Vacuum dryer
By using electricity and electrostatic attraction in a vacuum dryer to adjust the distribution of photoresist, the problem of uneven thickness of the photoresist layer is solved, uniform drying is achieved and support pin position adjustment is simplified, improving the efficiency and stability of the equipment. .
Patent Information
- Application Number
- CN202010226950.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-03-27
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-03-27
AI Technical Summary
The existing vacuum dryer can easily cause the thickness of the photoresist layer to be uneven during the drying process, causing problems with display spots, and the position adjustment of the support pin is complicated, which may cause defects during the attachment or detachment process.
A vacuum dryer was designed that uses voltage and thermal conductivity to adjust the voltage level of the support pins by arranging support pins in the chamber and supplying power to them, combined with electrostatic attraction, so that the solvent of the photoresist is on the substrate Evenly distributed, thus reducing thickness differences. The support pins can be of different shapes and adjusted in position via lifters and support plates to independently control the power supply to each support pin.
It achieves uniform drying of the photoresist layer, reduces the occurrence of display spots, simplifies the position adjustment of the support pin, reduces the risk of defects during attachment and removal, and improves drying efficiency and accuracy.
Smart Images

Figure CN111752107B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2019-0036164, filed on Mar. 28, 2019, the disclosure of which is hereby incorporated by reference in its entirety. Technical Field
[0003] Various embodiments of the present disclosure relate to a vacuum dryer. Background Art
[0004] The display device includes a wire formed on a substrate, a transistor coupled to the wire, and a light emitting element configured to emit light in response to a current supplied from the transistor.
[0005] Various patterns (and / or insulating layers) for forming lines, transistors, and light-emitting elements can be formed on a substrate by photolithography. For example, a pattern can be formed on a substrate by a process including the following steps: applying a photoresist to a substrate, drying the substrate to which the photoresist has been applied by a dryer, and processing the substrate by pattern exposure processing, development processing, heat treatment, etc.
[0006] The photoresist layer formed immediately after the operation of applying the photoresist is performed may have fluidity. Therefore, during the transfer process for the subsequent process, the thickness of the photoresist layer may change. Therefore, in order to prevent the thickness of the photoresist layer from changing, a drying process may be performed on the substrate having the photoresist layer thereon.
[0007] The dryer may include a chamber and support pins disposed on a bottom of the chamber. The substrate may be supported by the support pins. The dryer may dry the substrate by decompressing an inner space of the chamber.
[0008] The thickness of the photoresist in the region of the substrate corresponding to each support pin (or the position of the support pin) may be different from the thickness of the photoresist in other regions. Due to the difference in thickness, the photoresist may have uneven drying spots, which may appear as display spots on the display image of the display device.
[0009] In order to prevent spots from occurring due to the support pins, the support pins may be disposed in a non-display area of the substrate in which an image is not displayed. However, since display devices have a variety of different sizes, additional effort and time may be required to change the positions of the support pins, and additional defects (e.g., defects due to particles formed during the process of attaching or detaching the support pins) may occur. Summary of the invention
[0010] Various embodiments of the present disclosure relate to a vacuum dryer capable of forming a photoresist layer having a uniform or substantially uniform thickness.
[0011] According to an embodiment of the present disclosure, a vacuum dryer includes a chamber configured to provide an internal space, a support pin near a bottom of the chamber in the internal space, a power source configured to supply power to the support pin, and a pump coupled to the internal space in the chamber.
[0012] In an embodiment, the vacuum dryer may include a substrate to be dried in an inner space, and the supporting pins may directly support the substrate.
[0013] In an embodiment, the vacuum dryer includes a photoresist on a substrate, and the photoresist may include a solvent having polarity.
[0014] In an embodiment, the voltage level of the electric power may be based on the magnitude of the polarity of the solvent, and the voltage level of the electric power may be configured to decrease as the polarity of the solvent increases.
[0015] In an embodiment, a temperature of a contact portion of the substrate that contacts one of the support pins may be higher than a temperature of a non-contact portion of the substrate that is spaced apart from the support pin.
[0016] In an embodiment, each of the supporting pins may have any one of a cylindrical shape, a hemispherical shape, a conical shape, and a needle shape.
[0017] In an embodiment, each of the support pins may include a core and a shell configured to surround the core. The core may include a conductive material, and the shell may include an insulating material.
[0018] In an embodiment, the thermal conductivity of the support pin may be 0.3 W / mK or less.
[0019] In an embodiment, the voltage level of the power may be based on the thermal conductivity, and the voltage level of the power may be configured to increase as the thermal conductivity increases.
[0020] In an embodiment, the power supply may include a power generation circuit configured to generate power and a switch circuit configured to couple an output terminal of the power generation circuit to a support pin in response to a first control signal.
[0021] In an embodiment, the switch circuit may be configured to couple the support pin to ground in response to the second control signal.
[0022] In an embodiment, the switch circuit may be configured to couple the support pin to ground before the internal space is depressurized.
[0023] In an embodiment, the switch circuit may be configured to couple the output terminal of the power supply to the support pin when the internal space is depressurized.
[0024] In an embodiment, when each of the support pins is energized by power from a power source, the thickness of the photoresist in the first region of the substrate may become greater than the thickness of the photoresist in the second region of the substrate. The first region of the substrate may overlap with one of the support pins, and the second region of the substrate may be spaced apart from the support pin.
[0025] In an embodiment, when the inner space is depressurized, the thickness of the photoresist in the first region may be reduced to be the same as the thickness of the photoresist in the second region.
[0026] In an embodiment, the chamber may include a substrate and a cover. The power supply may be configured to supply power having a first voltage level to the support pin when the cover is in close contact with the substrate.
[0027] In an embodiment, the power supply may be configured to adjust a voltage level of the power to a ground voltage level when the cover is spaced apart from the substrate.
[0028] In an embodiment, the vacuum dryer may further include a support plate and a lifter, wherein the support plate is located above the base plate, and the lifter is coupled to the support plate and configured to adjust the height of the support plate in the internal space. The support pins may be distributed on the support plate.
[0029] In an embodiment, the support pins may be electrically coupled to each other by power lines in the support plate.
[0030] In an embodiment, the support pins may be coupled to a power source independently of each other. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] These and other features and benefits of the embodiments of the present disclosure will become more apparent by referring to the following detailed description when considered in conjunction with the accompanying drawings. In the accompanying drawings, the same reference numerals are used throughout the drawings to refer to the same features and components. The drawings are not necessarily drawn to scale.
[0032] Figure 1A and Figure 1B is a cross-sectional view illustrating an example of a vacuum dryer according to various embodiments of the present disclosure.
[0033] Figure 2 The embodiment of the present disclosure includes Figure 1A Diagram of the support pins and support plates in a vacuum dryer.
[0034] Figure 3A and Figure 3B is a diagram showing a comparative example of forming a photoresist by a vacuum dryer.
[0035] Figure 3C It is shown Figure 3B A diagram of the temperature of the first region.
[0036] Figure 3D The embodiment of the present disclosure includes Figure 1A Figure 2 is a diagram of various examples of support pins in a vacuum dryer.
[0037] Figure 4 The embodiment of the present disclosure includes Figure 1A Diagram of the support pins and power supply in a vacuum desiccator.
[0038] FIG. 5A to FIG. 5C It is used for Figure 4 The operation of the support pin and the power supply will be described in detail in FIG. DETAILED DESCRIPTION
[0039] Reference will now be made in detail to various embodiments of the present disclosure, and since the embodiments of the present disclosure may be modified in many different forms, specific examples of various embodiments of the present disclosure are shown in the accompanying drawings and described below. However, the present disclosure is not limited to the following embodiments and may be modified in various forms.
[0040] Some elements that are not directly related to the features of the present disclosure may be omitted in the accompanying drawings to clearly illustrate the present disclosure. In addition, the sizes, proportions, etc. of some elements in the accompanying drawings may be slightly exaggerated. It should be noted that in all the accompanying drawings, the same reference numerals are used to represent the same or similar elements, and repeated descriptions will be omitted.
[0041] Figure 1A and Figure 1B is a cross-sectional view illustrating an example of a vacuum dryer 10 according to various embodiments of the present disclosure. Figure 1A The sealed state (or closed state) of the vacuum dryer 10 is shown, and Figure 1B The vacuum dryer 10 is shown in an unsealed state (or open state). Figure 2 The embodiment of the present disclosure includes Figure 1A FIG. 1 is a diagram of a series of support pins 220 and support plates 210 in a vacuum dryer 10 .
[0042] Reference Figure 1A , Figure 1B and Figure 2 The vacuum dryer 10 is configured to reduce the pressure of an internal space thereof (or to form a vacuum or a substantial vacuum in the internal space) to remove a solvent from a photoresist (or a photoresist solvent) applied on a substrate 20 .
[0043] In one or more embodiments, the vacuum dryer 10 may include a chamber 100, a support pin 220 (or a plurality of support pins), a first valve 410, a second valve 420, and a pump 430. The vacuum dryer 10 may further include a support plate 210 and a lifter 230.
[0044] In one or more embodiments, the chamber 100 may include a substrate 110 and a cover 120. The substrate 110 may have a planar structure (e.g., a flat plate). The cover 120 may have a structure in which its lower surface is concave in the third direction DR3 (or upward). For example, in one or more embodiments, the cover 120 may include an upper planar structure (e.g., an upper plate) and one or more flanges, wherein the one or more flanges extend around the periphery of the upper planar structure and extend downward toward the substrate 110 opposite to the third direction DR3. Although Figure 2 The substrate 110 is shown to have a rectangular planar shape, but this is for illustration purposes only, and the planar shape of the substrate 110 and the shape of the cover 120 corresponding to the shape of the substrate 110 may be changed in various ways.
[0045] The substrate 110 may be fixed, and the cover 120 may move upward and / or downward. When the cover 120 moves downward and thus comes into close contact with the substrate 110, an inner space or a built-in space (or a sealed space) may be formed between the substrate 110 and the cover 120 (ie, in the chamber 100).
[0046] The chamber 100 may further include a sealing member 130. The sealing member 130 may be disposed between the substrate 110 and the cover 120 and disposed along the periphery of the lower surface of the cover 120. For example, the sealing member 130 may be a filler having elasticity, or may seal a space between the substrate 110 and the cover 120 of the chamber 100 when the cover 120 is in close contact with the substrate 110.
[0047] A hole (or exhaust hole) HOLE communicating with an external fluid may be formed in the substrate 110. The hole HOLE may be coupled to the pump 430 through a pipe. By the operation of the pump 430, the built-in space of the chamber 100 may reduce pressure or be in a vacuum state or substantially in a vacuum state.
[0048] The support plate 210 may be disposed on the substrate 110. The support plate 210 may have a planar structure (e.g., a flat plate). In an embodiment, the support plate 210 may include a plurality of plates disposed on a plane (e.g., a plane defined by the first direction DR1 and the second direction DR2). For example, the support plate 210 may include a first plate corresponding to a central portion of the substrate 110 and a second plate corresponding to a peripheral portion of the substrate 110.
[0049] The support plate 210 is mounted to the lifter 230 and can be adjusted in height relative to the base plate 110 by upward / downward operation of the lifter 230. For example, the first plate can be mounted to the lifter 230 so that the height of the first plate can be adjusted by the lifter 230.
[0050] One or more support pins 220 may protrude from the upper surface of the support plate 210 in the third direction DR3 (or in the thickness direction). In one or more embodiments in which the vacuum dryer 10 includes a series of support pins 220, the support pins 220 may be distributed and arranged at positions spaced a predetermined distance apart from each other on the upper surface of the support plate 210. Although in the illustrated embodiment, each of the one or more support pins 220 has a cylindrical shape or a pin shape, the present disclosure is not limited thereto.
[0051] One or more supporting pins 220 may support the substrate 20. For example, the one or more supporting pins 220 may contact the lower surface of the substrate 20 so that each of the one or more supporting pins 220 is opposite to the upper surface of the substrate 20 to which the photoresist (or photoresist solvent) is applied. In one or more embodiments, the one or more supporting pins 220 may directly support the substrate 20.
[0052] Although Figures 1A to 2 It is shown that one or more support pins 220 are disposed on the support plate 210, but the present disclosure is not limited thereto. One or more support pins 220 may be disposed on the base plate 110 as needed.
[0053] Will refer to below Figure 3D and Figure 4 The configuration (ie, shape and structure) of one of the support pins 220 is described in detail.
[0054] The lifter 230 may be disposed below the support plate 210 to support the support plate 210 and to move the support plate 210 upward or downward relative to the substrate 110. The lifter 230 may adjust the height (i.e., the position relative to the third direction DR3) of the substrate 20 between the lifter 230 and a conveying unit (e.g., a conveying arm) that transfers the substrate 20 to the vacuum dryer 10. For example, after the lid 120 is lifted to open the chamber 100, the conveying unit having the substrate 20 loaded thereon may be moved into the chamber 100. Thereafter, by the operation of the lifter 230, one or more supporting pins 220 (and the support plate 210) are moved upward to a predetermined position along the third direction DR3 so that the one or more supporting pins 220 may support the substrate 20. Subsequently, the conveying unit may be moved out of the chamber 100, and the one or more supporting pins 220 and the substrate 20 may be moved downward by the operation of the lifter 230.
[0055] The power supply 300 (or power supply device) may apply power (or voltage) to the one or more support pins 220. For example, the power supply 300 may be electrically coupled to each of the one or more support pins 220 via a power line PL. Figure 1A The power line PL is shown to be coupled to one or more support pins 220 via the lifter 230 and the support plate 210, but this is for illustration purposes only and the present disclosure is not limited thereto. The shape and arrangement of the power line PL may be changed in various ways as long as the power source 300 and the one or more support pins 220 can be electrically coupled to each other. Figure 1A Each of the one or more support pins 220 is shown to be electrically coupled to another support pin 220 via a power line PL, but the present disclosure is not limited thereto. For example, in one or more embodiments where the vacuum dryer 10 includes a series of support pins 220, each support pin 220 can be coupled to the power source 300 independently of the other support pins 220, and the power to be applied to each of the support pins 220 can be independently controlled.
[0056] When the power supply 300 applies power to the one or more support pins 220, each of the one or more support pins 220 may be energized or become a charged body. The one or more charged support pins 220 may cause the photoresist (e.g., a solvent included in the photoresist) applied on the upper surface of the substrate 20 to flow in one or more contact portions (or contact areas) of the substrate 20 that are in contact with the support pins 220. The flow of the photoresist may make the overall thickness of the photoresist uniform. The operation of the power supply 300 will be described below with reference to FIG. 5A to FIG. 5C Described together with the drying process.
[0057] The first valve 410 and the second valve 420 may be provided between the chamber 100 and the pump 430. The first valve 410 may be directly coupled to the hole HOLE, and the second valve 420 may be directly coupled to the pump 430. The first valve 410 and the second valve 420 may control a flow rate between the chamber 100 and the pump 430. When the chamber 100 is sealed, the first valve 410 and the second valve 420 may be opened, and air in the chamber 100 may be removed to the outside by the pump 430.
[0058] As reference Figures 1A to 2 As described, the vacuum dryer 10 may include a power source 300 coupled to the one or more support pins 220. Therefore, by energizing the one or more support pins 220 from the power source 300, a variation (deviation) in the thickness of the photoresist on the substrate 20 caused by contact between the substrate 20 and the one or more support pins 220 may be compensated or mitigated.
[0059] Figure 3A and Figure 3B is a diagram showing a comparative example of forming a photoresist by a vacuum dryer. Figure 3A The substrate 20 is shown as not being completely dry. Figure 3B The substrate 20 is shown having been completely dried. Figure 3C It is shown Figure 3B A diagram of the temperature of the first region.
[0060] Reference Figure 3A and Figure 3B , the substrate 20 may include a base layer 21 , a lower layer 22 and a photoresist layer 23 .
[0061] The base layer 21 may form a base member of a display device, a display panel, etc. The base layer 21 may be rigid or flexible, and there is no particular limitation on its material or properties. For example, the base layer 21 may be formed of glass.
[0062] The lower layer 22 may be formed on the base layer 21 and include at least one layer, pattern, etc. formed before applying a photoresist thereto. In one or more embodiments, the lower layer 22 may be omitted.
[0063] The photoresist layer 23 may be formed on the lower layer 22 and may have fluidity. In an implementation, the photoresist layer 23 may include a photoresist material (or a photosensitive compound, hereinafter referred to as "PAC"), a resin, and a solvent.
[0064] In various embodiments, the solvent may include polar molecules. For example, the solvent may include n-butyl acetate (nBA), methyl methoxypropionate (MMP), propylene glycol monomethyl ether (PGME), propylene glycol monomethyl ether acetate (PGMEA), ethyl ethoxypropionate (EEP), ethyl lactate (EL), propylene glycol monomethyl ester acetate (PGMEP), etc. In embodiments where the solvent of the photoresist layer 23 includes polar molecules, an electrostatic attraction may be applied to the solvent in a space where an electric field is formed.
[0065] As reference Figures 1A to 2 As depicted, the substrate 20 may be supported by one or more support pins 220 .
[0066] During the operation of vacuum drying the substrate 20 , the solvent in the photoresist layer 23 is evaporated, and thus the temperature of the substrate 20 may be lowered.
[0067] Since the one or more support pins 220 are in direct contact with the substrate 20 (or the base layer 21), the heat required to evaporate the solvent (i.e., the solvent in the photoresist layer 23) through the one or more support pins 220 may be transferred to the substrate 20. Therefore, the temperature of the contact portion P1 (or the first area A1) of the substrate 20 that contacts or overlaps with one of the one or more support pins 220 may be higher than the temperature of the non-contact portion P2 (i.e., an area that does not contact or overlap with any of the one or more support pins 220, or an area spaced apart from each of the one or more support pins 220). In other words, the overall temperature of the substrate 20 may not be uniform.
[0068] like Figure 3C As shown in , as the drying time TIME elapses, the difference between the temperature TEMP@P1 of the contact portion P1 and the temperature TEMP@P2 of the non-contact portion P2 (i.e., TEMP@P1-TEMP@P2) may increase (as shown by the curve CURVE1). Even when one or more support pins 220 are made of a material having a relatively low thermal conductivity (e.g., polyetheretherketone (PEEK)), a temperature difference may occur, although the temperature difference is relatively small.
[0069] If the temperature difference occurs, the evaporation rate of the solvent in the contact portion P1 (or the first area A1) may be relatively increased, and the PAC and the resin in the photoresist layer 23 may move to the non-contact portion P2 containing a relatively large amount of solvent. In other words, due to the change in concentration of the photoresist layer 23, the solute (ie, PAC and the resin) may be moved.
[0070] Therefore, as shown in 3B, in the substrate 20 that has been completely dried, the thickness of the photoresist layer 23 (or photoresist) in the contact portion P1 may be less than the thickness of the photoresist layer 23 in the non-contact portion P2. The difference in the thickness of the photoresist layer 23 leads to a difference in the critical dimension (e.g., the width of the pattern) after the exposure process. Therefore, the difference in the thickness of the photoresist layer 23 may cause spots visible to the user.
[0071] Figure 3D It is a diagram showing various embodiments according to the present disclosure including Figure 1A FIG. 2 is a diagram of various examples of support pins 220 in a vacuum dryer. Figure 3D Differences in thickness of photoresist (ie, photoresist formed on the substrate 20 through a drying process) corresponding to different shapes of the support pins 220 are shown.
[0072] Reference Figure 3D The support pin 220 may have various shapes. For example, the support pin 220 may have a cylindrical shape TYPE1, a hemispherical shape TYPE2, a triangular pyramid shape TYPE3, or a needle shape TYPE4.
[0073] In the embodiment of the hemispherical shape TYPE2, the surface area of the contact portion P1 of the substrate 20 that contacts or overlaps with the support pin 220 is relatively large, so that the change in thickness of the contact portion P1 can be the largest among the cylindrical shape TYPE1, the hemispherical shape TYPE2, the triangular pyramid shape TYPE3, and the needle shape TYPE4. In the case of the needle shape TYPE4, the surface area of the contact portion P1 of the substrate 20 that contacts or overlaps with the support pin 220 is relatively small, so that the change in thickness of the contact portion P1 can be the smallest.
[0074] In order to minimize the surface area of the portion of the substrate 20 that contacts the support pin 220, that is, to minimize the heat conduction from the support pin 220 to the substrate 20, the support pin 220 may have a needle shape TYPE4. However, in this case, as Figure 3D As shown in , it is also impossible to prevent the difference in thickness from occurring.
[0075] In the vacuum dryer 10 according to various embodiments of the present disclosure, one or more support pins 220 may be powered by supplying power from the power supply 300 to the one or more support pins 220. Therefore, the difference in the thickness of the photoresist may be more significantly reduced or eliminated. In addition, since the working principle of the vacuum dryer 10 is different from the working principle of the method for minimizing heat conduction, the one or more support pins 220 provided in the vacuum dryer 10 according to various embodiments of the present disclosure may have Figure 3D In other words, although the support pin 220 has various shapes (eg, cylindrical shape TYPE1, hemispherical shape TYPE2, triangular pyramid shape TYPE3, or needle shape TYPE4), due to the characteristics of the vacuum dryer 10, the difference in the thickness of the photoresist can be minimized or eliminated.
[0076] Figure 4 The embodiment of the present disclosure includes Figure 1A FIG. 1 is a diagram of a support pin 220 and a power source 300 in a vacuum dryer 10 .
[0077] Reference Figure 4 , the support pin 220 may include a core 221 (or a central portion, or an electrode) and a shell 222 (or a peripheral portion, or an outer portion).
[0078] Although the core 221 may have a rectangular cross-sectional shape (eg, when the support pin 220 has a reference Figure 3DAlthough the cylindrical shape TYPE1 or the needle shape TYPE4 is described, this is for illustration purposes only, and the shape of the core 221 can be changed in various ways. For example, if the support pin 220 has a hemispherical shape TYPE2, the core 221 can have a hemispherical shape.
[0079] The core 221 may include a conductive material, such as a metal. When power is applied from the power supply 300 to the support pin 220, the core 221 may become a charged body. For example, when a positive voltage or a negative voltage is applied to the support pin 220, the core 221 may be energized to carry a positive (+) charge or a negative (-) charge.
[0080] The shell 222 may surround the core 221. The shell 222 may include an insulating material such as PEEK, carbon PEEK, and / or polyvinylidene fluoride (PVDF). When the core 221 is energized, the shell 222 may be polarized (or dielectrically polarized).
[0081] In various embodiments, the shell 222 may include a material with low thermal conductivity. For example, the thermal conductivity of the shell 222 may be 0.3W / mK or less, and the shell 222 may include, for example, polyphenylene sulfide (PPS) with a thermal conductivity of 0.29W / mK, PEEK with a thermal conductivity of 0.26W / mK, polytetrafluoroethylene with a thermal conductivity of 0.5W / mK, or any other suitable material with lower thermal conductivity. The voltage level of the power supplied by the power supply 300 may be set or determined based on the thermal conductivity of the shell 222 (or the support pin 220). In other words, in an embodiment where the thermal conductivity of the shell 222 is relatively high, the voltage level of the power supplied by the power supply 300 may increase with an increase in the heat transfer rate from the support pin 220 to the substrate 20. In this case, the high voltage level of the power supplied by the power supply 300 may produce defective products. Therefore, the shell 222 (or the support pin 220) may be made of a material with low thermal conductivity to prevent or reduce defective products due to high voltage levels.
[0082] The power supply 300 may include a power generation circuit 310 and a switching circuit 320 .
[0083] The power generation circuit 310 may generate power (or voltage) having a fixed voltage level. For example, the power generation circuit 310 may be implemented as a direct current (DC) converter.
[0084] In some embodiments, the power generation circuit 310 can be based on the photoresist layer 23 (see Figure 3A) determines the voltage level of the supplied power based on the characteristics of the solvent in the solvent. For example, if the polarity of the solvent is relatively high, the power generation circuit 310 can relatively reduce the voltage level (or size) of the power. For example, if the polarity of the solvent is relatively low, the power generation circuit 310 can relatively increase the voltage level of the power.
[0085] In some embodiments, the power generation circuit 310 may determine the voltage level of the supplied power based on the thermal conductivity of the support pin 220. For example, if the thermal conductivity of the support pin 220 is relatively high, the power generation circuit 310 may relatively increase the voltage level (or size) of the power. For example, if the thermal conductivity of the support pin 220 is relatively low, the power generation circuit 310 may relatively reduce the voltage level of the power.
[0086] The switch circuit 320 may couple the power line PL to the power generation circuit 310 in response to a control signal CS provided from an external device. FIG. 5A to FIG. 5C As described, the switch circuit 320 may connect the power line PL to the output terminal of the power generation circuit 310 when or after the drying process starts (ie, upon receiving the control signal CS indicating that the drying process starts or has started).
[0087] In some embodiments, the switch circuit 320 may couple the power line PL to a reference power source (e.g., ground) in response to the control signal CS. In embodiments where the power line PL is left floating when the drying process is not performed, static electricity may be caused or generated through the power line PL. Therefore, when the drying process is not performed, the switch circuit 320 may couple the power line PL to the reference power source.
[0088] As reference Figure 4 As described, one or more support pins 220 may include metal and thus be energized by power provided from power source 300. Power source 300 may apply power to one or more support pins 220 through switch circuit 320, or couple one or more support pins 220 to ground.
[0089] Although Figure 4 The power supply 300 is shown to include a switch circuit 320, but the present disclosure is not limited thereto. For example, the power supply 300 (or the power generation circuit 310) can control the voltage level of the power in response to the control signal CS so that the power has a first voltage level (i.e., a voltage level for energizing one or more support pins 220) or a ground voltage level (i.e., a voltage level for grounding one or more support pins 220).
[0090] FIG. 5A to FIG. 5C It is used for Figure 4 The operation of one of the one or more support pins 220 and the power supply 300 will be described in detail. FIG. 5A to FIG. 5C Operations of the power supply 300 including a first task of supplying the substrate 20, a second task immediately before decompression (or immediately after decompression), and a third task during decompression during the drying process are shown.
[0091] In the case of the first task, such as Figure 5A As shown in , the support pin 220 can be connected to the ground. For example, before the vacuum dryer 10 starts to decompress, the first control signal CS1 can be provided to the power supply 300, and the switch circuit 320 can connect the support pin 220 to the ground in response to the first control signal CS1. For example, in an embodiment where the chamber 100 is opened or the cover 120 is spaced apart from the substrate 110, the first control signal CS1 can be provided to the power supply 300, and the switch circuit 320 can connect the support pin 220 to the ground in response to the first control signal CS1.
[0092] Thereafter, in the case of the second task, if Figure 5B As shown in , power is applied to the support pin 220 from the power generation circuit 310, and the support pin 220 can be energized. For example, immediately before or after the vacuum dryer 10 starts to decompress, the second control signal CS2 can be provided to the power supply 300, the switch circuit 320 can couple the support pin 220 to the power generation circuit 310 in response to the second control signal CS2, and the power generated from the power generation circuit 310 can be provided to the support pin 220. For example, in an embodiment in which the chamber 100 is closed or the cover 120 is in close contact with the substrate 110, the second control signal CS2 can be provided to the power supply 300, the switch circuit 320 can couple the support pin 220 to the power generation circuit 310 in response to the second control signal CS2, and the power generated from the power generation circuit 310 can be provided to the support pin 220.
[0093] For example, the core 221 of each support pin 220 may be energized to have a negative (-) charge, the inner portion of the shell 222 (i.e., the portion of the shell 222 adjacent to the core 221) may be polarized to a positive (+) polarity, and the outer portion of the shell 222 (i.e., the portion of the shell 222 adjacent to the substrate 20) may be polarized to a negative (-) polarity. In other words, the support pin 220 may be energized to have a negative (-) charge.
[0094] Although Figure 5B The support pin 220 is shown to be energized to have a negative (−) charge, but this is for illustration purposes only, and the support pin 220 may be energized to have a positive (+) charge.
[0095] The charged support pins 220 can use electrostatic attraction to pull the solvent SOL of the photoresist layer 23, so that the solvent SOL of the photoresist layer 23 can move to the first area A1 (i.e., the portion of the substrate 20 that contacts or overlaps with the support pins 220). That is, the solvent SOL having polarity can be pulled or attracted to the first area A1 by the electrostatic attraction of the support pins 220. Therefore, the thickness of the first area A1 of the photoresist layer 23 can be relatively increased.
[0096] Thereafter, in the case of the third task, if Figure 5C As shown in , the solvent SOL of the photoresist layer 23 can be evaporated. Since the support pins 220 are in direct contact with the substrate 20, heat can be transferred to the substrate 20 through the support pins 220, and the evaporation rate of the solvent SOL in the first area A1 can be relatively high compared to the area or part of the substrate 20 that is not in contact with one or more support pins 220 and does not overlap with one or more support pins 220. If the moving speed of the solvent SOL caused by the electrostatic attraction of the support pins 220 is set to be equal to or approximate to the difference in evaporation speed (i.e., the difference between the evaporation speed of the contact portion P1 (or the first area A1) and the evaporation speed of the non-contact portion P2), the thickness of the photoresist layer 23 (or photoresist) in the first area A1 can be maintained the same or substantially the same as the thickness of the photoresist layer 23 in other areas (i.e., the non-contact portion P2). In other words, the overall thickness of the photoresist layer 23 can be maintained uniform or substantially uniform.
[0097] As reference FIG. 5A to FIG. 5C As described, since the solvent SOL of the photoresist layer 23 may move to the first region A1 by the electrostatic attraction of the support pins 220 , even if the solvent SOL in the first region A1 evaporates relatively quickly, occurrence of a difference in thickness of the photoresist layer 23 may be mitigated or prevented.
[0098] In the vacuum dryer according to various embodiments of the present disclosure, the support pins supporting the substrate to be dried can be energized by applying power to the support pins, so that the solvent of the photoresist (i.e., the solvent including polar molecules) can be attracted (or concentrated) from the non-contact portion of the substrate to the contact portion of the substrate by electrostatic force. Therefore, even if the solvent evaporates relatively quickly on the contact portion, the thickness of the photoresist on the contact portion can be the same or substantially the same as the thickness of the photoresist on the non-contact portion. In other words, the thickness of the photoresist can be kept uniform or substantially uniform.
[0099] Although the spirit and scope of the present disclosure are described by detailed exemplary embodiments, it should be noted that the above embodiments are only illustrative and should not be considered as limiting. It should be understood by those skilled in the art that various changes, substitutions and conversions may be made herein without departing from the scope of the present disclosure as defined by the appended claims.
[0100] The scope of the present disclosure is not limited by the detailed description of this specification, but should be defined by the appended claims. In addition, all changes or modifications of the present disclosure derived from the meaning and scope of the claims and their equivalents should be interpreted as being included in the scope of the present disclosure.
Claims
1. Vacuum dryer, include: a chamber configured to provide an interior space; a support pin located in the interior space near the bottom of the chamber; a power source configured to supply power to the support pin to charge the support pin; as well as A pump is coupled to the interior space in the chamber.
2. The vacuum dryer according to claim 1, further comprising: include: a substrate to be dried in the inner space, wherein the supporting pins directly support the substrate; and A photoresist is on the substrate, wherein the photoresist includes a polar solvent.
3. The vacuum dryer according to claim 2, in, The voltage level of the electrical force is based on the magnitude of the polarity of the solvent, and wherein the voltage level of the electric power is configured to decrease as the polarity of the solvent increases.
4. The vacuum dryer according to claim 2, in, A temperature of a contact portion of the substrate that contacts one of the support pins is higher than a temperature of a non-contact portion of the substrate that is spaced apart from each of the support pins.
5. The vacuum dryer according to claim 1, in, Each of the support pins has one of a cylindrical shape, a hemispherical shape, a conical shape, and a needle shape.
6. The vacuum dryer according to claim 1, in, Each of the support pins includes a core and a shell configured to surround the core, wherein the core comprises a conductive material, and Wherein, the shell comprises insulating material.
7. The vacuum dryer according to claim 6, in, The thermal conductivity of at least one of the support pins is 0.3 W / mK or less, wherein the voltage level of the electrical power is based on the thermal conductivity, and Wherein, the voltage level of the electric power is configured to increase as the thermal conductivity increases.
8. The vacuum dryer according to claim 3, in, The power supply comprises: a power generation circuit configured to generate the power; and a switch circuit configured to couple an output terminal of the power generation circuit to the support pin in response to a first control signal, wherein the switch circuit is configured to couple the support pin to ground in response to a second control signal, wherein the switch circuit is configured to couple the support pin to the ground before the internal space is depressurized, and wherein the switch circuit is configured to couple the output terminal of the power supply to the support pin when the internal space is depressurized.
9. The vacuum dryer according to claim 8, in, When each of the support pins is energized by the power from the power source, a thickness of the photoresist in a first region of the substrate overlaps with one of the support pins and the second region of the substrate is spaced apart from the support pin, becomes greater than a thickness of the photoresist in a second region of the substrate, and When the internal space is decompressed, the thickness of the photoresist in the first region is reduced to be the same as the thickness of the photoresist in the second region.
10. The vacuum dryer according to claim 1, further comprising: include: a support plate disposed on a base plate of the chamber; as well as a lifter coupled to the support plate and configured to adjust the height of the support plate in the interior space, and Wherein, the support pins are distributed on the support plate, wherein the support pins are electrically connected to each other via power lines in the support plate, or The support pins are coupled to the power source independently of each other.
Citation Information
Patent Citations
Method and apparatus of analyzing for network design in wireless communication system
KR1020190036164A
Display panel and manufacturing method thereof
CN103838021A
Liquid crystal display
CN104375342A
Decompression dry device and method
CN1758142A
Thin film formation device and thin film formation
JP1995283108A