A self-enhanced electrochemiluminescent composite and its application

By constructing a porous structural framework and a self-enhanced electrochemiluminescent complex embedded with perfluoro-15 crown-5 ether, combined with biotinylated glucose oxidase, the sensitivity problems of gas fixation and glucose detection were solved, and high sensitivity of glucose was achieved. and wide linear detection.

CN116285957BActive Publication Date: 2024-10-11NANJING UNIV OF SCI & TECH
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202211504820.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-28
Publication Date
2024-10-11
Estimated Expiration
2042-11-28

AI Technical Summary

Technical Problem

The existing technology fails to realize that the self-enhanced electrochemiluminescence complex of gas is fixed on the electrode surface, which limits the application of gas electrochemiluminescence detection, especially the lack of high sensitivity and rapid detection methods in glucose monitoring.

Method used

A self-enhanced electrochemiluminescent composite was prepared by constructing a porous structural framework by constructing tetrahydroxyphenylzinc porphyrin, fluorinated carbon chain and carboxyl-polyethylene glycol-biotin, and embedding perfluoro-15 crown-5 ether in it. It combines streptavidin and biotinylated glucose oxidase to fix oxygen on the electrode surface to form a self-enhanced electrochemiluminescence biosensor.

Benefits of technology

It achieves effective gas fixation and high-sensitivity detection of glucose, with a linear detection range of 0.1mM to 10mM, a minimum detection limit of 62μM, and good anti-interference and adjustable functions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116285957B_ABST
    Figure CN116285957B_ABST
Patent Text Reader

Abstract

The invention discloses a self-enhanced electrochemiluminescent composite and application, wherein the composite is first prepared by constructing a porous structure framework of tetrahydroxyphenyl zinc porphyrin, a fluorinated carbon chain and carboxyl-polyethylene glycol-biotin, and then embedding a perfluoro-15-crown-5 ether with high oxygen carrying capacity in the porous structure. The fluorinated carbon chain can be perfluorosuccinic acid, perfluoroglutaric acid, perfluoroadipic acid, perfluorooctanedioic acid, perfluoroazelaic acid or perfluorodecanedioic acid, so as to construct a composite with different pore sizes. By comparing the electrochemiluminescent signals of these six substances, it is found that the electrochemiluminescent intensity of the composite prepared by perfluorodecanedioic acid is the largest. Therefore, by utilizing the affinity between streptavidin and biotin, biotinylated glucose oxidase is fixed on the surface of the composite prepared by perfluorodecanedioic acid to form a self-enhanced electrochemiluminescent biosensor, and the sensor can quantitatively detect glucose, showing a wide detection linear range and high sensitivity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of physical and chemical analysis, and in particular relates to a self-enhanced electrochemiluminescent compound and its application. Background Art

[0002] As a powerful and sensitive analytical technique, electrochemiluminescence (ECL) is a process in which highly active substances are generated on the electrode surface, and excited states are generated through high-energy electron transfer reactions for light emission. It effectively combines the unique advantages of both electrochemistry and chemiluminescence, showing high sensitivity, low background, wide dynamic range, easy control and simple equipment. Therefore, ECL has been widely used in organic analysis, immunosensors, DNA probe detection and enzyme biosensors. In these applications, how to achieve signal amplification is a key link. The self-enhanced ECL complex that can be fixed on the electrode surface as a luminophore has obvious advantages, including shortening the electron transfer distance between the two, reducing energy loss, achieving luminescence stability and enhancing luminescence efficiency, reducing reagent consumption, simplifying the analysis process, and expanding its application range. At present, there is no self-enhanced ECL luminophore for fixing gas on the electrode surface. Therefore, it is necessary to explore a suitable nanocarrier to realize the gas self-enhanced electrochemiluminescence complex.

[0003] As we all know, porous materials have aroused great interest due to their high surface area, high porosity and easy surface modification. Among various porous material families, covalent organic framework (COP) has received extensive research attention in recent years. COP is an emerging multidimensional and multifunctional material composed of organic monomers connected by stable covalent bonds. It has many unique properties, including excellent thermal and chemical stability, adjustable and designable structure and function. In particular, luminescent functionalized COP. By integrating electrochemiluminescent bodies into the framework or cavity of COP, a new platform for constructing self-enhanced ECL is provided.

[0004] Perfluorocarbons (PFCs) are a class of chemically inert molecules composed of carbon and fluorine atoms. They are divided into two categories according to their structure: aliphatic and aromatic. Under the same atmospheric pressure, oxygen dissolved in PFCs 2 ) is much higher than that in water, even up to 1000 times. Drawing on the successful manufacturing of PFC as an artificial blood substitute, nanodroplets of PFC with good biocompatibility and high oxygen solubility are very useful as oxygen delivery carriers and are widely used in photodynamic therapy (PDT).

[0005] Glucose testing is crucial in clinical diagnostics, biotechnology, and the food industry. Glucose is not only the main energy source for the human body, but is also closely related to diabetes. Millions of diabetics need to test their blood sugar levels every day. Abnormal blood sugar levels caused by diabetes can lead to serious complications, including blindness, cardiovascular disease, and kidney failure. In addition, in order to control glucose levels, normal people (normal glucose levels in the blood are between 4.4 and 6.6 mmol·L -1 Glucose monitoring should also be performed on patients with diabetes and non-diabetic emergency cases. Therefore, monitoring many samples is very beneficial for the early detection, prevention, diagnosis and management of diabetes. It is clinically important to develop a simple, rapid and sensitive method to monitor glucose levels. Summary of the invention

[0006] The purpose of the present invention is to address the deficiencies of the prior art and provide a self-enhanced electrochemiluminescent complex as an ECL luminophore, which can fix the gas on the electrode surface and be applied to electrochemiluminescence detection of glucose with good detection performance.

[0007] The object of the present invention is achieved through the following technical solution: A self-enhanced electrochemiluminescent composite is obtained by the following preparation method:

[0008] (1) first weighing tetrahydroxyphenylporphyrin and zinc acetate, dissolving them in dimethylformamide, and shaking until they are uniformly mixed, wherein the molar ratio of the tetrahydroxyphenylporphyrin to the zinc acetate is 1:5-9; then heating in an oil bath to 110-120° C., and refluxing for 45-60 minutes; cooling to room temperature, pouring deionized water, and allowing to stand, centrifuging to obtain a precipitate, and drying the precipitate to obtain tetrahydroxyphenyl zinc porphyrin;

[0009] (2) dissolving the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine obtained in step (1) in tetrahydrofuran, wherein the molar ratio of the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine is 1:1.5:20:20, heating to 40-50° C. in the dark and stirring until the mixture is uniformly mixed, and the reaction time is 12-18 hours; then adding carboxyl-polyethylene glycol-biotin, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine, wherein the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine are mixed, and the mixture is stirred for 12-18 hours. Hydroxyphenyl zinc porphyrin, carboxyl-polyethylene glycol-biotin, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine are reacted in a molar ratio of 1:4:10:10 at 40-50°C in the dark for 18-20 hours; then, after evaporation and concentration to obtain a solid substance, the solid substance is first dissolved with methanol and then precipitated with ice ether, and the precipitate is repeatedly dissolved until the supernatant is colorless; then, the precipitate is dialyzed to remove impurities, and finally, it is freeze-dried to obtain a biotinylated zinc perfluoro aromatic framework and stored in the dark at 2-8°C for standby use; the biotinylated zinc perfluoro aromatic framework is labeled as ZnPAFn-b;

[0010] (3) Dissolving the ZnPAFn-b obtained in step (2) in deionized water, adding perfluoro-15-crown-5 ether, wherein the molar ratio of ZnPAFn-b to perfluoro-15-crown-5 ether is 1:64; then ultrasonicating in a water bath, centrifuging, collecting the upper layer liquid, and obtaining a self-enhanced electrochemiluminescent complex, labeled as PCE@ZnPAFn-b.

[0011] Furthermore, the fluorinated carbon chain is perfluorosuccinic acid, perfluoroglutaric acid, perfluoroadipic acid, perfluorooctanedioic acid, perfluoroazelaic acid or perfluorodecanedioic acid.

[0012] Furthermore, the fluorinated carbon chain is perfluorosebacic acid.

[0013] Furthermore, n in ZnPAFn-b and PCE@ZnPAFn-b is 4, 6, 8, 12, 14 or 16; n is the number of fluorine atoms.

[0014] Furthermore, the molecular weight cut-off of the dialysis is greater than or equal to 2000Da.

[0015] Application of the above-mentioned self-enhanced electrochemiluminescent complex in the preparation of an electrode for quantitative detection of glucose.

[0016] Furthermore, the application is specifically:

[0017] (1) Grind the electrode until the surface is smooth;

[0018] (2) The electrode polished in step (1) is ultrasonically treated in anhydrous ethanol and deionized water, and then blown dry with nitrogen;

[0019] (3) PCE@ZnPAF 16 -b is dropped on the electrode surface, and the above steps are repeated after the electrode is dried to obtain GCE / PCE@ZnPAF 16 -b electrode;

[0020] (4) TOAB was dropped onto the electrode surface in step (3) and dried to obtain GCE / PCE@ZnPAF 16 -b / TOAB modified electrode;

[0021] (5) Soaking the modified electrode in step (4) in a streptavidin solution; incubating at room temperature for 1 hour, and then washing with phosphate buffer to obtain GCE / PCE@ZnPAF 16 -b / TOAB / SA modified electrode.

[0022] (6) The modified electrode in step (5) was immersed in a biotinylated glucose oxidase solution and incubated for 1 hour, and then rinsed again with phosphate buffer to obtain GCE / PCE@ZnPAF 16 -b / TOAB / SA / b-Gox modified electrode.

[0023] (7) Place the modified electrode in step (6) in a small gas hood filled with oxygen to obtain GCE / O 2 -PCE@ZnPAF 16 -b / TOAB / SA / b-Gox modified electrode, also known as self-enhanced electrochemiluminescence biosensor.

[0024] The beneficial effects of the present invention are as follows:

[0025] (1) The present invention constructs a porous structural framework with tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chains and carboxyl-polyethylene glycol-biotin, and then embeds perfluoro-15-crown-5 ether with high oxygen carrying capacity in the porous structure. By selecting fluorinated carbon chains of different lengths, a series of self-enhanced electrochemiluminescent composites with different pore sizes are prepared. The composite can fix gas on the electrode surface and has the characteristics of oxygen-rich, catalytic and adjustable function.

[0026] (2) After comparing a series of self-enhanced electrochemiluminescent complexes with different pore sizes, the self-enhanced electrochemiluminescent complex with the strongest ECL signal is selected, and streptavidin is used as an intermediate. Through the affinity between streptavidin and biotin, biotinylated glucose oxidase is immobilized on the surface of the self-enhanced electrochemiluminescent complex to obtain a self-enhanced electrochemiluminescent biosensor;

[0027] (3) The self-enhanced electrochemiluminescence biosensor was used to detect glucose. The constructed sensor had a wide linear detection range of 0.1 mM to 10 mM for glucose and high sensitivity, with a minimum detection limit of 62 μM. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 For GCE / O 2 -PCE@ZnPAFn-b / TOAB electrode ECL signal intensity comparison diagram and ECL-time curve diagram, where (a) is GCE / O 2 -PCE@ZnPAFn-b / TOAB electrode ECL signal intensity comparison diagram, Figure (b) is GCE / O 2 -ECL-time curve of PCE@ZnPAFn-b / TOAB electrode;

[0029] Figure 2 The specific process for preparing the self-enhanced electrochemiluminescence biosensor;

[0030] Figure 3 This is the electrochemical impedance spectroscopy diagram during the assembly process of the self-enhanced electrochemiluminescence biosensor;

[0031] Figure 4 ECL-concentration graphs and linear curves obtained for the self-enhanced electrochemiluminescence biosensor to detect different concentrations of glucose, wherein (a) is the ECL-concentration graph and (b) is the linear curve;

[0032] Figure 5 This is a graph showing the experimental results of the interference of the self-enhanced electrochemiluminescence biosensor with ascorbic acid, uric acid, cysteine, fructose, sucrose and citric acid;

[0033] Figure 6 It is a test table for glucose in serum samples. DETAILED DESCRIPTION

[0034] Exemplary embodiments will be described in detail herein, examples of which are shown in the accompanying drawings. When the following description refers to the drawings, unless otherwise indicated, the same numbers in different drawings represent the same or similar elements. The embodiments described in the following exemplary embodiments do not represent all embodiments consistent with the present invention. Instead, they are merely examples of devices and methods consistent with some aspects of the present invention as detailed in the appended claims.

[0035] The present invention is described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the features of the following embodiments and implementations can be combined with each other.

[0036] A self-enhanced electrochemiluminescent composite of the present invention is obtained by the following preparation method:

[0037] (1) first weighing tetrahydroxyphenylporphyrin and zinc acetate, dissolving them in dimethylformamide, and shaking until they are uniformly mixed, wherein the molar ratio of the tetrahydroxyphenylporphyrin to the zinc acetate is 1:5-9; then heating in an oil bath to 110-120° C., and refluxing for 45-60 minutes; cooling to room temperature, pouring deionized water, and allowing to stand, centrifuging to obtain a precipitate, and drying the precipitate to obtain tetrahydroxyphenyl zinc porphyrin;

[0038] (2) dissolving the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine obtained in step (1) in tetrahydrofuran, wherein the molar ratio of the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine is 1:1.5:20:20, heating to 40-50° C. in the dark and stirring until the mixture is uniformly mixed, and the reaction time is 12-18 hours; then adding carboxyl-polyethylene glycol-biotin, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine, wherein the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine are mixed, and the mixture is stirred for 12-18 hours. Hydroxyphenyl zinc porphyrin, carboxyl-polyethylene glycol-biotin, N,N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine are reacted in a molar ratio of 1:4:10:10 at 40-50°C in the dark for 18-20 hours; then, after evaporation and concentration to obtain a solid substance, the solid substance is first dissolved with methanol and then precipitated with ice ether, and the precipitate is repeatedly dissolved until the supernatant is colorless; then, the precipitate is dialyzed to remove impurities, and finally, it is freeze-dried to obtain a biotinylated zinc perfluoro aromatic framework and stored in the dark at 2-8°C for standby use; the biotinylated zinc perfluoro aromatic framework is labeled as ZnPAFn-b;

[0039] (3) Dissolving the ZnPAFn-b obtained in step (2) in deionized water, adding perfluoro-15-crown-5 ether, wherein the molar ratio of ZnPAFn-b to perfluoro-15-crown-5 ether is 1:64; then ultrasonicating in a water bath, centrifuging, collecting the upper layer liquid, and obtaining a self-enhanced electrochemiluminescent complex, labeled as PCE@ZnPAFn-b.

[0040] In some embodiments, the fluorinated carbon chain is perfluorosuccinic acid, perfluoroglutaric acid, perfluoroadipic acid, perfluorosuberic acid, perfluoroazelaic acid, or perfluorosebacic acid; preferably perfluorosebacic acid.

[0041] Where n in ZnPAFn-b and PCE@ZnPAFn-b is the number of fluorine atoms;

[0042] If the fluorinated carbon chain is perfluorosuccinic acid, then n = 4, and PCE@ZnPAF is prepared. 4 -b;

[0043] If the fluorinated carbon chain is perfluoroglutaric acid, then n = 6, and PCE@ZnPAF is prepared. 6 -b;

[0044] If the fluorinated carbon chain is perfluoroadipic acid, then n = 8, and PCE@ZnPAF is prepared. 8 -b;

[0045] If the fluorinated carbon chain is perfluorooctanedioic acid, then n = 12, and PCE@ZnPAF is prepared. 12 -b;

[0046] If the fluorinated carbon chain is perfluoroazelaic acid, then n = 14, and PCE@ZnPAF is prepared. 14 -b;

[0047] If the fluorinated carbon chain is perfluorosebacic acid, then n = 16, and PCE@ZnPAF is prepared. 16 -b.

[0048] Example 1: GCE / O 2 Preparation of -PCE@ZnPAFn-b / TOAB electrode

[0049] (1) The glassy carbon electrode (GCE) was polished with a 0.05 μm alumina suspension to obtain a smooth mirror surface. The electrode was then ultrasonically treated in anhydrous ethanol and deionized water, and then dried with nitrogen.

[0050] (2) Take 20 μL of 1 mg / mL PCE@ZnPAFn-b (n=4, 6, 8, 12, 14, 16) solution and drop it on the surface of the pretreated glassy carbon electrode. After the electrode is dried, repeat the above steps to obtain a modified electrode called GCE / PCE@ZnPAFn-b electrode;

[0051] (3) 10 μL of 25 mM tetraoctylammonium bromide (TOAB) was dropped onto the electrode surface obtained in step (2). After drying, the modified electrode obtained was called GCE / PCE@ZnPAFn-b / TOAB electrode.

[0052] (4) Place the GCE / PCE@ZnPAFn / TOAB electrode in a self-made small gas hood. The inlet of the small gas hood is connected to an oxygen tank, and the outlet covers the electrode to provide oxygen (O 2 ) environment, so that the electrode is oxygenated and the oxygen is fixed on the electrode surface, marked as GCE / O 2 -PCE@ZnPAFn-b / TOAB electrode.

[0053] The preparation method of Example 1 was used to obtain GCE / O 2 -PCE@ZnPAF4 -b / TOAB electrode, GCE / O 2 -PCE@ZnPAF 6 -b / TOAB electrode, GCE / O 2 -PCE@ZnPAF 8 -b / TOAB electrode, GCE / O 2 -PCE@ZnPAF 12 -b / TOAB electrode, GCE / O 2 -PCE@ZnPAF 14 -b / TOAB electrode, GCE / O 2 -PCE@ZnPAF 16 -b / TOAB electrode.

[0054] Example 2: ECL signal detection

[0055] The GCE / O 2 -PCE@ZnPAFn-b / TOAB (n=4, 6, 8, 12, 14, 16) electrode was used as the working electrode, platinum wire electrode was used as the auxiliary electrode, and Ag / AgCl (saturated KCl) electrode was used as the reference electrode; the parameters of the electrochemiluminescence analysis system were set as follows: the amplification level was 3, a potential of -2 to 0 V was applied to the working electrode, the photomultiplier tube bias voltage was -600 V, and the scanning rate was 0.3 V / s; the ECL buffer used in the experiment was air-saturated pH 7.4, 10 mM Tris (hydroxymethyl) aminomethane (Tris) buffer (containing 0.3 M potassium chloride); GCE / O were recorded at room temperature. 2 -ECL signal comparison and ECL-time diagram of PCE@ZnPAFn-b / TOAB (n=4, 6, 8, 12, 14, 16) electrodes.

[0056] like Figure 1 As shown, Figure 1 (a) is GCE / O 2 -PCE@ZnPAFn-b / TOAB (n=4, 6, 8, 12, 14, 16) electrode ECL signal comparison diagram, specific test results show that GCE / O 2 The ECL intensity of the -PCE@ZnPAFn-b / TOAB electrode increases with the increase of n, i.e., I ECL (ZnPAF 4 -b) ECL (ZnPAF 6 -b) ECL (ZnPAF 8 -b) ECL ​​​(ZnPAF 12 -b) ECL (ZnPAF 14 -b) ECL (ZnPAF 16 -b), where I ECL (ZnPAF 4 -b) indicates ZnPAF 4 -b electrochemiluminescence intensity, I ECL (ZnPAF 6 -b) indicates ZnPAF 6 -b electrochemiluminescence intensity, I ECL (ZnPAF 8 -b) indicates ZnPAF 8 -b electrochemiluminescence intensity, I ECL (ZnPAF 12 -b) indicates ZnPAF 12 -b electrochemiluminescence intensity, I ECL (ZnPAF 14 -b) indicates ZnPAF 14 -b electrochemiluminescence intensity, I ECL (ZnPAF 16 -b) indicates ZnPAF 16 -b electrochemiluminescence intensity; Figure 1 (b) is GCE / O 2 -The ECL-time diagram of PCE@ZnPAFn-b / TOAB (n=4, 6, 8, 12, 14, 16) electrode. The specific test results show that during the continuous 10-cycle scanning process, its ECL luminescence intensity shows excellent stability.

[0057] As can be seen from Example 2, GCE / O 2 -PCE@ZnPAF 16 -b / TOAB electrode has the largest ECL intensity, so PCE@ZnPAF is used in Example 3 16 -b Preparation of self-enhanced electrochemiluminescence biosensor.

[0058] Example 3: Preparation of self-enhanced electrochemiluminescence biosensor

[0059] (1) The glassy carbon electrode (GCE) was polished with a 0.05 μm alumina suspension to obtain a smooth mirror surface. The electrode was then ultrasonically treated in anhydrous ethanol and deionized water, and then dried with nitrogen.

[0060] (2) Add 20uL 1mg / mL PCE@ZnPAF 16 ​​-b solution was dropped onto the surface of the pretreated glassy carbon electrode, and the above steps were repeated after the electrode was dried. The resulting modified electrode was called GCE / PCE@ZnPAF 16 -b electrode;

[0061] (3) 10 μL of 25 mM tetraoctylammonium bromide (TOAB) was added dropwise to the electrode surface in step (2). After drying, the modified electrode obtained was called GCE / PCE@ZnPAF. 16 -b / TOAB modified electrode;

[0062] (4) The electrode in step (3) was immersed in a 1 mg / mL streptavidin (SA) solution. After incubation at room temperature for 1 hour, it was rinsed with pH = 7.4, 10 mM phosphate buffer to remove unbound SA. The resulting modified electrode was called GCE / PCE@ZnPAF 16 -b / TOAB / SA electrode;

[0063] (5) The electrode in step (4) was immersed in a 4 mg / mL biotinylated glucose oxidase (b-GOx) solution and incubated for 1 hour, and then rinsed again with pH = 7.4, 10 mM phosphate buffer to obtain a modified electrode called GCE / PCE@ZnPAF 16 -b / TOAB / SA / b-Gox electrode;

[0064] (6) Place the electrode in step (5) in a small gas hood filled with oxygen to obtain oxygen (O 2 ) is fixed on the electrode surface, and the modified electrode obtained is called GCE / O 2 -PCE@ZnPAF 16 -b / TOAB / SA / b-Gox electrode, also known as self-enhanced electrochemiluminescence biosensor.

[0065] The biotinylated glucose oxidase (b-GOx) is formed by linking biotin N-hydroxysuccinimide ester to glucose oxidase.

[0066] The specific process of preparing the self-enhanced electrochemiluminescence biosensor is as follows Figure 2 shown.

[0067] Electrochemical impedance spectroscopy (EIS) is often used to characterize interface changes during electrode modification. Figure 3 Indicates the impedance change during the electrode modification process. Figure 3 It can be seen that compared with the bare electrode, PCE@ZnPAF 16-b modified electrode exhibits a large impedance, indicating that PCE@ZnPAF 16 -b coverage hinders electron transfer at the electrode / electrolyte interface. In order to make the electrode more stable, after modification with TOAB, the impedance value increased sharply, indicating that TOAB hinders the transfer of electrons from the redox probes of potassium ferrocyanide and potassium ferrocyanide to the electrode surface. Subsequently, SA and b-GOx were modified on the electrode layer by layer, and the diameter of the semicircular arc on the impedance graph increased layer by layer, indicating that the impedance value also gradually increased, which was attributed to the insulating properties of the protein molecule. Finally, after the modified electrode was oxygenated, the impedance value decreased significantly. It shows that the glucose biosensor can effectively improve the electron transfer capacity of the modified electrode after carrying oxygen. From the impedance change, it can be seen that the assembly process of the self-enhanced electrochemiluminescence biosensor is successful.

[0068] Example 4: Glucose Detection

[0069] (1) A self-enhanced electrochemiluminescence biosensor was used as the working electrode, a platinum wire electrode was used as the auxiliary electrode, and an Ag / AgCl (saturated KCl) electrode was used as the reference electrode;

[0070] (2) Setting the parameters of the electrochemiluminescence analysis system to 3 amplification levels, applying a potential of -2 to 0 V on the working electrode, a photomultiplier tube bias voltage of -800 V, and a scan rate of 0.3 V / s;

[0071] (3) The ECL buffer used in the experiment was air-saturated pH 7.4, 10 mM Tris buffer (containing 0.3 M potassium chloride);

[0072] (4) Add different concentrations of glucose to the ECL buffer so that the concentration gradient of the substance is 0-12 mM, and then measure at room temperature.

[0073] like Figure 4 As shown, Figure 4 (a) is the ECL-concentration diagram obtained by detecting glucose. The ECL signal intensity of the self-enhanced electrochemiluminescence biosensor decreases with the increase of glucose concentration. This is because the immobilized glucose oxidase competitively consumes oxygen in the process of catalyzing glucose, resulting in a decrease in the production of singlet oxygen, thereby weakening the ECL light intensity. Figure 4 (b) is a linear curve obtained by detecting glucose. In the range of 0.1mM-10mM, the decrease of the ECL signal of the self-enhanced electrochemiluminescence biosensor shows a good linear relationship with the concentration of glucose, and the concentration of glucose can be quantitatively detected. The linear equation is: ECL =-626.06C glu +9223.52, the correlation coefficient is R 2=0.991, its linear detection range is 0.1mM-10mM, and the detection limit reaches 62μM, indicating that the ECL electrochemical biosensor can achieve wide linearity and high sensitivity detection of glucose.

[0074] The linear equation obtained above is obtained through fitting, that is, after the software inputs the data points, it selects the linear fitting curve to obtain the linear equation; the correlation coefficient R 2 It is the relative deviation of each original data point from the fitting curve, and also indicates the credibility of the fitting curve; I ECL The ECL signal of the self-enhanced electrochemiluminescence biosensor in glucose solutions with different concentrations; C glu is the concentration of glucose.

[0075] The detection range of 0.1mM-10mM has many practical applications in industry and life. For example, the glucose level in normal human blood is between 4.4 and 6.6mmol·L -1 Within the detection range of 0.1mM-10mM, the glucose level in human blood can be detected.

[0076] Example 5: Anti-interference

[0077] A 4.5 mM glucose standard solution was prepared, and 0.1 mM ascorbic acid, uric acid, cysteine, fructose, sucrose and citric acid were added as interference substances of grapes. The difference between this embodiment and embodiment 4 is that a 4.5 mM glucose standard solution was selected in step (4) for interference detection. The detection results are shown in FIG. Figure 5 As shown, the interfering substances have little effect on the ECL signal of the sensor detecting glucose, indicating that the sensor has good anti-interference ability to glucose.

[0078] The sensor has good anti-interference properties to glucose and can be used in clinical diagnosis, biotechnology and food industry.

[0079] Example 6: Determination of Glucose in Serum Samples

[0080] In order to determine the practicality of the prepared self-enhanced electrochemiluminescence biosensor, several glucose solutions with different concentrations were measured using the developed biosensor and the standard addition method. The difference between this example and Example 4 is that different concentrations of glucose were selected as the test samples in step (4). The specific test results are shown in Figure 6 The recovery rates ranged from 94.04% to 102.97%, indicating that the proposed biosensor has a good recovery rate. These results confirm that the self-enhanced electrochemiluminescence biosensor has practical application value.

[0081] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

[0082] The above embodiments are only used to illustrate the design ideas and features of the present invention, and their purpose is to enable those skilled in the art to understand the content of the present invention and implement it accordingly. The protection scope of the present invention is not limited to the above embodiments. Therefore, any equivalent changes or modifications made based on the principles and design ideas disclosed by the present invention are within the protection scope of the present invention.

[0083] Those skilled in the art will readily appreciate other embodiments of the present application after considering the description and practicing the contents disclosed herein. The present application is intended to cover any variations, uses or adaptations of the present application, which follow the general principles of the present application and include common knowledge or customary technical means in the art that are not disclosed in the present application. The description and examples are intended to be exemplary only.

[0084] It should be understood that the present application is not limited to the exact construction that has been described above and shown in the drawings, and that various modifications and changes may be made without departing from the scope thereof.

Claims

1. A self-enhanced electrochemiluminescent composite, characterized in that: It is obtained by the following preparation method: (1) Weigh tetrahydroxyphenylporphyrin and zinc acetate, dissolve them in dimethylformamide, and shake until they are uniformly mixed, wherein the molar ratio of tetrahydroxyphenylporphyrin to zinc acetate is 1:5-9; then heat in an oil bath to 110-120° C., reflux for 45-60 minutes; cool to room temperature, pour in deionized water, let stand, centrifuge to obtain a precipitate, and dry the precipitate to obtain tetrahydroxyphenyl zinc porphyrin; (2) dissolving the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N, N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine obtained in step (1) in tetrahydrofuran, wherein the molar ratio of the tetrahydroxyphenyl zinc porphyrin, fluorinated carbon chain, N, N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine is 1:1.5:20:20, heating to 40-50° C. in the dark and stirring until the mixture is uniformly mixed, and the reaction time is 12-18 hours; then adding carboxyl-polyethylene glycol-biotin, N, N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine, wherein the molar ratio of the tetrahydroxyphenyl zinc porphyrin, carboxyl-polyethylene glycol-biotin, N, N'-dicyclohexylcarbodiimide and 4-dimethylaminopyridine is 1:4:10:10, and heating at 40-50° C. The reaction was carried out under dark conditions for 18 to 20 hours; then, after evaporation and concentration, a solid substance was obtained, which was first dissolved with methanol and then precipitated with ice ether, and the precipitate was repeatedly dissolved until the supernatant was colorless; then, the precipitate was dialyzed to remove impurities, and finally, it was freeze-dried to obtain a biotinylated zinc perfluoroaromatic framework and stored in the dark at 2 to 8°C for future use; the biotinylated zinc perfluoroaromatic framework was labeled as ZnPAFn-b; (3) dissolving the ZnPAFn-b obtained in step (2) in deionized water, adding perfluoro-15-crown-5 ether, wherein the molar ratio of ZnPAFn-b to perfluoro-15-crown-5 ether is 1:64; then ultrasonicating in a water bath, centrifuging, collecting the upper layer liquid, and obtaining a self-enhanced electrochemiluminescent complex, labeled as PCE@ZnPAFn-b; The fluorinated carbon chain is perfluorosuccinic acid, perfluoroglutaric acid, perfluoroadipic acid, perfluorooctanedioic acid, perfluoroazelaic acid or perfluorodecanedioic acid, and n in ZnPAFn-b and PCE@ZnPAFn-b is 4, 6, 8, 12, 14 or 16 respectively; n is the number of fluorine atoms.

2. A self-enhanced electrochemiluminescent composite according to claim 1, characterized in that: The fluorinated carbon chain is perfluorosebacic acid.

3. A self-enhanced electrochemiluminescent composite according to claim 1, characterized in that: The molecular weight cut-off of the dialysis is greater than or equal to 2000Da.

4. Use of a self-enhanced electrochemiluminescent composite according to any one of claims 1 to 3 in preparing an electrode for quantitative detection of glucose.

5. The use according to claim 4, characterized in that: The application is specifically: (1) Grind the electrode until the surface is smooth; (2) The electrode polished in step (1) is ultrasonically treated in anhydrous ethanol and deionized water, and then blown dry with nitrogen; (3) PCE@ZnPAF 16 -b is dropped on the electrode surface, and the above steps are repeated after the electrode is dried to obtain GCE / PCE@ZnPAF 16 -b electrode; (4) Drop TOAB on the electrode surface in step (3) and dry it to obtain GCE / PCE@ZnPAF 16 -b / TOAB modified electrode; (5) The modified electrode in step (4) was immersed in a streptavidin solution; after incubation at room temperature for 1 hour, it was rinsed with phosphate buffer to obtain GCE / PCE@ZnPAF 16 -b / TOAB / SA modified electrode; (6) The modified electrode in step (5) was immersed in a biotinylated glucose oxidase solution and incubated for 1 hour, and then rinsed again with phosphate buffer to obtain GCE / PCE@ZnPAF 16 -b / TOAB / SA / b-Gox modified electrode; (7) Place the modified electrode in step (6) in a small gas hood filled with oxygen to obtain GCE / O2-PCE@ZnPAF 16 -b / TOAB / SA / b-Gox modified electrode, also known as self-enhanced electrochemiluminescence biosensor.

Citation Information

Patent Citations

  • Dissociable nanoparticles with inter alia transition-metal complex catalysts

    US20190091673A1