A diffuse laminar flow reaction chamber and control method
By using diffuse laminar flow reaction chambers and control methods in semiconductor manufacturing, laminar flow interface layers and diffuse interface layers are formed, which solves the problem of temperature uniformity difficulties in cold wall cavities and impurity particles in hot wall cavities, and improves substrate efficiency. Temperature uniformity and process efficiency reduce vapor nucleation and particulate matter generation.
Patent Information
- Application Number
- CN202211330849.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-27
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2042-10-27
AI Technical Summary
In semiconductor manufacturing, the large temperature gradient in the cold wall cavity makes it difficult to control the uniformity of the substrate temperature, and there are more impurity particles generated by gas phase reactions in the hot wall cavity, which affects the quality of the process.
Using a diffuse laminar flow reaction chamber, a laminar flow interface layer is formed on the substrate surface, and a diffuse interface layer is formed on it. Materials such as porous plates, ceramics or transparent quartz are used as diffuse surfaces to adjust the process gas flow rate and laminar flow interface. layer thickness to reduce gas phase nucleation and the generation of particulate matter.
The substrate temperature uniformity and growth rate are improved, gas nucleation and particulate matter on the reaction chamber wall are reduced, the generation of deposits is reduced, and the efficiency and quality of the chemical vapor deposition process are improved.
Smart Images

Figure CN115537781B_ABST
Abstract
Description
Technical Field
[0001] The present invention generally relates to the field of semiconductor manufacturing technology. Specifically, the present invention relates to a diffuse laminar flow reaction chamber and a control method. Background Art
[0002] There are a large number of gas phase chemical processes in the semiconductor and pan-semiconductor industries, especially chemical vapor deposition processes. Chemical vapor deposition processes usually require high temperatures to activate the reaction gas. According to the temperature of the reaction chamber relative to the substrate being processed (such as silicon wafers, gallium nitride, etc.), the reaction chamber is usually divided into a hot wall chamber and a cold wall chamber. The hot wall chamber refers to a chamber whose wall temperature is higher than the substrate temperature, and the cold wall chamber refers to a chamber whose wall temperature is lower than the substrate temperature.
[0003] Figure 1 FIG. 2 shows a schematic diagram of the structure of a cold wall cavity in the prior art. Figure 1 As shown, the cold wall cavity is a quartz cavity with multiple sealing flange surfaces that can be sealed with a metal flange through a sealing ring. Infrared light is used to heat the outside of the cold wall cavity. Since the cavity wall temperature is too high, the reaction precursor will be deposited on the cavity wall, thereby preventing the infrared light from transmitting on the cavity wall. Therefore, the temperature of the cavity wall must be reduced to below the starting temperature of the deposition reaction. Traditionally, a high-speed fan is usually used to air-cool the surface of the quartz cavity to inhibit the deposition of the reaction precursor on the cavity wall.
[0004] In a cold wall cavity, there is a greater temperature gradient between the cold wall and the substrate than in a hot wall cavity. Therefore, it is more difficult to control the temperature uniformity of the substrate in a cold wall cavity under high temperature conditions, which is more technically challenging. In a hot wall cavity, due to the smaller temperature gradient, better temperature uniformity can be achieved on the substrate and the growth rate is also higher. However, in a hot wall cavity, the space between the cavity wall and the substrate meets the conditions for gas phase reaction generation, so gas phase reaction may occur in this space to generate particles, which will produce more impurity particles. Summary of the invention
[0005] In order to at least partially solve the above problems in the prior art, the present invention provides a diffuse laminar flow reaction chamber, characterized in that it comprises:
[0006] Substrate and / or base;
[0007] a main gas inlet configured to inject a process gas into the reaction chamber to form a laminar interface layer on a surface of the substrate; and
[0008] The diffuse surface is configured to inject or suck diffuse gas into or out of the reaction chamber to form a diffuse interface layer on the laminar interface layer.
[0009] In one embodiment of the present invention, it is provided that the diffuse interface layer is configured so that the flow rate of the process gas is increased, and / or
[0010] The diffuse interface layer reduces the thickness of the laminar interface layer.
[0011] In one embodiment of the present invention, it is provided that the diffusion surface comprises a porous plate, porous ceramics, porous transparent quartz or a permeable membrane.
[0012] In one embodiment of the present invention, it is provided that microchannels are arranged on the diffusion surface.
[0013] In one embodiment of the present invention, it is provided that the diffuse laminar flow reaction chamber further comprises:
[0014] A heater is arranged inside and / or outside the diffuse laminar flow reaction chamber, and the heater is configured to heat the substrate.
[0015] In one embodiment of the present invention, it is provided that the diffuse laminar flow reaction chamber further comprises:
[0016] A preheat ring surrounds the substrate, wherein the preheat ring is configured to heat the substrate.
[0017] In one embodiment of the present invention, it is provided that the diffuse laminar flow reaction chamber further comprises:
[0018] The base is rotatable, and the preheating ring is arranged around the base.
[0019] In one embodiment of the present invention, it is provided that the preheating ring is an integrated heating ring such that there is no gap under the heating ring for process gas to enter.
[0020] In one embodiment of the present invention, it is provided that the diffusion surface is arranged on an upper wall of the chamber above the substrate; and / or
[0021] The diffusion surface is arranged at the lower wall of the chamber below the substrate so as to purge the bottom to reduce the impact on the substrate process.
[0022] In one embodiment of the present invention, it is provided that the chamber upper wall and / or the chamber lower wall is dome-shaped.
[0023] In one embodiment of the present invention, it is provided that the diffuse gas is injected from the microchannel to form a diffuse surface, and the height of the diffuse surface is represented by d 0 -d 1 , the laminar flow process gas is compressed, and the thickness of the laminar interface layer is expressed as follows:
[0024]
[0025] where d 0 represents the distance between the substrate and the upper wall of the cavity, d 1 represents the distance between the lower interface of the diffuse surface and the substrate, x represents the horizontal coordinate, δ(x) 0 It is the thickness of the laminar interface layer when no diffuse surface is formed.
[0026] In one embodiment of the present invention, it is provided that the diffusion flux of the substrate It is expressed as follows:
[0027]
[0028] Where P par Indicates the partial pressure of gas, P S represents the gas surface pressure, T′ represents the local temperature of the substrate, J represents the molar flow rate of the carrier gas, ρ g Indicates the density of the airflow, μ g It is the dynamic viscosity of the airflow, P tot Indicates total pressure, R represents the gas constant, A represents the cross-sectional area of the cavity, and D represents the gas diffusion coefficient.
[0029] The gas phase reaction rate on the substrate depends on the diffusion flux By adjusting the parameters in the above formula, the To increase the reaction speed.
[0030] In one embodiment of the present invention, it is provided that the diffuse interface layer is used to compress the characteristic size of the cavity, reduce the Reynolds coefficient of the substrate laminar flow, and thus increase the growth rate.
[0031] In one embodiment of the present invention, it is provided that the substrate and / or the base is parallel to the diffusion surface;
[0032] The direction of injection of the main process gas is parallel to the substrate;
[0033] The diffusely injected gas has a component perpendicular to the substrate.
[0034] In one embodiment of the present invention, it is provided that the diffuse laminar flow reaction chamber includes one or more of the following structural features:
[0035] The diffuse laminar flow reaction chamber is heated on one side or two sides;
[0036] The top of the diffuse laminar flow reaction chamber is: A infrared transparent wall, through which the external infrared heater heats by transmission; B infrared blocking wall; or C dome heating wall.
[0037] The present invention proposes a diffuse laminar flow control method, using the diffuse laminar flow reaction chamber, the method comprises the following steps:
[0038] injecting a process gas into the reaction chamber from a main gas inlet to form a laminar interface layer on a surface of the substrate; and
[0039] A diffuse gas is injected into or sucked out of the reaction chamber to form a diffuse interface layer on the laminar interface layer, wherein the diffuse interface layer is configured to increase the flow rate of the process gas and reduce the thickness of the laminar interface layer.
[0040] In one embodiment of the present invention, it is provided that the diffuse laminar flow control method further comprises:
[0041] The thickness of the diffuse interface layer is adjusted to adjust the flow rate of the process gas and the thickness of the laminar interface layer, wherein the thickness of the diffuse interface layer is adjusted by adjusting the temperature of the diffuse surface and / or adjusting the height of the diffuse surface.
[0042] In one embodiment of the present invention, it is provided that the diffuse laminar flow control method further comprises:
[0043] uniformly injecting the diffusion gas into the reaction chamber on the diffusion surface; or
[0044] The amount of diffuse gas injected on the diffuse surface is decreased exponentially or linearly along the direction of process gas injection.
[0045] In one embodiment of the present invention, it is provided that the diffuse gas increases the thickness of the diffuse interface layer, reduces gas phase nucleation on the diffuse surface leading to generation of particles and / or defects on the substrate and / or reduces deposition on the diffuse surface.
[0046] In one embodiment of the present invention, it is provided that the diffuse gas is an inert gas or an inactive gas to reduce the content of the reaction precursor in the diffuse boundary layer, and reduce the generation of particles and / or defects on the substrate caused by gas phase nucleation on the diffuse surface and / or reduce deposition on the diffuse surface; or
[0047] The diffuse gas is an etching gas, which etches the deposits on the diffuse surface and etches the gas phase nucleation of the diffuse interface layer, thereby reducing the generation of particles and / or defects on the substrate.
[0048] This reduces the deposition on the top of the reaction chamber, allowing the transparent top to operate at a temperature higher than the non-diffuse controlled top temperature without generating deposition.
[0049] In one embodiment of the present invention, the deposition on the diffuse surface is minimized so that the quartz cold wall external heater chamber relying on infrared transmission can operate at a temperature point higher than the traditional temperature. The increased temperature of the diffuse surface further thins the boundary layer of the substrate.
[0050] In one embodiment of the invention, it is provided that the physical height of the diffusion surface is adjusted in order to optimize the respective process result.
[0051] In one embodiment of the present invention, it is provided that the total bottom purge flow rate and the corresponding purge flow rate distribution are adjusted to further optimize the purge effect and reduce the impact on the substrate process.
[0052] In one embodiment of the present invention, it is provided that an etching gas is added to the bottom diffuse purge gas so as to etch away the bottom deposits in real time during the process production.
[0053] In one embodiment of the present invention, it is provided that the diffuse interface layer makes the laminar interface layer thinner, thereby improving the deposition speed and / or uniformity of the film formation.
[0054] The present invention has at least the following beneficial effects: the present invention proposes a diffuse laminar flow reaction chamber and a control method, by forming a diffuse interface layer on the laminar interface layer, the flow rate of the process gas can be increased and the thickness of the laminar interface layer can be reduced, thereby accelerating the reaction speed and inhibiting gas phase nucleation on the reaction chamber wall and reducing particles in the reaction process. BRIEF DESCRIPTION OF THE DRAWINGS
[0055] To further illustrate the advantages and features of various embodiments of the present invention, a more detailed description of various embodiments of the present invention will be presented with reference to the accompanying drawings. It will be understood that these drawings only depict typical embodiments of the present invention and are therefore not to be considered as limiting the scope thereof. In the accompanying drawings, for clarity, identical or corresponding parts will be represented by identical or similar reference numerals.
[0056] Figure 1 The figure shows a schematic structural diagram of a cold wall cavity in the prior art.
[0057] Figure 2 A schematic diagram showing the principle of the interface layer theory.
[0058] Figure 3 A schematic structural diagram of a diffuse laminar flow reaction chamber in one embodiment of the present invention is shown.
[0059] Figure 4 A schematic diagram showing fluid velocity distribution and gas streamlines in a process chamber according to an embodiment of the present invention is shown.
[0060] Figure 5 A schematic diagram showing the effect of diffuse surface on chemical vapor deposition process according to one embodiment of the present invention.
[0061] Fig. 6A and Figure 6BSchematic diagrams of fluid velocity envelopes in the process chamber when diffuse gas is sucked out from the upper wall of the chamber or injected into the process chamber are shown respectively.
[0062] Figure 7 A schematic diagram of a preheating ring and a heater in a reaction chamber in one embodiment of the present invention is shown.
[0063] Figure 8 A schematic diagram of the component temperatures of a reaction chamber is shown.
[0064] Fig. 9 A schematic diagram of a cookbook showing the relationship between process control parameter input and process result output in one embodiment of the present invention.
[0065] Fig.10 A schematic diagram of a neural network based on input parameters and output results of a chemical vapor deposition process in one embodiment of the present invention is shown.
[0066] Fig.11 A schematic structural diagram of a reaction chamber having an inclined diffusion layer in one embodiment of the present invention is shown.
[0067] Fig.12 A schematic diagram showing fluid velocity distribution and gas streamlines in a process chamber having an inclined diffuse layer according to an embodiment of the present invention is shown.
[0068] Fig.13 This is a simulation diagram of hydrogen concentration distribution with diffusion in the upper dome and single-point axial sweeping in the lower dome according to an embodiment of the present invention. DETAILED DESCRIPTION
[0069] It should be noted that the components in the figures may be shown exaggeratedly for the sake of illustration and are not necessarily true to scale. In the figures, identical or functionally identical components are provided with the same reference numerals.
[0070] In the present invention, unless otherwise specified, "arranged on...", "arranged above..." and "arranged above..." do not exclude the existence of an intermediate between the two. In addition, "arranged on or above..." merely indicates the relative positional relationship between two components, and in certain cases, such as after reversing the product direction, it can also be converted into "arranged below or below...", and vice versa.
[0071] In the present invention, each embodiment is only intended to illustrate the aspects of the present invention and should not be construed as limiting.
[0072] In the present invention, unless otherwise specified, the quantifiers "a", "an" and "an" do not exclude the presence of a plurality of elements.
[0073] It should also be noted that in the embodiments of the present invention, for the sake of clarity and simplicity, only a portion of the parts or components may be shown, but those of ordinary skill in the art will understand that under the teachings of the present invention, the required parts or components may be added according to the needs of the specific scenario. In addition, unless otherwise specified, the features in different embodiments of the present invention may be combined with each other. For example, a feature in the second embodiment may be used to replace a corresponding or functionally identical or similar feature in the first embodiment, and the resulting embodiment also falls within the disclosure scope or recorded scope of the present application.
[0074] It should also be noted that within the scope of the present invention, the terms "same", "equal", "equal to" and the like do not mean that the values of the two are absolutely equal, but allow a certain reasonable error, that is, the terms also cover "substantially the same", "substantially equal", "substantially equal to". By analogy, in the present invention, the terms "perpendicular to", "parallel to" and the like indicating directions also cover the meanings of "substantially perpendicular to" and "substantially parallel to".
[0075] In addition, the numbering of the steps of the methods of the present invention does not limit the execution order of the method steps. Unless otherwise specified, the method steps can be executed in different orders.
[0076] The present invention will be further described below in conjunction with specific embodiments with reference to the accompanying drawings.
[0077] The principle on which the present invention is based is described below.
[0078] Figure 2 A schematic diagram of the principle of interface layer theory is shown. Figure 2 As shown, the chemical vapor deposition on the substrate can be represented as the interface layer transmission above the substrate. The arrow 201 represents the fluid velocity vector at each vertical height at the horizontal axis distance x, V 0 Indicates the maximum flow rate, V s represents the flow velocity on the substrate surface, and δv represents the thickness of the interface layer.
[0079] According to the Reynolds number Calculate the thickness of the interface layer δ, expressed as follows
[0080] δ=(x / Re x ) 1 / 2 .
[0081] Reynolds number The calculation can be expressed as follows:
[0082]
[0083] where ρ g represents the density of the airflow, v grepresents the average velocity of the airflow, μ g It represents the dynamic viscosity of the airflow, and d represents the pipe diameter or characteristic dimension.
[0084] Average speed g It can be calculated based on the gas flow rate Q, expressed as the following formula:
[0085] Q=JRT′
[0086]
[0087] Where T' represents the local temperature of the substrate, J represents the molar flow rate of the carrier gas, R represents the gas constant, and P tot represents the total pressure and A represents the cross-sectional area of the cavity.
[0088] According to the above calculation, the thickness of the interface layer can be expressed as follows:
[0089]
[0090] A first-order approximation is made, in which the gas concentration gradient in the boundary layer is assumed to be linear and the diffusion flux of the substrate is It is expressed as follows:
[0091]
[0092] Where P par Indicates the partial pressure of gas, P S represents the gas surface pressure, D represents the gas diffusion coefficient, where the gas phase reaction rate on the substrate depends on the mass transfer on the substrate surface, that is, on the diffusion flux Therefore, the parameters in the above formula can be adjusted to increase To increase the reaction speed. The diffuse laminar flow control method of the present invention is used to reduce the thickness of the boundary layer on the substrate and increase the growth speed of the substrate.
[0093] Figure 3 FIG. 2 shows a schematic diagram of the structure of a diffuse laminar flow reaction chamber in one embodiment of the present invention. Figure 3 As shown, the reaction chamber includes a heater 301 , a preheating ring 302 , a substrate 303 , a chamber upper wall 304 , and a main gas inlet 305 .
[0094] The heater 301 is arranged below the substrate 303, the preheating ring 302 surrounds the substrate 303, the chamber upper wall 304 is arranged above the substrate 303, and the main gas inlet 305 is arranged on the first side of the substrate 303. The process gas enters the reaction chamber from the main gas inlet 305 and flows from the first side to the second side of the substrate 303. The chamber upper wall 304 is constructed so that the diffuse gas flows in or out from the chamber upper wall 304 to form a diffuse surface. The schematic diagram of the fluid velocity envelope in the process chamber when the diffuse gas is sucked out of or injected into the process chamber from the chamber upper wall 304 is shown in FIG. Fig. 6A and Figure 6B As shown, V plate Indicates the speed of the diffuse gas moving downward, V plate >0 means injecting diffuse gas into the process chamber, V plate <0 means that the diffuse gas is sucked out from the process chamber.
[0095] Figure 4 FIG. 1 is a schematic diagram showing the fluid velocity distribution and gas streamlines in a process chamber in one embodiment of the present invention. Figure 4 As shown, the upper wall 304 of the cavity may be an upper plate or dome, and a diffusion channel may be provided on the upper wall 304 of the cavity. The diffusion channel may be a plurality of through holes or micro-pipes, wherein a diffusion gas is injected from the diffusion channel to form a diffusion surface, and flows from the first side to the second side of the substrate 304 along with the process gas. The diffusion gas may be an inert gas etching gas or an inactive gas such as hydrogen, and hydrogen is preferably used when performing a silicon epitaxial process.
[0096] Specifically, Figure 41A is a schematic diagram of the gas velocity distribution in the reaction chamber when a normal upper plate or dome is used; 2A is a schematic diagram of the gas velocity distribution in the chamber when a diffuse upper plate or dome is used in the present invention and the diffuse gas is injected into the reaction chamber; 3A is a schematic diagram of the gas velocity distribution in the chamber when a diffuse upper plate or dome is used in the present invention and the diffuse gas is sucked out of the reaction chamber; 1B is a schematic diagram of the gas streamline in the reaction chamber when a normal upper plate or dome is used in the prior art; 2B is a schematic diagram of the gas streamline in the reaction chamber when a diffuse upper plate or dome is used in the present invention and the diffuse gas is injected into the reaction chamber; 3B is a schematic diagram of the gas streamline in the reaction chamber when a diffuse upper plate or dome is used in the present invention and the diffuse gas is injected into the reaction chamber; dome) and the diffuse gas is sucked out of the reaction chamber, a schematic diagram of the gas streamlines in the reaction chamber.
[0097] Figure 4 In 1A, 2A and 3B, the U-shaped curve between the upper cover plate or dome and the substrate represents the gas velocity contour line, the dotted line starting from the upper cover plate or dome and approaching the center line represents the boundary layer of the upper cover plate or dome, and the dotted line starting from the substrate and approaching the center line represents the substrate boundary layer.
[0098] The purpose of designing a permeable upper plate or dome is first to control the substrate boundary layer thickness and some other important deposition parameters by controlling the boundary layer of the upper plate or dome (the vertical component of the velocity of the diffuse gas provides an important control factor), and secondly, to provide additional upper plate or dome purge protection and / or reduce gas phase nucleation (particle formation), and even to remove plate deposition and / or reduce gas phase nucleation (particle formation) by etching gas.
[0099] Figure 5 FIG. 1 is a schematic diagram showing the effect of diffuse surface on chemical vapor deposition process in one embodiment of the present invention. Figure 5 As shown, where U represents the horizontal flow rate of the process gas, d 0 represents the distance between the substrate 303 and the upper wall 304 of the cavity, d 1represents the distance between the lower interface of the diffusion surface and the substrate 303, and z represents the height of the diffusion surface. The process gas flows into the reaction chamber, forming an upper interface layer below the upper wall 304 of the chamber and a lower interface layer above the substrate 303. The process gas can be TCS, DCS, SiH4 and hydrogen when performing silicon epitaxy. Figure 5 The medium thick dashed line 501 indicates the boundary between the upper and lower interface layers when a diffuse surface is formed on the cavity upper wall 304. The thin dashed line 502 indicates the boundary between the upper and lower interface layers when no diffuse surface is formed on the cavity upper wall 304.
[0100] In the process chamber, the chamber cross-sectional area is represented as A, and the total injection flow rate of the process gas per unit time is represented as F. Then the flow rate of the process gas can be expressed as follows: V avg =F / A;
[0101] The dwell time (relaxation time) can be expressed as: L / V avg , L represents the length of the process chamber;
[0102] Additional injection diffusion area = injection rate * average bed residence time V plate Injection, the height of the diffuse surface at the outlet Z = V plate *Tre=V plate *L*A / F.
[0103] The thickness of the lower interface layer can be expressed as follows:
[0104]
[0105] Among them, μ g represents the viscosity coefficient, ρ g represents gas density, v represents gas velocity, and x represents the horizontal coordinate.
[0106] When no diffuse surface is formed on the upper wall 304 of the cavity, the process gas enters the cavity at a speed of U and forms upper and lower interface layers. At this time, the thickness of the lower interface layer can be expressed as follows:
[0107]
[0108] When a diffusion channel is provided on the upper wall 304 of the cavity, the diffusion gas is injected from the diffusion channel to form a diffusion surface. The height of the diffusion surface can be expressed as d 0 -d 1 , (that is, the characteristic size of the cavity is determined by d 0 Reduce to d 0 -d 1 ) The process gas originally flowing in laminar flow is compressed, and the upper interface of the process gas is also the lower interface of the diffuse surface. The density of the process gas increases to The flow rate of the process gas increases to At this time, the thickness of the lower interface layer can be expressed as follows:
[0109]
[0110] That is to say, when the diffuse surface is formed at the upper wall 304 of the cavity, the thickness of the lower interface layer will become thinner to the original thickness.
[0111] The deposition rate of chemical vapor deposition is limited by the chemical reaction rate and the concentration of substrate reaction gas. When the chemical reaction rate is sufficient, the deposition rate is mainly limited by the concentration of substrate reaction gas. The substrate reaction gas comes from the process gas diffused from the reaction chamber to the substrate and is affected by the diffusion flux.
[0112] According to Fick's first law Where J represents the diffusion flux of the gas, C represents the concentration of the reaction gas in the chamber, and d represents the diffusion distance. It can be seen that the diffusion flux is proportional to the gas concentration. Therefore, when there is a diffuse surface, the thickness of the lower interface layer will become thinner than the original The concentration gradient and diffusion flux of the gas also increase, thereby increasing the reaction rate and film formation rate on the substrate.
[0113] In addition, since the density of the diffuse gas, such as hydrogen, is usually lower than that of the process gas, the diffuse gas in the diffuse layer will be suspended in the d below the upper wall 304 of the chamber. 0 -d 1 The process gas can be prevented from contacting with the upper wall 304 of the chamber and forming a film, which is beneficial to the chemical vapor deposition process and reduces the maintenance frequency of the chamber.
[0114] Fig.11 A variation of the aforementioned embodiment is shown in which the upper dome diffuse surface is inclined. Fig.12 The schematic diagram of the fluid velocity distribution and gas streamlines in a process chamber with an inclined diffuse layer in one embodiment of the present invention is shown. The diffuse surface gas has only a horizontal flow rate (flow velocity) to the right, and the vertical downward component of its velocity vector is zero. The advantage of this design is that its fluid configuration is close to or similar to the traditional horizontal laminar flow (upper and lower parallel plates or tubes) model. A simplified model is that the flow velocity of the diffuse area of the right triangle is equal, which is V 水平 ; The vertical component is zero. The control and simulation of this model is also simpler than the previous diffuse model with a parallel dome and a downward velocity component. Another benefit of this configuration is that the diffuse purge has no downward vertical component, which is less likely to interfere with the substrate process.
[0115] Figure 7FIG. 1 is a schematic diagram showing a preheating ring and a heater in a reaction chamber in one embodiment of the present invention. Figure 7 As shown, the preheating ring 302 can use an integrated single-sided heating structure. A base 701 can also be set in the reaction chamber, and the material of the base 701 can be 0P quartz. The heater 301 can be buried in the base 701, and the preheating ring 302 can be arranged on the base 701. By burying the heater 301 in the base 701 and cooperating with the preheating ring 302, the heating components of the reaction chamber can be arranged more compactly, forming homogeneous heating to obtain better heating uniformity, and the lower cavity of the reaction chamber can be reduced to obtain smaller thermal inertia and generate less pollution. In addition, in Figure 1 In the conventional reaction chamber shown in the figure, the bottom purge flow is too small, and the purge gas is directly discharged from the tail. It is difficult to get a good purge in the first half of the bottom. If the bottom purge flow is increased, the bottom purge gas will easily overflow from the front edge of the base, and the overflowed purge gas will mix with the process gas and interfere with the process. Figure 7 When the integrated preheating ring is shown, the space that needs to be purged between the bottom of the preheating ring and the lower wall 702 of the cavity is eliminated. Furthermore, a diffuse purge similar to that at the upper wall 304 of the cavity can also be used at the lower wall 702 of the cavity. Thereby, the bottom is completely purged while the impact on the substrate process is minimized. By designing a reasonable total bottom purge flow rate and a corresponding purge flow distribution rule, it can be further optimized, that is, the purge effect is optimal and the impact on the substrate process is minimized. Furthermore, by adding etching gas to the bottom diffuse purge gas, the bottom deposits can be etched away in real time during the process production.
[0116] Fig.13 It is a simulation diagram of the hydrogen concentration distribution of the upper dome diffuse and the lower dome bottom single-point axial purge according to an embodiment of the present invention. The left coordinate is the concentration ratio of hydrogen. A higher hydrogen content means that the reaction gas content is lower and the proportion of hydrogen is higher, and the purge protection is better. The simulation shows that when there is only a single point (axis) purge at the bottom, the purge can only cover part (the latter half of the circle) of the lower dome bottom (lower dome / plate), while the diffuse purge of the upper dome can completely protect the entire upper dome. Obviously, a single point or multiple points of diffuse purge can provide complete purge coverage of the entire upper dome and / or lower dome bottom.
[0117] A susceptor 703 may also be provided in the reaction chamber. The susceptor 703 is rotatable and may be made of graphite with a high-purity coating. One or more substrates 303 may be placed horizontally on the susceptor 703 .
[0118] A diffusion channel may be provided on the upper wall 304 of the cavity, and the diffusion channel may be a plurality of through holes or micro-pipes, wherein the diffuse gas is injected from the diffusion channel to form a diffuse surface. And the upper wall 304 of the cavity may exchange heat through one or more of water cooling, air cooling and micro-channel heat exchange surface. By adjusting the heat exchange amount of the upper wall 304 of the cavity, the upper wall 304 of the cavity may be kept in a set temperature range. The material at the diffuse surface of the upper wall 304 of the cavity may be a high-purity non-metallic material, such as high-purity porous ceramics, quartz or (coated) graphite microchannels, and high-purity high-temperature resistant membranes, so that the diffuse gas may be injected into the diffuse surface according to a set rule. The rule for the injection of the diffuse gas may be to uniformly inject the diffuse gas at the upper wall 304 of the cavity, or to exponentially or linearly decrease the injection amount of the diffuse gas at the upper wall 304 of the cavity along the direction of the process gas injection, wherein different injection rules may be switched through a fluid control valve, a mass flow meter, and the like. The thickness of the diffuse boundary layer can be controlled by adjusting the height of the cavity upper wall 304 .
[0119] One possible structure of the so-called diffuse channel is formed by a microstructure, which is provided with microchannels, and / or microtubes, and / or millichannels, and / or millitubes. Among them, the channel and tube structures are relatively similar, the difference is that the cross section of the channel structure is a two-dimensional figure, and the cross section of the tube structure is an axisymmetric figure. The difference between "micro" and "fine" lies in the size of the channel. "Micro" usually refers to the characteristic size of 0.1 micron to hundreds of microns, and "fine" usually refers to the characteristic size of 0.1 millimeter to hundreds of millimeters. The characteristic size of the "channel" or "tube" of the present invention can be between 0.1 micron and several centimeters. Of course, the present invention is also applicable to smaller nanoscale sizes.
[0120] The main body of the cavity upper wall 304 may be made of a heat-insulating material or transparent quartz.
[0121] The heater 301 may be an induction coil, which may heat the pedestal 703 to heat the substrate 303 to form single-sided heating, or the induction coil may simultaneously heat the cavity upper wall 304 and the pedestal 703 to form double-sided heating.
[0122] The heater 301 may also be an infrared lamp (such as a halogen lamp) or a resistive heating element.
[0123] When the main body of the cavity upper wall 304 is made of a heat-insulating material or an opaque material or a transparent material with an infrared reflective material, an infrared heater lamp or an induction coil may be arranged only below the substrate 303 for single-sided heating.
[0124] The infrared resistance heater can be a homogeneous heater with a heating area greater than 20% or a one-dimensional linear dimension greater than 20%. The material of the infrared resistance heater can be graphite or carbon material, and the infrared resistance heater can be arranged with silicon carbide or other high-purity coatings so that the infrared resistance heater is arranged in the reaction chamber to contact the reaction gas.
[0125] It should be understood that the embodiments of the components in the above reaction chamber can be combined arbitrarily, and the different technical solutions formed can be shown in Table 1 to Table 4:
[0126] Table 1
[0127]
[0128]
[0129] Table 2
[0130]
[0131] Table 3
[0132]
[0133]
[0134] Table 4
[0135]
[0136] Figure 8 FIG. 2 shows a schematic diagram of the temperature of components of a reaction chamber in the prior art. Figure 8 As shown, the temperature boundary condition of the cold wall reaction chamber using an infrared heater requires that the temperature of the chamber wall be controlled below 740K. If the temperature of the chamber wall is increased, the laminar boundary layer of the process gas can be lowered, the flow rate of the process gas can be increased, and the growth rate of the substrate and the generation uniformity of the substrate can be increased. However, more gas phase nucleation will be generated, resulting in more particles. In the present invention, by constructing the upper wall surface 304 of the chamber so that the diffuse gas flows in or out of the upper wall 304 of the chamber to form a diffuse surface, the gas phase nucleation and gas phase growth of the upper wall 304 of the chamber can be suppressed while the temperature of the upper wall 304 of the chamber is increased, thereby suppressing the generation of particulate matter, which is beneficial to the chemical vapor deposition process and reduces the maintenance frequency of the chamber.
[0137] Fig. 9 A schematic diagram of a cookbook showing the relationship between process control parameter input and process result output in one embodiment of the present invention. Fig. 9As shown, the thickness of the diffuse interface layer and the laminar interface layer can be adjusted by adjusting the flow rate of the process gas, the flow rate of the diffuse gas injection, the temperature of the diffuse surface (DOME), and the height of the diffuse surface, thereby changing the reaction rate, film thickness uniformity, gas phase nucleation and particle size on the substrate.
[0138] Fig.10 FIG. 1 is a schematic diagram of a neural network based on input parameters and output results of a chemical vapor deposition process in one embodiment of the present invention. Fig.10 As shown, it can be based on Fig. 9 The input and output relationship shown in generates a neural network including an input layer, an output layer, and two intermediate layers, and the neural network is a multiple-input multiple-output system (MIMO).
[0139] The parameters input into the process and equipment parameter input layer of the neural network include the flow rate of the process gas flow, the flow rate and control rules of the diffuse injection gas flow, the flow rate of the doping gas flow, the temperature of the upper wall (Dome) of the chamber, the height of the upper wall (Dome) of the chamber, the total pressure and other inputs. The parameters processed and generated by the fluid configuration (primary) intermediate layer include the process gas flow rate, the doping gas flow rate, the temperature gradient, the partial pressure of different gases and other primary intermediate operators. The parameters processed and generated by the reaction kinetics (secondary) intermediate layer include the substrate boundary layer thickness, the diffuse boundary layer thickness, the doping boundary layer thickness, the thickness of other kinetic boundary layers and other secondary intermediate operators. The parameters output by the process result output layer include doping uniformity, film deposition rate, film thickness uniformity, gas phase nucleation and particle size, doping rate and doping uniformity.
[0140] Although various embodiments of the present invention are described above, it should be understood that they are presented as examples only and not as limitations. It is obvious to those skilled in the relevant art that various combinations, modifications and changes can be made thereto without departing from the spirit and scope of the present invention. Therefore, the breadth and scope of the present invention disclosed herein should not be limited by the exemplary embodiments disclosed above, but should only be defined according to the attached claims and their equivalents.
Claims
1. A diffuse laminar flow reaction chamber, It is characterized in that include: Substrate and / or base; a main gas inlet configured to inject a process gas into the reaction chamber to form a laminar interface layer on a surface of the substrate; as well as a diffuse surface configured to inject or suck diffuse gas into or out of the reaction chamber to form a diffuse interface layer on the laminar interface layer; The thickness of the diffuse interface layer and the laminar interface layer is adjusted by adjusting the flow rate of the process gas, the flow rate of the diffuse gas injection, the temperature of the diffuse surface, and the height of the diffuse surface.
2. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffuse interface layer is configured to increase the flow rate of the process gas, and / or The diffuse interface layer reduces the thickness of the laminar interface layer.
3. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffusion surface includes a porous plate, porous ceramics, porous transparent quartz or a permeable membrane.
4. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffusion surface is provided with microchannels.
5. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that Also includes: A heater is arranged inside and / or outside the diffuse laminar flow reaction chamber, and the heater is configured to heat the substrate.
6. The diffuse laminar flow reaction chamber according to claim 5, It is characterized in that Also includes: A preheat ring surrounds the substrate, wherein the preheat ring is configured to heat the substrate.
7. The diffuse laminar flow reaction chamber according to claim 6, It is characterized in that Also includes: The base is rotatable, and the preheating ring is arranged around the base.
8. The diffuse laminar flow reaction chamber according to claim 6, It is characterized in that The preheating ring is an integrated heating ring such that there is no gap under the heating ring for process gas to enter.
9. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffusion surface is arranged at the upper wall of the chamber above the substrate; and / or The diffusion surface is arranged at the lower wall of the chamber below the substrate so as to purge the bottom to reduce the impact on the substrate process.
10. The diffuse laminar flow reaction chamber according to claim 9, It is characterized in that The chamber upper wall and / or the chamber lower wall is dome-shaped.
11. The diffuse laminar flow reaction chamber according to claim 4, It is characterized in that The diffuse gas is injected from the microchannel to form a diffuse surface, and the height of the diffuse surface is represented by d 0 -d 1 , the laminar flow process gas is compressed, and the thickness of the laminar interface layer is expressed as follows: where d 0 represents the distance between the substrate and the upper wall of the cavity, d 1 represents the distance between the lower interface of the diffuse surface and the substrate, x represents the horizontal coordinate, δ(x) 0 It is the thickness of the laminar interface layer when no diffuse surface is formed.
12. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that Diffusion flux of substrate It is expressed as follows: Where P par Indicates the partial pressure of gas, P S represents the gas surface pressure, T′ represents the local temperature of the substrate, J represents the molar flow rate of the carrier gas, ρ g Indicates the density of airflow, μ g It is the dynamic viscosity of the airflow, P tot Indicates total pressure, R represents the gas constant, A represents the cross-sectional area of the cavity, and D represents the gas diffusion coefficient. The gas phase reaction rate on the substrate depends on the diffusion flux By adjusting the parameters in the above formula, the To increase the reaction speed.
13. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffuse interface layer is used to compress the characteristic size of the cavity, reduce the Reynolds coefficient of the substrate laminar flow, and increase the growth rate.
14. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The substrate and / or base are parallel to the diffuse surface; The direction of injection of the main process gas is parallel to the substrate; The diffusely injected gas has a component perpendicular to the substrate.
15. The diffuse laminar flow reaction chamber according to claim 1, It is characterized in that The diffuse laminar flow reaction chamber includes one or more of the following structural features: The diffuse laminar flow reaction chamber is heated on one side or two sides; The top of the diffuse laminar flow reaction chamber is: A infrared transparent wall, through which the external infrared heater heats by transmission; B infrared blocking wall; or C dome heating wall.
16. A diffuse laminar flow control method, It is characterized in that Using the diffuse laminar flow reaction chamber according to any one of claims 1 to 15, the method comprises the following steps: injecting a process gas into the reaction chamber from a main gas inlet to form a laminar interface layer on the surface of the substrate; as well as A diffuse gas is injected into or sucked out of the reaction chamber to form a diffuse interface layer on the laminar interface layer, wherein the diffuse interface layer is configured to increase the flow rate of the process gas and reduce the thickness of the laminar interface layer.
17. The diffuse laminar flow control method according to claim 16, It is characterized in that Also includes: The thickness of the diffuse interface layer is adjusted to adjust the flow rate of the process gas and the thickness of the laminar interface layer, wherein the thickness of the diffuse interface layer is adjusted by adjusting the temperature of the diffuse surface and / or adjusting the height of the diffuse surface.
18. The diffuse laminar flow control method according to claim 17, It is characterized in that Also includes: uniformly injecting the diffusion gas into the reaction chamber on the diffusion surface; or The amount of diffuse gas injected on the diffuse surface is decreased exponentially or linearly along the direction of process gas injection.
19. The diffuse laminar flow control method according to claim 16, It is characterized in that The diffuse gas increases the thickness of the diffuse interface layer, reduces gas phase nucleation on the diffuse surface leading to generation of particles and / or defects on the substrate, and / or reduces deposition on the diffuse surface.
20. The diffuse laminar flow control method according to claim 16, It is characterized in that The diffuse gas is an inert gas or an inactive gas to reduce the content of the reaction precursor in the diffuse boundary layer, and reduce the generation of particles and / or defects on the substrate caused by gas phase nucleation on the diffuse surface and / or reduce deposition on the diffuse surface; or The diffuse gas is an etching gas, which etches the deposits on the diffuse surface and etches the gas phase nucleation of the diffuse interface layer, thereby reducing the generation of particles and / or defects on the substrate. This reduces the deposition on the top of the reaction chamber, allowing the transparent top to operate at a temperature higher than the non-diffuse controlled top temperature without generating deposition.
21. The diffuse laminar flow control method according to claim 20, It is characterized in that The deposition on the diffuse surface is minimized, so that the quartz cold wall external heater cavity relying on infrared transmission can operate at a temperature point higher than the traditional temperature. The increased temperature of the diffuse surface further thins the boundary layer of the substrate.
22. The diffuse laminar flow control method according to claim 16, It is characterized in that Adjust the physical height of the diffuse surface to optimize process results.
23. The diffuse laminar flow control method according to claim 16, It is characterized in that Adjust the total bottom purge flow and the corresponding purge flow distribution to further optimize the purge effect and reduce the impact on substrate process.
24. The diffuse laminar flow control method according to claim 23, It is characterized in that Etching gas is added to the bottom diffuse purge gas so that the bottom deposits can be etched away in real time during process production.
25. The diffuse laminar flow control method according to any one of claims 16 to 24, It is characterized in that The diffuse interface layer makes the laminar interface layer thinner, thereby improving the deposition speed and / or uniformity of the film.