Method for inspecting the coating on the probe surface
Through holographic interferogram data and digital reconstruction technology, the depth expression and properties of the coating are automatically evaluated, which solves the subjectivity and time-consuming problems of coating mechanical resistance evaluation, and achieves rapid and objective coating evaluation.
Patent Information
- Application Number
- CN202080027893.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-04-09
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2040-04-09
AI Technical Summary
The existing technology relies on artificial visual analysis when evaluating the mechanical resistance of coatings, which is subjective and time-consuming. Especially in quality control under high pressure, it is difficult to obtain comparable results quickly and objectively.
By providing sensing data to determine the depth representation of the coating and deriving coating properties based on the depth representation, using holographic interferogram data and digital reconstruction technology, depth histograms and layer profiles are generated to automatically evaluate the geometry and functionality of the coating. .
It achieves the objective properties of the coating in a short time, reduces the reliance on subjective evaluation, improves the evaluation speed and repeatability, and can evaluate the mechanical resistance and structural properties of the coating.
Smart Images

Figure CN113748329B_ABST
Abstract
Description
Field of the Invention
[0001] The present invention relates to a method and an inspection device for inspecting a coating on a probe surface, and further relates to a method and a system for performing an impact test on a coating on a probe surface. Background of the Invention
[0003] Various coatings are used in many technical fields to impart the desired functionality to surfaces, such as the surfaces of individual parts of machines or even the surfaces of entire products. This functionality may be to provide protection for the bulk material below the coating, or may be to impart additional performance to the coated parts. Although protection may be improved to prevent corrosion or chemical influences, additional features may be directional guidance of light, designable reflective properties, improved fluid dynamics behavior, or changes in the blocking or transmission characteristics of certain substances. Commonly used coating types include those that are liquid before contact with the bulk material surface, such as gloss paints or varnishes, and those that have been pre-hardened, such as films or foils, which may again impart additional, typically polymeric coatings. Polymer coatings may be applied in liquid or powder form. Other important coating types include electrically applied coatings and passivating coatings that may be applied electrically or chemically.
[0004] In any case, in order to verify certain property functions of a coating, or more generally, in order to measure characteristics of interest, the provision of appropriate coating inspection and testing devices in development, production and quality control is an obvious prerequisite. Since the results of this inspection and testing are interpreted as defining characteristics of the respective coating or coated product, and since these defining characteristics need to be communicated between production sites and companies, the inspection and testing devices are usually designed to produce results that are as objective and reproducible as possible, and are therefore comparable to each other. The common efforts to achieve this comparability are manifested in the form of public standards, such as those published by the German Institute for Standardization (DIN) and / or the International Organization for Standardization (ISO), or company standards adapted to the specific needs of manufacturers.
[0005] However, in some cases, even test procedures that have been agreed upon in generally accepted standards still rely on manual evaluation of the test results. This is the case, for example, in the DIN EN ISO 20567-1 standard chip drop impact test for evaluating the mechanical resistance of coatings, which is widely used, for example, in the automotive industry. In these tests, a sample of a predetermined type of stone or steel fragment is fired onto a bulk material probe, the surface of which has been provided with a coating of interest, usually a glossy paint or varnish. After firing, the probe is visually analyzed by an expert, and his or her visual impression of the coating that has been damaged to varying degrees by the fragments at different locations is matched with a standardized image of the damaged probe, each image representing a separate resistance grade. However, even the best-trained experts do not always agree on which grade a given test result belongs to. In addition, the more carefully an expert may aim to grade the test results, the more time he or she will spend. However, quality control often needs to be carried out under high time pressure, especially if a large number of probes are to be tested, which is not uncommon. The time pressure is even higher when the quality of certain parts of a machine needs to be evaluated during an ongoing production process. Therefore, a method of inspecting coatings is desired which allows less subjective results to be obtained in a shorter time.
[0006] Some evaluation schemes also rely on the assessment of the severity of a single impact. Among other things, the severity of a single impact is often judged by its apparent color, based on the assumption that a more severe impact will leave a darker and / or larger impact. Of course, this assumption relies on perceptible color differences between the layers. If the layers have the same color, then the severity of a single defect cannot therefore be determined. Therefore, a method of inspecting coatings that allows for the assessment of a single mechanical impact even if the coatings have the same color is also desired.
[0007] The article by Budini et al.: “Applied Optics-Characterization of drying paint coatings by dynamic speckle and holographic interferometry measurements” mentions the dynamic speckle and holographic interferometry techniques for characterizing the drying process of solvent-based paint coatings.
[0008] US 2013 / 0045663A1 relates to an apparatus for optically measuring the thickness of an object, such as a slice of semiconductor material, by interferometry. An optical interferometry reading of the thickness of the object can be taken, a rough thickness value can be obtained, and a frequency indicating how often the rough thickness value occurs can be evaluated.
[0009] US 9,488,470 B1 relates to a method for evaluating the condition of a ceramic coating deposited on a substrate. The method comprises illuminating the ceramic coating with light, measuring the intensity of the light returned from the ceramic coating as a function of the depth in the coating and the lateral position on the coating, and analyzing the measured light intensity to obtain, for example, the intensity of the light returned from the exposed coating surface relative to the intensity of the light returned from the coating.
[0010] Brief description of the invention
[0011] Therefore, an object of the present invention is to provide a method and an apparatus for inspecting a coating of a probe surface objectively and in a relatively short time.
[0012] In a first aspect of the invention, there is provided a method of inspecting a coating on a probe surface, comprising the steps of: a) providing sensed data indicative of the depth of the coating at each of a predetermined subset of probe surface points, b) determining a depth expression of the coating from the sensed data, and c) deriving a property of the coating based on the depth expression.
[0013] Since the sensed data provided indicates the depth of the coating at different points, the sensed data can be used to determine the depth expression of the coating. Since the coating properties are further derived, the properties of the coating itself are obtained, and thus objective characteristics of the coating are obtained that are independent of any subjective evaluation, thus facilitating reproducible evaluation. Since expert intervention is no longer necessary, the speed of the inspection will also be increased, for example by implementing the method on an automated system such as a computer. In addition, since the coating properties, i.e., the objective characteristics of the coating, are derived based on the depth expression of the coating, they carry objective information about the geometric configuration or structure of the coating, which can be used to evaluate the functionality of the coating due to its geometric configuration or structure.
[0014] In the context of the provided method, the probe is understood to have a surface on which a coating can be applied and any material sheet that can maintain the method. In this sense, the probe can be, for example, a part of a product, such as a sheet cut out from a vehicle chassis, or some imaginary substrates that are only present for supporting the coating to be checked. Preferably, the coating is composed of one or more material layers or structures different from the probe, wherein the thickness of the coating is much less than the thickness of the probe. Although the probe surface is preferably understood to be a part of the probe itself, so that the coating forms a separate entity, the probe and the coating can alternatively be understood to form a connected entity with a surface having a non-zero thickness including the coating and the probe surface. The example of the coating includes gloss paint and varnish, preferably including those used in the automotive industry to protect the chassis from scratches caused by stone chip impact or other means, such as car wash brushes, and those used in the furniture industry to improve the resistance of furniture to chemicals or climate effects. However, the coating described herein also includes those used in other fields and for other applications, such as films and foils and the coating of films and foils made of polymers, such as the purpose is to provide the microstructure required for various purposes.
[0015] The sensing data provided according to the method is data collected by any sensing device, which is suitable for collecting data indicating the coating depth at a given point on the probe surface. Preferably, the coating depth at a given probe surface point is the Euclidean distance from a selected reference plane to a point on the coating surface, which is located above a given probe surface point in a direction perpendicular to the probe surface. Wherein, the coating surface is defined as the side of the coating facing away from the probe, that is, forming an interface with the surrounding medium such as air. Similarly, the coating depth at a given probe surface point may preferably be the Euclidean distance from a selected reference plane to a point inside the coating, which is located above a given probe surface point in a direction perpendicular to the probe surface. In this case, the depth is a partial depth. It may correspond to the position of an interface between, for example, coatings. If the reference plane is selected so that it is substantially coincident with the coating surface in a region where the coating is regular, that is, for example, in a region where the coating is not damaged, the depth is a defect depth measuring the degree of deviation of the coating from the plane in a given region. In the case where the deviation originates from the mechanical impact of a ballistic object (such as a fragment used in a standard test procedure), the defect depth may also be referred to as penetration depth. On the other hand, if the reference plane is selected to substantially coincide with the probe surface (which is possible if the probe surface is substantially planar), the depth can be referred to as the full depth or thickness of the coating. By selecting the reference plane, the depth can also be a partial depth, which indicates the Euclidean distance from the probe surface to a specific point in the coating (i.e., inside the coating). The partial depth can also be understood as the height of a specific point above the probe surface. In particular, this point of particular interest can be located at the interface between two coatings. Of course, according to the present invention, other choices for distance measurements defining depth are also possible, particularly including other choices of reference planes. Basically, this choice will only correspond to the choice of coordinates. In principle, any coordinate system can be used. However, the preferred coordinate system is suitable for the geometry of the probe and / or coating surface. For example, the coordinates can be coordinates of a Cartesian coordinate system, in which two axes, i.e., the x-axis and the y-axis, are located in the probe or coating surface, if the surface is a plane. In this case, the third direction of the Cartesian coordinate system, i.e., the z-direction, is used to measure the depth of the coating. In other cases where the probe surface and / or coating surface is not planar, other coordinate systems and / or depth measurements may be preferred, perhaps relative to a reference sphere rather than a plane, and defined using spherical polar coordinates.
[0016] The sensing device may have a limited resolution so that the number of probe surface points providing sensing data may be limited, i.e. they may form a subset of the full set of probe surface points. Preferably, the subset, or at least the number of points contained therein, is predetermined. The sensing device may be an optical device, such as a profilometer, a deflectometry device or even a conventional microscope. However, it is particularly preferred that a holographic device is used to collect the sensing data. An advantage of using holography is that the sensing data not only indicates depth information, but also conveys information about the optical properties of the coating, since the phase information of the light used for sensing is not lost, at least not within a multiple of its wavelength.
[0017] In any case, from the provided sensing data, three-dimensional information about the coating geometry can be obtained, as captured by the step of determining the depth expression. In the particularly simple case where the sensing data may consist of the coating thickness at a subset of the probe surface points, the depth expression may simply be a mapping of the coordinates of the probe surface points to the corresponding thickness value of the coating, i.e., the full depth. In this case, the depth expression may be, for example, a three-dimensional image or a two-dimensional projection of a three-dimensional image. Alternatively, the depth expression may be a two-dimensional map, for example coordinated by the coordinates of the probe surface points, in which additional depth information is encoded in the contour or in the color or grayscale. The depth expression may also be a combination, such as a two-dimensional projection of a three-dimensional image, in which the depth information is additionally encoded in color or grayscale.
[0018] Regardless of its visualization, the information carried by the depth representation is used to derive coating properties, i.e., coating properties related to, for example, its geometrical characteristics, the possible layered structure of the coating or one or more materials it contains. For example, the subjective roughness of the coating surface perceived tactilely or visually can be objectified by choosing the coating properties as a length scale that characterizes the changes in the coating surface geometry that cause its roughness. Similarly, the coating properties can objectively quantify the uniformity of the coating surface geometry by measuring the deviation from a given reference geometry, or the degree of periodicity by indicating the length scale of the re-occurrence of geometric substructures, which may be important for achieving certain functional properties of the coating. In addition, if the coating has been treated in a well-defined and known way before the inspection, the coating properties can also generate information beyond the geometry itself, i.e., for example, about how the coating responds to the treatment used. In other words, the information encoded by the depth representation can be interpreted using information related to the past. For example, in an impact test, defects are generated in the coating, windows are generated inside it, and thus it is also convenient to examine structural properties, such as the material composition of the different layers. To validate a produced film coating or even a film coating being applied, the partial depth values may be used to assess whether the internal structure of the coating, such as interfaces between layers, has been acceptably formed.
[0019] In some embodiments of the method, the sensed data comprises holographic interferogram data indicative of an interaction of light with the coating, wherein the step of determining the depth expression comprises calculating reconstructed holographic interferogram data by applying digital holographic reconstruction to the holographic interferogram data, and determining the depth expression of the coating based on the reconstructed holographic interferogram data. The holographic interferogram data is preferably data relating to an interference pattern produced by a holographic device, wherein in this case the interaction of light with the coating is typically a transmission / reflection of a coherent light beam, such as may be produced by a laser, through / at the probe, the probe surface, or a coating covering the probe surface.
[0020] A holographic device for producing such an interference pattern typically comprises a light source for producing a coherent or at least substantially coherent light beam, and a beam splitting device for splitting the produced light beam into at least two beams, one of which is typically referred to as an object beam and the other of which is typically referred to as a reference beam. The object beam then interacts with an object, such as a coating, in the above sense by reflection or transmission, and subsequently, the object beam and the reference beam are redirected by a mirror device such that they recombine with each other to form a superimposed beam. The mirror device may comprise a mirror, which is adapted to be adjustable so as to change the distance travelled by the reference beam, i.e. its path length, before being superimposed with the object beam. For example, the mirror device may comprise a standard reference mirror, as used in a standard holographic setup, for adjusting the path length of the reference beam before being superimposed with the object beam.
[0021] The superimposed beam is usually directed to a photosensitive medium. Since the object beam has interacted with the object (i.e. the coating in our case), it will carry a different phase than the phase of the reference beam when superimposed, which means that the intensity of the superimposed beam will vary in space when it reaches the photosensitive medium. The photosensitive medium will record the spatially varying intensity in the form of an interference pattern, which can also be called an interference pattern. The interference pattern is further affected by the adjusted path length of the reference beam. Adjusting the path length of the reference beam can be particularly advantageous if information about the interior of the object is to be collected. For example, adjusting the path length of the reference beam by changing the position of a reference mirror can result in interference pattern data, which includes data corresponding to different depths or partial depth positions in the coating. If the coating is at least partially transparent, based on the interference pattern data, a layer profile can be determined. The layer profile represents the interfaces between different layers of the coating. From the layer profile, the layer thickness can be derived as the width of the layer, as represented by the layer profile as the depth difference between two interfaces indicated by the layer profile, i.e., for example, the width can be derived from a number of pixels belonging to the layer in a direction perpendicular to the interface, as shown in the layer profile.
[0022] When the photosensitive medium is coupled to a digital processing device, data representing the interference pattern, i.e., the interference pattern data, can be stored and / or further processed digitally. While in conventional holography, the interference pattern in analog form is used for optical reconstruction of the image of an object interacting with an object beam by shining a reconstruction beam on the photosensitive medium, the holographic interference pattern data can be similarly used to digitally reconstruct the image of the object. This is the basic idea of digital holographic reconstruction techniques. Digital reconstruction techniques exploit the insight that the interference pattern is related to the Fourier transform of the object, where the inverse transform of the object can be determined.
[0023] In a preferred embodiment of the present invention, the holographic interferogram data comprises at least two sets of interferogram data, wherein each set of interferogram data indicates the interaction of coherent light of a different wavelength with the coating, and wherein the reconstructed holographic interferogram data comprises synthetic reconstructed holographic interferogram data. Here, the term "synthetic" emphasizes the use of digital processing means to calculate the reconstructed holographic interferogram data, which includes information about the hypothetical interaction of light of a certain wavelength with the coating, the hypothetical interaction being a function of at least two wavelengths actually used, i.e. light of synthetic wavelength. Preferably, the synthetic wavelength corresponds to the beat frequency of the hypothetical superposition of coherent light beams with at least two different wavelengths. Thus, for example, in the case of two different wavelengths, the synthetic wavelength can be their sum or their difference. Synthetic wavelengths that are larger than the wavelength used to record the actual interferogram are particularly advantageous for examining coatings with depth variations of quite different scales, such as coatings with fine surface structures interrupted by relatively large functional elements, or, in fact, impact areas generated by the test procedure. This is because the longer synthetic wavelength allows phase ambiguity to be avoided at larger structures, while still maintaining a higher basic resolution due to the smaller wavelength actually employed.
[0024] The digitally reconstructed holographic interferogram data may simply be a digital image of the object, i.e. an image of, for example, the probe surface and the coating overlying it. In this case, the depth representation may simply be an image represented in a suitably adjusted coordinate system, wherein preferably one axis points in a direction perpendicular to the probe surface. The increased resolution provided by the digital holographic reconstruction will then be reflected in a very detailed and accurate depth representation of the coating, for example.
[0025] In some embodiments of the method, the depth representation comprises a topographic map of the coating surface. The topographic map carries full depth or penetration depth information, but no partial depth information, and therefore does not rely on sensed values from inside the coating. Thus, the topographic map can even be determined to sense values recorded by a device that is not suitable for sensing inside the coating, as is the case with optical sensing devices and non-transparent coatings.
[0026] In some embodiments of the method of the present invention, coating properties are derived based on topography, including generating a depth histogram by counting the number of probe surface points in a subset of the coating depth indicated by the topography for each of a plurality of predetermined depth intervals, and the counting result is associated with the corresponding depth interval. Therefore, the topography generates a depth histogram, which provides information about the depth distribution on the coating. This has the advantage that the objective characteristics of the coating become reproducible. For example, in the case where the coating surface is completely flat and parallel to a reference plane (measuring the coating depth relative to the reference plane), the depth histogram will only include a single non-zero entry, which corresponds to the number of points in a subset of the probe surface points for which sensing data has been provided, wherein the number will be associated via a histogram with an interval of depth values (wherein the depth indicated by the sensing data provided falls into the interval of the depth value). The predetermined depth intervals are preferably equal in size, and their size determines the fineness or coarseness of the histogram. The minimum size of the depth interval is reasonably selected to be equal to the minimum distance between the depths indicated by the sensing data, wherein the maximum size will be equal to the maximum distance between the depths indicated by the sensing data. Advantageously, in order to preserve the amount of information contained in the sensed data, the size of the depth intervals of the histogram corresponds to the resolution characterizing the sensed data. It will be appreciated by those skilled in the art that a coating having a regular thickness distribution, such as a periodic pattern whose periodic length is much smaller than the spatial extent of the portion of the coating for which the sensed data is provided, will result in a fairly flat depth histogram, i.e., a depth histogram in which the count results associated with most depth intervals are fairly similar to each other, even though the periodic pattern in the coating may show large depth differences between different points. On the other hand, a coating geometry characterized by a large portion having a relatively high thickness and only a small portion having a substantially lower thickness will result in a depth histogram including correspondingly large differences in the count results. In the case of defects in the coating produced by mechanical impact according to a well-defined test procedure, the shape of the depth histogram can be used to deduce the properties of the coating in the well-defined test procedure. However, even in the more general case of examining a coating that is not related to an impact test, a depth histogram can be used to objectively obtain the structural properties of the coating.
[0027] In some embodiments, deriving coating properties based on the topographic map further includes determining a peak depth interval indicating the position of a local maximum in the histogram. In this way, a depth interval is identified, which includes frequently encountered depth values, that is, indicating the coating thickness present on many probe surface points where sensing data has been provided. It should be understood that the term "local maximum" does not carry the meaning of spatial locality because it is for a histogram, that is, the spatial local maximum of the coating depth is not described. On the contrary, the expression "local" means that the depth histogram may include more than one local maximum, that is, other peaks, each corresponding to a count value higher than the count value corresponding to the depth interval in the neighborhood. Determining the position of the local maximum in the depth histogram is particularly advantageous for coating inspection because it allows the particularly meaningful properties of the coating to be derived. For example, if the coating includes two layers of different materials, and if the coating has been subjected to mechanical impact by a ballistic object, such as done in a standard stone chip impact test procedure, the position of the local maximum indicates that the coating has been damaged. In particular, different layers of the coating become distinguishable, even if they are not different in color. Identifying local maxima is also particularly advantageous for inspecting coatings without impact testing, as local maxima are often indicative of important structural features of the coating.
[0028] In some embodiments, determining the peak depth interval includes the steps of providing a tolerance threshold indicating a basic depth change, calculating a count difference by subtracting the count results associated with the selected depth interval, determining the sign of the selected count difference and / or comparing the count results associated with the selected depth interval, and determining the peak depth interval based on the provided tolerance threshold, the calculated count difference and the determined sign and / or the compared count results. Preferably, these steps are equivalent to calculating the discretized derivative of the depth histogram and determining where it changes sign, wherein the depth interval where the discretized derivative changes sign is taken as a candidate position for the local maximum. If the count results of all depth intervals in the neighborhood of the candidate peak position are less than the count results associated with the depth interval corresponding to the candidate peak position, and if the count results exceed a predetermined basic depth change, the candidate peak position is accepted as the true peak position. The basic depth change is the number of counts replaced by all or substantially all depth intervals.
[0029] In some embodiments, coating properties are derived based on determined peak depth intervals. Since the peaks in the histogram carry basic information about the depth variation of the coating, this basic information is captured by the coating properties in this way. For example, simply the coating properties are selected as depth values from the determined peak depth intervals, such as border or center values. In this case, it will be particularly suitable for facilitating objective and reproducible inspections.
[0030] In some embodiments, the coating property indicates the change of the structure and / or material of the coating, and / or indicates the thickness of the coating. The change of structure and / or material usually occurs at the interface between the two layers of the coating. Preferably, more than one coating property is determined so that if more than one change of the structure and / or material of the coating, i.e. more than one interface between the coatings is indicated by more than one coating property, the relationship between the interfaces can be determined. In particular, if the coating property is a depth value from two peak depth intervals, the layer thickness is estimated by their difference. In addition, other coating properties can be derived based on the depth value indicated by the coating property.
[0031] In some embodiments, the method further comprises the step of evaluating the mechanical resistance of the coating based on the derived coating properties. In particular, the mechanical resistance can be evaluated according to a standard classification, which indicates the distribution of defects generated during a standardized test procedure, as measured in terms of statistical properties (e.g., the average depth or average size of the defects).
[0032] In particular, the evaluation comprises estimating the characteristic size of each of a plurality of regions in the coating based on the determined coating properties. Preferably, the evaluation is further based on the determined topography. For example, the typical size of a defect, i.e., the impact area resulting from the impact of a ballistic object in a test such as a stone chip impact test, can be estimated by assigning a size to each defect, i.e., a size that can be inferred from the topography, and then estimating the typical size of the defect from a plurality of sizes of different defects. For example, by measuring the extent of a given defect in a direction parallel to the probe surface at a depth value corresponding to the interface between two layers, a measurement of the size of a given defect is objectively obtained. If the derived coating property indicates a layer interface depth value, the measurement can be performed using the topography. A direction parallel to the probe surface where the measurement is performed can, for example, maximize the measurement, i.e., make it consistent with the direction in which the defect has the maximum extent at the depth value indicated by the coating property.
[0033] More particularly, the area may indicate a mechanical impact to the coating. As described, the mechanical impact is preferably generated by a standard test procedure, such as a standard stone chip impact test. It should be understood that the area is not necessarily a defect area, i.e. a damaged portion of the coating, but may also include an intact, undamaged portion of the coating.
[0034] In some embodiments, the coating is at least partially transmissive to the light beam, wherein the holographic interference pattern data indicates the interaction of the light beam with the internal region of the coating, and wherein the depth expression includes a layer profile indicating the interface between the layers of the coating. In other words, due to the transmittance of the coating, information about the internal region of the coating can be obtained. This can include, for example, the position and shape of the interface between the layers. Therefore, the layer profile should be understood as any expression of information from the inside of the coating. For example, it can include a cross-sectional visualization of the coating in a plane perpendicular to the coating surface. If the coating includes more than one layer, the interface can become visible in the layer profile. The layer profile can be determined, for example, using digital holographic reconstruction technology.
[0035] In some embodiments, the interaction comprises a phase jump in the light beam, wherein an interface is indicated in a layer profile based on the detected phase jump. This manner of detecting a layer interface is particularly preferred when it is known that the layer comprises different refractive indices. This is because, if the second refractive index is higher than the first refractive index, the phase associated with a light beam that passes through a first layer having a first refractive index and is at least partially reflected at an interface to a second layer having a second refractive index will undergo a 180° change. Information about this phase jump will be encoded in the interferogram data and can be used to determine a particularly accurate layer profile, for example during digital holographic reconstruction.
[0036] In some embodiments, the coating property is a layer thickness, wherein deriving the layer thickness includes estimating the layer thickness based on a layer profile, and correcting the estimated layer thickness based on a known refractive index of the layer. For example, the refractive index of the first layer can be known from prior knowledge about the material of the first layer. The refractive index of various materials is known from the literature. For a particular material, it may be preferred to perform a reference measurement. The estimated layer thickness at a given probe surface point corresponds, for example, to the difference between the full coating depth at that point and the partial depth of the interface between the first topmost layer and the second layer at that point. This can be determined directly from the layer profile by measuring the degree to which the first layer is perpendicular to the coating surface in this case, for example by counting pixels. Preferably, the estimated layer thickness is corrected by multiplying the estimated layer thickness by the known refractive index.
[0037] In another aspect of the invention, a method of performing an impact test on a coating on a probe surface is provided, comprising the steps of firing a ballistic object into the coating, cleaning the coating by removing the ballistic object from the coating, collecting sensed data indicative of the depth of the coating at each of a predetermined subset of probe surface points, and inspecting the coating according to the method previously described.
[0038] In another aspect, an inspection device for inspecting a coating on a probe surface is provided, the device comprising a providing unit for providing sensing data indicating the coating depth at each of a predetermined subset of probe surface points, a determining unit for determining a topographic map of the coating from the sensing data, and a deriving unit for deriving coating properties based on the topographic map. The providing unit may be any hardware suitable for providing sensing data. For example, the providing unit may include a universal input device, which is suitable for receiving input data from a universal type storage medium having sensing data stored thereon, and passing the input data to the determining unit. In addition, the providing unit itself may include a storage device, which is suitable for storing sensing data and transmitting them to the determining unit upon request or command. The determining unit and the deriving unit typically each include a data processing device, which is suitable for receiving the sensing data and processing them in a controllable manner. The determining unit and the deriving unit may share parts of the processing device, but may also be completely disjoint in structure.
[0039] On the other hand, a system is provided, comprising: a sensing device adapted to collect sensing data indicating the depth of the coating at each of a predetermined subset of probe surface points; and an inspection device for inspecting the coating on the probe surface. The sensing device preferably comprises a holographic device, wherein the sensing data at this time comprises holographic interferogram data indicating the interaction of the light beam with the coating, wherein the light beam is preferably an object beam. In some embodiments, the interaction is the interaction of the object beam with the internal region of the coating. The internal region may include different layers of the coating, in which case, preferably, the depth expression generated by the inspection device comprises a layer profile. At this time, preferably, the holographic device comprises a mirror device for adjusting the path length of the reference beam, wherein the adjusted path length indicates the internal region, at which the interaction between the object beam and the coating indicated by the holographic interferogram data occurs. In this way, multiple sets of holographic interferogram data are recorded, each set of holographic interferogram data indicating the interaction of the object beam with different regions in the coating. These embodiments are particularly preferred if the coating is transparent to the light beam.
[0040] In yet another aspect, a system for performing an impact test on a coating on a probe surface is presented, comprising a ballistic device adapted to receive a plurality of ballistic objects and launch the ballistic objects at a predetermined test position, wherein the system is adapted to receive a probe at the predetermined test position and in a certain orientation so that when the ballistic object is launched by the ballistic device, the ballistic object is able to hit the coating on the probe surface, the system further comprising a cleaning device adapted to remove the ballistic object from the coating, a sensing device adapted to collect sensing data indicating the depth of the coating at each of a predetermined subset of probe surface points, and an inspection device as defined above.
[0041] Another aspect of the invention relates to a computer program for inspecting a coating on a probe surface, comprising instructions which, when executed on a computer, cause the computer to perform the method for inspecting a coating on a probe surface as defined above.
[0042] In one aspect, the present invention also relates to a computer program for performing an impact test on a coating on a probe surface, comprising instructions which, when executed on a computer controlling a system as defined above, cause the system to perform a method for performing an impact test on a coating on a probe surface as defined above.
[0043] It shall be understood that the method of claim 1, the method of claim 11, the inspection device of claim 12, the system of claim 13 and the computer program of claims 14 and 15 have similar and / or identical preferred embodiments, in particular as defined in the dependent claims.
[0044] It shall be understood that a preferred embodiment of the invention can also be any combination of the dependent claims or the above-mentioned embodiments with the respective independent claim.
[0045] These and other aspects of the invention will be apparent from and elucidated with reference to the embodiments described hereinafter. Brief introduction of the attached figure
[0046] In the following figures:
[0047] Figure 1 Schematically and exemplarily, an embodiment of a system of the present invention for performing an impact test on a coating on a probe surface is shown,
[0048] Figure 2 A flow chart illustrating a method of performing an impact test on a coating on a probe surface according to the present invention is shown schematically and exemplarily,
[0049] Figure 3 A flow chart illustrating the steps performed for inspecting a coating according to the invention is shown schematically and exemplarily,
[0050] Figure 4 shows an exemplary depth histogram generated for inspecting a coating in one embodiment of the present invention,
[0051] Figure 5 It shows that Figure 4 An exemplary curve of the derivative of the depth histogram is shown,
[0052] Figure 6 Schematic and exemplary illustrations of impact areas in a coating of a probe surface are shown.
[0053] Detailed description of implementation plan
[0054] Figure 1 The schematic and exemplary illustration of the system for performing impact test on the coating of the probe surface according to some embodiments of the present invention is shown. The system 100 is preferably a single automated system, which combines all the equipment necessary for automatically performing the fragment impact test on the probe surface coating and subsequently collecting the test results and performing its appropriate analysis. Alternatively, the system 100 may not combine all the necessary equipment in one position, in which case the method will not be fully automated, but requires manual interaction, for example, manually transferring the probe from one device to another and / or manually controlling these devices. In order to perform the impact test, the system 100 includes a ballistic device 110. The ballistic device is suitable for receiving ballistic objects for impact testing. Generally, the ballistic object is a steel or stone piece of predetermined size and predetermined weight, wherein the size and weight distribution of the fragments can be subject to company or international standards. The ballistic device 110 receives the fragments by a container with an opening toward the inside of the device, so that multiple fragments can be supplied to the container without passing all the fragments through the opening at one time. On the contrary, the fragments can pass through the opening in a controlled manner and at a controlled speed, so that the fragments of a predetermined amount reach the inside of the ballistic device 110 at a predetermined time step. When the ballistic device uses a launcher to launch fragments at a predetermined test position, the fragments that have arrived inside the ballistic device are preferably further supplied to the launcher. The launcher can be operated pneumatically, i.e., operated by air pressure, and is suitable for launching fragments one by one at a settable frequency and a settable time, wherein the fragments arrive at the test position because the ballistic device is suitable for launching the fragments to a suitable direction at a suitable speed. The system 100 is suitable for receiving the probe at a certain orientation at the test position so that its surface faces the ballistic device of the ballistic device 110. Therefore, once the probe is coated on its surface and is located at the test position, and its surface faces the launcher, the ballistic device 110 can be operated to launch the fragments onto the coating on the probe surface and possibly into the coating on the probe surface. In this way, the coating is usually damaged.
[0055] The system 100 further includes a cleaning device 120, which is suitable for removing debris from the coating that adheres thereto after the impact. In order to remove stone chips from the coating, the cleaning device 120 includes, for example, a device for rolling an adhesive tape and for contacting the adhesive tape with a coating probe located at a test position, and therefore also for contacting the adhesive tape with any debris adhered to the coating. The adhesive tape preferably includes an adhesive so that when the adhesive tape is repeatedly contacted with the debris adhered to the coating and peeled off from the coating, the stone chips will adhere to the adhesive tape and can be removed from the coating. Preferably, removing the debris from the coating includes several repetitions of contacting the adhesive tape with the coating and then removing it from the coating, wherein each repetition is followed by a translational movement of the adhesive tape so that each repetition is performed with a fresh portion of the adhesive tape.
[0056] System 100 further includes a sensing device 130 suitable for sensing the surface geometry of the coated probe. Preferably, the sensing device is an optical device. In this way, the geometry can be sensed contactlessly. If the coating surface is not transmissive in the frequency range of the light used for sensing, the geometry sensed will be limited to the surface geometry. If the coating surface is transmissive in the frequency range used, and if the rest of the coating is also transmissive, the sensing data of the position inside the coating can also be obtained. The sensing device 130 usually has a limited resolution, which means that in the case of it being an analog device, it will determine the distance under which the difference in the sensing data cannot be detected, and in the case of it being a digital device, it will only collect a limited number of data points. The calibration of the sensing device will determine the distribution of points at the test position or on the coated probe surface, and the sensing device 130 can collect the sensing data of these points.
[0057] The system 100 further comprises an inspection device 140, such as a computer, for analyzing the sensing data provided by the sensing device 130, and is therefore suitable for inspecting the coating of the probe surface. The inspection device 140 comprises a providing unit 141, such as an interface that can be electronically coupled to the sensing device 130, which is suitable for providing the sensing data. The providing unit can also be understood as a reading unit that is suitable for reading the sensing data stored on any storage medium and providing the sensing data for further analysis. The inspection device 140 also comprises a determining unit 142, which can be implemented by a processor of the computer 140, which is suitable for determining a depth expression of the coating based on the sensing data, and a deriving unit 143, which can be similar or identical to the determining unit 142, which is suitable for deriving the coating property based on the determined depth expression.
[0058] In applications unrelated to fragment impact testing, such as quality control during an ongoing production process in which a structured coating is deposited on a film or foil, the sensing device 130 and the inspection device 140 can alternatively be used independently of the rest of the system 100, for example in the form of a holographic camera. In this case, it is particularly preferred that the sensing device is adapted to collect optical sensing data from the interior of the coating, provided that the coating is transparent to the light used for sensing. The sensing data then indicates the interaction of the light with the interior area of the coating. This can be achieved, for example, by using an additional slidable mirror to adjust the travel distance of the reference beam. In this way, the relative phase shifts collected by the beam along its path through the coating can enter the sensing data and thus allow conclusions to be drawn about the refractive index of the layer at different partial depths. The change in refractive index can be interpreted by the inspection device 140 as indicating the position of the interface between the layers. Preferably, a phase jump of 180° occurring during the reflection of the light at the interface towards the optically thicker layer is identified. Based on this identification of the phase jump in the sensing data provided by the providing unit 141, i.e., for example in the holographic interferogram data, the determining unit 142 can determine the layer profile of the coating. The determination unit 142 may be adapted to determine the layer profile using standard techniques of digital holographic reconstruction known to a person skilled in the art, wherein if the interferogram data comprises data for more than one actual wavelength, the reconstruction may preferably be performed for a synthetic wavelength. From the layer profile, a layer thickness may be derived as a coating property by a derivation unit 143. For example, a layer thickness as derivable in the layer profile by, for example, based on the number of pixels between two interfaces may be corrected by multiplying by a corresponding refractive index known from a previous independent measurement.
[0059] Furthermore, the layer profiles generated by the holographic device directly determine the layer thickness and / or the interface position, i.e. the interface partial depth, which can also be applied in the stone evaluation results of the stone impact test, i.e. whether the coating is transparent or partially transparent. In this case, the characteristic size of the defect can be determined based on the position of the layer interface determined directly from the layer profile.
[0060] Figure 2 Schematically shows Figure 1 The system 100 described above can be used to perform impact testing on a coating on a probe surface. The general procedure of the present invention is as follows: In a first step 1, a ballistic object is shot into the coating using the ballistic device 110 of the system 100. Then, in a second step 2, the coating is cleaned by removing the ballistic object that has been shot into the coating and adhered therein from the coating using the cleaning device 120. Then, in a third step 3, sensing data is collected using the sensing device 130. In a fourth step 4, the cleaned coating is inspected using the inspection device 140. Reference will be made to Figure 3 Step 4 is described in more detail.
[0061] Figure 3A flow chart schematically and exemplarily illustrating the steps of inspecting a coating as its own method, which can be performed using the aforementioned inspection device 140, is shown. Thus, a first step 41 consists in providing sensing data indicating the depth of the coating at each of a subset of probe surface points. In a particular embodiment, the sensing data comprises a first set of data and a second set of data representing a holographic interferogram generated using a laser defined by a first wavelength and a second wavelength, respectively, and recorded using a photosensitive medium. The interference encoded in the interferogram originates from the phase modulation generated due to the interaction of a portion of the laser beam with the coating, wherein the portion, i.e., the probe beam, has been separated from the original source laser beam by an interferometric measurement device, then interacted with the coating, and thereafter superimposed again with the remainder of the source beam used as a reference beam. Since the phase modulation is different for different wavelengths, the corresponding interference patterns and therefore the two sets of holographic interferogram data will be different from each other, which means that more information about the coating is provided compared to the information provided when using only the interference pattern data collected for a single wavelength.
[0062] In this embodiment, step 42 includes a step 421 of calculating reconstructed holographic interferogram data by applying digital holographic reconstruction to the holographic interferogram data, which involves determining reconstruction data corresponding to a synthetic wavelength. The synthetic wavelength preferably corresponds to the beat frequency of the imaginary superposition of a laser beam having a first wavelength and a laser beam having a second wavelength, i.e., is inversely proportional to it. It is particularly preferred that the synthetic wavelength is equal to the sum of the first and second wavelengths. In this way, large depth changes can be accurately and unambiguously determined without sacrificing short-range resolution. Then, in step 422, a depth expression of the coating is determined based on the reconstructed holographic interferogram data. For example, the depth expression is a two-dimensional projection of a three-dimensional image produced by a visual reconstruction of the coating surface geometry, in which a Cartesian coordinate system can be imagined with a reference xy plane coinciding with the probe surface below the coating, which is assumed to be planar in this example. In this configuration, the z value of a point on the coating surface is interpreted as the full depth, i.e., the thickness of the coating. In the preferred case of a digital holographic reconstruction that produces reconstruction data corresponding to synthetic wavelengths exceeding the first and second wavelengths, the microstructure of the coating surface as well as significantly larger geometric variations in coating thickness are resolved by the topography.
[0063] Preferably, the damage caused by the impact test is controlled by the ballistic device 110 to be limited to a limited area of the coated probe surface, for example a square area of 75 mm×75 mm. In many cases, the topographic map will only show this square area. However, depth values can also be collected outside the square area. Then, the possible tilted position of the coated probe surface can be detected, that is, by averaging the depth values outside the square at more than one, preferably at least three positions, which can be, for example, the positions at the corners of the probe. Then, all depth values, including those from inside the impact area and therefore included in the topographic map, can be corrected for the tilted position.
[0064] In step 43, coating properties are derived based on the depth expression. In the embodiment described in the present invention, the depth expression includes a topographic map, and step 43 itself includes a step 431 of generating a depth histogram, a step 432 of determining peak depth intervals indicating the locations of local maxima in the histogram, and a step 433 of deriving coating properties based on the determined peak depth intervals. Step 431 in turn includes a step 4311 of counting, for each predetermined depth interval, the number of probe surface points in the subset whose coating depths indicated by the topographic map are located in the corresponding depth interval, and a step 4312 of associating the count results with the corresponding depth interval. In this particular embodiment, the predetermined depth intervals are selected to have equal size, where the size is determined to be 1 μm, and where the number of depth intervals is taken to be equal to the estimated maximum coating depth, which corresponds to the coating depth in the undamaged area. Typically, in this way, the number of depth intervals is at least 100, because it is expected that the coating damage caused by the impact test will result in a reduction of the coating depth in the impact area by up to 100 μm. Then, counting is performed by traversing all points in the topographic map and determining for each of them whether the depth associated therewith is within a given depth interval. Determining whether a depth value is within a given depth interval comprises comparing the depth value with the boundaries of the depth interval. For example, if the depth value is greater than or equal to the lower boundary of the depth interval but less than the upper boundary of the depth interval, then the depth value is determined to be within the depth interval. In this way, determinations can be made accordingly for all depth intervals without the risk of any depth values not being shown in the depth histogram.
[0065] In the case of a fragment impact test, the depth value may be the penetration depth value d p , which indicates the deviation between the coating thickness at a given probe surface point and the full coating depth. The full coating thickness may correspond to the coating thickness outside the impact region. The penetration depth may also be determined without knowing the actual coating thickness, but simply by determining the difference between the z-coordinate value z0 corresponding to the full coating surface (which may be corrected for tilted probe position as described above) and the z-coordinate value of the coating surface at the corresponding point, i.e., dp =z0-z. Preferably, by setting a corresponding margin around z0 in both directions, only penetration depth values with an absolute value exceeding a predeterminable rough level are taken into account. The size of this margin can be set manually or automatically. When set automatically, it is preferably learned from a reference pattern such as a reference probe and applied to all other probes thereafter. In impact tests, this margin can also be used to ignore the impact of fragments that bounce off the coating surface without substantial damage. The margin generally depends on the type of coating and can range from a value as small as 0.5 μm for a small neglect level to a value as high as 5 μm for a transparent coating such as a varnish.
[0066] In reference Figure 3 In the particular embodiment described, the step 432 of determining the peak depth interval indicating the location of the local maximum in the histogram includes: a step 4321 of providing a tolerance threshold indicating a change in the base depth; a step 4322 of calculating a count difference by subtracting the count results associated with the selected depth interval; a step 4323 of determining the sign of the selected count difference and / or comparing the count results associated with the selected depth interval; and a step 4324 of determining the peak depth interval based on the provided tolerance threshold, the calculated count difference, and the determined sign and / or the compared count results. In this embodiment, the tolerance threshold is used to eliminate the baseline level, that is, the number of counts that are almost detected for substantially all depth intervals, and the tolerance threshold is automatically determined. Its existence is due to the fact that the shape of the defects is generally non-uniform. In other embodiments, the tolerance threshold is manually set. Step 4322 preferably uses standard techniques to determine the discrete derivative of a function, where in this case, the function is given by the count results that depend on the coating depth. In this embodiment, step 4323 is realized by detecting the sign change of the discrete derivative of the count result (i.e., count difference) between two adjacent depth intervals, wherein only the depth interval associated with the count result exceeding the provided tolerance threshold is detected. Once the peak depth interval is determined, then in step 433, coating properties are derived based on it. Then, the evaluation 44 of coating can be carried out based on the derived coating properties. Coating properties preferably indicate the change of the structure and / or material of coating. This is because the ballistic object shot on the coating or shot into the coating will leave defects therein, and the defect preferably shows the depth corresponding to the change of the structure and / or material in the coating, such as the depth that may be given by the interface between two coatings. The defect of the first type causes a spike due to the significant flakes of coating at the layer interface. The defect of the second type causes a wider peak in the histogram. If the ballistic object enters the coating in a more excavated manner, the defect of the second type occurs, thereby showing a larger layer portion along the defect wall.
[0067] Preferably, the coating comprises a thin surface layer, a first main defect layer below the surface layer, and a second main defect layer below the first main defect layer. In this case, the histogram comprises three peak depth intervals, wherein the first peak depth interval indicates the surface layer of the coating, the second peak depth interval indicates the first main defect layer of the coating, and the third peak depth interval indicates the second main defect layer of the coating. Then, the coating properties can be derived as an interface local depth value, which indicates, for example, the position where a transition occurs between the first main defect layer and the second main defect layer. In a specific embodiment, the characteristic size of each defect can be estimated by measuring the range of the defect in the direction parallel to the probe surface and at the depth corresponding to the determined interface partial depth in the topographic map. The characteristic sizes of multiple defects can be statistically analyzed, wherein the statistical analysis can be used to evaluate the mechanical resistance of the coating according to a standard reference value. For example, the standard reference value may depend on the average characteristic size of multiple defects. Additionally or alternatively, it may depend on the total score of the damaged area of the coating surface. The estimation of the damaged area can be given by the total number of points attributed to the defect. This number can also be estimated based on the depth histogram, i.e., by summing the counting results associated with the peak. A count result may be associated with a peak if it is associated with a depth interval that is within a predetermined range around a corresponding determined peak depth interval that indicates a maximum value of the peak. For example, a count result may be included if it is within 6σ of a peak, where σ represents the standard deviation. However, other ranges may also be applied, which may be known from the model system. Furthermore, only those count results associated with depth intervals that indicate a location beyond a determined depth of the interface portion may be included.
[0068] Figure 4 An exemplary depth histogram H of the embodiment described with respect to the previous figures is shown. The horizontal axis represents the penetration depth d in the coating in units of 1 μm. p , the vertical axis represents the coating result n, i.e. the number of points in a predetermined subset of probe surface points for which sensing data representing the corresponding penetration depth were initially provided. For example, there are approximately 10,000 points on an inspection portion of the coating where the measured penetration depth is 7±0.5 μm. The histogram H shows three maxima, two of which are strongly pronounced, while the first maximum has a significantly lower peak. The corresponding peak depth intervals are located between 2 μm and 6 μm for the first peak, between 45 μm and 57 μm for the second peak, and between 87 μm and 98 μm for the third peak. Between the peaks, a threshold of approximately 17,000 counts is not exceeded. At the same time, the count results are also not close to 0 within the displayed range of the penetration depth. This base level of counts between 0 and 17,000 can be understood as being irrelevant to the derivation of coating properties and can therefore be eliminated by setting the tolerance threshold equal to 17,000.
[0069] Figure 5 Shows Figure 4 The discrete derivative H' of the histogram H of . Again, the horizontal axis represents the penetration depth d p , in μm, while the vertical axis now measures how the counts n change from one penetration depth interval to the next. p This change is expressed in micrometers. -1 Measured in units of . The second and third maxima are fairly easily detected based on clearly distinguishable sign changes of the discrete derivative at about 51 μm and about 92 μm, respectively, where in both cases the sign changes from positive to negative. In order to determine the first peak depth position, two penetration depth values are used as candidates, namely a value of about 5 μm and a value of about 7 μm, since at these two values the sign of the discrete derivative changes from positive to negative. In this case, the true peak depth interval position is calculated by taking the average, i.e., in this case, resulting in 6 μm. In other embodiments, the true peak depth interval position is determined by fitting an analytical peak function, which may be of Gaussian shape, to the counting results around the peak, and the peak position is estimated as the position of the maximum of the analytical peak function.
[0070] Figure 6 A cross section of an exemplary portion of a probe covered with a multi-layer coating having defects resulting from debris impact during a debris impact testing procedure is shown. Figure 6 It can also be seen as a schematic visualization of a layer profile, which is determined based on sensing data also from inside the coating and, in this case, also from the probe. The probe comprises a body portion PB and a probe surface PS. The coating covers the probe surface PS and comprises three layers. The top layer is a relatively thin surface layer LS. Below is a first main layer L1 and a second main layer L2, wherein the surface layer LS and the first main layer are separated by an interface IS1. In this example, the first main layer L1 is sandwiched between the surface layer LS and the second main layer L2, the second layer being in direct contact with the probe surface PS. The defect D affects all three layers. In other examples, the coating may include other layers, the layers below being deep enough to be unaffected by the impact of debris. Due to the defect D in Figure 6In the example shown, both the first main layer L1 and the second main layer L2 are significantly affected, so they can also be referred to as the first and second main defect layers, respectively. The characteristic dimension of the defect D is assumed to be given by its width w, as measured in the cross-section along the interface I12 between the first main defect layer L1 and the second main defect layer L2. The position of the interface, i.e., the partial depth, is known either from the corresponding peak depth interval determined by the depth histogram or, in the case of a transparent or partially transparent coating, from the layer profile, as explained above. For example, according to the company's articles of association, a cross-section for measuring W can be selected such that W is maximized. Optionally, W can be further corrected to W'=(W + W perp ) / 2, where W perp is the maximum extent of the defect measured along the interface I12 in a cross-section perpendicular to the original cross-section. Then, the defects are again classified into severity levels defined by a given threshold according to the articles of association. For example, defects with W(')≤1mm will be classified into the lowest severity level, while defects with 1mm < W(')≤1mm have been classified as more severe. The distribution of the severity levels over all the defects - which may be approximately parameterized by the average severity level and / or the standard deviation - precisely measures the resistance of the test coating to fragment impact. Its characteristics can be used to evaluate the mechanical resistance of the 44 coating.
[0071] Although the embodiments described above with reference to the accompanying drawings relate to the application of the present invention for inspecting a coating against impacts caused by an impact test procedure and using digital holographic techniques, it should be understood that the same or similar principles can also be applied to other purposes and using different means. In particular, the disclosed method is not limited to being used in combination with holographic imaging techniques, but can equally utilize other means to provide sensing suitable for determining depth representation. In particular, such means include profilometry and deflectometry and / or imaging systems. In addition, it should be understood that the method is also applicable to monitoring an ongoing production process in which a structured coating is applied to a film or foil, or for evaluating the results, such as whether a specific coating structure required to obtain a specific function has been achieved. In particular, although the determination of the depth histogram has only been proposed for stone impact tests, it should be understood that the depth histogram described herein will also be advantageous in other types of inspections of coatings by deriving objective characteristics therefrom. On the other hand, it should be noted that in impact tests on transparent or partially transparent coatings such as varnishes, in addition to or instead of determining the depth histogram from the topographic map of the coating, coating properties such as the position of the layer interface can also be derived from the layer profile.
[0072] Other variations of the disclosed embodiments can be understood and implemented by those skilled in the art by studying the drawings, the disclosure, and the appended claims, and the claimed invention can be practiced.
[0073] In the claims, the word "comprising" does not exclude other elements or steps, and the indefinite article "a" or "an" does not exclude a plurality.
[0074] A single unit or device may fulfill the functions of several items recited in the claims. The mere fact that certain measures are recited in mutually different dependent claims does not indicate that a combination of these measures cannot be used to advantage.
[0075] Procedures such as providing sensing data, determining a depth representation of the coating from the sensing data, and deriving a property of the coating based on the depth representation, and procedures such as firing a ballistic object into the coating, cleaning the coating, and collecting sensing data—described as being performed by one or several units or devices—may be performed by any other number of units or devices. These procedures and / or operations of the system may be executed as instructions of a computer program and / or dedicated hardware.
[0076] The computer program may be stored and / or distributed on an appropriate medium provided together with or as part of other hardware, such as an optical storage medium or a solid-state storage medium, and may also be distributed in other forms, such as via the Internet or other wired or wireless communication systems. Any reference signs in the claims should not be construed as limiting the scope.
Claims
1. A method (4) for inspecting a coating on a probe surface, comprising the following steps: - providing (41) sensed data indicative of the coating depth at each of a predetermined subset of probe surface points, - determining (42) a depth representation of the coating from the sensed data, and - deriving (43) coating properties based on depth representation, The depth representation includes the topography of the coating surface, and Wherein deriving (43) the coating properties based on the topographic map includes generating (431) a depth histogram (H) by: - for each of a plurality of predetermined depth intervals, counting (4311) the number of probe surface points in the subset whose coating depth indicated by the topographic map is in the corresponding depth interval, and - Associate the count results with the corresponding depth intervals (4312).
2. The method of claim 1, wherein the sensed data comprises holographic interferogram data indicative of interaction of the light beam with the coating.
3. The method of claim 1, wherein the step of determining the depth representation (42) comprises: - calculating (421) reconstructed holographic interferogram data by applying digital holographic reconstruction to the holographic interferogram data, and - Determining (422) a depth representation of the coating based on the reconstructed holographic interferogram data.
4. The method of claim 2, wherein the step of determining the depth representation (42) comprises: - calculating (421) reconstructed holographic interferogram data by applying digital holographic reconstruction to the holographic interferogram data, and - Determining (422) a depth representation of the coating based on the reconstructed holographic interferogram data.
5. The method of claim 1, wherein deriving (43) coating properties based on the topographic map further comprises: - determining (432) peak depth intervals indicating locations of local maxima in the histogram (H).
6. The method of claim 5, wherein coating properties are derived (433) based on the determined peak depth intervals.
7. The method according to any one of claims 1 to 6, wherein the coating property is indicative of a change in structure and / or material of the coating and / or is indicative of a thickness of the coating.
8. The method according to any one of claims 1 to 6, further comprising the following steps: - assessing (44) a mechanical resistance of the coating based on the derived coating property, wherein the assessing comprises estimating a characteristic size of each of a plurality of regions in the coating based on the determined coating property, the regions being indicative of a mechanical impact to the coating.
9. The method according to claim 7, further comprising the steps of: - assessing (44) a mechanical resistance of the coating based on the derived coating property, wherein the assessing comprises estimating a characteristic size of each of a plurality of regions in the coating based on the determined coating property, the regions being indicative of a mechanical impact to the coating.
10. The method of claim 3, wherein the coating is at least partially transmissive to the light beam, wherein the holographic interference pattern data indicates interaction of the light beam with an internal region of the coating, and wherein the depth representation includes a layer profile indicating interfaces between layers of the coating.
11. The method of claim 4, wherein the coating is at least partially transmissive to the light beam, wherein the holographic interference pattern data indicates interaction of the light beam with an internal region of the coating, and wherein the depth representation includes a layer profile indicating interfaces between layers of the coating.
12. The method of claim 10, wherein the interaction comprises a phase jump in the light beam, wherein an interface is indicated in a layer profile based on the detected phase jump.
13. The method of claim 11, wherein the interaction comprises a phase jump in the light beam, wherein an interface is indicated in a layer profile based on the detected phase jump.
14. The method of claim 12, wherein the coating property is layer thickness, wherein deriving the layer thickness comprises: - estimate layer thickness based on layer profiles, and - Correcting the estimated layer thickness based on the known refractive index of the layer.
15. The method of claim 13, wherein the coating property is layer thickness, wherein deriving the layer thickness comprises: - estimate layer thickness based on layer profiles, and - Correcting the estimated layer thickness based on the known refractive index of the layer.
16. A method for performing an impact test on a coating on a probe surface, comprising the steps of: - firing a ballistic object into (1) the coating, - cleaning (2) the coating by removing ballistic objects from the coating, - collecting (3) sensed data indicative of coating depth at each of a predetermined subset of probe surface points, and - Inspecting (4) the coating according to claim 1.
17. An inspection device (140) for inspecting a coating on a probe surface, comprising: - a providing unit for providing sensed data indicative of the coating depth at each of a predetermined subset of probe surface points, - a determination unit for determining a depth representation of the coating from the sensing data, and - a derivation unit for deriving coating properties based on the depth representation, The depth representation includes the topography of the coating surface, and The deriving of coating properties based on the topographic map includes generating a depth histogram (H) by: - for each of a plurality of predetermined depth intervals, counting the number of probe surface points in the subset whose coating depth indicated by the topographic map is in the corresponding depth interval, and - Associate the count results with the corresponding depth intervals.
18. A system (100) for performing an impact test on a coating on a probe surface, comprising: - a ballistic device (110) adapted to: - receive multiple projectile objects, and - firing a ballistic object at a predetermined test location, wherein the system is adapted to receive the probe at the predetermined test location and in a direction such that the ballistic object is able to hit the coating on the probe surface when the ballistic object is fired by the ballistic device, - a cleaning device (120) suitable for removing ballistic objects from the coating, - a sensing device (130) adapted to collect sensing data indicative of the coating depth at each of a predetermined subset of probe surface points, and - Inspection device (140) according to claim 17.
Citation Information
Patent Citations
Method and apparatus for optically measuring by interferometry the thickness of an object
US20130045663A1
Method and apparatus for optically measuring by interferometry the thickness of an object
CN102892552A
Method for non-destructive evaluation of ceramic coatings
US9488470B1