Processing tool capable of forming a carbon layer on a substrate
By generating plasma in the processing chamber and using DC voltage pulses to control the bombardment of carbon ions on the substrate surface, the problems of low deposition rate and high stress in the existing diamond-like carbon layer are solved, realizing efficient and low-cost carbon layer deposition and implantation, which is suitable for semiconductor wafers.
Patent Information
- Application Number
- CN202080047253.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-06-27
- Filing Date
- 2020-06-25
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2040-06-25
AI Technical Summary
Existing technologies struggle to effectively form high-quality diamond-like carbon layers in large-scale industrial production, especially on semiconductor wafers, where issues such as low deposition rates, high costs, or excessive stress leading to wafer bending and warping arise.
By generating carbon ion and non-carbon ion plasma in the processing chamber, carbon ions are suspended using RF energy and bombarded on the substrate surface by DC voltage pulse control. Combined with electrode neutralization and vacuum pump to remove non-carbon ions, a high-energy carbon layer is formed.
It enables efficient deposition and implantation of carbon layers on substrates to form a variety of carbon layers with desired thicknesses, suitable for semiconductor wafers, reducing stress, increasing deposition rate and reducing cost.
Smart Images

Figure CN114096696B_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This application claims the benefit of priority to U.S. Application No. 62 / 867,770, filed on June 27, 2019, which is incorporated herein by reference for all purposes. Technical Field
[0003] The present invention relates to a substrate processing tool, and more particularly, to a substrate processing tool capable of forming a carbon layer on a substrate by sequentially performing the following operations: (1) generating a plasma containing carbon ions and non-carbon ions in a processing chamber, (2) suspending the carbon ions and non-carbon ions in the processing chamber, (3) removing a majority of the non-carbon ions from the processing chamber, and (4) bombarding the substrate surface with a majority of the carbon ions. In an alternative embodiment, the sequence (1) to (4) can be repeated multiple times until the carbon layer has a desired thickness. Background Art
[0004] Diamond-like carbon or "DLC" is a class of carbon materials with diamond-like properties, including extreme hardness, wear resistance, and "smoothness." The most common DLC is tetrahedral carbon or "ta-C," which is the hardest, most wear-resistant, and smoothest of its kind.
[0005] Various plasma-based deposition techniques have been used to deposit ta-C onto substrates such as semiconductor wafers. Such techniques include mass selected ion beam (MSIB), filtered cathode vacuum arc (FCVA), pulsed laser ablation (PLA) and electron cyclotron wave resonance (ECWR). Although each of these plasma-based techniques can be used to form ta-C on a substrate in a laboratory environment, they are not practical for full-scale manufacturing of semiconductor wafers. For example, the deposition rates of MSIB, FCVA and PLA are very low because each relies on a beam-based plasma source that must scan the entire wafer. As a result, the deposition rate is too slow for large-scale industrial-scale semiconductor wafer manufacturing. ECWR overcomes the low deposition rate of the above-mentioned other techniques to some extent. However, ECWR tools are extremely expensive, and the cost is too high to be actually used for large-scale industrial-scale semiconductor wafer manufacturing.
[0006] It is also known to deposit a carbon layer onto a substrate using a plasma enhanced chemical vapor deposition (PECVD) tool that includes a graphite target. Using these tools, carbon is released from the graphite target and radio frequency (RF) is applied, thereby producing a plasma containing only carbon. The problem with these tools is that the carbon ions have relatively low energy when deposited on the substrate surface. As a result, a polycrystalline diamond-like carbon film with a larger crystal structure (1 to many microns) and strong bonds is formed. Such carbon layers are generally not suitable for certain types of substrates, such as semiconductor wafers, because they can apply a lot of stress, causing the wafer to bend, warp, or even crack. Therefore, for certain applications, such as patterned masks, amorphous, "dust-like" carbon with random and / or sub-nanometer bonding is preferred because such a layer exerts much less stress on the underlying wafer.
[0007] There is therefore a need for a PECVD tool and method for forming carbon layers on a large industrial scale. Summary of the invention
[0008] The present invention relates to a plasma tool and method for producing a carbon layer on a substrate. To form the carbon layer, the tool performs a series of steps, which include: generating a plasma containing carbon ions and non-carbon ions in a process chamber; suspending the carbon ions and non-carbon ions in the process chamber by removing RF energy applied to the plasma; removing most of the suspended non-carbon ions from the process chamber; and then bombarding the substrate surface with most of the suspended carbon ions in the process chamber. By controlling the relative voltage potential of the carbon ions with respect to the substrate during the bombardment, the carbon ions can have sufficient energy to be deposited on the substrate surface and implanted into the bulk of the substrate. As a result, a carbon layer is formed.
[0009] The steps of removing a majority of the non-carbon ions and bombarding the substrate may optionally be repeated until the carbon layer has a desired thickness. This is achieved by applying a varying DC voltage in the form of a series of negative and positive voltage pulses to an electrode located in the process chamber at the distal end of the substrate. During the negative pulse, most of the non-carbon ions are attracted to the electrode and then removed from the chamber. As a result, a very high proportion of carbon ions remain in the process chamber. During the subsequent positive pulse, the carbon ions remaining in the process chamber bombard the substrate. It is generally preferred to apply a varying DC voltage while suspending the carbon ions and hydrogen ions after removing the RF energy.
[0010] In various embodiments, the plasma is generated using precursors containing carbon and non-carbon. Representative precursors include, but are not limited to, acetylene (C2H2), methane (CH4), or some other precursor containing carbon and hydrogen. With the precursors located in the processing chamber, RF energy is applied to the electrodes, thereby generating a plasma of non-carbon ions and carbon ions in the processing chamber.
[0011] In various alternative embodiments, the application of RF for generating the plasma may be interspersed with a series of negative and positive pulses. Alternatively, the plasma may be generated only when needed to replenish the carbon in the process chamber. In alternative embodiments, RF may be applied to the same electrode as the negative and positive DC voltage pulses, or may be applied to a second electrode in the process chamber.
[0012] In yet another non-exclusive embodiment, the electrode also neutralizes the charge of ions it contacts by surface recombination neutralization.A vacuum pump located near the electrode removes the neutralized ions from the process chamber.
[0013] In specific but non-exclusive embodiments, the carbon layer can be a plurality of different types of carbon layers, including various types of diamond-like carbon (DLC) layers, such as hydrogenated amorphous carbon (aC:H) and hydrogenated tetrahedral amorphous carbon (ta-C:H) and tetrahedral amorphous carbon or "ta-C" and / or other types of carbon layers having primarily sp3 bonds, such as diamond layers, carbon layers having relatively large crystalline structures (1 to many microns) or relatively small crystalline structures (sub-nanometer size), carbon layers comprising primarily sp2 bonds (such as graphite and so-called amorphous carbon, which is often characterized as "dusty"), and carbon layers having virtually no sp3 and / or sp2 bonds. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] The present application and its advantages may be best understood by referring to the following description taken in conjunction with the accompanying drawings, in which:
[0015] Figure 1 is a diagram of a processing tool capable of forming a carbon layer on a substrate according to a non-exclusive embodiment of the present invention.
[0016] Figure 2 is a flow chart of the operation of a processing tool according to a non-exclusive embodiment of the present invention, illustrating a series of steps for forming a carbon layer on a substrate.
[0017] Figure 3 is a timing diagram illustrating radio frequency (RF) interspersed with a series of positive and negative DC voltage pulses applied to electrodes in a process chamber of a process tool in accordance with a non-exclusive embodiment of the present invention.
[0018] Figure 4A and Figure 4B is a diagram of a non-exclusive embodiment of an electrode in a process chamber of a process tool.
[0019] Figure 5 is a diagram illustrating a substrate having a carbon layer formed thereon according to a non-exclusive embodiment of the present invention.
[0020] Figure 6 is a diagram illustrating a flow chart for manufacturing a semiconductor wafer using a carbon mask according to the present invention.
[0021] Figure 7 is a flow chart of the operation of a processing tool according to a non-exclusive embodiment of the present invention, illustrating a series of steps for forming a layer on a substrate.
[0022] In the drawings, the same reference numerals are sometimes used to denote the same structural elements. It should also be understood that the depictions in the drawings are schematic and not necessarily drawn to scale. DETAILED DESCRIPTION
[0023] The present application will now be described in detail with reference to several non-exclusive embodiments of the present application as shown in the accompanying drawings. In the following description, many specific details are set forth to provide a thorough understanding of the present disclosure. However, it is apparent to those skilled in the art that the present disclosure can be put into practice without some or all of these specific details. In other cases, in order to avoid making the present disclosure unnecessarily difficult to understand, well-known processing steps and / or structures are not described in detail.
[0024] refer to Figure 1 , a diagram of a processing tool 10 according to the present invention is shown. In various embodiments, the processing tool 10 can include one or more processing chambers. For simplicity, the following discussion only relates to a single processing chamber.
[0025] The processing tool 10 includes a process chamber 12 defined by insulating walls 14A and a base plate 14B coupled to ground, a substrate pedestal 16 for supporting a substrate 18 within the process chamber 12, a grounded cage 20 formed around the insulating walls 14A and the base plate 14B of the process chamber 12 but separated by an atmospheric gap 22, and a controller 24.
[0026] The insulating wall 14A of the processing chamber may be made of any of a variety of different insulating materials, such as aluminum oxide (Al2O3), quartz, sapphire, or other dielectric materials.
[0027] The substrate pedestal 16 includes an anode ring 25 that is at least partially positioned below a portion of the substrate 18 that extends beyond the substrate pedestal 16. In a particular embodiment, the anode ring 25 is coupled to a DC ground via the base plate 14B. The substrate pedestal 16 and anode ring 25 are used to clamp the substrate 18 in place using any number of known clamping methods, including electrostatic (ESC), vacuum, mechanical clamping, or any combination thereof.
[0028] In a non-exclusive embodiment, the anode ring 25 is also held to both DC ground and RF ground. One way to achieve DC and RF grounding is to securely bolt or otherwise mechanically clamp the anode ring 25 to the substrate 14B. If other grounding techniques are used, such as a thin wire connected between the anode ring 25 and the substrate 14B, other problems may arise. For example, such a thin wire may have an inductive impedance that may simply be too high at RF / VHF frequencies, causing the anode ring 25 to "float" relative to the RF / VHF.
[0029] A ground cage 20, preferably made of a highly conductive material such as aluminum, isotropic graphite or other suitable material, is coupled to ground. Air is provided in a gap 22 between the ground cage 20 and the walls 14 defining the process chamber 12.
[0030] The processing tool 10 also includes a number of other features and / or elements that facilitate the formation of a carbon layer on the substrate 18. These features and / or elements include an electrode 26 located remote from the substrate 18 in the processing chamber 12, a variable DC voltage source 28, a radio frequency (RF) source 30, and a pair of switches S1 and S2 and a vacuum pump 34 fluidly coupled to the space just above or near the electrode 26. The switches S1 and S2 operate together to selectively connect the electrode 26 to:
[0031] (a) RF source 30;
[0032] (b) the negative (-) terminal of the variable DC voltage source 28; or
[0033] (c) The positive (+) terminal of the variable DC voltage source 28.
[0034] It should be understood that, as described throughout this application, switches S1 and S2 can be implemented using two physical switches or other circuits that can implement switching logic or functions similar to those described herein. For example, in the latter case, the functions of switches S1 and S2 can be implemented by changing the signal level of a voltage amplifier to generate positive and negative DC pulses.
[0035] Electrode 26 performs a variety of functions. These functions include:
[0036] When connected to RF source 30 via switch S1, the electrode allows RF energy to enter processing chamber 12. When one or more reactants are introduced into processing chamber 12 along with the RF energy, plasma 36 is generated. In a non-exclusive embodiment, the reactant is acetylene (C2H2), methane (CH4), or any other reactant containing carbon and hydrogen. Using such reactants, a plasma having an overall positive charge is generated, which includes a mixture of hydrogen ions and carbon ions, both of which have a positive net charge. For example, the plasma is sometimes referred to as a "Debye sheath" or "Debye plasma" because of its greater density of positive ions, named after Peter Debye, a Dutch scientist who discovered this phenomenon.
[0037] In one non-exclusive embodiment, the RF source 30 is 100 MHz. In other embodiments, the RF source 30 may be 13 MHz, 27 MHz, or any other RF frequency suitable for generating the plasma 36 within the processing chamber 12. Such suitable frequencies may fall within the range of radio frequencies generally considered to be low, medium, or high, and may range from 400 kHz to 5 GHz. In other alternative embodiments, the electrode 26 may be capacitively or inductively coupled to the RF source 30.
[0038] Since the anode ring 25 is in contact with the substrate 18 and both are DC grounded and RF grounded, several benefits are achieved with respect to the electrode 26. During the application of RF, the substrate 18 is used as an RF reference ground, rather than a DC ground, because the substrate is "floating" and its impedance to the DC ground approaches infinity. As a result, in a non-exclusive embodiment, the area ratio between the substrate 18 and the electrode 26 is equal to or close to 1:1. However, it should be understood that the ratio is not required to be 1:1. In other embodiments, the surface area ratio of the substrate 18 to the electrode 26 may be greater or less than 1:1.
[0039] The electrode 26 also provides negative and positive DC pulses within the processing chamber 12. With S1 connected to S2 (opposite to the RF source 30), S2 can be controlled to produce a series of negative or positive pulses applied to the electrode 26. For example, by switching to the negative terminal for 1 to 2 microseconds, a pulse with a negative amplitude and a duration of 1 to 2 microseconds is generated. Alternatively, by switching to the positive terminal for 10 to 15 microseconds, a pulse with a positive amplitude and a duration of 10 to 15 microseconds is generated. The amplitude (positive or negative) of the pulse is determined by the variable DC voltage source 28. Since the DC voltage source is variable, the amplitude of a given pulse can vary widely. Therefore, by controlling the switches S1 and S2 and the variable DC voltage source 28, pulses with varying pulse widths, amplitudes, and polarities can be generated and applied to the electrode 26.
[0040] The negative and positive DC pulses applied to the electrode 26 provide useful functions in forming a carbon layer on the substrate. For the negative pulses, positive ions in the plasma sheath are attracted to the electrode 26. Since hydrogen ions have a lower atomic mass than carbon ions, the hydrogen ions accelerate toward the electrode and move much faster than the carbon ions. In contrast, the higher mass carbon ions have greater inertia and therefore move more slowly in response to the negative voltage applied to the electrode 26. Therefore, by intentionally limiting the duration or width of the negative pulse, far more hydrogen ions can be removed from the processing chamber 12 than carbon ions. For example, the applicant has found that by limiting the width of the negative pulse to 1 to 2 microseconds, a large percentage (e.g., more than 90%) of hydrogen ions can be removed from the plasma sheath, while a relatively small percentage (e.g., less than 10% or 15%) of carbon ions can be removed. As a result, the vast majority of ions remaining in the plasma sheath are carbon.
[0041] When a subsequent positive DC pulse is applied to electrode 26, the positive voltage will repel most of the carbon ions and accelerate them toward substrate 18. In addition, since substrate 18 is biased at or near ground by anode ring 25, the carbon atoms have sufficient energy to bombard the surface of substrate 18. As a result, the carbon atoms are not only deposited on the surface of substrate 18, but are also sub-implanted into the bulk of substrate 18. As a result, a carbon layer is formed.
[0042] In a non-exclusive embodiment, the electrode 26 can also act as a charge neutralization "trap" for ions removed from the plasma sheath. Through a process called surface recombination neutralization, charged ions exchange their charges when in contact with the surface of the electrode 26, thereby becoming charge neutral. In this case, the hydrogen ions and carbon ions of the plasma sheath carry a positive charge. The negative charge applied to the electrode 26 attracts the positively charged ions. When the ions contact the surface of the electrode 26, charge exchange occurs, thereby neutralizing the ions. The electrode 26 can therefore be referred to as a sub-Debye neutralizer. In certain non-exclusive embodiments, the electrode 26 can include a catalytic material that contributes to charge neutralization. Such catalytic materials can include, but are not limited to, aluminum, aluminum nitride, aluminum oxide, graphite, or any other material that can contribute to charge neutralization.
[0043] exist Figure 1In the illustrated embodiment, the electrode 26 is located near the top of the processing chamber 12 so that the plasma 36 is located between the substrate 18 and the electrode 26. With this arrangement, negative pulses from the variable DC voltage source 28 attract hydrogen ions to the electrode 26 in a direction opposite to the substrate 18. In an alternative embodiment (not shown), the electrode can be positioned below the substrate 18 near the bottom of the processing chamber 12. In this arrangement, positive pulses from the variable DC voltage source 28 applied to the electrode repel hydrogen ions in a direction away from the substrate 18 and the electrode 26. This arrangement also helps with sub-implantation control when bombarding the wafer with carbon ions.
[0044] The pump 34 is provided in close proximity to or directly above the electrode 26. The function of the pump 34 is to remove the trapped ions neutralized by the electrode 26 from the processing chamber 12 by evacuating the chamber. In a non-exclusive embodiment, the pump 34 has a capacity to pump about 500 liters per second from the processing chamber 12. In other embodiments, the pumping capacity can vary widely within a suitable range. By keeping the gap or space between the electrode 26 and the pump 34 relatively small, and the vacuum pressure high, the plasma can be prevented from occurring during the period when the RF source 30 is connected to the electrode 26.
[0045] The controller 24 is used to control the overall operation and processing sequence of the processing tool 10. In particular, the controller 24 is provided to manage and control the overall operation of the processing tool 10 by operating various components, including but not limited to switches S1 and S2, variable DC voltage source 28, RF source 30, pump 34, generation of plasma 36, supply of one or more reactant gases into the processing chamber 12, and substantially all other operations of the processing tool 10 described herein.
[0046] The controller 24 typically includes one or more non-transitory computer-readable media devices for storing system control software or code and one or more processors for executing the code. The term "non-transitory computer-readable media" is generally used to refer to media such as main memory, secondary memory, removable storage devices, and storage devices such as hard disks, flash memory, disk drive memory, CD-ROMs, and other forms of permanent memory, but not transient subjects such as carrier waves or signals. The processor may include a CPU or computer, multiple CPUs or computers, analog and / or digital input / output connections, motor controller boards, etc.
[0047] In some embodiments, a controller 24 running or executing system software or code controls all or at least most of the activities of the processing tool 10, including such things as controlling the timing of processing operations, the operating frequency and power of the RF source 30, the pressure within the processing chamber 12, the flow rate, concentration and temperature of any gases entering the processing chamber 12 and their relative mixing, the temperature of the substrate 18 supported by the substrate pedestal 16, and the like.
[0048] The controller 24 may also include a user interface (not shown). The user interface may include a display screen, a graphical software display indicating operating parameters and / or processing conditions of the processing tool 10, and a user input device, such as a pointing device, a keyboard, a touch screen, a microphone, etc., which allows a human operator to interface with the processing tool 10.
[0049] Information transmitted between the controller 24 and the various above-listed components of the processing tool 10 may be in the form of signals such as electronic, electromagnetic, optical or other signals capable of being sent and / or received via any signal-carrying communications link, and may be implemented using wire or cable, optical fiber, telephone lines, cellular telephone links, radio frequency links and / or other communications channels.
[0050] Precursor
[0051] Carbon is required to form a carbon layer on substrate 18. In various non-exclusive embodiments, the carbon is introduced into processing chamber 12 in the form of one or more precursor gases, such as acetylene (C2H2), methane (CH4), or some other gas that contains at least carbon. While such precursors contain the necessary carbon, they also typically contain hydrogen, which may be somewhat detrimental to the formation of various carbon layers as defined herein. As described herein, applicants have discovered a method for depositing carbon at virtually any desired thickness using processing tool 10 by modulating pulses and / or RF applied to electrode 26.
[0052] Processing Flow
[0053] refer to Figure 2 , a flow chart 50 of the operation of the processing tool 10 is shown, which illustrates a sequence for forming a carbon layer of nearly any desired thickness on the substrate 18. As described above, the sequence is primarily controlled and implemented by the controller 24.
[0054] In step 52, a carbon-containing precursor is introduced into the processing chamber 12. The precursor can be acetylene (C2H2), methane (CH4), or any other carbon-containing precursor. Depending on the precursor used, hydrogen or some other element may also be present in the processing chamber. As described below, the hydrogen or other element is at least partially removed in subsequent steps, and most of the carbon remains in the processing chamber 12.
[0055] In step 54, RF source 30 is activated and connected to electrode 26 via switch S1. As a result, plasma 36 is generated between substrate 18 and electrode 26 in processing chamber 12. Using the above-described precursors, the resulting plasma includes a mixture of carbon ions and hydrogen ions, both of which are positively charged.
[0056] In step 56, the RF source 30 is disconnected from the electrode 26 via switch S1. As a result, the plasma sheath enters an "afterglow" state, wherein a mixture of carbon and hydrogen ions is "suspended" within the processing chamber 12.
[0057] In step 58, switches S1 and S2 are switched to provide a relatively short duration negative pulse to electrode 26. As previously described, the lighter hydrogen ions move faster than the carbon ions. As a result, during the duration of the short pulse, a disproportionately greater percentage of hydrogen ions are attracted to electrode 26 relative to carbon ions. As a result, a majority of the carbon ions remain in processing chamber 12 after the negative pulse is completed.
[0058] In step 60, switches S1 and S2 are switched to provide a relatively long duration positive pulse to electrode 26. When the electrode is at a positive DC voltage and substrate pedestal 16 is biased to ground, positively charged carbon ions are accelerated toward and bombard substrate 18. By controlling the amplitude of the positive pulse as well as the bias of the substrate, the carbon ions can have sufficient energy to not only deposit on the surface of substrate 18, but also to implant into the bulk of substrate 18. As a result, carbon is formed on the surface of substrate 18 during the duration of the positive DC voltage pulse.
[0059] In decision 62, it is determined whether the carbon formed on substrate 18 has a desired thickness. If so, the above process stops.
[0060] In decision 64, it is determined whether there is sufficient carbon in process chamber 12. If there is sufficient carbon, another cycle of steps 56 through 62 is performed. On the other hand, if more carbon is needed, steps 52-62 are repeated.
[0061] The voltage applied to the electrode 26 is essentially a series of alternating negative and positive DC voltage pulses through multiple cycles of steps 58 and 60. For each negative pulse, hydrogen ions are removed from the plasma sheath, neutralized, and pumped out of the processing chamber 12. Between the negative pulses, most of the carbon ions bombard the substrate 18 during the positive pulses. By repeating this cycle multiple times, a carbon layer can be formed on the substrate 18 to almost any desired thickness.
[0062] Exemplary embodiments
[0063] Reference Figure 3, shows an exemplary timing diagram showing a repeating sequence of radio frequency (RF) interspersed with a series of negative and positive DC voltage pulses applied to the electrode 26. In this example, RF is initially applied for a duration of about 50 microseconds, as shown by reference numeral 72. Thereafter, a negative DC voltage pulse of about -1K volts is applied for a short period of time (e.g., 1 to 2 microseconds), as shown by reference numeral 74. Next, a positive DC voltage pulse having an amplitude of about +100 volts (+ / - 20%) and a duration of 5 microseconds is applied, as shown by reference numeral 76. By repeating the above sequence, the carbon and hydrogen ions in the plasma sheath are periodically replenished before each cycle to (a) remove most of the hydrogen ions and (b) bombard the substrate with most of the carbon ions. By repeating the cycles 72, 74 and 76, the resulting carbon layer can be deposited to almost any desired thickness.
[0064] It should be understood that Figure 3 The various time and voltage values provided in the graphs are illustrative and should not be construed as limiting in any way. For example:
[0065] The duration of the time period 72 during which RF is applied can vary widely. When RF is applied, the reactant gas molecules in the processing chamber 12 are broken and ionized. Therefore, the duration of the time period 72 depends at least in part on the desired degree or percentage of ion conversion. If a smaller percentage of ionization is desired or expected, the time period 72 is relatively short. On the other hand, if a high percentage or substantially all of the molecules are desired to be ionized, the duration of the time period 72 can be longer. Therefore, the duration of the time period 72 can vary over a wide range from one microsecond or less to more than 1 second, depending on the circumstances.
[0066] The duration and amplitude of the negative pulse 74 can also vary widely. During the negative pulse, the main goal is to balance the removal of as many low-quality ions (e.g., hydrogen) as possible from the plasma sheath without removing too many higher-quality carbon ions. (The main factor moving positive ions from the plasma sheath is the Bohn field, that is, when positive ions enter the plasma sheath, they will be accelerated by the E field of the sheath). By adjusting the negative amplitude, the electron temperature Te of the electrons of the ions in the plasma sheath can be indirectly controlled. The amplitude of the pulse 74 can therefore vary widely, for example from -100 volts to -5K volts, to control the rate at which hydrogen ions are swept out of the plasma sheath to reach the electrode 26. In addition, the longer the duration of the pulse 74, the more chances that carbon ions of larger mass are accelerated to sweep out of the plasma sheath and contact the electrode 26. Therefore, it is preferred to select the duration of the negative pulse 74 so that a significant percentage (e.g., 90%-99%) of hydrogen ions are removed. Once the desired threshold percentage is reached, the pulse is terminated. Similarly, it should be understood that this percentage range is exemplary and can be higher or lower. Thus, the duration of the pulses can range widely from 0.1 microseconds or less to 2 milliseconds or longer.
[0067] The duration and amplitude of the positive pulse 76 can also vary widely, again depending on the circumstances. The amplitude depends largely on the number and depth of sub-implantations required. Generally speaking, the higher the amplitude, the greater the energy of the carbon ions relative to the substrate, and the deeper the sub-implantations will be. Regarding the duration, the limiting factor is usually the charge accumulation on the substrate 18 during the bombardment. As the bombardment continues, the positive surface charge accumulates, increasing the potential of the substrate. Eventually, the voltage difference between the plasma sheath and the substrate becomes small enough that the carbon ions no longer have the energy required for sub-implantation. At this point, it is preferred to terminate the pulse 76. Therefore, the duration of the pulse can vary widely from 1 microsecond or less to 30 microseconds or more. The amplitude of the pulse 76 can also vary widely, for example, from +50 volts or less to +500 volts or more.
[0068] As previously described, the controller 24 is responsible for controlling the switches S1 and S2 to produce the desired duration of the RF application and the duration of the negative pulse 74 and the positive pulse 76 during the time period 72. The switch S1 is controlled to couple the electrode 26 to either (a) the RF source 30 or the switch S2, which is used to select the positive or negative terminal of the variable DC voltage source 28. The switch S2 thus controls the polarity and duration of the pulses 74 and 76, while the variable DC voltage source defines the amplitude.
[0069] Electrode 26
[0070] As mentioned above, the electrode 26 can also be used to neutralize ions removed from the plasma sheath by surface recombination neutralization. To achieve this function, the larger the surface area of the electrode 26, the better.
[0071] Reference Figure 4A and Figure 4B , a diagram of a non-exclusive embodiment of an electrode 26 is shown. In this particular embodiment, the electrode is circular in shape and substantially spans the processing chamber 12 in the X and Y directions. The electrode 26 also defines a grid of vertical grooves 80, which are drilled or otherwise formed through the thickness of the electrode in the Z direction. For example, the diameter of each groove 80 can range from 1 to 5 mm, the spacing ranges from 1.2 to 1.5 mm, and the height is about 4 mm. With this arrangement, the electrode 26 can have thousands of grooves 80, each of which increases the total surface area. With a larger surface area, more ions may contact the electrode 26 and be neutralized. It should be understood that the electrode 26 can be of any shape or have any features that can increase the total surface area. With this in mind, the embodiments shown and described herein are merely exemplary and should not be interpreted as being restrictive in any respect.
[0072] The aspect ratio (height to diameter) of the groove 80 can vary widely. As a general rule, the aspect ratio is preferably selected to provide sufficient surface area so that the vast majority of ions attracted to the electrode 26 are neutralized by surface recombination. If too many ions pass through the groove 80 without neutralization, the plasma actually "surrounds" the electrode 26 and forms above the electrode 26, which is undesirable. Therefore, the aspect ratio of the groove is preferably "sub-Bai", which means that the aspect ratio is selected to prevent the plasma sheath from surrounding the electrode 26. In a non-exclusive embodiment, the applicant has found that the aspect ratio of 4:1 is sufficient to neutralize the vast majority of ions, thereby preventing the wrap-around effect. The unneutralized ions are too few to produce the wrap-around effect and are usually swept away by the pump 34. However, it should be understood again that the groove 80 with an aspect ratio of 4:1 and a diameter of 1 mm is one of many examples that can complete Sub-Bai neutralization and prevent wrap-around. Therefore, grooves 80 with larger or smaller aspect ratios, diameters, and pitches can be used as long as they meet the Sub-Bai target.
[0073] However, the taller or thicker the electrode, the more difficult and expensive it is to manufacture. For example, in the case of an aspect ratio of 4:1, the grooves 80 of the electrode 26 are "subabysmal" in that they prevent the plasma sheath from wrapping around the electrode 26.
[0074] Thus far, electrode 26 has been characterized as an electrode for providing RF energy and negative and positive pulses into process chamber 12. However, it should be understood that this is by no means a requirement. Instead, a second electrode may be used for RF, while electrode 26 is used to apply negative and positive DC voltage pulses within process chamber 12.
[0075] Carbon layer
[0076] The above-described processes can be used to deposit a variety of different types of carbon layers, such as various types of diamond-like carbon (DLC) layers, such as hydrogenated amorphous carbon (aC:H) and hydrogenated tetrahedral amorphous carbon (ta-C:H) and tetrahedral amorphous carbon or "ta-C" and / or other types of carbon layers having primarily sp3 bonds, such as diamond layers, carbon layers having relatively large crystalline structures (1 to many microns) or relatively small crystalline structures (sub-nanometer size), carbon layers that primarily include sp2 bonds (such as graphite and so-called amorphous carbon that is often characterized as "dusty"), and carbon layers that have little or no sp3 and / or sp2 bonds. With the dust-like properties and minimal sp3 bonding at the nanometer scale, the amorphous carbon layer exerts significantly reduced surface stress on the underlying substrate, thereby significantly preventing the substrate from bending, warping and / or cracking.
[0077] "Hard masks" are often used as patterning masks in the semiconductor industry instead of other "soft" organic materials, such as polymer resists. "Soft" polymer masks are susceptible to degradation using common etchant gases used for wafer patterning (e.g., fluorine, chlorine, etc.). As a result, the patterned features on the semiconductor wafer are generally less precise. On the other hand, various carbon layers are significantly more stable, with very low and predictable etch rates, which makes such layers very suitable for use as hard masks in the semiconductor manufacturing industry. Compared to polymer resins, carbon hard masks exhibit significantly less degradation when exposed to fluorine and / or chlorine etching chemicals, resulting in more precise etching, finer geometries, and fewer processing defects.
[0078] Reference Figure 5 , a cross-section of an exemplary semiconductor wafer 90 is shown. The semiconductor wafer 90 includes a layer (or layers) 92, such as but not limited to an insulating layer, a polysilicon layer, a metallization layer, a silicon oxide layer, etc. (for simplicity, only one layer 92 is shown). The semiconductor wafer 90 also includes a carbon layer 94 formed over the one or more layers 92. In a non-exclusive embodiment, the carbon layer 94 is formed using a processing tool 10 as described herein. In various alternative embodiments, the carbon layer 94 is any of the above-described types of carbon layers. In other embodiments, the carbon layer 94 is a patterning mask for patterning and / or doping the underlying one or more layers 92.
[0079] Large-scale semiconductor wafer manufacturing
[0080] The ability to form carbon layer 94 in a conventional PECVD tool enables the use of any of the above-described types of carbon layers as hard masks, or for other types of layers, in large-scale industrial production of semiconductor wafers.
[0081] Reference Figure 6, a flow chart 100 is shown for using a carbon layer 94 as a patterning mask during large-scale industrial manufacturing of semiconductor wafers.
[0082] In an initial step 102, any layers 92 to be patterned and / or doped are formed on semiconductor wafer 90. Such layers may include, but are not limited to, silicon layers, polysilicon layers, metal layers (e.g., aluminum, copper, tungsten, etc.), insulating layers, oxide layers, and the like.
[0083] In step 104, an amorphous carbon layer 94 is formed on a semiconductor wafer as described herein. Amorphous carbon layer 94 may be any of the types of carbon described above.
[0084] In step 106 , carbon layer 94 is patterned to expose certain areas while covering other areas.
[0085] In step 108, the exposed areas on the semiconductor wafer are etched, doped, or both. The areas of semiconductor wafer 90 that remain covered by carbon layer 94 remain protected and are not etched and / or doped.
[0086] In decision 110, it is determined whether additional layers on semiconductor wafer 90 are to be etched and / or doped. If so, operations 102-108 are repeated. If not, the wafer will typically undergo other processing steps until fabrication is complete, as is well known in the semiconductor art.
[0087] Likewise, because the one or more carbon layers 94 may be formed and / or patterned in a processing tool 10 as described herein, the above-described processing may be performed on a large industrial scale.
[0088] Types of PECVD Tools
[0089] Various types of PECVD tools are known. Such PECVD tools include, but are not limited to, low pressure (LPCVD), ultra-high vacuum (UHVCVD), atomic layer deposition (ALD), plasma enhanced atomic layer deposition (PEALD), etc. In addition, the above-listed PECVD tools may also have a single processing chamber capable of processing one or more substrates or multiple processing chambers, each processing chamber capable of processing one or more substrates. Regardless of the type of PECVD tool or the number of chambers, each can be used to form a carbon layer as described herein on one or more substrates.
[0090] Alternative Implementation
[0091] Thus far, the present invention has been described in the context of (1) producing a mixture of carbon and hydrogen ions, (2) removing a significant percentage of the hydrogen ions from the mixture, and (3) depositing the majority of the remaining carbon ions onto a substrate surface. However, it should be understood that the present invention is by no means limited to hydrogen and carbon. Rather, the present invention can be used with any substance that (1) can be separated by atomic mass and (2) the remaining substance is to be deposited onto a workpiece.
[0092] Figure 7 is a flow chart 150 of the operations of a processing tool according to a non-exclusive embodiment of the present invention, illustrating a series of steps for forming a layer of other substances on a substrate.
[0093] In step 152, chemicals are introduced into the processing chamber 12. The chemicals include one or more species to be removed by mass separation and one or more species to be deposited on the substrate.
[0094] In step 154, plasma is generated in the processing chamber 12 by applying RF from the RF source 30 to the electrode 26. The plasma contains a mixture of ions of one or more species respectively included in the chemical species.
[0095] In step 156, the RF source is removed from the electrode 26. As a result, a mixture of ions, including those ions to be removed and those ions to be deposited on the workpiece, are suspended within the chamber.
[0096] In step 158, the ions to be removed are removed from the mixture by applying a varying DC voltage to electrode 26. During the pulses of the first polarity, the ions are removed from the mixture, either by being attracted to electrode 26 or repelled away from electrode 26, depending on the charge of the ions, the first polarity, and the position of electrode 26.
[0097] The remaining ions in the mixture are deposited onto the workpiece in step 160. During this step, the variable DC power supply may or may not provide a second pulse of a second polarity. In the case where no pulse or second polarity is used, only one polarity is turned on and off.
[0098] In step 162, it is determined whether the deposited layer on the workpiece has sufficient thickness. If so, the process is complete. If not, it is determined in step 164 whether the ions in the mixture need to be replenished. If not, steps 158 and 160 are repeated. If yes, steps 152-162 are repeated.
[0099] In another non-exclusive embodiment, the above process can be used to deposit a silicon nitride layer onto a workpiece. Using the above process, hydrogen, silicon, and nitride chemicals (e.g., nitrogen and SiH4) are introduced into the chamber, RF is applied, and a mixture of hydrogen, silicon, and nitrogen ions is produced. When a varying DC voltage is applied, the hydrogen ions are mostly removed from the mixture during the pulse of one polarity. As a result, silicon and nitrogen ions are deposited onto the workpiece between pulses of one polarity, regardless of whether a second pulse of a second polarity is used. In either case, a silicon nitride layer is formed.
[0100] It should be understood that the embodiments provided herein are exemplary only and should not be construed as being restrictive in any respect. Although only a few embodiments have been described in detail, it should be understood that the present application may be implemented in many other forms without departing from the spirit or scope of the disclosure provided herein. Therefore, the embodiments provided should be considered illustrative rather than restrictive, and are not limited to the details given herein, but may be modified within the scope and equivalents of the appended claims.
Claims
1. A deposition tool comprising: a substrate holder for holding a substrate within a processing chamber; and A controller configured to sequence: (a) providing a mixture of carbon ions and non-carbon ions in the processing chamber; (b) removing a majority of said non-carbon ions from said processing chamber; and (c) bombarding the substrate with a majority of carbon ions, wherein the bombardment of the carbon ions forms a carbon layer on the substrate; Wherein the non-carbon ions are removed by: applying a negative DC voltage pulse to an electrode in the process chamber positioned away from the substrate, the negative DC voltage pulse causing more of the non-carbon ions to be attracted to the electrode relative to the carbon ions; When the attracted non-carbon ions contact the surface of the electrode, the charge of the non-carbon ions is neutralized by surface recombination neutralization; as well as A vacuum is applied in the vicinity of the electrode to remove the neutralized non-carbon ions from the process chamber.
2. The deposition tool according to claim 1, wherein: The controller is further arranged to repeat at least (b) and (c) until a predetermined thickness of the carbon layer is reached.
3. The deposition tool according to claim 1, wherein: The controller is further configured to repeat (a) when the carbon ions in the process chamber need to be replenished.
4. The deposition tool of claim 1, wherein (a) further comprises: (i) introducing reactants containing carbon and non-carbon into the process chamber; (ii) generating a plasma from the reactants by providing radio frequency (RF) energy within the process chamber, the plasma comprising the carbon ions and the non-carbon ions; as well as (iii) levitating the plasma by removing the RF energy within the processing chamber.
5. The deposition tool of claim 1, wherein: Because the non-carbon ions have smaller atomic masses relative to the carbon ions, relatively more of the non-carbon ions are attracted to, contacted by, and neutralized by the electrode relative to the carbon ions.
6. The deposition tool of claim 1, wherein: The electrode includes a catalytic material to help neutralize the charge of the non-carbon ions.
7. The deposition tool of claim 1 , wherein bombarding the substrate with carbon ions in the process chamber further comprises: A positive DC voltage pulse is applied to an electrode in the process chamber positioned away from the substrate, the positive DC voltage pulse causing the carbon ions to accelerate toward and bombard the substrate.
8. A method of forming a carbon layer on a substrate in a processing chamber, the method comprising: (a) at least partially removing non-carbon ions from carbon ions in a processing chamber; (b) after (a), bombarding the substrate with a majority of the carbon ions in the process chamber; as well as (c) forming a carbon layer by the carbon ions bombarding the substrate, wherein a higher ratio of the carbon ions relative to the non-carbon ions bombarding the substrate than would be the case if the non-carbon ions were not at least partially removed from the processing chamber; and wherein the non-carbon ions are removed by: applying a negative DC voltage pulse to an electrode in the process chamber positioned away from the substrate, the negative DC voltage pulse causing more of the non-carbon ions to be attracted to the electrode relative to the carbon ions; When the attracted non-carbon ions contact the surface of the electrode, the charge of the non-carbon ions is neutralized by surface recombination neutralization; as well as A vacuum is applied in the vicinity of the electrode to remove the neutralized non-carbon ions from the process chamber.
9. The method of claim 8, wherein the substrate is a semiconductor wafer and the carbon layer is used as a patterning mask.
10. The method of claim 8, further comprising repeating (a) and (b) until the carbon layer has a desired thickness on the substrate.
11. The method according to claim 8, before executing (a), (b) and (c), further comprising: (i) introducing a precursor into the process chamber, the precursor comprising carbon and non-carbon elements; (ii) generating a plasma in the process chamber using an RF source, the plasma comprising the carbon ions and the non-carbon ions; as well as (iii) suspending the carbon ions and the non-carbon ions in the processing chamber by removing the RF source.
12. The method of claim 11, further comprising periodically repeating (i), (ii) and (iii) as needed to replenish the carbon ions in the process chamber.
13. A method for deposition, comprising: generating a mixture of first ions and second ions in a processing chamber; At least partially separating the first ions from the second ions in the mixture by applying a varying DC voltage to electrodes, the varying DC voltage causing: (a) removing more of the first ion from the mixture than the second ion; and (b) more of the second ion remains in the mixture than the first ion, Wherein the removal of more of the first ions from the mixture than the second ions is at least partially due to the first ions having a first mass and the second ions having a second mass different from the first mass.
14. The method of claim 13, wherein the first mass is lighter than the second mass, the lighter first mass causing the first ions to accelerate and move faster than the second ions in response to the varying DC voltage, thereby causing more of the first ions to be removed from the mixture than the second ions.
15. The method of claim 13, further comprising bombarding a surface of the workpiece with a majority of the second ions by providing a bias to the workpiece, the bias causing the second ions in the mixture to accelerate toward the surface of the workpiece.
16. The method of claim 13, wherein the varying DC voltage is a series of pulses including a first pulse of a first polarity and a second pulse of a second polarity.
17. The method according to claim 13, wherein: During a first pulse of a first polarity of the varying DC voltage, more of the first ions are removed from the mixture than the second ions.
18. The method of claim 13, further comprising bombarding a surface of a workpiece in the processing chamber with a majority of the second ions during a second pulse of a second polarity of the varying DC voltage, the second pulse of the second polarity causing the second ions to move in a direction toward the surface of the workpiece.
19. The method of claim 13, wherein the mixture is produced by: (c) introducing a chemical into the processing chamber; (d) generating a plasma in the process chamber from the chemical species by applying RF energy within the process chamber, the plasma comprising the first ions and the second ions; and (e) removing the RF energy after the plasma is generated.