Strain-balanced semiconductor structures

By using germanium substrate and germanium epitaxial layer to adjust the lattice constant in VCSEL, the strain increase problem caused by lattice mismatch and thickness increase in GaAs-AlGaAs system is solved, and a more stable semiconductor structure is achieved and bending is reduced. and warp.

CN111492464BActive Publication Date: 2024-11-08IQE
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201880073421.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2017-12-19
Filing Date
2018-11-21
Publication Date
2024-11-08
Estimated Expiration
2038-11-21

AI Technical Summary

Technical Problem

The existing VCSEL GaAs-AlGaAs system has increased strain due to lattice mismatch and increased thickness in more complex designs and longer wavelength ranges, resulting in reduced bending and stability of semiconductor structures.

Method used

Using germanium as the substrate or epitaxial layer, by growing the GaAs/AlAs layer on the germanium substrate and introducing an intermediate germanium layer if necessary, the difference in lattice constants is adjusted to achieve strain equilibrium and reduce lattice mismatch and bending.

Benefits of technology

It effectively reduces the bending and wafer warpage of VCSEL, improves the stability and mechanical strength of the semiconductor structure, and reduces the performance limitations caused by lattice mismatch.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111492464B_ABST
    Figure CN111492464B_ABST
Patent Text Reader

Abstract

Systems and methods for growing layered structures are described herein. The layered structures include: a first germanium substrate layer having a first lattice constant; a second layer having a second lattice constant and epitaxially grown on the first germanium substrate layer, wherein the second layer has a composite of a first component and a second component and has a first ratio between the first component and the second component; a third layer having a third lattice constant and epitaxially grown on the second layer, wherein the third layer has a composite of a third component and a fourth component and has a second ratio between the third component and the fourth component, wherein the first ratio and the second ratio are selected such that the first lattice constant is between the second lattice constant and the third lattice constant.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims the benefit under 35 U.S.C. §119(e) of U.S. Provisional Patent Application No. 62 / 589,994, filed on November 22, 2017, and U.S. Provisional Patent Application No. 62 / 607,857, filed on December 19, 2017, both of which are hereby incorporated by reference in their entireties. Technical Field

[0003] The present application relates to using a germanium (Ge) substrate or an epitaxial layer to perform strain balancing on a semiconductor structure. Background Art

[0004] A vertical cavity surface emitting laser (VCSEL) is a semiconductor laser diode that emits a laser beam perpendicular to the upper surface of a semiconductor structure. VCSELs for wavelengths from 650nm to 1300nm are usually grown on a gallium arsenide (GaAs) substrate and have a structure composed of GaAs and aluminum gallium arsenide (AlGaAs). x Ga (1-x) As) formed distributed Bragg reflector (DBR). x Ga (1-x) As (for a wide range of x) is generally considered to be lattice-matched to the GaAs substrate, and this GaAs-AlGaAs system is widely used. For the next generation of VCSELs, more complex designs will lead to thicker epitaxial stacks, where the assumed lattice match in the GaAs-AlGaAs system becomes unacceptable due to a higher degree of crystal defects and increased wafer curvature caused by the increased thickness of the stack. This situation becomes even more complicated in designs that introduce GaAs and AlAs. Because moving to longer wavelengths requires increasing layer thickness, the lattice mismatch increases in thick stacks. The increase in thickness may cause an increase in the overall lattice mismatch between the substrate and other layers grown on the substrate, resulting in increased strain in the semiconductor structure. Strain and lattice mismatch contribute to bending in semiconductor wafers, thereby reducing the stability of VCSELs. Summary of the invention

[0005] This article describes a layered structure that strain balances a semiconductor structure by using germanium (Ge) as a substrate or epitaxial layer. This layered structure includes a first germanium substrate layer having a first lattice constant, and a second layer having a second lattice constant and epitaxially grown on the first germanium substrate layer. The second layer has a composite of a first component and a second component, and has a first ratio between the first component and the second component. A third layer has a third lattice constant and is epitaxially grown on the second layer. The third layer has a composite of a third component and a fourth component, and has a second ratio between the third component and the fourth component. The first ratio and the second ratio are selected so that the first lattice constant is between the second lattice constant and the third lattice constant.

[0006] In some embodiments, the first component of the second layer is the same as the third component of the third layer, and the second component of the second layer is the same as the fourth component of the third layer. In some embodiments, the first component is different from the third component.

[0007] In some embodiments, the first component, the second component, the third component or the fourth component in the third layered structure is a III-V binary alloy selected from the group consisting of AlP, GaP, InP, AlAs, GaAs, InAs, AlSb, GaSb and InSb.

[0008] In some embodiments, the second layer in the layered structure has a first thickness, the third layer has a third thickness, and the first thickness and the third thickness are selected so that a total strain in the layered structure, at least partially defined by the first thickness, the second thickness, and the lattice constant difference between adjacent layers, is close to zero. In some embodiments, a repeating body of the second layer and the third layer is grown on the third layer.

[0009] In some embodiments, the layered structure is implemented as a vertical cavity surface emitting laser (VCSEL) epitaxial wafer. In some embodiments, the curvature of the VCSEL epitaxial wafer is measured to be less than 10 μm. In some embodiments, the first germanium substrate layer in the layered structure is a germanium single crystal wafer, and the lattice constant of the upper surface of the germanium single crystal wafer is equal to that of a bulk germanium substrate. In some embodiments, the first germanium substrate layer of the layered structure comprises a germanium wafer on an oxide layer on a silicon layer. The lattice constant of the upper surface of the germanium wafer is equal to that of a bulk germanium substrate.

[0010] In some embodiments, the first germanium substrate layer comprises a germanium wafer on a silicon layer, and the lattice constant of the upper surface of the germanium wafer is equal to that of a bulk germanium substrate. In some embodiments, the first germanium substrate layer comprises one or more porous germanium layers within a bulk germanium wafer, and the lattice constant of the upper surface of the bulk germanium wafer adjacent to the second layer is equal to that of the bulk germanium substrate (without the porous portion).

[0011] In some embodiments, the first germanium substrate layer includes a patterned germanium wafer having a first germanium portion and a second germanium portion that does not spatially overlap with the first germanium portion, and the lattice constant of the upper surface of the first region or the second region in the patterned germanium wafer is equal to that of a bulk germanium substrate.

[0012] In some embodiments, the first germanium substrate layer of the layered structure comprises germanium tin (Ge x Sn 1-x , 0≤x≤1) wafer. In some embodiments, an epitaxial germanium layer is grown on a first germanium substrate layer, wherein the epitaxial germanium layer is used to host an embedded device, and wherein the embedded device is selected from the group consisting of a germanium APD, a GaAs PIN, and a germanium transistor. In some embodiments, the layered structure further comprises a second germanium layer having the first lattice constant located directly or indirectly on the third layer; and a fourth layer having a first component and a second component epitaxially grown on the second germanium layer, wherein a third ratio between the first component and the second component in the fourth layer is selected to give the fourth layer a third lattice constant, and the third lattice constant of the fourth layer is used to offset the total strain of the layers under the second germanium layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Other features of the present disclosure, its nature and various advantages will become more apparent after considering the following detailed description and the accompanying drawings, in which:

[0014] Figure 1 According to an exemplary embodiment, a layered structure for growing a strain-balanced vertical cavity surface emitting laser on a germanium substrate is depicted.

[0015] Figure 2 According to an exemplary embodiment, a layered structure including an intermediate germanium layer for growing a strain-balanced vertical cavity surface emitting laser on a germanium substrate is depicted.

[0016] Figure 3 An example graph 300 showing data plots comparing lattice mismatch, wafer bow, and wafer warpage, respectively, of different types of substrates is provided according to an embodiment.

[0017] Figure 4According to an illustrative embodiment, a graph illustrating wafer bow is depicted.

[0018] Figure 5 According to an exemplary embodiment, lattice dislocations of various layered structures are depicted.

[0019] Figure 6 According to an exemplary embodiment, a Figure 1-2 Various exemplary substrate structures of the germanium substrate 102 .

[0020] Figure 7 is a flow chart depicting a process 700 for growing a layered structure 100 according to an illustrative embodiment. DETAILED DESCRIPTION

[0021] The structure and method described herein provide a strain-balanced semiconductor structure. For example, the semiconductor structure described herein can be applied to VCSEL. The structure and method disclosed herein include growing a GaAsAl layer on a germanium substrate.

[0022] Figure 1 An exemplary diagram of a layered structure 100 is shown depicted in accordance with an exemplary embodiment. Figure 1 The layered structure 100 depicted in the drawings can be fabricated in a single epitaxial process, which can be molecular beam epitaxy (MBE), metal organic vapor phase epitaxy (MOCVD), or any other well-known epitaxial deposition technique. The process requires that the deposition tool for depositing the material can be a single chamber; or use a well-known cluster tool format, where specific parts of the process are completed in different interconnected chambers, or multiple deposition tools can be used. For example, the additional layer 106 can include, but is not limited to, a Group IV layer, a Group III-V semiconductor layer, a rare earth pnictide layer, a rare earth oxide layer, etc.

[0023] Figure 1The layered structure 100 in includes a germanium substrate 102, a GaAs / AlAs layer 104 grown on the substrate 102, and an additional layer 106 grown on the GaAs / AlAs layer 104. In some embodiments, the 104 layer may include multiple sublayers of GaAs and AlAs. In some embodiments, if a conventional GaAs substrate is used to grow the 104 layer, an increase in the aluminum concentration in the 104 layer (e.g., in a VCSEL) may result in a lattice mismatch. For example, in a VCSEL, the thickness of the 104 layer may be above 3 microns (3 μm), and the lattice mismatch between the AlAs sublayer in the 104 layer and the conventional GaAs substrate may have a significant effect when the mismatch over multiple sublayers of the overall thickness of the 104 layer is accumulated. In addition, since any layer grown on a GaAs substrate may have a certain degree of lattice mismatch, the lattice mismatch may be significant when the lattice mismatch increases due to the composition of the layers grown on the GaAs, or when multiple GaAs-layer pairs are repeatedly used in a semiconductor structure. Lattice mismatch may cause bending of structure 200, for example, the center point of the middle surface of the unclamped wafer corresponding to structure 100 may be offset from the middle surface to the reference surface. The radius of curvature of the resulting bending may increase with the increase of the wafer size, for example, the larger the wafer, the more significant the radius of curvature corresponding to the bending. For example, the radius of curvature corresponding to the bending of a 200mm wafer may be larger than the radius of curvature corresponding to the bending of a 100mm wafer. Such bending may limit the scalability of GaAs-based laser structures. Thus, in order to avoid or reduce the bending caused by the lattice mismatch caused by the use of a GaAs substrate, a germanium substrate 102 is used in the layered structure 100 to grow a GaAs / AlAs layer 104 with a high Al concentration. The lattice constant of the germanium layer is close to that of the GaAs / AlAs layer, for example, the lattice constant of the germanium wafer is generally between the GaAs layer and the AlAs layer. Thus, the germanium layer can be used to reduce the lattice mismatch caused by growing the GaAs / AlAs layer in the layered structure 100. Since the Young's modulus of germanium is 90×10 9 Pa (greater than GaAs, for example 85×10 9 Pa), germanium provides better mechanical strength than GaAs, making it a stronger substrate than conventional GaAs for 200 mm wafers when bending may affect significant areas of the wafer (102). In addition, germanium has a much lower etch pitch density relative to GaAs, which produces wafers with reduced impurities, although the wafers may have inherent defects.

[0024] In some embodiments, the layered structure 100 can include one or more intermediate layers between the germanium substrate 102 and the GaAs / AlAs layer 104. In some examples, the intermediate layers can be common III-V layers.

[0025] Figure 2 An example diagram of a layered structure 200 depicted in accordance with an exemplary embodiment is shown. The layered structure 200 may be built on the layered structure 100. For example, a second germanium layer 208 may be epitaxially grown on the additional layer 106, whereby a further layer stack of GaAs / AlAs may be grown on the second germanium layer 208.

[0026] In some embodiments, a second germanium layer 208 (or multiple germanium layers) is grown in the layered structure 200. In some embodiments, layer 208 may be Ge 1-x-y Si x Sn y (0≤x, y≤1) is equivalent to a germanium layer when x=y=0. The intermediate germanium layer improves the lattice mismatch caused by the high concentration of aluminum in layer 104. This reduces the strain between the substrate layer 102 and layer 104. This reduction in strain between layers 102 and 104 increases the stability of the layered structure 200. It is worth noting that Figure 2 The two germanium layers 102 and 208 are shown for illustration purposes only. Multiple (more than 2) germanium layers can be used in the layered structure, so that multiple repeats of the germanium layer and the GaAs / AlAs layer grown on the germanium layer can be used in a single layered structure to increase the stability of the layered structure 200.

[0027] In some embodiments, the thickness of the germanium layers 102 and 208 may be different. The thickness of the second germanium layer 208 may depend on the lattice mismatch caused by the layers below the second germanium layer 208 or the layers above the second germanium layer 208. In some embodiments, more than one intermediate germanium layer may be grown in the lattice structure 200 to induce stability of the lattice structure 200.

[0028] Figure 3 An example graph 300 is provided according to an embodiment, showing data graphs 302, 308, and 314 comparing lattice mismatch, wafer bow, and wafer warpage of different types of substrates, respectively. Data graph 302 compares the performance of GaAs wafers and Ge wafers using the product of thickness and lattice mismatch as a performance metric. Bar 304 depicts the product of thickness and lattice mismatch for a layered structure having a GaAs wafer and an epitaxial film on the GaAs wafer. Bar 306 depicts the product of thickness and lattice mismatch for a layered structure having a Ge wafer and an epitaxial film on the Ge wafer (with Figure 1 The product of the thickness of the crystal (similar to 100 in FIG. 1 ) and the lattice mismatch. Figure 3 As depicted, by replacing the GaAs wafer with a Ge wafer, the product of thickness and lattice mismatch drops from approximately 0.4 to −0.05 as shown by bar 306 .

[0029] Data graph 308 compares the performance of GaAs wafers and Ge wafers using wafer bow measurements as a performance indicator. Bar 310 depicts the bow measurements produced in a layered structure having a GaAs wafer and an epitaxial film on the GaAs wafer. Bar 312 depicts the bow measurements produced in a layered structure having a Ge wafer and an epitaxial film on the Ge wafer (with Figure 1 The curvature measurement value generated by Figure 3 As depicted, replacing the GaAs wafer with a Ge wafer as the substrate reduces the resulting bow from approximately 90 μm to −5 μm as shown by bar 312 .

[0030] Data graph 314 compares the performance of GaAs wafers and Ge wafers using wafer bow measurements as a performance indicator. Bar 316 depicts the warpage measurements produced in a layered structure having a GaAs wafer and an epitaxial film on the GaAs wafer. Bar 318 depicts the warpage measurements produced in a layered structure having a Ge wafer and an epitaxial film on the Ge wafer (with Figure 1 The warpage measurement value generated by Figure 3 As depicted, by replacing the GaAs wafer with a Ge wafer as the substrate, the resulting warp is reduced from 180 μm to 40 μm as shown by column 318.

[0031] The significant reduction in the measured values ​​of the product of thickness and lattice mismatch, wafer bow, and wafer warpage is due to the fact that the lattice constant of the germanium substrate is between that of GaAs and AlAs, so the stress applied by the GaAs layer to the Ge layer is in the opposite direction to the stress applied by the AlAs layer to the Ge layer, and the opposite stresses cancel each other out to a certain extent. In the case where the substrate is GaAs, since the GaAs substrate has the smallest or equal lattice constant compared to other materials on the GaAs substrate, the GaAs / AlAs layer applies stress to the epitaxial film in the same direction.

[0032] Figure 4 According to an exemplary embodiment, a three-dimensional map of a layered structure using Ge or GaAs as a substrate is shown. The three-dimensional map 402 depicts a layered structure having a Ge wafer and an epitaxial film on the Ge wafer (with Figure 1 100 in FIG. 101 . The three-dimensional map 404 depicts a layered structure having a GaAs wafer and an epitaxial film on the GaAs wafer. It is clear from the three-dimensional map 404 that the high degree of curvature caused by the GaAs wafer and the epitaxial film exceeds the maximum curvature allowed to obtain a complete wafer map. Figure 4A graph 406 is included showing measured wafer bow for a layered structure comprising 10% epitaxial AlGaAs grown on a GaAs substrate and 90% epitaxial AlGaAs grown on a Ge substrate. As clearly shown in the graph, the bow produced by the epitaxial film on the GaAs wafer is much higher than the bow produced by the epitaxial film on the Ge substrate. The reduced bow of the Ge wafer increases the performance of the layered structure with the Ge wafer.

[0033] Figure 5 Lattice misalignment 500 in various layered structures shown in 502, 504 and 508 is shown according to an exemplary embodiment. Lattice misalignment is represented by a slip line on the wafer. The slip line is inside the wafer and is the main cause of device reliability problems. In some embodiments, a wafer with a large curvature value has an inherent mechanical force that causes and drives misalignment inside the layered structure, thereby increasing the slip line on the layered structure substrate. Therefore, reducing the wafer curvature can reduce or eliminate the slip line on the layered structure substrate. Figure 502 shows a snapshot of a Ge wafer. The Ge wafer snapshot contains a horizontal line 516 across the wafer, which is a measurement artifact. Figure 504 shows a snapshot of a Ge wafer and an epitaxial film on the Ge wafer. Figure 504 depicts a slip line region 506 generated in the Ge wafer due to strain caused by the epitaxial film on the Ge wafer. Figure 508 shows a snapshot of a GaAs wafer and an epitaxial film on the GaAs wafer. Graph 508 depicts the slip line regions 510, 512, and 514 that are created in a GaAs wafer due to the epitaxial films grown on the GaAs wafer. As these snapshots clearly show, the GaAs wafer has more slip lines than the Ge wafer. This is because the stress created by the epitaxial films on the Ge wafer is much less than the stress created by the epitaxial films on the GaAs wafer.

[0034] Figure 6 According to an exemplary embodiment, Figure 1-2 Various exemplary substrate structures of the germanium substrate 102 are described in Figure 1-2 102) in may include a single crystal, or a layered structure. Figure 6 The various substrate structures depicted in the drawings may have different compositions containing various germanium portions therein. For example, the various substrates may be a germanium wafer (see, e.g., 602), a layered structure of germanium grown on oxide and silicon (see, e.g., 608), a layered structure of a germanium layer containing a porous germanium portion (see, e.g., 618), or a layered structure of germanium grown on a silicon layer (see, e.g., 626), etc. Figure 6The exemplary substrate structures 602, 608, 618, and 626 depicted in the drawings can serve as starting templates for growing additional layers, and the lattice constant of the upper surface of the exemplary substrate structures 602, 608, 618, and 626 is equal to that of a bulk germanium substrate. The various exemplary substrate structures can differ in various properties, such as mechanical strength, thermal conductivity, and etch pitch density, which in turn support different functionalities based on the combination of these substrates.

[0035] Layered structure 602 depicts a germanium wafer 606 upon which other layers 604 may be grown. The lattice constant of the upper surface of germanium wafer 606 is substantially equal to that of the bulk germanium substrate.

[0036] The layered structure 608 depicts a substrate structure 634 including a germanium layer 612, an oxide layer 614, and a silicon layer 616. The germanium layer 612 is grown on the oxide layer 614, and the oxide layer 614 is grown on the silicon layer 616. In another implementation, the growth of the germanium layer 612 on the oxide 614 layer can be the result of a bonding process. The other layers 610 of the layered structure 608 can be grown on the germanium layer 610. The upper surface of the germanium wafer 612 has a substantially equal lattice constant as the bulk germanium substrate.

[0037] The layered structure 618 depicts a substrate structure 636 including a porous germanium portion / sublayer 624. The substrate structure 636 may be a bulk germanium wafer having a porous sublayer 624 between germanium sublayers 622 and 640. The other layers 620 may be grown on the germanium layer 622. In another implementation, multiple repeats of the porous germanium sublayer 624 and the germanium sublayer 640 may be used to achieve the desired lattice constant level in the layered structure 618. The germanium sublayer 622 may be grown on multiple repeats of the porous germanium sublayer 624 and the germanium sublayer 640. The upper surface of the bulk germanium wafer 636, i.e., the upper surface of the germanium sublayer 622, has a lattice constant that is substantially consistent with the bulk germanium substrate (not including the porous portion).

[0038] Layered structure 626 depicts a substrate structure 638 including a germanium layer 630 and a silicon layer 632, wherein germanium layer 630 is grown on silicon layer 632. The upper surface of germanium wafer 630 has a lattice constant that is substantially consistent with a bulk germanium substrate.

[0039] In some embodiments, the lattice constant of substrates 634, 636, and 638 is substantially equal to the lattice constant of germanium 606 in layered structure 602. In some embodiments, germanium 606 can be replaced with any one of 634, 636, and 638.

[0040] In some embodiments, the germanium substrate 606 may include a patterned germanium wafer. For example, the germanium wafer has spatially non-overlapping germanium portions, such as stripes, grids, etc. The lattice constant of the upper surface of the patterned germanium wafer is equal to that of the bulk germanium substrate.

[0041] In some embodiments, the germanium substrate 606 may include germanium tin (Ge x Sn 1-x , 0≤x≤1) chip.

[0042] In some embodiments, an additional epitaxial germanium layer may be grown on the germanium substrate. The epitaxial germanium layer may be used to carry an embedded device, and wherein the embedded device is selected from the group consisting of a germanium APD, a GaAs PIN, and a germanium transistor.

[0043] Figure 7 1 is a flow chart of a process 700 for growing a layered structure 100 according to an exemplary embodiment. The process begins at 702 when a first germanium substrate (eg, Figure 1 A germanium substrate 102 in is obtained.

[0044] In 704, a second layer 104 (e.g., a GaAs / AlAs layer 104) having a second lattice constant is formed on the germanium substrate layer 102. The second layer has a composite of a first component (e.g., GaAs) and a second component (e.g., AlAs) and has a first ratio between the first component and the second component. For example, "construction" refers to (epitaxial) growth or arrangement, or otherwise manufacturing an additional layer present on a layer. In some embodiments, the first component or the second component can be a III-V binary alloy, such as, but not limited to, AlP, GaP, InP, AlAs, GaAs, InAs, AlSb, GaSb, and InSb.

[0045] At 706, a third layer (eg, Figure 1Any additional layer 106 in the first germanium substrate is constructed (e.g., epitaxially grown or disposed) on the second layer. The third layer has a composite of a third component and a fourth component and has a second ratio between the third component and the fourth component. In some embodiments, the third component or the fourth component can be a III-V binary alloy, such as but not limited to AlP, GaP, InP, AlAs, GaAs, InAs, AlSb, GaSb and InSb. The first ratio and the second ratio are selected so that the first lattice constant is between the second lattice constant and the third lattice constant. In this way, the strain caused by the lattice mismatch between the first germanium substrate and the second layer can be offset by the lattice mismatch (in opposite directions) between the second layer and the third layer. Specifically, the thickness of the second layer and the thickness of the third layer are selected so that the total strain in the layered structure, which is at least partially defined by the thickness of each layer and the lattice constant difference between adjacent layers, is close to zero.

[0046] The growth and / or deposition described herein may be achieved using one or more of the following methods: compound vapor deposition (CVD), metal-organic chemical vapor deposition (MOCVD), organometallic vapor phase epitaxy (OMVPE), atomic layer deposition (ALD), molecular beam epitaxy (MBE), halide vapor phase epitaxy (HVPE), pulsed laser deposition (PLD), and / or physical vapor deposition (PVD).

[0047] As described herein, a layer refers to a generally uniform thickness of material covering a surface. A layer can be continuous or discontinuous (i.e., have gaps between regions of material). For example, a layer can completely or partially cover a surface, or be segmented into discrete regions that collectively define the layer (i.e., regions formed using selective area epitaxy).

[0048] Monolithic integration means formation on the surface of a substrate, typically by deposition of layers disposed on the surface.

[0049] "Disposed on" means "existing on" an underlying material or layer. The layer may include intermediate layers, such as transition layers, as necessary to ensure a suitable surface. For example, if a material is described as being "disposed on a substrate," this may mean: (1) the material is in intimate contact with the substrate; or (2) the material is in contact with one or more transition layers located on the substrate.

[0050] Single crystal means a crystalline structure consisting essentially of only one unit cell. However, a single crystal layer may show some crystal defects, such as stacking faults, dislocations or other commonly occurring crystal defects.

[0051] Monodomain means a crystalline structure that contains essentially only one unit cell structure and the unit cell is essentially in one direction. In other words, a monodomain crystal does not show twin or anti-phase domains.

[0052] Single phase means a crystal structure that is both single crystalline and single domain.

[0053] Substrate means the material on which the deposited layer is formed. Exemplary substrates include, but are not limited to, bulk germanium wafers, bulk silicon wafers, where the wafer contains a uniform thickness of single crystal silicon or germanium; composite wafers, such as silicon-on-insulator wafers, which contain a silicon layer disposed on a silicon dioxide layer disposed on a bulk silicon handle wafer; or porous germanium, germanium on oxide and silicon, germanium on silicon, patterned germanium, germanium tin on germanium, etc., such as Figure 6 or any other material as a base layer on which a device is formed or therein. Other suitable materials that can be applied as a substrate layer or bulk substrate include, but are not limited to: aluminum oxide, gallium arsenide, indium phosphide, silica, silicon dioxide, borosilicate glass, pyrex glass, and sapphire. The substrate can have a single block wafer or multiple sublayers. Specifically, the substrate (e.g., silicon, germanium, etc.) can include multiple discontinuous porous portions. The multiple discontinuous porous portions can have different densities and can be distributed horizontally or stacked vertically.

[0054] A beveled substrate means that the surface crystal structure of the substrate is at a certain angle to the associated orientation of the crystal structure of the substrate. For example, a 6° beveled <100> Silicon wafers contain <100> The crystal orientation is towards another main crystal orientation such as <110> Cut at an angle of 6° <100> Silicon wafers. Typically the bevel angle can be up to about 20°, but this is not necessary. Unless otherwise specified, the phrase "beveled substrate" includes beveled wafers having any principal crystal orientation, i.e., <011> Direction bevel <111> Chip, <110> Direction bevel <100> Chip, and <001> Direction bevel <011> Chip.

[0055] Semiconductor refers to any solid substance with an electrical conductivity between that of an insulator and most metals. An exemplary semiconductor layer is composed of silicon. The semiconductor layer may comprise a single block wafer, or multiple sublayers. Specifically, the silicon semiconductor layer may comprise multiple discontinuous porous portions. The multiple discontinuous porous portions may have different densities and may be distributed horizontally or stacked vertically.

[0056] Semiconductor-on-Insulator means a composition comprising a single crystal semiconductor layer, a single phase dielectric layer and a substrate, wherein the dielectric layer is interposed between the semiconductor layer and the substrate. This structure is reminiscent of existing silicon-on-insulator ("SOI") compositions, which typically comprise a single crystal silicon substrate, a non-single phase dielectric layer (e.g., amorphous silicon dioxide, etc.) and a single crystal silicon semiconductor layer. Several important differences between the prior art SOI wafer and the semiconductor-on-insulator composition of the present invention are:

[0057] Semiconductor-on-insulator compositions include dielectric layers that are single-phase in morphology, whereas SOI wafers are not. In fact, the insulator layer of a typical SOI wafer is not even single crystalline.

[0058] The semiconductor-on-insulator composition comprises a silicon, germanium, or silicon-germanium "active" layer, while the prior art SOI wafers use a silicon active layer. In other words, exemplary semiconductor-on-insulator compositions include, but are not limited to: silicon-on-insulator, germanium-on-insulator, and silicon-germanium-on-insulator.

[0059] The first layer described and / or depicted herein as "constructed on the second layer", "on the second layer" or "above the second layer" indicates that the first layer and the second layer may be directly adjacent, or one or more intermediate layers may exist between the first layer and the second layer. The first layer described and / or depicted herein as "directly on the second layer or substrate" or "directly above the second layer or substrate" indicates that the first layer and the second layer or substrate are directly adjacent, without intermediate layers, unless an intermediate alloy layer may be formed due to mixing of the first layer with the second layer or substrate. In addition, the first layer described and / or depicted herein as "on the second layer or substrate", "above the second layer or substrate", "directly on the second layer or substrate" or "directly above the second layer or substrate" indicates that the first layer may cover the entire second layer or substrate, or a portion of the second layer or substrate.

[0060] During layer growth, the substrate is placed on a substrate holder so that the top or upper surface is the substrate surface or layer farthest from the substrate holder, and the bottom or lower surface is the substrate surface or layer closest to the substrate holder. Any structure depicted and described herein may be part of a larger structure having additional layers above and / or below the depicted structure. For clarity, the figures herein may omit these additional layers, although these additional layers may be part of the disclosed structure. In addition, the described structures may be repeated in units, even if the repetition is not depicted in the figures.

[0061] It is clearly presented in the above description that various different technologies can be used to implement the concepts described herein without departing from the scope of the present disclosure. The described embodiments should be regarded as exemplary and non-restrictive in all respects. It should be understood that the techniques and structures described herein are not limited to the specific examples described herein, but can be implemented in other examples without departing from the scope of the present disclosure. Similarly, although the operations are depicted in a specific order in the accompanying drawings, this should not be understood as these operations need to be performed in the specific order shown or in sequence, or all the operations shown need to be implemented to achieve the desired results.

Claims

1. A layered structure comprising a vertical cavity surface emitting laser (VCSEL) epitaxial wafer, the layered structure comprising: a first germanium substrate layer having a first lattice constant; and a second layer having a second lattice constant and epitaxially grown on the first germanium substrate layer, wherein the second layer has a composite of a first component and a second component and has a first ratio between the first component and the second component; a third layer having a third lattice constant and epitaxially grown on the second layer, wherein the third layer has a composite of a third component and a fourth component and has a second ratio between the third component and the fourth component, The first ratio and the second ratio are selected such that the first lattice constant is between the second lattice constant and the third lattice constant.

2. The layered structure of claim 1, wherein the first component is the same as the third component, and the second component is the same as the fourth component.

3. The layered structure of claim 1, wherein the first component is different from the third component.

4. The layered structure of claim 1, wherein the first, second, third or fourth component is a Group III-V binary alloy selected from the group consisting of AlP, GaP, InP, AlAs, GaAs, InAs, AlSb, GaSb and InSb.

5. The layered structure of claim 1 , wherein the second layer has a first thickness, the third layer has a third thickness, and wherein the first thickness and the third thickness are selected so that a total strain in the layered structure defined at least in part by the first thickness, the second thickness, and the lattice constant differences between adjacent layers is close to zero.

6. The layered structure of claim 1, further comprising: A repeating body of the second layer and the third layer is grown on the third layer.

7. The layered structure of claim 1, wherein the bow of the VCSEL epitaxial wafer measures less than 10 μm.

8. The layered structure of claim 1, wherein the first germanium substrate layer is a germanium single crystal wafer, and the lattice constant of the upper surface of the germanium single crystal wafer is equal to that of a bulk germanium substrate.

9. The layered structure of claim 1, wherein the first germanium substrate layer comprises a germanium wafer on an oxide layer on a silicon layer, and The lattice constant of the upper surface of the germanium wafer is equal to that of the bulk germanium substrate.

10. The layered structure of claim 1, wherein the first germanium substrate layer comprises a germanium wafer on a silicon layer, and The lattice constant of the upper surface of the germanium wafer is equal to that of the bulk germanium substrate.

11. The layered structure of claim 1, wherein the first germanium substrate layer comprises one or more porous germanium sublayers between two germanium sublayers, and The lattice constant of the upper surface of the first germanium substrate layer adjacent to the second layer is equal to the lattice constant of the bulk germanium substrate.

12. The layered structure of claim 1, wherein the first germanium substrate layer comprises a patterned germanium wafer having a first germanium portion and a second germanium portion that spatially does not overlap the first germanium portion, and The lattice constant of the upper surface of the first germanium portion or the second germanium portion in the patterned germanium wafer is equal to that of a bulk germanium substrate.

13. The layered structure of claim 1, wherein the first germanium substrate layer comprises germanium tin (Ge x Sn 1-x , 0≤x≤1) layered structure of the chip.

14. The layered structure of claim 1, further comprising: An epitaxial germanium layer is grown on the first germanium substrate layer, wherein the epitaxial germanium layer is used to carry an embedded device, and wherein the embedded device is selected from the group consisting of a germanium APD, a GaAs PIN, and a germanium transistor.

15. The layered structure of claim 1, further comprising: a second germanium layer having the first lattice constant located directly or indirectly on the third layer; and a fourth layer having a first composition and a second composition epitaxially grown on the second germanium layer, The third ratio between the first component and the second component in the fourth layer is selected to give the fourth layer a third lattice constant, and the third lattice constant of the fourth layer is used to offset the total strain of the layers under the second germanium layer.

16. A method of growing a layered structure, the layered structure comprising a vertical cavity surface emitting laser (VCSEL) epitaxial wafer, the method comprising: obtaining a first germanium substrate layer having a first lattice constant; and epitaxially constructing a second layer having a second lattice constant on the first germanium substrate layer, wherein the second layer has a composite of a first component and a second component and has a first ratio between the first component and the second component; epitaxially constructing a third layer having a third lattice constant on the second layer, wherein the third layer has a composite of a third component and a fourth component and has a second ratio between the third component and the fourth component, The first ratio and the second ratio are selected such that the first lattice constant is between the second lattice constant and the third lattice constant.

17. The method of claim 16, further comprising: constructing a second germanium layer having a first lattice constant directly or indirectly on the third layer; and forming a fourth layer epitaxially grown on the second germanium layer and having the first component and the second component, The third ratio between the first component and the second component in the fourth layer is selected to give the fourth layer a third lattice constant, and the third lattice constant of the fourth layer is used to offset the total strain of the layers under the second germanium layer.

18. The method of claim 16, wherein the second layer has a first thickness, the third layer has a third thickness, and wherein the first thickness and the third thickness are selected so that a total strain in the layered structure defined at least in part by the first thickness, the second thickness, and the lattice constant difference between adjacent layers is close to zero.

19. The method of claim 16, wherein the first germanium substrate layer comprises a patterned germanium wafer having a first germanium portion and a second germanium portion that spatially does not overlap the first germanium portion, and The lattice constant of the upper surface of the first germanium portion or the second germanium portion in the patterned germanium wafer is equal to that of a bulk germanium substrate.

Citation Information

Patent Citations

  • Semi-conductor construction and forming method thereof

    CN101383356A

  • Semiconductor structure for providing strained crystalline layer on insulator and method for fabricating same

    US20040150006A1

  • Layered semiconductor substrate and method for manufacturing it

    US20140048848A1

  • Direct-gap germanium-tin multiple-quantum-well electro-optical devices on silicon or germanium substrates

    US5548128A