An oil-proof, seepage-proof and boiling water-proof coating for a microphone dust-proof net
By applying oil-proof, anti-seepage and anti-boiling water coatings on the dustproof network of the electronic cigarette head, the problems of e-liquid penetration and damage to high-temperature boiling water are solved, and long-term protection and mesh strength are improved.
Patent Information
- Application Number
- CN202211208475.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-08
- Publication Date
- 2025-03-28
- Estimated Expiration
- 2042-10-08
AI Technical Summary
The existing electronic cigarette head dustproof net cannot effectively prevent e-liquid penetration and damage from high-temperature boiling water, resulting in functional damage.
An oil-proof, anti-seepage and anti-boiling water coating is adopted, including the dust-proof mesh main body and coating layer. The coating is uniformly applied to the high-temperature resistant layers on both sides of the mesh through dip coating and spraying technology, forming the functions of boiling oil, long-term anti-seepage, anti-boiling water, and anti-siphon.
Effective protection of e-liquid and boiling water is achieved, and the anti-seepage time can reach more than 10 days, avoiding damage to the mesh cloth due to high temperature damage, and at the same time enhancing the overall strength of the mesh cloth.
Smart Images

Figure CN115556429B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of electronic cigarettes, and in particular to an oil-proof, seepage-proof and boiling water-proof coating for a dust-proof net of a microphone head. Background Art
[0002] The microphone of the electronic cigarette is an important component of the electronic cigarette and an indispensable component. Improving its reliability has become the direction of efforts of all parties in the electronic cigarette factory. Especially due to the structural factors of the electronic cigarette itself, all electronic cigarettes have the risk of oil leakage. In order to prevent the oil produced by the electronic cigarette from contacting the microphone and causing damage to the microphone, a dustproof net is generally set on the outside of the microphone.
[0003] However, the current e-cigarette oil-proof net can simply achieve the hydrophobic effect by making a hydrophobic coating. The smoke oil will stick to the dust-proof net. Over time, it will penetrate into the microphone head and cause functional damage and it is not resistant to boiling water.
[0004] Therefore, we propose an oil-proof, seepage-proof, and boiling water-proof coating for the dustproof net of the microphone head. This coating is applied on the dustproof net. Compared with the previous hydrophobic coating, this coating has the characteristics of not sticking to oil drops, and the oil-proof time can be up to more than 10 days. During the use of electronic cigarettes, high-temperature condensed water (boiling water) will be generated. This coating can solve this pain point and has the characteristics of boiling oil, oil-proof, seepage-proof, and boiling water-proof. Summary of the invention
[0005] 1. Technical issues to be resolved
[0006] In view of the deficiencies in the prior art, the present invention discloses an oil-proof, seepage-proof and boiling water-proof coating for a dust-proof net of a microphone head to solve the problems raised in the above-mentioned background technology.
[0007] (II) Technical solution
[0008] To achieve the above objectives, the present invention is implemented through the following technical solutions: an oil-proof, seepage-proof, and boiling water-proof coating of a dustproof net of a microphone head, comprising: a dustproof net body, the dustproof net body comprising a mesh, a first high temperature resistant layer, a second high temperature resistant layer, a first coating layer, and a second coating layer, the first coating layer and the second coating layer preventing smoke oil and boiling water from contacting the mesh, and the first high temperature resistant layer and the second high temperature resistant layer resistant to high temperature absorption temperature, preventing the high temperature of boiling water from damaging the mesh;
[0009] The first high temperature resistant layer and the second high temperature resistant layer are respectively fixedly connected to two sides of the mesh, and the first coating layer and the second coating layer are respectively sprayed on the opposite sides of the first high temperature resistant layer and the second high temperature resistant layer.
[0010] Preferably, the mesh fabric comprises a plurality of reinforcing strips, a plurality of fabric layers, and a plurality of first connecting layers and a plurality of second connecting layers;
[0011] The plurality of fabric layers are respectively fixedly connected between the plurality of reinforcement strips.
[0012] Preferably, the plurality of first connection layers and the plurality of second connection layers are fixedly connected between the plurality of reinforcement strips;
[0013] And the plurality of first connection layers and the plurality of second connection layers are respectively fixedly connected to two sides of the plurality of fabric layers.
[0014] Preferably, one side of the plurality of reinforcement strips and the side walls of the plurality of first connection layers are fixedly connected to the first high temperature resistant layer.
[0015] Preferably, the other side of the plurality of reinforcing strips and the side walls of the plurality of second connecting layers are fixedly connected to the second high temperature resistant layer.
[0016] A method for processing an oil-proof, seepage-proof and boiling water-proof coating of a microphone dustproof net comprises the following steps:
[0017] S1, coating production; S2, coating processing, S3, inspection.
[0018] Preferably, the coating is made by first selecting raw materials, selecting a certain amount of ingredients such as tetraethyl orthosilicate, ammonia water, heptadecafluorotriethoxysilane, ethanol and deionized water, putting a certain amount of tetraethyl orthosilicate, ammonia water, heptadecafluorotriethoxysilane, ethanol and deionized water into a reactor, setting the stability of the reactor to 65 degrees Celsius, and reacting and synthesizing in the reactor at 65 degrees Celsius for 30 minutes to finally form a liquid coating material.
[0019] Preferably, the coating processing: the liquid coating material is evenly coated on the outer surfaces of the first high temperature resistant layer and the second high temperature resistant layer on both sides of the mesh cloth by dipping and spraying, so that the liquid coating material forms a first coating layer and a second coating layer on the outer surfaces of the first high temperature resistant layer and the second high temperature resistant layer respectively, so that it has the functions of rolling oil, long-term anti-seepage, anti-boiling water, anti-siphonage and the like.
[0020] Preferably, the inspection: the inspection standard is that the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, the smoke oil dripping onto the first coating layer or the second coating layer can slide away quickly, 2-3 drops of smoke oil are dropped on the first coating layer or the second coating layer, and it will not penetrate to the back side for ten days, and at the same time, 100° boiling water is poured on the first coating layer or the second coating layer, and there will be no sticking, penetration and siphoning on the first coating layer or the second coating layer.
[0021] The present invention discloses an oil-proof, seepage-proof and boiling-water-proof coating for a microphone dustproof net, which has the following beneficial effects:
[0022] 1. The anti-oil, anti-seepage and anti-opening water coating of the dustproof net of the microphone head is provided with a first coating layer and a second coating layer, and the liquid coating material is evenly coated on the outer surfaces of the first high-temperature resistant layer and the second high-temperature resistant layer on both sides of the mesh cloth by dipping and spraying, so that the liquid coating material forms the first coating layer and the second coating layer on the outer surfaces of the first high-temperature resistant layer and the second high-temperature resistant layer respectively, so that it has the functions of rolling oil, long-term anti-seepage, anti-opening water, anti-siphoning, etc., and the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, and the smoke oil drips onto the first coating layer or the second coating layer. The second coating layer can slide off quickly, 2-3 drops of e-liquid are dropped on the first coating layer or the second coating layer, and it will not penetrate into the back side for ten days. At the same time, 100° boiling water is poured on the first coating layer or the second coating layer, and there will be no sticking, penetration and siphoning on the first coating layer or the second coating layer. Compared with the previous hydrophobic coating, it has the characteristics of oil-free and oil-proof time of more than 10 days. In addition, electronic cigarettes will produce high-temperature condensed water during use. This coating can solve such pain points and has the characteristics of boiling oil, oil-proof, seepage-proof and boiling water-proof.
[0023] 2. The oil-proof, seepage-proof and boiling water-proof coating of the microphone dustproof net can further prevent the mesh from boiling water by setting the first high-temperature resistant layer and the second high-temperature resistant layer. The first high-temperature resistant layer and the second high-temperature resistant layer can absorb high temperature to prevent the high temperature of boiling water from damaging the mesh.
[0024] 3. The oil-proof, seepage-proof and boiling water-proof coating of the microphone dustproof net is provided with a plurality of reinforcing strips, and a plurality of fabric layers are respectively fixedly connected between the plurality of reinforcing strips, thereby strengthening the strength of the plurality of fabric layers, making it difficult for the plurality of fabric layers to be damaged. At the same time, a plurality of first connecting layers and a plurality of second connecting layers are respectively fixedly connected to both sides of the plurality of fabric layers, thereby effectively protecting the plurality of fabric layers and increasing the overall strength of the mesh. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a schematic diagram of the structure of the present invention;
[0026] Figure 2 It is an exploded view of the present invention;
[0027] Figure 3 It is an exploded view of the mesh of the present invention.
[0028] In the figure: 1. dustproof net body; 101. mesh cloth; 1011. reinforcement strip; 1012. cloth layer; 1013. first connecting layer; 1014. second connecting layer; 102. first high temperature resistant layer; 103. second high temperature resistant layer; 104. first coating layer. DETAILED DESCRIPTION
[0029] Embodiment 1:
[0030] The embodiment of the present invention discloses an oil-proof, seepage-proof and water-proof coating for a dustproof net of a microphone head, such as Figure 1-3 As shown,
[0031] The dustproof net body 1 includes a mesh 101, a first high temperature resistant layer 102, a second high temperature resistant layer 103, a first coating layer 104 and a second coating layer 105, wherein the first coating layer 104 and the second coating layer 105 prevent smoke oil and boiling water from contacting the mesh 101, and the first high temperature resistant layer 102 and the second high temperature resistant layer 103 are resistant to high temperature absorption to prevent the high temperature of boiling water from damaging the mesh 101;
[0032] By providing the first high temperature resistant layer 102 and the second high temperature resistant layer 103, the mesh 101 can be further protected from boiling water. The first high temperature resistant layer 102 and the second high temperature resistant layer 103 can absorb the high temperature and prevent the high temperature of boiling water from damaging the mesh 101.
[0033] The first high temperature resistant layer 102 and the second high temperature resistant layer 103 are fixedly connected to both sides of the mesh 101 , respectively, and the first coating layer 104 and the second coating layer 105 are sprayed on opposite sides of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 , respectively.
[0034] The mesh 101 includes a plurality of reinforcing strips 1011 , a plurality of fabric layers 1012 , a plurality of first connecting layers 1013 , and a plurality of second connecting layers 1014 ;
[0035] The plurality of fabric layers 1012 are respectively fixedly connected between the plurality of reinforcement strips 1011 .
[0036] The plurality of first connection layers 1013 and the plurality of second connection layers 1014 are fixedly connected between the plurality of reinforcement strips 1011;
[0037] The plurality of first connection layers 1013 and the plurality of second connection layers 1014 are fixedly connected to two sides of the plurality of fabric layers 1012 , respectively.
[0038] By setting up multiple reinforcing strips 1011, multiple fabric layers 1012 are respectively fixedly connected between the multiple reinforcing strips 1011, so that the strength of the multiple fabric layers 1012 can be strengthened, making it difficult for the multiple fabric layers 1012 to be damaged. At the same time, multiple first connecting layers 1013 and multiple second connecting layers 1014 are respectively fixedly connected to both sides of the multiple fabric layers 1012, so that the multiple fabric layers 1012 can be effectively protected, thereby increasing the overall strength of the mesh 101.
[0039] One side of the plurality of reinforcing strips 1011 and the side walls of the plurality of first connection layers 1013 are fixedly connected to the first high temperature resistant layer 102 .
[0040] The other side of the plurality of reinforcing strips 1011 and the side walls of the plurality of second connection layers 1014 are fixedly connected to the second high temperature resistant layer 103 .
[0041] Working principle: By setting the first high temperature resistant layer 102 and the second high temperature resistant layer 103, the mesh 101 can be further protected from boiling water. The first high temperature resistant layer 102 and the second high temperature resistant layer 103 can absorb the high temperature and prevent the high temperature of boiling water from damaging the mesh 101.
[0042] By setting up multiple reinforcing strips 1011, multiple fabric layers 1012 are respectively fixedly connected between the multiple reinforcing strips 1011, so that the strength of the multiple fabric layers 1012 can be strengthened, making it difficult for the multiple fabric layers 1012 to be damaged. At the same time, multiple first connecting layers 1013 and multiple second connecting layers 1014 are respectively fixedly connected to both sides of the multiple fabric layers 1012, so that the multiple fabric layers 1012 can be effectively protected, thereby increasing the overall strength of the mesh 101.
[0043] Embodiment 2:
[0044] A method for processing an oil-proof, seepage-proof and boiling water-proof coating of a microphone dustproof net comprises the following steps:
[0045] S1, coating production; S2, coating processing, S3, inspection.
[0046] Preferably, the coating is made by first selecting raw materials, selecting a certain amount of ingredients such as tetraethyl orthosilicate, ammonia water, heptadecafluorotriethoxysilane, ethanol and deionized water, putting a certain amount of tetraethyl orthosilicate, ammonia water, heptadecafluorotriethoxysilane, ethanol and deionized water into a reactor, setting the stability of the reactor to 65 degrees Celsius, and reacting and synthesizing in the reactor at 65 degrees Celsius for 30 minutes to finally form a liquid coating material.
[0047] Preferably, coating processing: the liquid coating material is evenly coated on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 on both sides of the mesh 101 by dipping and spraying, so that the liquid coating material forms a first coating layer 104 and a second coating layer 105 on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 respectively, so that it has the functions of boiling oil, long-term anti-seepage, anti-boiling water, and anti-siphonage.
[0048] Preferably, inspection: the inspection standard is that the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, the smoke oil dripping onto the first coating layer 104 or the second coating layer 105 can slide away quickly, 2-3 drops of smoke oil are dropped on the first coating layer 104 or the second coating layer 105, and it will not penetrate to the back side for ten days, and at the same time, 100° boiling water is poured on the first coating layer 104 or the second coating layer 105, and there will be no sticking, penetration and siphoning on the first coating layer 104 or the second coating layer 105.
[0049] By setting the first coating layer 104 and the second coating layer 105, the liquid coating material is evenly coated on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 on both sides of the mesh 101 by dipping and spraying, so that the liquid coating material forms the first coating layer 104 and the second coating layer 105 on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 respectively, so that it has the functions of boiling oil, long-term anti-seepage, anti-boiling water, anti-siphoning, etc., and the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, and the smoke oil drips onto the first coating layer 104 or the second coating layer 105 It can slide away quickly, drop 2-3 drops of e-liquid on the first coating layer 104 or the second coating layer 105, and it will not penetrate into the back for ten days. At the same time, 100° boiling water is poured on the first coating layer 104 or the second coating layer 105, and there will be no sticking, penetration and siphoning on the first coating layer 104 or the second coating layer 105. Compared with the previous hydrophobic coating, it has the characteristics of oil-free and oil-proof time of more than 10 days. In the process of using electronic cigarettes, high-temperature condensed water and boiling water will be generated. This coating can solve this kind of pain point, and has the characteristics of boiling oil, oil prevention, seepage prevention and boiling water prevention.
[0050] In summary: by setting the first coating layer 104 and the second coating layer 105, the liquid coating material is evenly coated on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 on both sides of the mesh 101 by dipping and spraying, so that the liquid coating material forms the first coating layer 104 and the second coating layer 105 on the outer surfaces of the first high temperature resistant layer 102 and the second high temperature resistant layer 103 respectively, so that it has the functions of boiling oil, long-term anti-seepage, anti-boiling water, anti-siphoning, etc., and the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, and the smoke oil drips onto the first coating layer 104 or the second coating layer 10 5 can slide away quickly, drop 2-3 drops of e-liquid on the first coating layer 104 or the second coating layer 105, and it will not penetrate to the back for ten days. At the same time, 100° boiling water is poured on the first coating layer 104 or the second coating layer 105, and there will be no sticking, penetration and siphoning on the first coating layer 104 or the second coating layer 105. Compared with the previous hydrophobic coating, it has the characteristics of not sticking to oil drops, and the anti-oil seepage time can be more than 10 days. In the process of using electronic cigarettes, condensed water with high temperature will be generated. This coating can solve this kind of pain point, and has the characteristics of boiling oil, oil prevention, anti-seepage and anti-boiling water.
[0051] By providing the first high temperature resistant layer 102 and the second high temperature resistant layer 103, the mesh 101 can be further protected from boiling water. The first high temperature resistant layer 102 and the second high temperature resistant layer 103 can absorb the high temperature and prevent the high temperature of boiling water from damaging the mesh 101.
[0052] By setting up multiple reinforcing strips 1011, multiple fabric layers 1012 are respectively fixedly connected between the multiple reinforcing strips 1011, so that the strength of the multiple fabric layers 1012 can be strengthened, making it difficult for the multiple fabric layers 1012 to be damaged. At the same time, multiple first connecting layers 1013 and multiple second connecting layers 1014 are respectively fixedly connected to both sides of the multiple fabric layers 1012, so that the multiple fabric layers 1012 can be effectively protected, thereby increasing the overall strength of the mesh 101.
[0053] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. An oil-proof, seepage-proof and boiling-water-proof coating for a microphone dustproof net, comprising: The dustproof net body (1) is characterized in that the dustproof net body (1) comprises a mesh (101), a first high temperature resistant layer (102), a second high temperature resistant layer (103), a first coating layer (104) and a second coating layer (105), wherein the first coating layer (104) and the second coating layer (105) prevent smoke oil and boiling water from contacting the mesh (101), and the first high temperature resistant layer (102) and the second high temperature resistant layer (103) are resistant to high temperature absorption to prevent the high temperature of boiling water from damaging the mesh (101); the first coating layer (104) and the second coating layer (105) are made of tetraethyl orthosilicate, ammonia water, heptadecafluorotriethoxysilane, ethanol and deionized water; The first high temperature resistant layer (102) and the second high temperature resistant layer (103) are respectively arranged on both sides of the mesh cloth (101), and the first coating layer (104) and the second coating layer (105) are respectively sprayed on the opposite sides of the first high temperature resistant layer (102) and the second high temperature resistant layer (103); The mesh cloth (101) comprises a plurality of reinforcing strips (1011), a plurality of cloth layers (1012), a plurality of first connecting layers (1013) and a plurality of second connecting layers (1014); The plurality of fabric layers (1012) are respectively arranged between the plurality of reinforcement strips (1011); A plurality of the first connection layers (1013) and a plurality of the second connection layers (1014) are all arranged between a plurality of reinforcement strips (1011); and the plurality of first connection layers (1013) and the plurality of second connection layers (1014) are respectively arranged on both sides of the plurality of fabric layers (1012); One side of the plurality of reinforcing strips (1011) and the side walls of the plurality of first connection layers (1013) are fixedly connected to the first high temperature resistant layer (102).
2. The oil-proof, seepage-proof and boiling water-proof coating of the dust-proof net of a microphone according to claim 1, characterized in that: The other sides of the plurality of reinforcing strips (1011) and the side walls of the plurality of second connection layers (1014) are fixedly connected to the second high temperature resistant layer (103).
3. A method for processing the oil-proof, seepage-proof and boiling water-proof coating of the dust-proof net of the microphone according to any one of claims 1-2, characterized in that: The following steps are involved: S1, coating production; S2, coating processing, S3, inspection; The coating process comprises: using a dipping and spraying method to uniformly coat the liquid coating material on the outer surfaces of the first high temperature resistant layer (102) and the second high temperature resistant layer (103) on both sides of the mesh cloth (101), so that the liquid coating material forms a first coating layer (104) and a second coating layer (105) on the outer surfaces of the first high temperature resistant layer (102) and the second high temperature resistant layer (103), respectively, so that the first coating layer (104) and the second coating layer (105) have the functions of oil boiling, long-term seepage prevention, boiling water prevention and siphon prevention.
4. The method according to claim 3, characterized in that: The coating is prepared by first selecting raw materials, selecting a certain amount of tetraethyl orthosilicate, ammonia water, triethoxysilane heptadecafluorodecene, ethanol and deionized water components, putting a certain amount of tetraethyl orthosilicate, ammonia water, triethoxysilane heptadecafluorodecene, ethanol and deionized water into a reactor, setting the stability of the reactor to 65 degrees Celsius, and reacting and synthesizing in the reactor at 65 degrees Celsius for 30 minutes to finally form a liquid coating material.
5. The method according to claim 3, characterized in that: The inspection: the inspection standard is that the water drop angle is greater than 175°, the oil drop angle is greater than 120° and ∠45°, the smoke oil dripped onto the first coating layer (104) or the second coating layer (105) can slide away quickly, 2-3 drops of smoke oil are dripped on the first coating layer (104) or the second coating layer (105), and it will not penetrate to the back for ten days, and at the same time, 100° boiling water is poured on the first coating layer (104) or the second coating layer (105), and there will be no sticking, penetration and siphoning on the first coating layer (104) or the second coating layer (105).
Citation Information
Patent Citations
Preparation method of transparent superhydrophobic coating
CN110669363A
Fireproof anti-siphon water-stop cloth
CN204426818U