A cathode plate for titanium-aluminum-titanium electrolytic zinc

By covering the electrolytic zinc cathode plate with a titanium layer and applying corrosion-resistant paint, combined with the design of conductive rods and insulating edge strips, the problem of poor corrosion resistance of the cathode plate is solved, the service life is extended, the production cost is reduced, and the electrolysis efficiency is improved. Economic Benefits of the Zinc Industry.

CN114703507BActive Publication Date: 2024-10-18LUOYANG SUNRUI TI PRECISION CASTING
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202210251694.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-15
Publication Date
2024-10-18
Estimated Expiration
2042-03-15

AI Technical Summary

Technical Problem

The existing cathode plates in the electrolytic zinc industry have poor corrosion resistance and short service life, which causes the electrolytic zinc plant to need frequent replacement, reducing production efficiency and increasing costs.

Method used

Titanium aluminum titanium electrolytic zinc cathode plate is used. By covering the aluminum plate with a titanium layer and applying corrosion-resistant paint and plastic tape, a multi-layer structure is formed to improve corrosion resistance, combined with the design of conductive rods and insulating edge strips.

Benefits of technology

The service life of the cathode plate is significantly extended, production efficiency is improved, production costs are reduced, and economic benefits are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114703507B_ABST
    Figure CN114703507B_ABST
Patent Text Reader

Abstract

A titanium-aluminum-titanium electrolytic zinc cathode plate includes a plate panel and a conductive rod, the conductive rod is located on one side of the plate panel along the height direction, the plate panel includes a core aluminum plate and a surface titanium layer, the surface titanium layer covers two sections of the core aluminum plate, and there is a strip gap between the edge of the surface titanium layer close to the conductive rod and the conductive rod, and corrosion-resistant paint is applied on the strip gap. The surface of the corrosion-resistant paint is provided with a plastic sealing tape, and a plurality of plastic sealing holes are opened on the plate panel located between the plastic sealing tapes on both sides, and the plastic sealing tapes on both sides cover the two ends of the plastic sealing holes respectively, so as to enhance the bonding force between the plastic sealing tape and the plate panel. Compared with the existing cathode plate made of pure aluminum, the titanium layer on the surface of the present invention has good corrosion resistance in the electrolytic solution, and is protected by the corrosion-resistant paint and the plastic sealing tape, which can increase the service life of the electrolytic zinc cathode plate, improve production efficiency, solve the problem of short service life of the cathode plate, reduce the production cost of the factory, and improve economic benefits.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of electrolytic zinc cathode plates, in particular to a titanium-aluminum-titanium electrolytic zinc cathode plate. Background Art

[0002] The cathode plate of electrolytic zinc is the main equipment in the electrolytic zinc industry. At present, the cathode plates of pure aluminum are used in the electrolytic systems of electrolytic zinc production. Under the action of direct current, zinc flakes are deposited on the surface of the cathode plates. The zinc flakes are peeled off manually or mechanically, and then melted and cast to obtain the final product - zinc ingots. In the prior art, the cathode plates have poor corrosion resistance and short service life, usually 8-18 months, which is a major obstacle to the development of the electrolytic zinc industry. Electrolytic zinc plants have to regularly replace new cathode plates, which reduces the production efficiency of the factory and increases production costs. Summary of the invention

[0003] The purpose of the present invention is to provide a titanium-aluminum-titanium electrolytic zinc cathode plate, which can increase the service life of the cathode plate, improve the production efficiency of the factory, reduce the production cost of the factory, and improve the economic benefits.

[0004] The technical solution adopted by the present invention to solve the above technical problems is: a titanium-aluminum-titanium electrolytic zinc cathode plate, including a plate panel and a conductive rod, the plate panel is a rectangular flat plate structure, the conductive rod is a rectangular long strip structure, the conductive rod is located on one side of the plate panel along the height direction, the length direction of the conductive rod is parallel to the length direction of the plate panel, a length×width side of the conductive rod is welded to a length×width side of the plate panel, the plate panel includes a core aluminum plate and a surface titanium layer, the surface titanium layer covers two length×height planes of the core aluminum plate, and a strip-shaped portion is formed between the edge of the surface titanium layer close to the conductive rod and the conductive rod. The strip-shaped gap is parallel to the length direction of the conductive rod, the width of the strip-shaped gap along the height direction of the plate panel is 3 to 5 mm, the strip-shaped gap is coated with corrosion-resistant paint, and the surface of the corrosion-resistant paint is provided with a plastic sealing tape, one side of the plastic sealing tape extends to the side of the conductive rod facing the plate panel, and the other side of the plastic sealing tape extends to the surface titanium layer, and a plurality of plastic sealing holes are opened on the plate panel between the plastic sealing tapes on both sides, the axis of the plastic sealing holes is parallel to the width direction of the plate panel, and the plurality of plastic sealing holes are arranged alternately at intervals, and the plastic sealing tapes on both sides cover the two ends of the plastic sealing holes respectively, so as to enhance the bonding force between the plastic sealing tape and the plate panel.

[0005] Preferably, a conductive head and a lifting ring are connected to the conductive rod.

[0006] Preferably, insulating edge strips are provided on both sides of the width×height of the electrode panel.

[0007] According to the above technical solution, the beneficial effects of the present invention are:

[0008] In the present invention, both sides of the core aluminum plate of the cathode panel are covered with a surface titanium layer to form a multi-layer structure of "titanium, aluminum and titanium". Compared with the existing cathode plate made of pure aluminum, the surface titanium layer has good corrosion resistance in the electrolytic solution and is protected by corrosion-resistant coating and plastic sealing tape. Therefore, the service life of the electrolytic zinc cathode plate can be greatly improved, which is helpful to improve production efficiency, solves the problem of short service life of traditional cathode plates, and can reduce the production cost of the factory and improve economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is a front view schematic diagram of the present invention;

[0010] Figure 2 for Figure 1 Section view along AA.

[0011] Markings in the figure: 1. Plate panel, 2. Conductive rod, 3. Conductive head, 4. Insulation clamping strip, 5. Plastic sealing tape, 6. Lifting ring, 7. Core aluminum plate, 8. Surface titanium layer. DETAILED DESCRIPTION

[0012] With reference to the accompanying drawings, the specific implementation is as follows:

[0013] A titanium-aluminum-titanium electrolytic zinc cathode plate comprises a plate panel 1 and a conductive rod, wherein the plate panel 1 is a rectangular flat plate structure, and the conductive rod 2 is a rectangular long strip structure. The conductive rod 2 is located on one side of the plate panel 1 along the height direction, and the length direction of the conductive rod 2 is parallel to the length direction of the plate panel 1. A length×width side surface of the conductive rod 2 is welded to a length×width side surface of the plate panel 1, and a conductive head 3 and a lifting ring 6 are connected to the conductive rod 2. The conductive head 3 is a copper-aluminum conductive head, and one end thereof in contact with the electrode is made of red copper, and the other end in contact with the conductive rod is made of pure aluminum. Insulating edge strips 4 are respectively arranged on both sides of the width×height of the plate panel 1, and the insulating edge strips 4 are made of ABS material.

[0014] like Figure 2 As shown, the plate panel 1 includes a core aluminum plate 7 and a surface titanium layer 8, the surface titanium layer 8 covers two length × height planes of the core aluminum plate 7, and there is a strip gap between the edge of the surface titanium layer 8 close to the conductive rod 2 and the conductive rod 2, the length direction of the strip gap is parallel to the length direction of the conductive rod 2, the width of the strip gap along the height direction of the plate panel 1 is 3 to 5 mm, and the strip gap is coated with corrosion-resistant paint.

[0015] like Figure 2As shown, a plastic sealing tape 5 is provided on the surface of the corrosion-resistant coating, one side of the plastic sealing tape 5 extends to the side of the conductive rod 2 facing the electrode panel 1, and the other side of the plastic sealing tape 5 extends to the surface titanium layer 8. A plurality of plastic sealing holes are provided on the electrode panel 1 between the plastic sealing tapes 5 on both sides, and the axis of the plastic sealing holes is parallel to the width direction of the electrode panel 1. The plurality of plastic sealing holes are arranged alternately at intervals, and the plastic sealing tapes 5 on both sides respectively cover the two ends of the plastic sealing holes to enhance the bonding force between the plastic sealing tape 5 and the electrode panel 1.

[0016] The manufacturing method of the novel titanium-aluminum-titanium electrolytic zinc cathode plate of the present invention is as follows:

[0017] Step 1: Level the hot-rolled titanium-aluminum-titanium composite plate to a roughness of less than or equal to 3mm, process it to the specified size according to the drawing, and process the bottom V-shaped groove. Grind off the titanium layer within 3cm of the upper end of the plate panel according to the drawing, and process the plastic sealing opening according to the drawing.

[0018] Step 2: Pour the molten aluminum into the conductive rod mold, and after solidification, weld the lifting ring to the conductive rod. Use screws to install the copper-aluminum conductive head to the conductive rod.

[0019] Step three, assemble the plate panel and the conductive rod onto the welding tooling, align the corresponding positions, perform manual TIG welding or MIG welding, and fully weld on both sides.

[0020] Step 4: Install the insulating edge strips. Apply corrosion-resistant paint to the exposed aluminum layer above the plate. After the corrosion-resistant paint is air-dried, plastic sealing is performed. The plastic sealing area is within 5 cm of the upper end of the panel.

[0021] Step 5: Check the flatness and verticality of the plate after welding.

Claims

1. A cathode plate for titanium-aluminum-titanium electrolytic zinc, Features: The invention comprises a plate panel (1) and a conductive rod, wherein the plate panel (1) is a rectangular flat plate structure, and the conductive rod (2) is a rectangular long strip structure. The conductive rod (2) is located on one side of the plate panel (1) along the height direction, and the length direction of the conductive rod (2) is parallel to the length direction of the plate panel (1). A length×width side surface of the conductive rod (2) is welded to a length×width side surface of the plate panel (1). The plate panel (1) comprises a core aluminum plate (7) and a surface titanium layer (8). The surface titanium layer (8) covers two length×height planes of the core aluminum plate (7). A strip-shaped gap is provided between the edge of the surface titanium layer (8) close to the conductive rod (2) and the conductive rod (2), and the length direction of the strip-shaped gap is parallel to the length direction of the conductive rod (2). The width of the strip-shaped gap along the height direction of the plate panel (1) is 3 to 5 mm, the strip-shaped gap is coated with a corrosion-resistant coating, and a plastic sealing tape (5) is provided on the surface of the corrosion-resistant coating, one side of the plastic sealing tape (5) extends to the side of the conductive rod (2) facing the plate panel (1), and the other side of the plastic sealing tape (5) extends to the surface titanium layer (8), and a plurality of plastic sealing holes are provided on the plate panel (1) between the two sides of the plastic sealing tape (5), and the axes of the plastic sealing holes are parallel to the width direction of the plate panel (1), and the plurality of plastic sealing holes are arranged alternately at intervals, and the two sides of the plastic sealing tape (5) respectively cover the two ends of the plastic sealing holes, so as to enhance the bonding force between the plastic sealing tape (5) and the plate panel (1); and insulating clamping strips (4) are respectively provided on the two sides of the width×height of the plate panel (1); The manufacturing method of the titanium-aluminum-titanium electrolytic zinc cathode plate comprises: Step 1: level the hot-rolled titanium-aluminum-titanium composite plate, with an unevenness of less than or equal to 3 mm, process it to the specified size according to the drawing, and process the bottom V-groove; grind off the titanium layer within 3 cm of the upper end of the plate panel according to the drawing, and process the plastic sealing opening according to the drawing; Step 2: Pour the molten aluminum into the conductive rod mold, and after solidification, weld the lifting ring to the conductive rod; use screws to install the copper-aluminum conductive head to the conductive rod; Step 3: Assemble the plate panel and the conductive rod onto the welding tool, align the corresponding positions, perform manual TIG welding or MIG welding, and fully weld on both sides; Step 4: Install the insulating edge strips; apply corrosion-resistant paint on the exposed aluminum layer above the plate; after the corrosion-resistant paint is air-dried, perform plastic sealing, and the plastic sealing area is within 5 cm of the upper end of the panel; Step 5: Check the flatness and verticality of the plate after welding.

2. A titanium-aluminum-titanium electrolytic zinc cathode plate according to claim 1, Features: A conductive head (3) and a lifting ring (6) are connected to the conductive rod (2).

Citation Information

Patent Citations

  • Protective layer of electrolytic negative / positive plate and preparation method thereof

    CN102134730A

  • Connecting structure of titanium-aluminum-titanium composite polar plate

    CN214088695U

  • Cathode plate for electrolytic refining

    KR1020010073546A