Emulsified cosmetics and method for producing the same

By combining water-soluble cationic polymers and anionic polymers in emulsified cosmetics to form a stable coating, the problem of insufficient water resistance and friction resistance of existing emulsified cosmetics is solved, and better film durability and protection are achieved. UV effect.

CN112654342BActive Publication Date: 2024-11-26KOSE CORPORATION
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980058468.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-11-01
Filing Date
2019-10-30
Publication Date
2024-11-26
Estimated Expiration
2039-10-30

AI Technical Summary

Technical Problem

During the use of existing emulsified cosmetics, there are problems such as insufficient water resistance and friction resistance, which leads to the coating film being easily shedded and its functionality is reduced.

Method used

Add water-soluble cationic polymer to the oil phase and add water-soluble anionic polymer to the water phase to condense it to form a solid coating film, thereby improving the water resistance and friction resistance of the coating film.

Benefits of technology

It achieves high water resistance and friction resistance of emulsified cosmetics, improves the stability and sense of use of the preparation, and ensures the durability of the coating and UV protection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0002965363370000141
    Figure BDA0002965363370000141
  • Figure BDA0002965363370000161
    Figure BDA0002965363370000161
  • Figure BDA0002965363370000171
    Figure BDA0002965363370000171
Patent Text Reader

Abstract

The present invention provides an emulsified cosmetic which forms a coating film having excellent water resistance and friction resistance and also has formulation stability and good usability. An emulsified cosmetic comprising an oil phase and an aqueous phase, wherein the oil phase comprises (a) a water-soluble cationic polymer and the aqueous phase comprises (b) a water-soluble anionic polymer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an emulsified cosmetic, and more particularly to an emulsified cosmetic containing an oil phase and an aqueous phase, wherein the oil phase contains a water-soluble cationic polymer and the aqueous phase contains a water-soluble anionic polymer, and a method for producing the same. Background Art

[0002] In recent years, the demand for functional cosmetics has been growing, and various functional cosmetics have been developed according to the purpose of use. There are many products that embody functions by forming a coating film on the skin and hair, for example, products that prevent frizziness (Japanese original: うねり) of hair during the day when humidity is high, and cosmetics with high UV protection in foundation and sunscreen that protect the skin from UVA (long-wavelength ultraviolet rays with a wavelength of 320 to 400nm) and UVB (medium-wavelength ultraviolet rays with a wavelength of 290 to 320nm).

[0003] However, it is known that the coating film formed when applying cosmetics will fall off over time and its functionality will decrease. In particular, the coating film will fall off more significantly when subjected to physical friction, sweating, bathing in a swimming pool or the sea, etc., so it is sought to develop cosmetics that are less likely to decrease in functionality.

[0004] Therefore, the following technologies have been developed, etc.: In order to solidify an oily component containing hydrophobized fine zinc oxide and an oil-soluble ultraviolet absorber into a coating film, a technology of imparting high water resistance by selecting silicic anhydride as a gelling agent (for example, Japanese Patent Publication No. 2018-76313); a fine metal oxide having a surface coated with a specific compound is dispersed in an oil phase together with a specific partially cross-linked organopolysiloxane polymer and polyhydroxystearic acid, and this is combined with a (sodium acrylate / sodium acryloyldimethyl taurate) copolymer to form an oil-in-water emulsified cosmetic, thereby forming a soft and uniform cosmetic film to impart water resistance (for example, Japanese Patent Publication No. 2017-137300); a technology of obtaining a stable oil-in-water emulsion composition by using a polyion complex formed by a specific combination of a cationic polymer and an anionic polymer as an emulsifier, and various oil components can be added, and the obtained oil-in-water emulsion exhibits excellent water resistance (for example, Japanese Patent Publication No. 2011-32249). Summary of the invention

[0005] However, the above-mentioned technologies have problems such as poor touch as cosmetics and insufficient water resistance and friction resistance.

[0006] Therefore, an object of the present invention is to provide an emulsified cosmetic which forms a coating film having excellent water resistance and abrasion resistance and further has formulation stability and good usability.

[0007] In view of the above circumstances, the inventors have tried to combine a cationic polymer and an anionic polymer in the same phase. Then, the inventors have found the following problems: when the cationic polymer and the anionic polymer are combined in the same phase, coagulation occurs and a preparation cannot be made. As a result of intensive studies, the following findings have been obtained: by containing a water-soluble cationic polymer in the oil phase and a water-soluble anionic polymer in the water phase, the stability as a preparation is achieved. Furthermore, when coating, the water-soluble cationic polymer and the water-soluble anionic polymer coagulate to form a firm coating film, whereby the water resistance and abrasion resistance of the coating film are improved, and good usability is obtained, thus completing the present invention.

[0008] That is, the present invention is as described below.

[0009] (1) An emulsified cosmetic, which contains an oil phase and a water phase, wherein the oil phase contains (a) a water-soluble cationic polymer and the water phase contains (b) a water-soluble anionic polymer.

[0010] (2) The emulsified cosmetic according to (1), wherein the emulsified cosmetic contains at least one of (c) a metal oxide or a plate-like powder.

[0011] (3) The emulsified cosmetic according to (1) or (2), wherein the emulsified cosmetic contains (d) stearoyl inulin.

[0012] (4) The emulsified cosmetic according to any one of (1) to (3), wherein the mass ratio (a) / (b) of the content of (a) the water-soluble cationic polymer to the content of (b) the water-soluble anionic polymer is 0.05 to 20.

[0013] (5) The emulsified cosmetic according to any one of (1) to (4), wherein (a) the water-soluble cationic polymer is selected from one or more of a dimethyldiallylammonium chloride / acrylamide copolymer, 2-hydroxy-3-(trimethylammonio)propyl poly(ethylene oxide) cellulose ether (Japanese original: chloride O-[2-hydroxy-3-(trimethylammonio)propyl] hydroxyethyl cellulose), and guar gum hydroxypropyltrimethylammonium chloride (Japanese original: chloride O-[2-hydroxy-3-(trimethylammonio)propyl] guar gum).

[0014] (6) The emulsified cosmetic according to any one of (1) to (5), wherein (b) the water-soluble anionic polymer is selected from one or more of a carboxyvinyl polymer, an acrylic acid / alkyl methacrylate copolymer, and a sodium acrylate / sodium acryloyldimethyltaurate copolymer.

[0015] (7) The emulsified cosmetic according to any one of (1) to (6), wherein the emulsified cosmetic is an oil-in-water emulsified cosmetic.

[0016] (8) The emulsified cosmetic according to any one of (1) to (7), wherein the emulsified cosmetic contains (e) benzalmalonate polysiloxane.

[0017] (9) A method for producing an emulsified cosmetic, wherein the emulsified cosmetic comprises an oil phase and an aqueous phase, wherein the oil phase comprises (a) a water-soluble cationic polymer, and the aqueous phase comprises (b) a water-soluble anionic polymer. DETAILED DESCRIPTION

[0018] Below, the preferred embodiments of the present invention are described in detail. However, the present invention is not limited to the following preferred embodiments and can be freely changed within the scope of the present invention. In addition, in this specification, "~" represents a range of numerical values ​​including the range before and after it. In addition, unless otherwise specified, the operation and the measurement of physical properties are carried out under the conditions of room temperature (20~25℃) / relative humidity 40~50%RH.

[0019] The emulsified cosmetic of the present invention contains a water-soluble cationic polymer in the oil phase and a water-soluble anionic polymer in the water phase, so that an emulsified cosmetic having high water resistance, strong friction resistance (high friction resistance), excellent feeling in use (for example, no stickiness, sliminess, and moist touch), and excellent stability can be provided.

[0020] (Emulsified cosmetics)

[0021] The emulsified cosmetic of the present invention is an emulsified cosmetic in which either an oil phase containing component (a) a water-soluble cationic polymer or an aqueous phase containing component (b) a water-soluble anionic polymer exists as emulsified droplets, and may contain other components within a range that does not impair the effects of the present invention.

[0022] The water-soluble cationic polymer (a) used in the present invention (hereinafter, also referred to as component (a)) is a polymer having a cationic group in the molecule. The water-soluble cationic polymer (a) is not particularly limited as long as it is a water-soluble cationic polymer generally used in cosmetics. From the advantages of the feel and water resistance when forming a coating film with a water-soluble anionic polymer, it is preferably a water-soluble cationic polymer containing an amino group or an ammonium group bonded to the polymer chain, or containing dimethyldiallylammonium halide as a constituent unit.

[0023] As the component (a), there is no particular limitation, and examples thereof include vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate copolymer diethyl sulfate, dimethyldiallylammonium chloride / acrylamide copolymer, acrylamide / acrylic acid / dimethyldiallylammonium chloride copolymer, dimethyldiallylammonium chloride / acrylic acid copolymer, polydimethylmethylene piperidinium chloride, 2-hydroxy-3-(trimethylammonio)propyl poly(ethylene oxide) cellulose ether, guar gum hydroxypropyltrimethylammonium chloride, vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate copolymer diethyl sulfate, guar gum hydroxypropyltrimethylammonium chloride, 2-methacryloyloxyethyl phosphorylcholine / 2-hydroxy-3-methacryloyloxypropyltrimethylammonium chloride copolymer, O-(2-hydroxy-3-(trimethylammonio)propyl) locust bean gum chloride, hydroxypropyltriammonium chloride starch, vinylpyrrolidone / N,N-dimethylaminoethyl methacrylate / stearyl acrylate / tripropylene glycol diacrylate copolymer, hyaluronic acid hydroxypropyltriammonium salt, etc., and one or more of them can be used. Among them, from the viewpoints of water resistance and abrasion resistance of the formed coating film, dimethyldiallylammonium chloride / acrylamide copolymer, 2-hydroxy-3-(trimethylammonio)propyl poly(ethylene oxide) cellulose ether, and guar gum hydroxypropyltrimethylammonium chloride are particularly preferred, and dimethyldiallylammonium chloride / acrylamide copolymer is most preferred.

[0024] Commercially available examples of the component (a) in the present invention include, for example, chlorinated 2-hydroxy-3-(trimethylamino)propyl polyethylene oxide cellulose ether, such as LEOGARD GP (manufactured by Lion) and Catinal HC-100 (manufactured by Toho Chemical Industry Co., Ltd.), which are polyquaternium 10; dimethyldiallylammonium chloride / acrylamide copolymers, such as Lipoflow MN (manufactured by Lion), MERQUAT 550PR, and MERQUAT 740POLYMER (manufactured by Lubrizol Japan Co., Ltd.), which are aqueous solutions of polyquaternium-7; and acrylamide / acrylic acid / dimethyldiallylammonium chloride copolymers, such as MERQUAT 900, which are aqueous solutions of polyquaternium-39. 3331PR (manufactured by Lubrizol, Japan), as dimethyldiallylammonium chloride / acrylic acid copolymer, MERQUAT295Polymer (manufactured by Lubrizol, Japan) as an aqueous solution of polyquaternium-22, as guar hydroxypropyltrimonium chloride, JAGUAR C-14S (C) (manufactured by SOLVAY) can be mentioned, as an aqueous solution of hydroxypropyltriammonium chloride starch, SENSOMER CI50 (manufactured by Lubrizol, Japan), as hyaluronic acid hydroxypropyltriammonium salt, Hyaloveil P (manufactured by Kewpie), etc.

[0025] The content of component (a) in the present invention is not particularly limited, and can be 0.001 to 3% by mass (hereinafter referred to as "%") in the emulsified cosmetic, preferably 0.001 to 1%, more preferably 0.01 to 1% by mass, further preferably 0.01 to 0.5%, and particularly preferably 0.1 to 0.3%. Within this range, excellent stability is achieved, and water resistance and abrasion resistance can be imparted while maintaining a good feeling of use.

[0026] The component (a) can be contained in the oil phase by dissolving and dispersing the component (a) in the oil phase during the production process.

[0027] The water-soluble anionic polymer (b) used in the present invention (hereinafter also referred to as component (b)) is a polymer having an anionic group in the molecule. The water-soluble anionic polymer (b) is not particularly limited as long as it is a water-soluble anionic polymer commonly used in cosmetics. From the viewpoint of excellent touch, water resistance and friction resistance when forming a coating film with a water-soluble cationic polymer, for example, carboxyvinyl polymers, acrylic acid / alkyl methacrylate copolymers, sodium acrylate / sodium acryloyldimethyltaurate copolymers, alkyl acrylate / alkyl methacrylate / methacrylate polyoxyethylene stearyl ether (20E.O.) copolymers and other acrylic acid-based water-soluble polymers, anionic polysaccharides, anionic polyamino acids, etc., can be cited, and one or more of them can be used. Among them, from the viewpoint of water resistance and friction resistance of the resulting coating film, the water-soluble anionic polymer of component (b) is preferably selected from one or more of carboxyvinyl polymer, acrylic acid / alkyl methacrylate copolymer, sodium acrylate / sodium acryloyl dimethyl taurate copolymer, preferably acrylic acid water-soluble polymer, more preferably acrylic acid / alkyl methacrylate copolymer (preferably acrylic acid / alkyl acrylate (C10-C30) cross-linked polymer), sodium acrylate / sodium acryloyl dimethyl taurate copolymer. Furthermore, from the viewpoint of excellent water resistance and friction resistance, it is particularly preferred to use acrylic acid / alkyl methacrylate copolymer and sodium acrylate / sodium acryloyl dimethyl taurate copolymer in combination. When acrylic acid / alkyl methacrylate copolymer and sodium acrylate / sodium acryloyl dimethyl taurate copolymer are used in combination, the mass ratio of their contents is, for example, acrylic acid / alkyl methacrylate copolymer:sodium acrylate / sodium acryloyl dimethyl taurate copolymer = 1:0.1 to 50, preferably 1:5 to 40, from the viewpoint of excellent water resistance and friction resistance.

[0028] Examples of commercially available products of component (b) include CARBOPOL 940, 941, 980, 981 (carbomer; manufactured by Lubrizol Advanced Materials Inc.), PEMULEN TR-1, TR-2, CARBOPOL POLYMER, 1342 POLYMER, 1382 POLYMER (acrylic acid / alkyl acrylate (C10-C30)) crosslinked polymer; manufactured by Lubrizol Advanced Materials Inc.), SIMULGEL EG (sodium acrylate / sodium acryloyldimethyl taurate copolymer;

[0029] SEPPIC), ACULYN 22 (alkyl acrylate / stearyl alcohol polyether-20 methacrylate copolymer, ROHM GMBH), etc.

[0030] The content of component (b) in the present invention is not particularly limited, but is preferably 0.001 to 2% in the emulsified cosmetic, more preferably 0.001 to 1%, further preferably 0.01 to 0.8%, and particularly preferably 0.01 to 0.5%. Within this range, excellent stability can be achieved, and water resistance and abrasion resistance can be imparted while maintaining a good feeling of use.

[0031] The component (b) can be contained in the aqueous phase by dissolving and dispersing the component (b) in the aqueous phase during the production process.

[0032] The mass ratio (a) / (b) of component (a) and component (b) in the present invention is not particularly limited, but is preferably 0.05 to 20, more preferably 0.1 to 10. Within this range, the stability of the formulation and the water resistance and abrasion resistance of the formed coating film are further improved.

[0033] In the present invention, it is preferred to further contain a component (c) of a metal oxide and / or a plate-like powder (hereinafter, also referred to as component (c)). By adding a component (c) of a metal oxide and / or a plate-like powder, water resistance, abrasion resistance and formulation stability can be further improved. Component (c) can be added to either the aqueous phase or the oil phase, and is particularly preferably added to the oil phase. This is because by adding it to the oil layer, component (a) can be stably added to the oil phase, and formulation stability can be further improved.

[0034] The metal oxide of component (c) used in the present invention is not particularly limited to the shape of sphere, plate, needle, etc., the particle size of smoke, microparticles, pigment grade, etc., porous, non-porous, etc., as long as it is a metal oxide that can be used in general cosmetics, and any one can be used. As the metal oxide of component (c), zinc oxide, titanium oxide, cerium oxide, zirconium oxide, iron oxide, etc. can be listed, and one or more of these can be used in combination, or they can be further composited. From the viewpoint of improving water resistance and friction resistance, zinc oxide or titanium oxide is preferred, and zinc oxide is particularly preferred. In addition, there is no particular limitation on the particle size of the metal oxide, but from the viewpoint of the stability of component (a) in the oil phase, the average primary particle size is preferably in the range of 1 to 100 nm. In addition, in the present invention, the average particle size refers to the average value of the width and length of the powder measured in a dispersed state in water using a laser diffraction / scattering particle size distribution measuring device on the device (the average particle size value of 50% of the cumulative volume). In addition, as necessary, those obtained by surface-treating with a known method using an organic silicon compound, a fluorine compound, a metal soap, collagen, a hydrocarbon, a higher fatty acid, lecithin, a higher alcohol, an ester, a wax, a surfactant, a trialkoxysilane, etc., and further compounding them can be used.

[0035] The plate-like powder of component (c) used in the present invention can be formulated in any phase of the aqueous phase and the oil phase, and is particularly preferably formulated in the oil phase. There is no particular limitation as long as it is a plate-like powder that can be generally used in cosmetics, and examples thereof include mica, sericite, boron nitride, synthetic phlogopite, synthetic sericite, aluminum silicate, magnesium silicate, barium sulfate, magnesium aluminum silicate, cleaved talc, plate-like silicic anhydride, plate-like kaolin, plate-like boron nitride, plate-like cellulose and other physical powders, mica titanium, bismuth oxychloride, etc., and these can be used alone or in combination of two or more. Among them, from the viewpoint of emulsification stability when component (a) is formulated in the oil phase, sericite and boron nitride are preferably used, and sericite is more preferably used. The average particle size of the plate-like powder of component (c) used in the present invention is not particularly limited, and it is preferably 1 to 100 μm, and more preferably 1 to 50 μm. In addition, the aspect ratio is preferably 5 to 500, and more preferably 10 to 100. In the present invention, the average particle size refers to the average value of the width and length of the powder measured in a dispersed state in water using a laser diffraction / scattering particle size distribution measuring device (average particle size value of 50% by volume). In addition, these plate-like powders can be surface-treated using one or more of fluorine compounds, silicone compounds, metal soaps, lecithin, hydrogenated lecithin, collagen, hydrocarbons, higher fatty acids, higher alcohols, esters, waxes, waxes, surfactants and trialkoxysilanes.

[0036] Examples of the organosilicon compounds used for the surface treatment of component (c) include chain organosilicones such as dimethylpolysiloxane with a low degree of polymerization, dimethylpolysiloxane with a high degree of polymerization, methylhydrogenpolysiloxane, and methylphenylpolysiloxane; modified organosilicones such as organosilicon triester phosphates and amino-terminated polydimethylsiloxane, alkyl-modified organosilicones, alkoxy-modified organosilicones, silicone resins such as trimethylsiloxysilicate and acrylate silicone, silicone rubbers, partially or completely crosslinked organopolysiloxanes, and various silylating agents.

[0037] The trialkoxyalkylsilane in the trialkoxyalkylsilane treatment is a compound in which three alkoxy groups and one alkyl group are bonded to a silicon atom, and is a compound that chemically coats the surface of the powder by reacting the alkoxy group with a hydroxyl group on the surface of the powder. The alkoxy group in the trialkoxyalkylsilane is preferably a methoxy group, ethoxy group, propoxy group, etc. having 1 to 3 carbon atoms. In addition, the alkyl group in the trialkoxyalkylsilane is preferably a hexyl group, octyl group, decyl group, octadecyl group, etc. having 6 to 18 carbon atoms. Such trialkoxyalkylsilanes include, for example, trimethoxyhexylsilane, trimethoxyoctylsilane, trimethoxydecylsilane, trimethoxyoctadecylsilane, triethoxyhexylsilane, triethoxyoctylsilane (triethoxyoctanoylsilane), triethoxydecylsilane, triethoxyoctadecylsilane, etc.

[0038] The surface treatment amount is preferably 0.5 to 30% by mass, more preferably 1 to 20% by mass, based on the powder.

[0039] The component (c) used in the present invention can use one of metal oxide and plate-like powder or two or more of them in combination, but from the viewpoint of the emulsification stability of component (a) in the oil phase, it is preferred to use two of them in combination, and it is more preferred to use a metal oxide and a plate-like powder in combination. When the metal oxide and the plate-like powder are used in combination, the mixing ratio of the two is not particularly limited, for example, metal oxide: plate-like powder = 1:0.1 to 10 (mass ratio). A particularly preferred combination is zinc oxide that can be surface treated and sericite that can be surface treated, which is surface treated zinc oxide and surface treated sericite. When two of them are used in combination, a composite substance such as titanium dioxide coated mica, titanium dioxide coated synthetic phlogopite, titanium dioxide coated bismuth oxychloride, iron oxide mica titanium, titanium dioxide coated glass powder, etc. can be used.

[0040] The content of component (c) in the present invention is not particularly limited, but is preferably 1 to 30% in the emulsified cosmetic, particularly preferably 5 to 20%. Within this range, a preparation having excellent water resistance, friction resistance and stability can be provided.

[0041] In the present invention, it is preferred to further include component (d) inulin fatty acid ester (hereinafter, also referred to as component (d)). By including inulin fatty acid ester, the adhesion to the skin is improved, thereby further improving water resistance, friction resistance, usability (especially no sticky feeling) and formulation stability. Component (d) can be formulated in any phase of the water phase and the oil phase, and is particularly preferably formulated in the oil phase. By formulating in the oil layer, water resistance, friction resistance, usability (especially no sticky feeling) and formulation stability are further improved due to the thickening effect of the oil phase.

[0042] Inulin fatty acid ester, component (d) used in the present invention, is an ester compound of a linear or branched saturated or unsaturated fatty acid having 8 to 32 carbon atoms and inulin, and is contained in the oil phase. There is no particular limitation on inulin, as long as it is inulin that is usually formulated in cosmetics. Inulin is preferably a substance containing a chain of β-1, 2-linked furanose units, a structure having α-D-glucose linked to sucrose at the reducing end, and about 2 to 60 furanose units. In addition, hydrolyzed inulin can also be used. As component (d), stearoyl inulin is preferred. As commercially available products, Rheopearl ISK2 and Rheopearl ISL2 (both manufactured by Chiba Flour Milling Co., Ltd.) as stearoyl inulin can be listed.

[0043] The content of component (d) in the present invention is not particularly limited, but is preferably 0.1 to 10% in the emulsified cosmetic, and particularly preferably 1 to 5%. Within this range, the dispersibility of (a) in the oil phase is improved, and when a powder (e.g., component (c)) is added, the dispersibility of the powder is improved, and a preparation having excellent water resistance, friction resistance, and stability can be provided.

[0044] In the present invention, it is preferred to further include component (e) benzalmalonate polysiloxane. It is known that the component (e) benzalmalonate polysiloxane used in the present invention is represented by the INCI (INTERNATIONAL NOMENCLATURE of COSMETIC INGREDIENTS) name of polysilicone-15, which is a silicone derivative in which about 7.5% of dimethyl polysiloxane with a chain length of about 60 is substituted by two substituents. It has a high UV protection ability by itself, and improves the values ​​of SPA and PA (booster effect) through synergistic effects with other UV inhibitors. In the present invention, component (e) is preferably contained in the oil phase, and also functions as a component that improves the water resistance and friction resistance of the coating film, and contributes to the stability of the cosmetics. As a commercially available product, PARSOL SLX (manufactured by DSM Nutritional Products) can be exemplified.

[0045] The content of component (e) in the present invention is not particularly limited, but is preferably 0.1 to 10% in the emulsified cosmetic, and particularly preferably 1 to 5%. Within this range, not only a high UV protection effect can be obtained, but also the stability of the preparation is good, which is preferred.

[0046] The emulsified cosmetic of the present invention may contain, in addition to the above-mentioned ingredients, ingredients used in conventional cosmetics as appropriate within a range not impairing the effects of the present invention, for example, oily ingredients other than ingredient (e), ultraviolet absorbers, surfactants such as cationic surfactants, nonionic surfactants, anionic surfactants, and amphoteric surfactants, water, water-soluble polymers other than ingredient (a) and ingredient (b), aqueous ingredients such as polyols and lower alcohols, antibacterial agents, preservatives, pH adjusters, cooling agents, powders other than ingredient (c), beauty ingredients such as vitamins and amino acids, and fragrances.

[0047] The emulsified cosmetics of the present invention can be implemented in various forms such as liquid, emulsion, cream, solid, gel, paste, etc. In addition, there is no particular limitation on the dosage form of the cosmetics of the present invention, such as oil-in-water emulsion system, water-in-oil emulsion system, etc., but from the perspective of moisturizing usability and the requirement to improve water resistance in water-in-oil emulsions with lower water resistance, water-in-oil emulsion system is preferred. That is, a preferred embodiment of the present invention is water-in-oil emulsion cosmetics. It can be implemented in the form of various cosmetics such as skin care cosmetics such as emulsion, cream, beauty essence, lip balm, sunscreen, foundation, base, blush, eye shadow, lipstick, lip gloss, and color cosmetics such as conditioner, hair cream, hair dressing, and scalp or hair cosmetics.

[0048] In addition, one embodiment of the present invention is an emulsified sunscreen cosmetic. In addition, another embodiment of the present invention further includes a UV absorber. By improving the water resistance and friction resistance of the cosmetic coating, a UV absorber can be made that is not easily removed by sweat or water and has a high UV protection ability. The UV absorber can be used without particular limitation as long as it is a UV absorber commonly used in sunscreen cosmetics. Examples of UV absorbers include ethylhexyl methoxycinnamate, 2-[4-(diethylamino)-2-hydroxybenzoyl] benzoic acid hexyl ester, ethyl para-aminobenzoate, benzophenone-1, benzophenone-3, benzophenone-6, benzophenone-9, 2,4,6-tris[4-(2-ethylhexyloxycarbonyl)anilino]-1,3,5-triazine, dioctylbutyramide triazone, 4-tert-butyl 4-(2-ethyl-hexyloxy)-2-hydroxy]-phenyl}-6-(4-methoxyphenyl)-(1,3,5)-triazine, 2,2'-methylenebis[6-(2H-benzotriazol-2-yl)-4-(1,1,3,3-tetramethylbutyl)phenol], polysiloxane-15, etc., one or more of them can be used. Among them, ethylhexyl methoxycinnamate, hexyl 2-[4-(diethylamino)-2-hydroxybenzoyl]benzoate, 4-tert-butyl-4'-methoxy-dibenzoylmethane, 2,4-bis{[4-(2-ethyl-hexyloxy)-2-hydroxy]-phenyl}-6-(4-methoxyphenyl)-(1,3,5)-triazine, and polysilicone-15 are preferred, and ethylhexyl methoxycinnamate, hexyl 2-[4-(diethylamino)-2-hydroxybenzoyl]benzoate, and 2,4-bis{[4-(2-ethyl-hexyloxy)-2-hydroxy]-phenyl}-6-(4-methoxyphenyl)-(1,3,5)-triazine are more preferred. The content of the ultraviolet absorber in the emulsified cosmetic is, for example, 1 to 10%.

[0049] The emulsified cosmetic of the present invention may be used by hand, finger, or cotton, by impregnating nonwoven fabric or the like, or by using it as a spray or aerosol.

[0050] The present invention also provides a method for producing an emulsified cosmetic, wherein the emulsified cosmetic contains an oil phase and an aqueous phase, wherein the oil phase contains (a) a water-soluble cationic polymer, and the aqueous phase contains (b) a water-soluble anionic polymer. Regarding the emulsification method, reference may be made to methods known in the art as appropriate.

[0051] Example

[0052] Hereinafter, the present invention will be described in more detail with reference to Examples, Test Examples, etc. However, the present invention is not limited to these Examples, etc.

[0053] [Example 1 (Inventive Products 1 to 14) and Comparative Examples 1 to 4: Emulsified Cosmetics]

[0054] Emulsified cosmetics were prepared by the composition shown in Table 1 and the following production method. The water resistance, friction resistance and functional evaluation of the obtained emulsified cosmetics were evaluated by the following methods, and the results are collectively shown in Tables 1 to 3.

[0055] [Table 1]

[0056]

[0057] (Note 1) SIMULGEL EG (manufactured by SEPPIC) (sodium acrylate / sodium acryloyldimethyl taurate copolymer 37.5% mixture. The content in the formula indicates the content of the pure compound)

[0058] (Note 2) PEMULENE TR-1 (manufactured by Lubrizol Advanced Materials Inc.)

[0059] (Note 3) ACULYN 22 (manufactured by ROHM GMBH) (30% aqueous solution of alkyl acrylate / alkyl methacrylate / polyoxyethylene stearyl ether of methacrylate (20 E.O.) copolymer. The content in the formula indicates the content of the pure compound)

[0060] (Note 4) CARBOPOL 980 (manufactured by Lubrizol Advanced Materials Inc.)

[0061] (Note 5) MERQUAT 740 POLYMER (manufactured by Lubrizol Japan, dimethyldiallylammonium chloride / acrylamide copolymer, 43% aqueous solution. The content in the formula indicates the amount of pure compound)

[0062] (Note 6) Rheopearl ISK2 (manufactured by Chiba Flour Milling Co., Ltd.)

[0063] (Note 7) TINOSORB S (manufactured by BASF)

[0064] (Note 8) Uvinul A PLUS GRANULAR (manufactured by BASF)

[0065] (Note 9) PARSOL SLX (manufactured by DSM Nutritional Products)

[0066] (Note 10) NIKKOL HCO-40 (manufactured by Nippon Surfactant Industries)

[0067] (Note 11) Catinal HC-100 (manufactured by Toho Chemical Co., Ltd.)

[0068] (Note 12) JAGUAR C-14S(C) (manufactured by SOLVAY)

[0069] [Table 2]

[0070]

[0071] [Table 3]

[0072]

[0073] (Manufacturing method)

[0074] A: Components 1 to 3 were uniformly dispersed at 70°C.

[0075] B: Components 10 to 15 were uniformly dissolved at 70°C.

[0076] C: Components 16 to 22 are mixed and dispersed.

[0077] D: Add C into B and disperse evenly.

[0078] E: Add D to A and emulsify at 70°C.

[0079] F: Cool E to room temperature.

[0080] G: Components 4 to 9 are mixed with F to obtain an oil-in-water emulsified cosmetic.

[0081] (Evaluation method: (a) Water resistance evaluation)

[0082] The above samples were concentrated at 2 mg / cm 2After coating on a PMMA plate (manufactured by Labsphere, HELIOPLATE HD6), the sample was allowed to stand for 20 minutes to obtain a sample, and the sample was subjected to SPF measurement using an SPF analyzer (UV-2000S manufactured by Labsphere) to measure the SPF value before the water bath. Next, a water bath was performed. The water bath conditions were to attach the sample to the side of a container storing 35°C, 2L of water, and to stir the water in the container at 300rpm using a paddle stirrer for 5 minutes. After the water bath, after standing and drying for 20 minutes, the SPF value after the water bath was measured using the above-mentioned SPF analyzer. Based on the SPF values ​​before and after the water bath, water resistance was evaluated and determined in 4 grades according to the following (a) evaluation criteria.

[0083] (a) 4-level evaluation criteria

[0084] (Evaluation): (Judgment)

[0085] (SPF value after bathing) / (SPF value before bathing) = 0.7 or more: ◎

[0086] (SPF measured value after bathing) / (SPF measured value before bathing) = 0.5 or more: ○

[0087] (SPF value after bathing) / (SPF value before bathing) = 0.3 or more: △

[0088] (SPF measured value after bathing) / (SPF measured value before bathing)=less than 0.3: ×.

[0089] (Evaluation method: (b) Friction resistance evaluation)

[0090] The above samples were subjected to 2 mg / cm 2 The sample obtained by coating on a PMMA plate and letting it stand for 20 minutes was subjected to SPF measurement using an SPF analyzer (UV-2000S manufactured by Labsphere) to determine the SPF value before friction. Then, friction was applied under the conditions of using a texture analyzer TA.XT PLUS (manufactured by Eikon Seiki Co., Ltd.), fixing the towel cloth at the front end of the fixture, and applying a certain load to make it reciprocate left and right five times. After the friction was completed, the SPF value after friction was measured using the above-mentioned SPF analyzer. Based on the SPF values ​​before and after friction obtained, the friction resistance was evaluated and judged in 4 levels according to the following (b) evaluation criteria.

[0091] (b) Four-level evaluation criteria

[0092] (Evaluation): (Judgment)

[0093] (SPF measured value after friction) / (SPF measured value before friction) = 0.7 or more: ◎

[0094] (SPF measured value after friction) / (SPF measured value before friction) = 0.5 or more: ○

[0095] (SPF measured value after friction) / (SPF measured value before friction) = 0.3 or more: △

[0096] (SPF measured value after friction) / (SPF measured value before friction)=less than 0.3: ×.

[0097] (Evaluation method: (c) No stickiness)

[0098] Twenty professional evaluation panelists applied each of the above samples on their forearms and evaluated and judged the stickiness during use on a 4-level basis according to the following evaluation criteria (c).

[0099] (c) 4-level evaluation criteria

[0100] (Evaluation): (Judgment)

[0101] No stickiness at all: 4 points

[0102] Almost no stickiness: 3 points

[0103] Sticky feeling: 2 points

[0104] Very sticky feeling: 1 point

[0105] According to the above evaluation criteria, the evaluation scores were averaged and judged based on the following judgment criteria.

[0106] <Judgment criteria>:

[0107] [Average score]: [Judgment]

[0108] 3.25 and above: ◎

[0109] 2.5 or more and less than 3.25: ○

[0110] 1.75 or more and less than 2.5: △

[0111] Less than 1.75: ×.

[0112] (Evaluation method: (d) No sticky feeling)

[0113] Twenty professional evaluation panelists applied each of the above samples on their forearms and evaluated and judged the slimy feeling during use on a 4-level basis according to the following evaluation criteria (d).

[0114] (d) 4-level evaluation criteria

[0115] (Evaluation): (Judgment)

[0116] No sticky feeling at all: 4 points

[0117] Almost no sticky feeling: 3 points

[0118] Slippery feeling: 2 points

[0119] Very sticky feeling: 1 point

[0120] According to the above evaluation criteria, the evaluation scores were averaged and judged based on the following judgment criteria.

[0121] <Judgment criteria>:

[0122] [Average score]: [Judgment]

[0123] 3.25 and above: ◎

[0124] 2.5 or more and less than 3.25: ○

[0125] 1.75 or more and less than 2.5: △

[0126] Less than 1.75: ×.

[0127] (Evaluation method: (e) Moisture)

[0128] Twenty professional evaluation panelists applied each of the above samples on their forearms and evaluated and judged the moist feeling during use on a 4-level basis according to the following evaluation criteria (e).

[0129] (e) 4-level evaluation criteria

[0130] (Evaluation): (Judgment)

[0131] Very moist feeling: 4 points

[0132] Slightly moisturizing: 3 points

[0133] Basically no moist feeling: 2 points

[0134] No moist feeling at all: 1 point

[0135] According to the above evaluation criteria, the evaluation scores were averaged and judged based on the following judgment criteria.

[0136] <Judgment criteria>:

[0137] [Average score]: [Judgment]

[0138] 3.25 and above: ◎

[0139] 2.5 or more and less than 3.25: ○

[0140] 1.75 or more and less than 2.5: △

[0141] Less than 1.75: ×.

[0142] (Evaluation method: (f) Preparation stability)

[0143] Each of the above samples was placed in a standard glass bottle and stored in a thermostatic chamber at 50° C. for 1 month. The state after 1 month was observed and judged using the following (f) 4-level judgment standard.

[0144] (f) 4 Level Judgment Criteria

[0145] (Evaluation): (Judgment)

[0146] The appearance is completely unchanged:◎

[0147] Almost no change in appearance: ○

[0148] Some separation and agglomeration can be seen:

[0149] Separation and agglomeration can be seen: ×.

[0150] As is clear from the results in Tables 1 to 3, the emulsified cosmetics of the present invention products 1 to 14 are excellent emulsified cosmetics that have high water resistance and friction resistance by blending a water-soluble anionic polymer and a water-soluble cationic polymer in different phases, have a moist feeling when used, and do not have a sticky or slimy feeling on the skin. In addition, the emulsified cosmetics of the present invention products 1 to 14 are also excellent in formulation stability. In addition, the present invention products 7 to 10 are formulations obtained by changing the mass ratio (a) / (b) of the components (a) and (b) from the present invention product 1, and the present invention product 11 is a formulation obtained by changing the blending amount of the components (a) and (b) from the present invention product 1. On the other hand, the results of Comparative Examples 1, 2, and 3, in which the components (a) and (b) are not blended, are that there is no water resistance and friction resistance, and there is a sticky and slimy touch. In Comparative Example 4 in which a water-soluble anionic polymer was blended in the oil phase and a water-soluble cationic polymer was blended in the water phase, the water-soluble cationic polymer and the water-soluble anionic polymer formed aggregates in the preparation, and the stability of the preparation was poor.

[0151] Example 2: Cream (oil-in-water type)

[0152]

[0153]

[0154] (Note 13) MERQUAT 550PR (manufactured by Lubrizol Japan, dimethyldiallylammonium chloride / acrylamide copolymer, 9% aqueous solution. The content in the formula represents the amount of pure compound.)

[0155] (Manufacturing method)

[0156] A: Components (1) to (3) and (17) are heated to 70°C and uniformly mixed.

[0157] B: Components (4) to (16) are heated to 80°C and mixed uniformly.

[0158] C: Add B to A and stir.

[0159] D: Components (18) to (28) heated to 70°C are added to C and emulsified.

[0160] E: D was cooled to room temperature while being stirred to obtain a cream.

[0161] The cream of Example 2 is a cosmetic product that is excellent in water resistance and friction resistance, has an excellent feeling during use, can fully exert the UV protection function of the UV absorber and UV scatterer, and has excellent emulsification stability.

[0162] Example 3: Shake-type sunscreen (water-in-oil type)

[0163]

[0164]

[0165] (Note 14) KF-96-10CS (manufactured by Shin-Etsu Chemical Co., Ltd.)

[0166] A sunscreen (shake type) was prepared by the following production method.

[0167] (Manufacturing method)

[0168] A: Components (1) to (8) are heated to 80°C and mixed uniformly.

[0169] B: Components (9) to (15) were uniformly mixed using a roller.

[0170] C: Add B into A and mix well.

[0171] D: Add ingredients (16) to (18) to C and mix well.

[0172] E: Add (19) to (22) to D and emulsify.

[0173] F: By cooling E to room temperature, a shake-type sunscreen (water-in-oil type) is obtained.

[0174] The sunscreen of Example 3 (shaken well) is a cosmetic product that has excellent water resistance and friction resistance, excellent feeling during use, can fully exert the UV protection function of the UV absorber and UV scatterer, and has excellent emulsification stability.

[0175] Example 4: Sunscreen (cream) (water-in-oil type)

[0176]

[0177]

[0178] (Note 15) KF-6028P (manufactured by Shin-Etsu Chemical Co., Ltd.)

[0179] (Note 16) TOSPEARL 3000A (manufactured by Momentive Performance Materials Japan)

[0180] The sunscreen (cream) was prepared by the following production method.

[0181] (Manufacturing method)

[0182] A: Components (1) to (6) are uniformly mixed using a roller.

[0183] B: Components (7) to (19) are heated to 80°C and mixed uniformly.

[0184] C: Add B into A and mix well.

[0185] D: Add ingredients (20) to (26) and mix well.

[0186] E: Add D to C and emulsify.

[0187] F: Return E to room temperature to obtain a sunscreen (cream).

[0188] The sunscreen (cream) of Example 4 is a cosmetic product that is excellent in water resistance and friction resistance, has an excellent feeling during use, can fully exert the UV protection function of the UV absorber and the UV scatterer, and has excellent emulsification stability.

[0189] Example 5: Cosmetic base (water-in-oil type)

[0190]

[0191]

[0192] (Note 17) KP-578P (manufactured by Shin-Etsu Chemical Co., Ltd.)

[0193] (Note 18) Catinal HC-200 (manufactured by Toho Chemical Co., Ltd.)

[0194] The cosmetic base was prepared by the following production method.

[0195] (Manufacturing method)

[0196] A: Components (1) to (7) are uniformly mixed using a roller.

[0197] B: Components (8) to (18) are heated to 80°C and mixed uniformly.

[0198] C: Add B into A and mix well.

[0199] D: Add ingredients (18) to (26) and mix well.

[0200] E: Add D to C and emulsify.

[0201] F: Return E to room temperature to obtain a makeup base.

[0202] The cosmetic base of Example 5 is a cosmetic having excellent water resistance and friction resistance, excellent feeling during use, capable of fully utilizing the UV protection function of the UV absorber and UV scatterer, and excellent emulsification stability.

[0203] Example 6: Aerosol sunscreen (oil-in-water type)

[0204]

[0205]

[0206] (Note 19) Unifilma HVY (manufactured by Chiba Flour Milling Co., Ltd.)

[0207] (Note 29) Catinal LC-100 (manufactured by Toho Chemical Co., Ltd.)

[0208] The aerosol sunscreen was prepared by the following production method.

[0209] (Manufacturing method)

[0210] A: Components (1) to (6) were dispersed using three rolls.

[0211] B: Components (7) to (17) were uniformly dissolved at 70°C.

[0212] C: Add B into A and mix well.

[0213] D: Add (18) to (23) to C and emulsify.

[0214] E: An aluminum pressure-resistant container was filled with 6 g of the stock solution obtained in D, and the valve was fixed. The pressure-resistant container was then filled with a propellant (LPG 0.15: 14 g) through the valve to obtain an aerosol-type sunscreen.

[0215] The aerosol sunscreen preparation of Example 6 is a cosmetic product that has excellent water resistance and friction resistance, excellent feeling during use, can fully exert the UV protection function of the UV absorber and the UV scatterer, and has excellent emulsification stability.

[0216] Example 7: Hair cosmetics (oil-in-water type)

[0217]

[0218]

[0219] (Note 21) KF-96-6CS (manufactured by Shin-Etsu Chemical Co., Ltd.)

[0220] The hair cosmetics were prepared by the following production method.

[0221] (Manufacturing method)

[0222] A: Mix ingredients (1) to (5) uniformly.

[0223] B: Components (6) to (13) are uniformly dissolved.

[0224] C: Add B to A and emulsify.

[0225] D: Add (14) to (15) into C and mix.

[0226] E: Add (16) to (20) to D and mix.

[0227] F: E is filled into a dispenser container to obtain a hair cosmetic.

[0228] The hair cosmetic of Example 7 is a cosmetic having excellent water resistance and friction resistance, a good touch, and excellent emulsion stability.

[0229] As described in detail above, by including a water-soluble cationic polymer in the oil phase and a water-soluble anionic polymer in the water phase, an emulsified cosmetic having improved water resistance and abrasion resistance of the coating film and good feel during use can be provided.

[0230] This application is based on Japanese Patent Application No. 2018-206251 filed on November 1, 2018, the disclosure of which is incorporated herein by reference in its entirety.

Claims

1. An emulsified cosmetic comprising an oil phase and an aqueous phase, wherein the oil phase comprises (a) a water-soluble cationic polymer, and the aqueous phase comprises (b) a water-soluble anionic polymer, (a) the water-soluble cationic polymer is dimethyldiallylammonium chloride / acrylamide copolymer, and Acrylic acid / alkyl methacrylate copolymer and sodium acrylate / sodium acryloyldimethyl taurate copolymer are used as (b) water-soluble anionic polymers.

2. The emulsified cosmetic according to claim 1, wherein The emulsified cosmetic contains (c) at least one of a metal oxide or a plate-like powder.

3. The emulsified cosmetic according to claim 1 or 2, wherein: The emulsified cosmetic contains (d) inulin fatty acid ester.

4. The emulsified cosmetic according to claim 1 or 2, wherein: The content mass ratio (a) / (b) of the (a) water-soluble cationic polymer to the (b) water-soluble anionic polymer is 0.05 to 20.

5. The emulsified cosmetic according to claim 1 or 2, wherein: The emulsified cosmetic is an oil-in-water emulsified cosmetic.

6. The emulsified cosmetic according to claim 1 or 2, wherein: The emulsified cosmetic contains (e) benzalmalonate polysiloxane.

7. A method for producing an emulsified cosmetic, wherein: The emulsified cosmetic comprises an oil phase and a water phase, wherein the oil phase comprises (a) a water-soluble cationic polymer, and the water phase comprises (b) a water-soluble anionic polymer. (a) the water-soluble cationic polymer is dimethyldiallylammonium chloride / acrylamide copolymer, and Acrylic acid / alkyl methacrylate copolymer and sodium acrylate / sodium acryloyldimethyl taurate copolymer are used as (b) water-soluble anionic polymers.