Cracking of long-chain hydrocarbons from plastic-containing waste and organic liquids
By controlling the temperature and pressure in the heating zone, using antioxidants and multiple heating sections, the problem of soot and solid carbon generation when waste plastics convert to hydrocarbon resources is solved, and efficient long-chain hydrocarbon cracking and separation is achieved.
Patent Information
- Application Number
- CN202080079446.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-20
- Filing Date
- 2020-09-18
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2040-09-18
AI Technical Summary
When the prior art converts waste plastic into hydrocarbon resources, it produces more unpopular soot and solid carbon, and it is difficult to effectively control the cracking process of long-chain hydrocarbons, resulting in the formation of heavy hydrocarbons and solid carbon.
By heating the material containing long-chain hydrocarbons to the cracking temperature in the heating zone and adjusting the cracking process while controlling the pressure and temperature, using additives such as antioxidants and zeolites to limit the recombination of the hydrocarbon chain, multiple heating segments and The structure is separated to separate and reheat the incompletely cracked material, reducing the formation of soot and solid carbon.
The formation of solid carbon and heavy hydrocarbons is significantly reduced, the generation efficiency of short-chain hydrocarbons is improved, the separation effect of hydrocarbons is enhanced, and the heat transfer and separation efficiency of the material is improved.
Smart Images

Figure CN114746530B_ABST
Abstract
Description
Technical Field
[0001] The present invention generally relates to a method and apparatus for processing used plastics and polyolefins. Background Art
[0002] While unprocessed waste plastics have created problems for the environment, they also provide a resource that at least partially replaces hydrocarbons typically recovered from crude oil and other fossil fuel sources. When waste plastics are used as a resource, known processes tend to produce larger amounts of less desirable soot (i.e., heavy hydrocarbons and / or solid carbon), while lighter hydrocarbons with shorter chain lengths are much more desirable in the industry.
[0003] WO 2016 / 116114 A1 relates to a method for recovering hydrocarbons from plastic waste, in particular waste rich in polyolefins, by pure pyrolytic cracking without the use of catalysts, the method comprising melting the plastic waste in two heating devices, wherein a recycle stream originating from a cracking reactor and purified in a separation system is mixed with the molten plastic waste from the heating device. The mixed plastic stream is further heated in the second heating device and is conducted from the device to a cracking reactor, in which the plastic material is cracked and separated into diesel and low-boiling compounds by subsequent distillation.
[0004] US 10,160,920 B2 describes a sequential cracking process for thermal cracking of a hydrocarbon feedstock in a cascade of cracking units, wherein the hydrocarbon feedstock is heated to a predetermined maximum temperature in a furnace and thermally cracked in a cascade cracking unit, thereby reducing the formation of coke. BRIEF DESCRIPTION OF THE DRAWINGS
[0005] The drawings are not drawn to scale.
[0006] Figure 1 An assembly for cracking long chain hydrocarbons is shown; and
[0007] Figure 2 One embodiment of a separation structure and a release structure is shown. DETAILED DESCRIPTION
[0008] Figure 1 An assembly 10 for cracking long chain hydrocarbons according to one embodiment of the present invention is shown. Before further describing the details of the described embodiment, general aspects of the present invention are set forth below.
[0009] According to a first aspect, a method for cracking long-chain hydrocarbons from plastic-containing waste and organic liquids based on crude oil comprises:
[0010] -Providing materials containing long-chain hydrocarbons;
[0011] - heating a quantity of a material containing long chain hydrocarbons to a cracking temperature at which the hydrocarbon chains in the material begin to crack into shorter chains; and
[0012] - for said quantity of material having a temperature above the cracking temperature, exposing said quantity of material to heat not exceeding 50°C above the temperature of said material.
[0013] It has been found that by exposing a material containing long chain hydrocarbons to a temperature less than 50°C above the temperature of the material, the formation of solid carbon, soot and less useful heavy hydrocarbons is significantly reduced. Typically, subjecting the amount of material to heating will occur in a heating zone. Although the following description will refer to an amount of material, it should be understood that the material is an amount of material containing long chain hydrocarbons that undergoes a cracking process and thereby becomes a material containing more and more short chain hydrocarbons as the cracking process proceeds. In addition, the method is considered to be a continuous process with different levels of cracked material at the same point in time. In the context of the present application, cracking refers to the decomposition of longer chain or more complex structured hydrocarbons into shorter chain or less complex structured hydrocarbons, usually by breaking carbon-carbon bonds.
[0014] In some embodiments, the pressure of the amount of material containing long-chain hydrocarbons is adjusted while being heated to limit the gas content. When the material containing long-chain hydrocarbons is sent through the heating zone, usually by means of a pump or an extruder (e.g., an auger arranged before the heating zone), it is sufficient to arrange a pressure control valve after the heating structure, which regulates the flow of material to form a pressure in the heating zone. The thermal conductivity of the gas of the same substance is generally lower than that of its liquid. The higher the pressure, the higher the boiling point of the liquid. Therefore, by increasing the pressure, the thermal conductivity inside the substance will increase, thereby enhancing the heat transfer to the substance (here, the material containing long-chain hydrocarbons).
[0015] In some embodiments, while being heated, the pressure of the material containing long-chain hydrocarbons is adjusted to 10 to 35 bar, preferably to 20 bar. The proposed range provides a good balance between increasing thermal conductivity and the tendency of the material containing long-chain hydrocarbons to crack.
[0016] In some embodiments, an additive is provided while the material is heated until the material is sufficiently fluid, the additive preferably being an antioxidant, the additive being particularly useful for providing hydrides to the chain ends after cracking long chain polymers, the additive preferably containing butylated hydroxytoluene (BHT) and / or zeolite. Thus, there is no need to introduce the additive when the material containing long chain hydrocarbons is already under increased pressure. Furthermore, in the case of early introduction, the additive is thoroughly mixed with the material when the material containing long chain hydrocarbons is about to be cracked.
[0017] In some embodiments, the method further comprises reducing the pressure of the material after subjecting the quantity of material to heating. That is, the shorter chain material can be evaporated as a gas when the material containing the long chain hydrocarbons is no longer heated further.
[0018] In some embodiments, the method further comprises adjusting the temperature of the material after subjecting the amount of material to heat to adjust the type of gas evaporated from the amount of material. In this context, the type of gas particularly refers to the number of carbon atoms contained in one molecule of the gas.
[0019] In some embodiments, the temperature is adjusted by cooling the quantity of material. Cooling the quantity of material generally keeps longer chain molecules in a liquid state so that they are less likely to evaporate.
[0020] In some embodiments, the evaporated gas passes through a partial condenser configured to separate the long-chain hydrocarbons from the gas. Thus, the amount of material is allowed to be separated after being heated, for example in a separation structure. The partial condenser particularly prevents small droplets of the long-chain hydrocarbons from leaving the separation structure with the gas.
[0021] In some embodiments, after evaporating the gas, the amount of material is reheated to crack the remaining long chain hydrocarbons, preferably at a temperature less than 25°C higher than the temperature of the material before reheating, and the reheated material is mixed with the first heated material, preferably in a ratio of between 5:1 and 15:1, more preferably between 8:1 and 10:1. Thus, for the material that has not been fully cracked, the reheating is performed in a feedback loop. That is, when the material enters the separation structure from the heating zone, the gas evaporates, and the remaining material containing the long chain hydrocarbons is sent back to be heated again to break the long chains. The remaining material is then sent to the first heated material so that it enters the separation structure again and the gas evaporates.
[0022] In some embodiments, the method further comprises separating coke from the material after subjecting the quantity of material to heat.
[0023] In some embodiments, the certain amount of material enters a separation container after being heated, in which the gas is preferably evaporated via a partial condenser, and the coke is separated via an outlet structure, which outlet structure preferably maintains a minimum liquid level of liquid material in the separation container, and has a separation tank opening leading to the outlet structure below the minimum liquid level of the liquid material.
[0024] In some embodiments, the outlet structure includes a locking portion, which can be opened toward the separation container to separate the coke, and the outlet structure can also be blocked from the separation container to release the coke in the locking portion.
[0025] In some embodiments, the outlet structure includes a valve and cooling structure that maintains a minimum level of liquid material in the separation vessel and releases the coke when the temperature of the coke drops below its combustion temperature.
[0026] In some embodiments, the separation vessel provides a quieting zone proximate the separation tank opening to the outlet structure.
[0027] According to a second aspect, a device for executing the method of any one of the above embodiments is provided.
[0028] According to a third aspect that replaces or supplements the above aspect, a method for cracking long-chain hydrocarbons from plastic-containing waste and organic liquid based on crude oil comprises:
[0029] - providing a material containing long chain hydrocarbons in a separation structure that allows evaporation of short chain hydrocarbons,
[0030] - circulating a material containing long-chain hydrocarbons from a separation structure and heating this material to a cracking temperature at which the hydrocarbon chains in said material begin to crack into shorter chains in a heating zone separate from the separation structure,
[0031] - Recycle the material into the separation structure.
[0032] The heating zone of the foregoing aspect is separate from the separation structure in that a quantity of material being processed in the heating zone is external to the separation structure.
[0033] In one embodiment, the heating zone separated from the separation structure adjusts the temperature of the material according to a certain amount of material inside the separation structure. In some embodiments, the heating zone separated from the separation structure adjusts the temperature of the material to adjust the cracking rate of the material. In some embodiments, the cracking rate is a measure of the cracking events per unit time period. In other embodiments, the cracking rate is a measure of the cracking events per unit amount of material. By adjusting the cracking rate, the amount of short-chain hydrocarbons can be adjusted, which in turn can adjust the evaporation of the material because the evaporation temperature of the cracked hydrocarbons is generally lower than the evaporation temperature of the same hydrocarbons before cracking. Therefore, by increasing the temperature of the material, evaporation in the material can be promoted and the volume of the material can be increased. Therefore, increasing the temperature of the material will increase the material filling level within the separation structure.
[0034] In some embodiments, the evaporated hydrocarbons are separated from the long-chain hydrocarbons in the separation structure. In other embodiments, the evaporated hydrocarbons are not circulated with the material containing the long-chain hydrocarbons from the separation structure. The volume of the material in the separation structure is increased by increasing the evaporation of the material until the evaporated hydrocarbons are separated. Since the volume of the certain amount of material in the gas phase is much larger than the volume of the material in the liquid phase, the volume of the material in the separation structure can be adjusted over a wide range by adjusting the evaporation. In some embodiments, the hydrocarbons separated from the long-chain hydrocarbons in the separation structure are replaced by the material containing the long-chain hydrocarbons added to the material circulating from the heating zone separate from the separation structure before circulating into the separation structure.
[0035] According to a fourth aspect that replaces or supplements the above aspect, a method for cracking long-chain hydrocarbons from plastic-containing waste and organic liquid based on crude oil comprises:
[0036] - providing a material containing long-chain hydrocarbons in a feed device and heating the material in the feed device to a temperature at which the material has increased fluidity,
[0037] - releasing the material into a heating structure and raising the temperature of the material containing long-chain hydrocarbons to a cracking temperature at which the hydrocarbon chains in the material begin to crack into shorter chains, wherein an additive supporting the cracking is added to the material while the material is in the feed device.
[0038] The additive of the aforementioned aspects supports cracking by preventing the recombination of the cracked hydrocarbon chains. In some embodiments, after cracking, the additive provides hydrogen atoms to the open chain ends. In some embodiments, the additive is an antioxidant. In some embodiments, the additive comprises zeolite, calcium and / or butylated hydroxytoluene (BHT). It has been found that it is advantageous to add the additive in the feed device because the addition of such additives in subsequent stages may require additional measures, such as pressurizing or heating the additive separately.
[0039] According to a fifth aspect that replaces or supplements the above aspect, a method for cracking long-chain hydrocarbons from plastic-containing waste and organic liquid based on crude oil comprises:
[0040] -Providing materials containing long-chain hydrocarbons;
[0041] - heating a quantity of a material containing long chain hydrocarbons to a cracking temperature at which the hydrocarbon chains in the material begin to crack into shorter chains; and
[0042] - Maintaining the pressure of the quantity of material containing long-chain hydrocarbons to prevent evaporation of the material when heated.
[0043] Maintaining the pressure as described in the previous aspects includes maintaining the pressure at a value above atmospheric pressure, such as between 10 bar and 40 bar. In some embodiments, the pressure is maintained at about 20 bar. The proposed range provides a good balance between increasing the thermal conductivity of the heat transfer from the heat exchanger to the material containing long-chain hydrocarbons and the tendency of the material to crack.
[0044] According to a sixth aspect that replaces or supplements the above aspect, an apparatus for cracking long-chain hydrocarbons from plastic-containing waste and organic liquid based on crude oil comprises:
[0045] - a heating structure configured to heat a quantity of a material containing long chain hydrocarbons to a cracking temperature at which hydrocarbon chains in the material begin to crack into shorter chains; and
[0046] - a back pressure control element configured to maintain the pressure of the quantity of material containing long-chain hydrocarbons to prevent evaporation of the material when heated,
[0047] The back pressure control element is arranged at the output of the heating structure.
[0048] One embodiment of the foregoing aspect includes a feeding device, such as an extruder, configured to prevent pressure release therethrough. In some embodiments, the back pressure control element includes a valve and / or a pressure sensor configured to regulate pressure within the heating structure.
[0049] According to a seventh aspect that replaces or supplements the above aspect, a method for removing heavy hydrocarbons and solid carbon from a certain amount of material containing hydrocarbons of different chain lengths comprises:
[0050] - providing a quantity of a material containing hydrocarbons in a separation structure,
[0051] - generating a vortex in said quantity of hydrocarbon-containing material about a vertical axis, and
[0052] - Extracting hydrocarbons from the bottom of the certain amount of material and introducing the extracted hydrocarbons into a locking chamber, which extends between heights similar to the liquid level of the certain amount of hydrocarbon-containing material in the separation structure, wherein, during extraction, the locking chamber is connected to the fluid of the separation structure and the top of the upper surface of the separation structure containing the certain amount of material and the top of the locking chamber are subjected to the same fluid pressure.
[0053] In some embodiments, the lock chamber is in fluid communication with the separation structure, and subjecting the top of the separation structure and the top of the lock chamber to the same fluid pressure causes the liquid in the separation structure to fill the lock chamber substantially under gravity at that pressure. In some embodiments, the hydrocarbons are cooled prior to release into a subsequent container or into the atmosphere. In some embodiments, the vortex is generated by delivering the material containing the hydrocarbons tangentially into the quantity of material.
[0054] According to an eighth aspect that replaces or supplements the above aspect, an apparatus for removing heavy hydrocarbons and solid carbon from a certain amount of material containing hydrocarbons of different chain lengths comprises:
[0055] - a separation structure configured to contain hydrocarbons,
[0056] - the separation structure is configured to generate a vortex about a vertical axis in a volume of hydrocarbon-containing material within the separation structure, and
[0057] - A lock chamber configured to receive hydrocarbons from a bottom of the separation structure and extending between a similar height as the separation structure, wherein the lock chamber is configured to be in fluid communication with the separation structure when receiving hydrocarbons, and wherein the top of the separation structure and the top of the lock chamber are configured to be at the same fluid pressure when receiving hydrocarbons.
[0058] In some embodiments, the lock chamber is configured to cool the hydrocarbons prior to releasing the hydrocarbons into a subsequent container or into the atmosphere.
[0059] Please refer again Figure 1 As shown in FIG. 1 , the assembly 10 includes a heating structure 11 and a separation structure 12. The heating structure 11 is in communication with the separation structure 12 to supply a fluid into the separation structure 12. In particular, the heating structure 11 supplies a fluid containing cracked hydrocarbons into the separation structure 12.
[0060] In some embodiments, a feed device 7 is arranged to fill the material containing long-chain hydrocarbons (e.g., waste plastics or crude oil) into the heating structure 11. In various embodiments, the feed device includes a component for storage and / or a component for crushing any solid material exceeding a predetermined size. In some embodiments, the predetermined size is about 100 mm or about 50 mm. In some embodiments, the feed device includes an actuator 8 for heating and / or conveying the material containing long-chain hydrocarbons. In some embodiments, the actuator is an auger 8 arranged to heat and / or convey the material containing long-chain hydrocarbons. In some embodiments, the auger moves 8 material, and the internal friction in the material causes the material to heat and melt. In other embodiments, the feed device 7 includes a heating device, such as an electric heater or a heating device infused with a heating medium (e.g., hot oil). In various embodiments, heating causes water to evaporate. In various embodiments, the feed device 7 includes a pump (e.g., a liquid ring pump) to remove water and / or halogens by degassing. The feed device 7 conveys the material containing long-chain hydrocarbons to the heating structure 11.
[0061] In some embodiments, additives that enhance and / or optimize cracking are injected into the material in the feed device 7. It has been found that adding additives in the feed device 7 can distribute the additives more evenly with the material. In addition, injecting the additives at the feed device 7 can avoid the structure required to inject the additives into the material under increased pressure and heat, even if the additives only work in subsequent stages. In some embodiments, the additive is an antioxidant. In some embodiments, the additive comprises zeolite, calcium and / or butylated hydroxytoluene (BHT). In various embodiments, the additive prevents the recombination of the cracked hydrocarbon chains. In other embodiments, the additive is combined with interferents such as chlorine.
[0062] The heating structure 11 receives the material containing long-chain hydrocarbons. In various embodiments, the heating structure includes at least one heating zone 1, 2, 3, 4. The heating zones 1, 2, 3, 4 are arranged to expose the material containing long-chain hydrocarbons to a limited temperature increase. In other words, the material containing long-chain hydrocarbons is exposed to a temperature that is less than a predetermined temperature higher than the temperature of the material. It has been found that by limiting the temperature increase, the yield of usable material containing hydrocarbons with the desired chain length resulting from the operation of the assembly 10 is increased and the amount of solid carbon produced is limited. In various embodiments, the heating zones 1, 2, 3, 4 are arranged to expose the material containing long-chain hydrocarbons to a predetermined temperature of about 50°C or less.
[0063] Hereinafter, the temperature to which the material containing long-chain hydrocarbons is exposed will be referred to as an exposure temperature. However, the exposure temperature may have different values depending on the position in the component and the corresponding temperature of the material containing long-chain hydrocarbons.
[0064] For example, for a material containing long-chain hydrocarbons entering heating zones 1, 2, 3, 4 and having a temperature of approximately 200°C, heating zones 1, 2, 3, 4 expose the material containing long-chain hydrocarbons to an exposure temperature of 250°C or less at the entrance of heating zones 1, 2, 3, 4. When the material containing long-chain hydrocarbons begins to increase in temperature, heating zones 1, 2, 3, 4 expose the material to a correspondingly increased exposure temperature. For example, when the material containing long-chain hydrocarbons is heated to a temperature of 250°C, heating zones 1, 2, 3, 4 expose the material to an exposure temperature of up to 300°C.
[0065] In various embodiments, the heating zones 1, 2, 3, 4 thus provide a batch process in which a batch of material containing long-chain hydrocarbons is heated at a temperature not exceeding 50°C above the material temperature until a predetermined maximum temperature is reached. After a predetermined holding time to crack at least a portion of the long-chain hydrocarbons, the material containing long-chain hydrocarbons is released to a device downstream of the assembly 10. In some embodiments, there is no holding time, i.e., the holding time is close to zero, and the material is released immediately after heating.
[0066] In various embodiments, the heating zones 1, 2, 3, 4 provide a flow path for the material containing long chain hydrocarbons. The heating zones 1, 2, 3, 4 continuously or gradually increase the exposure temperature along the flow path. In some embodiments, the heating zones 1, 2, 3, 4 provide a first tube for the material containing long chain hydrocarbons. The material generally flows through the first tube in a first direction. The heating zones 1, 2, 3, 4 also provide a second tube that contacts the first tube along most of the length of the heating zones 1, 2, 3, 4 so that heat can be transferred from the interior of the second tube to the first tube. The second tube provides a flow path for the heating medium.
[0067] In some of these embodiments, the heating medium flows in a direction opposite to the first direction, so that the material containing long-chain hydrocarbons is heated while flowing in the first direction, while the heating medium cools along the flow path in the second direction. In some of these embodiments, when the heating medium enters the second tube along the heating zones 1, 2, 3, 4, the heating medium is controlled to have a temperature no higher than a predetermined final temperature by no more than 50°C, and when entering the heating zones 1, 2, 3, 4, the heating medium has a temperature no higher than the temperature of the material containing long-chain hydrocarbons by no more than 50°C. In some embodiments, the temperature, velocity and / or pressure of the heating medium in the second tube and / or the material containing long-chain hydrocarbons in the first tube are controlled. In some embodiments, the size of the second tube is such that the heating medium flowing therethrough at a predetermined velocity and having a predetermined starting velocity has predetermined temperature characteristics. In some embodiments, the first tube extends coaxially within the second tube.
[0068] In some embodiments, the second tube extends coaxially within the first tube. In some embodiments, the second tube surrounds the first tube. In some embodiments, the first tube is formed tortuously within the second tube, and the first tube is arranged so that the material containing the long-chain hydrocarbon enters the first tube on a side adjacent to where the heating medium exits the second tube, and the material exits the first tube on a side of the second tube adjacent to where the heating medium enters the second tube.
[0069] In some embodiments, heating zones 1, 2, 3, 4 include a plurality of heating segments, each of which exposes the material containing long-chain hydrocarbons to a predetermined temperature. The heating segments are configured so that the material containing long-chain hydrocarbons flows through each of them successively. Each heating segment exposes the material to a higher exposure temperature than the previous heating segment. The heating segments are configured so that the exposure temperature does not exceed 50°C above the temperature of the material containing long-chain hydrocarbons when the material enters the corresponding heating segment.
[0070] exist Figure 1 In an embodiment, heating zones 1, 2, 3, 4 include four heating sections. For example, for a material containing long-chain hydrocarbons that enters the first heating section 1 and has a temperature of approximately 200°C, the heating section 1 exposes the material containing long-chain hydrocarbons to a first exposure temperature of 250°C or less. As the material containing long-chain hydrocarbons flows through the first heating section 1, the material containing long-chain hydrocarbons heats up and its temperature approaches the first exposure temperature. In some embodiments, the first exposure temperature is between 200°C and 370°C. In some embodiments, the first exposure temperature is between 220°C and 320°C. In some embodiments, the first exposure temperature is approximately 250°C.
[0071] Whether cracking occurs in the first heating section 1 depends not only on the temperature, but also on the long-chain hydrocarbons contained in the material and other substances contained in the material intentionally or unintentionally, and the pressure of the material. In some cases, cracking will not substantially occur at low temperatures (e.g., between 200° C. and 250° C.) because other parameters do not promote cracking. In this case, the exposure temperature may be more than 50° C. higher than the material temperature. In some embodiments, the exposure temperature may be 50° C. higher than the lowest temperature at which cracking substantially occurs.
[0072] Upon exiting the first heating section 1, the material proceeds to a second heating section 2 downstream of the first heating section 1. The second heating section 2 exposes the material containing long-chain hydrocarbons to a higher exposure temperature than the first heating section 1, i.e., a second exposure temperature. The second exposure temperature is no more than 50°C above the temperature of the material containing long-chain hydrocarbons. In various embodiments, the second exposure temperature is between 250°C and 400°C. In some embodiments, the second exposure temperature is between 270°C and 370°C. In some embodiments, the second exposure temperature is about 300°C. The material containing long-chain hydrocarbons flows through the second heating section 2 and is heated toward the second exposure temperature.
[0073] The material containing long-chain hydrocarbons proceeds from the second heating section 2 to a third heating section 3 downstream of the second heating section 2. The third heating section 3 exposes the material to a third exposure temperature. The third exposure temperature is higher than the second exposure temperature. The third exposure temperature is no more than 50°C above the temperature of the material. In various embodiments, the third exposure temperature is between 300°C and 400°C. In some embodiments, the third exposure temperature is between 320°C and 380°C. In some embodiments, the third exposure temperature is about 370°C. The material containing long-chain hydrocarbons flows through the third heating section 3 and is heated toward the third exposure temperature.
[0074] The material containing long-chain hydrocarbons proceeds from the third heating section 3 to the fourth heating section 4 downstream of the third heating section 3. The fourth heating section 4 exposes the material to a fourth exposure temperature. The fourth exposure temperature is no more than 50°C above the temperature of the material. The fourth exposure temperature substantially determines the maximum temperature at which the long-chain hydrocarbons are cracked. In some embodiments, the fourth exposure temperature is between 350°C and 450°C. In other embodiments, the fourth exposure temperature is between 380°C and 420°C. The material containing long-chain hydrocarbons flows through the fourth heating section 4 and is heated toward the fourth exposure temperature.
[0075] When the material containing long-chain hydrocarbons flows through the fourth heating section 4, some of the long-chain hydrocarbons are cracked. In some embodiments, when the material flows through the third heating section 3, some of the long-chain hydrocarbons are cracked. In some embodiments, when the material flows through the second heating section 2, some of the long-chain hydrocarbons are cracked. In some embodiments, when the material flows through the first heating section 1, some of the long-chain hydrocarbons are cracked. In principle, the hotter the heating section, the more cracking occurs. When a large amount of long-chain hydrocarbons are cracked, the heating section limits the exposure temperature to a maximum temperature of 50°C higher than the temperature of the material. Therefore, the material containing long-chain hydrocarbons also contains cracked hydrocarbons. That is, compared with the material before entering the heating zone, the proportion of hydrocarbons with shorter chain lengths is increased. The material leaving the fourth heating section 4 is conveyed to the separation structure 12.
[0076] In various embodiments, the heating sections are constructed of the same structure so that the same type of heating section can be used at each position in a series of heating sections. In various embodiments, the heating sections are designed to heat to a temperature of 450°C. In various embodiments, the heating sections are designed to operate at a pressure between 0 bar and 40 bar. In various embodiments, hot oil is supplied to the heating sections as a heating medium. In various embodiments, the hot oil is selected to have a boiling point higher than the operating temperature of the heating sections and / or a solidification temperature lower than 40°C.
[0077] In some embodiments, each of the first to third heating sections is arranged to allow material to exit only when a certain minimum temperature is reached, so that the exposure temperature of the next heating section is no more than 50°C above the temperature of the material entering the next heating section. In other words, each of the first to third heating sections is arranged to allow material to exit only when a temperature is reached that is less than 50°C lower than the exposure temperature of the corresponding subsequent heating section.
[0078] In other embodiments, the throughput of the material containing long chain hydrocarbons is regulated to ensure that the material leaving the first to fourth heating stages has reached a specific corresponding temperature. For the first to third heating stages, the specific temperature is less than 50°C lower than the exposure temperature of the corresponding subsequent heating stage. For the fourth heating stage 4, the specific temperature is a predetermined maximum temperature.
[0079] The above features are also applicable to heating structures with more or fewer heating sections.
[0080] In some embodiments, back pressure control elements 5a, 5b are provided downstream of the heating zones 1, 2, 3, 4. The back pressure control elements 5a, 5b are arranged to adjust the pressure of the material containing long chain hydrocarbons in the heating zone. In various embodiments, the back pressure control element controls the throughput of the material passing through the heating zone. The back pressure control element is arranged between the heating zone and the separation structure 12. The material containing long chain hydrocarbons leaving the back pressure control elements 5a, 5b is conveyed to the separation structure 12. In some embodiments, the back pressure control element comprises an adjustable valve 5a and a pressure sensor 5b. The pressure sensor 5b is configured to detect the pressure of the material in the heating zone. The adjustable valve 5a is configured to release the material as long as the pressure sensor 5b detects a pressure within a specific range. In some embodiments, the specific range is between 10 bar and 40 bar. In some embodiments, the specific range is about 20 bar. If the material in the heating zone has a pressure beyond the range, the valve 5a controls the throughput of the material. For example, if the pressure in the heating zone drops below the lower limit of the pressure range, the valve 5a reduces the throughput until the pressure in the heating zone increases. If the pressure in the heating zone exceeds the upper limit, the valve 5a allows a higher throughput until the pressure drops. In some embodiments, the valve 5a has a structure of a pressure reducing valve, that is, the valve 5a is kept in a closed state by a preloaded spring, and once a predetermined pressure is exceeded, the valve 5a opens toward the subsequent separation structure 12, and once the pressure drops below the predetermined pressure, the valve 5a closes. In other embodiments, the valve 5a is a gate valve, and the opening and closing of the gate valve can adjust the throughput, thereby adjusting the pressure detected by the pressure sensor 5b. In some embodiments, the valve 5a is arranged to always allow a smaller throughput, in other words, the valve 5a is arranged not to be completely closed.
[0081] Once the material passes through the back pressure control element, the pressure in the material decreases. In particular, short chain hydrocarbons produced by cracking evaporate into the gas phase, producing a gas containing hydrocarbons.
[0082] The material containing liquid and hydrocarbon-containing gas is conveyed to a separation structure 12. In the separation structure 12, the hydrocarbon-containing gas is separated from the liquid containing longer hydrocarbon chains of the material. The hydrocarbon-containing gas rises from the liquid. The separation structure 12 releases the gas containing hydrocarbons having a chain length equal to or less than a predetermined chain length. In some embodiments, the separation structure 12 includes a gas release device at its top. The gas release device is preferably equipped with a partial condenser 21.
[0083] In various embodiments, the separation structure 12 includes a partial condenser 21, a separation zone 25 containing a gas-liquid interface of hydrocarbon material, and a settling zone 28 for accumulating heavy hydrocarbons and / or solid carbon. In some embodiments, the separation structure 12 includes a cylindrical middle portion 24 containing the separation zone 25, and a funnel-shaped bottom 27 containing the settling zone 28, the funnel terminating in an outlet for heavy hydrocarbons and / or solid carbon.
[0084] The partial condenser 21 is configured to allow the gas containing hydrocarbons with the largest chain length to pass. The partial condenser 21 cools the gas containing hydrocarbons to a condensation temperature, which condenses hydrocarbons of a specific chain length and longer. The partial condenser recycles the condensed hydrocarbons back into the liquid. In some embodiments, the condensation temperature is between 270° C. and 370° C. In other embodiments, the condensation temperature is 320° C.
[0085] In some embodiments, the partial condenser 21 includes a condensation vessel 22 that provides a flow path for the gas containing hydrocarbons and a cooling pipe 23 for a cooling medium (e.g., hot oil) for cooling the gas. In some embodiments, the cooling pipe 23 intersects the condensation vessel 22. In some embodiments, the cooling pipe extends in a zigzag, spiral, and / or spiral manner in the condensation vessel 22. In some embodiments, the condensation vessel 22 and the cooling pipe 23 are configured so that the gas flows along a vertical direction and one or more horizontal directions. In other words, the gas cannot pass through the partial condenser 21 in a straight line. In some embodiments, the cooling pipe 23 provides cooling ribs and / or baffles, which are used to increase the contact surface with the gas, especially to guide and / or hinder the gas flow in the partial condenser 21. In some embodiments, the partial condenser 21 includes randomly arranged cooling ribs and / or baffles. In some embodiments, the cooling pipe 23, the cooling ribs and / or baffles are inclined to guide the condensed hydrocarbons away from the main gas flow, for example, to the side of the condensation vessel 22, so that it flows back or falls back into the liquid.
[0086] Therefore, partial condenser 21 is arranged to pass gas containing hydrocarbons whose chain length includes or is less than a predetermined chain length. In some embodiments, the predetermined chain length is 30 carbon atoms. In other embodiments, the predetermined chain length is 25 carbon atoms. In other embodiments, the predetermined chain length is 22 or 20 carbon atoms. Hydrocarbons whose chain length exceeds the predetermined chain length are circulated back into the liquid in separation structure 12.
[0087] In various embodiments, the separation structure 12 releases a liquid containing hydrocarbons having a chain length greater than a predetermined chain length. The separation structure 12 removes heavy hydrocarbons and / or solid carbon produced by cracking.
[0088] In some embodiments, the heating structure 11 includes a reheating zone 6. The liquid containing hydrocarbons is sent from the separation structure 12 through the reheating zone 6 through a pipeline. The reheating zone 6 heats the liquid containing hydrocarbons again so that more long-chain hydrocarbons are cracked. In some embodiments, the reheating zone is arranged to provide an exposure temperature that is no more than 50°C higher than the temperature of the liquid containing hydrocarbons. The limited exposure temperature can limit the carbonization of hydrocarbons. In some embodiments, the reheating zone 6 is arranged to at least partially compensate for the heat loss of the material in the separation structure 12 due to the separation of gas and carbon, as well as the heat loss occurring through the walls of the separation structure 12 and any pipelines. In some embodiments, the reheating zone 6 provides an exposure temperature of 380°C to 450°C. In other embodiments, the reheating zone 6 provides an exposure temperature of 390°C to 410°C.
[0089] In some embodiments, the liquid containing hydrocarbons is passed through a filter 9 to remove particles. In some embodiments, the liquid containing hydrocarbons is delivered using a pump 10 arranged to regulate the flow rate of the liquid.
[0090] The liquid leaves the reheating zone 6 and evaporates the gas containing the cracked hydrocarbon chains. In some embodiments, the liquid in the reheating zone 6 is not pressurized, so that some of the cracked hydrocarbons have evaporated into gas containing cracked hydrocarbon chains in the reheating zone 6. In some embodiments, the liquid and / or gas leaving the reheating zone 6 is fed into the separation structure 12 to release the evaporated gas. In some embodiments, the liquid and / or gas leaving the reheating zone 6 is mixed with the material leaving the heating zones 1, 2, 3, 4. In some embodiments, the liquid and / or gas leaving the reheating zone 6 is mixed with the material leaving the back pressure control elements 5a, 5b. In some embodiments, the mixing ratio of the liquid and / or gas leaving the reheating zone 6 and the material leaving the heating zones 1, 2, 3, 4 is between 5:1 and 15:1, more preferably between 8:1 and 10:1, according to the flow meter. In some embodiments, the mixing ratio is adjusted by the feed device 7, the heating zone, the back pressure control element and the pump 10. In some embodiments, hot oil is supplied to the reheating zone 6, such as the hot oil used in the first to fourth heating sections 1, 2, 3, 4. In some embodiments, the reheating zone 6 receives hot oil having the same temperature as the fourth heating zone 4 .
[0091] In some embodiments, the reheating zone 6 adjusts the temperature of the material based on a certain amount of material in the separation structure 12. In some embodiments, the reheating zone adjusts the temperature of the material to adjust the cracking rate of the material. In some embodiments, the cracking rate is a measure of the cracking events per unit time period. In other embodiments, the cracking rate is a measure of the cracking events per unit amount of material. By adjusting the cracking rate, the amount of short-chain hydrocarbons in the material can be adjusted, which in turn can adjust the evaporation of the material because the evaporation temperature of the cracked hydrocarbons is generally lower than the evaporation temperature of the same hydrocarbons before cracking. In addition, by heating the material, more material evaporates. Therefore, by increasing the temperature of the material, evaporation in the material can be promoted and the amount of liquid material can be reduced. In some embodiments, this is used to adjust the liquid level of the liquid material in the separation structure 12.
[0092] In an exemplary embodiment, the heating sections 1, 2, 3, 4, the reheating zone 6 and the hot oil used provide the following parameters:
[0093]
[0094] Where "PM inlet temperature" indicates the temperature of the material containing long-chain hydrocarbons when it is input into the corresponding heating section, "PM outlet temperature" indicates the temperature of the material containing long-chain hydrocarbons when it is output from the corresponding heating section, "TO inlet temperature" indicates the temperature of the hot oil used as the heating medium in this exemplary embodiment when it is applied to the corresponding heating section, and "TO outlet temperature" indicates the temperature of the hot oil after it is applied to the corresponding heating zone. It can be seen from the table that the maximum difference between the TO inlet temperature and the PM outlet temperature and between the TO outlet temperature and the PM inlet temperature does not exceed 50°C. Since the flow direction of the hot oil is opposite to the flow direction of the material through the corresponding heating section, the exposure temperature will not exceed 50°C above the material temperature.
[0095] In various embodiments, the hydrocarbon-containing material enters the separation structure 12 from the heating structure 11 through the inlet 26. In some embodiments, the inlet is configured to transport the material tangentially into the separation zone 25. In other words, the material flows into the cylindrical middle portion 24 from a position deviating from the vertical axis of the cylindrical middle portion 24. Therefore, the liquid in the middle portion is caused to rotate. The heavy hydrocarbons and / or solid carbon move to the outside of the separation zone 25. On the outside, the heavy hydrocarbons and / or solid carbon rub against the side walls of the separation zone 25 (e.g., the inner wall of the cylindrical middle portion 24). The heavy hydrocarbons and / or solid carbon slow down and sink to the bottom. In various embodiments, the heavy hydrocarbons and solid carbon accumulate in the settling zone 28. In some embodiments, the funnel-shaped bottom 27 guides the heavy hydrocarbons and solid carbon to the outlet of the heavy hydrocarbons and / or solid carbon.
[0096] In various embodiments, the settling zone 28 includes a separation cone 29 arranged above the funnel-shaped bottom 27. The separation cone 29 includes a thin plate forming a lateral cone, the bottom of the cone facing the bottom 27, and the top of the cone facing the top of the separation structure 12. In various embodiments, the separation cone 29 is substantially formed as a right circular cone, the vertex of which is adjacent to or coincides with the vertical axis of the cylindrical middle part 24. In various embodiments, the separation cone 29 has a truncated form and includes an opening at the vertex. The separation cone 29 is arranged so that a gap is left between the separation cone 29 and the inner wall of the cylindrical middle part 24 and / or the funnel-shaped bottom 27, so that solid carbon and / or heavy hydrocarbons can reach the outlet through the gap. The gap is preferably arranged around the circumference of the separation cone 29. The separation cone 29 prevents the rotating liquid in the middle part 24 from agitating the heavy hydrocarbons and / or solid carbon accumulated in the funnel-shaped bottom 27. This allows the heavy hydrocarbons and / or solid carbon to accumulate more densely at the outlet and can be removed along with smaller amounts of liquid hydrocarbons.
[0097] In various embodiments, heavy hydrocarbons and / or solid carbon are released through a valve structure 13, which is configured to adjust the filling level in the separation structure 12 so that it is maintained at least at a predetermined minimum level. In various embodiments, the valve structure 13 includes at least a first and a second lock valve 31, 32 and a lock chamber between the first and second lock valves 31, 32, wherein at least one valve is normally closed during operation. In some embodiments, a control element 33 controls the lock valves 31, 32. During operation, the first lock valve 31 adjacent to the bottom 27 opens and allows heavy hydrocarbons and / or solid carbon to leave the separation structure 12. The heavy hydrocarbons and / or solid carbon enter the lock chamber. Before releasing the heavy hydrocarbons and / or solid carbon, the first lock valve 31 is closed. Then, the second lock valve 32 opens.
[0098] Figure 2 One embodiment of a separation structure 12 and a valve structure 13 is shown. Figure 2 The valve structure 13 includes a first lock valve 31, a lock chamber 34, a second lock valve 32 and a compensation line 35. The compensation line includes a compensation valve 36. The lock chamber 34 is arranged to extend between similar heights as the separation zone 25 and the settling zone 28. The compensation line 35 passing through the compensation valve 36 causes the separation structure 12 and the lock chamber 34 to be subjected to the same fluid pressure at their tops, so that the liquid in the separation structure fills the lock chamber 34 under pressure.
[0099] When operating the separation structure 12, it is advantageous to always have a certain level of liquid in the separation structure 12. As long as the first lock valve 31 and the compensation valve 36 are open and the second lock valve 32 is closed, the filling level of the lock chamber 34 corresponds to the filling level of the separation structure 12. As heavy hydrocarbons and / or solid carbon accumulate in the settling zone 28, the heavy hydrocarbons and / or solid carbon are flushed out of the separation structure 12 and into the lock chamber 34. Since the filling level in the lock chamber corresponds to the filling level in the separation structure 12, the capacity of the lock chamber 34 increases as the filling level increases. However, when the filling level of the separation structure 12 is low, the capacity of the lock chamber 34 is low, so that the separation structure will not be completely discharged into the lock chamber 34, and therefore will not be emptied. When filling the lock chamber 34, the first lock valve 31 and the compensation valve 36 are in a closed state. The second lock valve 32 is open. In various embodiments, the lock chamber 34 is pressurized with an inert gas to drive off heavy hydrocarbons and / or solid carbon. When the lock chamber 34 is emptied, the second lock valve 32 is closed, and the first lock valve 31 and the make-up valve 36 are opened. More heavy hydrocarbons and / or solid carbon from the settling area 28 are allowed to enter the lock chamber 34.
[0100] In various embodiments, the heavy hydrocarbons and / or solid carbon in the lock chamber 34 are above their ignition temperature. Therefore, the heavy hydrocarbons and / or solid carbon can be cooled before contacting with air. Therefore, in some embodiments, before releasing the heavy hydrocarbons and / or solid carbon, they are sent to a cooling chamber for cooling. In some embodiments, the heavy hydrocarbons and / or solid carbon leave the cooling chamber after their temperature drops below a certain maximum temperature. In some embodiments, the maximum temperature of the heavy hydrocarbons and / or solid carbon is the ignition temperature.
Claims
1. A method for cracking long-chain hydrocarbons from plastic-containing waste and organic liquids based on crude oil, comprising: - Provide materials containing long-chain hydrocarbons; - heating a quantity of said material to a material temperature above a cracking temperature at which hydrocarbon chains in said material begin to crack into shorter chains; and - exposing the certain amount of the material to a heating structure having a temperature higher than the temperature of the material until a predetermined maximum temperature is reached, wherein the heating structure includes at least one heating zone, the at least one heating zone includes a plurality of heating segments, the plurality of heating segments are configured to make the material containing long-chain hydrocarbons flow through each of the plurality of heating segments successively, and to expose the material containing long-chain hydrocarbons to an exposure temperature higher than that of a previous heating segment, the plurality of heating segments are configured so that the temperature difference between the exposure temperature of the material containing long-chain hydrocarbons when entering the corresponding heating segment and the temperature of the material containing long-chain hydrocarbons is less than or equal to 50°C, wherein the plurality of heating segments include four or more heating segments.
2. The method of claim 1, wherein the pressure of the quantity of the material is adjusted while exposing to limit gas content.
3. The method of claim 2, wherein the pressure of the quantity of the material is adjusted to between 10 and 35 bar while exposing.
4. The method of claim 3, wherein the pressure of the quantity of the material is adjusted to 20 bar while exposing.
5. The method of claim 1, wherein: An additive is provided while heating the amount of the material until the material can sufficiently flow, the additive being an antioxidant for providing hydrides to chain ends after cleaving long-chain polymers.
6. The method of claim 5, wherein the additive comprises butylated hydroxytoluene (BHT) and / or zeolite.
7. The method of claim 1, further comprising reducing a pressure of the quantity of material after subjecting the quantity of the material to heat.
8. The method of claim 1, further comprising adjusting a temperature of the quantity of the material after subjecting the quantity of the material to heat to adjust a type of gas evaporated from the quantity of the material.
9. The method of claim 8, wherein the temperature is adjusted by cooling the quantity of material.
10. The method of claim 8, wherein the evaporated gas is passed through a partial condenser configured to separate long chain hydrocarbons from the gas.
11. The method of claim 8, wherein the quantity of material after boiling off the gas is reheated to crack remaining long chain hydrocarbons, and wherein the reheated quantity of material is mixed with additional material that has been heated a first time.
12. The method of claim 11, wherein the reheating temperature is less than 25°C higher than the temperature of the quantity of material prior to reheating.
13. The method of claim 11, wherein the mixing ratio of the reheated material to the material that has been heated for the first time is between 5:1 and 15:
1.
14. A method as claimed in claim 13, wherein the mixing ratio of the reheated material to the material that has been heated for the first time is between 8:1 and 10:
1.
15. The method of claim 1 further comprising separating coke from the quantity of material after subjecting the quantity of material to heat.
16. A method as claimed in claim 15, wherein the certain amount of material enters a separation container after being heated, in which the gas is evaporated via a partial condenser and the coke is separated via an outlet structure, and the outlet structure maintains a minimum liquid level of liquid material in the separation container, and has a separation tank opening leading to the outlet structure below the minimum liquid level of the liquid material.
17. The method of claim 16, wherein the outlet structure includes a lock that opens toward the separation vessel to separate the coke, or the outlet structure is blocked from the separation vessel to release the coke in the lock.
18. The method of claim 16, wherein the outlet structure includes a valve and cooling structure that maintains a minimum level of liquid material in the separation vessel and releases the coke when the coke temperature drops below its combustion temperature.
19. The method of claim 16, wherein the separation vessel provides a settling zone adjacent a separation tank opening to the outlet structure.
20. An apparatus for performing the method of any one of claims 1-19.