A preparation method for personalized customized porcelain teeth
Through personalized customized porcelain teeth preparation methods, including multiple sintering and fine grinding, the problem of poor service life of existing porcelain teeth is solved, the strength and aesthetics of porcelain teeth are improved, and the service life is extended.
Patent Information
- Application Number
- CN202210805301.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-08
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2042-07-08
AI Technical Summary
The existing porcelain teeth preparation process is traditional, and the service life of the finished product is poor.
Use personalized customized porcelain teeth preparation methods, including receiving oral model of the patient, filling gypsum, cutting teeth models, soaking wax, embedding materials, centrifugal casting, multiple sintering and polishing to ensure the integrity of the teeth and the metal porcelain teeth. The crown thickness and surface smoothness enhance the strength and aesthetics of porcelain teeth.
Through multiple sintering and fine grinding, the dense performance and surface finish of porcelain teeth are improved, the service life is extended, and the integrity of the tooth morphology and the strength and aesthetics of metal porcelain teeth are improved.
Smart Images

Figure CN115006029B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of denture preparation methods, and in particular to a preparation method for personalized customized porcelain teeth. Background Art
[0002] Dentures are what people often call false teeth, just like artificial legs and limbs are called artificial limbs. Dentures mean teeth that fulfill their duties for humans. In medicine, it is a general term for restorations made after partial or complete tooth loss in the upper and lower teeth. Dentures are divided into removable and fixed. Fixed dentures cannot be taken on and off by the patient themselves, while removable dentures can be taken on and off conveniently by the patient.
[0003] The invention patent with Chinese patent application number 202110479527.7 discloses a method for preparing dentures, which belongs to the field of denture processing technology, and specifically relates to a method for preparing dentures, comprising the following steps: (1) obtaining a three-dimensional model of the patient's oral cavity; (2) designing a base, and designing a paraffin base tooth on the base; (3) designing multiple tooth monomers according to the base; (4) selecting a block of zirconium oxide, sintering the block of zirconium oxide, and then cutting to obtain a zirconium oxide tooth, reserving a retention hole at the bottom of the zirconium oxide tooth, and re-sintering the zirconium oxide tooth; trimming the re-sintered zirconium oxide tooth, and then glazing it; (5) preliminarily arranging the processed zirconium oxide teeth in order and fixing them on the paraffin base teeth of the base; (6) finally fixing the zirconium oxide teeth by embedding filling or injection filling to obtain a denture. The above scheme can be used to customize dentures according to the patient's condition. In addition to being more suitable for individuals, the use of zirconium oxide to make teeth has better performance in terms of strength, aesthetics, color, etc. However, in the process of personalized customization of dentures, since the base teeth are not completely damaged and cannot be used, most consumers tend to make caps to cover the base teeth. On the one hand, it will not produce a foreign body sensation, and on the other hand, it can be adapted to the original base teeth and have good stability. Porcelain teeth came into being. Porcelain teeth are also called porcelain crowns. The crown means a cap. Most existing porcelain crowns are made of a single material and structure. They are prepared by the factory after being received by the dentist's clinic. The hardness of the dentures after production is poor and the service life is not long. Summary of the invention
[0004] Therefore, in view of the above problems, the present invention proposes a method for preparing personalized customized porcelain teeth, which solves the technical problems of traditional process and poor service life of finished products in the existing porcelain teeth preparation process.
[0005] To achieve the above object, the present invention adopts the following technical solution: a method for preparing a personalized customized porcelain tooth, comprising the following steps:
[0006] 1) Receive oral models from patients, register and disinfect the oral models;
[0007] 2) Fill the oral model with plaster and shake it back and forth five to eight times. After waiting for thirty to fifty minutes for the plaster to completely solidify, remove the plaster to obtain a tooth model consistent with the patient's oral cavity;
[0008] 3) Place the tooth model on a standard base for positioning;
[0009] 4) Cut the tooth model, separate the teeth that need to be operated, and trim their neck edges with a grinder;
[0010] 5) Waxing: immersing the trimmed teeth in liquid wax so that the outer part of the teeth is completely covered with the liquid wax, and the liquid wax is air-dried and solidified, and then taken out to obtain a wax-type porcelain crown;
[0011] 6) Seal the neck edge of the wax-type porcelain crown and then insert the casting channel;
[0012] 7) Use the embedding material to completely embed the wax-type porcelain crown after the sprue is inserted, and wait for the embedding material to solidify;
[0013] 8) Burning the ring, placing the embedded material into the ring burning furnace and burning the ring;
[0014] 9) Place the investment material on the centrifugal casting machine with tongs, rotate the hollow rotating shaft clockwise for three to five turns until it is in standby mode, add the specified metal powder, heat the metal powder, and make it molten and then flow into the wax-type porcelain crown along the casting channel. The centrifugal casting machine starts working, and the molten metal fills the entire wax-type cavity under the action of centrifugal force;
[0015] 10) Obtaining the metal porcelain dental crown, cutting the sprue, grinding and polishing the metal porcelain dental crown, applying opaque porcelain, and then placing it in a sintering furnace for the first sintering, with a sintering target temperature of 800-900 degrees Celsius and a holding time of 90-120 minutes;
[0016] 11) The upper body porcelain is then placed in a sintering furnace for a second sintering. The heating efficiency during the sintering process is 8 degrees Celsius / minute, the sintering target temperature is 1200 degrees Celsius, and the holding time is 0 minutes;
[0017] 12) Grinding and polishing, adjusting the occlusal relationship, glazing, and then sintering for the third time, with the sintering target temperature of 200 degrees Celsius and the holding time of 45-60 minutes;
[0018] 13) Surface cleaning, disinfection, done.
[0019] Furthermore, in step 4), the bottom of the tooth is firstly smoothed by a grinder, and then the excess plaster tumors on the tooth are trimmed to make the tooth shape clear and complete.
[0020] Furthermore, after step 11) is completed, the thickness of the metal porcelain crown is greater than or equal to 0.7 mm.
[0021] Furthermore, the body porcelain includes dentin porcelain and enamel porcelain.
[0022] Furthermore, the surface roughness Ra of the metal porcelain crown after grinding and polishing in step 12) is less than or equal to 0.025 microns.
[0023] Furthermore, in step 4), the grinder comprises a cylindrical handle, a rotary motor built in the handle, a clamping groove integrally formed with the output end of the rotary motor, and a grinding head movably connected with the clamping groove, wherein the grinding head comprises an extension portion and a grinding portion, wherein the extension portion is 4-6 cm in length, and the grinding portion comprises a first grinding portion, a second grinding portion and a third grinding portion integrally formed thereon;
[0024] The first polishing portion is close to one side of the extension portion, and the first polishing portion is a hemispherical structure;
[0025] The second polishing portion is a cylindrical structure, and the height of the second polishing portion is 1-3 mm;
[0026] The third grinding portion is a conical structure, and the height of the third grinding portion is 3-5 mm.
[0027] Furthermore, the grinder is provided with a recovery mechanism for recovering tooth scraps, the recovery mechanism comprising a bowl-shaped recovery plate fixedly provided on the handle and a recovery tube built into the handle, the recovery plate is provided with a recovery through hole, the recovery tube is connected to the recovery through hole, and the angle between the recovery plate and the axis of the handle is 45°-60°.
[0028] Furthermore, the centrifugal casting machine includes a reactor, a hollow rotating shaft vertically set at the center of the reactor, a liquid inlet is arranged on the top of the hollow rotating shaft, a circulation pipe for the circulation of molten metal is integrally formed on the hollow rotating shaft, the circulation pipe and the hollow rotating shaft are interconnected, a first clamping portion for clamping the embedding material model is arranged on the free end of the circulation pipe, a clamping ring that can rotate freely 360° along the central axis of the reactor is arranged around the inner side wall of the reactor, and a second clamping portion for clamping the embedding material model is arranged on the clamping ring.
[0029] Furthermore, the circulation pipe is inclined downward along the horizontal plane, and the angle between the circulation pipe and the hollow rotation axis is 45°-60°.
[0030] Furthermore, a cooling fan is provided at the bottom of the reactor, and the cooling fan is arranged around the hollow rotating shaft.
[0031] By adopting the above technical solution, the beneficial effects of the present invention are:
[0032] 1. Fill the oral model with plaster and shake it back and forth five to eight times. This step can eliminate the bubbles in the plaster and ensure the integrity of the tooth model. By placing the tooth model on a standard base, it is convenient to cut the individual tooth model later. By rotating the hollow rotating shaft clockwise for three to five times to the standby state, the purpose is to check whether the centrifugal casting machine rotates smoothly. The first sintering temperature is 800-900 degrees Celsius, and the temperature is maintained for 90-120 minutes. At the above temperature, the solid particles of the opaque porcelain green body are mutually bonded, the grains grow, and the voids (pores) and grain boundaries gradually decrease. Through the transfer of matter, its total volume shrinks and the density increases, and finally it becomes a dense polycrystalline sintered body with a microstructure. After sintering, the opaque porcelain has better density. During the process of body porcelain, the body porcelain Used to restore the original shape of teeth, body porcelain includes dentin porcelain and enamel porcelain. Since instantaneous high-temperature sintering will cause the color of body porcelain to change, which will affect subsequent work, during the second sintering process, the porcelain tooth is placed in the sintering furnace at room temperature. The heating efficiency during the sintering process is 8 degrees Celsius / minute. When the sintering target temperature reaches 1200 degrees Celsius, the porcelain tooth is taken out and cooled naturally. The slow heating process can ensure that the surface temperature of the body porcelain will not change; the third sintering is carried out after glazing. The purpose of the third sintering is mainly to make the glaze layer firmly adhere to the porcelain tooth. The purpose of the glaze layer is to ensure the smoothness of the surface of the porcelain tooth. The sintering target temperature is 200 degrees Celsius and the insulation time is 45-60 minutes. Through medium and low temperature insulation treatment, the glaze layer structure can be dense and firmly adhere to the porcelain tooth.
[0033] 2. In step 4), the bottom of the tooth is first smoothed by a grinder, and then the excess plaster tumors on the tooth are trimmed to make the tooth shape clear and complete. Ensuring a clear and complete tooth shape can improve the accuracy of the wax model in the subsequent wax dipping process. The wax model is relatively fragile, and secondary processing of the wax model can easily damage the wax model.
[0034] 3. After step 11) is completed, the thickness of the inner crown of the metal porcelain tooth is greater than or equal to 0.7mm. Usually, the vertical height from the inner top surface to the outer surface of the finished porcelain tooth is 2.5mm-3.5mm. The inner crown mainly plays the role of matching and supporting the original teeth, and bears half of the overall strength of the porcelain tooth. Therefore, increasing the thickness of the inner crown of the porcelain tooth can greatly enhance the overall strength of the porcelain tooth.
[0035] 4. In step 12), the surface roughness Ra of the metal porcelain crown after grinding and polishing is less than or equal to 0.025 microns. After grinding and polishing, the finished porcelain crown is obtained, and its surface roughness should be flat and smooth in visual effect. Ra should be controlled within 0.025, that is, Ra should be greater than or equal to level 13.
[0036] 5. The grinding part of the grinder includes the first grinding part, the second grinding part and the third grinding part which are integrally formed. Since the tooth surface is irregular and concave and convex, the first grinding part is a hemispherical structure, which is responsible for line grinding of the porcelain tooth, the second grinding part is a cylindrical structure, which is responsible for surface grinding of the porcelain tooth, and the third grinding part is a conical structure, which is responsible for point grinding of the uneven parts on the surface of the porcelain tooth. As known in the industry, in the process of grinding porcelain teeth, workers need to hold the porcelain tooth in one hand and the grinder in the other hand for grinding. When grinding different parts, the grinding head needs to be replaced. Since porcelain teeth are precision accessories, point, line and surface grinding is very important. If there is an error in the grinding, it will have a great impact on the overall appearance of the porcelain tooth, and it will also cause discomfort to the patient after wearing it. The fine grinding operation requires high-intensity concentration. Frequent replacement of grinding heads can easily distract the staff's original concentration. At the same time, the original gripping strength will also change. As a result, after replacing the grinding head, it is often necessary to practice with practice models to regain the strength. The whole process is time-consuming and laborious, which reduces the grinding efficiency and makes the workers more tired. The integrated grinding head avoids the above problems, and it can perform point, line and surface grinding operations on the same metal porcelain tooth in the same grinding process.
[0037] 6. Normally, metal porcelain teeth need to be polished again according to the occlusal conditions after being worn on the oral model. Some patients are asked to give their own feedback on the occlusal conditions after wearing them, and then the dentist performs polishing operations directly according to the patient's feedback. At this time, the construction environment is directly in the patient's mouth. By setting up a recycling mechanism for recycling tooth chips, the debris generated by the grinding process can be absorbed at the first time, avoiding tooth chips from splashing into the patient's mouth or body and causing discomfort during the grinding process. Even if the construction environment is not in the patient's mouth, the recycling mechanism is necessary to ensure the cleanliness of the surrounding environment. Tooth chips are made of a special material, different from other materials. They are hard materials. If the tooth chips are not cleaned, the surrounding environment will be polluted. Tooth chips may enter people's clothes and cause discomfort to the human epidermis.
[0038] 7. The centrifugal casting machine is provided with a first clamping part and a second clamping part, which can clamp the front and back of the embedded material model at the same time during the operation of the centrifugal casting machine, thereby preventing the embedded material model from shaking or shifting during the rotation process.
[0039] 8. The circulation pipe is inclined downward along the horizontal plane, and the angle between it and the hollow rotating shaft is 45°-60°. During the operation of the centrifugal casting machine, the hollow rotating shaft rotates, and the molten metal in the circulation pipe is subjected to its own downward gravity and the centrifugal force horizontally outward along the hollow rotating shaft during the rotation process. The combined force of the two is the force inclined downward along the hollow rotating shaft. The circulation pipe is inclined downward, which is consistent with the direction of the combined force, so that the molten metal can flow smoothly into the cavity during the rotation process, which effectively eliminates the problem of insufficient density caused by the inconsistency between the circulation pipe and the combined force direction.
[0040] 9. A cooling fan is arranged at the bottom of the reactor, and the cooling fan is arranged around the hollow rotating shaft to cool the molten metal immediately after the centrifugal casting machine completes its work. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] Figure 1 It is a schematic diagram of the overall structure of the grinding machine in the present invention;
[0042] Figure 2 It is a front view of the grinding machine of the present invention;
[0043] Figure 3 It is a cross-sectional view of the clamping groove structure of the grinder in the present invention;
[0044] Figure 4 yes Figure 3 Enlarged view of point A in the middle;
[0045] Figure 5 It is a top view of the grinding machine recovery mechanism of the present invention;
[0046] Figure 6 It is a schematic diagram of the internal structure of the centrifugal casting machine in the present invention;
[0047] Figure 7 yes Figure 6 Enlarged view of point B in the middle;
[0048] Figure 8 It is a schematic diagram of the force on the molten metal when the centrifugal casting machine of the present invention is running. DETAILED DESCRIPTION
[0049] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.
[0050] refer to Figures 1 to 8 This embodiment 1 proposes a method for preparing a personalized customized porcelain tooth, comprising the following steps:
[0051] 1) Receive oral models from patients, register and disinfect the oral models;
[0052] 2) Fill the oral model with plaster and shake it back and forth five to eight times. After waiting for thirty to fifty minutes for the plaster to completely solidify, remove the plaster to obtain a tooth model consistent with the patient's oral cavity;
[0053] 3) Place the tooth model on a standard base for positioning;
[0054] 4) Cut the tooth model, separate the teeth that need to be operated, and trim their neck edges with a grinder;
[0055] 5) Waxing: immersing the trimmed teeth in liquid wax so that the outer part of the teeth is completely covered with the liquid wax, and the liquid wax is air-dried and solidified, and then taken out to obtain a wax-type porcelain crown;
[0056] 6) Seal the neck edge of the wax-type porcelain crown and then insert the casting channel;
[0057] 7) Use the embedding material to completely embed the wax-type porcelain crown after the sprue is inserted, and wait for the embedding material to solidify;
[0058] 8) Burning the ring, placing the embedded material into the ring burning furnace and burning the ring;
[0059] 9) Place the investment material on the centrifugal casting machine with tongs, rotate the hollow rotating shaft clockwise for three to five turns until it is in standby mode, add the specified metal powder, heat the metal powder, and make it molten and then flow into the wax-type porcelain crown along the casting channel. The centrifugal casting machine starts working, and the molten metal fills the entire wax-type cavity under the action of centrifugal force;
[0060] 10) Obtaining the metal porcelain dental crown, cutting the sprue, grinding and polishing the metal porcelain dental crown, applying opaque porcelain, and then placing it in a sintering furnace for the first sintering, with a sintering target temperature of 800 degrees Celsius and a holding time of 90 minutes;
[0061] 11) The upper body porcelain is then placed in a sintering furnace for a second sintering. The heating efficiency during the sintering process is 8 degrees Celsius / minute, the sintering target temperature is 1200 degrees Celsius, and the holding time is 0 minutes;
[0062] 12) Grinding and polishing, adjusting the occlusal relationship, glazing, and then sintering for the third time, with the sintering target temperature of 200 degrees Celsius and the holding time of 45 minutes;
[0063] 13) Surface cleaning, disinfection, done.
[0064] In the above method, in step 4), the bottom of the tooth needs to be firstly leveled by a grinder, and then the excess plaster tumors on the tooth are trimmed to make the tooth shape clear and complete. In step 11), the thickness of the metal porcelain crown after the upper body porcelain is completed is 0.7 mm, and the body porcelain includes dentin porcelain and enamel porcelain, wherein the dentin porcelain and enamel porcelain are both known materials and will not be described in detail here. In step 12), the surface roughness Ra of the metal porcelain crown after grinding and polishing is 0.025 microns.
[0065] In step 4), the grinding machine includes a cylindrical handle 1, a rotary motor (known driving component) built into the handle 1, a clamping slot 13 integrally formed with the output end 11 of the rotary motor, and a grinding head 2 movably connected to the clamping slot 13. The grinding head 2 includes an extension portion 21 and a grinding portion 22. The extension portion 21 is 4 cm long. The extension portion 21 keeps the handle 1 away from the denture to be ground, facilitating the grinding operation. The grinding portion 22 includes an integrally formed first grinding portion 223, a second grinding portion 222, and a third grinding portion 221.
[0066] The first grinding portion 223 is close to one side of the extension portion 21, and the first grinding portion 223 is a hemispherical structure, which is convenient for grinding the edge where the top surface and the side surface of the denture meet;
[0067] The second grinding part 222 is a cylindrical structure, and the height of the second grinding part is 3 mm; the cylindrical structure is convenient for grinding the side of the denture;
[0068] The third grinding part 221 is a conical structure, and the height of the third grinding part is 3 mm; the conical structure provides point grinding, which is convenient for grinding the grooved part on the top surface of the denture.
[0069] Through the grinding parts with different structures, the same denture can be completely ground without changing the grinding head, which reduces the working hours of changing the grinding head and improves the work efficiency.
[0070] The grinding machine is provided with a recovery mechanism for recovering tooth scraps, the recovery mechanism comprises a bowl-shaped recovery plate 3 fixedly provided on the handle 1 and a recovery tube 12 built into the handle 1, the recovery plate 3 is provided with a recovery through hole 31, the recovery tube 12 is connected to the recovery through hole 31, the included angle α between the recovery plate 3 and the axis of the handle 1 is 45°, and can actually be adjusted between 45°-60°, such as 55° or 60°, the recovery plate 3 adopts a bowl-shaped structure, and cooperates with the recovery through hole 31 thereon, so that it is like a cover, and a negative pressure environment is formed in its surrounding area, and the dust and small particles of tooth scraps generated during the grinding process will be restricted by it and recovered through the recovery through hole 31;
[0071] The centrifugal casting machine includes a reactor 4, a hollow rotating shaft 5 vertically set up at the center of the reactor 4, the hollow rotating shaft 5 is driven to rotate by a motor, a liquid inlet 51 is arranged on the top of the hollow rotating shaft 5, a circulation pipe 7 for the circulation of molten metal is integrally formed on the hollow rotating shaft 5, the circulation pipe 7 and the hollow rotating shaft 5 are mutually connected, a first clamping portion 71 for clamping the embedding material model is arranged on the free end of the circulation pipe 7, a clamping ring 41 which can rotate freely 360° along the central axis of the reactor 1 is arranged around the inner side wall of the reactor 1, the clamping ring 41 passively follows the rotation when the hollow rotating shaft rotates, and is connected to the inner side wall of the reactor 4 by a ball, and the structure is like the inner and outer rings of a ball bearing, the clamping ring 4 1 is provided with a second clamping portion 411 for clamping the embedding material model C, which is used in conjunction with the embedding material model C so that both ends of the embedding material model C can be clamped without being separated from the equipment due to the centrifugal force, causing safety hazards. The circulation pipeline 7 is inclined downward along the horizontal plane, and the angle β between it and the hollow rotating shaft is 45°. In fact, the centrifugal force can be further determined according to the rotation direction of the hollow rotating shaft 5. Combined with the gravity of the molten metal, the angle β is adjusted within the range of 45°-60°, such as 55° or 60°. A cooling fan 6 is provided at the bottom of the reactor 1. The cooling fan 6 is arranged around the hollow rotating shaft 5, and can cool the molten metal in the embedding material model C as soon as possible after the centrifugal work, so that it can solidify as soon as possible.
[0072] The slot 13 of the grinder is covered with a rubber layer 131, and a locking protrusion 133 is provided for fixing with the extension part 21. The locking protrusion 133 is arranged in the slot through a spring 132. The purpose of covering the rubber layer 131 is that during the grinding process, since the denture is mostly fixed on the claws or manually held, and the grinding head 2 and the denture are both made of hard materials, if the operator does not have a good grasp of the force during the contact between the two, the denture is easy to break or be bounced off. Therefore, the rubber layer 131 is covered in the slot 13, which plays a role of buffering and shock absorption, so that there is a certain buffering displacement space when the grinding head 2 contacts the denture, to avoid the denture from breaking or being bounced off due to poor grasp of the force.
[0073] refer to Figure 8 , which shows the force applied to the molten metal during the centrifugal operation in the centrifugal casting machine, wherein the centrifugal force is F1, the weight of the molten metal itself is G, and the direction of the resultant force is F2. The direction of the resultant force F2 is consistent with the direction of the flow pipe 7, which can ensure that the flow resistance of the molten metal in the flow pipe 7 is minimal, thereby improving the work efficiency and ensuring that the embedding material model C can be filled completely.
[0074] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.
Claims
1. A method for preparing a personalized porcelain tooth, characterized in that: The following steps are involved: 1) Receive oral models from patients, register and disinfect them; 2) Fill the oral model with plaster and shake it back and forth five to eight times. After waiting for thirty to fifty minutes for the plaster to completely solidify, remove the plaster to obtain a tooth model consistent with the patient's mouth; 3) Place the tooth model on a standard base for positioning; 4) Cut the tooth model, separate the teeth to be operated, and trim the neck edges with a grinder. First, the bottom of the teeth is flattened by the grinder, and then the excess plaster tumors on the teeth are trimmed to make the tooth shape clear and complete. The grinder includes a cylindrical handle, a rotating motor built into the handle, a clamping groove integrally formed with the output end of the rotating motor, and a grinding head movably connected to the clamping groove. The grinding head includes an extension part and a grinding part. The extension part is 4-6 cm long. The grinding part includes a first grinding part, a second grinding part and a third grinding part integrally formed. The first grinding part is close to one side of the extension part, the first grinding part is a hemispherical structure, the second grinding part is a cylindrical structure, the height of the second grinding part is 1-3mm, the third grinding part is a conical structure, the height of the third grinding part is 3-5mm, the grinding machine is provided with a recovery mechanism for recovering tooth scraps, the recovery mechanism includes a bowl-shaped recovery plate fixedly provided on the handle and a recovery tube built into the handle, the recovery plate is provided with a recovery through hole, the recovery tube is connected to the recovery through hole, and the recovery plate and the axis of the handle are at an angle of 45°-60°; 5) Wax dipping: immerse the trimmed teeth in liquid wax so that the outer part of the teeth is completely covered with liquid wax. Wait for the liquid wax to air dry and solidify, then take it out to obtain a wax-type porcelain crown; 6) Seal the neck edge of the wax-type porcelain crown and then insert the casting channel; 7) Use the embedding material to completely embed the wax-type porcelain crown after the casting channel is placed, and wait for the embedding material to solidify; 8) Burning ring: put the embedded material into the burning ring furnace and burn it; 9) Use pliers to place the embedding material on the centrifugal casting machine, rotate the hollow rotating shaft clockwise for three to five circles to the standby state, put in the specified metal powder, heat the metal powder, make it molten, and then flow into the wax-type porcelain crown along the casting channel, the centrifugal casting machine starts to work, and the molten metal fills the entire wax-type cavity under the action of centrifugal force. The centrifugal casting machine includes a reactor, a hollow rotating shaft vertically set at the center of the reactor, a liquid inlet is arranged on the top of the hollow rotating shaft, a circulation pipe for the circulation of molten metal is integrally formed on the hollow rotating shaft, the circulation pipe and the hollow rotating shaft are mutually connected, a first clamping part for clamping the embedding material model is arranged on the free end of the circulation pipe, a clamping ring that can rotate freely 360° along the central axis of the reactor is arranged around the inner side wall of the reactor, and a second clamping part for clamping the embedding material model is arranged on the clamping ring; 10) Obtain the metal porcelain dental crown, cut the casting channel, grind and polish the metal porcelain dental crown, apply opaque porcelain, and then put it into the sintering furnace for the first sintering. The sintering target temperature is 800-900 degrees Celsius and the holding time is 90-120 minutes; 11) The upper body porcelain is then placed in a sintering furnace for a second sintering. The heating efficiency during the sintering process is 8 degrees Celsius / minute, the sintering target temperature is 1200 degrees Celsius, and the holding time is 0 minutes; 12) Grinding and polishing, adjusting the occlusal relationship, glazing, and then sintering for the third time. The sintering target temperature is 200 degrees Celsius and the holding time is 45-60 minutes; 13) Surface cleaning, disinfection, done.
2. The method for preparing a personalized customized porcelain tooth according to claim 1, characterized in that: Step 11) After completion, the thickness of the metal porcelain crown is greater than or equal to 0.7mm.
3. The method for preparing a personalized customized porcelain tooth according to claim 2, characterized in that: The body porcelain includes dentin porcelain and enamel porcelain.
4. The method for preparing a personalized customized porcelain tooth according to claim 1, characterized in that: The surface roughness Ra of the metal porcelain crown after grinding and polishing in step 12) is less than or equal to 0.025 microns.
5. The method for preparing a personalized porcelain tooth according to claim 1, characterized in that: The circulation pipe is inclined downward along the horizontal plane, and the angle between the circulation pipe and the hollow rotation axis is 45°-60°.
6. The method for preparing a personalized porcelain tooth according to claim 5, characterized in that: A cooling fan is arranged at the bottom of the reaction kettle, and the cooling fan is arranged around the hollow rotating shaft.