Stress corrosion and fatigue long-life monitoring method and device for nuclear power steam turbine

By obtaining and analyzing the stress and material data of the monitoring components of nuclear power turbines and calculating the long-life monitoring data of stress corrosion and fatigue cracks, the problem of stress corrosion in nuclear power turbines is solved, and effective safety of crack growth life of nuclear power turbines is achieved Sex monitoring ensures the long life and safe operation of the equipment.

CN116776588BActive Publication Date: 2024-11-22SHANGHAI POWER EQUIPMENT RESEARCH INSTITUTE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310716803.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-06-15
Publication Date
2024-11-22
Estimated Expiration
2043-06-15

AI Technical Summary

Technical Problem

Nuclear power turbines do not consider stress corrosion in the crack growth life safety monitoring, resulting in insufficient operating safety.

Method used

By obtaining the stress calculation basic data of nuclear power turbine monitoring components and material test basic data, long-life monitoring data for stress corrosion and fatigue cracks, including low- and high-period fatigue crack propagation life, based on these data, determine the crack propagation calendar life, and Carry out security monitoring.

Benefits of technology

Taking into account the impact of stress corrosion and fatigue on the life of monitoring components, we ensure the long life and safe operation of nuclear power turbines, and improve the safety monitoring capability of crack growth life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116776588B_ABST
    Figure CN116776588B_ABST
Patent Text Reader

Abstract

The present disclosure provides a method and device for long-life monitoring of stress corrosion and fatigue of a nuclear power steam turbine. The method includes: obtaining stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtaining the long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life; based on the long-life monitoring data required by the monitoring component, obtaining the crack growth calendar life of the monitoring component, and based on the crack growth calendar life, performing crack growth life safety monitoring on the monitoring component. Thus, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the technical field of nuclear power steam turbines, and in particular to a method, device, electronic equipment, storage medium and platform for long-life monitoring of stress corrosion and fatigue of nuclear power steam turbines. Background Art

[0002] At present, with the aggravation of energy shortage, people are in urgent need of developing new energy to meet people's energy needs. Nuclear power is a clean energy, with no carbon dioxide emissions and little environmental impact; nuclear power is an efficient energy with high energy density and low resource consumption; nuclear power is a stable energy without intermittency, long utilization hours and stable power supply capacity; nuclear power is a safe energy with low possibility of accidents, and is an important option to enhance energy security. Nuclear power turbines are important equipment in nuclear power technology. In related technologies, crack propagation life safety monitoring of nuclear power turbines is required to ensure the normal operation of nuclear power turbines. However, the crack propagation life safety monitoring of nuclear power turbines does not take stress corrosion into consideration. Summary of the invention

[0003] The present disclosure aims to solve one of the technical problems in the above-mentioned technologies at least to some extent.

[0004] To this end, the first objective of the present disclosure is to provide a stress corrosion and fatigue long-life monitoring method for a nuclear power steam turbine.

[0005] The second objective of the present disclosure is to provide a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine.

[0006] A third objective of the present disclosure is to provide an electronic device.

[0007] A fourth objective of the present disclosure is to provide a computer-readable storage medium.

[0008] The fifth objective of the present disclosure is to provide a monitoring platform suitable for nuclear power steam turbines.

[0009] The first aspect of the present disclosure provides a method for long-life monitoring of stress corrosion and fatigue of a nuclear power steam turbine, comprising: obtaining stress calculation basic data and material test basic data of a monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtaining long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life; based on the long-life monitoring data required by the monitoring component, obtaining the crack growth calendar life of the monitoring component, and based on the crack growth calendar life, performing crack growth life safety monitoring on the monitoring component.

[0010] The second aspect embodiment of the present disclosure proposes a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine, comprising: an acquisition module, used to acquire stress calculation basic data and material test basic data of a monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, acquire long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life; a monitoring module, used to obtain the crack growth calendar life of the monitoring component based on the long-life monitoring data required by the monitoring component, and based on the crack growth calendar life, perform crack growth life safety monitoring on the monitoring component.

[0011] The third aspect embodiment of the present disclosure proposes an electronic device, comprising: a memory, a processor, and a computer program stored in the memory and executable on the processor. When the processor executes the program, the stress corrosion and fatigue long-life monitoring method for a nuclear power steam turbine as described in the first aspect embodiment of the present disclosure is implemented.

[0012] The fourth aspect of the present application provides a computer-readable storage medium having a computer program stored thereon. When the program is executed by a processor, the method for long-life monitoring of stress corrosion and fatigue of a nuclear power steam turbine as described in the first aspect of the present disclosure is implemented.

[0013] The fifth aspect embodiment of the present application proposes a monitoring platform suitable for a nuclear power steam turbine, including a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine as described in the second aspect embodiment of the present disclosure; or an electronic device as described in the third aspect embodiment of the present disclosure; or a computer-readable storage medium as described in the fourth aspect embodiment of the present disclosure.

[0014] The technical solution provided by the embodiment of the present disclosure brings at least the following beneficial effects: obtaining the stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtaining the long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life, based on the long-life monitoring data required by the monitoring component, obtaining the crack growth calendar life of the monitoring component, and based on the crack growth calendar life, performing crack growth life safety monitoring on the monitoring component. Thus, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.

[0015] It is to be understood that the foregoing general description and the following detailed description are exemplary and explanatory only and are not restrictive of the present disclosure. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The above and / or additional aspects and advantages of the present disclosure will become apparent and easily understood from the following description of the embodiments in conjunction with the accompanying drawings, in which:

[0017] Figure 1 A schematic flow chart of a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to an embodiment of the present disclosure;

[0018] Figure 2 It is a flow chart of a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to another embodiment of the present disclosure;

[0019] Figure 3 A schematic diagram of a process for obtaining stress corrosion crack growth life in a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to an embodiment of the present disclosure;

[0020] Figure 4 A schematic diagram of a process for obtaining stress corrosion crack growth life in a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to another embodiment of the present disclosure;

[0021] Figure 5 A schematic diagram of a process for obtaining low-cycle fatigue crack growth life in a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to an embodiment of the present disclosure;

[0022] Figure 6 A schematic diagram of a process for obtaining low-cycle fatigue crack growth life in a stress corrosion and fatigue long-life monitoring method for a nuclear power steam turbine according to another embodiment of the present disclosure;

[0023] Figure 7 A schematic diagram of a process for obtaining high cycle fatigue crack growth life in a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to an embodiment of the present disclosure;

[0024] Figure 8 It is a flow chart of a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to another embodiment of the present disclosure;

[0025] Fig. 9 It is a flow chart of a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to another embodiment of the present disclosure;

[0026] Fig.10It is a structural schematic diagram of a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine according to an embodiment of the present disclosure;

[0027] Fig.11 The figure is a schematic diagram of the structure of an electronic device according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0028] Embodiments of the present disclosure are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present disclosure, and should not be construed as limiting the present disclosure.

[0029] The following describes the stress corrosion and fatigue long-life monitoring method, device, electronic equipment, storage medium and platform for nuclear power steam turbines according to the embodiments of the present disclosure in conjunction with the accompanying drawings.

[0030] Figure 1 The present invention is a flow chart of a method for monitoring the stress corrosion and fatigue of a nuclear power steam turbine for a long life according to an embodiment of the present invention.

[0031] like Figure 1 As shown, the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to an embodiment of the present disclosure includes:

[0032] S101, obtaining stress calculation basic data and material test basic data of monitoring components of a nuclear power steam turbine.

[0033] It should be noted that the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to the embodiment of the present disclosure can be executed by the stress corrosion and fatigue long-life monitoring device of a nuclear power steam turbine according to the embodiment of the present disclosure, and the stress corrosion and fatigue long-life monitoring device of a nuclear power steam turbine according to the embodiment of the present disclosure can be configured in any monitoring platform suitable for a nuclear power steam turbine to execute the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to the embodiment of the present disclosure.

[0034] It should be noted that there are no excessive restrictions on the basic data for stress calculation and the basic data for material testing.

[0035] The following takes the rotor as an example of the monitored component to describe the basic data for stress calculation and material testing of the rotor.

[0036] For example, the basic data for stress calculation include the maximum stress σ at the rotor crack site maxH , the maximum stress σ at the rotor crack site under normal shutdown transient conditions maxn , Maximum stress σ at the rotor crack site under transient conditions of 110% overspeed test max110%, Maximum stress σ at the rotor crack site under 120% overspeed transient condition max120% wait.

[0037] For example, the basic test data of rotor materials include the fracture toughness K of the rotor material. IC , Stress corrosion fracture toughness K of rotor material ISCC , annual average stress corrosion crack growth rate test value Crack shape parameter Q, high cycle fatigue crack growth threshold of rotor material Test values, etc.

[0038] The following takes the cylinder as an example of the monitored component to describe the basic data of stress calculation and material testing of the cylinder.

[0039] For example, the basic data for stress calculation include the maximum stress σ at the cylinder crack site of a nuclear power steam turbine under steady-state load operation. max0 , the maximum stress σ at the cylinder crack position of nuclear power steam turbine during cold start transient condition maxc , the maximum stress σ at the cylinder crack position of nuclear power steam turbine during warm start transient condition maxw , the maximum stress σ at the cylinder crack position of nuclear power steam turbine hot start transient condition maxh wait.

[0040] For example, the basic data of material testing includes the fracture toughness K of the cylinder material. IC , stress corrosion fracture toughness K of cylinder material ISCC , annual average stress corrosion crack growth rate test value Crack shape parameters Q, etc.

[0041] In one embodiment, basic data for stress calculation and basic data for material testing of monitoring components of a nuclear power steam turbine are obtained, including obtaining a mapping relationship among the basic data for stress calculation, basic data for material testing and monitoring components, and based on the mapping relationship, obtaining basic data for stress calculation and basic data for material testing of the monitoring components.

[0042] In one embodiment, obtaining stress calculation basic data and material test basic data of a monitoring component of a nuclear power steam turbine includes performing stress calculation on the monitoring component to obtain stress calculation basic data, and performing material testing on the monitoring component to obtain material test basic data. It should be noted that stress calculation can be implemented using any stress calculation method in the relevant technology, and material testing can be implemented using any material testing method in the relevant technology, and no further limitations are given here.

[0043] S102, based on the stress calculation basic data and the material experiment basic data, obtaining the long-life monitoring data required for the monitoring component, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life.

[0044] It should be noted that the stress corrosion crack growth life refers to the crack growth life of the monitored component when the damage type to which the monitored component is subjected includes stress corrosion; the low-cycle fatigue crack growth life refers to the crack growth life of the monitored component when the damage type to which the monitored component is subjected includes low-cycle fatigue; and the high-cycle fatigue crack growth life refers to the crack growth life of the monitored component when the damage type to which the monitored component is subjected includes high-cycle fatigue.

[0045] In one embodiment, the method further includes, if the monitored component is a rotor, determining that the long-life monitoring data required for the rotor includes stress corrosion crack growth life, low cycle fatigue crack growth life, and high cycle fatigue crack growth life; if the monitored component is a cylinder, determining that the long-life monitoring data required for the cylinder includes stress corrosion crack growth life and low cycle fatigue crack growth life.

[0046] In one embodiment, based on the stress calculation basic data and the material experiment basic data, obtaining the long-life monitoring data required for the monitoring component includes inputting the stress calculation basic data and the material experiment basic data into a setting model, and the setting model outputs the long-life monitoring data required for the monitoring component. It should be noted that there is no excessive limitation on the setting model, for example, it may include a deep learning model.

[0047] S103, obtaining the crack growth calendar life of the monitored component based on the long-life monitoring data required by the monitored component.

[0048] In one embodiment, the crack growth calendar life of the monitored component is obtained based on the long-life monitoring data required for the monitored component, including if the monitored component is a rotor, the crack growth calendar life of the rotor is obtained based on the stress corrosion crack growth life, low cycle fatigue crack growth life and high cycle fatigue crack growth life of the rotor.

[0049] In one embodiment, the crack growth calendar life of the monitored component is obtained based on the long-life monitoring data required for the monitored component, including if the monitored component is a cylinder, the crack growth calendar life of the cylinder is obtained based on the stress corrosion crack growth life and low cycle fatigue crack growth life of the cylinder.

[0050] In one embodiment, based on the long-life monitoring data required by the monitoring component, the crack growth calendar life of the monitoring component is obtained, including inputting the long-life monitoring data required by the monitoring component into a setting model, and the setting model outputs the crack growth calendar life of the monitoring component. It should be noted that there is no excessive limitation on the setting model, for example, it may include a deep learning model.

[0051] S104, based on the crack growth calendar life, performing crack growth life safety monitoring on the monitoring component.

[0052] In one embodiment, crack growth life safety monitoring is performed on a monitoring component based on the crack growth calendar life, including if the nuclear power steam turbine is in the design stage, obtaining a crack growth life safety monitoring criterion value of the monitoring component, if the crack growth calendar life is less than the crack growth life safety monitoring criterion value, judging that the crack growth calendar life does not meet the monitoring qualification conditions, so as to perform crack growth life safety monitoring on the monitoring component, or, if the crack growth calendar life is greater than or equal to the crack growth life safety monitoring criterion value, judging that the crack growth calendar life meets the monitoring qualification conditions, so as to perform crack growth life safety monitoring on the monitoring component.

[0053] In some examples, a mapping relationship between the model of a monitoring component and a crack propagation life safety monitoring criterion value can be established in advance to obtain the crack propagation life safety monitoring criterion value of the monitoring component, including querying the crack propagation life safety monitoring criterion value in the above mapping relationship based on the model of the monitoring component, and determining the queried crack propagation life safety monitoring criterion value as the crack propagation life safety monitoring criterion value of the monitoring component.

[0054] In one embodiment, if the crack propagation calendar life does not meet the monitoring qualification conditions, it also includes generating indication information for indicating that a safety abnormality has occurred in the monitoring component, which requires optimization and improvement in the design stage.

[0055] In summary, according to the stress corrosion and fatigue long-life monitoring method of the nuclear power steam turbine of the embodiment of the present disclosure, the stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine are obtained, and based on the stress calculation basic data and the material test basic data, the long-life monitoring data required by the monitoring component is obtained, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life. Based on the long-life monitoring data required by the monitoring component, the crack growth calendar life of the monitoring component is obtained, and based on the crack growth calendar life, the crack growth life safety monitoring of the monitoring component is performed. Therefore, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.

[0056] Figure 2 The figure is a flow chart of a method for monitoring stress corrosion and fatigue long life of a nuclear power steam turbine according to another embodiment of the present disclosure.

[0057] like Figure 2 As shown, the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to an embodiment of the present disclosure includes:

[0058] S201, obtaining stress calculation basic data and material test basic data of monitoring components of a nuclear power steam turbine.

[0059] For the relevant contents of step S201, please refer to the above embodiment, which will not be described again here.

[0060] S202, determining a set of crack extension dimensions of the monitored component based on stress calculation basic data and material experiment basic data.

[0061] It should be noted that there are no excessive restrictions on the crack extension size set.

[0062] In one implementation, based on stress calculation basic data and material experiment basic data, a set of crack extension sizes of the monitoring component is determined, including the following possible implementations:

[0063] Method 1: Determine the stress corrosion crack extension size threshold of the monitored component based on the crack shape parameters of the monitored component, the stress corrosion fracture toughness of the material of the monitored component, and the maximum stress at the crack site of the monitored component under steady-state conditions of nuclear power steam turbine under load operation.

[0064] Method 2: Determine the low-cycle fatigue critical crack size of the monitoring component under the set operating condition of the nuclear power steam turbine based on the crack shape parameters of the monitoring component, the fracture toughness of the material of the monitoring component and the maximum stress at the crack site of the monitoring component under the set operating condition of the nuclear power steam turbine.

[0065] Method 3: Determine the high cycle fatigue crack extension size threshold of the monitored component based on the crack shape parameters of the monitored component, the test value of the high cycle fatigue crack extension threshold of the material of the monitored component, and the high cycle fatigue stress range of the crack location of the monitored component under steady-state conditions of nuclear power turbine under load operation.

[0066] Method 4: Determine the high cycle fatigue critical crack size of the monitoring component based on the crack shape parameters of the monitoring component, the fracture toughness of the material of the monitoring component, and the maximum stress at the crack site of the monitoring component under steady-state conditions of nuclear power steam turbine operation with load.

[0067] The following takes the rotor as an example of a monitored component to describe how to obtain a set of crack extension sizes of the rotor.

[0068] For example, the crack growth size set includes the stress corrosion crack growth size threshold a SCC , high cycle fatigue crack growth size threshold value a th , high cycle fatigue critical crack size a cH , Low cycle fatigue critical crack size a of the rotor of nuclear power steam turbine under normal shutdown transient condition cn 、Critical crack size of low cycle fatigue of rotor in transient condition of nuclear power steam turbine 110% overspeed test a c110% , Low cycle fatigue critical crack size a of the rotor of nuclear power steam turbine under transient condition of 120% overspeed operation c120% wait.

[0069] In one implementation, based on stress calculation basic data and material experiment basic data, a set of crack extension sizes of a rotor is determined, including the following possible implementations:

[0070] Method 1: Determine the threshold value of the rotor stress corrosion crack extension size based on the rotor crack shape parameters, the rotor material stress corrosion fracture toughness and the maximum stress at the rotor crack site under steady-state conditions of nuclear power steam turbine under load operation.

[0071] Method 2: Determine the high-cycle fatigue crack extension size threshold of the rotor based on the crack shape parameters of the rotor, the test value of the high-cycle fatigue crack extension threshold of the rotor material, and the high-cycle fatigue stress range of the rotor under steady-state conditions of load operation of the nuclear power steam turbine.

[0072] Method 3: Determine the high cycle fatigue critical crack size of the rotor based on the crack shape parameters of the rotor, the fracture toughness of the rotor material, and the maximum stress at the rotor crack site under steady-state conditions of nuclear power steam turbine operation with load.

[0073] Method 4: Based on the crack shape parameters of the rotor, the fracture toughness of the rotor material, and the maximum stress at the rotor crack site under the normal shutdown transient condition of the nuclear power steam turbine, the low-cycle fatigue critical crack size of the rotor under the normal shutdown transient condition of the nuclear power steam turbine is determined.

[0074] Method 5: Based on the crack shape parameters of the rotor, the fracture toughness of the rotor material, and the maximum stress at the rotor crack site under the transient operating condition of the nuclear power steam turbine 110% overspeed test, the low-cycle fatigue critical crack size of the rotor under the transient operating condition of the nuclear power steam turbine 110% overspeed test is determined.

[0075] Method 6: Based on the crack shape parameters of the rotor, the fracture toughness of the rotor material, and the maximum stress at the rotor crack site under the transient operating condition of 120% overspeed of the nuclear power steam turbine, the low-cycle fatigue critical crack size of the rotor under the transient operating condition of 120% overspeed of the nuclear power steam turbine is determined.

[0076] For example, for a certain type of 1200MW nuclear power steam turbine, the weak part of the weld life of the welded low-pressure rotor is the weld on the outer surface of the rotor. During the design stage of the nuclear power steam turbine, the basic data for stress calculation and material testing of the welded low-pressure rotor are shown in Tables 1 and 2 respectively.

[0077] Table 1 Basic data for stress calculation of welded low-pressure rotor

[0078]

[0079] Table 2 Basic data of material test for welded low-pressure rotor

[0080]

[0081]

[0082] The calculation process of the crack growth size set of the welded low-pressure rotor is as follows:

[0083]

[0084]

[0085]

[0086]

[0087]

[0088]

[0089] The following takes the cylinder as an example of a monitored component to describe how to obtain a set of crack extension sizes of the cylinder.

[0090] For example, the crack growth size set includes the stress corrosion crack growth size threshold a SCC , Low cycle fatigue critical crack size a of the cylinder of nuclear power steam turbine under transient cold start condition cc , Low cycle fatigue critical crack size a of cylinder of nuclear power steam turbine under transient condition of warm start cw , Low cycle fatigue critical crack size a of cylinder of nuclear power steam turbine under transient condition of hot start ch wait.

[0091] In one implementation, based on stress calculation basic data and material experiment basic data, a set of crack extension sizes is determined, including the following possible implementations:

[0092] Method 1: Determine the threshold value of the stress corrosion crack extension size of the cylinder based on the crack shape parameters of the cylinder, the stress corrosion fracture toughness of the cylinder material and the maximum stress at the cylinder crack site under steady-state conditions of nuclear power steam turbine under load operation.

[0093] Method 2: Based on the crack shape parameters of the cylinder, the fracture toughness of the cylinder material, and the maximum stress at the cylinder crack site under the transient operating conditions of the nuclear power steam turbine cold start, the low-cycle fatigue critical crack size of the cylinder under the transient operating conditions of the nuclear power steam turbine cold start is determined.

[0094] Method 3: Based on the crack shape parameters of the cylinder, the fracture toughness of the cylinder material, and the maximum stress at the cylinder crack site under the transient condition of warm start of the nuclear power steam turbine, the low-cycle fatigue critical crack size of the cylinder under the transient condition of warm start of the nuclear power steam turbine is determined.

[0095] Method 4 determines the low-cycle fatigue critical crack size of the cylinder under the transient condition of hot start of the nuclear power steam turbine based on the crack shape parameters of the cylinder, the fracture toughness of the cylinder material, and the maximum stress at the cylinder crack site under the transient condition of hot start of the nuclear power steam turbine.

[0096] For example, the inner cylinder of the low-pressure cylinder of a certain type of 1000MW nuclear power steam turbine is made of Q235B. It tends to suffer from stress corrosion cracking when the water vapor contains NaOH and seawater leaked from the condenser. The weak part of the low-pressure inner cylinder is the connection between the low-pressure inner cylinder and the second-stage steam extraction pipe. The radius of the structural transition fillet at the structural discontinuity of the second-stage steam extraction pipe and the low-pressure connection is 5mm. This part works in the transition zone between superheated steam and wet steam, near the saturated steam line (Wilson), and is prone to stress corrosion cracking. During the design stage of the nuclear power steam turbine, the basic data for stress calculation and material testing of the low-pressure inner cylinder are shown in Tables 3 and 4 respectively.

[0097] Table 3 Basic data for stress calculation of low pressure inner cylinder

[0098] Serial number project Data Value 1 <![CDATA[The maximum stress σ at the crack location of the cylinder under steady-state operation with load max0 / MPa]]> 283.855 2 <![CDATA[The maximum stress σ at the cylinder crack location under cold start transient conditions maxc / MPa]]> 331.770 3 <![CDATA[The maximum stress σ at the cylinder crack location under warm startup transient conditions maxw / MPa]]> 343.971 4 <![CDATA[The maximum stress σ at the cylinder crack location under the transient condition of hot start maxh / MPa]]> 300.304

[0099] Table 4 Basic data of material test for low pressure inner cylinder

[0100]

[0101] The calculation process of the crack growth size set of the low-pressure inner cylinder of a certain model of 1000MW nuclear power steam turbine is as follows:

[0102]

[0103]

[0104]

[0105]

[0106] S203, based on the crack extension size set, obtaining long-life monitoring data required for monitoring the component.

[0107] In one embodiment, obtaining long-life monitoring data required for monitoring a component based on a crack growth size set includes obtaining long-life monitoring data required for monitoring a component based on at least one crack growth size in the crack growth size set.

[0108] In one embodiment, based on a crack extension size set, obtaining a stress corrosion crack extension life includes obtaining at least one crack extension size that matches the stress corrosion crack extension life from the crack extension size set, and obtaining the stress corrosion crack extension life based on at least one crack extension size that matches the stress corrosion crack extension life.

[0109] It should be noted that, based on the crack growth size set, the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life can be obtained. The relevant content of obtaining the stress corrosion crack growth life based on the crack growth size set can be referred to, which will not be repeated here.

[0110] S204, obtaining the crack growth calendar life of the monitored component based on the long-life monitoring data required by the monitored component.

[0111] S205, based on the crack growth calendar life, performing crack growth life safety monitoring on the monitoring component.

[0112] For the relevant contents of steps S204-S205, please refer to the above embodiment and will not be repeated here.

[0113] In summary, according to the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to the embodiment of the present disclosure, the crack extension size set of the monitoring component is determined based on the stress calculation basic data and the material experiment basic data, and the long-life monitoring data required for the monitoring component is obtained based on the crack extension size set. Therefore, the crack extension size set of the monitoring component can be determined by comprehensively considering the stress calculation basic data and the material experiment basic data, and the long-life monitoring data required for the monitoring component can be obtained based on the crack extension size set.

[0114] On the basis of any of the above embodiments, based on the crack growth size set, the stress corrosion crack growth life is obtained, including the stress corrosion crack growth life based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low cycle fatigue critical crack size of the monitoring component of the set working condition of the nuclear power steam turbine. Therefore, the method can comprehensively consider the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low cycle fatigue critical crack size of the monitoring component of the set working condition of the nuclear power steam turbine to obtain the stress corrosion crack growth life.

[0115] In one embodiment, a stress corrosion crack growth life is obtained based on a stress corrosion crack growth size threshold value, an annual average stress corrosion crack growth rate test value of a material of a monitoring component, and a low cycle fatigue critical crack size of a monitoring component under set operating conditions of a nuclear power steam turbine, including obtaining multiple types of stress corrosion crack growth lives based on the stress corrosion crack growth size threshold value, an annual average stress corrosion crack growth rate test value of a material of a monitoring component, and a low cycle fatigue critical crack size of a monitoring component under set operating conditions of a nuclear power steam turbine, and determining a stress corrosion crack growth life based on multiple types of stress corrosion crack growth lives.

[0116] In some examples, determining the stress corrosion crack growth life based on multiple types of stress corrosion crack growth lives includes determining a minimum value among the multiple types of stress corrosion crack growth lives as the stress corrosion crack growth life.

[0117] The following takes the rotor as an example of a monitored component to describe how to obtain the stress corrosion crack growth life of the rotor.

[0118] Based on any of the above embodiments, Figure 3 As shown, the stress corrosion crack growth life of the rotor is obtained, including:

[0119] S301, obtaining basic stress calculation data and material test basic data of a nuclear power steam turbine rotor.

[0120] S302, determining a threshold value of a stress corrosion crack extension size of the rotor based on stress calculation basic data and material test basic data.

[0121] S303, based on the stress calculation basic data and the material test basic data, determine the low cycle fatigue critical crack size of the rotor of the nuclear power steam turbine in the normal shutdown transient condition.

[0122] For the relevant contents of steps S301 - S303 , please refer to the above embodiment and will not be described again here.

[0123] S304, based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the rotor material, and the low-cycle fatigue critical crack size of the rotor under normal shutdown transient conditions of the nuclear power steam turbine, the stress corrosion crack growth life is obtained.

[0124] In one embodiment, the calculation process of stress corrosion crack growth life is as follows:

[0125]

[0126] For example, continuing to take the welded low-pressure rotor of a certain type of 1200MW nuclear power steam turbine in the above embodiment as an example, the basic data for stress corrosion life damage design monitoring of the welded low-pressure rotor is shown in Table 5.

[0127] Table 5 Basic data for stress corrosion life damage design monitoring of welded low-pressure rotors

[0128]

[0129] The calculation process of stress corrosion crack growth life of welded low-pressure rotor is as follows:

[0130]

[0131] Therefore, this method can comprehensively consider the threshold value of stress corrosion crack growth size, the annual average stress corrosion crack growth rate test value of the rotor material, and the low-cycle fatigue critical crack size of the rotor under normal shutdown transient conditions of the nuclear power steam turbine to obtain the stress corrosion crack growth life.

[0132] The following takes the cylinder as an example of the monitored component to describe how to obtain the stress corrosion crack growth life of the cylinder.

[0133] Based on any of the above embodiments, Figure 4 As shown, the stress corrosion crack growth life of the cylinder is obtained, including:

[0134] S401, obtaining stress calculation basic data and material test basic data of a cylinder of a nuclear power steam turbine.

[0135] S402, determining a set of crack extension dimensions based on stress calculation basic data and material experiment basic data.

[0136] For the relevant contents of steps S401 - S402 , please refer to the above embodiment and will not be described again here.

[0137] S403, based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the cylinder material, and the low-cycle fatigue critical crack size of the cylinder under the transient working condition of the nuclear power steam turbine cold start, the first stress corrosion crack growth life is obtained.

[0138] In one embodiment, the first stress corrosion crack growth life N fSCC1 The calculation process is as follows:

[0139]

[0140] S404, based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the cylinder material, and the low-cycle fatigue critical crack size of the cylinder under the transient working condition of warm start of nuclear power steam turbine, the second stress corrosion crack growth life is obtained.

[0141] In one embodiment, the second stress corrosion crack growth life N fSCC2 The calculation process is as follows:

[0142]

[0143] S405, based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the cylinder material, and the low-cycle fatigue critical crack size of the cylinder under the transient working condition of the nuclear power steam turbine hot start, the third stress corrosion crack growth life is obtained.

[0144] In one embodiment, the third stress corrosion crack growth life N fSCC3 The calculation process is as follows:

[0145]

[0146] For example, continuing to take the low-pressure inner cylinder of a certain model of 1000MW nuclear power steam turbine in the above embodiment as an example, the basic data for design monitoring of stress corrosion cracking of the low-pressure inner cylinder is shown in Table 6.

[0147] Table 6 Basic data for design monitoring of stress corrosion cracking of low-pressure inner cylinder

[0148]

[0149] The calculation process of various types of stress corrosion crack growth life of low-pressure inner cylinder is as follows:

[0150]

[0151]

[0152]

[0153] S406, determining the minimum value among the first stress corrosion crack growth life, the second stress corrosion crack growth life, and the third stress corrosion crack growth life as the stress corrosion crack growth life.

[0154] For example, taking the low-pressure inner cylinder of a certain type of 1000MW nuclear power steam turbine in the above embodiment as an example, the first stress corrosion crack growth life N of the low-pressure inner cylinder is fSCC1 The second stress corrosion crack growth life is 12.836 years. fSCC2 The third stress corrosion crack growth life is 11.690 years. fSCC3 The stress corrosion crack growth life of the low-pressure inner cylinder is 16.457 years. fSCC The calculation process is as follows:

[0155] N fSCC =min{N fSCC1 ,N fSCC2 ,N fSCC3}=min{12.836,11.690,16.457}=11.690years

[0156] Therefore, this method can comprehensively consider the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the cylinder material and the low-cycle fatigue critical crack size, obtain multiple types of stress corrosion crack growth life, and determine the minimum value of the multiple types of stress corrosion crack growth life as the stress corrosion crack growth life.

[0157] On the basis of any of the above embodiments, the fatigue crack growth life includes the low-cycle fatigue crack growth life, and based on the crack growth size set, the low-cycle corrosion crack growth life is obtained, including obtaining the low-cycle fatigue crack growth life of at least one stage of the set working condition of the nuclear power steam turbine based on the target parameters of the monitoring component, the crack shape parameters of the monitoring component, the low-cycle fatigue crack growth test constants of the material of the monitoring component, and the maximum stress of the crack part of the monitoring component under the set working condition of the nuclear power steam turbine, wherein the target parameter is the initial crack size of the monitoring component and any two parameters in the crack growth size set. Therefore, the method can comprehensively consider the target parameters of the monitoring component, the crack shape parameters of the monitoring component, the low-cycle fatigue crack growth test constants of the material of the monitoring component, and the maximum stress of the crack part of the monitoring component under the set working condition of the nuclear power steam turbine, and obtain the low-cycle fatigue crack growth life of at least one stage of the set working condition of the nuclear power steam turbine.

[0158] The following takes the rotor as an example of the monitored component to describe how to obtain the low-cycle fatigue crack growth life of the rotor.

[0159] Based on any of the above embodiments, the crack expansion stage of the rotor includes three stages, wherein in the first stage, the crack size of the rotor increases from the initial crack size a 0 Extended to the high cycle fatigue crack growth size threshold a th In the second stage, the crack size of the rotor increases from the high cycle fatigue crack growth threshold value a th Extend to the stress corrosion crack growth size threshold a SCC In the third stage, the crack size of the rotor increases from the stress corrosion crack growth threshold value a SCC Extended to the critical crack size of low cycle fatigue a cj Among them, the critical crack size of low cycle fatigue is a cj for a cn or a c110% or a c120% .

[0160] Based on any of the above embodiments, Figure 5 As shown, the low cycle fatigue crack growth life of the rotor is obtained, including:

[0161] S501, obtaining basic stress calculation data and material test basic data of a nuclear power steam turbine rotor.

[0162] S502: Determine a crack extension size set of the rotor based on stress calculation basic data and material test basic data.

[0163] For the relevant contents of steps S501-S502, please refer to the above embodiment and will not be repeated here.

[0164] S503, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the first stage of the normal shutdown transient condition of the nuclear power steam turbine.

[0165] In one embodiment, based on a crack extension size set, a low-cycle fatigue crack extension life of a first stage of a nuclear power steam turbine normal shutdown transient operating condition is obtained, including an initial crack size of the rotor, a high-cycle fatigue crack extension size threshold value, a crack shape parameter of the rotor, a low-cycle fatigue crack extension test constant of the rotor material, and a maximum stress at a rotor crack site of a nuclear power steam turbine normal shutdown transient operating condition, to obtain a low-cycle fatigue crack extension life of a first stage of a nuclear power steam turbine normal shutdown transient operating condition.

[0166] In some examples, the low-cycle fatigue crack growth life N of the first stage of the normal shutdown transient condition of a nuclear power steam turbine is fn,1 The calculation process is as follows:

[0167]

[0168] Among them, C 0 、m 0 Low cycle fatigue crack growth test constant of rotor material.

[0169] S504, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the second stage of the normal shutdown transient condition of the nuclear power steam turbine.

[0170] In one embodiment, based on the crack growth size set, the low-cycle fatigue crack growth life of the second stage of the normal shutdown transient condition of the nuclear power steam turbine is obtained, including based on the high-cycle fatigue crack growth size threshold value, the stress corrosion crack growth size threshold value, the crack shape parameters of the rotor, the low-cycle fatigue crack growth test constants of the rotor material, and the maximum stress of the rotor crack site of the normal shutdown transient condition of the nuclear power steam turbine, to obtain the low-cycle fatigue crack growth life of the second stage of the normal shutdown transient condition of the nuclear power steam turbine.

[0171] In some examples, the low-cycle fatigue crack growth life N of the second stage of the normal shutdown transient condition of a nuclear power steam turbine is fn,2 The calculation process is as follows:

[0172]

[0173] S505, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the third stage of the normal shutdown transient condition of the nuclear power steam turbine.

[0174] In one embodiment, based on the crack extension size set, the low-cycle fatigue crack extension life of the third stage of the normal shutdown transient condition of the nuclear power steam turbine is obtained, including the low-cycle fatigue critical crack size of the rotor under the normal shutdown transient condition of the nuclear power steam turbine based on the stress corrosion crack extension size threshold value, the low-cycle fatigue critical crack size of the rotor under the normal shutdown transient condition of the nuclear power steam turbine, the crack shape parameters of the rotor, the low-cycle fatigue crack extension test constant of the rotor material, and the maximum stress of the rotor crack site under the normal shutdown transient condition of the nuclear power steam turbine, so as to obtain the low-cycle fatigue crack extension life of the third stage of the normal shutdown transient condition of the nuclear power steam turbine.

[0175] In some examples, the low-cycle fatigue crack growth life N of the third stage of the normal shutdown transient condition of a nuclear power steam turbine is fn,3 The calculation process is as follows:

[0176]

[0177] S506, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the first stage of the nuclear power steam turbine 110% overspeed test transient condition.

[0178] In one embodiment, based on a crack extension size set, a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a 110% overspeed test transient condition is obtained, including an initial crack size of the rotor, a high-cycle fatigue crack extension size threshold, a crack shape parameter of the rotor, a low-cycle fatigue crack extension test constant of the rotor material, and a maximum stress at a rotor crack site of a nuclear power steam turbine in a 110% overspeed test transient condition, to obtain a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a 110% overspeed test transient condition.

[0179] In some examples, the low-cycle fatigue crack growth life N of the first stage of transient conditions of a nuclear power steam turbine 110% overspeed test is f110%,1 The calculation process is as follows:

[0180]

[0181] S507, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the second stage of the nuclear power steam turbine 110% overspeed test transient condition.

[0182] In one embodiment, based on the crack extension size set, the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine 110% overspeed test transient condition is obtained, including based on the high-cycle fatigue crack extension size threshold value, the stress corrosion crack extension size threshold value, the crack shape parameters of the rotor, the rotor material low-cycle fatigue crack extension test constant, and the maximum stress of the rotor crack site of the nuclear power steam turbine 110% overspeed test transient condition, to obtain the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine 110% overspeed test transient condition.

[0183] In some examples, the low-cycle fatigue crack growth life N of the second stage of the transient condition of the nuclear power steam turbine 110% overspeed test is f110%,2 The calculation process is as follows:

[0184]

[0185] S508, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the third stage of the nuclear power steam turbine 110% overspeed test transient condition.

[0186] In one embodiment, based on the crack extension size set, the low-cycle fatigue crack extension life of the third stage of the nuclear power steam turbine 110% overspeed test transient condition is obtained, including the low-cycle fatigue critical crack size of the rotor of the nuclear power steam turbine 110% overspeed test transient condition, the crack shape parameters of the rotor, the rotor material low-cycle fatigue crack extension test constant, and the maximum stress of the rotor crack site of the nuclear power steam turbine 110% overspeed test transient condition, so as to obtain the low-cycle fatigue crack extension life of the third stage of the nuclear power steam turbine 110% overspeed test transient condition.

[0187] In some examples, the low-cycle fatigue crack growth life N of the third stage of transient conditions of a nuclear power steam turbine 110% overspeed test is f110%,3 The calculation process is as follows:

[0188]

[0189] S509, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the first stage of the nuclear power steam turbine 120% overspeed transient operation condition.

[0190] In one embodiment, based on a crack extension size set, a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a 120% overspeed transient operating condition is obtained, including an initial crack size of the rotor, a high-cycle fatigue crack extension size threshold value, a crack shape parameter of the rotor, a low-cycle fatigue crack extension test constant of the rotor material, and a maximum stress at a rotor crack site in a nuclear power steam turbine in a 120% overspeed transient operating condition, to obtain a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a 120% overspeed transient operating condition.

[0191] In some examples, the low-cycle fatigue crack growth life N of the first stage of a nuclear power steam turbine transient operating condition of 120% overspeed operation is f120%,1 The calculation process is as follows:

[0192]

[0193] S510, based on the crack growth size set, obtaining the low cycle fatigue crack growth life of the second stage of the nuclear power steam turbine 120% overspeed transient operation condition.

[0194] In one embodiment, based on the crack extension size set, the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine 120% overspeed transient operating condition is obtained, including based on the high-cycle fatigue crack extension size threshold value, the stress corrosion crack extension size threshold value, the crack shape parameters of the rotor, the rotor material low-cycle fatigue crack extension test constants, and the maximum stress of the rotor crack site of the nuclear power steam turbine 120% overspeed transient operating condition, to obtain the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine 120% overspeed transient operating condition.

[0195] In some examples, the low-cycle fatigue crack growth life N of the second stage of a nuclear power steam turbine under 120% overspeed transient condition is f120%,2 The calculation process is as follows:

[0196]

[0197] S511, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the third stage of the nuclear power steam turbine 120% overspeed transient operating condition.

[0198] In one embodiment, based on a crack extension size set, a low-cycle fatigue crack extension life of a third stage of a nuclear power steam turbine under a 120% overspeed transient operating condition is obtained, including a stress corrosion crack extension size threshold value, a low-cycle fatigue critical crack size of a rotor under a 120% overspeed transient operating condition of a nuclear power steam turbine, a crack shape parameter of a rotor, a low-cycle fatigue crack extension test constant of a rotor material, and a maximum stress at a rotor crack site under a 120% overspeed transient operating condition of a nuclear power steam turbine, to obtain a low-cycle fatigue crack extension life of a third stage of a nuclear power steam turbine under a 120% overspeed transient operating condition.

[0199] In some examples, the low-cycle fatigue crack growth life N of the third stage of a nuclear power steam turbine under 120% overspeed transient condition is f120%,3 The calculation process is as follows:

[0200]

[0201] For example, continuing to take the welded low-pressure rotor of a certain type of 1200MW nuclear power steam turbine in the above embodiment as an example, the basic data for low-cycle fatigue life damage design monitoring of the welded low-pressure rotor is shown in Table 7.

[0202] Table 7 Basic data for low cycle fatigue life damage design monitoring of welded low pressure rotor

[0203]

[0204] The calculation process of the low cycle fatigue crack growth life of the rotor is as follows:

[0205]

[0206]

[0207]

[0208]

[0209]

[0210]

[0211]

[0212]

[0213]

[0214] Therefore, this method can comprehensively consider the crack shape parameters of the rotor, the low-cycle fatigue crack growth test constants of the rotor material, the maximum stress at the rotor crack site, and the crack growth size set of the rotor to obtain the low-cycle fatigue crack growth life.

[0215] The following takes the cylinder as an example of the monitored component to describe how to obtain the low-cycle fatigue crack growth life of the cylinder.

[0216] Based on any of the above embodiments, the crack expansion stage of the cylinder includes two stages, wherein in the first stage, the crack size of the cylinder increases from the initial crack size a to 0 Extend to the stress corrosion crack growth size threshold a SCC In the second stage, the crack size of the cylinder increases from the stress corrosion crack growth threshold value a SCC Extended to the critical crack size of low cycle fatigue a cj Among them, the critical crack size of low cycle fatigue is a cj for a cc or a cw or a ch .

[0217] Based on any of the above embodiments, Figure 6 As shown, the multi-stage low-cycle fatigue crack growth life of the cylinder is obtained, including:

[0218] S601, obtaining basic data for stress calculation and basic data for material testing of a cylinder of a nuclear power steam turbine.

[0219] S602, determining a set of crack extension sizes of the cylinder based on stress calculation basic data and material test basic data.

[0220] For the relevant contents of steps S601-S602, please refer to the above embodiment and will not be repeated here.

[0221] S603, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the first stage of the nuclear power steam turbine cold start transient condition.

[0222] In one embodiment, based on the crack growth size set, the low-cycle fatigue crack growth life of the first stage of the nuclear power steam turbine cold start transient condition is obtained, including the initial crack size of the cylinder, the stress corrosion crack growth size threshold value, the crack shape parameters of the cylinder, the cylinder material low-cycle fatigue crack growth test constant, and the maximum stress at the cylinder crack site of the nuclear power steam turbine cold start transient condition, so as to obtain the low-cycle fatigue crack growth life of the first stage of the nuclear power steam turbine cold start transient condition.

[0223] In some examples, the low-cycle fatigue crack growth life N of the first stage of the cold start transient condition of a nuclear power steam turbine is fc,1 The calculation process is as follows:

[0224]

[0225] Among them, C 0 、m 0 Low cycle fatigue crack growth test constants of cylinder materials.

[0226] S604, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the second stage of the nuclear power steam turbine cold start transient condition.

[0227] In one embodiment, based on the crack extension size set, the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine cold start transient condition is obtained, including the low-cycle fatigue critical crack size of the cylinder under the nuclear power steam turbine cold start transient condition, the crack shape parameters of the cylinder, the low-cycle fatigue crack extension test constant of the cylinder material, and the maximum stress of the cylinder crack site under the nuclear power steam turbine cold start transient condition, so as to obtain the low-cycle fatigue crack extension life of the second stage of the nuclear power steam turbine cold start transient condition.

[0228] In some examples, the low-cycle fatigue crack growth life N of the second stage of the cold start transient condition of a nuclear power steam turbine is fc,2 The calculation process is as follows:

[0229]

[0230] S605, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the first stage of the warm start transient condition of the nuclear power steam turbine.

[0231] In one embodiment, based on a set of crack extension sizes, a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a warm start transient condition is obtained, including an initial crack size of the cylinder, a stress corrosion crack extension size threshold, a crack shape parameter of the cylinder, a low-cycle fatigue crack extension test constant of the cylinder material, and a maximum stress at a cylinder crack site in a warm start transient condition of a nuclear power steam turbine, to obtain a low-cycle fatigue crack extension life of a nuclear power steam turbine in the first stage of a warm start transient condition.

[0232] In some examples, the low-cycle fatigue crack growth life N of the first stage of warm start transient conditions of nuclear power steam turbines is fw,1 The calculation process is as follows:

[0233]

[0234] S606, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the second stage of the warm start transient condition of the nuclear power steam turbine.

[0235] In one embodiment, based on the crack growth size set, the low-cycle fatigue crack growth life of the second stage of the warm start transient condition of the nuclear power steam turbine is obtained, including the low-cycle fatigue critical crack size of the cylinder under the warm start transient condition of the nuclear power steam turbine based on the stress corrosion crack growth size threshold value, the low-cycle fatigue critical crack size of the cylinder under the warm start transient condition of the nuclear power steam turbine, the crack shape parameters of the cylinder, the low-cycle fatigue crack growth test constant of the cylinder material, and the maximum stress at the cylinder crack site under the warm start transient condition of the nuclear power steam turbine, so as to obtain the low-cycle fatigue crack growth life of the second stage of the warm start transient condition of the nuclear power steam turbine.

[0236] In some examples, the low-cycle fatigue crack growth life N of the second stage of warm start transient conditions of nuclear power steam turbines is fw,2 The calculation process is as follows:

[0237]

[0238] S607, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the first stage of the nuclear power steam turbine hot start transient condition.

[0239] In one embodiment, based on the crack growth size set, the low-cycle fatigue crack growth life of the first stage of the hot start transient condition of the nuclear power steam turbine is obtained, including the initial crack size of the cylinder, the stress corrosion crack growth size threshold value, the crack shape parameters of the cylinder, the low-cycle fatigue crack growth test constant of the cylinder material, and the maximum stress at the cylinder crack site of the hot start transient condition of the nuclear power steam turbine, so as to obtain the low-cycle fatigue crack growth life of the first stage of the hot start transient condition of the nuclear power steam turbine.

[0240] In some examples, the low-cycle fatigue crack growth life N of the first stage of the hot start transient condition of a nuclear power steam turbine is fh,1 The calculation process is as follows:

[0241]

[0242] S608, based on the crack growth size set, obtain the low cycle fatigue crack growth life of the second stage of the nuclear power steam turbine hot start transient condition.

[0243] In one embodiment, based on the crack growth size set, the low-cycle fatigue crack growth life of the second stage of the nuclear power steam turbine hot start transient condition is obtained, including the low-cycle fatigue critical crack size of the cylinder under the nuclear power steam turbine hot start transient condition, the crack shape parameters of the cylinder, the low-cycle fatigue crack growth test constants of the cylinder material, and the maximum stress at the cylinder crack site under the nuclear power steam turbine hot start transient condition, so as to obtain the low-cycle fatigue crack growth life of the second stage of the nuclear power steam turbine hot start transient condition.

[0244] In some examples, the low-cycle fatigue crack growth life N of the second stage of the hot start transient condition of a nuclear power steam turbine is fh,2 The calculation process is as follows:

[0245]

[0246] For example, continuing to take the low-pressure inner cylinder of a certain type of 1000MW nuclear power steam turbine in the above embodiment as an example, the basic data for low-cycle fatigue cracking design monitoring of the low-pressure inner cylinder is shown in Table 8.

[0247] Table 8 Basic data for low cycle fatigue cracking design monitoring of low pressure inner cylinder

[0248]

[0249]

[0250] The calculation process of the multi-stage low-cycle fatigue crack growth life of the low-pressure inner cylinder is as follows:

[0251]

[0252]

[0253]

[0254]

[0255]

[0256]

[0257] Therefore, this method can comprehensively consider the crack shape parameters of the cylinder, the low-cycle fatigue crack growth test constants of the cylinder material, the maximum stress at the cylinder crack site, and the crack growth size set of the cylinder to obtain the multi-stage low-cycle fatigue crack growth life.

[0258] On the basis of any of the above embodiments, the fatigue crack growth life includes the high-cycle fatigue crack growth life, and the high-cycle fatigue crack growth life is obtained based on the crack growth size set, including the high-cycle fatigue crack growth size threshold value, the high-cycle fatigue critical crack size, the crack shape parameters of the monitoring component, the high-cycle fatigue crack growth test constant of the material of the monitoring component, and the high-cycle fatigue stress range of the crack part of the monitoring component under the steady-state working condition of the nuclear power steam turbine under load operation, so as to obtain the high-cycle fatigue crack growth life. Therefore, the method can comprehensively consider the high-cycle fatigue crack growth size threshold value, the high-cycle fatigue critical crack size, the crack shape parameters of the monitoring component, the high-cycle fatigue crack growth test constant of the material of the monitoring component, and the high-cycle fatigue stress range of the crack part of the monitoring component under the steady-state working condition of the nuclear power steam turbine under load operation to obtain the high-cycle fatigue crack growth life.

[0259] The following takes the rotor as an example of the monitored component to describe how to obtain the high cycle fatigue crack growth life of the rotor.

[0260] Based on any of the above embodiments, Figure 7 As shown, the high cycle fatigue crack growth life of the rotor is obtained, including:

[0261] S701, obtaining basic stress calculation data and material test basic data of a nuclear power steam turbine rotor.

[0262] S702: Determine a high cycle fatigue crack growth size threshold of the rotor based on stress calculation basic data and material test basic data.

[0263] S703, determining a high cycle fatigue critical crack size of the rotor based on stress calculation basic data and material test basic data.

[0264] For the relevant contents of steps S701 to S703, please refer to the above embodiment and will not be repeated here.

[0265] S704, based on the high cycle fatigue crack growth size threshold value, high cycle fatigue critical crack size, crack shape parameters of the rotor, high cycle fatigue crack growth test constants of rotor materials, and high cycle fatigue stress range of the rotor under steady-state conditions of nuclear power steam turbine under load operation, obtain the high cycle fatigue crack growth life.

[0266] In one embodiment, the high cycle fatigue crack growth life is calculated as follows:

[0267]

[0268] For example, continuing to take the welded low-pressure rotor of a certain type of 1200MW nuclear power steam turbine in the above embodiment as an example, the basic data for high-cycle fatigue life damage design monitoring of the welded low-pressure rotor is shown in Table 9.

[0269] Table 9 Basic data for high cycle fatigue life damage design monitoring of welded low pressure rotor

[0270]

[0271] The calculation process of high cycle fatigue crack growth life of welded low pressure rotor is as follows:

[0272]

[0273] Therefore, this method can comprehensively consider the high-cycle fatigue crack growth size threshold value, high-cycle fatigue critical crack size, rotor crack shape parameters, rotor material high-cycle fatigue crack growth test constants, and rotor high-cycle fatigue stress range of nuclear power steam turbine under steady-state load operation to obtain the high-cycle fatigue crack growth life.

[0274] Figure 8 The present invention is a flow chart of a method for monitoring the stress corrosion and fatigue of a nuclear power steam turbine for a long life according to an embodiment of the present invention.

[0275] like Figure 8 As shown, the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to an embodiment of the present disclosure includes:

[0276] S801, obtaining stress calculation basic data and material test basic data of monitoring components of nuclear power steam turbine.

[0277] S802, based on the stress calculation basic data and the material experiment basic data, obtain the long-life monitoring data required for the monitoring component, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life.

[0278] For the relevant contents of steps S801-S802, please refer to the above embodiment and will not be repeated here.

[0279] S803, based on the long-life monitoring data required by the monitoring component, obtain the multi-stage calendar life of the monitoring component.

[0280] S804, based on the multi-stage calendar life of the monitored component, obtain the crack growth calendar life.

[0281] In one embodiment, based on the long-life monitoring data required by the monitoring component, the multi-stage calendar life of the monitoring component is obtained, including obtaining at least one long-life monitoring data matching any stage from the long-life monitoring data, and obtaining the calendar life of any stage based on at least one long-life monitoring data matching any stage.

[0282] In one embodiment, the crack growth calendar life is obtained based on the multi-stage calendar life of the monitoring component, including determining the sum of the multi-stage calendar life of the monitoring component as the crack growth calendar life.

[0283] The following takes the rotor as an example of the monitored component to describe how to obtain the crack growth calendar life of the rotor.

[0284] In one embodiment, the calendar life of the first stage is obtained based on the low-cycle fatigue crack growth life of the first stage of the normal shutdown transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the first stage of the 110% overspeed test transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the first stage of the 120% overspeed operation transient condition of the nuclear power steam turbine, the average annual number of normal shutdowns of the nuclear power steam turbine, the average annual number of 110% overspeed tests and the average annual number of 120% overspeed operations.

[0285] In one embodiment, the calendar life of the second stage is obtained based on the high-cycle fatigue crack growth life, the low-cycle fatigue crack growth life of the second stage of the normal shutdown transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the second stage of the 110% overspeed test transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the second stage of the 120% overspeed operation transient condition of the nuclear power steam turbine, the average annual normal shutdown times of the nuclear power steam turbine, the average annual 110% overspeed test times, the average annual 120% overspeed operation times and the average annual fatigue times of the rotor.

[0286] In one embodiment, it also includes the calendar life of the third stage based on the stress corrosion crack growth life, the high cycle fatigue crack growth life, the low cycle fatigue crack growth life of the third stage of the normal shutdown transient condition of the nuclear power steam turbine, the low cycle fatigue crack growth life of the third stage of the 110% overspeed test transient condition of the nuclear power steam turbine, the low cycle fatigue crack growth life of the third stage of the 120% overspeed operation transient condition of the nuclear power steam turbine, the average annual normal shutdown times of the nuclear power steam turbine, the average annual 110% overspeed test times, the average annual 120% overspeed operation times and the average annual fatigue times of the rotor.

[0287] In one embodiment, the method further includes obtaining a crack growth calendar life based on the calendar life of the first stage, the calendar life of the second stage, and the calendar life of the third stage. For example, obtaining a crack growth calendar life based on the calendar life of the first stage, the calendar life of the second stage, and the calendar life of the third stage includes determining the sum of the calendar life of the first stage, the calendar life of the second stage, and the calendar life of the third stage as the crack growth calendar life.

[0288] In some examples, the crack growth calendar life τ CL The calculation process is as follows:

[0289]

[0290]

[0291]

[0292] τ CL =τ CL1 +τ CL2 +τ CL3

[0293] Among them, τ CL1 is the calendar life of the first stage, τ CL2 is the calendar life of the second stage, τ CL3 is the calendar life of the third stage, y n is the annual average number of normal shutdowns of nuclear power steam turbines, y 110% is the annual average number of 110% overspeed tests, y 120% is the annual average of 120% overspeed operation times, y H is the annual average high cycle fatigue number of the rotor.

[0294] In some examples, the average annual operating hours of nuclear power turbines can be based on t y and the operating speed n of the nuclear power steam turbine 0 , the annual average high cycle fatigue number of the rotor y is obtained H For example, this can be achieved by the following formula:

[0295]

[0296] For example, continuing to take the welded low-pressure rotor of a certain model of 1200MW nuclear power steam turbine in the above embodiment as an example, the calendar design monitoring basic data of the welded low-pressure rotor is shown in Table 10.

[0297] Table 10 Calendar design monitoring basic data for welded low-pressure rotor

[0298] Serial number project Data Value 1 <![CDATA[Average annual normal shutdown times y n / time]]> 99 2 <![CDATA[Annual average number of 110% overspeed tests y 110% / times]]> 1 3 <![CDATA[Annual average number of times of running at 120% over speed y 120% / times]]> 0.2 4 <![CDATA[Annual average operating hours t y / h]]> 7000 5 <![CDATA[Operating speed n 0 / r / min]]> 1500 6 <![CDATA[The crack propagation life safety monitoring criterion value τ 0 / year]]> 60

[0299] The calculation process of the annual average high-cycle fatigue number of welded low-pressure rotors is as follows:

[0300]

[0301] The calculation process of the crack growth calendar life of the welded low-pressure rotor is as follows:

[0302]

[0303]

[0304]

[0305] τ CL =τ CL1 +τ CL2 +τ CL3 =133.54+11.37+17.78=162.69 years

[0306] The following takes the cylinder as an example of the monitored component to describe how to obtain the crack growth calendar life of the cylinder.

[0307] In one embodiment, it also includes the low-cycle fatigue crack growth life of the first stage of the nuclear power steam turbine cold start transient condition, the low-cycle fatigue crack growth life of the first stage of the nuclear power steam turbine warm start transient condition, the low-cycle fatigue crack growth life of the first stage of the nuclear power steam turbine hot start transient condition, the average annual number of cold starts, the average annual number of warm starts and the average annual number of hot starts of the nuclear power steam turbine, to obtain the calendar life of the first stage.

[0308] In one embodiment, it also includes obtaining the calendar life of the second stage based on the target stress corrosion crack growth life, the low-cycle fatigue crack growth life of the second stage of the cold start transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the second stage of the warm start transient condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of the second stage of the hot start transient condition of the nuclear power steam turbine, the average annual number of cold starts, the average annual number of warm starts and the average annual number of hot starts of the nuclear power steam turbine.

[0309] In one embodiment, the method further includes obtaining a crack growth calendar life based on the calendar life of the first stage and the calendar life of the second stage. For example, obtaining a crack growth calendar life based on the calendar life of the first stage and the calendar life of the second stage includes determining the sum of the calendar life of the first stage and the calendar life of the second stage as the crack growth calendar life.

[0310] In some examples, the crack growth calendar life τ CL The calculation process is as follows:

[0311]

[0312]

[0313] τ CL =τ CL1 +τ CL2

[0314] Among them, τ CL1 is the calendar life of the first stage, τ CL2 is the calendar life of the second stage, y c is the annual average number of cold starts of nuclear power steam turbines, y w is the annual average number of warm-state starts, y h is the average number of hot starts per year.

[0315] For example, continuing to take the low-pressure inner cylinder of a certain model of 1000MW nuclear power steam turbine in the above embodiment as an example, the calendar design monitoring basic data of the low-pressure inner cylinder is shown in Table 11.

[0316] Table 11 Calendar design monitoring basic data of low pressure inner cylinder

[0317] Serial number project Data Value 1 <![CDATA[Annual average cold start times y c / times]]> 4 2 <![CDATA[Annual average temperature state start-up times y w / times]]> 20 3 <![CDATA[Annual average number of hot starts y h / times]]> 75 4 <![CDATA[The safety monitoring criterion value τ of crack propagation life 0 / year]]> 60

[0318] The calculation process of the crack growth calendar life of the low-pressure inner cylinder is as follows:

[0319]

[0320]

[0321] τ CL =τ CL1 +τ CL2 =45.13+8.81=53.94 years

[0322] S805, based on the long-life monitoring data required by the monitoring component, obtain the crack growth calendar life of the monitoring component.

[0323] S806: Based on the crack growth calendar life, crack growth life safety monitoring is performed on the monitoring component.

[0324] For the relevant contents of steps S805-S806, please refer to the above embodiment and will not be repeated here.

[0325] In summary, according to the long-life monitoring method for stress corrosion and fatigue of a nuclear power steam turbine of the embodiment of the present disclosure, the multi-stage calendar life of the monitored component is obtained based on the long-life monitoring data required by the monitored component, and the crack propagation calendar life is obtained based on the multi-stage calendar life of the monitored component. Thus, the multi-stage calendar life of the monitored component can be obtained based on the long-life monitoring data required by the monitored component to obtain the crack propagation calendar life.

[0326] Fig. 9 The present invention is a flow chart of a method for monitoring the stress corrosion and fatigue of a nuclear power steam turbine for a long life according to an embodiment of the present invention.

[0327] like Fig. 9 As shown, the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine according to an embodiment of the present disclosure includes:

[0328] S901, obtaining stress calculation basic data and material test basic data of monitoring components of nuclear power steam turbine.

[0329] S902, based on the stress calculation basic data and the material experiment basic data, obtain the long-life monitoring data required for the monitoring component, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life.

[0330] S903: If the nuclear power steam turbine is in the design stage, obtain the crack growth life safety monitoring criterion value of the monitored component.

[0331] S904: If the crack growth calendar life is less than the crack growth life safety monitoring criterion value, it is determined that the crack growth calendar life does not meet the monitoring qualification condition.

[0332] For the relevant contents of steps S901 - S904 , please refer to the above embodiment and will not be described again here.

[0333] For example, taking the welded low-pressure rotor of a certain type of 1200MW nuclear power steam turbine in the above embodiment as an example, the crack propagation calendar life τ of the welded low-pressure rotor is CL The crack growth life safety monitoring criterion value τ of the welded low-pressure rotor is 162.69 years. 0 As shown in Table 10, τ 0 = 60 years, then τ CL >τ 0 , it can be judged that the crack extension calendar life meets the monitoring qualification conditions.

[0334] For example, taking the low-pressure inner cylinder of a certain type of 1000MW nuclear power steam turbine in the above embodiment as an example, the crack growth calendar life τ of the low-pressure inner cylinder is CLis 53.94 years, and the safety monitoring criterion value of crack growth life of low-pressure inner cylinder is τ 0 As shown in Table 11, τ 0 = 60 years, then τ CL <τ 0 , it can be judged that the crack propagation calendar life does not meet the monitoring qualification conditions.

[0335] S905: If the crack growth calendar life does not meet the monitoring qualification condition, obtain the abnormal data of the monitoring component in the design stage.

[0336] S906, optimizing and improving the abnormal data of the monitoring component in the design phase, and returning to execute the process of obtaining the crack growth calendar life, until the obtained crack growth calendar life meets the monitoring qualification condition.

[0337] The following describes the optimization and improvement of the rotor by taking the rotor as an example of the monitoring component.

[0338] It should be noted that there are not too many restrictions on the abnormal data of the rotor in the design stage. For example, it may include the design process parameters of the rotor, the basic data for stress calculation of the rotor in the design stage, the basic data for rotor material testing, etc.

[0339] In one embodiment, the abnormal data of the rotor in the design stage is optimized and improved, including selecting materials with good stress corrosion resistance; selecting materials with good fatigue performance; adopting a welded rotor structure; adopting a whole rotor structure; avoiding structures that cause stress concentration in high stress areas; increasing the fillet radius of the rotor blade root slot structure to reduce the stress concentration coefficient; changing the axial key of the set impeller to a radial key; increasing the assembly gap between the set rotor key and the keyway; optimizing the starting parameter change curve of the nuclear power steam turbine to reduce the rotor thermal stress under the starting transient condition; optimizing the normal shutdown parameter change curve of the nuclear power steam turbine to reduce the rotor thermal stress under the shutdown transient condition; optimizing the load change parameter change curve of the nuclear power steam turbine to reduce the rotor thermal stress under the starting transient condition; using heat treatment technology to improve material toughness; improving processing accuracy and eliminating machining stress concentration; using heat treatment technology to reduce residual tensile stress; rolling the impeller surface to form surface compressive stress; shot peening the blade root slot to improve fatigue performance, etc.

[0340] The following takes the cylinder as an example of the monitored component to describe the optimization and improvement of the cylinder.

[0341] It should be noted that there are not too many restrictions on the abnormal data of the cylinder in the design stage. For example, it may include the design process parameters of the cylinder, the basic data for stress calculation of the cylinder in the design stage, the basic data for cylinder material testing, etc.

[0342] In one embodiment, the abnormal data of the cylinder in the design stage is optimized and improved, including selecting materials with good stress corrosion resistance; selecting materials with good low-cycle fatigue performance; avoiding structures that cause stress concentration in high stress areas; adopting structural fillet transition at the structural discontinuity of the connection between the turbine steam inlet pipe and the cylinder; adopting structural fillet transition at the structural discontinuity of the connection between the turbine steam extraction pipe and the cylinder; increasing the fillet radius of the connection between the cylinder and the steam extraction pipe to reduce the stress concentration coefficient; designing the cylinder weld to be away from the stress concentration; optimizing the nuclear power steam turbine starting parameter change curve to reduce the cylinder thermal stress under the starting transient working condition; optimizing the nuclear power steam turbine load change parameter change curve to reduce the cylinder thermal stress under the starting transient working condition; using heat treatment technology to improve material toughness; improving processing accuracy to eliminate machining stress concentration; using heat treatment technology to reduce welding residual tensile stress; rolling the cylinder surface to form surface compressive stress; shot peening the cylinder surface to improve fatigue performance, etc.

[0343] For example, continuing to take the low-pressure inner cylinder of a certain model of 1000MW nuclear power steam turbine in the above embodiment as an example, the low-pressure inner cylinder has a weak life, that is, the connection between the inner cylinder and the second-stage steam extraction pipe, and the structural transition fillet radius of the structural discontinuity at the connection between the second-stage steam extraction pipe and the low-pressure inner cylinder is increased from the original design of 5mm to 20mm, and the low-pressure inner cylinder is structurally optimized and improved.

[0344] A model of the optimized structure of the low-pressure inner cylinder is established, the temperature field and stress field are calculated, and the basic data of stress calculation and material test of the low-pressure inner cylinder are updated. The specific data are shown in Table 12.

[0345] Table 12 Basic data for design and monitoring of low-pressure inner cylinder

[0346]

[0347]

[0348] Using the updated stress calculation basic data and material test basic data of the low-pressure inner cylinder shown in Table 12, the crack growth size set of the low-pressure inner cylinder, various types of stress corrosion crack growth life, target stress corrosion crack growth life, multi-stage low-cycle fatigue crack growth life, multi-stage calendar life and crack growth calendar life are recalculated. The specific data are shown in Tables 13, 14, 15 and 16.

[0349] Table 13 Crack extension size set of low pressure inner cylinder

[0350] Serial number project Data Value 1 <![CDATA[Threshold value a of stress corrosion crack size SCC / m]]> 0.008264 2 <![CDATA[Critical crack size a for low-cycle fatigue under cold start transient conditions cc / m]]> 0.042375 3 <![CDATA[Critical crack size a of low cycle fatigue under warm start transient conditions cw / m]]> 0.038012 4 <![CDATA[Critical crack size a for low-cycle fatigue under hot start transient conditions ch / m]]> 0.047979

[0351] Table 14 SCC growth life and target SCC growth life of various types of low pressure inner cylinders

[0352] Serial number project Data Value 1 <![CDATA[The first stress corrosion crack growth life N fSCC1 / year]]> 22.741 2 <![CDATA[The second stress corrosion crack growth life N fSCC2 / year]]> 19.832 3 <![CDATA[The third stress corrosion crack growth life N fSCC3 / year]]> 26.477 4 <![CDATA[Target stress corrosion crack growth life N fSCC / year]]> 19.832

[0353] Table 15 Multi-stage low-cycle fatigue crack growth life of low-pressure inner cylinder

[0354]

[0355]

[0356] Table 16 Multi-stage calendar life and crack growth calendar life of low-pressure inner cylinder

[0357] Serial number project Data Value 1 <![CDATA[Calendar life τ of the first stage CL1 / year]]> 123.73 2 <![CDATA[Calendar life τ of the second stage CL1 / year]]> 14.96 3 <![CDATA[Crack propagation calendar life τ CL / year]]> 138.69

[0358] It can be seen from Table 16 that after the structural optimization and improvement of the low-pressure inner cylinder, the crack growth calendar life τ of the low-pressure inner cylinder CL =138.69 years, which is greater than the crack growth life safety monitoring criterion value τ of nuclear power steam turbine 0 =60 years, the crack propagation calendar life of the low-pressure inner cylinder meets the monitoring qualification conditions, and the crack propagation life safety monitoring of the low-pressure inner cylinder is ended.

[0359] In summary, according to the stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine in an embodiment of the present disclosure, if the crack propagation calendar life does not meet the monitoring qualification conditions, the abnormal data of the monitoring component in the design stage is obtained, the abnormal data of the monitoring component in the design stage is optimized and improved, and the process of obtaining the crack propagation calendar life is returned to execute until the obtained crack propagation calendar life meets the monitoring qualification conditions, which helps to improve the safety of the monitoring component in the design stage and is suitable for the monitoring of the monitoring component in the design stage of the nuclear power steam turbine.

[0360] In order to realize the above-mentioned embodiment, the present disclosure also proposes a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine.

[0361] Fig.10 The figure is a schematic structural diagram of a stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine according to an embodiment of the present disclosure.

[0362] like Fig.10 As shown, the stress corrosion and fatigue long-life monitoring device 100 for a nuclear power steam turbine according to an embodiment of the present disclosure includes: an acquisition module 110 and a monitoring module 120 .

[0363] An acquisition module 110 is used to acquire stress calculation basic data and material test basic data of a monitoring component of a nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, acquire long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life;

[0364] The monitoring module 120 is used to obtain the crack growth calendar life of the monitoring component based on the long-life monitoring data required by the monitoring component, and perform crack growth life safety monitoring on the monitoring component based on the crack growth calendar life.

[0365] In one embodiment of the present disclosure, the acquisition module 110 is further used to: acquire the mapping relationship between the stress calculation basic data, the material test basic data and the monitoring component; and acquire the stress calculation basic data and the material test basic data of the monitoring component based on the mapping relationship.

[0366] In one embodiment of the present disclosure, the acquisition module 110 is further used to: if the monitored component is a rotor, determine that the long-life monitoring data required for the rotor includes the stress corrosion crack growth life, the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life; if the monitored component is a cylinder, determine that the long-life monitoring data required for the cylinder includes the stress corrosion crack growth life and the low-cycle fatigue crack growth life.

[0367] In one embodiment of the present disclosure, the acquisition module 110 is further used to: determine the crack extension size set of the monitoring component based on the stress calculation basic data and the material experiment basic data; and acquire the long-life monitoring data required for the monitoring component based on the crack extension size set.

[0368] In one embodiment of the present disclosure, the acquisition module 110 is also used to: determine the stress corrosion crack extension size threshold value of the monitored component based on the crack shape parameters of the monitored component, the stress corrosion fracture toughness of the material of the monitored component and the maximum stress at the crack site of the monitored component under the steady-state condition of load operation of the nuclear power steam turbine; determine the low-cycle fatigue critical crack size of the monitored component under the set operating condition of the nuclear power steam turbine based on the crack shape parameters of the monitored component, the fracture toughness of the material of the monitored component and the maximum stress at the crack site of the monitored component under the set operating condition of the nuclear power steam turbine.

[0369] In one embodiment of the present disclosure, the acquisition module 110 is also used to: determine the high-cycle fatigue crack extension size threshold value of the monitored component based on the crack shape parameters of the monitored component, the test value of the high-cycle fatigue crack extension threshold value of the material of the monitored component, and the high-cycle fatigue stress range of the crack site of the monitored component under steady-state conditions of load operation of the nuclear power steam turbine; determine the high-cycle fatigue critical crack size of the monitored component based on the crack shape parameters of the monitored component, the fracture toughness of the material of the monitored component, and the maximum stress at the crack site of the monitored component under steady-state conditions of load operation of the nuclear power steam turbine.

[0370] In one embodiment of the present disclosure, the acquisition module 110 is also used to obtain the stress corrosion crack growth life based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low-cycle fatigue critical crack size of the monitoring component under the set operating conditions of the nuclear power turbine.

[0371] In one embodiment of the present disclosure, the acquisition module 110 is also used to: obtain multiple types of stress corrosion crack growth life based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low-cycle fatigue critical crack size of the monitoring component under the set operating conditions of the nuclear power turbine; and determine the stress corrosion crack growth life based on multiple types of stress corrosion crack growth life.

[0372] In one embodiment of the present disclosure, the acquisition module 110 is further configured to: determine a minimum value among multiple types of stress corrosion crack growth life as the stress corrosion crack growth life.

[0373] In one embodiment of the present disclosure, the fatigue crack growth life includes a low-cycle fatigue crack growth life, and the acquisition module 110 is further used to: obtain the low-cycle fatigue crack growth life of at least one stage of the set operating condition of the nuclear power steam turbine based on the target parameters of the monitoring component, the crack shape parameters of the monitoring component, the low-cycle fatigue crack growth test constant of the material of the monitoring component, and the maximum stress at the crack site of the monitoring component under the set operating condition of the nuclear power steam turbine; wherein the target parameters are the initial crack size of the monitoring component and any two parameters in the crack growth size set.

[0374] In one embodiment of the present disclosure, the fatigue crack growth life includes a high cycle fatigue crack growth life, and the acquisition module 110 is further used to obtain the high cycle fatigue crack growth life based on the high cycle fatigue crack growth size threshold value, the high cycle fatigue critical crack size, the crack shape parameters of the monitoring component, the high cycle fatigue crack growth test constant of the material of the monitoring component, and the high cycle fatigue stress range of the crack part of the monitoring component under the steady-state condition of the nuclear power steam turbine under load operation.

[0375] In one embodiment of the present disclosure, the monitoring module 120 is further used to: obtain the multi-stage calendar life of the monitoring component based on the long-life monitoring data required by the monitoring component; and obtain the crack extension calendar life based on the multi-stage calendar life of the monitoring component.

[0376] In one embodiment of the present disclosure, the monitoring module 120 is further used to determine the sum of the multi-stage calendar life of the monitored component as the crack extension calendar life.

[0377] In one embodiment of the present disclosure, the monitoring module 120 is also used for: if the nuclear power steam turbine is in the design stage, obtaining the crack propagation life safety monitoring criterion value of the monitoring component; if the crack propagation calendar life is less than the crack propagation life safety monitoring criterion value, judging that the crack propagation calendar life does not meet the monitoring qualification condition, so as to perform crack propagation life safety monitoring on the monitoring component; or, if the crack propagation calendar life is greater than or equal to the crack propagation life safety monitoring criterion value, judging that the crack propagation calendar life meets the monitoring qualification condition, so as to perform crack propagation life safety monitoring on the monitoring component.

[0378] In one embodiment of the present disclosure, the monitoring module 120 is also used to: if the crack propagation calendar life does not meet the monitoring qualification conditions, obtain abnormal data of the monitoring component in the design stage; optimize and improve the abnormal data of the monitoring component in the design stage, and return to execute the process of obtaining the crack propagation calendar life until the crack propagation calendar life obtained meets the monitoring qualification conditions.

[0379] It should be noted that for details not disclosed in the stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine in the embodiment of the present disclosure, please refer to the details disclosed in the stress corrosion and fatigue long-life monitoring method for a nuclear power steam turbine in the embodiment of the present disclosure, which will not be repeated here.

[0380] In summary, the stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine of the disclosed embodiment obtains the stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtains the long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes the stress corrosion crack growth life and the fatigue crack growth life, and the fatigue crack growth life includes at least one of the low-cycle fatigue crack growth life and the high-cycle fatigue crack growth life, and based on the long-life monitoring data required by the monitoring component, the crack growth calendar life of the monitoring component is obtained, and based on the crack growth calendar life, the crack growth life safety monitoring of the monitoring component is performed. Therefore, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.

[0381] In order to implement the above embodiment, Fig.11 As shown, an embodiment of the present disclosure proposes an electronic device 200, including: a memory 210, a processor 220, and a computer program stored in the memory 210 and executable on the processor 220. When the processor 220 executes the program, the above-mentioned stress corrosion and fatigue long-life monitoring method of the nuclear power steam turbine is implemented.

[0382] In one embodiment of the present disclosure, the electronic device 200 further includes: a wireless communication component, the wireless communication component is connected to the nuclear power steam turbine, and data is transmitted between the electronic device and the nuclear power steam turbine via the wireless communication component.

[0383] In one embodiment of the present disclosure, the memory 210 is used to store the crack propagation calendar life of the monitoring component of the nuclear power steam turbine; the processor 220 is used to obtain a crack propagation life safety monitoring instruction, and based on the crack propagation life safety monitoring instruction, obtain the crack propagation calendar life of the target monitoring component of the nuclear power steam turbine to be monitored from the memory 210, and perform crack propagation life safety monitoring on the target monitoring component based on the crack propagation calendar life of the target monitoring component.

[0384] In one embodiment of the present disclosure, the electronic device 200 also includes: a remote client, which is connected to the processor 220; the remote client is used to send the crack extension life safety monitoring instruction to the processor 220, and receive the monitoring results fed back by the processor 220.

[0385] In one embodiment of the present disclosure, the remote client is further used to obtain control information of a user who controls the remote client, and generate the crack extension life safety monitoring instruction based on the control information.

[0386] In one embodiment of the present disclosure, the processor 220 is further configured to determine a monitoring component of a nuclear power steam turbine associated with the remote client as the target monitoring component.

[0387] The electronic device of the disclosed embodiment executes a computer program stored in a memory through a processor to obtain stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtains the long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life, based on the long-life monitoring data required by the monitoring component, obtains the crack growth calendar life of the monitoring component, and based on the crack growth calendar life, performs crack growth life safety monitoring on the monitoring component. Thus, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.

[0388] In order to implement the above-mentioned embodiment, the embodiment of the present disclosure proposes a computer-readable storage medium on which a computer program is stored. When the program is executed by a processor, the above-mentioned stress corrosion and fatigue long-life monitoring method of a nuclear power steam turbine is implemented.

[0389] The computer-readable storage medium of the disclosed embodiment acquires stress calculation basic data and material test basic data of the monitoring component of the nuclear power steam turbine by storing a computer program and being executed by a processor, and acquires the long-life monitoring data required by the monitoring component based on the stress calculation basic data and the material test basic data, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life, and the crack growth calendar life of the monitoring component is obtained based on the long-life monitoring data required by the monitoring component, and crack growth life safety monitoring is performed on the monitoring component based on the crack growth calendar life. Thus, the influence of stress corrosion and fatigue on the life of the monitoring component can be comprehensively considered to perform crack growth life safety monitoring on the monitoring component to ensure the long-life safe operation of the nuclear power steam turbine.

[0390] In order to implement the above embodiment, the present disclosure provides a monitoring platform suitable for nuclear power steam turbines, including the above Fig.10 The stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine shown; or the above-mentioned electronic device; or the above-mentioned computer-readable storage medium.

[0391] The monitoring platform applicable to nuclear power steam turbines of the disclosed embodiment obtains stress calculation basic data and material test basic data of the monitoring components of the nuclear power steam turbine, and obtains the long-life monitoring data required by the monitoring components based on the stress calculation basic data and the material test basic data, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life, and based on the long-life monitoring data required by the monitoring components, the crack growth calendar life of the monitoring components is obtained, and based on the crack growth calendar life, the crack growth life safety monitoring of the monitoring components is performed. Thus, the influence of stress corrosion and fatigue on the life of the monitoring components can be comprehensively considered to perform crack growth life safety monitoring on the monitoring components to ensure the long-life safe operation of the nuclear power steam turbine.

[0392] In the description of the present disclosure, it needs to be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present disclosure and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present disclosure.

[0393] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present disclosure, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0394] In the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to specific circumstances.

[0395] In the present disclosure, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0396] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present disclosure. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, without contradiction.

[0397] Although the embodiments of the present disclosure have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present disclosure. A person skilled in the art may change, modify, replace and vary the above embodiments within the scope of the present disclosure.

Claims

1. A method for monitoring the stress corrosion and fatigue life of nuclear power steam turbines. It is characterized in that include: Obtain stress calculation basic data and material test basic data of a monitoring component of a nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, obtain long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life, wherein, based on the stress calculation basic data and the material test basic data, obtaining the stress corrosion crack growth life includes: Determining a stress corrosion crack extension size threshold value of the monitoring component based on the crack shape parameters of the monitoring component, the stress corrosion fracture toughness of the material of the monitoring component, and the maximum stress at the crack site of the monitoring component under the steady-state condition of the nuclear power steam turbine under load operation; Determining a low cycle fatigue critical crack size of the monitoring component under the set operating condition of the nuclear power steam turbine based on a crack shape parameter of the monitoring component, a fracture toughness of a material of the monitoring component, and a maximum stress at a crack site of the monitoring component under the set operating condition of the nuclear power steam turbine; The stress corrosion crack growth life is obtained by the difference between the low cycle fatigue critical crack size and the stress corrosion crack growth size threshold value of the monitoring component based on the set working conditions of the nuclear power steam turbine and the ratio of the annual average stress corrosion crack growth rate test value of the material of the monitoring component; Based on the long-life monitoring data required by the monitoring component, the crack growth calendar life of the monitoring component is obtained, and based on the crack growth calendar life, the crack growth life safety monitoring of the monitoring component is performed.

2. The method according to claim 1, It is characterized in that The step of obtaining the stress calculation basic data and material test basic data of the monitoring components of the nuclear power steam turbine includes: Acquire a mapping relationship between the stress calculation basic data, the material test basic data and the monitoring component; Based on the mapping relationship, the stress calculation basic data and the material test basic data of the monitoring component are acquired.

3. The method according to claim 1, It is characterized in that The method further comprises: If the monitored component is a rotor, determining the long-life monitoring data required for the rotor includes the stress corrosion crack growth life, the low cycle fatigue crack growth life and the high cycle fatigue crack growth life; If the monitored component is a cylinder, the long-life monitoring data required for determining the cylinder includes the stress corrosion crack growth life and the low cycle fatigue crack growth life.

4. The method according to claim 1, It is characterized in that The step of obtaining the long-life monitoring data required by the monitoring component based on the stress calculation basic data and the material test basic data includes: Determining a set of crack extension sizes of the monitoring component based on the stress calculation basic data and the material test basic data; Based on the crack growth size set, long-life monitoring data required by the monitoring component is obtained.

5. The method according to claim 4, It is characterized in that The step of determining the crack extension size set of the monitoring component based on the stress calculation basic data and the material test basic data includes: Determine the high cycle fatigue crack extension size threshold value of the monitoring component based on the crack shape parameters of the monitoring component, the test value of the high cycle fatigue crack extension threshold value of the material of the monitoring component, and the high cycle fatigue stress range of the crack part of the monitoring component under the steady-state working condition of the nuclear power steam turbine under load operation; Based on the crack shape parameters of the monitoring component, the fracture toughness of the material of the monitoring component, and the maximum stress at the crack site of the monitoring component under steady-state conditions of the nuclear power steam turbine under load operation, the high-cycle fatigue critical crack size of the monitoring component is determined.

6. The method according to claim 1, It is characterized in that Based on the crack extension size set, obtaining the stress corrosion crack extension life includes: The stress corrosion crack growth life is obtained based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low-cycle fatigue critical crack size of the monitoring component under the set operating conditions of the nuclear power steam turbine.

7. The method according to claim 6, It is characterized in that The stress corrosion crack growth life is obtained based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low cycle fatigue critical crack size of the monitoring component under the set working condition of the nuclear power steam turbine, including: Based on the stress corrosion crack growth size threshold value, the annual average stress corrosion crack growth rate test value of the material of the monitoring component, and the low cycle fatigue critical crack size of the monitoring component under the set working condition of the nuclear power steam turbine, multiple types of stress corrosion crack growth life are obtained; The stress corrosion crack growth life is determined based on multiple types of stress corrosion crack growth life.

8. The method according to claim 7, It is characterized in that The stress corrosion crack growth life is determined based on multiple types of stress corrosion crack growth life, including: The minimum value among the multiple types of stress corrosion crack growth life is determined as the stress corrosion crack growth life.

9. The method according to claim 1, It is characterized in that The fatigue crack growth life includes a low-cycle fatigue crack growth life. Based on the crack growth size set, the low-cycle corrosion crack growth life is obtained, including: Based on the target parameters of the monitoring component, the crack shape parameters of the monitoring component, the low-cycle fatigue crack growth test constant of the material of the monitoring component, and the maximum stress of the crack part of the monitoring component under the set working condition of the nuclear power steam turbine, the low-cycle fatigue crack growth life of at least one stage of the set working condition of the nuclear power steam turbine is obtained; wherein, The target parameters are any two parameters in the set of the initial crack size of the monitored component and the crack extension size.

10. The method according to claim 5, It is characterized in that The fatigue crack growth life includes a high cycle fatigue crack growth life, and based on the crack growth size set, obtaining the high cycle fatigue crack growth life includes: The high cycle fatigue crack growth life is obtained based on the high cycle fatigue crack growth size threshold value, the high cycle fatigue critical crack size, the crack shape parameters of the monitoring component, the high cycle fatigue crack growth test constant of the material of the monitoring component, and the high cycle fatigue stress range of the crack part of the monitoring component under the steady-state condition of the nuclear power steam turbine under load operation.

11. The method according to claim 1, It is characterized in that The step of obtaining the crack growth calendar life of the monitoring component based on the long-life monitoring data required by the monitoring component comprises: Based on the long-life monitoring data required by the monitoring component, obtain the multi-stage calendar life of the monitoring component; The crack growth calendar life is obtained based on the multi-stage calendar life of the monitored component.

12. The method according to claim 9, It is characterized in that The step of obtaining the crack growth calendar life based on the multi-stage calendar life of the monitoring component comprises: The sum of the multi-stage calendar lives of the monitored component is determined as the crack growth calendar life.

13. The method according to any one of claims 1 to 12, It is characterized in that The step of performing crack growth life safety monitoring on the monitoring component based on the crack growth calendar life includes: If the nuclear power steam turbine is in the design stage, obtaining a crack extension life safety monitoring criterion value of the monitoring component; If the crack growth calendar life is less than the crack growth life safety monitoring criterion value, it is determined that the crack growth calendar life does not meet the monitoring qualification condition, so as to perform crack growth life safety monitoring on the monitoring component; or, If the crack growth calendar life is greater than or equal to the crack growth life safety monitoring criterion value, it is determined that the crack growth calendar life meets the monitoring qualification condition, so as to perform crack growth life safety monitoring on the monitoring component.

14. The method according to claim 13, It is characterized in that The method further comprises: If the crack growth calendar life does not meet the monitoring qualification condition, obtaining abnormal data of the monitoring component in the design stage; The abnormal data of the monitoring component in the design phase is optimized and improved, and the process of obtaining the crack growth calendar life is returned to be executed until the obtained crack growth calendar life meets the monitoring qualification condition.

15. A stress corrosion and fatigue long-life monitoring device for nuclear power steam turbines. It is characterized in that include: An acquisition module is used to acquire stress calculation basic data and material test basic data of a monitoring component of a nuclear power steam turbine, and based on the stress calculation basic data and the material test basic data, acquire long-life monitoring data required by the monitoring component, wherein the long-life monitoring data includes stress corrosion crack growth life and fatigue crack growth life, and the fatigue crack growth life includes at least one of low-cycle fatigue crack growth life and high-cycle fatigue crack growth life. Based on the stress calculation basic data and the material test basic data, acquiring the stress corrosion crack growth life includes: Determining a stress corrosion crack extension size threshold value of the monitoring component based on the crack shape parameters of the monitoring component, the stress corrosion fracture toughness of the material of the monitoring component, and the maximum stress at the crack site of the monitoring component under the steady-state condition of the nuclear power steam turbine under load operation; Determining a low cycle fatigue critical crack size of the monitoring component under the set operating condition of the nuclear power steam turbine based on a crack shape parameter of the monitoring component, a fracture toughness of a material of the monitoring component, and a maximum stress at a crack site of the monitoring component under the set operating condition of the nuclear power steam turbine; Among them, the difference between the low-cycle fatigue critical crack size and the stress corrosion crack growth size threshold value of the monitoring component based on the set working conditions of the nuclear power steam turbine, and the ratio of the annual average stress corrosion crack growth rate test value of the material of the monitoring component, the stress corrosion crack growth life is obtained; A monitoring module is used to obtain the crack growth calendar life of the monitoring component based on the long-life monitoring data required by the monitoring component, and to perform crack growth life safety monitoring on the monitoring component based on the crack growth calendar life.

16. The device according to claim 15, It is characterized in that The acquisition module is further used for: Acquire a mapping relationship between the stress calculation basic data, the material test basic data and the monitoring component; Based on the mapping relationship, the stress calculation basic data and the material test basic data of the monitoring component are acquired.

17. The device according to claim 15, It is characterized in that The acquisition module is further used for: If the monitored component is a rotor, determining the long-life monitoring data required for the rotor includes the stress corrosion crack growth life, the low cycle fatigue crack growth life and the high cycle fatigue crack growth life; If the monitored component is a cylinder, the long-life monitoring data required for determining the cylinder includes the stress corrosion crack growth life and the low cycle fatigue crack growth life.

18. The device according to claim 15, It is characterized in that The acquisition module is further used for: Determining a set of crack extension sizes of the monitoring component based on the stress calculation basic data and the material test basic data; Based on the crack growth size set, long-life monitoring data required by the monitoring component is obtained.

19. The device according to claim 15, It is characterized in that The monitoring module is also used for: Based on the long-life monitoring data required by the monitoring component, obtain the multi-stage calendar life of the monitoring component; The crack growth calendar life is obtained based on the multi-stage calendar life of the monitored component.

20. The device according to any one of claims 15 to 19, It is characterized in that The monitoring module is also used for: If the nuclear power steam turbine is in the design stage, obtaining a crack extension life safety monitoring criterion value of the monitoring component; If the crack growth calendar life is less than the crack growth life safety monitoring criterion value, it is determined that the crack growth calendar life does not meet the monitoring qualification condition, so as to perform crack growth life safety monitoring on the monitoring component; or, If the crack growth calendar life is greater than or equal to the crack growth life safety monitoring criterion value, it is determined that the crack growth calendar life meets the monitoring qualification condition, so as to perform crack growth life safety monitoring on the monitoring component.

21. The device according to claim 20, It is characterized in that The monitoring module is also used for: If the crack growth calendar life does not meet the monitoring qualification condition, obtaining abnormal data of the monitoring component in the design stage; The abnormal data of the monitoring component in the design phase is optimized and improved, and the process of obtaining the crack growth calendar life is returned to be executed until the obtained crack growth calendar life meets the monitoring qualification condition.

22. An electronic device, It is characterized in that include: A memory, a processor, and a computer program stored in the memory and executable on the processor, wherein when the processor executes the program, a method for monitoring the long life of a nuclear power steam turbine due to stress corrosion and fatigue is implemented as described in any one of claims 1 to 14.

23. The electronic device according to claim 22, It is characterized in that Also includes: A wireless communication component is connected to the nuclear power steam turbine, and data is transmitted between the electronic device and the nuclear power steam turbine via the wireless communication component.

24. The electronic device according to claim 22, It is characterized in that The memory is used to store the crack growth calendar life of the monitoring component of the nuclear power steam turbine; The processor is used to obtain a crack growth life safety monitoring instruction, obtain the crack growth calendar life of a target monitoring component of the nuclear power steam turbine to be monitored from the memory based on the crack growth life safety monitoring instruction, and perform crack growth life safety monitoring on the target monitoring component based on the crack growth calendar life of the target monitoring component.

25. The electronic device according to claim 24, It is characterized in that Also includes: a remote client, the remote client being connected to the processor; The remote client is used to send the crack extension life safety monitoring instruction to the processor and receive the monitoring result fed back by the processor.

26. A computer-readable storage medium having a computer program stored thereon, It is characterized in that When the program is executed by a processor, the stress corrosion and fatigue long-life monitoring method for a nuclear power steam turbine as described in any one of claims 1 to 14 is implemented.

27. A monitoring platform suitable for nuclear power steam turbines, It is characterized in that include: A stress corrosion and fatigue long-life monitoring device for a nuclear power steam turbine as described in any one of claims 15 to 21; or an electronic device as described in any one of claims 22 to 25; or a computer-readable storage medium as described in claim 26.