Method for manufacturing molded product

By measuring and correcting the cutting line on the peripheral surface of the molded body, the problem of reducing the burr cutting accuracy caused by the inclination or shrinkage of the molded body is solved, and high-precision burr cutting is achieved, ensuring the quality of the finished product.

CN114521166BActive Publication Date: 2024-11-05KYORAKU CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080065783.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-02-10
Filing Date
2020-10-26
Publication Date
2024-11-05
Estimated Expiration
2040-10-26

AI Technical Summary

Technical Problem

In the prior art, when the molded body is inclined or unevenly shrinks, the burr cutting accuracy is difficult to ensure, resulting in inaccurate cutting or damage to the finished product.

Method used

By measuring the position of the circumference of the molded body, correcting the cutting line, and burr cutting along the corrected cutting line, ensuring that high-precision cutting can still be achieved when the molded body is inclined or unevenly shrinks.

Benefits of technology

Improve the accuracy and consistency of burr cutting, avoiding inaccurate burr cutting or finished product damage caused by tilting or shrinking of the molded body.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114521166B_ABST
    Figure CN114521166B_ABST
Patent Text Reader

Abstract

The present invention provides a method for manufacturing a molded product that can improve the cutting accuracy of burrs formed on the peripheral surface of a molded product. According to the present invention, a method for manufacturing a molded product is provided, which comprises a measuring step, a correction step, and a burr cutting step. In the measuring step, the position of at least one point on the peripheral surface of the molded product is measured in a state where the molded product is positioned. In the correction step, a standard cutting line is corrected according to the measurement result of the measuring step to determine a corrected cutting line. In the burr cutting step, the burrs formed on the peripheral surface of the molded product are cut along the corrected cutting line.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for producing a molded product. Background Art

[0002] Patent Document 1 discloses a technique for removing burrs formed on the peripheral surface of a molded body by cutting with a knife.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: Japanese Patent Application Publication No. 2020-1100 Summary of the invention

[0006] (Problems to be solved by the invention)

[0007] In the method of Patent Document 1, burrs are cut along a specific cutting line set by teaching. In this method, if positioning is performed with the molded body tilted or the shrinkage degree of the molded body is uneven, the accuracy of burr cutting may be reduced.

[0008] The present invention has been made in view of the above circumstances, and provides a method for manufacturing a molded product that can improve the cutting accuracy of burrs formed on the peripheral surface of a molded product.

[0009] (Technical solutions to solve problems)

[0010] According to the present invention, a method for manufacturing a molded product is provided, which comprises a measuring step, a correction step and a burr cutting step. In the measuring step, the position of at least one point on the peripheral surface of the molded body is measured when the molded body has been positioned. In the correction step, a standard cutting line is corrected according to the measurement result of the measuring step to determine a corrected cutting line. In the burr cutting step, the burrs formed on the peripheral surface of the molded body are cut along the corrected cutting line.

[0011] In the present invention, the position of at least one point on the circumferential surface of the molded body is measured, the cutting line is corrected based on the result, and the burrs are cut along the corrected cutting line. Therefore, even if the molded body is positioned in a tilted state or the shrinkage degree of the molded body is uneven, the burrs can be cut with high precision.

[0012] Various embodiments of the present invention are described below.

[0013] Preferably, in the above method, in the measuring step, at least one of the inclination and the expansion and contraction of the molded body is measured, and in the correcting step, at least one of the inclination and the expansion and contraction of the standard cutting line is corrected based on the measurement result of the measuring step.

[0014] Preferably, in the above method, the correction of the expansion / contraction amount is performed by parallel moving a part of the cutting line before correction.

[0015] Preferably, in the above method, the cutting of the burrs is performed by pressing a cutter for cutting the burrs against the peripheral surface while moving the cutter.

[0016] The method for manufacturing a molded product preferably comprises a burr cutting step and a burr removing step, wherein in the burr cutting step, burrs formed on the peripheral surface of the molded body are cut and dropped onto a burr treatment table, and in the burr removing step, the burrs are removed from the burr treatment table by rotating the burr treatment table.

[0017] Preferably, in the above method, in the burr removal step, the burr treatment table is rotated by 90 degrees or more.

[0018] Preferably, in the above method, the burr processing station comprises a molded body carrier and a burr receiving portion, and the burr receiving portion is arranged at a position adjacent to the molded body carrier and lower than the upper surface of the molded body carrier. In the burr cutting step, the burr is cut while the molded body is fixed on the upper surface of the molded body carrier, so that it falls onto the burr receiving portion.

[0019] Preferably, the method further comprises a positioning step before the burr cutting step, wherein the molded body is positioned by placing the molded body on a suction pad and moving the molded body while air is blown from the suction pad toward the molded body.

[0020] Preferably, in the above method, a positioning step is provided before the burr cutting step, in which the molded body is positioned by pushing the peripheral surface of the molded body with a positioning block to move the molded body, and the positioning block has a positioning surface abutting the peripheral surface of the molded body and an interference avoidance groove for avoiding interference with the burr.

[0021] Preferably, in the above method, in the burr cutting step, the burr is cut along a cutting line determined according to an inclination amount and an expansion / contraction amount of the molded body. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 middle, Figure 1 A is a three-dimensional view of the molded body 4, Figure 1 B is Figure 1 Magnified view of area B in A.

[0023] Figure 2 middle, Figure 2 A is a perspective view of a manufacturing system 10 for a molded product 4b. Figure 2 B is Figure 2Magnified view of area B in A.

[0024] Figure 3 middle, Figure 3 A is from Figure 2 B is a diagram in which the molded body carrier 3c, the burr receiving portion 3f and the pole 3g are removed. Figure 3 B is Figure 3 Magnified view of area B in A.

[0025] Figure 4 This is a diagram used to explain the loading process. Figure 2 A corresponds to the stereogram.

[0026] Figure 5 middle, Figure 5 A is Figure 4 Front view of Figure 5 B is Figure 5 Magnified view of area B in A.

[0027] Figure 6 middle, Figure 6 A is a diagram for explaining the positioning process. Figure 2 A corresponds to a stereogram, Figure 6 B is Figure 6 Magnified view of area B in A.

[0028] Figure 7 middle, Figure 7 A is a diagram for explaining the positioning process. Figure 2 A corresponds to a stereogram, Figure 7 B is for change Figure 7 A magnified view of area B in A.

[0029] Figure 8 middle, Figure 8 A~ Figure 8 D is an explanatory diagram of the cutting line determination process.

[0030] Fig. 9 middle, Fig. 9 A represents the cutting line before correction. Fig. 9 B indicates the corrected cutting line.

[0031] Fig.10 middle, Fig.10 A is a diagram for explaining the burr cutting process. Figure 2 A corresponds to a stereogram, Fig.10 B is Fig.10 Magnified view of area B in A.

[0032] Fig.11 middle, Fig.11 A is a diagram for explaining the burr cutting process. Figure 2 A corresponds to a stereogram, Fig.11 B is Fig.11 Magnified view of area B in A.

[0033] Fig.12 This is a diagram used to illustrate the burr removal process. Figure 2 A corresponds to the stereogram. DETAILED DESCRIPTION

[0034] The following describes the embodiments of the present invention. The various features shown in the embodiments shown below can be combined with each other. In addition, each feature can independently constitute an invention.

[0035] 1. Manufacturing system 10 for molded product 4b

[0036] like Figure 1-2 As shown, a system 10 for manufacturing a molded product 4 b according to an embodiment of the present invention includes a transfer robot 1 , a cutting robot 2 , and a burr treatment station 3 .

[0037] The manufacturing system 10 is used to form Figure 1 The burrs 4a of the peripheral surface 4c of the molded body 4 shown in the figure are cut to obtain a molded product 4b. The molded body 4 is a molded body formed using a pair of split molds, and can be any of a blow molded body, a vacuum molded body, an injection molded body, etc. The burrs 4a are formed on the joint surface of the split molds. In addition, the molded body 4 can be in a state just taken out of the split mold, or it can be in a state after the molded body obtained by opening the split mold has been pre-treated.

[0038] As a pre-treatment, a treatment of removing part of the burrs formed when molding using a split mold can be cited. In particular, when a molded body is formed by a method such as blow molding or vacuum molding in which a parison or a resin sheet is clamped by a split mold to form a molded body, large burrs are easily formed around the molded product 4b. Therefore, as a pre-treatment, it is preferable to remove the burrs formed during molding except for the burrs 4a.

[0039] The molded product 4b is, for example, a plate-shaped component such as a luggage board. The molded product 4b may be a final product directly, or the molded product 4b may be post-processed to form a final product.

[0040] The manipulators 1 and 2 are mounted on a robot arm of a mechanical device (Robot) not shown in the figure. The robot arm has a function of moving the manipulator 1. The robot arm may have a number of axes required to realize the various processes described below, and preferably has six or more axes.

[0041] The robot 1 is used to hold the molded body 4 formed in the previous process and move it to the burr treatment station 3. The robot 1 includes a base 1a, an arm 1b, and an adsorption pad 1c. The base 1a is mounted on the robot arm. The arm 1b is extended from the base 1a. The arm 1b is elongated and provided with a pair. The adsorption pad 1c is configured to adsorb the molded body 4 by vacuum suction. The adsorption pad 1c is provided on the arm 1b. A plurality of adsorption pads 1c are provided on each arm 1b (three are provided in the present embodiment).

[0042] In one example, among the three suction pads 1c provided on each arm 1b, the two suction pads 1c on the front end 1b1 side are connected to the first vacuum system, and the remaining suction pad 1c is connected to the second vacuum system. With such a configuration, if the molded body 4 is of a size that can be sucked by the three suction pads 1c, the molded body 4 can be sucked by activating the first and second vacuum systems; if the molded body 4 is small and cannot be sucked by the three suction pads 1c, only the first vacuum system can be activated to suck the molded body 4 with the two suction pads 1c on the front end side. Thus, air leakage when sucking a small molded body 4 can be prevented.

[0043] The manipulator 2 includes a base 2a, a tool 2b, and a distance measuring device 2c. The tool 2b and the distance measuring device 2c are fixed to the base 2a. The tool 2b is, for example, an ultrasonic knife, which is used to move the tool 2b along the peripheral surface 4c of the molded body 4 at the boundary between the burr 4a and the molded product 4b to cut the burr 4a. The tool 2b can apply force in a direction orthogonal to the width direction of the blade of the tool 2b, thereby being able to move the tool 2b while pressing it against the peripheral surface 4b to cut the burr 4a. The force can be applied by a spring or a cylinder mechanism. The distance measuring device 2c is used to measure the distance between the distance measuring device 2c and the peripheral surface 4c of the molded body 4. Using the distance measuring device 2c, when the molded body 4 is fixed to the burr treatment table 3, distance measurement is performed at multiple measuring points along the peripheral surface 4c of the molded body 4, and the coordinates of the multiple measuring points along the peripheral surface 4c of the molded body 4 can be obtained, thereby being able to calculate the inclination and expansion of the molded body 4. The robot 2 is configured to cut the burrs 4a along a cutting line determined according to the calculated inclination and expansion / contraction amount. With such a configuration, even if the molded body 4 is fixed to the burr treatment table 3 in an inclined state, or when the deviation of the expansion / contraction amount of the molded body 4 is large, the burrs 4a can be cut with high precision.

[0044] The number of the robot arms 2 may be one or more than two. By using a plurality of robot arms 2 to perform distance measurement and cutting, it is possible to achieve high-speed processing.

[0045] The burr treatment station 3 includes a base 3a, a delivery suction unit 3b, a molded product placement body 3c, a fixed suction unit 3d, a positioning unit 3e, a burr receiving portion 3f, a rod 3g, and a rotating unit 3h.

[0046] The rotating unit 3h includes a rotating drive unit 3h1 and a bearing unit 3h2. The base 3a is clamped by the rotating drive unit 3h1 and the bearing unit 3h2, and is configured to be rotationally driven by the rotating drive unit 3h1 while being axially supported by the bearing unit 3h2. The angle of the rotating axis of the rotation drive relative to the horizontal plane is preferably 45 degrees or less, more preferably 30 degrees or less, and further preferably 5 degrees or less. Specifically, the angle is, for example, 0, 5, 10, 15, 20, 25, 30, 35, 40, 45 degrees, and may also be within the range between any two of the exemplified values.

[0047] The transfer adsorption unit 3b includes a driving unit 3b1 and an adsorption pad 3b2. The driving unit 3b1 is preferably a cylinder mechanism, and includes a fixed portion 3b11 fixed to the base 3a and a movable portion 3b12 configured to be movable (preferably slidable) relative to the fixed portion 3b11. The adsorption pad 3b2 is configured to adsorb the molded body 4 by vacuum suction and is fixed to the movable portion 3b12.

[0048] The molded body carrier 3c is preferably fixed to the wall of the base 3a, and the burrs 4a are cut off in a state where the molded body 4 is placed and fixed on the molded body carrier 3c. The molded body 4 is fixed to the molded body carrier 3c by the fixed suction unit 3d.

[0049] A plurality of fixed adsorption units 3d are arranged at positions where the molded body 4 can be adsorbed. The fixed adsorption units 3d are preferably arranged at positions adjacent to the outer periphery of the molded body 4. In this case, the molded body 4 is less likely to be misaligned when the burrs 4a are cut. Each fixed adsorption unit 3d includes a support 3d1 and an adsorption pad 3d2. The adsorption pad 3d2 is fixed to the support 3d1, and the support 3d1 is fixed to the base 3a. The adsorption pad 3d2 is configured to adsorb the molded body 4 by vacuum suction.

[0050] like Figure 2-3 As shown, a plurality of positioning units 3e are arranged along the outer periphery of the molded body 4. Each positioning unit 3e includes a pedestal 3e1, a driving unit 3e2, and a positioning block 3e3. The pedestal 3e1 is fixed to the base 3a. The driving unit 3e2 is preferably a linear slider mechanism, including a fixed portion 3e21 fixed to the pedestal 3e1 and a movable portion 3e22 configured to be movable (preferably slidable) relative to the fixed portion 3e21. The positioning block 3e3 is fixed to the movable portion 3e22. The molded body 4 is moved by moving the positioning block 3e3 with the driving unit 3e2 and the positioning block 3e3 is pressed against the peripheral surface 4c of the molded body 4, thereby positioning the molded body 4. The positioning block 3e3 includes a positioning surface 3e31 that abuts against the peripheral surface 4c of the molded body 4, and an interference avoidance groove 3e32 for avoiding interference with the burr 4a.

[0051] like Figure 2As shown in FIG. 1B, the burr receiving portion 3f is arranged at a position adjacent to the molded body carrier 3c and lower than the upper surface 3c1 of the molded body carrier 3c. Thus, the burr 4a can be cut and dropped onto the burr receiving portion 3f while the molded body 4 is fixed on the upper surface of the molded body carrier 3c. Wiring and piping required for driving various units are arranged around the molded body carrier 3c, but if the cut burr 4a is entangled with the wiring or piping, it may cause a malfunction. In this embodiment, the occurrence of malfunctions can be suppressed by causing the burr 4 to fall onto the burr receiving portion 3f. The burr 4a on the burr receiving portion 3f can be removed by rotating the burr treatment table 3 by the rotating unit 3h. A conveyor belt not shown in the figure can also be arranged below the burr treatment table 3. In this case, the burr 4a can fall onto the conveyor belt and be moved to the exhaust gas or recovery line by the conveyor belt.

[0052] like Figure 2 As shown in FIG. 2B , the burr receiving portion 3f is arranged at the same height as or higher than the moving portion 3e22. This can prevent the falling burrs 4a from getting caught on the moving portion 3e22. The position where the burr receiving portion 3f is fixed is not limited, and the burr receiving portion 3f can be fixed to the base 3a or to the molded body carrier 3c, for example.

[0053] like Figure 2 As shown in B, the rod 3g is fixed to the base 3a at a position adjacent to the positioning block 3e3. Fig.10 As shown in FIG. 2B , when the molded body 4 is placed on the upper surface 3c1 of the molded body carrier 3c, the upper end 3g1 of the rod 3g is located higher than the burr 4a. Fig.10 As shown in FIG. 2B , when cutting the burr 4a, the positioning block 3e3 is moved back so that the front end 3e33 of the positioning block 3e3 is located at a position farther away from the burr 4a than the rod 3g. This can prevent the burr 4a from getting stuck in the positioning block 3e3. The rod 3g is preferably cylindrical, but can be other shapes as long as it can achieve the above purpose.

[0054] 2. Manufacturing method of molded products

[0055] The following describes a method for manufacturing the molded product 4b using the manufacturing system 10. The method includes a loading step, a positioning step, a cutting line determining step, a burr cutting step, a unloading step, and a burr removing step. Each step is described below.

[0056] 2-1. Importing process

[0057] like Figure 2 to Figure 5 As shown, in the carrying-in process, the molded body 4 is carried into the burr treatment station 3 using the robot 1. The specific process is as follows.

[0058] In the initial state, if Figure 2As shown in B, the suction pad 3b2 of the transfer suction unit 3b rises, and the height difference between the upper surface of the suction pad 3b2 and the upper surface 3c1 of the molded product carrier 3c is greater than the total height of the arm 1b and the suction pad 1c.

[0059] First, the molded body 4 placed on a mounting table (not shown) provided outside the burr treatment table 3 is Figure 2 The suction pad 1c of the robot 1 shown in A is sucked, and the robot 1 is moved in this state to move the molded body 4 on the suction pad 3b2. Figure 5 As shown in B, the robot 1 is moved so that the arm 1b is disposed between the molded object 4 and the molded object mounting body 3c. Thus, since the molded object 4 is located above the arm 1b, it is possible to prevent the molded object 4 from being accidentally separated from the suction pad 1c.

[0060] Thereafter, the molded body 4 is sucked by the suction pad 3b2, and at the same time, the suction of the suction pad 1c is released, so that the arm 1b is separated from the space between the molded body 4 and the molded body mounting body 3c.

[0061] 2-2. Positioning process

[0062] like Figure 6-7 As shown, in the positioning step, the molded body 4 is positioned by moving the molded body 4 on the burr treatment table 3. The specific steps are as follows.

[0063] First, if Figure 6 As shown in B, when the positioning block 3e3 of the positioning unit 3e is retreated, the driving Figure 2 The driving unit 3b1 shown in B lowers the suction pad 3b2, causing the molded body 4 to contact the suction pad 3d2, thereby releasing the suction of the suction pad 3b2. In this state, the molded body 4 is placed on the suction pad 3d2. Figure 5 As shown in B, the upper surface 3d21 of the adsorption pad 3d2 is located slightly higher than the upper surface 3c1 of the molded body carrier 3c, so the molded body 4 does not contact the upper surface 3c1 of the molded body carrier 3c, or even if it contacts the upper surface 3c1 of the molded body carrier 3c, at least part of the load of the molded body 4 will be applied to the adsorption pad 3d2.

[0064] In this state, when the molded body 4 is moved in the in-plane direction (i.e., in the in-plane direction of the surface formed by the plurality of adsorption pads 3d2), the molded body 4 slides on the adsorption pads 3d2, but when the load of the molded body 4 is applied to the adsorption pads 3d2, the friction between the molded body 4 and the adsorption pads 3d2 increases, and the adsorption pads 3d2 may be deformed when the molded body 4 is moved. If the adsorption pads 3d2 are deformed, the adsorption and fixing of the molded body 4 by the adsorption pads 3d2 may be insufficient.

[0065] Therefore, in this embodiment, air is blown from the upper surface 3d21 of the suction pad 3d2 toward the molded body 4 to reduce the load applied by the molded body 4 to the suction pad 3d2, and the molded body 4 is moved in this state. As a result, the friction between the molded body 4 and the suction pad 3d2 is reduced, and deformation of the suction pad 3d2 when the molded body 4 moves can be suppressed.

[0066] The molded body 4 can be moved using the positioning unit 3e. Specifically, the drive Figure 3 The driving unit 3e2 shown in A causes the positioning block 3e3 to move toward the peripheral surface 4c of the molded body 4, as shown in FIG. Figure 7 As shown in FIG. 2B , the molded body 4 can be moved by making the positioning surface 3e31 of the positioning block 3e3 abut against the peripheral surface 4c of the molded body 4 and pressing the peripheral surface 4c. In addition, the molded body 4 can be positioned by clamping the molded body 4 with the positioning blocks 3e3 of the plurality of positioning units 3e. In addition, during positioning, since the burrs 4a are accommodated in the interference avoidance grooves 3e32, it is possible to prevent the burrs 4a from hindering the positioning.

[0067] After the positioning block 3e3 is positioned, the following steps may be provided: the suction pad 3b2 is raised to lift the molded body 4 with the suction pad 3b2, so that the molded body 4 is separated from the suction pad 3d2, and then the suction pad 3b2 is lowered. By performing this step, even if the suction pad 3d2 is deformed during the positioning of the molded body 4, the suction pad 3d2 can be restored to its original shape when the molded body 4 is lifted by the suction pad 3b2.

[0068] Next, the molded body 4 is adsorbed by the adsorption pad 3d2 to fix the position of the molded body 4. In addition, the molded body 4 is adsorbed by the adsorption pad 3d2, so that the molded body 4 is pressed against the upper surface 3c1 of the molded body carrier 3c. With such a configuration, the molded body 4 can be stably held on the upper surface 3c1 of the molded body carrier 3c.

[0069] Afterwards, drive Figure 3 The driving unit 3e2 shown in A causes the positioning block 3e3 to retreat to leave the peripheral surface 4c of the molded body 4. Fig.10 As shown in FIG. 3B, the positioning block 3e3 is moved back so that the front end 3e33 of the positioning block 3e3 is located further away from the burr 4a than the rod 3g. This prevents the burr 4a cut off in the following burr cutting process from getting stuck in the positioning block 3e3.

[0070] 2-3. Cutting line determination process

[0071] The cutting line determination process includes the measurement process and the correction process. Figure 8As shown, in the measuring step, the position of at least one point on the peripheral surface 4c of the molded body 4 is measured while the molded body 4 is positioned. In the correcting step, the standard cutting line L0 is corrected based on the measurement result of the measuring step to determine the corrected cutting line L2. Figure 8 As shown, in the cutting line determination process, with the molded body 4 fixed on the burr processing table 3, the coordinates of multiple measurement points along the circumferential surface 4c of the molded body 4 are measured, and the inclination and expansion and contraction of the molded body 4 are calculated based on the measured coordinates. Based on the calculated inclination and expansion and contraction, the corrected cutting line L2 for cutting the burr 4a is determined.

[0072] The coordinates can be measured using the distance measuring device 2c. Since the distance measuring device 2c knows its own coordinates and orientation, the coordinates of the measurement point can be obtained by measuring the distance from the distance measuring device 2c to the measurement point on the peripheral surface 4c.

[0073] Here, the method of determining the cutting line is described in detail.

[0074] In the mechanical device equipped with the robot 2, according to Figure 8 The coordinate correction of the XY axis shown in B is used as the standard cutting line L0 as the reference and stored. The standard cutting line L0 can be determined by teaching the cutting line to the mechanical device using a standard workpiece. As the standard workpiece, a cooled molded body can be used, or a newly formed molded body can be used. When the former is used, there is an advantage that the size does not change during the teaching operation. When the latter is used, since the temperature and size are similar to the molded body during the actual burr cutting process, there is an advantage that the burr cutting accuracy can be improved. Therefore, it is preferred to first use a cooled molded body for teaching to preliminarily determine the standard cutting line, and then use the newly formed molded body to fine-tune the preliminarily determined standard cutting line to improve accuracy. In addition, in the standard cutting line L0, it is preferred to configure the standard cutting line L0 in such a way that the intersection of the straight line parallel to the X-axis and the straight line parallel to the Y-axis coincides with the origin of the XY coordinates.

[0075] In addition, the standard cutting line L0 can also be changed according to the historical data of the past cycles. For example, the corrected cutting line L2 just before can be used as the standard cutting line L0 for the next cycle, or the cutting line obtained by taking the average of the corrected cutting lines L2 of the past several times can be used as the standard cutting line L0 for the next cycle.

[0076] The standard cutting line L0 is the cutting line when the molded body 4 is fixed to the burr treatment table 3 without tilting in the plane and the size of the molded body 4 is the standard size. However, in reality, there are cases where the molded body 4 is tilted when fixed to the burr treatment table 3, and there are also deviations in the amount of expansion and contraction when the molded body 4 is cooled after molding. Therefore, if the burr 4a is cut along the standard cutting line L0, there is a case where the burr 4a is not removed sufficiently or the molded product 4b is damaged. Therefore, it is necessary to correct the standard cutting line L0 according to the tilt and expansion of the molded body 4. Below, the correction method of the cutting line is explained by taking the case where the molded body 4 is fixed to the burr treatment table 3 in a tilted state and the molded body 4 is smaller than the molded body 4d of the standard size as an example.

[0077] First, get Figure 8 Coordinates of measurement points A to C are shown in A. From the coordinates of measurement points A to C, a straight line Lx connecting measurement points A and B and a straight line Ly passing through measurement point C and orthogonal to straight line Lx are obtained.

[0078] Then, if Figure 8 As shown in C, the XY axis of the mechanical device is rotated so that the XY axis of the mechanical device coincides with the straight line Lx, Ly. As a result, the standard cutting line L0 is also rotated to become the corrected cutting line L1.

[0079] Next, get Figure 8 Coordinates of measurement points D and E are shown in A. From the coordinates of measurement points D to E, the expansion and contraction amounts of the molded body 4 in the X-axis direction and the Y-axis direction are obtained.

[0080] Then, if Figure 8 D, the corrected cutting line L1 is expanded or contracted according to the expansion or contraction amount in the X-axis direction and the Y-axis direction, thereby obtaining the corrected cutting line L2. It should be noted that, instead of obtaining the expansion or contraction amount in each of the two axes, one expansion or contraction amount may be obtained, and the corrected cutting line L1 may be similarly expanded or contracted according to the expansion or contraction amount to obtain the corrected cutting line L2.

[0081] The corrected cutting line L2 is a cutting line determined based on the amount of inclination and the amount of expansion and contraction of the molded body 4. Therefore, by cutting the burrs 4a along the corrected cutting line L2, the burrs 4a can be appropriately removed.

[0082] In the above description, both the inclination and the expansion of the molded body 4 are measured, and both the inclination and the expansion of the standard cutting line L0 are corrected based on the measurement results. However, only one of the inclination and the expansion may be measured and corrected.

[0083] In addition, the correction of the expansion and contraction amount can be performed by multiplying the X-coordinate and Y-coordinate values ​​of the point group of the cutting line before correction (for example, the standard cutting line L0 or the cutting line after correction L1) by the coefficient corresponding to the expansion and contraction amount. However, there are cases where the control program cannot change the X-coordinate and Y-coordinate values ​​at the same time or cannot multiply by the coefficient. In this case, the correction of the expansion and contraction amount can be performed by parallel moving a part of the cutting line before correction.

[0084] use Fig. 9 The correction of the expansion and contraction amount by parallel translation will be described in further detail.

[0085] Fig. 9 A represents the cutting line L before correction. The cutting line L is a line that smoothly connects the points A to T, and the cutting line L also moves when the points A to T move. Fig. 9 A~ Fig. 9 The left-right direction of B is the X-axis direction, and the up-down direction is the Y-axis direction. The cutting line L is composed of two lines Ly0 and Ly1 parallel to the Y-axis, two lines Lx0 and Lx1 parallel to the X-axis, a curved line Lc1 connecting lines Ly0 and Lx1, and a curved line Lc2 connecting lines Ly1 and Lx1.

[0086] Here, the position of the peripheral surface of the molded body 4 was measured by the above method. The result showed that the molded body 4 was smaller by 0.2 mm in the X-axis direction and by 0.1 mm in the Y-axis direction compared with the molded body 4 d of the standard size.

[0087] At this time, without moving line Ly0, line Ly1 is moved -0.2 mm in the X-axis direction, so that expansion and contraction in the X-axis direction can be achieved. Fig. 9 As shown in B, the line Ly1 can be moved by moving the X coordinates of points D to H (underlined points) close to the line Ly1 by -0.2 mm. The points to be moved can be adjusted appropriately. For example, point D may not be moved or point I may be moved.

[0088] In addition, without moving line Lx0, line Lx1 is moved -0.1 mm in the Y-axis direction to achieve expansion and contraction in the Y-axis direction. Fig. 9 As shown in B, the line Lx1 can be moved by moving the Y coordinates of points I to N (points in bold) close to the line Lx1 by -0.1 mm. The points to be moved can be adjusted appropriately. For example, point I may not be moved or point O may be moved.

[0089] By adopting such a method, the amount of expansion and contraction can be easily corrected.

[0090] On the other hand, when the above method is used, there are cases where the parts that are not parallel to both the X-axis and the Y-axis (hereinafter referred to as non-parallel parts, such as the bending lines Lc1 and Lc2) cannot be properly corrected. However, the cutting of the burrs 4a can be performed in the following manner: the tool 2b is forced in a direction orthogonal to the direction in which the cutting line extends (in other words, the blade width direction of the tool 2b), so that the tool 2b is pressed against the peripheral surface 4b1 and moved at the same time. By using such a method, even in non-parallel parts, the tool 2b can be moved along the peripheral surface 4b1, and the burrs 4a can be cut with good accuracy.

[0091] 2-4. Burr cutting process

[0092] like Figure 10-11 As shown, in the burr cutting step, the burrs 4a formed on the peripheral surface 4c of the molded body 4 are cut and dropped onto the burr treatment table 3. Thus, the molded body 4 is separated into the burrs 4a and the molded product 4b.

[0093] The burrs 4a can be cut along the corrected cutting line L2 determined in the cutting line determination process. Fig.11 As shown in FIG. 2B , the burrs 4a fall onto the burr receiving portion 3f. The molded product 4b is placed on the molded product carrier 3c and is adsorbed by the adsorption pad 3d2. The peripheral surface 4b1 of the molded product 4b is aligned with the peripheral surface 4c of the molded product 4.

[0094] The burrs 4a may be annular or non-annular. When the cut burrs 4a are thin and light, the burrs 4a may not fall but adhere to the molded product 4b by static electricity or the like. Such burrs 4a may fall to a place where the molded product 4b should not fall after being removed from the burr treatment table 3. Therefore, it is preferable to cut the burrs 4a in such a way that the thin and light burrs 4a are not separated from the thick and heavy burrs 4a.

[0095] 2-5. Unloading process

[0096] In the unloading step, the molded product 4 b is unloaded from the burr treatment station 3 .

[0097] Specifically, the suction pad 3d2 is released from the molded product 4b, and the molded product 4b is sucked by the suction pad 3b2, so that the suction pad 3b2 is lifted. Next, the arm 1b is inserted into the space between the molded product 4b and the molded product carrier 3c with the suction pad 1c facing upward (see Figure 4 ). Next, the suction pad 3b2 releases the suction of the molded product 4b, and the suction pad 1c sucks the molded product 4b. Next, in this state, the molded product 4b is moved out of the burr treatment station 3 by the moving robot 1.

[0098] 2-6. Burr removal process

[0099] like Fig.12 As shown, in the burr removal process, the burr 4a is removed from the burr treatment table 3 by rotating the burr treatment table 3. As a result, the burr 4a placed on the burr receiving portion 3f falls down under the action of gravity and is removed. The fallen burr 4a is transported by a conveyor belt or the like and is recovered or disposed of.

[0100] The burr treatment table 3 is driven and rotated by the rotation drive part 3h1 while being axially supported by the bearing part 3h2. The rotation angle of the burr treatment table 3 is preferably 90 degrees or more, for example, 90 to 270 degrees, preferably 120 to 240 degrees, specifically, for example, 90, 120, 150, 180, 210, 240, 270 degrees, and can also be within the range between any two of the exemplified values. By rotating the burr treatment table 3 at such an angle, the burr 4a can be dropped from the burr treatment table 3 even when the burr 4a is annular or when the burr 4a is elongated and easily caught on other parts.

[0101] The burr removal process may be performed once each time the burr cutting process is performed, or may be performed once each time the burr cutting process is performed a plurality of times.

[0102] (Explanation of symbols)

[0103] 1: moving robot, 1a: base, 1b: arm, 1b1: front end, 1c: suction pad, 2: cutting robot, 2a: base, 2b: tool, 2c: distance measuring device, 3: burr treatment table, 3a: base, 3b: transfer suction unit, 3b1: drive unit, 3b11: fixed part, 3b12: moving part, 3b2: suction pad, 3c: molded body carrier, 3c1: upper surface, 3d: fixed suction unit, 3d1: support, 3d2: suction pad, 3d21: upper surface, 3e: positioning unit, 3e1: table Seat, 3e2: driving unit, 3e21: fixing part, 3e22: moving part, 3e3: positioning block, 3e31: positioning surface, 3e32: interference avoidance groove, 3e33: front end, 3f: burr receiving part, 3g: rod, 3g1: upper end, 3h: rotating unit, 3h1: rotating driving part, 3h2: bearing part, 4: molded body, 4a: burr, 4b: molded product, 4b1: peripheral surface, 4c: peripheral surface, 4d: molded body, 10: manufacturing system, L0: standard cutting line, L1: corrected cutting line, L2: corrected cutting line.

Claims

1. A method for manufacturing a molded product, It has a measuring process, a correction process, and a burr cutting process. In the measuring step, the position of at least one point on the peripheral surface of the molded body is measured while the molded body is positioned. In the correction step, the standard cutting line is corrected according to the measurement result of the measurement step, and the corrected cutting line is determined. In the burr cutting step, the burrs formed on the peripheral surface of the molded body are cut along the corrected cutting line. In the measuring step, the expansion and contraction amount of the molded body is measured. In the correction step, the expansion and contraction amount of the standard cutting line is corrected according to the measurement result of the measurement step. The correction of the expansion and contraction amount is performed by parallel moving a part of the cutting line before correction.

2. The method for producing a molded article according to claim 1, wherein: The cutting of the burrs is performed by pressing a cutter for cutting the burrs against the peripheral surface while moving the cutter.

3. A method for manufacturing a molded product, It has burr cutting process and burr removing process. In the burr cutting step, the burrs formed on the peripheral surface of the molded body are cut and dropped onto the burr processing table. In the burr removal step, the burr is removed from the burr treatment table by rotating the burr treatment table. In the burr removal step, the burr treatment table is rotated more than 120 degrees. In the burr cutting step, the burr is cut along a cutting line determined according to the inclination amount and the expansion and contraction amount of the molded body.

4. The method for producing a molded article according to claim 3, wherein: The burr treatment station comprises a molded body carrier and a burr receiving portion. The burr receiving portion is provided at a position adjacent to the molded body carrier and lower than the upper surface of the molded body carrier. In the burr cutting step, the burr is cut and dropped onto the burr receiving portion while the molded body is fixed on the upper surface of the molded body carrier.