A new type of negative pressure composite net
By adopting the design of braided ribs and connecting components and high-temperature forging process in the composite mesh, the problem of easy damage and frequent replacement of the composite mesh is solved, the service life and stability are improved, and the cost and human resource consumption are reduced.
Patent Information
- Application Number
- CN202011037454.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-28
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-09-28
AI Technical Summary
The existing composite mesh is easily damaged during weaving and needs to be replaced frequently, resulting in a waste of human resources, delays in construction, and increased costs.
A new type of negative pressure composite mesh is designed, which uses braided bars combined with connecting components to ensure the stability between the braided bars through structures such as snap-on installation slots, return springs, snap-on plates, upper and lower circular splints, and anti-collision rubber pads. Fix, reduce damage, and improve the strength and toughness of the steel wire through the secondary annealing, wire drawing, cold rolling and quenching processes of the steel.
It improves the service life and stability of the composite mesh, reduces the replacement frequency, reduces human resource consumption and production costs, and ensures the safety and convenience of the process.
Smart Images

Figure CN112170199B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of composite nets, in particular to a novel negative pressure composite net. Background Art
[0002] Composite mesh is a sintered mesh product with a wide range of uses. Composite mesh is made of multiple layers of stainless steel wire mesh stacked together in a fixed structure and processed through sintering, rolling and other processes. Composite mesh is generally divided into five layers, consisting of four parts: protective layer, filter layer, separation layer and support layer. Sintered mesh material is easy to form, process and weld, and can be processed into various forms of filter elements such as round, cylindrical, conical, corrugated, etc.
[0003] However, the composite mesh currently on the market is generally woven into three or four layers, which is easily damaged during use and needs to be replaced every five days. This requires continuous supervision by personnel during use, which increases human resources. At the same time, the replacement is more troublesome, which greatly delays the construction period, resulting in increased costs and waste of raw materials. Summary of the Invention
[0004] The present invention provides a new type of negative pressure composite net, which can effectively solve the problem proposed in the above background technology that the composite net is generally three or four layers of net when woven, which is easily damaged during use and needs to be replaced every five days, so that personnel need to continue to supervise it during use, which increases human resources. At the same time, the replacement is relatively troublesome, which greatly delays the construction period, resulting in increased costs and waste of raw materials.
[0005] To achieve the above-mentioned object, the present invention provides the following technical solutions: a novel negative pressure composite net, comprising a braided rib, a connecting assembly being installed on one side of the braided rib, the connecting assembly comprising a clamping mounting groove, a return spring, a clamping plate, a mounting bayonet, an upper circular clamping plate, a fixed connecting rod, an anti-collision rubber pad, a lower circular clamping plate, a clamping groove, a clamping column, a clamping spring plate, a fixing frame, a connecting port, a clamping fixing groove, an extrusion spring, and a clamping mounting plate;
[0006] The top end face of said sliding arm is fixedly provided with a toothed connecting strip which is cooperatively connected with said toothed connecting strip.
[0007] Preferably, the width of the mounting bayonet is equal to the width of the clamping plate, the bottom end of the upper circular clamping plate and the top end of the lower circular clamping plate are both bonded with protective pads, and the top end of the clamping column is welded with a limiting circular plate.
[0008] Preferably, the length of the clamping mounting plate is greater than the length of the connecting port, and both ends of the clamping mounting plate are embedded and mounted inside the clamping fixing groove.
[0009] A new method for manufacturing a negative pressure composite net.
[0010] S1: Steel material selection: Select the required steel as the raw material for composite mesh wire drawing;
[0011] S2: Steel crystallization: The selected steel is subjected to secondary annealing to change the internal structure of the steel, undergo secondary crystallization, and reduce its internal stress;
[0012] S3: Steel wire drawing: The steel after secondary annealing is drawn to reach the braiding diameter;
[0013] S4: Steel wire cold rolling: The drawn steel wire is passed through a cold rolling mill for bending and cold rolling to achieve the curvature required for braiding.
[0014] S5: Secondary remelting: The cold-rolled steel wire is quenched by a high-frequency electromagnetic coil to increase its hardness;
[0015] S6: Steel wire braiding: Place the quenched steel wire into the braiding machine for braiding;
[0016] S7: Steel mesh trimming: Place the woven steel mesh on the cutting machine for trimming to make it neat;
[0017] S8: Welding frame: Place the wire mesh into the frame and spot weld the connection between the frame and the wire mesh to fix it.
[0018] Preferably, when selecting steel in S1, ordinary carbon steel is generally selected as the raw material of the woven mesh, pure iron and low carbon steel can also be used as raw materials for the woven mesh, and when ordinary carbon steel is recrystallized in S2, the recrystallization temperature is 900°C to 980°C, and the recrystallization time is one hour. The recrystallization temperature for pure iron is 450°C to 550°C, and the recrystallization time is one hour. The recrystallization temperature for low carbon steel is 540°C to 680°C, and the recrystallization time is one hour.
[0019] Preferably, the steel is drawn in S3, and after the annealing of the steel is completed, the steel that still has a certain temperature is placed in a wire drawing machine for wire drawing, and the steel that has not been drawn at the rear end is continued to be heated during wire drawing. During wire drawing, the wire drawing temperature of ordinary carbon steel should be maintained between 1200°C and 1250°C, the wire drawing temperature of pure iron should be maintained between 850°C and 1050°C, and the wire drawing temperature of low carbon steel should be maintained between 900°C and 1100°C.
[0020] Preferably, when the steel wire is cold rolled in S4, the curvature of the steel wire shall not exceed 120 degrees. When the cold rolled steel wire is returned to the furnace in S5, the steel wire should be slowly quenched and heated by a high-frequency electromagnetic coil. When ordinary carbon steel wire is quenched and heated, the heating temperature should be maintained between 840°C and 860°C, and attention should be paid to slow cooling to avoid initial thermal stress fracture. When pure iron wire is quenched, the temperature should be maintained between 740°C and 760°C, and attention should be paid to slow cooling to avoid initial thermal stress fracture. Low carbon steel should not be quenched by high-frequency quenching, and generally a strong quenching process is used. The temperature is maintained between 920°C and 940°C during quenching.
[0021] Preferably, the steel wires are braided in S6 according to the herringbone weaving method, and anti-collision gaskets are filled inside the steel wires during the weaving process to prevent the connection positions from being hit and damaging the anti-rust layer.
[0022] Preferably, when cutting the wire mesh in S7, the protruding steel wires at both ends need to be cut off first, and after the cutting is completed, the wire mesh is cut into a required length as needed.
[0023] Preferably, when welding is performed in S8, a frame having the same length and width as the wire mesh needs to be selected for welding to avoid bending of the wire mesh, and the frame has good flexibility and is convenient for use with the machine.
[0024] Compared with the prior art, the present invention has the following beneficial effects: the present invention has a scientific and reasonable structure and is safe and convenient to use:
[0025] A connecting component is provided, and the woven ribs are isolated by means of a clamping plate and an anti-collision rubber pad to avoid collision between the woven ribs and damage to the anti-rust layer. At the same time, the single-layer weaving avoids internal damage to the mesh layer due to interference between multiple layers of mesh. The woven ribs are fixed by the upper circular splint and the lower circular splint to ensure their stability during use and avoid loosening due to shaking. At the same time, the clamping mounting plate is used to facilitate the connection between the composite mesh and the machine.
[0026] The present invention is provided with steel crystallization, steel wire drawing, steel wire cold rolling, secondary remelting and steel wire weaving. The selected steel is subjected to secondary crystallization through high-temperature forging, so that the steel produces new strain-free crystals, reducing the stress inside the steel. At the same time, through high-temperature wire drawing, the toughness of the steel wire is increased while the stress inside the steel is further reduced, and the strength of the steel wire is increased. It is directly pressed into shape through cold rolling to avoid the cooling deformation during high-temperature forming. At the same time, its hardness is increased through secondary remelting, ensuring the suitable service life of the steel wire during use. At the same time, through the herringbone cross weaving, the contact area between the steel wires is increased, and the steel wires are crossed with each other to share the load, thereby reducing the load-bearing of a single steel wire, thereby increasing the service life of the composite mesh. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention.
[0028] In the attached figure:
[0029] Figure 1 It is a structural schematic diagram of the present invention;
[0030] Figure 2 is a schematic structural diagram of the connection assembly of the present invention;
[0031] Figure 3 This is a schematic diagram of the installation structure of the upper circular splint of the present invention;
[0032] Figure 4 It is a schematic diagram of the installation structure of the clamping installation plate of the present invention;
[0033] Figure 5 It is a schematic flow chart of the production method of the present invention;
[0034] Numbers in the figure: 1, braided reinforcement;
[0035] 2. Connecting assembly; 201. Snap-fit mounting groove; 202. Reset spring; 203. Snap-fit plate; 204. Mounting bayonet; 205. Upper circular clamping plate; 206. Fixed connecting rod; 207. Anti-collision rubber pad; 208. Lower circular clamping plate; 209. Snap-fit groove; 210. Snap-fit column; 211. Snap-fit spring plate; 212. Fixed frame; 213. Connecting port; 214. Snap-fit fixing groove; 215. Extrusion spring; 216. Snap-fit mounting plate. DETAILED DESCRIPTION
[0036] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0037] Example 1: Figure 1-4 As shown, the present invention provides a new negative pressure composite net technical solution, a new negative pressure composite net, including a braided rib 1, a connecting assembly 2 is installed on one side of the braided rib 1, and the connecting assembly 2 includes a clamping installation groove 201, a return spring 202, a clamping plate 203, a mounting bayonet 204, an upper circular clamping plate 205, a fixed connecting rod 206, an anti-collision rubber pad 207, a lower circular clamping plate 208, a clamping groove 209, a clamping column 210, a clamping spring plate 211, a fixing frame 212, a connecting port 213, a clamping fixing groove 214, an extrusion spring 215 and a clamping installation plate 216;
[0038] A snap-fitting mounting groove 201 is equidistantly provided at one end of the braided reinforcement 1, and a reset spring 202 is symmetrically welded on both sides of one end of the snap-fitting mounting groove 201. The top of the reset spring 202 is spot-welded and mounted on the bottom end of the snap-fitting plate 203. A mounting bayonet 204 is provided in the middle of the top end of the snap-fitting plate 203. The width of the mounting bayonet 204 is equal to the width of the snap-fitting plate 203, which is convenient for snapping together the two snap-fitting plates 203. An upper circular splint 205 is placed at the top of the intersection between the two braided reinforcements 1, and the bottom ends of the upper circular splint 205 are symmetrical on both sides. A fixed connecting rod 206 is welded, and one end of the fixed connecting rod 206 is sleeved with an anti-collision rubber pad 207. A lower circular splint 208 is placed at the bottom end of the intersection between the two woven reinforcements 1. The bottom end of the upper circular splint 205 and the top end of the lower circular splint 208 are both bonded with protective pads to facilitate the protection of the surface of the woven reinforcement. A snap-in groove 209 is provided on both sides of one end of the upper circular splint 205 and the lower circular splint 208, and a snap-in column 210 is embedded in the inner side of the snap-in groove 209. A limiting circular plate is welded to the top end of the snap-in column 210. It is convenient to fix the upper circular splint 205 and the lower circular splint 208, so as to fix the braided ribs. A clamping spring plate 211 is welded to the bottom of one end of the clamping column 210, and one end of multiple braided ribs 1 is welded and installed on the inner side of the fixing frame 212. Connecting ports 213 are symmetrically provided at both ends of the fixing frame 212, and clamping fixing grooves 214 are symmetrically provided at both ends of the connecting port 213. Extrusion springs 215 are symmetrically welded on both sides of the clamping fixing groove 214 at one end of the connecting port 213, and a clamping mounting plate 216 is welded on the end of the extrusion spring 215 away from the clamping fixing groove 214. The length of the clamping mounting plate 216 is greater than the length of the connecting port 213. Both ends of the clamping mounting plate 216 are embedded and installed on the inner side of the clamping fixing groove 214, which is convenient for it to be connected with external machinery.
[0039] Example 2: Figure 5 As shown, the present invention provides a technical solution for a novel method for manufacturing a negative pressure composite net, a novel method for manufacturing a negative pressure composite net,
[0040] S1: Steel material selection: Select the required steel as the raw material for composite mesh wire drawing;
[0041] S2: Steel crystallization: The selected steel is subjected to secondary annealing to change the internal structure of the steel, undergo secondary crystallization, and reduce its internal stress;
[0042] S3: Steel wire drawing: The steel after secondary annealing is drawn to reach the braiding diameter;
[0043] S4: Steel wire cold rolling: The drawn steel wire is passed through a cold rolling mill for bending and cold rolling to achieve the curvature required for braiding.
[0044] S5: Secondary remelting: The cold-rolled steel wire is quenched by a high-frequency electromagnetic coil to increase its hardness;
[0045] S6: Steel wire braiding: Place the quenched steel wire into the braiding machine for braiding;
[0046] S7: Steel mesh trimming: Place the woven steel mesh on the cutting machine for trimming to make it neat;
[0047] S8: Welding frame: Place the wire mesh into the frame and spot weld the connection between the frame and the wire mesh to fix it.
[0048] When selecting steel in S1, ordinary carbon steel is generally selected as the raw material for the woven mesh. Pure iron and low carbon steel can also be used as raw materials for the woven mesh. When ordinary carbon steel is recrystallized in S2, the recrystallization temperature is 900°C to 980°C, and the recrystallization time is one hour. The recrystallization temperature for pure iron is 450°C to 550°C, and the recrystallization time is one hour. The recrystallization temperature for low carbon steel is 540°C to 680°C, and the recrystallization time is one hour.
[0049] In S3, the steel is drawn. After the annealing of the steel is completed, the steel that still has a certain temperature is placed in the wire drawing machine for wire drawing, and the steel at the rear end that has not been drawn is continued to be heated during wire drawing. During wire drawing, the wire drawing temperature of ordinary carbon steel should be maintained between 1200℃ and 1250℃, the wire drawing temperature of pure iron should be maintained between 850℃ and 1050℃, and the wire drawing temperature of low carbon steel should be maintained between 900℃ and 1100℃.
[0050] When the steel wire is cold rolled in S4, the curvature of the steel wire shall not exceed 120 degrees. When the cold-rolled steel wire is returned to the furnace in S5, the steel wire should be slowly quenched and heated by a high-frequency electromagnetic coil. When quenching and heating ordinary carbon steel wire, the heating temperature should be maintained between 840℃ and 860℃, and attention should be paid to slow cooling to avoid initial thermal stress fracture. When quenching pure iron wire, the temperature should be maintained between 740℃ and 760℃, and attention should be paid to slow cooling to avoid initial thermal stress fracture. Low carbon steel is not suitable for high-frequency quenching. Generally, a strong quenching process is used, and the temperature should be maintained between 920℃ and 940℃ during quenching.
[0051] When weaving the steel wire in S6, it needs to be woven according to the herringbone weaving method. At the same time, anti-collision gaskets are filled inside the steel wire during the weaving process to prevent the connection position from impacting and damaging the anti-rust layer.
[0052] When cutting the wire mesh in S7, it is necessary to first cut off the protruding wires at both ends, and then cut the wire mesh into the required length as needed after the cutting is completed.
[0053] When welding in S8, you need to choose a frame that is equal to the length and width of the wire mesh to avoid bending of the wire mesh. The frame should be flexible and easy to use with the machine.
[0054] The working principle and use process of the present invention are as follows: when it is necessary to weave the wire mesh, the staff will combine multiple braided bars in a herringbone connection method, and align the installation bayonet 204 of the two clamping plates 203. After alignment, the installation bayonet 204 will be clamped to each other so that the clamping plates 203 fit together. When the clamping plates 203 fit together, the reset spring 202 is squeezed, and the two clamping plates 203 fit together more tightly under the reset action of the reset spring 202. After the braided bars 1 are clamped to each other, the upper circular splint 205 is placed at the intersection of the two braided bars 1, and the anti-collision rubber pad 207 is placed between the two braided bars 1. The fixed connecting rod 206 passes through the anti-collision rubber pad 207, and the clamping column 210 passes through the clamping groove 209, and then the lower circular clamping plate 208 is placed at the bottom end of the intersection of the two braided reinforcements 1, and the clamping column 210 passes through the clamping groove 209 again, and the upper circular clamping plate 205 and the lower circular clamping plate 208 are fixed under the clamping and resetting action of the clamping spring plate 211, so as to clamp and fix the two braided reinforcements 1, thereby completing the weaving of the wire mesh, and after the weaving is completed, the wire mesh is trimmed, and after the trimming is completed, the composite mesh is placed in the fixing frame 212, and the connection between the wire mesh and the fixing frame 212 is welded, thereby completing the production of the composite mesh;
[0055] When the composite net needs to be used, the staff pulls the snap-fit mounting plate 216 and snap-fits the snap-fit mounting plate 216 to the external machine, and snaps the snap-fit mounting plate 216 into the snap-fit fixing groove 214, and fixes the snap-fit mounting plate 216 to the external machine under the resetting snap-fitting action of the extrusion spring 215.
[0056] Finally, it should be noted that the above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art will be able to modify the technical solutions described in the aforementioned embodiments or substitute equivalents for some of the technical features. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention shall be included within the scope of protection of the present invention.
Claims
1. A novel negative pressure composite net, comprising braided ribs (1), Features: A connecting assembly (2) is installed on one side of the braided reinforcement (1), and the connecting assembly (2) comprises a clamping installation groove (201), a return spring (202), a clamping plate (203), a mounting bayonet (204), an upper circular clamping plate (205), a fixed connecting rod (206), an anti-collision rubber pad (207), a lower circular clamping plate (208), a clamping groove (209), a clamping column (210), a clamping spring plate (211), a fixing frame (212), a connecting port (213), a clamping fixing groove (214), a compression spring (215) and a clamping installation plate (216); One end of the braided rib (1) is provided with a snap-fit installation groove (201) at equal intervals, and a return spring (202) is symmetrically welded on both sides of one end of the snap-fit installation groove (201), and the top end of the return spring (202) is spot-welded and installed on the bottom end of the snap-fit plate (203), and a mounting bayonet (204) is provided in the middle of the top end of the snap-fit plate (203), and an upper circular clamping plate (205) is placed at the top end of the intersection between the two braided ribs (1), and fixed connecting rods (206) are symmetrically welded on both sides of the bottom end of the upper circular clamping plate (205), and one end of the fixed connecting rod (206) is sleeved with an anti-collision rubber pad (207), and a lower circular clamping plate (208) is placed at the bottom end of the intersection between the two braided ribs (1), and the upper circular clamping plate (205) is provided with a plurality of fixed connecting rods (206) at the bottom end. ) and one end of the lower circular clamping plate (208) are provided with a clamping groove (209) on both sides, a clamping column (210) is embedded in the inner side of the clamping groove (209), a clamping spring plate (211) is welded at the bottom of one end of the clamping column (210), one end of the plurality of braided ribs (1) is welded and installed on the inner side of the fixing frame (212), connecting ports (213) are symmetrically provided at both ends of the fixing frame (212), and clamping fixing grooves (214) are symmetrically provided at both ends of the connecting port (213), and extrusion springs (215) are symmetrically welded on both sides of the inner side of the clamping fixing groove (214) located at one end of the connecting port (213), and a clamping installation plate (216) is welded at one end of the clamping fixing groove (214); The width of the mounting bayonet (204) is equal to that of the clamping plate (203); the bottom end of the upper circular clamping plate (205) and the top end of the lower circular clamping plate (208) are both bonded with protective pads; and a limiting circular plate is welded to the top end of the clamping column (210); The length of the clamping installation plate (216) is greater than the length of the connection port (213), and both ends of the clamping installation plate (216) are embedded and installed inside the clamping fixing groove (214).
2. The method for manufacturing the novel negative pressure composite net according to claim 1, It is characterized in that S1: Steel material selection: Select the required steel as the raw material for composite mesh wire drawing; S2: Steel crystallization: The selected steel is subjected to secondary annealing to change the internal structure of the steel, undergo secondary crystallization, and reduce its internal stress; S3: Steel wire drawing: The steel after secondary annealing is drawn to reach the braiding diameter; S4: Steel wire cold rolling: The drawn steel wire is bent and cold rolled through a cold rolling mill to achieve the curvature required for braiding; S5: Secondary remelting: The cold-rolled steel wire is quenched by a high-frequency electromagnetic coil to increase its hardness; S6: Steel wire braiding: The quenched steel wire is placed in the braiding machine for braiding; S7: Steel mesh trimming: Place the woven steel mesh on the cutting machine for trimming to make it neat; S8: Welding frame: Place the wire mesh into the frame, and spot weld the connection between the frame and the wire mesh to fix it.
3. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that In S1, when selecting steel, ordinary carbon steel is generally selected as the raw material of the woven mesh. Pure iron and low carbon steel can also be used as raw materials for the woven mesh. When ordinary carbon steel is recrystallized in S2, the recrystallization temperature is 900°C to 980°C, and the recrystallization time is one hour. The recrystallization temperature for pure iron is 450°C to 550°C, and the recrystallization time is one hour. The recrystallization temperature for low carbon steel is 540°C to 680°C, and the recrystallization time is one hour.
4. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that In the S3, the steel is drawn. After the annealing of the steel is completed, the steel that still has a certain temperature is placed in a wire drawing machine for wire drawing, and the steel that has not been drawn at the rear end is continuously heated during wire drawing. During wire drawing, the wire drawing temperature of ordinary carbon steel should be maintained between 1200°C and 1250°C, the wire drawing temperature of pure iron should be maintained between 850°C and 1050°C, and the wire drawing temperature of low carbon steel should be maintained between 900°C and 1100°C.
5. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that When the steel wire is cold rolled in S4, the curvature of the steel wire shall not exceed 120 degrees. When the cold rolled steel wire is returned to the furnace in S5, the steel wire should be slowly quenched and heated by a high-frequency electromagnetic coil. When ordinary carbon steel wire is quenched and heated, the heating temperature should be maintained between 840°C and 860°C, and attention should be paid to slow cooling to avoid initial thermal stress fracture. When pure iron wire is quenched, the temperature should be maintained between 740°C and 760°C, and attention should be paid to slow cooling to avoid initial thermal stress fracture. High-frequency quenching is not suitable for low-carbon steel. Generally, a strong quenching process is used, and the temperature is maintained between 920°C and 940°C during quenching.
6. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that In the S6, the steel wires need to be braided according to the herringbone braiding method, and anti-collision gaskets are filled inside the steel wires during the braiding process to prevent the connection positions from impacting and damaging the anti-rust layer.
7. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that When cutting the wire mesh in S7, the protruding steel wires at both ends need to be cut off first, and after the cutting is completed, the wire mesh is cut into a required length according to needs.
8. A method for manufacturing a novel negative pressure composite net according to claim 2, It is characterized in that When welding is performed in S8, it is necessary to select a frame that is equal to the length and width of the wire mesh for welding to avoid bending of the wire mesh, and the frame has good flexibility and is easy to use with the machine.