An experimental method and device for dynamically evaluating the corrosion resistance of bottom wells
By simulating the dynamic corrosion of drilling fluid filter cake and cement ring in the downhole environment, combined with macro and micro analysis, the neglected problem of cement interface corrosion changes in the research on bottom-hole corrosion in the existing technology is solved, and the corrosion resistance of the underground water is achieved The scientific evaluation provides more accurate experimental results.
Patent Information
- Application Number
- CN202210321348.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-30
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2042-03-30
AI Technical Summary
When studying the corrosion problem of bottom wells, the existing technology mainly focuses on the cementing cement ring itself, and fails to effectively consider the corrosion process of the casing and cementing interface, especially the corrosion changes at the interface cementing of the drilling fluid filter cake. This leads to differences between the simulation and the actual situation, and it is impossible to truly evaluate the corrosion resistance of the underground hole.
An experimental method and device for dynamically evaluating corrosion resistance at the bottom of the well was designed. By simulating the underground environment, artificial well wall and drilling fluid filter cake were prepared, combined with cement ring and casing, and curing and hole-making treatment were carried out, using different methods. The corrosive media conducts dynamic corrosion experiments, and conducts macroscopic and microscopic analysis to evaluate the corrosion conditions of each cement interface.
This method and device can scientifically and intuitively evaluate the corrosion resistance of underground cementing projects, provide simulation results that are closer to the real working conditions, improve the rigor and reference value of the experiment, and can more accurately evaluate the corrosion performance of the underground cement interface. .
Smart Images

Figure CN114934767B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil and gas exploration and drilling, and more specifically to an experimental method and device for dynamically evaluating the anti-corrosion performance of a bottom hole. Background Art
[0002] As a key link in connecting oil and gas production, cementing engineering plays an important role in casing support and isolation of formation fluids, and plays a vital role in the service life of oil and gas wells. During the cementing process, cementing cement rings are formed through circulation on the ground, wellhead, casing and casing annulus. With the increase in exploration efforts, the direction of exploration and development tends to be deep and complex, especially when developing oil and gas resources in acidic formations. High concentrations of acidic gases such as CO2 and H2S in the formation and high-mineralization formation water will corrode the bottom well casing and cementing cement ring, causing casing damage and significant changes in the mechanical properties of cementing cement stone. For example, the strength of cement stone itself is reduced and cracks and pores are generated, which significantly increases its own permeability, causing interlayer crossflow, losing the interlayer isolation effect, and even causing the casing annulus to be pressurized, bringing additional well repair and remedial costs, especially having a serious impact on the service life of oil and gas wells and the efficiency of oil and gas development. Therefore, a true understanding of the bottom well corrosion process and corrosion degree is of great practical significance for wellbore safety and anti-corrosion research of cementing engineering.
[0003] However, the current research on bottom hole corrosion problems mainly focuses on the cement sheath itself, but there is little research on the corrosion changes of the casing and the bonding interface between the two.
[0004] For example, on March 26, 2019, a patent application was published with the publication number CN109520878A and the name “Dynamic Corrosion Device for Migration of High-Temperature and High-Pressure Corrosive Medium”. This patent technology takes into account the high-temperature and high-pressure dynamic corrosive medium to simulate the corrosion process of cement stone and evaluate its corrosion resistance, but its action object only considers the cement stone itself, while the corrosion process of casing corrosion and cementing bonding interface is not considered, which is still different from the actual situation underground.
[0005] For example, on September 28, 2018, a patent application for invention with the publication number CN108593533A and the name "Experimental device and experimental method for simulating the corrosion process of cement ring in the formation" was disclosed. The patent technology uses fine sand and modulated formation water to simulate the formation cementing environment, but under real cementing conditions, there must be drilling fluid filter cake on the well wall. The patent technology does not take into account the corrosion of the cement ring and the drilling fluid filter cake bonding surface.
[0006] There are also some simulation technologies. After placing cement stone in a plastic mold, AB glue is used to wrap the cement stone to fill the gap between the cement stone and the mold to simulate the downhole casing and drilling fluid filter cake. However, this method is quite different from the actual situation downhole and cannot evaluate the corrosion process of the cementing interface.
[0007] From the above, it can be seen that most of the previous studies on bottom hole corrosion problems focused on cementing cement itself, while the corrosion process and changes at the interface between casing and cementing, especially the corrosion changes at the interface bonding of the attached drilling fluid filter cake, were basically not involved. Therefore, it is necessary to develop a set of experimental methods and devices that can truly simulate the dynamic corrosion of the well based on the actual environment of the well, so as to scientifically and intuitively evaluate the corrosion resistance of the well cementing project and provide new technical means. Summary of the invention
[0008] In order to overcome the defects and deficiencies in the above-mentioned prior art, the present invention provides an experimental method and device for dynamically evaluating the bottom hole corrosion resistance. The purpose of the present invention is to provide a real and reliable experimental method to simulate the bottom hole corrosion process in the downhole environment and evaluate the degree of corrosion; at the same time, another purpose of the present invention is to design and provide an experimental device that simulates the dynamic corrosion process of the bottom hole based on the actual downhole conditions. The experimental method for dynamically evaluating the bottom hole corrosion of the present invention mainly includes pressing the well wall filter cake, preparing cement slurry for cementing, pouring cement slurry into the outer ring hole of the casing, and curing and waiting for it to solidify. After the curing is completed, it is subjected to hole making treatment to simulate the downhole perforating operation; different corrosive media are used to treat it in a dynamic and static manner. After the corrosion is completed, the test piece is taken out, and the macroscopic and microscopic performance analysis is performed to obtain the experimental results. The present invention can scientifically and intuitively evaluate the corrosion resistance of downhole cementing engineering and provide new technical means.
[0009] The first aspect of the present invention provides an experimental method for dynamically evaluating the anti-corrosion performance of a well bottom, the method comprising the following steps:
[0010] S1, a step of preparing an artificial well wall, drilling a core from a target formation, and processing the core to obtain an artificial well wall;
[0011] S2, a step of preparing a drilling fluid filter cake, placing the artificial well wall obtained in step S1 into the kettle cavity, and sealing the upper and lower ends of the artificial well wall; adding drilling fluid into the inner cavity of the artificial well wall, and sealing the kettle after injecting the drilling fluid; heating and pressurizing the inside of the kettle, and after the pressure is increased to a set pressure, maintaining the pressure for a period of time to press the well wall drilling fluid filter cake; in the process of pressing the well wall drilling fluid filter cake, the speed of the internal motor set in the kettle is controlled to simulate the flow or static state of the drilling fluid at the bottom of the well;
[0012] S3, kettle flushing step, after the drilling fluid filter cake on the well wall is pressed, the pressure inside the kettle is released, the drilling fluid in the kettle is discharged, and the inside of the kettle is flushed with flushing fluid;
[0013] S4, cement ring preparation step, placing the casing into the kettle cavity, and the casing is located in the inner cavity of the artificial well wall, sealing the upper and lower ends of the casing, pouring the prepared cement into the annulus between the casing and the artificial well wall, sealing the kettle, and heating and pressurizing the kettle for curing and setting;
[0014] S5, hole making step, after the curing age, the kettle body is cooled and depressurized, and the sample with the artificial well wall, drilling fluid filter cake, cementing cement ring and casing four-in-one cementing is taken out; a hole is drilled on one side of the sample cylinder through the side wall to form an artificial hole making channel;
[0015] S6, corrosion experiment steps, after the sample hole is completed, the sample is put back into the kettle; the corrosion experiment is carried out; corrosive liquid medium is added into the sample and the external annulus between the sample and the kettle, and the kettle is sealed; the kettle is heated to the set temperature, and corrosive gas medium is introduced into the external annulus between the sample and the kettle; during the corrosion experiment, the rotation speed of the external motor in the external annulus of the kettle and the internal motor inside the sample is controlled to simulate the static and flowing state of the corrosive fluid medium;
[0016] S7. After the corrosion experiment is completed, the samples are taken out from the kettle body, and the corrosion test results of the artificial well wall, drilling fluid filter cake, cement ring, casing and different cementing interfaces are analyzed by macro and micro analysis methods.
[0017] Furthermore, the corrosive liquid medium includes a combination of one or more of formation brine, oil-water mixture and crude oil; and the corrosive gas medium is an acidic gas medium.
[0018] The upper and lower ends of the artificial well wall are sealed, specifically, sealing materials are applied to the upper and lower end surfaces of the artificial well wall.
[0019] Furthermore, in step S5, a lathe is used to drill holes in the sample, and vibration generated during the drilling process is controlled.
[0020] The second aspect of the present invention provides an experimental device for dynamically evaluating the corrosion resistance of the bottom of a well, which includes a kettle body, a top cover, an artificial well wall and a casing. An internal motor is arranged on the top cover in the middle of the inner cavity of the artificial well wall, and a plurality of external motors are arranged on the top cover of the external annulus between the artificial well wall and the kettle body, wherein the internal motor is connected to a plurality of internal stirring rods, and the internal stirring rods extend into the inner cavity of the artificial well wall; the external motor is connected to the external stirring rods, and the external stirring rods extend into the external annulus; a pressure relief pipeline and an internal air intake pipeline are arranged on the top cover at the top of the inner cavity of the artificial well wall; and a plurality of external air intake pipelines are arranged on the top cover at the top of the external annulus.
[0021] Furthermore, a heating layer and a heat-insulating layer are sequentially arranged on the inside of the kettle body from the inside to the outside.
[0022] Several external drainage pipelines are arranged at the bottom of the external annulus.
[0023] An internal drainage pipeline is arranged at the bottom of the inner cavity of the artificial well wall.
[0024] The experimental device also includes a base, and the kettle body is assembled on the base.
[0025] The kettle body and the top cover are fixed and sealed together by bolts.
[0026] Compared with the prior art, the beneficial technical effects brought by the present invention are as follows:
[0027] 1. The present invention selects the core of the target formation to make an artificial wellbore wall, and restores and simulates the wellbore condition of the target wellbore to the greatest extent; the drilling fluid filter cake is pressed on the inner wall of the artificial wellbore through the drilling fluid filter cake preparation step, and then the cementing cement ring is prepared, so that the four-in-one sample formed by the casing, the cementing cement ring, the drilling fluid filter cake and the artificial wellbore wall is closer to the actual wellbore working condition, ensuring the rigor of the simulation experiment, making the corrosion test results closer to the actual working condition, and the corrosion test results are more valuable for reference.
[0028] 2. When the present invention is used to press the well wall drilling fluid filter cake, the upper and lower ends of the artificial well wall are sealed, which can effectively prevent the injected drilling fluid from overflowing from the upper and lower ends of the artificial well wall, thereby simulating the formation of the well wall drilling fluid filter cake under real drilling conditions.
[0029] 3. After the wellbore drilling fluid filter cake is pressed, the kettle is flushed to effectively avoid the influence of drilling fluid on the maintenance of cementing cement ring, making it closer to the actual drilling conditions. At the same time, during the experiment, the wellbore drilling fluid filter cake is pressed and the cementing cement ring is prepared, which can make the cementing interface between the wellbore drilling fluid filter cake and the well artificial wellbore, the cementing interface between the wellbore drilling fluid filter cake and the cementing cement ring, and the cementing interface between the cementing cement ring and the casing closer to the actual working conditions. After the corrosion experiment, the analysis results of the corrosion results of each cementing interface have more specific reference value.
[0030] 4. The corrosion experiment of the present invention also simulates the drilling and perforating process. The corrosive medium can enter each cementing interface through the artificial drilling channel, so as to analyze and study the corrosion resistance of each cementing interface.
[0031] 5. The present invention can realistically simulate the process of bottom hole corrosion in the downhole environment and evaluate the degree of corrosion. It can more scientifically and intuitively evaluate the corrosion resistance of downhole cementing engineering and provide new technical means.
[0032] 6. The experimental device for dynamically evaluating bottom hole corrosion provided by the present invention has a simple structure, can truly simulate the downhole environment, and provides better hardware support for the experimental method for dynamically evaluating bottom hole corrosion.
[0033] 7. The experimental device of the present invention is easy to operate and can better perform experiments for dynamically evaluating bottom hole corrosion. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 The flowchart of the experimental method for dynamically evaluating bottom hole corrosion of the present invention;
[0035] Figure 2 This is a schematic diagram of the structure of an experimental device for dynamically evaluating bottom hole corrosion according to the present invention;
[0036] Figure 3 A schematic diagram of the top view of the experimental device for dynamically evaluating bottom hole corrosion according to the present invention;
[0037] Figure numerals: 1. external air inlet pipeline, 2. external motor, 3. top cover, 4. heating layer, 5. insulation layer, 6. corrosive liquid medium, 7. external stirring rod, 8. artificial hole making channel, 9. external drainage pipeline, 10. internal drainage pipeline, 11. base, 12. internal stirring rod, 13. casing, 14. cementing cement ring, 15. external annulus, 16. drilling fluid filter cake on the well wall, 17. artificial well wall, 18. internal air inlet pipeline, 19. internal motor, 20. pressure relief pipeline. DETAILED DESCRIPTION
[0038] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention is described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0039] Example 1
[0040] As a preferred embodiment of the present invention, refer to the attached specification Figure 1 As shown, this embodiment discloses an experimental method for dynamically evaluating the anti-corrosion performance of the bottom of a well, and the method comprises the following steps:
[0041] S1, a step of preparing the artificial well wall 17, drilling a core from a target formation, and processing the core to obtain the artificial well wall 17;
[0042] S2, a step of preparing a drilling fluid filter cake, placing the artificial well wall 17 obtained in step S1 into the kettle body cavity, and sealing the upper and lower ends of the artificial well wall 17; adding drilling fluid into the inner cavity of the artificial well wall 17, and sealing the kettle body after injecting the drilling fluid; heating and pressurizing the inside of the kettle body, and after the pressure is increased to a set pressure, maintaining the pressure for a period of time to press the well wall drilling fluid filter cake 16; in the process of pressing the well wall drilling fluid filter cake 16, the rotation speed of the internal motor 19 provided in the kettle body is controlled to simulate the flow or static state of the drilling fluid at the bottom of the well;
[0043] S3, kettle flushing step, after the well wall drilling fluid filter cake 16 is pressed, the pressure inside the kettle is released, the drilling fluid in the kettle is discharged, and the inside of the kettle is flushed with flushing fluid;
[0044] S4, cement ring preparation step, placing the casing 13 into the kettle cavity, and the casing 13 is located in the inner cavity of the artificial well wall 17, the upper and lower ends of the casing 13 are sealed, and the prepared cement is poured into the annulus between the casing 13 and the artificial well wall 17, the kettle is sealed, and the kettle is heated and pressurized for curing and solidification;
[0045] S5, hole making step, after the curing age, the kettle is cooled and depressurized, and the sample of the artificial well wall 17, the drilling fluid filter cake, the cementing cement ring 14 and the casing 13 that are bonded together are taken out; a hole is drilled through the side wall of the sample cylinder on one side to form an artificial hole making channel 8;
[0046] S6, corrosion experiment steps, after the sample hole making is completed, the sample is put back into the kettle; the corrosion experiment is carried out; corrosive liquid medium 6 is added into the sample and the external annulus 15 between the sample and the kettle, and the kettle is sealed; the kettle is heated to a set temperature, and corrosive gas medium is introduced into the external annulus 15 between the sample and the kettle; during the corrosion experiment, the rotation speed of the external motor 2 in the external annulus 15 inside the kettle and the internal motor 19 inside the sample is controlled to simulate the static and flowing state of the corrosive fluid medium;
[0047] S7. After the corrosion experiment is completed, the sample is taken out from the kettle body, and the corrosion test results of the artificial well wall 17, the drilling fluid filter cake, the cement ring 14, the casing 13 and the different cementing interfaces are analyzed by means of macroscopic and microscopic analysis methods.
[0048] Example 2
[0049] As another preferred embodiment of the present invention, this embodiment is an implementation of the corrosive liquid medium 6 in Example 1. Specifically, the corrosive liquid medium 6 can be a combination of one or more of formation brine, oil-water mixture and crude oil; however, the corrosive liquid medium 6 is not limited to the above-mentioned liquid media.
[0050] Furthermore, the corrosive gas medium is an acidic gas medium, such as H2S, CO2, etc.
[0051] Furthermore, the upper and lower ends of the artificial well wall 17 are sealed, specifically, sealing materials are applied to the upper and lower end surfaces of the artificial well wall 17. The sealing materials can be soft rubber materials, or oily sealing materials such as butter.
[0052] As another implementation of this embodiment, in step S5, a lathe is used to drill holes in the sample, and the vibration generated by the drilling process is controlled to prevent the vibration generated during the hole-making process from damaging the bonding interfaces.
[0053] Example 3
[0054] As another preferred embodiment of the present invention, refer to the attached specification Figure 2 and attached Figure 3As shown, this embodiment discloses an experimental device for dynamically evaluating the corrosion resistance of the bottom of a well, which includes a kettle body, a top cover 3, an artificial well wall 17 and a casing 13. An inner motor 19 is arranged on the top cover 3 in the middle of the inner cavity of the artificial well wall 17, and a plurality of outer motors 2 are arranged on the top cover 3 of the external annulus 15 between the artificial well wall 17 and the kettle body, wherein the inner motor 19 is connected to a plurality of inner stirring rods 12, and the inner stirring rods 12 extend into the inner cavity of the artificial well wall 17; the outer motor 2 is connected to the outer stirring rod 7, and the outer stirring rod 7 extends into the external annulus 15; a pressure relief pipeline 20 and an inner air intake pipeline 18 are arranged on the top cover 3 at the top of the inner cavity of the artificial well wall 17; and a plurality of outer air intake pipelines 1 are arranged on the top cover 3 at the top of the external annulus 15.
[0055] Example 4
[0056] As another preferred embodiment of the present invention, refer to the attached specification Figure 2 and attached Figure 3 As shown, this embodiment is an implementation of the experimental device in Example 1. A heating layer 4 and an insulation layer 5 are sequentially arranged on the inside of the kettle from the inside to the outside to facilitate heating and insulation. A plurality of external drainage pipelines 9 are arranged at the bottom of the external annulus 15. An internal drainage pipeline 10 is arranged at the bottom of the inner cavity of the artificial well wall 17 to facilitate drainage. The experimental device also includes a base 11, and the kettle is assembled on the base 11. The kettle and the top cover 3 are fixed and sealed together by bolts.
[0057] Example 5
[0058] As another preferred embodiment of the present invention, refer to the attached specification Figure 1 , Attachment Figure 2 and attached Figure 3 As shown, in this embodiment, an artificial well wall 17 with an inner diameter of 149.2 mm and a casing 13 with an outer diameter of 127 mm are taken as an example to specifically illustrate the technical solution of the present invention.
[0059] It should be noted that the size of the artificial well wall 17, the size of the cementing cement ring 14, the size of the casing 13, etc. are all determined according to the wellbore conditions of the target formation.
[0060] S1. A core is drilled from the target formation and the core is processed to obtain an artificial well wall 17; the processing of the core refers to processing the inner cavity wall of the artificial well wall 17 so that the inner cavity wall of the artificial well wall 17 is close to the well wall state of the real wellbore, wherein the inner diameter of the artificial well wall 17 is 149.2 mm; the upper end surface and the lower end surface of the artificial well wall 17 also need to be leveled so as to seal the upper end surface and the lower end surface to prevent drilling fluid, corrosive media, etc. from overflowing from the upper end surface and the lower end surface of the artificial well wall 17.
[0061] S2. Apply a layer of butter (mainly for sealing) evenly on the upper and lower ends of the prepared artificial well wall 17, then put it into the kettle, close the external and internal drain valves, then add drilling fluid into the artificial well wall 17, and then cover the top cover 3. The inside of the kettle is heated and pressurized, and after the pressure is increased to the set pressure, the pressure is maintained for a period of time to press the well wall drilling fluid filter cake 16; during the pressing of the well wall drilling fluid filter cake 16, the rotation speed of the internal motor 19 set in the kettle is controlled, and the internal motor 19 drives the internal stirring rod 12 to rotate, stirring the drilling fluid in the inner cavity of the artificial well wall 17 to simulate the flow or static state of the drilling fluid at the bottom of the well.
[0062] S3. After the well wall drilling fluid filter cake 16 is pressed, close the internal air inlet valve, open the pressure relief pipeline 20 to release the internal pressure of the kettle, open the top cover 3 and open the internal drainage valve to discharge the drilling fluid in the kettle, and flush the inside of the kettle with flushing fluid.
[0063] S4. Apply a layer of butter evenly on the upper and lower ends of the casing 13 (mainly for its sealing function), and then put it into the inner cavity of the artificial well wall 17. Adjust the position of the casing 13 to make it centered. The outer diameter of the casing 13 is 127 mm. Pour the prepared cementing slurry into the annulus between the casing 13 and the well wall drilling fluid filter cake 16, seal the kettle, heat and pressurize it, and then perform maintenance and solidification.
[0064] S5. After the curing period, the kettle is cooled and depressurized, and the sample of the artificial well wall 17, drilling fluid filter cake, cementing cement ring 14 and casing 13 that have been bonded together is taken out. A hole is drilled through the side wall of the sample cylinder on one side to form an artificial hole channel 8. The number and diameter of the holes can be selected according to the experimental needs, and no hole is drilled on the other side.
[0065] S6. After drilling the hole for the sample, put the sample back into the kettle, close the external liquid drainage pipeline 9 and the internal liquid drainage pipeline 10, add corrosive liquid medium 6 (corrosive liquid medium 6 can be formation brine, oil-water mixture, crude oil, etc.) to the inside of the sample and the external annulus 15 according to the experimental needs, cover the top cover 3, close the pressure relief pipeline 20, and close the internal air intake pipeline 18; according to the experimental needs, heat the kettle to the required temperature, and introduce acidic gases such as H2S and CO2 into the external air intake pipeline 1, and close or open the external motor 2 and the internal motor 19 to simulate the static and flowing states of the corrosive fluid medium.
[0066] S7. After the corrosion experiment is completed, the sample is taken out from the kettle body, and the corrosion test results of the artificial well wall 17, the drilling fluid filter cake, the cement ring 14, the casing 13 and the different cementing interfaces are analyzed by means of macroscopic and microscopic analysis methods.
[0067] The above is only a preferred embodiment of the present invention and is not intended to limit the present invention in any form. Any simple modification, equivalent change or modification made by any person skilled in the art without departing from the concept and principle of the technical solution of the present invention shall fall within the scope of protection of the present invention.
Claims
1. An experimental method for dynamically evaluating the anti-corrosion performance of a bottom hole, characterized in that: The method comprises an experimental device for dynamically evaluating the anti-corrosion performance of a well bottom, the experimental device comprising a kettle body, a top cover (3), an artificial well wall (17) and a casing (13), an inner motor (19) is arranged on the top cover (3) in the middle of the inner cavity of the artificial well wall (17), and a plurality of outer motors (2) are arranged on the top cover (3) of the outer annulus (15) between the artificial well wall (17) and the kettle body, wherein the inner motor (19) is connected to a plurality of inner stirring rods (12), and the inner stirring rods (12) extend toward the inner cavity of the artificial well wall (17); the outer motor (2) is connected to the inner motor (19) and the inner stirring rods (12) extend toward the inner cavity of the artificial well wall (17); An external stirring rod (7) is connected, and the external stirring rod (7) extends into the external annulus (15); a pressure relief pipeline (20) and an internal air intake pipeline (18) are arranged on the top cover (3) at the top of the inner cavity of the artificial well wall (17); a plurality of external air intake pipelines (1) are arranged on the top cover (3) at the top of the external annulus (15); a heating layer (4) and a heat insulation layer (5) are arranged in sequence from the inside to the outside on the inside of the kettle body; a plurality of external liquid discharge pipelines (9) are arranged at the bottom of the external annulus (15); and an internal liquid discharge pipeline (10) is arranged at the bottom of the inner cavity of the artificial well wall (17); The experimental method for dynamically evaluating the bottom hole corrosion resistance specifically includes the following steps: S1, a step of preparing the artificial well wall (17), drilling a core from a target formation, and processing the core to obtain the artificial well wall (17); S2, a step of preparing a drilling fluid filter cake, wherein the artificial well wall (17) obtained in step S1 is placed in the cavity of the kettle body, and the upper and lower ends of the artificial well wall (17) are sealed; drilling fluid is added to the inner cavity of the artificial well wall (17), and the kettle body is sealed after the drilling fluid is injected; the interior of the kettle body is subjected to a temperature and pressure increase process, and after the pressure is increased to a set pressure, the pressure is maintained for a period of time to press the well wall drilling fluid filter cake (16); during the process of pressing the well wall drilling fluid filter cake (16), the rotation speed of an internal motor (19) provided in the kettle body is controlled to simulate the flow or static state of the drilling fluid at the bottom of the well; S3, kettle flushing step, after the drilling fluid filter cake (16) on the well wall is pressed, the pressure inside the kettle is released, the drilling fluid in the kettle is discharged, and the inside of the kettle is flushed with a flushing fluid; S4, a cement ring preparation step, wherein the casing (13) is placed in the cavity of the kettle body, and the casing (13) is located in the inner cavity of the artificial well wall (17), the upper end and the lower end of the casing (13) are sealed, and the prepared cement is poured into the annulus between the casing (13) and the artificial well wall (17), the kettle body is sealed, and the kettle body is heated and pressurized for curing and solidification; S5, a hole-making step, after the curing period, the kettle is cooled and depressurized, and a sample of the artificial well wall (17), the well wall drilling fluid filter cake (16), the cementing cement ring (14) and the casing (13) that have been cemented together is taken out; a hole is drilled through the side wall of the sample cylinder on one side to form an artificial hole-making channel (8); S6, corrosion experiment steps, after the sample hole is made, the sample is put back into the kettle; the corrosion experiment is carried out; corrosive liquid medium (6) is added into the sample and into the external annulus (15) between the sample and the kettle, and the kettle is sealed; the kettle is heated to a set temperature, and corrosive gas medium is introduced into the external annulus (15) between the sample and the kettle; during the corrosion experiment, the rotation speed of the external motor (2) in the external annulus (15) inside the kettle and the internal motor (19) inside the sample is controlled to simulate the static and flowing states of the corrosive fluid medium; S7. After the corrosion test is completed, the sample is taken out from the kettle body, and the corrosion test results of the artificial well wall (17), the well wall drilling fluid filter cake (16), the cementing cement ring (14), the casing (13) and different cementing interfaces are analyzed by means of macroscopic and microscopic analysis methods; The corrosive liquid medium (6) includes one or more combinations of formation brine, oil-water mixture and crude oil; and the corrosive gas medium is an acidic gas medium.
2. The experimental method for dynamically evaluating the bottom hole corrosion resistance according to claim 1, characterized in that: The upper and lower ends of the artificial well wall (17) are sealed, specifically, sealing material is applied to the upper and lower end surfaces of the artificial well wall (17).
3. The experimental method for dynamically evaluating the bottom hole corrosion resistance according to claim 1, characterized in that: In step S5, a lathe is used to drill holes in the sample, and the vibration generated by the drilling is controlled during the drilling process.
4. The experimental method for dynamically evaluating the bottom hole corrosion resistance according to claim 1, characterized in that: The experimental device also includes a base (11), and the kettle body is assembled on the base (11).
5. The experimental method for dynamically evaluating the bottom hole corrosion resistance according to claim 1, characterized in that: The kettle body and the top cover (3) are fixed and sealed together by bolts.