A cold crucible bottom for high-level radioactive waste glass solidification
By using a combination of high chromium refractory material plate and metal ring in the bottom of the cold crucible, the replacement of the material leakage valve under the condition of non-stop furnace is achieved, solving the complex problem of material leakage valve replacement in the existing technology, ensuring the cold The long-term stable operation of the crucible and the effect of glass curing.
Patent Information
- Application Number
- CN202211525223.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-30
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-11-30
AI Technical Summary
The existing cold crucible bottom is under highly corrosive radioactive waste liquid glass curing conditions, and the process of replacing the leak valve is complicated and difficult, and it is impossible to replace the leak valve without stopping the furnace, which affects the long-term operation of the cold crucible. .
The bottom design of the pot consisting of high chrome refractory material plate, water-cooled or air-cooled metal ring, ceramic insulating sleeve and ceramic insulating pipe is achieved through induction heating of the metal ring and cooling medium adjustment, and auxiliary heating and temperature control of the leakage hole are achieved to ensure that Replace the leak valve when the glass melt does not leak.
The ability to safely replace the leaking valve under the condition of no stopping furnace is achieved, avoiding restarting the cold crucible, extending the service life of the cold crucible, and reducing the risk of crystallization of glass melt.
Smart Images

Figure CN115893806B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of high-level radioactive waste liquid glass solidification, in particular to a crucible bottom for a radioactive waste liquid cold crucible, and is particularly suitable for replacing a leaking valve for glass solidification of a highly corrosive radioactive waste liquid cold crucible. Background Art
[0002] The development of nuclear power technology is conducive to reducing greenhouse gas emissions. However, the treatment and disposal of spent fuel produced by nuclear reactors has become the focus of attention. Since the 1950s, researchers have begun to study the solidification technology of high-level waste liquid produced by spent fuel reprocessing, and in the 1970s, France took the lead in realizing the engineering application of high-level waste liquid glass solidification. Subsequently, the United States, Russia, Germany, Japan, Britain, South Korea, India and other countries also developed their own high-level waste liquid glass solidification technology. So far, the most widely used are the third-generation Joule heating ceramic furnace glass solidification technology and the fourth-generation cold crucible glass solidification technology.
[0003] The cold crucible glass solidification technology uses a split metal cold crucible as a high-temperature glass melt heating container, and uses a high-frequency induction heating power supply and an induction coil to heat the glass melt in the cold crucible. The cold crucible body split and the bottom split are cooled by water, and a glass shell is formed on the body and the bottom to protect the body and the bottom from corrosion by the high-temperature glass melt, thereby extending the service life of the cold crucible. The leakage of cold crucible glass solidification is usually caused by freeze-thaw valve leakage and slide valve leakage. Since the bottom of the cold crucible is cooled, the cold shell layer at the bottom of the crucible needs to melt before leakage. This requires an auxiliary heating device at the bottom of the crucible to heat the cold shell layer at the bottom of the crucible, so that the cold shell layer melts before leakage. On the other hand, the freeze-thaw valve and the slide valve are in direct contact with the high-temperature glass melt when leaking, so that the leakage valve or slide valve needs to be replaced regularly because of the erosion of the glass melt. Under the conditions of radioactive glass solidification, restarting the cold crucible is complicated and difficult. Therefore, it is necessary to maintain a certain liquid level of the glass melt in the cold crucible and replace the leakage valve regularly without stopping the furnace. Therefore, developing a cold crucible bottom that can assist heating at the leakage hole and can replace the leakage valve in a hot state is of great significance for the long-term operation of cold crucible glass solidification.
[0004] Chinese patent CN 205048973 U discloses a cold crucible device, which uses a slide valve to leak material, and the slide valve is close to the bottom of the cold crucible. When it is necessary to leak material, the slide valve is pulled open to start leaking material; when it is necessary to stop leaking material, the slide valve is closed to stop leaking material. The patent does not have an auxiliary heating device at the bottom of the cold crucible and does not explain how to plug the leakage hole at the bottom of the crucible to replace the slide valve when the leakage slide valve fails and needs to be replaced.
[0005] U.S. Patent US 20160091249 A1 discloses a cold crucible device for melting materials, which uses a water-cooled tray to control leakage. When leakage is required, a mechanical mechanism is used to move the water-cooled tray away, and leakage begins. When it needs to be closed, the water-cooled tray is reset to hold the glass liquid in the cold crucible and stop leakage. The disadvantage of this patent is that there is no auxiliary heating device at the bottom of the cold crucible, and when the water-cooled tray needs to be replaced, the glass liquid in the cold crucible cannot be controlled to flow out. The cold crucible can only be replaced after the glass liquid in the cold crucible is completely emptied. This leakage valve design requires the cold crucible to be restarted after replacing the water-cooled tray.
[0006] Chinese patent CN 106123588 A discloses a high-temperature melt unloading device for a cold crucible, which uses a freeze-thaw valve to unload, and a leakage pipe passes through the cold shell layer at the bottom of the crucible and enters the cold crucible. A cavity is provided in the leakage pipe, which can be cooled by compressed air. When preparing to discharge, the leakage pipe is heated by a medium-frequency coil to melt the glass in the leakage pipe. Since the temperature of the cold shell layer around the leakage pipe is also increased during the heating process of the medium-frequency coil to melt the glass, the leakage can be achieved after the glass in the leakage pipe is melted. When the leakage is completed, the compressed air can be opened to cool the leakage pipe, so that the glass in the leakage pipe solidifies and stops the leakage. The device realizes the heating of the cold shell layer at the bottom of the crucible by the leakage pipe, but fails to provide a method for replacing the leakage pipe without emptying the glass liquid.
[0007] Patent US006620372B1 of the French Atomic Energy Commission discloses a discharge device for molten material in a cold crucible, which includes a long leakage hole, a water-cooled slide valve and a vertical bar. The function of the vertical bar is to form a heat bridge between the molten material and the bottom of the cold crucible, conduct the heat of the glass melt to the bottom of the crucible, and act as a heat source for heating the cold shell layer of the bottom of the crucible. When the material is leaking, open the water-cooled slide valve, and the glass in the leakage hole melts and flows out under the action of the heat conducted by the vertical bar. When the leakage is completed, close the slide valve. Although the patent takes into account the auxiliary heating at the leakage port, it does not provide a method for replacing the leakage slide valve. Summary of the invention
[0008] The technical problem to be solved by the present invention is to provide a cold crucible bottom for high-level radioactive waste glass solidification, which is suitable for the replacement of leakage and leakage valve of high-frequency induction heating cold crucible molten glass, especially in the field of induction heating cold crucible glass solidification of radioactive waste with strong corrosiveness of glass melt. The cold crucible bottom consists of five parts: a high-chromium refractory plate, a water-cooled or air-cooled metal ring, a ceramic insulating sleeve, a ceramic insulating tube and a water-cooled split stainless steel plate with a leakage valve (sliding valve or freeze-thaw valve). The water-cooled split stainless steel plate is a split structure, with a leakage valve (freeze-thaw valve or sliding valve) and a leakage hole under the stainless steel plate. A groove similar to the shape of the leakage hole is opened on the outside of the leakage hole on the water-cooled split stainless steel plate, and the groove is used to place the ceramic insulating sleeve. A metal ring is placed in the ceramic insulating sleeve. The metal ring is a hollow structure and protrudes a certain height from the water-cooled split stainless steel plate. The metal ring is provided with a cooling medium inlet and outlet pipe (the cooling medium is water or compressed air), and the cooling medium inlet and outlet pipe passes through the water-cooled split stainless steel plate through a ceramic insulating pipe to form a cooling circuit for the metal ring. Since the metal ring and the water-cooled split stainless steel plate are insulated from the water-cooled split stainless steel plate by a ceramic insulating sleeve and a ceramic insulating pipe, under the condition of high-frequency induction heating, the metal ring is heated by electromagnetic induction and the temperature rises. There is a high-chromium refractory plate on the top of the metal ring, and a groove for embedding the metal ring is opened at the bottom of the high-chromium refractory plate, and a hole is opened at the same position as the leakage hole of the water-cooled split stainless steel plate for leakage. When the leakage valve is not replaced, the cooling medium of the metal ring is compressed air, and the metal ring is heated under the action of high-frequency induction heating. The flow rate of compressed air is adjusted to control the temperature of the metal ring, and the metal ring conducts heat to the glass at the leakage hole to prevent glass crystallization. When the freeze-thaw valve is used for leakage, the solid glass in the leakage pipe is melted by induction heating of the medium-frequency coil, and the glass melt can leak out. When the leakage pipe needs to be replaced, water is passed into the metal ring to lower the temperature of the molten glass in the leakage hole at the bottom of the crucible to solidify it, and the molten glass in the cold crucible is prevented from flowing out to replace the leakage pipe at the bottom of the cold crucible. When the sliding valve is used for leakage, the sliding valve is pulled open, and the glass at the leakage hole melts under the heating action of the induction heating metal ring, and the molten glass leaks out from the leakage hole. When the leakage sliding valve needs to be replaced, water is passed into the metal ring to lower the temperature at the leakage hole, so that the molten glass at the leakage hole solidifies and the molten glass in the cold crucible is prevented from leaking out. Replace the leakage sliding valve when the melt in the cold crucible does not leak out. After replacing the leakage valve, you can continue to add material to the cold crucible for induction heating and melting, avoiding restarting the cold crucible.
[0009] The technical solution adopted by the present invention is as follows:
[0010] A cold crucible bottom for high-level waste liquid glass solidification, characterized in that it comprises a refractory plate, a leakage valve, a water-cooled stainless steel plate, a metal ring, a cooling medium inlet and outlet pipe, a partition, a ceramic insulating sleeve, and a ceramic insulating pipe;
[0011] The refractory material plate is provided with a leakage hole for the leakage valve to leak material;
[0012] The bottom of the refractory material plate is provided with a first groove for the metal ring to be embedded and a second groove for the cooling medium inlet and outlet pipe to be embedded;
[0013] The ceramic insulating sleeve is arranged outside the metal ring, and the water-cooled split stainless steel plate is provided with a steel plate groove for the metal ring and the ceramic insulating sleeve to be embedded;
[0014] The ceramic insulating tube is sleeved outside the cooling medium inlet and outlet pipes and penetrates the water-cooled split stainless steel plate.
[0015] The metal ring is a hollow structure with a cavity in the middle for the cooling medium to flow. The metal ring is connected to the cooling medium inlet and outlet pipes, and the cavity of the metal ring is isolated from the inside of the cooling medium inlet and outlet pipes by a partition.
[0016] The refractory material plate is fixed to the water-cooled split stainless steel plate so that the first groove corresponds to the groove of the steel plate, and is used to accommodate the metal ring with a ceramic insulating sleeve;
[0017] The leakage valve is located at the lower part of the water-cooled split stainless steel plate and is communicated with the leakage hole.
[0018] When the cold crucible leaks, compressed air is passed through the metal ring, and the temperature of the metal ring is controlled by adjusting the flow rate of the compressed air, thereby controlling the temperature of the glass in the leakage hole, inhibiting glass crystallization, and promoting glass leakage;
[0019] When the cold crucible is not stopped for replacement of the leakage valve, cooling water is introduced into the metal ring, and the temperature of the metal ring is controlled by adjusting the cooling water flow rate, thereby controlling the temperature of the glass in the leakage hole, so that the glass in the leakage hole solidifies and blocks the leakage hole. The leakage valve can be replaced safely when the glass melt in the cold crucible cannot flow out because the leakage hole is blocked by solid glass.
[0020] After replacing the leakage valve, switch the cooling water in the metal ring to compressed air, control the temperature of the metal ring, and then start the next leakage operation.
[0021] The high chromium refractory plate is circular, and its size is determined according to the inner diameter of the cold crucible. 2 O 3 The content is 50-90%. The refractory plate is provided with leakage holes for leakage according to different leakage valves. When the leakage valve is a freeze-thaw valve, the hole is circular; when the leakage valve is a slide valve, the hole is elongated. At the lower end of the high chromium refractory plate, a groove is provided for the metal ring and the metal ring cooling medium inlet and outlet pipe to be embedded.
[0022] The metal ring is a hollow structure, and its shape is similar to the shape of the leakage hole at the bottom of the cold crucible. The metal ring is connected with a cooling medium inlet and outlet pipe, and the cooling medium inlet and outlet pipe is used for the cooling medium (compressed air or water) to enter and exit the metal ring. There is a partition between the cooling medium inlet and outlet pipes of the metal ring to separate the inlet and outlet cooling medium, so as to prevent the metal ring from having a cooling dead zone.
[0023] The ceramic insulating sleeve is placed in the groove of the water-cooled split stainless steel plate to place the metal ring and insulate the metal ring from the water-cooled split stainless steel plate. The shape of the ceramic insulating sleeve is similar to the shape of the leakage hole of the water-cooled split stainless steel plate.
[0024] The ceramic insulating tube passes through the water-cooled split stainless steel plate. The upper end of the ceramic insulating tube is annular, and its size is larger than the through hole opened in the water-cooled split stainless steel plate for the ceramic insulating tube to pass through, so as to prevent the ceramic insulating tube from falling from the water-cooled split stainless steel plate. The cooling medium inlet and outlet pipe of the metal ring passes through the water-cooled split stainless steel plate through the ceramic insulating tube.
[0025] The water-cooled split stainless steel plate is provided with a leakage hole for a freeze-thaw valve or a sliding valve and a groove similar in shape to the leakage hole for placing the ceramic insulating sleeve. The water-cooled split stainless steel plate is equipped with a freeze-thaw valve leakage pipe or a water-cooled sliding valve.
[0026] The beneficial effects of the present invention are:
[0027] 1) Under induction heating conditions, the metal ring can assist in heating the glass in the leakage hole, change the temperature distribution of the bottom of the cold crucible, and promote leakage. Especially for glass that is easy to crystallize, controlling the temperature distribution of the bottom of the crucible can inhibit the crystallization of the glass near the leakage hole.
[0028] 2) The metal ring can be cooled by water to quickly lower the glass in the leakage hole and solidify it, which is convenient for hot replacement of the leakage valve (freeze-thaw valve or sliding valve) without stopping the furnace, providing guarantee for the long-term operation of cold crucible glass solidification.
[0029] 3) A high-chromium refractory plate is provided at the bottom of the cold crucible to protect the metal ring from corrosion by the high-temperature glass melt. The high-chromium refractory plate changes the temperature distribution of the cold shell layer at the bottom of the crucible, thins the cold shell layer at the bottom of the crucible, reduces the risk of crystallization of the glass at the bottom of the crucible, and is conducive to material leakage. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 Schematic diagram of a cold crucible bottom equipped with a freeze-thaw valve and a slide valve, wherein 1A is a cold crucible bottom equipped with a freeze-thaw valve, and 1B is a cold crucible bottom equipped with a slide valve
[0031] Figure 2It is the upper part of the refractory plate of the bottom of the cold crucible equipped with a freeze-thaw valve and a sliding valve, wherein 2A is the upper part of the refractory plate of the bottom of the cold crucible equipped with a freeze-thaw valve, and 2B is the upper part of the refractory plate of the bottom of the cold crucible equipped with a sliding valve.
[0032] Figure 3 It is a metal ring of the bottom of a cold crucible equipped with a freeze-thaw valve and a sliding valve, wherein 3A is a metal ring of the bottom of a cold crucible equipped with a freeze-thaw valve, and 3B is a metal ring of the bottom of a cold crucible equipped with a sliding valve.
[0033] Figure 4 It is the lower part of the refractory plate of the bottom of the cold crucible equipped with a freeze-thaw valve and a sliding valve, wherein 4A is the lower part of the refractory plate of the bottom of the cold crucible equipped with a freeze-thaw valve, and 4B is the lower part of the refractory plate of the bottom of the cold crucible equipped with a sliding valve.
[0034] Figure 5 5A is a cross-sectional view of a metal ring of a cold crucible bottom equipped with a freeze-thaw valve and a sliding valve, wherein 5A is a cross-sectional view of a metal ring of a cold crucible bottom equipped with a freeze-thaw valve, and 5B is a cross-sectional view of a metal ring of a cold crucible bottom equipped with a sliding valve
[0035] Figure 6 It is a ceramic insulation sleeve of the bottom of a cold crucible equipped with a freeze-thaw valve and a sliding valve, wherein 6A is a ceramic insulation sleeve of the bottom of a cold crucible equipped with a freeze-thaw valve, and 6B is a ceramic insulation sleeve of the bottom of a cold crucible equipped with a sliding valve.
[0036] Figure 7 Ceramic insulated tube with cold crucible bottom and equipped with freeze-thaw valve and slide valve
[0037] Figure 8 It is a water-cooled split stainless steel plate at the bottom of a cold crucible equipped with a freeze-thaw valve and a slide valve, wherein 8A is a water-cooled split stainless steel plate at the bottom of a cold crucible equipped with a freeze-thaw valve, and 8B is a water-cooled split stainless steel plate at the bottom of a cold crucible equipped with a slide valve.
[0038] Fig. 9 9A is a schematic diagram of the assembly of the bottom of a cold crucible equipped with a freeze-thaw valve and a sliding valve, wherein 9A is a schematic diagram of the assembly of the bottom of a cold crucible equipped with a freeze-thaw valve, and 9B is a schematic diagram of the assembly of the bottom of a cold crucible equipped with a sliding valve. DETAILED DESCRIPTION
[0039] The present invention will be further described below in conjunction with the accompanying drawings and embodiments, but the protection scope of the present invention shall not be limited thereto.
[0040] See also Figure 1 and Fig. 9As shown in the figure, a cold crucible bottom for high-level radioactive waste liquid glass solidification includes a refractory plate 2, a leakage valve 5, a water-cooled stainless steel plate 4, a metal ring 9, a cooling medium inlet and outlet pipe 10, a partition 14, a ceramic insulating sleeve 15 and a ceramic insulating tube 17. The refractory plate 2 is provided with a leakage hole 3 for the leakage valve 5 to leak; the bottom of the refractory plate is provided with a first groove 11 for the metal ring 9 to be embedded and a second groove 12 for the cooling medium inlet and outlet pipe 10 to be embedded; the ceramic insulating sleeve 15 is sleeved outside the metal ring 9, and the water-cooled split stainless steel plate 4 is provided with a steel plate groove 16 for the metal ring 9 and the ceramic insulating sleeve 15 to be embedded; the ceramic insulating tube 17 is sleeved outside the cooling medium inlet and outlet pipe 10 and passes through the water-cooled split stainless steel plate 4, the metal ring 9 is a hollow structure, and a cavity 13 for compressed air or water to flow is opened in the middle, the metal ring 9 is connected to the cooling medium inlet and outlet pipe 10, and the cavity 13 of the metal ring 9 is separated from the inside of the cooling medium inlet and outlet pipe 10 by a partition; the refractory plate 2 is fixed on the water-cooled split stainless steel plate 4 so that the first groove 11 corresponds to the groove 16 of the water-cooled split stainless steel plate, which is used to accommodate the metal ring 9 of the ceramic insulating sleeve 15. The leakage valve 5 is installed at the lower part of the water-cooled split stainless steel plate 4 and communicates with the leakage hole 3 .
[0041] Compressed air is passed through the metal ring, and the temperature of the metal ring is controlled by adjusting the flow rate of the compressed air, thereby controlling the temperature of the glass in the leakage hole, inhibiting glass crystallization, and promoting glass leakage;
[0042] When the cold crucible is not stopped for replacement of the leakage valve, cooling water is introduced into the metal ring, and the temperature of the metal ring is controlled by adjusting the cooling water flow rate, thereby controlling the temperature of the glass in the leakage hole, so that the glass in the leakage hole solidifies and blocks the leakage hole. The leakage valve can be replaced safely when the glass melt in the cold crucible cannot flow out because the leakage hole is blocked by solid glass.
[0043] After replacing the leakage valve, switch the cooling water in the metal ring to compressed air, control the temperature of the metal ring, and then start the next leakage operation.
[0044] See also Figure 1 A. When the freeze-thaw valve is used for leakage, the leakage valve 5 includes a medium frequency coil 6 and a leakage pipe 7. Figure 1 B. When a slide valve is used for leakage, the leakage valve 5 includes a water-cooled slide valve 8.
[0045] See also Figure 2 A and Figure 2 B, the refractory plate 2 is provided with a leakage hole 3, and the leakage hole 3 is located at the center or eccentric position of the refractory plate. 2 O 3Made of high chromium refractory material with a content of 70wt%.
[0046] See also Figure 3 , a cold crucible bottom 1 for high-level waste liquid glass solidification, further comprising a metal ring 9 embedded in a water-cooled split stainless steel plate 4 and a refractory plate 2 and a metal ring cooling medium inlet and outlet pipe 10. The metal ring cooling medium inlet and outlet pipe is welded to the metal ring. Figure 3 A, the metal ring 9 of the leakage valve 5 when the freeze-thaw valve leaks is circular, see Figure 3 B. The metal ring 9 of the leakage valve 5 when the sliding valve is used for leakage is long and made of titanium.
[0047] See also Figure 4 The lower part of the refractory plate 2 is provided with grooves 11 and 12 for embedding the metal ring 9 and the cooling medium inlet and outlet pipes 10.
[0048] See also Figure 5 The metal ring 9 is a hollow structure with a cavity 13 for compressed air or water to flow. The cavity 13 has a partition 14 between the cooling medium inlet and outlet pipes 10 for separating the incoming cooling medium from the discharged cooling medium. Figure 5 A is the cross-sectional view of the metal ring of the freeze-thaw valve leakage valve. Figure 5 B is a cross-sectional view of the metal ring of the sliding valve which is a leakage valve.
[0049] See also Figure 6 A cold crucible bottom 1 for high-level waste liquid glass solidification, further comprising a ceramic insulating sleeve 15 between the water-cooled split stainless steel plate 4 and the metal ring 9, wherein the ceramic insulating sleeve 15 is provided with a groove 16 for the metal ring 9 to be embedded. Figure 6 A, the ceramic insulating sleeve 15 of the leakage valve 5 when the freeze-thaw valve leaks is round, see Figure 6 B. When the leakage valve 5 uses a slide valve for leakage, the ceramic insulating sleeve 15 is long.
[0050] See also Figure 7 The cooling medium inlet and outlet pipe 10 passes through the hole 18 of the ceramic insulating tube 17 and passes through the water-cooled split stainless steel plate.
[0051] See also Figure 8 The water-cooled split stainless steel plate 4 is provided with a groove 19 for embedding the ceramic insulating sleeve 15 and a material leakage hole 3 for material leakage. The ceramic insulating tube 17 passes through the water-cooled split stainless steel plate 4 through the hole 20.
[0052] See also Fig. 9, the assembly of the bottom of the cold crucible for high-level waste liquid glass solidification of the present invention is further described. The ceramic insulating sleeve 15 is placed in the groove 19 of the water-cooled split stainless steel plate 4, the ceramic insulating tube 17 passes through the water-cooled split stainless steel plate 4 through the hole 20, the metal ring 9 is placed in the ceramic insulating sleeve 15 and is higher than the ceramic insulating sleeve 15, which is convenient for electromagnetic induction heating, the hole 18 of the ceramic insulating tube 17 of the cooling medium inlet and outlet pipe 10 passes through the water-cooled split stainless steel plate 4, the refractory material plate 2 is placed on the water-cooled split stainless steel plate 4, and the part of the metal ring 9 that is higher than the water-cooled split stainless steel plate is embedded in the refractory material plate.
[0053] The use instructions of the cold crucible bottom for high-level radioactive waste glass solidification of the present invention are as follows:
[0054] The composition of high-level waste liquid is complex, the crystallization performance of the glass solidification body is poor, and the crystallization temperature range is wide. Therefore, it is necessary to accurately control the temperature of the bottom of the crucible of the high-level waste liquid cold crucible glass solidification to control the crystallization of the bottom of the cold crucible to avoid affecting the leakage. On the other hand, the leakage valve is in direct contact with the glass liquid and is severely corroded. It needs to be replaced regularly in a hot state without stopping the furnace to ensure the long-term stable operation of the cold crucible glass solidification. When the high-level waste liquid cold crucible glass solidification system is in operation, the metal ring placed at the bottom of the crucible is in an induction magnetic field, and the temperature rises due to the induction heating. The metal ring transfers heat to the surrounding refractory materials and heats the glass in the leakage hole, so that the glass temperature in the leakage hole is outside the crystallization temperature range and does not block the leakage hole due to crystallization. In order to prevent overheating of the glass in the leakage hole, the metal ring is cooled by compressed air to control the temperature of the glass in the leakage hole. When leakage is required, in addition to operating the leakage valve, the compressed air flow of the metal ring is adjusted to increase the temperature of the glass in the leakage hole for easy leakage. When the leakage valve needs to be replaced, the temperature of the glass in the leakage hole needs to be lowered so that the glass solidifies and blocks the leakage hole. At this time, the cooling medium is replaced with cooling water, the cooling of the metal ring is strengthened, the temperature of the glass in the leakage hole is quickly lowered, the leakage hole is blocked, and the glass melt in the furnace will not leak out of the leakage hole, making it easier to replace the leakage valve at the bottom of the crucible. After the leakage valve is replaced, the cooling water of the metal ring is switched to compressed air, and the auxiliary heating function of the metal ring is used to prevent the crystallization of the glass at the leakage port, promoting the smooth leakage.
Claims
1. A cold crucible bottom for high-level waste liquid glass solidification, characterized in that: It comprises a refractory plate (2), a leakage valve (5), a water-cooled stainless steel plate (4), a metal ring (9), a cooling medium inlet and outlet pipe (10), a partition (14), a ceramic insulating sleeve (15), and a ceramic insulating pipe (17). The refractory material plate (2) is provided with a leakage hole (3) for the leakage valve (5) to leak material; The bottom of the refractory material plate (2) is provided with a first groove (11) for the metal ring (9) to be embedded and a second groove (12) for the cooling medium inlet and outlet pipe (10) to be embedded; The ceramic insulating sleeve (15) is provided with a groove (16) for accommodating the metal ring (9), and the water-cooled split stainless steel plate (4) is provided with a groove (19) for the ceramic insulating sleeve (15) to be embedded in the water-cooled split stainless steel plate; The ceramic insulating tube (17) is arranged outside the cooling medium inlet and outlet tube (10) and passes through the water-cooled split stainless steel plate (4); The metal ring (9) is a hollow structure, with a cavity (13) in the middle for cooling medium to flow, the metal ring (9) is connected to the cooling medium inlet and outlet pipe (10), and the cavity (13) of the metal ring (9) is isolated from the inside of the cooling medium inlet and outlet pipe (10) by a partition; The refractory material plate (2) is located on the water-cooled split stainless steel plate (4) so that the first groove (11) corresponds to the groove (19) of the water-cooled split stainless steel plate (4) and is used to accommodate the ceramic insulating sleeve (15) and the metal ring (9).
2. The cold crucible bottom for high-level radioactive waste glass solidification according to claim 1, characterized in that: When the cold crucible leaks, compressed air is passed through the metal ring (9), and the temperature of the metal ring (9) is controlled by adjusting the flow rate of the compressed air, thereby controlling the temperature of the glass in the leakage hole (3), inhibiting glass crystallization, and promoting glass leakage; When the cold crucible is not shut down to replace the leakage valve (5), cooling water is introduced into the metal ring, and the temperature of the metal ring (9) is controlled by adjusting the cooling water flow rate, thereby controlling the temperature of the glass in the leakage hole (3), so that the glass in the leakage hole (3) solidifies and blocks the leakage hole (3), and the leakage valve (5) is safely replaced when the glass melt in the cold crucible cannot flow out because the leakage hole (3) is blocked by solid glass; After replacing the leakage valve (5), the cooling water in the metal ring is switched to compressed air, the temperature of the metal ring is controlled, and the next leakage operation can be started.
3. The cold crucible bottom for high-level radioactive waste glass solidification according to claim 1 or 2, characterized in that: The refractory plate is made of a high-chromium refractory material with a Cr2O3 content of 50-90wt%.
Citation Information
Patent Citations
High-temperature melt unloading device for cooling crucible
CN106123588A
Cold crucible device
CN205048973U
Crucibles for melting material and methods of transferring material therefrom
US20160091249A1
Cold crucible base and discharging method thereof
CN113137858A
Glass melting furnace
CN114249522A