Improved transfer for RF applications
By adding a dummy metal layer to the GaN chiplet and adjusting the stress of the packaging layer, the bending problem caused by mechanical stress during the micro-transfer printing process of the GaN chiplet in high-power RF applications is solved, improving the release and printing yield and ensuring Improves the reliability of high-frequency applications.
Patent Information
- Application Number
- CN202110222643.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-02-26
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-02-26
AI Technical Summary
In high-power RF applications, the mechanical stress causes a large amount of bending during the micro-transfer printing of GaN chiplets. Thin GaN chiplets make micro-transfer printing more difficult. It is difficult for existing technology to effectively solve this problem, resulting in low release. and print yield.
By adding a dummy metal layer on the GaN chiplet to provide mechanical strength, using a thicker encapsulation layer during the micro-transfer printing process to compensate for mechanical stress, and adjusting the stress type and frequency of the deposited layer to mitigate curvature, ensuring the mechanical stability of the chiplet. properties and transfer success rate.
Significantly improves the release and printing yield of GaN chiplets, reduces the risk of defects and cracks during micro-transfer printing, and ensures reliability and performance for high-frequency applications.
Smart Images

Figure CN113327977B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to semiconductor structures for radio frequency (RF) applications, and in particular to semiconductor structures comprising micro-transfer printed gallium nitride (GaN) chiplets on a target substrate. Background Art
[0002] GaN is a relatively new technology compared to other semiconductors, such as silicon (Si) and gallium arsenide (GaAs), but it has become the technology of choice for RF, power-hungry applications, such as those required to transmit signals over long distances or at high-end power levels. GaN transistors offer high power density, high operating temperature, improved efficiency, low on-resistance, and they can operate in different frequency bands ranging from 20kHz to 300GHz.
[0003] Figure 1 A schematic diagram of a cross section of a GaN transistor 2 is shown. A GaN layer 4 is formed on a high resistivity (HR) silicon substrate 6 and an aluminum gallium nitride (AlGaN) buffer layer 8. The n heavily doped (n++) regions of GaN 10 are connected to metal contacts 12 (drain and source). A gate 14 is isolated from the GaN layer 4 by a thin aluminum nitride (AlN) layer 16.
[0004] Silicon-on-insulator (SOI) technology is used in semiconductor manufacturing, especially microelectronics, to reduce parasitic capacitance by having a layered silicon-insulator-silicon substrate structure instead of bulk Si. SOI complementary metal oxide semiconductor (CMOS) provides lower power consumption for analog and digital RF hybrid circuits in the design of low-power RF transceivers due to its low leakage capability.
[0005] To realize some of the advantages of both GaN and SOI in high-power applications, attempts have been made to grow GaN on SOI using trench etching to isolate GaN transistors. Careful strain engineering is required to control the stress accumulated in the wafer during growth.
[0006] Alternatively, GaN devices can be transferred from a homogeneous / source wafer to a target SOI wafer using microtransfer printing (μTP) [1]. In this process, the GaN device is detached / lifted from the homogeneous substrate on which it was grown and reattached to the SOI substrate. A chiplet is a (small) piece of chip from which the homogeneous substrate has been removed.
[0007] [1] R. Lerner et al., “Heterogeneous Integration of Microscale Gallium Nitride Transistors by Micro-Transfer-Printing,” 2016 IEEE 66th Annual Conference on Electronic Components and Technologies, pp. 1186–1189. Summary of the invention
[0008] Aspects of the present invention provide a semiconductor structure for RF applications and a method of forming such a semiconductor structure as set out in the accompanying claims.
[0009] Preferred embodiments of the present invention will now be described, by way of example only, with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 is a schematic cross-sectional view of a GaN transistor on a silicon substrate;
[0011] Figure 2 shows a cross-sectional sequence of a GaN transistor on a silicon substrate illustrating the release process during microtransfer printing;
[0012] Figure 3 is a schematic cross-sectional view of a GaN chiplet that is flexed due to mechanical stress;
[0013] Figure 4a is a schematic top view of a GaN chiplet without a dummy metal layer;
[0014] Figure 4b is a schematic top view of a GaN chiplet with a dummy metal layer;
[0015] Figure 5a is a schematic top view of a second GaN chiplet without a dummy metal layer;
[0016] Figure 5b is a schematic top view of a second GaN chiplet having a dummy metal layer;
[0017] Figure 6 is a schematic cross-sectional view of a semiconductor structure including a GaN chiplet micro-transferred on an SOI wafer; and
[0018] Figure 7 is a flow chart illustrating the steps of a method of forming a semiconductor structure for RF applications. DETAILED DESCRIPTION
[0019] Embodiments described herein provide a semiconductor structure for RF applications. For example, the semiconductor structure can be a low noise amplifier (LNA) or a single pole double throw (SPDT) switch. The semiconductor structure includes a target substrate (preferably an SOI wafer or die) and a GaN chiplet micro-transferred on the target substrate, wherein the chiplet includes a GaN device (typically a GaN transistor, such as a pseudomorphic high electron mobility transistor: p-HEMT) and a dummy metal layer. The dummy metal layer increases the mechanical strength of the chiplet, thereby reducing warping and preventing cracking during the micro-transfer process.
[0020] As mentioned above, a chiplet is a (small) piece of chip whose homogeneous substrate has been removed. In semiconductor structures for RF applications, GaN layers and buffer layers need to be thin in order to meet specification standards. However, thin GaN chiplets make microtransfer printing more difficult due to the large amount of bending of the chiplet when it is released from the underlying silicon substrate during transfer to the SOI wafer. μTP GaN chiplets can include buffer layers (e.g., AlGaN) and GaN layers with a combined thickness of less than 3μm. For example, the buffer layer can have a thickness of 1μm, and the top GaN layer can have a thickness of 1.8μm, making the combined thickness only 2.8μm. This can be much thinner than the thickness of GaN semiconductor structures for high-power applications, which are suitable for existing microtransfer printing technology, where the individual GaN layers typically have a thickness of 5μm.
[0021] The dummy metal layer may have a thickness in the range of 0.3 μm to 4 μm, and preferably a thickness of 1.25 μm, which may provide sufficient mechanical strength. For dummy metal layers having a thickness in the range of 1 μm to 2 μm, advantageous properties in terms of the mechanical strength of the chiplet have been found. "Dummy" herein refers to the fact that the dummy metal layer is not used to form any electrical connection and does not (significantly) affect the final device performance. GaN devices generally include a device metal layer for electrically connecting to the GaN device (i.e., for electrically connecting to the doped region in the GaN layer), and the dummy metal layer does not contact the device metal layer. It may be advantageous to form both the dummy metal layer and the device metal layer in the top metal layer stacked at the back end of the GaN device, and to separate them when patterning the top metal layer. For example, the gap between the dummy metal layer and the device metal layer may have a width of at least 10 μm to avoid capacitive effects that may negatively affect device performance. For devices operating at frequencies below 5 GHz, smaller gaps may be used, while for high frequency applications (e.g., >20 GHz), a gap of at least 30 μm may be preferred. For GaN transistors, the device metal layers include metal contacts, such as source, drain, and gate contacts.
[0022] The dummy metal layer and the device metal layer can be arranged so that the metal is substantially uniformly distributed on the μTP GaN chiplet. Uniformly distributing the metal on the GaN chiplet can improve the mechanical properties of the chiplet and further reduce the occurrence of defects during microtransfer. To this end, the dummy metal layer can also be arranged substantially symmetrically on the μTP GaN chiplet. The dummy metal layer and / or the device metal layer can have x and / or y symmetry. In order to increase the mechanical strength of the GaN chiplet, it can be advantageous to cover a majority of the surface area of the chiplet with metal. The dummy metal layer and the device metal layer can together cover 20% to 90% of the total surface area of the μTP GaN chiplet.
[0023] The SOI wafer can be a thin SOI wafer of 200 mm (8 inches), which is suitable for semiconductor structures for RF applications. Micro-transfer printing of GaN on SOI wafer can achieve a monolithic design with shorter interconnects, which can prevent losses and transitions between the chip and the substrate. When micro-transfer printing is performed, one or more small chips (each containing one or more GaN devices) can be lifted from a homogeneous silicon substrate and placed on the SOI wafer. The SOI wafer can include a passivation layer on top, to which the GaN small chip can be attached. The μTP GaN small chip can be attached to the SOI wafer by a glue layer.
[0024] Also described herein are embodiments of a method of forming a semiconductor structure for RF applications. The method includes providing a GaN chiplet including one or more GaN devices and a dummy metal layer, and micro-transferring the GaN chiplet onto an SOI wafer.
[0025] The providing step may include depositing a metal layer (typically a top metal layer) and patterning the metal layer to form a dummy metal layer and to form a device metal layer including metal contacts for electrical connection to the GaN device.
[0026] Figure 2 Some of the steps in releasing a GaN chiplet from a homogeneous silicon substrate are shown. The passivation and dielectric layers of the back-end stack of the GaN device are etched to expose the underlying GaN layers around the chiplet. A GaN etch is then performed to isolate the GaN chiplet, followed by deposition of an encapsulation layer (e.g., SiN) to protect the chiplet. The encapsulation layer is etched to expose the top metal of the GaN chiplet to form a connection to the SOI wafer after transfer. Another GaN etch is performed around the chiplet to expose the underlying silicon substrate, followed by release of the chiplet by etching the silicon substrate beneath the GaN chiplet. After release, the GaN chiplet can be transferred and glued to an SOI wafer (not shown).
[0027] In the embodiments described herein, in addition to the dummy metal layer, the thickness of the encapsulation layer can also be used to compensate for the mechanical stress of the GaN chiplet. For example, a thicker encapsulation layer can be used in the μTP process to provide more support for the chiplet. For example, the encapsulation layer with increased thickness can have a thickness in the range of 0.5μm to 3μm. The exact thickness depends on the type of stress in the deposited encapsulation layer and the type of stress within the GaN chiplet. In addition, the deposition frequency of the encapsulation layer (i.e., the frequency of the RF generator used to excite the plasma in the deposition tool) can be changed to correct the curvature of the chiplet. For example, using plasma enhanced chemical vapor deposition (PECVD) or similar tools, the frequency of the RF generator can change the stress of the deposited layer.
[0028] Figure 3 A cross section of a thin GaN chiplet 18 released from its homogeneous silicon wafer 20 is shown. To relieve mechanical stress, the chiplet 18 is bent into a cantilever with an end displacement / deflection 22 (δ). Stoney's formula can be used to estimate the end displacement (δ) of the cantilever for a given stress (σ):
[0029]
[0030] , where δ is the tip deflection of the cantilever (in this case, the chiplet), σ is the applied stress, v is Poisson's ratio, E is Young's modulus, L is the length, and t is the thickness of the cantilever.
[0031] Using Equation 1, for no dummy metal layer and σ = 10 7 For an RF GaN chiplet (with a GaN layer thickness of 1.8 μm) with a thickness of 1.25 μm, δ = 3.83 μm. The deflection is relatively large compared to a high-power GaN chiplet (with a GaN layer thickness of 5 μm) (δ = 0.5 μm under the same applied stress). Therefore, using existing micro-transfer printing technology suitable for high-power GaN, if applied directly to thinner RF GaN chiplets, cracking may occur, resulting in very low release and printing yield. However, an RF GaN chiplet (with a GaN layer thickness of 1.8 μm) including a dummy metal layer with a thickness of 1.25 μm has δ = 0.54 μm (for σ = 10 7 Pa), which is closer to the delta value of high-power GaN chiplets. Therefore, the use of dummy metal layers can significantly improve the release and printing yield of GaN chiplets for RF applications.
[0032] Figure 4aA schematic top view of a GaN chiplet 24 is shown, which includes one or more GaN devices (not shown), such as one or more of transistors, resistors, and transmission lines. The chiplet 24 includes a device metal layer 26, which is a transistor top metal layer used to connect to the GaN devices (e.g., source, drain, and gate connections).
[0033] Figure 4b A schematic top view of a corresponding GaN chiplet 24 is shown, which includes the same GaN device and device metal layer 26, and also includes a dummy metal layer 28 arranged substantially symmetrically on the chiplet 24. For ease of understanding, similar or corresponding features are given the same reference numerals, and these reference numerals are not intended to be limiting. The metal on the chiplet (including the dummy metal and the device metal) is evenly distributed across the entire surface of the chiplet 24 (with the dummy metal and the device metal being uniformly distributed across the entire surface of the chiplet 24). Figure 4a Different from the small chips in Figure 4a 2, the metal is concentrated in the center of the chiplet). The device metal layer 26 covers 4.3% of the surface area of the chiplet 24, and the dummy metal layer 28 covers 44.4% of the surface area of the chiplet, so that a total of 48.7% of the surface area of the chiplet is covered by metal (i.e., a total chiplet density of 48.7%). Without the dummy metal layer 28, the GaN device cannot generally be successfully microtransferred.
[0034] Figure 5a A schematic top view of a GaN chiplet 24 is shown, which includes various GaN devices (not shown) and a device metal layer 26 for connecting to the GaN devices 26 .
[0035] Figure 5b A schematic top view of a corresponding GaN chiplet 24 is shown, which includes the same GaN device and device metal layer 26, and also includes a dummy metal layer 28. The dummy metal layer 28 has a substantially mirror symmetry on the y-axis. The dummy metal layer 28 is arranged relative to the device metal layer 28 so that there is a gap 30 between them. The gap 30 has a width of at least 30 μm to minimize its effect on the GaN device through capacitive effects (other embodiments may have smaller gaps, but where the width of the gap is at least 10 μm). The device metal layer 26 covers 16.4% of the surface area of the chiplet 24, and the dummy metal layer 28 covers 19.5% of the surface area of the chiplet, so that a total of 35.9% of the surface area of the chiplet is covered by metal (i.e., 35.9% of the total chiplet density).
[0036] Figure 6A cross-sectional schematic diagram of a portion of a semiconductor structure for RF applications 32 is shown. The semiconductor structure includes a μTP GaN chiplet 34 attached to an SOI wafer 36 by a glue layer 38. The GaN chiplet 34 includes a GaN layer 40 on a buffer layer 42, a device metal layer 44, and a dummy metal layer 46. The GaN layer 40 has a thickness of about 1.8 μm, and the buffer layer 42 has a thickness of about 1 μm. The dummy metal layer 46 can have a thickness of 1.25 μm. A passivation layer 48 including one or more dielectric layers covers the top metal of the back end including the dummy metal layer 46. The chiplet 34 is partially enclosed in a protective encapsulation layer 50 formed before release from a homogeneous substrate (not shown). The SOI wafer 36 includes an upper silicon layer 52 (e.g., an epitaxial layer) and a lower silicon layer 54 separated by an insulator layer 56 (typically including an oxide). A passivation layer 58 (e.g., SiON) covers the upper silicon layer 52. The upper silicon layer 52 of the SOI wafer 36 is shown as a single layer, but includes the entire back end (all metal layers), dielectric layers for separation metallization, and silicon layers for creating the active portion of the SOI device. The passivation layer 58 is patterned to expose the top metal layer connection pads 60 (e.g., aluminum pads) in the SOI wafer 36. The GaN chiplets 34 are electrically connected to the SOI wafer 36 via a copper redistribution layer (RDL) 62, which is connected to the device metal layer 44 of the GaN chiplets 34 and the top metal layer connection pads 60 of the SOI wafer 36. Another passivation layer 64 covers the RDL 62, the GaN chiplets 34, and the SOI wafer 36. This passivation layer 64 can eventually be opened to allow connection to other circuits, PCBs, and / or other structures for connection thereto.
[0037] Figure 7 is a flow chart showing the steps of a method for forming a semiconductor structure. The method includes forming a GaN device (e.g., a p-HEMT) on a silicon substrate (e.g., a high-resistivity silicon substrate) (step S1), wherein the step of forming the GaN device includes: depositing a metal layer (step S1a), and patterning the metal layer to form a dummy metal layer and a device metal layer on a GaN chiplet including the GaN device (step S1b). The method also includes: etching and releasing the GaN chiplet from the silicon substrate (step S2); attaching the GaN chiplet to an SOI wafer (step S3); and forming an RDL that electrically connects the GaN device to the SOI wafer (step S4). Typically, the RDL is formed to connect the top metal layer of the GaN device to the top metal layer of the semiconductor device in the SOI wafer. The method also includes providing a passivation layer on the SOI wafer, the RDL, and the GaN chiplet (step S5). Before the GaN chiplet is released from the homogeneous substrate, the method may include depositing a packaging layer to cover the GaN chiplet.
[0038] Although specific embodiments of the present invention have been described above, it should be understood that the present invention may be practiced in a manner other than that described. The above description is intended to be illustrative rather than limiting. It will be apparent to those skilled in the art that modifications may be made to the described invention without departing from the scope of the appended claims.
[0039] Each and every feature disclosed or shown in this specification may be included in the present invention either alone or in any suitable combination with any other features disclosed or shown herein.
Claims
1. A semiconductor structure for RF applications, comprising: target substrate; as well as A micro-transfer printed GaN chiplet on the target substrate, wherein the chiplet comprises: GaN devices; a device metal layer including metal contacts for connecting to the gallium nitride device; and A dummy metal layer not used to form any electrical connection, wherein the dummy metal layer and the device metal layer are composed of metal layers and separated by a gap, wherein the dummy metal layer is arranged to increase the mechanical strength of the micro-transfer-printed gallium nitride chiplet by having a thickness in the range of 0.3 μm to 4 μm and by covering 20% to 90% of the total surface area of the micro-transfer-printed gallium nitride chiplet together with the device metal layer.
2. The semiconductor structure according to claim 1, wherein: The target substrate is a silicon-on-insulator wafer or die.
3. The semiconductor structure according to claim 1, wherein: The micro-transfer gallium nitride chiplet includes a buffer layer and a gallium nitride layer on the buffer layer, and wherein a combined thickness of the buffer layer and the gallium nitride layer is less than 3 μm.
4. The semiconductor structure according to claim 3, wherein: The gallium nitride layer has a thickness of 1.8 μm.
5. The semiconductor structure according to claim 1, wherein: The dummy metal layer is substantially symmetrically arranged on the micro-transfer gallium nitride chiplet.
6. The semiconductor structure according to claim 1, wherein: A gap between the dummy metal layer and the device metal layer has a width of at least 10 μm.
7. The semiconductor structure according to claim 1, wherein: The dummy metal layer and the device metal layer are arranged such that metal is substantially evenly distributed on the micro-transfer gallium nitride chiplet.
8. The semiconductor structure of claim 1, further comprising an encapsulation layer covering the micro-transfer printed gallium nitride chiplet.
9. The semiconductor structure according to claim 8, wherein: The encapsulation layer has a thickness in the range of 0.5 μm to 3 μm.
10. A method of forming a semiconductor structure for RF applications, the method comprising: Provides GaN chiplets, including: GaN devices; a device metal layer including metal contacts for connecting to the gallium nitride device; and a dummy metal layer not used to form any electrical connection, wherein the dummy metal layer and the device metal layer are composed of metal layers and are separated by a gap, wherein the dummy metal layer is arranged to increase the mechanical strength of the gallium nitride chiplet by having a thickness in the range of 0.3 μm to 4 μm and by covering 20% to 90% of the total surface area of the gallium nitride chiplet together with the device metal layer; and The gallium nitride chiplet is micro-transfer printed onto a target substrate.
11. The method according to claim 10, wherein: The providing step includes: depositing a metal layer, and patterning the metal layer to form the dummy metal layer, and forming a device metal layer including metal contacts for connecting to the gallium nitride device.
12. The method according to claim 10, wherein: The micro-transfer printing step includes depositing an encapsulation layer covering the gallium nitride chiplet before the gallium nitride chiplet is released from a homogeneous substrate.
Citation Information
Patent Citations
Vertical Hetero Wide Bandgap Transistor
US20150014706A1
Methods of manufacturing nitride semiconductor devices
US20150187599A1
Method of automatically generating dummy metals for multilevel interconnection
US5798298A