surfaces of the layer element are electrically connected via conductive connections passing through the through openings.

3. The protection element according to claim 1 or 2, in, The distance between the first annular metal thin layer and the second annular metal thin layer is 0.1 mm to 5.0 mm.

4. The protection element according to claim 1 or 2, in, The width of the first annular metal thin layer is greater than the width of the second annular metal thin layer.

5. The protection element according to claim 1 or 2, in, The conductive metal thin layer includes nickel foil or copper foil.

6. An electrical device comprising the protection element according to any one of claims 1 to 5. 7 . A sealing body comprising the protection element according to claim 1 . 8 . A secondary battery cell comprising the protection element according to claim 1 .