A method for non-destructive processing of narrow slit cavity microholes using ultrashort pulse laser beams

Through the layer-by-layer scanning processing of ultra-short pulse laser beams and multi-feature point positioning technology, combined with the use of laser protective objects, the problems of inner cavity damage and positioning errors in the processing of air film holes in aeroengine turbine blades are solved. , achieving damage-free, high-quality micro-hole processing to meet design requirements.

CN115922111BActive Publication Date: 2024-10-18AECC AVIATION POWER CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202211567072.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-07
Publication Date
2024-10-18
Estimated Expiration
2042-12-07

AI Technical Summary

Technical Problem

On aero-engine turbine blades, the machining locations for special-purpose air film holes are complex and the space is narrow. Existing laser processing can easily damage the inner cavity of the blade, resulting in spatter residue and positioning errors, making it difficult to achieve damage-free and high-quality micro-hole processing.

Method used

It adopts ultra-short pulse laser beam non-destructive processing method, combines laser active protection technology and passive protection technology, and uses dynamic light beam to scan the surface layer by layer, and uses multi-feature point positioning and real-time monitoring system to achieve precise hole positioning and internal processing. High-quality machining without spatter in the cavity.

Benefits of technology

It achieves damage-free, high-quality narrow-slit cavity micro-hole processing, ensuring accurate hole position and no damage to the inner cavity. The process is simple, meets the design requirements, and improves the quality of micro-hole processing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115922111B_ABST
    Figure CN115922111B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of special processing, and in particular to a method for non-destructive processing of narrow slit cavity micropores by ultrashort pulse laser beams, comprising the following steps: S1, blade inner cavity protection: inserting a laser shield into the inner cavity of the narrow film hole processing part of the blade from the side of the slit of the exhaust edge of the blade; S2, positioning the processing position of the narrow film hole of the blade; S3, processing of the narrow film hole of the blade: using ultrashort pulse laser beam processing equipment to perform processing in a dynamic light beam layer-by-layer scanning manner, and monitoring the processing process through a CCD coaxial video monitoring system. The present invention integrates and innovates laser active protection technology (ultrashort pulse laser beam parameter control), laser passive protection technology (shield filling and removal), hole position precise positioning technology (multi-feature point positioning), and real-time processing monitoring technology (CCD coaxial video monitoring system) to form a complete set of processing methods.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of special processing, in particular to a method for processing narrow slit cavity microholes without damage by using an ultrashort pulse laser beam. Background Art

[0002] The high-pressure turbine blades of aircraft engines are made of high-temperature alloy directional precision casting. A large number of air film holes are designed on the leading edge and blade surface. The hole diameter is generally Φ0.2mm-Φ0.6mm, and the spatial angle is complex. Some air film holes for specific purposes are designed in semi-enclosed narrow cavities (cavity narrow slit 0.3~0.6mm) ( Figure 1 ), and the spatial angle is complex, the aperture is Φ0.25mm, and the processing is difficult. When laser processing this type of air film hole, it is easy to damage the spoiler column in the blade cavity and cause splash residue in the cavity, or due to large positioning errors and excessive positioning, damage the side wall and cause waste.

[0003] Faced with the development demand of new aircraft engine turbine blade film holes, the problem of damage-free laser hole making of turbine blade film cooling holes will become more prominent. The processing positions of film holes for certain specific purposes are becoming increasingly difficult to process, and the blade inner cavity space will become narrower and narrower. Both the precise positioning of the hole position and the protection against inner cavity damage will face more stringent conditions. The damage-free laser hole making process method is particularly important and critical. Summary of the invention

[0004] In view of the problems existing in the prior art, the present invention provides a method for damage-free processing of narrow slit cavity microholes by ultrashort pulse laser beam, which can achieve high-quality damage-free laser microhole processing with precise hole positioning, no splash adhesion in the inner cavity, and no damage to the cavity. The process flow is simple and meets the design requirements.

[0005] The present invention is achieved through the following technical solutions:

[0006] A method for non-destructive processing of narrow slit cavity microholes by ultrashort pulse laser beams comprises the following steps:

[0007] S1, blade inner cavity protection: insert the laser protection into the inner cavity of the narrow film hole processing part of the blade from the side of the slit on the exhaust side of the blade;

[0008] S2, locate the processing position of the narrow air film hole of the blade;

[0009] S3, processing of blade narrow film holes: using ultrashort pulse laser beam processing equipment to perform processing in a dynamic light beam scanning manner layer by layer, and monitoring the processing process through a CCD coaxial video monitoring system. Preferably, in S1, the laser shield is made of the same material as the blade.

[0010] Preferably, in S2, the specific steps of positioning are as follows:

[0011] S21, adopts falcon tooth structure positioning, and installs the blade fixture on the quick-change fixture positioning seat installed on the machine tool axis chuck through the positioning pin;

[0012] S22, using multi-feature point positioning technology to position the blade so that the workpiece reference coordinates are unified with the machine tool reference coordinates;

[0013] S23, selecting feature positioning points around the narrow slit cavity to locate the processing position of the air film hole.

[0014] Preferably, in S22, eight positioning points are selected, and the data of 6-8 positioning points are measured and collected by using an infrared laser rangefinder through a multi-feature point positioning control program, and compared and calculated with the theoretical blade positioning point data to perform interpolation compensation operations.

[0015] Preferably, in S22, the position positioning error is controlled to be less than 0.3 mm.

[0016] Preferably, in S23, the position positioning error is controlled to be less than 0.1 mm.

[0017] Preferably, in S3, during processing, multi-stage parameters are used for processing according to different positions of the air film holes.

[0018] Preferably, when the dynamic light beam is used for layer-by-layer scanning, the specific steps are as follows:

[0019] S31, dividing the air film holes into n processing areas according to the position structure;

[0020] S32, dividing each processing area into different numbers of circles and layers;

[0021] S33, dividing each processing area segment into different circles;

[0022] S34, respectively setting different circle powers for each processing area segment.

[0023] Preferably, in S31, the air film hole is divided into four sections according to different positions, which are recorded as the hole entrance, the hole upper end, the hole lower end and the hole exit.

[0024] Preferably, in S32, the air film holes are divided into the 1st to 25th layers at the hole entrance, the 26th to 50th layers at the hole upper end, the 51st to 60th layers at the hole lower end; and the 61st to 70th layers at the hole exit.

[0025] Compared with the prior art, the present invention has the following beneficial effects:

[0026] The invention discloses a method for non-destructive processing of narrow slit cavity micro-holes by ultra-short pulse laser beams. The method combines laser active protection technology (ultra-short pulse laser beam parameter control) and laser passive protection technology (protection material filling and removal) according to the characteristics of parts to achieve non-destructive high-quality hole making. The method utilizes real-time processing monitoring technology (CCD coaxial video monitoring system) to achieve processing process state control, achieve the purpose of non-destructive laser hole making, improve the micro-hole processing quality, and has a simple process flow that meets the design requirements.

[0027] Furthermore, accurate positioning is achieved by utilizing hole position precision positioning technology (multi-feature point positioning).

[0028] Furthermore, different laser energies are set in sections, layers and circles to achieve reasonable distribution of energy. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a structural diagram of a blade;

[0030] Figure 2 is a schematic diagram of the location of the laser shield;

[0031] Figure 3 This is a schematic diagram of quick-change fixture installation;

[0032] Figure 4 This is a schematic diagram of multi-feature point positioning (precise positioning);

[0033] Figure 5 This is a schematic diagram of the laser processing head accurately positioning to the air film hole processing position;

[0034] Figure 6 Schematic diagram of the ultrashort pulse laser beam (picosecond laser beam) hole making process (active protection). DETAILED DESCRIPTION

[0035] The present invention is further described in detail below in conjunction with specific embodiments, which are intended to explain the present invention rather than to limit it.

[0036] The present invention discloses a method for non-destructively processing narrow slit cavity micro-holes by ultrashort pulse laser beam, comprising the following steps:

[0037] S1, blade inner cavity protection: insert a laser shield made of the same material as the blade into the inner cavity of the narrow film hole processing part of the blade from the side of the slit of the blade exhaust side. In this embodiment, the laser shield is 15×1×1mm in length×width×height. Figure 2 , a laser beam protection barrier is formed in the inner cavity of the narrow cavity air film hole processing part of the blade to prevent damage to the inner cavity and the spoiler column.

[0038] S2, locate the processing position of the narrow air film hole of the blade, the specific steps are as follows:

[0039] S21, using falcon tooth structure positioning, refer to Figure 3 , the blade fixture is mounted on the quick-change fixture positioning seat mounted on the machine tool shaft chuck through the positioning pins;

[0040] S22, uses multi-feature point positioning technology to position the blade (key parts such as blade basin, blade back, air intake edge, edge plate, etc.) to unify the workpiece reference coordinates with the machine tool reference coordinates. The operation is as follows: eight positioning points are selected, and the infrared laser rangefinder is used to measure and collect 6-8 positioning point data through the multi-feature point positioning control program. The data is compared and calculated with the theoretical blade positioning point data, and interpolation compensation calculations are performed to control the position error to less than 0.3mm.

[0041] S23, selecting characteristic positioning points (8 characteristic points are selected in this embodiment) around the narrow slit cavity to locate the processing position of the air film hole, controlling the positioning error to be less than 0.1 mm, and accurately locating the processing position.

[0042] Then input the coordinates of the narrow cavity air film hole workpiece to accurately move the laser processing head to the narrow cavity air film hole processing position (such as Figure 4 and 5 as shown).

[0043] S3, Processing of narrow air film holes on blades: Ultrashort pulse laser beam processing equipment is used to perform processing in a dynamic light beam scanning manner layer by layer, and the processing process is monitored by a CCD coaxial video monitoring system.

[0044] During processing, multi-stage parameters are used according to the different positions of the air film holes. The air film holes are divided into four sections according to their positions, namely the hole entrance, the upper end of the hole, the lower end of the hole and the hole exit. When the dynamic light beam is used for layer-by-layer scanning,

[0045] The processing parameters are based on the diameter of the micropores in the blade narrow slit cavity (the diameter is φ0.25 +0.1 ~φ0.45 +0.1 The adjustment range in mm is as follows:

[0046] 1) Determine the laser pulse width (range: 15ps);

[0047] 2) Determine the pulse frequency (range: 100kHZ);

[0048] 3) Determine the laser power percentage (70%~90%);

[0049] 4) Defocus (range: -1-1mm);

[0050] 5) Determine the feed speed (range: 150~200mm / min);

[0051] 6) Determine the auxiliary gas and gas pressure (flow rate) parameters (argon gas range: 0.6~0.8MPa).

[0052] The specific steps are as follows:

[0053] S31, dividing the air film holes into n processing areas according to the position structure;

[0054] S32, dividing each processing area into different numbers of circles and layers;

[0055] S33, dividing each processing area segment into different circles;

[0056] S34, respectively setting different circle powers for each processing area segment.

[0057] The CCD coaxial video monitoring system can be used to monitor the hole-making status of the ultrashort pulse laser beam (picosecond laser beam) in real time. If any abnormality is found, the processing will be stopped immediately. After the abnormality is eliminated, the processing can be continued.

[0058] Abnormal situation 1

[0059] Through CCD video observation, during the laser processing, the monitor shows that the laser spot changes from bright to dark, and then a large amount of splashing light appears, indicating that the inner cavity filler is not filled sufficiently, damaging the inner wall, and the metal melt of the blade parts splashes. Elimination method: (1) Immediately press the emergency stop button to stop processing; (2) Clean the inner cavity filler and fill it again.

[0060] Abnormal situation 2

[0061] Through the CCD video screen, the laser spot displayed on the monitor is not bright during the laser processing. Solution: (1) Immediately press the emergency stop button to stop the processing; (2) Reset the laser processing parameters and restart the laser light source.

[0062] S4, removal of inner cavity protection: remove the laser protection (length × width × height: 15 × 1 × 1mm metal strip of the same material) inserted into the inner cavity of the blade.

[0063] S5, blade cleaning: Place the blades in an ultrasonic cleaning machine, add cleaning solution (pure water), clean the blades and remove impurities.

[0064] S6, inspection of blade film holes:

[0065] (1) Check the processing quality of the inner cavity of the air film hole through X-ray. There is no splash residue in the inner cavity of the blade, no damage to the spoiler column, and no damage to the side wall.

[0066] (2) The hole size is checked by plug gauge, and the hole size meets the design requirements. The hole size specification is 0.25 +0.1mm, and the measuring plug gauges are φ0.25mm and φ0.35mm.

[0067] Based on the processing of air film holes of a certain type of turbine blade (such as Figure 1 As shown in the figure, Figure 1 Middle holes 1, 2, and 3 are processing positions:

[0068] Three air film holes are machined in a narrow slit-shaped space near the trailing edge of a high-pressure turbine blade cover. The hole diameter is Φ0.25+0.1mm. There is an angle between the hole axis and the horizontal and vertical normals. The smallest part of the slit cavity is only 0.6mm. It is required that there is no damage to the inner cavity of the blade and no splash deposition. The specific steps are as follows:

[0069] (1) Blade cavity protection:

[0070] Passive protection technology is used to insert laser protection (length × width × height: 15 × 1 × 1mm metal strip of the same material) from the side of the slit on the exhaust side of the blade, and the position is as follows: Figure 2 shown.

[0071] (2) Precise positioning of air film holes in narrow blade cavities:

[0072] The blades are positioned using a falcon tooth structure, and high-precision quick-change tooling is used to install the fixture on the quick-change fixture positioning seat on the machine tool shaft chuck through positioning rivets.

[0073] The multi-feature point positioning technology is used to select 6-8 positioning points at key locations such as the blade basin, blade back, air intake edge, and edge plate. The multi-feature point positioning control program uses an infrared laser rangefinder to measure and collect 6-8 positioning point data, which are compared and calculated with the theoretical blade positioning point data, and interpolation compensation operations are performed to control the position error to less than 0.3mm, unify the workpiece reference coordinates with the machine tool reference coordinates, and automatically establish the processing coordinate system.

[0074] Eight characteristic positioning points are selected around the narrow slit cavity to accurately locate the processing position of the air film hole, control the positioning error to less than 0.1mm, and accurately locate the processing position.

[0075] Input the workpiece coordinates of the narrow cavity air film hole to accurately move the laser processing head to the narrow cavity air film hole processing position ( Figure 4 , Figure 5 ).

[0076] (3) Ultrashort pulse laser beam (picosecond laser beam) processing of air film holes in narrow blade cavities ( Figure 6 ):

[0077] The main process parameters of ultrashort pulse laser beam (picosecond laser beam) processing are: 1) Determine the laser pulse width (15ps); 2) Determine the pulse frequency (100kHZ); 3) Determine the laser power percentage (70%); 4) Defocus amount (0mm); 5) Determine the feed speed (200mm / min); 6) Determine the auxiliary gas and gas pressure (flow) parameters (argon gas range: 0.6-0.8MPa).

[0078] The 3D hole making process and multi-stage parameter processing are adopted. Different processing parameters (as shown in Table 1) are adopted according to the different positions of the hole entrance, the upper end of the hole, the lower end of the hole, and the hole exit to optimize the processing and improve the processing efficiency and quality. In this embodiment, the number of layers of the hole entrance is the 1st to 25th layer, the number of layers of the upper end of the hole is the 26th to 50th layer, the number of layers of the lower end of the hole is the 51st to 60th layer; the number of layers of the hole exit is the 61st to 70th layer.

[0079] Table 1 Parameter settings for machining film holes of a certain type of turbine blade

[0080]

[0081] S4, removal of inner cavity protection: remove the laser protection (length × width × height: 15 × 1 × 1mm metal strip of the same material) inserted into the inner cavity of the blade.

[0082] S5, blade cleaning: Place the blades in an ultrasonic cleaning machine, add cleaning solution (pure water), clean the blades and remove impurities.

[0083] S6, inspection of blade film holes:

[0084] (1) Check the processing quality of the inner cavity of the air film hole through X-ray. There is no splash residue in the inner cavity of the blade, no damage to the spoiler column, and no damage to the side wall.

[0085] (2) The hole size is checked by plug gauge and the hole size meets the design requirements.

[0086] The method for processing narrow slit cavity microholes without damage by ultrashort pulse laser beams of the present invention utilizes ultrashort pulse laser beam (picosecond laser beam) processing equipment, adopts active protection technology, uses ultrashort pulse laser beam (picosecond laser beam) hole making technology, uses a dynamic light beam layer-by-layer scanning method, adopts a 3D hole making process, accurately controls the laser energy field distribution in a three-dimensional scale, reduces the energy distribution in the processing depth direction, and relies on adjusting laser processing parameters (active protection) to achieve the purpose of protecting the inner cavity.

[0087] Compared with the existing laser processing methods, the present invention can achieve damage-free high-quality hole making by combining laser active protection technology (ultra-short pulse laser beam parameter control) and laser passive protection technology (filling and removal of protection materials) according to the characteristics of the parts; accurate positioning is achieved by using hole position precision positioning technology (multi-feature point positioning); real-time processing monitoring technology (CCD coaxial video monitoring system) is used to achieve processing process state control, so as to achieve the purpose of damage-free laser hole making and improve the quality of micro-hole processing. The process flow is simple and meets the design requirements.

[0088] The present invention integrates and innovates laser active protection technology (ultra-short pulse laser beam parameter control), laser passive protection technology (protection material filling and removal), hole position precision positioning technology (multi-feature point positioning), and real-time processing monitoring technology (CCD coaxial video monitoring system) to form a complete set of processing methods.

[0089] The above description is only a preferred embodiment of the present invention and is not intended to impose any limitation on the technical solution of the present invention. Those skilled in the art should understand that, without departing from the spirit and principles of the present invention, the technical solution can also be subjected to several simple modifications and substitutions, and these modifications and substitutions are also within the scope of protection covered by the claims.

Claims

1. A method for non-destructive processing of narrow slit cavity microholes by ultrashort pulse laser beam, characterized in that: The following steps are involved: S1, blade inner cavity protection: insert the laser protection into the inner cavity of the narrow film hole processing part of the blade from the side of the cleavage of the blade exhaust edge; the narrow slit of the narrow film hole of the blade is 0.3~0.6mm, and the hole diameter is Φ0.25mm; S2, locating the processing position of the narrow air film hole of the blade; wherein the specific steps of locating are as follows: S21, adopts falcon tooth structure positioning, and installs the blade fixture on the quick-change fixture positioning seat on the machine tool axis chuck through positioning pins; S22, use multi-feature point positioning technology to position the blade, so that the workpiece reference coordinates and the machine tool reference coordinates are unified; select eight positioning points, use the multi-feature point positioning control program to measure and collect 6-8 positioning point data using an infrared laser rangefinder, compare and calculate with the theoretical blade positioning point data, and perform interpolation compensation calculation; control the position error <0.3mm; S23, around the narrow slit cavity, select characteristic positioning points to locate the processing position of the air film hole; control the positioning error to be less than 0.1mm; S3, Processing of narrow film holes on blades: Ultrashort pulse laser beam processing equipment is used to perform layer-by-layer scanning of the dynamic light beam, and the processing process is monitored by a CCD coaxial video monitoring system; Among them, during processing, multi-stage parameters are used for processing according to different positions of the air film holes; when the dynamic light beam is used for layer-by-layer scanning, the specific steps are as follows: S31, dividing the air film hole into n processing areas according to the position structure; the air film hole is divided into four sections according to different positions, which are recorded as the hole entrance, the hole upper end, the hole lower end and the hole exit; S32, each processing area is divided into different circles and layers; the air film hole is divided into the 1st to 25th layers at the hole entrance, the 26th to 50th layers at the hole upper end, the 51st to 60th layers at the hole lower end; the 61st to 70th layers at the hole exit; S33, dividing each processing area segment into different circles; S34, respectively setting different circle powers for each processing area segment.

2. The method for non-destructive processing of narrow slit cavity microholes by ultrashort pulse laser beam according to claim 1, characterized in that: In S1, the laser shield is made of the same material as the blade.

Citation Information

Patent Citations

  • Laser processing method for air film holes of high-pressure turbine guiding blade

    CN109158776A

  • Femtosecond laser processing system and method for preparing turbine blade film hole

    CN115055844A

  • Self-adaptive positioning method for complex curved surface femtosecond laser micro-hole machining

    CN115255609A