Semiconductor memory structure and method for forming the same

By forming specific structures and doping regions in the cutoff region and the active region in the dynamic random access memory, the leakage current problem caused by the reduction of component size is solved, and the reliability and density of the memory are improved.

CN114792685BActive Publication Date: 2024-11-22WINBOND ELECTRONICS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110110180.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-01-26
Publication Date
2024-11-22
Estimated Expiration
2041-01-26

AI Technical Summary

Technical Problem

With the miniaturization of the size of dynamic random access memory components, the source/drain junction leakage current problem has become more prominent, and existing manufacturing methods are difficult to effectively solve, affecting the density and performance of the memory.

Method used

A semiconductor memory structure is adopted, in which an isolation structure is formed in the cutoff region, trenches are formed through the cutoff region and the active region, ion implantation is performed using a patterned masking layer to form a doped region, and a first and a first and a second are formed in the active region and the cutoff region. The two-gate structure ensures the distance relationship between the doped region and the gate structure to reduce the possibility of leakage circuit paths.

Benefits of technology

By balancing the conductive carriers induced by the bypass word lines, the formation of leakage circuit paths is reduced, the reliability and manufacturing yield of semiconductor memory is improved, and the density and overall performance of components are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114792685B_ABST
    Figure CN114792685B_ABST
Patent Text Reader

Abstract

A semiconductor memory structure and a method for forming the same, wherein the semiconductor memory structure comprises a semiconductor substrate, wherein the semiconductor substrate comprises an active region and a truncation region, wherein the semiconductor memory structure further comprises an isolation structure disposed in the truncation region, a first gate structure extending at least through the isolation structure in the truncation region, and a second gate structure extending at least through the active region, wherein the semiconductor memory structure further comprises a doped region disposed in the active region, wherein the distance between the doped region and the first gate structure is smaller than the distance between the doped region and the second gate structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to a semiconductor memory structure and a method for forming the same, and in particular to a dynamic random access memory. Background Art

[0002] Dynamic Random Access Memory (DRAM) devices are widely used in consumer electronic products. In order to increase the component density in the DRAM device and improve its overall performance, the current manufacturing technology of the DRAM device continues to strive towards the miniaturization of the component size. However, when the component size continues to shrink, many challenges arise. For example, improving the source / drain junction leakage. Therefore, the industry still needs to improve the manufacturing method of the DRAM device to overcome the problems caused by the reduction of the component size. Summary of the invention

[0003] An embodiment of the present invention provides a semiconductor memory structure. The semiconductor memory structure includes a semiconductor substrate, which includes an active region and a truncation region. The semiconductor memory structure also includes an isolation structure disposed in the truncation region, a first gate structure extending at least through the isolation structure in the truncation region, and a second gate structure extending at least through the active region. The semiconductor memory structure also includes a doped region disposed in the active region, wherein the distance between the doped region and the first gate structure is smaller than the distance between the doped region and the second gate structure.

[0004] An embodiment of the present invention provides a method for forming a semiconductor memory structure, the method comprising providing a semiconductor substrate, the semiconductor substrate comprising a truncation region and an active region. The method further comprises forming a first trench through the truncation region and forming a second trench through the active region, and forming a patterned mask layer to cover a portion of the second trench through the active region, the patterned mask layer having an opening exposing a portion of the first trench through the truncation region. The method further comprises performing an ion implantation process using the patterned mask layer to form a doped region in the active region, and forming a first gate structure in the first trench and forming a second gate structure in the second trench. BRIEF DESCRIPTION OF THE DRAWINGS

[0005] In order to make the features and advantages of the present invention more clearly understood, different embodiments are specifically described below with reference to the accompanying drawings as follows:

[0006] Figures 1A to 1K is a schematic plan view showing different stages of forming a semiconductor memory structure according to some embodiments of the present invention;

[0007] Figure 1A-1 to Figure 1K-1 as well as Figure 1A-2 to Figure 1K-2is a schematic cross-sectional view showing different stages of forming a semiconductor memory structure according to some embodiments of the present invention;

[0008] Figure 1K-3 yes Figure 1K-2 An enlarged schematic diagram of a semiconductor memory is shown to illustrate additional details of the semiconductor memory structure.

[0009] [Explanation of symbols]

[0010] 102: Semiconductor substrate

[0011] 104: Active Zone

[0012] 106: Quarantine

[0013] 108:Truncation area

[0014] 110: Isolation Structure

[0015] 112: Lining

[0016] 114: Insulation material

[0017] 116: Dielectric layer

[0018] 118: Patterned mask layer

[0019] 120: Opening pattern

[0020] 122: Groove

[0021] 124: Filling material

[0022] 126: Patterned mask layer

[0023] 128: Opening pattern

[0024] 130: Part

[0025] 132: Adulterants

[0026] 134: Doping area

[0027] 136: Gate dielectric layer

[0028] 138: Gate liner

[0029] 140: Gate electrode layer

[0030] 142: Gate structure

[0031] 142A: The gate structure 142 passes through the active region 104

[0032] 142C: The gate structure 142 passes through the portion of the isolation structure 110 in the cut-off region 108.

[0033] 144: Depression

[0034] 146: Covering layer

[0035] 148: Source / drain region

[0036] 150: Source / drain region

[0037] 152: Contact plug

[0038] 154: bit line

[0039] 158: Dielectric structure

[0040] 160: Contact plug

[0041] 160L: lower portion of contact plug 160

[0042] 160U: upper portion of contact plug 160

[0043] D1: First direction

[0044] D2: Second direction

[0045] D3: Third direction

[0046] A1:Size

[0047] A2: Size

[0048] A3: Distance

[0049] A4: Distance

[0050] A5: Depth

[0051] A6: Depth DETAILED DESCRIPTION

[0052] The present application is described more fully below with reference to the drawings of the embodiments of the present invention. However, the present application may be implemented in various different embodiments and should not be limited to the embodiments described herein. The thickness of layers and regions in the drawings may be exaggerated for clarity, and the same or similar reference numbers in the drawings represent the same or similar elements.

[0053] Figures 1A to 1K 1 is a schematic plan view showing different stages of forming a semiconductor memory structure according to some embodiments of the present invention. Figures 1A to 1K Reference directions are indicated, wherein the first direction D1 is the channel extension direction, the second direction D2 is the word line extension direction (or gate extension direction), and the third direction D3 is the bit line extension direction. An acute angle is formed between the first direction D1 and the second direction D2, and the range is, for example, about 10 degrees to about 80 degrees. The second direction D2 is substantially perpendicular to the third direction D3.

[0054] Figures 1A to 1K Reference cross sections are also indicated. Cross section AA is parallel to the axial direction of the active region (ie, the first direction D1 ) and passes through the surface of the active region. Cross section BB is parallel to the axial direction of the gate structure (ie, the second direction D2 ) and passes through the surface of the gate structure.

[0055] Figure 1A-1 to Figure 1K-1 Display along Figures 1A to 1K A schematic cross-sectional diagram of a semiconductor memory structure captured at section AA. Figure 1A-2 to Figure 1K-2 Display along Figures 1A to 1K A schematic cross-sectional diagram of a semiconductor memory structure captured by cross-section BB.

[0056] A semiconductor memory structure 100 is provided. The semiconductor memory structure 100 includes a semiconductor substrate 102. Figure 1A , Figure 1A-1 and Figure 1A-2 As shown in FIG. 1 , the semiconductor substrate 102 includes an active region 104, an isolation region 106, and a chop region 108. The active region 104 is a semiconductor block extending along a first direction D1, and each active region 104 is defined by two isolation regions 106 and two chop regions 108. An isolation structure 110 is formed in the isolation region 106 and the chop region 108 of the semiconductor substrate 102, thereby surrounding and electrically isolating the active regions 104.

[0057] The isolation regions 106 extend along the first direction D1 and are arranged at intervals in the second direction D2, thereby dividing the semiconductor substrate 102 into a plurality of semiconductor strips (not shown). The truncation regions 108 (indicated by dotted lines) are arranged corresponding to the semiconductor strips and truncate the semiconductor strips into a plurality of active regions 104. In the second direction D2, adjacent truncation regions 108 may be misaligned or non-overlapping.

[0058] In some embodiments, the semiconductor substrate 102 is an elemental semiconductor substrate, such as a silicon substrate or a germanium substrate; or a compound semiconductor substrate, such as a silicon carbide substrate or a gallium arsenide substrate. In some embodiments, the semiconductor substrate 102 may be a semiconductor-on-insulator (SOI) substrate.

[0059] The isolation structure 110 extends downward from the upper surface of the semiconductor substrate 102. The formation of the isolation structure 110 may include, for example, using a first patterning process (including a lithography process and an etching process) to form a trench corresponding to the isolation region 106 in the semiconductor substrate 102, and dividing a plurality of semiconductor strips. Then, using a second patterning process (including a lithography process and an etching process) to form a trench corresponding to the truncation region 108, and truncate the semiconductor strips into a plurality of active regions 104.

[0060] The formation of the isolation structure 110 may also include forming a liner 112 along the sidewalls and bottom surface of the trench and along the upper surface of the semiconductor substrate 102, and then forming an insulating material 114 to overfill the remaining portion of the trench. The insulating material 114 is nested in the liner 112. The liner 112 is formed of a dielectric material, such as silicon oxide (SiO), silicon nitride (SiN), silicon oxynitride (SiON), other suitable materials, and / or combinations thereof. The insulating material 114 is formed of a dielectric material, such as silicon nitride (SiN), silicon oxynitride (SiON), silicon oxide (SiO), other suitable materials, and / or combinations thereof. The insulating material 114 and the liner 112 may be formed of different materials. For example, the liner 112 is a silicon oxide layer, and the insulating material 114 is a silicon nitride layer.

[0061] The formation of the isolation structure 110 may also include performing a planarization process (e.g., an etch-back process) to remove the insulating material 114 formed on the upper surface of the semiconductor substrate 102 until the liner 112 is exposed. After the planarization process, gaps may be formed at the upper surface of the insulating material 114, especially at the upper surface of the insulating material 114 in the wider trench. A dielectric layer 116 may be formed on the upper surface of the semiconductor substrate 102 and fill the gap. The dielectric layer 116 may be a silicon oxide layer formed using atomic layer deposition (ALD).

[0062] A patterned mask layer 118 is formed on the upper surface of the semiconductor substrate 102, such as Figure 1B , Figure 1B-1 and Figure 1B-2 The patterned mask layer 118 has an opening pattern 120, and the opening pattern 120 extends along the second direction D2. In some embodiments, the patterned mask layer 118 can be a hard mask structure formed by one or more layers of dielectric materials, and the dielectric material includes silicon oxide (SiO), silicon nitride (SiN), silicon oxynitride (SiON), other suitable materials, and / or combinations thereof. During the formation of the patterned mask layer 118, the portion of the dielectric layer 116 exposed by the opening pattern 120 can be removed.

[0063] The semiconductor memory structure 100 is etched using the patterned mask layer 118 to remove portions of the semiconductor memory structure 100 that are not covered by the patterned mask layer 118. The opening pattern 120 of the patterned mask layer 118 is transferred to the active region 104 and the isolation structure 110 of the semiconductor substrate 102 to form a trench 122, such as Figure 1C , Figure 1C-1 and Figure 1C-2As shown. The etching depth of the trench 122 may be different in the active region 104 and the isolation structure 110. The trenches 122 extend along the second direction D2 and are arranged in the third direction D3. The trenches 122 extend alternately through the active region 104 and the isolation structure 110, two trenches 122 extend through one active region 104, and two trenches 122 extend through the truncation region 108 on both sides of the active region 104.

[0064] The dimension of the trench 122 in the third direction D3 needs to be smaller than the dimension of the truncation region 108 in the third direction D3. The etching process for forming the trench 122 removes part of the insulating material 114, and after the etching process, in the truncation region 108, the liner 112 of the isolation structure 110 is exposed from the trench 122. If the dimension of the trench 122 in the third direction D3 is too large, the thickness of the liner 112 will be too thin or completely disappear after the etching process, thereby negatively affecting the electrical properties (e.g., on-current) of the resulting semiconductor memory device. If the dimension of the trench 122 in the third direction D3 is too small, the amount of electrode material subsequently filled in the trench 122 will be reduced.

[0065] Form a filling material 124 on the semiconductor memory structure 100, such as Figure 1D , Figure 1D-1 and Figure 1D-2 As shown. Filling material 124 is formed on patterned mask layer 118 and seals trench 122. The upper portion of trench 122 is filled with filling material 124, and the lower portion of trench 122 remains unfilled. In some embodiments, filling material 124 is formed of a carbon-containing material, such as diamond-like carbon (DLC), high selectivity transparency (HST) carbon film, or the like. Filling material 124 is configured to provide a substantially flat upper surface, and a patterned mask layer is subsequently formed on this substantially flat upper surface.

[0066] Next, a patterned mask layer 126 is formed on the filling material 124. The patterned mask layer 126 has a plurality of opening patterns 128, which correspond to the cut-off region 108 of the semiconductor substrate 102 and expose the filling material 124. The patterned mask layer 126 may be a patterned photoresist layer. The lithography process for forming the patterned mask layer 126 and the lithography process for forming the cut-off region 108 may use the same main reticle. In some other embodiments, the patterned mask layer 126 may be a patterned hard mask layer.

[0067] The filling material 124 is etched using the patterned mask layer 126 to remove the portion of the filling material 124 exposed by the opening pattern 128, thereby opening the trench 122 sealed by the filling material 124. After the etching process, the portion of the trench 122 (labeled as 130) passing through the cut-off region 108 is exposed from the filling material 124 and the patterned mask layer 126, as shown in FIG. Figure 1E , Figure 1E-1 and Figure 1E-2 shown.

[0068] The semiconductor memory structure 100 is subjected to an ion implantation process using the patterned mask layer 126 and the patterned filling material 124 to form a doped region 134 in the active region 104, such as Figure 1F , Figure 1F-1 and Figure 1F-2 As shown. The tilt angle of the ion implantation process may range from about 5 degrees to about 20 degrees. During the ion implantation process, the dopant 132 passes through the opening pattern 128 of the patterned mask layer 126 and the opening pattern of the patterned filling material 124, through the liner 112 of the isolation structure 110, and then is implanted into the semiconductor material of the active region 104, thereby forming a doped region 134 at the side of the active region 104 facing the truncation region 108. The dopant 132 may be a p-type dopant (e.g., boron or BF2) or an n-type dopant (e.g., phosphorus or arsenic).

[0069] The doping region 134 is configured to balance the conductive carriers induced by the passing word line, which will be described in detail later. The conductivity type of the doping region 134 can be the same as the conductivity type of the active region 104 of the semiconductor substrate 102, for example, both are p-type. The doping concentration of the doping region 134 is greater than the doping concentration of the active region 104 of the semiconductor substrate 102. For example, the doping concentration of the doping region 134 is about 1 to 2 orders of magnitude higher than the doping concentration of the active region 104.

[0070] After the ion implantation process, the patterned mask layer 126 and the filling material 124 are removed by an ashing process or an etching process to expose the patterned mask layer 118 and open other portions of the trench 122, such as Figure 1G , Figure 1G-1 and Figure 1G-2 shown.

[0071] A gate dielectric layer 136, a gate liner 138, and a gate electrode layer 140 are sequentially formed on the semiconductor memory structure 100. Figure 1H , Figure 1H-1 and Figure 1H-2As shown. The gate dielectric layer 136 is formed along the sidewalls of the patterned mask layer 118 and the sidewalls and bottom surface of the trench 122 to partially fill the trench 122. In some embodiments, the gate dielectric layer 136 is formed of silicon oxide, silicon nitride, silicon oxynitride, a high-k dielectric material, and / or a combination thereof. In some embodiments, the gate dielectric layer 136 is formed using in-situ steam generation (ISSG), atomic layer deposition (ALD), chemical vapor deposition (CVD), or a combination thereof.

[0072] The gate liner 138 is formed on the gate dielectric layer 136 and partially fills the trench 122. In some embodiments, the gate liner 138 is formed of titanium nitride (TiN), tungsten nitride (WN), tantalum nitride (TaN), other suitable materials, and / or combinations thereof. The gate liner 138 can be deposited using physical vapor deposition (PVD) and / or atomic layer deposition (ALD).

[0073] The gate electrode layer 140 is formed on the gate liner 138 and overfills the remaining portion of the trench 122. In some embodiments, the gate electrode layer 140 is formed of a metal material, such as tungsten (W), aluminum (Al), copper (Cu), cobalt (Co), ruthenium (Ru), other suitable materials, and / or combinations thereof. The gate electrode layer 140 may be deposited using physical vapor deposition (PVD), chemical vapor deposition (CVD), and / or atomic layer deposition (ALD).

[0074] According to some embodiments, the gate electrode layer 140 and the gate liner 138 are etched to form a recess 144 extending into the semiconductor substrate 102, such as Fig. 1I , Figure 1I-1 and Figure 1I-2 As shown, after the etching process, a gate structure 142 is formed. The gate structure 142 can be used as a word line of the resulting semiconductor memory device, and can also be called a buried word line (BWL).

[0075] Each gate structure 142 extends alternately through the active region 104 and the isolation structure 110, two gate structures 142 extend through a single active region 104, and two gate structures 142 extend through the truncation regions 108 on both sides of the active region 104. The gate structure 142 includes a gate dielectric layer 136, a gate liner 138, and a gate electrode layer 140. The gate liner 138 has a U-shaped profile and is lined between the gate dielectric layer 136 and the gate electrode layer 140. The gate electrode layer 140 is nested in the gate liner 138. In addition, the levels of the upper surfaces of the gate liner 138 and the gate electrode layer 140 are higher than the level of the bottom surface of the doped region 134.

[0076] A capping layer 146 is formed in the recess 144, such as Figure 1J , Figure 1J-1 and Figure 1J-2 In some embodiments, the capping layer 146 is formed of a dielectric material, such as silicon oxide, silicon nitride, silicon oxynitride, other suitable materials, and / or combinations thereof. Forming the capping layer 146 may include depositing a dielectric material to fill the recess 144, and performing a planarization process to remove the dielectric material formed on the upper surface of the patterned mask layer 118.

[0077] According to some embodiments, source / drain regions 148 and 150 are formed in the active region 104 of the semiconductor substrate 102 by an ion implantation process, such as Figure 1K-1 As shown. The source / drain region 150 is located in the center of the active region 104, and the source / drain region 148 is located at both ends of the active region 104. The source / drain regions 148 and 150 and the portion of the gate structure 142 extending through the active region 104 can be combined to form a transistor, such as an n-type transistor or a p-type transistor, for the resulting semiconductor memory device.

[0078] The source / drain regions 148 and 150 are doped, and a PN junction is formed between the active region 104 and the source / drain region 148 or 150. The conductivity type of the source / drain regions 148 and 150 is opposite to that of the active region 104 of the semiconductor substrate 102, and is opposite to that of the doped region 134. For example, the active region 104 and the doped region 134 are p-type, and the source / drain regions 148 and 150 are n-type. The doping concentration of the source / drain regions 148 and 150 may be greater than the doping concentration of the doped region 134. For example, the doping concentration of the source / drain regions 148 and 150 is about 1 to 2 orders of magnitude higher than the doping concentration of the doped region 134. In addition, the bottom surface of the source / drain regions 148 and 150 (i.e., the PN junction) may be lower than the level of the upper surface of the gate liner 138 and the gate electrode layer 140.

[0079] A dielectric structure 158 may be formed on the semiconductor memory structure 100, and a conductive member may be formed in the dielectric structure 158 to electrically couple the source / drain regions 148 and 150. For example, Figure 1K , Figure 1K-1 and Figure 1K-2 As shown, contact plugs 152 are formed on source / drain regions 150; bit lines 154 are formed on contact plugs 152; and contact plugs 160 are formed on source / drain regions 148 and doped regions 134. During the formation of dielectric structure 158 and these conductive features, dielectric layer 116, patterned mask layer 118, and capping layer 146 on the upper surface of semiconductor substrate 102 may be removed.

[0080] In some embodiments, dielectric structure 158 includes multiple dielectric layers and is formed of a dielectric material such as silicon oxide, silicon nitride, silicon oxynitride, other suitable materials, multiple layers thereof, and / or combinations thereof.

[0081] In some embodiments, the contact plug 152 partially extends into the semiconductor substrate 102 and lands on the source / drain region 150. The contact plug 152 may be formed of a semiconductor material, such as polysilicon.

[0082] In some embodiments, the bit line 154 extends along the third direction D3 and is electrically coupled to the source / drain region 150 through the contact plug 152. The bit line 154 may be formed of a metal or a metal nitride, such as tungsten (W), aluminum (Al), copper (Cu), titanium (Ti), tantalum (Ta), titanium nitride (TiN), tantalum nitride (TaN), other suitable materials, multiple layers thereof, or combinations thereof. A silicide layer may be formed between the bit line 154 and the contact plug 152.

[0083] In some embodiments, the contact plug 160 falls on the source / drain region 148 and the doped region 134. The contact plug 160 may include a lower portion 160L and an upper portion 160U. For example, the lower portion 160L of the contact plug 160 is formed of a semiconductor material, such as polysilicon. The upper portion 160U of the contact plug 160 is formed of a metal or a metal nitride, such as tungsten (W), aluminum (Al), copper (Cu), titanium (Ti), tantalum (Ta), titanium nitride (TiN), tantalum nitride (TaN), other suitable materials, multiple layers thereof, or combinations thereof. A silicide layer may be formed between the lower portion 160L and the upper portion 160U of the contact plug 160.

[0084] Figure 1K-3 yes Figure 1K-2 , to illustrate additional details of the semiconductor memory structure 100. Figure 1K-3As shown, the portion of the gate structure 142 that passes through the isolation structure 110 in the cut-off region 108 is labeled as 142C, and the portion of the gate structure 142 that passes through the active region 104 is labeled as 142A. In some cases, during operation, the portion 142C of the gate structure 142 that extends through the cut-off region 108 (which may be referred to as a bypass word line) may induce conductive carriers (e.g., electrons or holes) in the active region 104 adjacent thereto (or on the sidewalls of the isolation structure 110), thereby forming a channel layer. This channel layer is undesirable and may provide various leakage paths, such as leakage from the source / drain region 148 to the contact plug on the source / drain region 150, and / or other conductive features, thereby causing degradation or loss of stored data in the semiconductor memory device.

[0085] According to the embodiment of the present invention, since the conductive carriers (e.g., holes or electrons) provided by the dopant in the doped region 134 are opposite to the conductive carriers induced by the bypass word line 142C, the doped region 134 can balance the conductive carriers induced by the bypass word line 142C, thereby reducing the possibility of the formation of a leakage path. Therefore, the reliability and manufacturing yield of the semiconductor memory device are improved.

[0086] In addition, the source / drain region 148 may be formed to overlap with a portion of the doped region 134 (the overlapping portion is indicated by a dotted line). The doped region 134 has a width A1 along the first direction D1, and the source / drain region 148 has a size A2 along the first direction D1. The ratio of the size A1 of the doped region 134 to the size A2 of the source / drain region 148 ranges from about 0.01 to about 0.05. If the ratio of the width A1 to the width A2 is too large, the doped region 134 may negatively affect the electrical properties (e.g., on-state current) of the resulting semiconductor memory device. If the ratio of the width A1 to the width A2 is too small, the doped region 134 may not be sufficient to balance the conductive carriers induced by the bypass word line.

[0087] The doped region 134 has a distance A3 from the portion 142C (the gate dielectric layer 136) of the gate structure 142 in the truncation region 108, and has a distance A4 from the portion 142A (the gate dielectric layer 136) of the gate structure 142 in the active region 104, and the distance A3 is smaller than the distance A4. The ratio of the distance A3 to the distance A4 ranges from about 0.01 to about 0.05. If the ratio of the distance A3 to the distance A4 is too large, the doped region 134 may negatively affect the electrical properties (e.g., on-state current) of the resulting semiconductor memory device. If the ratio of the distance A3 to the distance A4 is too small, the doped region 134 may not be sufficient to balance the conductive carriers induced by the bypass word line.

[0088] The top surface of the doped region 134 is coplanar with the top surface of the cap layer 146. The level of the bottom surface of the doped region 134 is lower than the level of the bottom surface of the source / drain region 148. That is, the depth A5 of the doped region 134 is greater than the depth A6 of the source / drain region 148. The ratio of the depth A5 of the doped region 134 to the depth A6 of the source / drain region 148 ranges from about 1.25 to about 1.5. If the ratio of the depth A5 to the depth A6 is too large, during the ion implantation process for forming the doped region 134, dopants may be undesirably implanted into other regions of the semiconductor substrate 102, such as the peripheral circuit region. If the ratio of the depth A5 to the depth A6 is too small, the doped region 134 may not be sufficient to balance the conductive carriers induced by the bypass word line.

[0089] Additional components may be formed on the semiconductor memory structure 100 to produce a semiconductor memory device. For example, a capacitor structure (not shown) may be formed on the dielectric structure 158, and the capacitor structure may be electrically coupled to the source / drain region 148 through the contact plug 160. In some embodiments, the semiconductor memory device is a dynamic random access memory (DRAM).

[0090] According to the above, the embodiment of the present invention forms a doped region at the side of the active region facing the bypass word line, and the doped region can balance the conductive carriers induced by the bypass word line, thereby reducing the possibility of leakage path formation. Therefore, the reliability and manufacturing yield of the semiconductor memory device are improved.

[0091] Although the present invention is disclosed as above with the aforementioned embodiments, it is not intended to limit the present invention. Those skilled in the art can make some modifications and improvements without departing from the protection scope of the present invention.

Claims

1. A semiconductor memory structure, characterized in that: include: A semiconductor substrate including an active region and a truncation region; an isolation structure disposed in the cut-off region; a first gate structure extending at least through the isolation structure in the truncation region; a second gate structure extending at least through the active region; a doped region disposed in the active region, wherein a first distance between the doped region and the first gate structure is smaller than a second distance between the doped region and the second gate structure; as well as A cap layer is disposed on the first gate structure, wherein a portion of the isolation structure is between the cap layer and the doped region.

2. The semiconductor memory structure according to claim 1, characterized in that: Also includes: A source / drain region is disposed in the active region and between the second gate structure and the isolation structure, wherein the doped region is between the source / drain region and the isolation structure.

3. The semiconductor memory structure according to claim 2, characterized in that: The doped region has a first conductivity type, and the source / drain region has a second conductivity type opposite to the first conductivity type.

4. The semiconductor memory structure according to claim 2, characterized in that: The bottom surface of the doped region is lower than the bottom surface of the source / drain region.

5. The semiconductor memory structure according to claim 2, characterized in that: Also includes: A contact plug is disposed on the source / drain region and the doped region.

6. The semiconductor memory structure according to claim 2, characterized in that: The doping concentration of the source / drain region is greater than the doping concentration of the doping region.

7. The semiconductor memory structure according to claim 1, wherein: The isolation structure includes: a liner and an insulating material disposed on the liner, wherein the liner of the isolation structure is between the first gate structure and the doped region, and the liner of the isolation structure is between the cap layer and the doped region.

8. The semiconductor memory structure according to claim 7, characterized in that: The top surface of the doped region is coplanar with the top surface of the cap layer.

9. The semiconductor memory structure according to claim 1, wherein: A bottom surface of the doped region is lower than an upper surface of a gate electrode layer of the first gate structure.

10. A method for forming a semiconductor memory structure, characterized in that: include: Providing a semiconductor substrate, the semiconductor substrate comprising a truncation region and an active region; forming a first trench through the cut-off region and forming a second trench through the active region; Forming a patterned mask layer to cover a portion of the second trench passing through the active region, wherein the patterned mask layer has an opening exposing a portion of the first trench passing through the cut-off region; Performing an ion implantation process using the patterned mask layer to form a doped region in the active region; as well as A first gate structure is formed in the first trench and a second gate structure is formed in the second trench.

11. The method for forming a semiconductor memory structure according to claim 10, wherein: Also includes: An isolation structure is formed in the cut-off region, wherein the first gate structure extends through the isolation structure in the cut-off region.

12. The method for forming a semiconductor memory structure according to claim 10, wherein: Also includes: A source / drain region is formed in the active region, wherein the doped region has a first conductivity type, and the source / drain region has a second conductivity type opposite to the first conductivity type.

13. The method for forming a semiconductor memory structure according to claim 10, wherein: Also includes: forming a filling material to seal the first trench and the second trench, wherein the patterned mask layer is formed on the filling material; as well as The filling material is etched using the patterned mask layer so that a portion of the first trench passing through the cut-off region is exposed from the filling material.