Optical systems including light-controlling films and Fresnel lenses

By combining a linear Fresnel lens and an optical absorption layer in the optical system, the problems of bright bands and light redirection in light control films on curved displays were solved, resulting in better optical performance.

CN117255958BActive Publication Date: 2026-11-103M INNOVATIVE PROPERTIES CO
View PDF 22 Cites 0 Cited by

Patent Information

Application Number
CN202280032679.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2021-05-10
Filing Date
2022-04-14
Publication Date
2026-11-10
Estimated Expiration
2042-04-14

AI Technical Summary

Technical Problem

When existing light control films are used on curved displays, they are difficult to effectively reduce bright bands and undesirable light redirection phenomena at higher viewing angles. At the same time, reflection of ambient light may cause adverse effects such as rainbow patterns.

Method used

A combination design of linear Fresnel lenses and optical absorption layers is adopted. The optical absorption layer is set on the sidewall of the Fresnel element and combined with reflection mitigation elements, such as structured surfaces or optical diffuser layers, to reduce light redirection and reflection effects.

Benefits of technology

It effectively reduces bright bands and light redirection at higher viewing angles, lowers ambient light reflectivity, and improves the visual effect of the display.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117255958B_ABST
    Figure CN117255958B_ABST
Patent Text Reader

Abstract

The present invention provides an optical system comprising an optical film curved about a first axis; and a light-controlling film curved about the first axis and extending substantially coexisting with the optical film. The optical film includes a first layer comprising a microstructured first main surface defining a linear Fresnel lens including a plurality of Fresnel elements extending along the first axis. The first main surface of the optical film faces the light-controlling film. The light-controlling film includes a plurality of spaced-apart optical absorption regions extending along the first axis and in a direction substantially perpendicular to the main surface of the light-controlling film. The optical film, or at least one of at least one layer disposed between the optical film and the light-controlling film, includes at least one reflection mitigation element.
Need to check novelty before this filing date? Find Prior Art

Description

Background Technology

[0001] The light-controlled film may include alternating optical transmission regions and optical absorption regions, and can be used to adjust the orientation of light transmitted through the film.

[0002] The display surface can be curved. Summary of the Invention

[0003] In some aspects, this disclosure provides an optical system comprising a light source; an optical film curved about a first axis; and a light-controlling film curved about the first axis and extending substantially coexisting with the optical film. The optical film includes a first layer comprising a microstructured first main surface, wherein the microstructured first main surface defines a linear Fresnel lens including a plurality of Fresnel elements extending along the first axis. The light-controlling film is disposed between the light source and the optical film. The first main surface of the optical film faces the light-controlling film. The light-controlling film includes a plurality of spaced-apart optical absorption regions extending along the first axis and in a direction substantially perpendicular to the main surface of the light-controlling film. At least one of the optical film or at least one layer disposed between the optical film and the light-controlling film includes at least one reflection mitigation element.

[0004] In some aspects, this disclosure provides an optical system comprising an optical film curved about a first axis; and a light-controlling film disposed adjacent to the optical film. The optical film includes a first layer comprising a microstructured first main surface, wherein the microstructured first main surface defines a linear Fresnel lens comprising a plurality of Fresnel elements extending along the first axis. Each Fresnel element includes an optical facet and a sidewall intersecting the optical facet at a ridge of the Fresnel element. For each Fresnel element, at least a majority of the Fresnel elements, an optical absorption layer is disposed on and substantially covers the sidewall. The optical absorption layer has an average thickness t, where 100 nm < t < 1 micrometer. The light-controlling film is curved about the first axis and extends substantially co-located with the optical film. The first main surface of the optical film faces the light-controlling film. The light-controlling film includes a plurality of spaced-apart optical absorption regions extending along the first axis and in a direction substantially perpendicular to the main surface of the light-controlling film. The optical film, or at least one of the layers disposed between the optical film and the light control film, includes at least one reflection mitigation element.

[0005] In some aspects, the present invention provides an optical film comprising: a first layer having a microstructured first main surface, wherein the microstructured first main surface defines a linear Fresnel lens comprising a plurality of Fresnel elements; and a second layer disposed on the first main surface of the first layer and having a main surface facing and substantially conforming to the first main surface of the first layer. The second layer bonds the optical film to a photocontrol film. In some embodiments, the second layer has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm. The optical film includes at least one reflection mitigation element.

[0006] These and other aspects will become apparent from the detailed description that follows. However, in no way should this brief overview be construed as limiting the subject matter for which protection may be claimed. Attached Figure Description

[0007] Figures 1 to 3 It is a schematic cross-sectional view of an optical system according to some implementation schemes.

[0008] Figures 4 to 6 It is a schematic cross-sectional view of an optical stack including optical films and light control films according to some implementation schemes.

[0009] Figures 7 to 8 This is a schematic cross-sectional view of an optical system that schematically shows the shape of the optical film and the light control film according to some embodiments.

[0010] Figure 9 This is a schematic top view of a linear Fresnel lens according to some implementation schemes.

[0011] Figure 10 This is a schematic top view of a light-controlled film based on some implementation schemes.

[0012] Figure 11 This is a schematic cross-sectional view of an optical film comprising multiple Fresnel elements according to some embodiments.

[0013] Figures 12 to 17 This is a schematic cross-sectional view of a portion of an optical film comprising multiple Fresnel elements, according to some embodiments.

[0014] Figures 18 to 20 This is a schematic cross-sectional view of a Fresnel element according to some implementation schemes.

[0015] Figure 21 This is a schematic diagram of the average deviation surface roughness based on some implementation schemes.

[0016] Figures 22 to 24 It is a graph showing the relative brightness versus position from various perspectives based on some implementation schemes.

[0017] Figure 25 It is a schematic cross-sectional view of the structured layers according to some implementation schemes.

[0018] Figure 26 This is a schematic cross-sectional view of an optical diffuser layer according to some implementation schemes.

[0019] Figure 27 It is a schematic cross-sectional view of a structured surface or interface according to some implementation scheme.

[0020] Figures 28 to 36 It is a schematic cross-sectional view of an optical system including various reflection mitigation elements according to some implementation schemes. Detailed Implementation

[0021] Reference is made in the following description to the accompanying drawings, which form part of the invention and illustrate various embodiments by way of example. The drawings are not necessarily drawn to scale. It should be understood that other embodiments may be conceived and practiced without departing from the scope or spirit of this specification. Therefore, the following detailed description should not be considered limiting.

[0022] A light-controlling film, also known as a collimating film or privacy filter, can be used to adjust the orientation of light transmitted through the film. The light-controlling film can be placed on a curved display, for example, to filter the display's light output. However, it is generally desirable to alter the directionality of the transmitted light (e.g., to direct the light primarily toward the observer rather than primarily along the normal to the display surface) compared to using a conventional light-controlling film placed on a curved display surface. This can be achieved by altering the tilt of the light-controlling film's grid (e.g., the light-absorbing area), for example, as described in International Application Publication No. WO 2020 / 261027 (Liu et al.). Alternatively, a linear Fresnel lens can be placed on a conventional light-controlling film to alter the directionality of the transmitted light. However, it has been found that this can result in undesirable bright bands at higher viewing angles. According to some embodiments of this specification, it has been found that a Fresnel lens can be positioned in the optical system such that the Fresnel element faces the light-controlling film, and this can reduce or substantially eliminate bright bands at higher viewing angles.

[0023] Furthermore, it has been found that, according to some embodiments, an optical absorption layer can be disposed on the sidewalls of a Fresnel element to reduce undesirable light redirection caused by the sidewalls. It has been found that using a thin optical absorption layer reduces the undesirable effects of the optical absorption layer (e.g., blocking light that is expected to be transmitted incident on the edges of the layer). When the optical absorption layer is thin, it preferably has a relatively high extinction coefficient to effectively absorb light. In some cases, a high extinction coefficient can interact with the sidewalls to create a reflective, metal-like interface. It has been found that adding a coating layer (e.g., a layer with an extinction coefficient less than that of the optical absorption layer but greater than that of the sidewall material) between the high extinction coefficient absorption layer and the sidewalls can reduce reflectivity, thereby reducing undesirable light redirection caused by the sidewalls.

[0024] Furthermore, it has been found that, according to some embodiments, in certain situations, the reflection of ambient light can be unpleasant, partly due to the dispersion of one or more layers of the optical film, which can lead to color separation (e.g., rainbow patterns) in the reflected light. For example, the material used to form the Fresnel element in the optical film may have a higher refractive index for blue wavelengths than for red wavelengths. However, it has been found that, according to some embodiments, including one or more reflection mitigation elements can reduce unpleasant effects. As used herein, a "reflection mitigation element" is any element that reduces undesirable reflection effects. According to some embodiments, a reflection mitigation element may be diffuse, such that the reflected light is less specularly reflected and therefore less unpleasant in some cases, and / or a reflection mitigation element may be antireflective to reduce the overall level of reflection. Suitable reflection mitigation elements may include, for example, one or more structured (e.g., microstructured) surfaces or interfaces, optically diffused layers (e.g., beads or particles dispersed in an adhesive), or antireflective coatings that may be disposed at surfaces or interfaces.

[0025] Figures 1 to 3These are schematic cross-sectional views of optical systems 100, 200, and 300, respectively. Optical systems 100, 200, and 300 include an optical film 110 bent about a first axis (z-axis) and a light-controlling film 120 bent about the first axis. The light-controlling film 120 may substantially extend co-exist with the optical film 110 (e.g., at least about 60%, or at least about 80%, or at least about 90% of the area of ​​each of the light-controlling film 120 and the optical film 110 may co-exist with each other). The optical film 110 includes a first layer 191, which includes a microstructured first main surface 112. The optical film 110 may also include a substrate 164, wherein the first layer 191 is disposed on the substrate 164, and wherein the first main surface 112 of the first layer 191 faces away from the substrate 164. The optical film may include a second main surface 114 opposite to the first main surface 112, wherein the second main surface 114 may be the main surface of the substrate 164 facing away from the first layer 191. The microstructured first primary surface 112 defines a linear Fresnel lens 111, which includes a plurality of Fresnel elements 115 extending longitudinally along a first axis. A light-controlling film 120 may be disposed close to the optical film 110, wherein the first primary surface 112 of the optical film 110 faces the light-controlling film 120. In some embodiments, the optical system includes a light source 130. The light-controlling film 120 may be disposed between the light source 130 and the optical film 110, wherein the first primary surface 112 of the optical film 110 faces the light-controlling film 120. The light-controlling film 120 includes a plurality of alternating optically transmitting regions 122 and optically absorbing regions 124 extending longitudinally along a first axis, such that in a cross-section orthogonal to the first axis (xy cross-section), for at least most of the optically transmitting regions 122, the center line 126 between adjacent optically absorbing regions is substantially perpendicular to the main surfaces 128 and / or 129 of the light-controlling film 120 (e.g., within 20 degrees, 10 degrees, 5 degrees, 3 degrees, or 2 degrees of the normal). Alternatively or additionally, the optically absorbing regions 124 may be described as extending along the first axis (z-axis) and in a direction substantially perpendicular to the main surface of the light-controlling film (e.g., along a direction parallel to the center line 126). The Fresnel lens 111 may be configured such that light 866 emitted from the light source 130 perpendicular to the light source emitting surface is redirected by the Fresnel lens to substantially the same redirection direction (y-direction).

[0026] As further described elsewhere herein, optical systems 100, 200, and 300 may include at least one reflection mitigation element. The at least one reflection mitigation element may be configured to reduce specular reflection and may substantially extend with the optical film. The at least one reflection mitigation element may include one or more structured (e.g., microstructured) surfaces or interfaces, optical diffuser layers (e.g., volume diffusers that may include beads dispersed in an adhesive), or anti-reflection coatings. At least one of (i) the optical film or (ii) at least one layer disposed between the optical film and the light-control film may include at least one reflection mitigation element. For example, optical film 110 may include at least one reflection mitigation element and / or a layer disposed on the side of light-control film 120 facing optical film 110 may include at least one reflection mitigation element. In some embodiments, at least one reflection mitigation element includes a plurality of reflection mitigation elements, wherein the optical film includes at least a first reflection mitigation element, and at least one layer disposed between the optical film and the light-control film includes at least a different second reflection mitigation element. Microstructures that can be used for any microstructured surface or interface of a reflection mitigation element include, for example, random diffuse microstructures, engineered pseudo-random (appearing random but made using deterministic processes) diffuse microstructures, and microstructures arranged in repeating patterns (e.g., quarter-wave / interference and / or anti-reflection microstructures).

[0027] Microstructured surfaces typically include microstructures (e.g., Fresnel element 115 can be a microstructure), wherein the microstructure is a structure having at least two orthogonal dimensions, such as a width and height less than 1 mm and greater than 100 nm. The microstructures can be formed in a polymer layer. The polymer layer is a layer comprising a continuous phase of an organic polymer. For example, the polymer layer may also comprise inorganic nanoparticles dispersed within the continuous phase of the organic polymer. Polymer microstructured layers can be formed on a substrate using casting and curing processes known in the art (see, for example, U.S. Patent Application Publication No. 2006 / 0114569 (Capaldo et al.) and U.S. Patent Nos. 5,175,030 (Lu et al.) and 5,183,597 (Lu)). Other methods for preparing polymer structured layers include extrusion, machining, and embossing. Any suitable material can be used. For example, acrylates (e.g., polymethyl methacrylate) can be cast and cured onto a polyester (e.g., polyethylene terephthalate) substrate. Acrylates can be incorporated with monomers containing nitrogen or bromine, for example, to increase their refractive index. In some embodiments, high-refractive-index nanoparticles may be included to increase the refractive index.

[0028] The light control film 120 can be any suitable light control film, including those described below: for example, U.S. Patent Nos. 8,213,082 (Gaides et al.); 9,335,449 (Gaides et al.); and 9,063,284 (Jones et al.), and those described below: for example, International Patent Application Publication No. WO 2019 / 118685 (Schmidt et al.); and WO 2020 / 026139 (Schmidt et al.).

[0029] In some embodiments (e.g., as shown for optical system 100), the light source 130 is or includes an organic light-emitting diode (OLED) display 132 bent around a first axis. The display 132 may alternatively be another type of emitting display, such as a microLED display. In some embodiments (e.g., as shown for optical systems 200, 300), the light source 130 includes a backlight 134. In some embodiments, the backlight 134 includes a light guide 136 bent around a first axis. In some embodiments, the light source 130 also includes one or more light-emitting elements 135 (e.g., light-emitting diodes). For example, the backlight 134 may be a direct-lit backlight or an edge-lit backlight. In some embodiments (e.g., as shown for optical system 200), the optical system may include a display panel 139 disposed between the backlight 134 and a light-control film 120. In some embodiments (e.g., as shown for optical system 300), the optical system may include a display panel 139, wherein an optical film 110 is disposed between the display panel 139 and the light-control film 120.

[0030] In some embodiments, the air gap 178 separates at least a majority of the first main surface 112 of the optical film 110 from the light control film 120. For example, the air gap can be provided by not bonding the optical film 110 and the light control film 120 together, by bonding the films together only at one or more edges, or by attaching the films together using elongated spacer members.

[0031] Figure 4This is a schematic cross-sectional view of an optical system or part of an optical system including an optical stack 400, which includes an optical film 110 and a light-controlling film 120. In some embodiments, the optical film 110 and the light-controlling film 120 are adhesively bonded to each other (e.g., with tape 176 or 177) along at least one edge 171 or 172 of the optical film 110 and respectively corresponding edges 181 or 282 of the light-controlling film 120. In some embodiments, the optical film 110 and the light-controlling film 120 are adhesively bonded to each other along at least two edges 171 and 172 of the optical film 110 and respectively corresponding edges 181 and 282 of the light-controlling film 120. Adhesive bonding along the edges should be understood to include applying tape close to the edge along at least a portion (e.g., at least a majority) of the edge length. One or more reflection mitigation elements may be disposed on the main surface of the light-controlling film 120 facing the optical film 110, as further described elsewhere herein. For example, a structured layer (see example...) may be... Figure 25 ) and / or anti-reflective coatings (e.g., Figures 34 to 35 An antireflective coating 744, schematically shown, is applied (e.g., via vapor deposition) to the main surface of the light control film 120 facing the optical film 110. The optical system in this case can be described as including at least one reflection mitigation element disposed between the optical film 110 and the light control film 120.

[0032] Figure 5 This is a schematic cross-sectional view of an optical system or part of an optical system including an optical stack 500, which includes an optical film 210 and a light-controlling film 120. The optical film 210 may correspond to the optical film 110, except that the first main surface 212 of the optical film 210 includes a plurality of elongated spacer members 142. In some embodiments, the first main surface 212 of the optical film 210 includes a plurality of elongated spacer members 142 extending toward the light-controlling film 120 and received by an adhesive layer 144 disposed on the light-controlling film 120. The elongated spacer members 142 may be formed together with a Fresnel element 115, or may be deposited after the Fresnel element 115 has been formed. The elongated spacer members 142 may also be referred to as an optical decoupling structure and may have any of the geometries of an optical decoupling structure described, for example, in International Application Publication No. WO2019 / 135190 (Pham et al.). Layer 144 may include one or more reflection mitigation elements as further described elsewhere herein (e.g., layer 144 may include beads dispersed in the adhesive, such as...). Figure 26 (Illustrated schematically). In this case... Figure 5 The optical system can be described as including at least one reflection mitigation element (layer 144) disposed between the optical film 110 and the light control film 120.

[0033] Figure 6This is a schematic cross-sectional view of an optical system or part thereof including an optical stack 600, which includes an optical film 110 and a light-controlling film 120. In some embodiments, the optical film 110 includes a first layer 191 disposed on a substrate 164, wherein the first layer 191 includes a microstructured first main surface 112. The optical system or optical stack 600 also includes a second layer 148 (e.g., a low-refractive-index layer) disposed on and in contact with at least a majority of the first main surface 112 of the optical film 110, and an optional third layer 144 (e.g., an optical adhesive) disposed between the second layer 148 and the light-controlling film 120. The third layer 144 may be an optical adhesive that bonds the second layer 148 to the light-controlling film 120. The main surface 149 of the second layer 148 facing the first main surface 112 may be substantially conformable to the first main surface 112 (e.g., nominally conformable to or conformable to a small variation compared to the height H of the Fresnel element 115 (e.g., less than about 20%, or less than about 10%, or less than about 5%)). The main surface of the second layer 149 opposite to the main surface 149 may be substantially unstructured or have a structure substantially different from that of the main surface 149. In some embodiments, the third layer includes a structured layer bonded to the photocontrol film, and wherein the second layer includes an adhesive bonded to the first main surface of the first layer and the structured main surface of the structured layer. For at least one wavelength in the range of about 400 nm to about 700 nm, the second layer may have a lower refractive index than the first layer. The second layer 148 may be considered as a layer of the optical film 110. In this case, the third layer 144 may also be considered as a layer of the optical film 110. Alternatively, the second layer 148 and the third layer 144 may be considered to be disposed between the optical film 110 (including layers 191 and 164) and the light control film 120. In some embodiments, the second layer 148 has a refractive index of no more than 1.45, or no more than 1.43, or no more than 1.42, or no more than 1.41, or no more than 1.4, or no more than 1.35, or no more than 1.25, or no more than 1.2 for at least one wavelength in the range of about 400 nm to about 700 nm. For example, the refractive index of the low refractive index layer 148 may be in the range of, for example, 1.05 to 1.45, or in the range of 1.1 to 1.35, or in the range of 1.1 to 1.25, or in the range of 1.05 to 1.2, or in the range of 1.35 to 1.43, or in the range of 1.35 to 1.42. The low refractive index layer 148 may be a nanoporous polymer layer as described in U.S. Patent 8,808,811 (Kolb et al.). Typically, the refractive index of the nanoporous polymer layer can be adjusted by appropriately selecting the volume of the nanopores (having at least two orthogonal sizes less than one micrometer) included in the layer. In some embodiments, the low refractive index layer 148 is methyl silicone.In some embodiments, the low refractive index layer 148 is an adhesive (e.g., silicone adhesive), and the adhesive layer 144 is omitted. For example, a METRICON 2010 prism coupler (METRICON Corporation Inc., Pennington, NJ) can be used to measure the refractive index. The refractive index can be determined, for example, according to the ASTM D542-14 test standard.

[0034] For at least one wavelength in the range of about 400 nm to about 700 nm (e.g., at least one of about 532 nm, about 550 nm, or about 633 nm), the optical film 110 or the first layer 191 of the optical film 110 including the Fresnel element 115 may have a refractive index greater than 1.5, or greater than 1.6, or greater than 1.7. The refractive index may be, for example, up to about 1.9. In some embodiments, the refractive index of the first layer 191 at about 420 nm is greater than the refractive index of the first layer 191 at about 680 nm, for example, by at least about 0.008, or at least about 0.01, or at least about 0.012, or at least about 0.014, or at least about 0.016, and in some embodiments, up to about 0.05, or up to about 0.04, or up to about 0.03.

[0035] Any of layers 164, 191, and 148 may include reflection mitigation elements (e.g., beads or particles in an adhesive) as further described elsewhere herein. The third layer 144 may also or alternatively include reflection mitigation elements (e.g., when the third layer 144 has a refractive index closer to that of the second layer 148 than that of the light-control film 120). The second primary surface 114 of the optical film 110, and / or the interface 222 between the first layer 148 and the substrate 164, and / or the interface 223 between the first layer 191 and the second layer 148, and / or the interface 226 between the second layer 148 and the third layer 144 may include reflection mitigation elements (e.g., structured surfaces or interfaces or anti-reflective coatings) as further described elsewhere herein. Alternatively or additionally, the interface 225 between the third layer 144 and the light-control film 120 may be structured or include an anti-reflective coating (e.g., when the third layer 144 has a refractive index closer to that of the second layer 148 than that of the light-control film 120). At least one reflection-reducing element may substantially coexist with the optical film 110. For example, the reflection-reducing element may be or include a plurality of beads substantially uniformly dispersed in a layer substantially coexisting with the optical film. In this case, the plurality of beads may be described as substantially coexisting with the optical film.

[0036] In some embodiments, the optical film 110 and the light control film 120 are substantially concentric. For example, the optical film 110 and the light control film 120 may have substantially similar shapes and may substantially extend together.

[0037] In some implementations, the optical system (e.g., 100, 200, or 300) is adapted to display an image 888 to an observer 870 (see example...). Figure 1 In a cross-section orthogonal to the first axis, the optical film 110 and the light-control film 120 each bulge towards the observer 870. The optical film 110 and the light-control film 120 may optionally have, for example... Figures 7 to 8 Different shapes are schematically shown in the diagram. Figure 7 This is a schematic cross-sectional view of an optical system 700, which includes an optical film 810 (e.g., corresponding to optical film 110) and a light control film 820 (e.g., corresponding to light control film 120) and is adapted to display an image 888 to an observer 870, wherein in a cross-section orthogonal to a first axis (z-axis), the optical film 810 and the light control film 820 are each recessed toward the observer 870. Figure 8 This is a schematic cross-sectional view of an optical system 800, which includes an optical film 910 (e.g., corresponding to optical film 110) and a light control film 920 (e.g., corresponding to light control film 120), and is adapted to display an image 888 to an observer 870, wherein in a cross-section orthogonal to a first axis, a first portion (910a and 920a, respectively) of each of the optical film 910 and the light control film 920 is recessed toward the observer 870, and a second portion (910b and 920b, respectively) of each of the optical film 910 and the light control film 920 protrudes toward the observer 870.

[0038] exist Figures 1 to 10 In the schematically illustrated embodiments, the Fresnel elements of the optical film and / or the optical transmission and absorption regions of the light-controlled film may extend along a first axis (z-axis). In some embodiments, the first main surface 112 of the optical film 110 defines a linear Fresnel lens 111, which includes a Fresnel element 115 extending longitudinally along the first axis (z-axis). Figure 9 This is a schematic top view (view facing the first main surface 112) of a linear Fresnel lens 111 when the optical film 110 is laid flat, according to some embodiments. Figure 10 This is a schematic top view of the light control film 120 when it is laid flat, according to some embodiments. In some embodiments, the light control film 120 includes a plurality of alternating optical transmission regions 122 and optical absorption regions 124 extending longitudinally along a first axis (z-axis).

[0039] In some embodiments, each Fresnel element 115 of the optical film 110 includes an optical facet 117 and a sidewall 118 intersecting the optical facet 117 at a ridge 119 of the Fresnel element. In some embodiments, at least a majority of each Fresnel element 115 includes one or more of the following: at least a partial coating of an inorganic optically transparent layer (e.g., a conformal coating), an optical absorption layer, a first layer disposed between the optical absorption layer and the sidewall, and a second layer disposed on the optical absorption layer opposite the sidewall, wherein the optical absorption of the first layer may be less than that of the optical absorption layer, wherein the optical absorption of the second layer may be less than that of the optical absorption layer, and may be one or more of a protective layer or an antireflective layer.

[0040] Figure 11 This is a schematic cross-sectional view of an optical film 310, corresponding to optical film 110. Optical film 310 includes a first layer 491 disposed on a substrate 164. In some embodiments, each Fresnel element 115 includes an optical facet 117 and a sidewall 118 intersecting the optical facet 117 at a ridge 119 of the Fresnel element. In some embodiments, for at least a majority of each Fresnel element, an optical absorption layer 152 is disposed on and substantially covers the sidewall 118. In some embodiments, a plurality of Fresnel elements include a plurality of polymeric Fresnel elements 334 at least partially coated (e.g., conformally coated) with an inorganic optically transparent layer 157 (e.g., see...). Figure 13 In some embodiments, for at least most of the Fresnel elements, the optical absorption layer 152 is disposed on and substantially covers the inorganic optical transparency layer 157 disposed on the sidewall 118.

[0041] As further described elsewhere herein, inorganic optically transparent layers can be used as etching barrier layers during the removal of optically absorbing layers and / or other layers from optical facets. Suitable materials for inorganic optically transparent layers include a-Si, SiOx, SiAlOx, SiCyOx, TiO2, and AlOx. The layer can be thin enough that, for example, greater than 60% of vertically incident visible light is transmitted through it. A layer can be considered optically transparent if its average optical transmittance (for unpolarized light, the unweighted average over wavelength) to visible light (wavelengths in the range of about 400 nm to about 700 nm) incident vertically onto it in air is at least 60%. In some embodiments, the average optical transmittance of the inorganic optically transparent layer is greater than 60%, or greater than 70%, or greater than 80%, or greater than 85%, or greater than 90%.

[0042] In some embodiments, the optical absorbing layer 152 has an average thickness t, where 100 nm < t < 2 micrometers or 100 nm < t < 1 micrometer. In some embodiments, the average thickness t is less than 500 nm. In some embodiments, for each Fresnel element 115a of at least a majority of the Fresnel elements 115, the sidewall 118 of the Fresnel element 115a has a height H from the bottom 185 of the adjacent Fresnel element 115b to the ridge 119 of the Fresnel element 115a, where H / t > 10, or H / t > 15, or H / t > 18, or H / t > 20.

[0043] In some embodiments (e.g., the optical film 110, 210 or 310), for each Fresnel element of at least a majority of the Fresnel elements, the sidewall 118 of the Fresnel element is substantially perpendicular to the second major surface 114 (e.g., within 30 degrees, or within 20 degrees, or within 10 degrees, or within 5 degrees of the normal). In some embodiments, the optical film 110, 210 or 310 includes a substrate 164, wherein the plurality of Fresnel elements 115 are formed on the major surface 162 of the substrate 164. In some embodiments, for each Fresnel element of at least a majority of the Fresnel elements, the sidewall 118 of the Fresnel element is substantially perpendicular to the major surface 162 of the substrate 164. In some embodiments, the sidewall 118 forms an angle with the major surface 162, or with the major surface 114, or with the bottom of the Fresnel element that is in the range of 85 degrees to 90 degrees or in other ranges described elsewhere herein.

[0044] Figure 12is a schematic cross-sectional view of a portion of an optical film (e.g., corresponding to optical film 110, 210, or 310). In some embodiments, for each Fresnel element 115 in at least a majority of the Fresnel elements, the first layer 154 is disposed between the sidewall 118 and the optical absorbing layer 152. The first layer 154, which may be referred to as a cladding layer, can be included to reduce light reflection at the interface between the sidewall and the optical absorbing layer 152. In some embodiments, the first layer 154 has an extinction coefficient k1, and the optical absorbing layer 152 has an extinction coefficient k2. In some embodiments, k2>k1. In some embodiments, the extinction coefficient k0 of the plurality of Fresnel elements is less than 0.05. In some embodiments, k2>k1>k0. The extinction coefficient k0 can be understood as defining the extinction coefficient of the material at the first major surface 112 of the Fresnel element. In some embodiments, k2-k1 is greater than 0.05, 0.1, 0.15, or 0.2. In some embodiments, k2-k1 is less than 1, or less than 0.8, or less than 0.5. In some embodiments, k1-k0 is greater than 0.001, 0.005, or 0.01. In some embodiments, k1-k0 is less than 0.15, or less than 0.1, or less than 0.05. In some embodiments, k0 is less than 0.01, or less than 0.005, or less than 0.002. In some embodiments, k1 is in the range of 0.005 to 0.15, or 0.01 to 0.1. In some embodiments, k2 is in the range of 0.1 to 0.5, or 0.2 to 0.4. In some embodiments, k1<0.5 k2. In some embodiments, 0.005<k1<0.5 k2. Instead of or in addition to describing the first layer 154 and the optical absorbing layer 152 in terms of extinction coefficients, the layers can be described in terms of the concentration of the optical absorbing material as further described elsewhere herein.

[0045] In some embodiments, the optical absorbing layer 152 has a refractive index n1, and the first layer 154 has a refractive index n2, where |n1-n2| is less than 0.5, or less than 0.3, or less than 0.2, or less than 0.1.

[0046] The extinction coefficient can be expressed as the imaginary part of the complex refractive index, and the refractive index can be expressed as the real part of the complex refractive index. When no other wavelength is indicated, the extinction coefficient and the refractive index can be understood as being evaluated at a wavelength of 550 nm.

[0047] For example, the extinction coefficient k of a thin film coating can be determined, for example, by ellipsometry or spectroscopy. k can be expressed as αλ / (4π), where α is the absorption coefficient and λ is the wavelength. For a thin film coating on a transparent substrate, the absorptivity A can be measured as 100%–T–R using spectroscopy, where T is the transmittance and R is the reflectance. The measured A can be appropriately corrected for the substrate's A to obtain the A of the thin film itself. α can then be determined using the obtained A according to the equation α=-ln[(100%-A) / 100%] / h, where h is the thickness of the thin film coating; this formula for α is an approximation used when R is relatively small and A is relatively large. The thickness h can be measured, for example, by stylus profilometry or cross-sectional scanning electron microscopy.

[0048] The light-absorbing material used for the optical absorption layer 152 and / or the first layer 154 may be one or more of dyes, pigments, or particles (e.g., nanoparticles). Suitable light-absorbing materials include carbon black nanopigments and other nanopigments, such as those available under the trade name CAB-O-JET from Cabot Corporation (Boston, MA). Other suitable light-absorbing materials include those described in International Patent Application Publication No. WO 2019 / 118685 (Schmidt et al.).

[0049] In some embodiments, the first layer 154 has a concentration C1 of light-absorbing material 184, and the optical absorption layer 152 has a concentration C2 of light-absorbing material 182, wherein C2 > C1. In some embodiments, C1 < 0.7 C2, or C1 < 0.5 C2.

[0050] The concentration of the light-absorbing material (e.g., light-absorbing nanoparticles) in the optical absorption layer can be at least 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, or 50 wt% of the optical absorption layer. In some embodiments, the concentration of the light-absorbing material in the optical absorption layer is at least 55 wt%, 60 wt%, 65 wt%, 70 wt%, 75 wt%, 80 wt%, 85 wt%, 90 wt%, or 95 wt% of the optical absorption layer. In some embodiments, the concentration of the light-absorbing material in the optical absorption layer is 100 wt%. In some embodiments, the concentration of the light-absorbing material in the optical absorption layer is 30 wt%-100 wt% or 75 wt%-90 wt% of the optical absorption layer.

[0051] The concentration of the light-absorbing material in the first layer (coating) is preferably lower than that in the optical absorption layer. The concentration of the light-absorbing material in the first layer is typically at least 0.5 wt%, 1 wt%, 5 wt%, 10 wt%, 15 wt%, 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, or 45 wt%. In some embodiments, the concentration of the light-absorbing material in the first layer does not exceed 20 wt%, 25 wt%, 30 wt%, 35 wt%, 40 wt%, 45 wt%, 50 wt%, 55 wt%, 60 wt%, 70 wt%, or 75 wt%. In some embodiments, the concentration of the light-absorbing material in the first layer is 0.5 wt% to 50 wt% or 25 wt% to 45 wt%.

[0052] In some embodiments, the light-controlling film 120 is generally described in, for example, International Patent Application Publication No. WO 2019 / 118685 (Schmidt et al.). In some such embodiments, the optical absorption layer of the grating includes an optical absorption core layer and a cladding layer on each side of the optical absorption core layer. The optical absorption core layer may be as described with respect to optical absorption layer 152, and the cladding layer may be as described with respect to first layer 154. The use of the cladding layer reduces the reflectivity of the grating, thereby reducing high-angle light leakage and ghosting. A light-controlling film including a core layer and a cladding layer is described in International Patent Application No. IB2019 / 056489 (Schmidt et al.).

[0053] Figures 13 to 17 This is a schematic cross-sectional view of a portion of an optical film (e.g., corresponding to optical films 110, 210, or 310). In some embodiments, such as Figure 13 The diagram schematically illustrates, for example, that multiple Fresnel elements 115 include a microstructured polymer layer 333 conformally coated with an inorganic optically transparent layer 157. The inorganic optically transparent layer 157 may include opposing first main surfaces 167 and second main surfaces 166, wherein the second main surface 166 faces the polymer layer 333. The polymer layer 333 has a main surface 113 facing the substrate layer 164. In some embodiments, such as... Figure 14 As schematically shown, for example, for at least most of the Fresnel elements 115, an optical absorption layer 152 is disposed on and substantially covers an inorganic optically transparent layer 157 disposed on a sidewall 118. In some embodiments, such as Figure 15 As schematically shown, for example, for at least most of the Fresnel elements 115, a first layer 154 is disposed between the sidewall 118 and the optical absorption layer 152. In some embodiments, such as Figure 14 The diagram is schematically shown, for example, the first layer 154 is omitted. In some embodiments, such as... Figure 16As schematically shown, for example, for at least most of the Fresnel elements 115, a second layer 156 is disposed on the optical absorption layer 152 opposite to the sidewall 118 or opposite to the first layer 154. For example, the second layer 156 may be a protective layer and / or an anti-reflective layer. The second layer may be as generally described for the first layer 154 (e.g., having an average thickness and / or extinction coefficient and / or concentration of light-absorbing material within the range described for the first layer 154). The inorganic optically transparent layer 157 may optionally be omitted.

[0054] In some implementation schemes, such as Figure 17 The diagram schematically illustrates that, for example, the microstructured surface 168 is only partially coated with an inorganic optically transparent layer 157 (e.g., only on the sidewalls). For example, the inorganic optically transparent layer may be conformally coated onto the microstructured surface 168 and then subsequently removed from the optical facets (or at least partially removed). Figures 13 to 16 In any of the embodiments shown, the inorganic optically transparent layer 157 may optionally be removed from or partially removed from the optical facets (e.g., a thin layer may be retained). In some embodiments, the first main surface 112 of the optical film may include the main surface of the inorganic optically transparent layer 157 (e.g., the surface 167 of the plurality of sidewalls 118). In some embodiments, the Fresnel element 115 of the microstructured surface, which is at least partially coated, may include an optical facet as part of the microstructured surface 168 of the polymer layer 333, and may include sidewalls as part of the main surface of the inorganic optically transparent layer 157. Alternatively, the Fresnel element 115 may be considered to include optical facets and sidewalls that are part of the microstructured surface 168 of the polymer layer 333, and the inorganic optically transparent layer 157 may be considered to be a coating on the polymer microstructured sidewalls.

[0055] In some embodiments, the optical film includes a polymer layer 333 comprising a microstructured surface 168 at least partially coated with an inorganic optically transparent layer 157. The at least partially coated microstructured surface 177 (which may include optical facets 117 and the surface 167 of the inorganic optically transparent layer 157 on the sidewalls) includes a plurality of Fresnel elements 115. Each Fresnel element 115 includes an optical facet 117 and a sidewall 118 intersecting the optical facet 117 at a ridge 119 of the Fresnel element 115. The optical facet 117 and the sidewall 118 may define an angle therebetween. For at least a majority of each Fresnel element 115, an optical absorption layer 152 is disposed on and substantially covers the sidewall 118.

[0056] In some embodiments, the optical film includes a polymer layer 333, which includes a main surface 168 comprising a plurality of Fresnel elements. Each Fresnel element includes an optical facet (e.g., 117) and a sidewall (e.g., a portion of the main surface 168 facing the sidewall portion of the inorganic optically transparent layer 157), the sidewall intersecting the optical facet at a ridge of the Fresnel element. The optical facet and the sidewall may define an angle of inclination therebetween. For each Fresnel element in at least a majority of the Fresnel elements: the inorganic optically transparent layer 157 is disposed on and substantially covers the sidewall; and an optical absorption layer 152 is disposed on the inorganic optically transparent layer 157, opposite to the sidewall of the inorganic optically transparent layer 157, which substantially covers the sidewall of the inorganic optically transparent layer 157.

[0057] In some embodiments, the inorganic optically transparent layer 157 may be disposed on the sidewall along with other layers such as an optically absorbing layer. The inorganic optically transparent layer may be conformally coated onto the microstructured polymer layer, and the optically absorbing layer (and optionally other layers) may be conformally coated onto the inorganic optically transparent layer. The optically absorbing layer (and optionally other layers) may be removed from the optical facet in a first etching step, and then the inorganic optically transparent layer may be removed or partially removed from the optical facet in a second etching step. For example, the first and second etching steps may utilize different etchants (e.g., oxygen-only plasma for the first etching step and fluorinated or other halide gases for the second etching step) to remove the desired layers in the corresponding etching steps.

[0058] In some embodiments, for at least most of the Fresnel elements 115, the first layer 154 has an average thickness t1, and the optical absorption layer 152 has an average thickness t2. In some embodiments, t1 and t2 are each greater than 100 nm and less than 2 μm, or less than 1 μm, or less than 500 nm. In some embodiments, t1 and t2 are each less than 500 nm. In some embodiments, for at least most of the Fresnel elements 115, the sidewall 118 of the Fresnel element has a height H from the bottom of the adjacent Fresnel element to the ridge 119 of the Fresnel element. In some embodiments, H / t1 > 10, or H / t1 > 12, or H / t1 > 15, or H / t1 > 18, or H / t1 > 20. In some embodiments, H / t1 < 100. In some implementations, H / t2 > 10, or H / t2 > 12, or H / t2 > 15, or H / t2 > 18, or H / t2 > 20. In some implementations, H / t2 < 100. For example, in some implementations, H / t1 > 15 and H / t2 > 15.

[0059] In some implementations, the optical facet 117 is planar for each Fresnel element, at least in most of the Fresnel elements (e.g., as in a typical conventional Fresnel lens). Figure 18 This is a schematic diagram of a Fresnel element having a planar optical facet 217, wherein the sidewall 218 of the Fresnel element forms an angle φ with the bottom 285 of the Fresnel element. In other embodiments, the optical facet 117 is curved for at least a majority of each of the Fresnel elements 115. For example, the facet may be curved to adjust various optical properties, as described, for example, in U.S. Statutory Patent Registration No. H423 (Mohon et al.). For example, the optical facet 117 may be curved, such as... Figure 19 The curved optical facet 317 is schematically depicted (recessed toward the sidewall 218 and / or toward the bottom 285 and / or toward the main surface 114) (see, for example, see...). Figure 1 ), or as Figure 20 The curved optical facet 417 is schematically depicted (protruding toward the sidewall 218 and / or toward the bottom 285 and / or toward the main surface 114). Figures 18 to 20 The angle φ can be in the range of 80 to 90 degrees or 85 to 90 degrees. In some embodiments, for example, due to manufacturing limitations, φ is less than 90 degrees (e.g., 85 to 89.5 degrees).

[0060] Figure 21is a schematic diagram of the mean deviation surface roughness Ra of a surface 517, which may be the surface of an optical facet. The mean deviation surface roughness Ra is the average of the absolute values of the deviations of the surface height from the mean surface height (e.g., the average over the length of a cross-section through the facet, for example, a cross-section orthogonal to the length of the facet). In the case of a curved facet, the deviation of the surface height may be defined relative to a mean or nominal curved surface. In some embodiments, the optical facet 117 has a mean deviation surface roughness Ra of <250 nm for each Fresnel element in at least a majority of the Fresnel elements 115. In some embodiments, Ra is less than 200 nm, 150 nm, 100 nm, 70 nm, 50 nm, 30 nm, or 20 nm. In some embodiments, Ra is greater than 50 nm, 70 nm, 90 nm. For example, in some embodiments, 50 nm < Ra < 200 nm or 70 nm < Ra < 200 nm. For some applications, it is desirable for the optical facet 117 to be optically smooth (e.g., Ra < 50 nm). For other applications, a certain degree of surface roughness may be desired (e.g., 50 nm < Ra < 250 nm or 90 nm < Ra < 200 nm). For example, having a certain degree of surface roughness for anti-reflection may be useful, for providing (e.g., weak) optical diffusion and / or for improving adhesion. It has been found that depositing and removing the optical absorbing layer from slanted facets using the methods described in International Patent Application No. WO 2019 / 118685 (Schmidt et al.) results in a surface roughness higher than desired for many applications (e.g., Ra greater than 300 nm or greater than 400 nm), even though the same method applied to horizontal facets results in low surface roughness. However, it has been found that surface roughness (e.g., Ra) can be reduced (e.g., to less than 250 nm or less than 200 nm), for example, by carefully controlling the exposure time of the optical facets to plasma in a reactive ion etching process. Furthermore, it has been found that applying an inorganic optically transparent layer as an etch stop layer prior to applying the optical absorbing layer (and / or other layers) can further reduce surface roughness and can produce optically smooth optical facets (e.g., Ra < 50 nm), even with longer etching times. The root mean square surface roughness Rq may also be determined and may be in any of the ranges described for Ra.

[0061] In some embodiments, at least one reflection mitigation element includes at least one of a structured surface, an antireflective coating, or a volume diffuser, in addition to a microstructured first master surface. The structured surface may be an exposed surface (e.g., the outermost master surface exposed to air) or a surface at an interface. Furthermore, the microstructured first master surface may be antireflective or diffuse, as further described elsewhere herein. A volume diffuser (also referred to as a main diffuser) is a diffuser that causes optical diffusion through scattering within the volume of the diffuser. A surface diffuser is a diffuser in which optical diffusion occurs through scattering at the master surface of the diffuser. In addition to volume diffusion, a volume diffuser may also employ surface diffusion (e.g., the volume diffuser may have a microstructured master surface for additional diffusion). In some embodiments, the volume diffuser includes a plurality of beads dispersed in an adhesive.

[0062] Surface roughness can be determined by measuring the surface profile, for example, by atomic force microscopy (AFM), stylus profilometry, or optical profilometry. For small surface roughness (e.g., less than 50 nm), AFM is generally preferred.

[0063] An inorganic optically transparent layer, a first layer (e.g., a coating layer), an optically absorbing layer, and / or a second layer (e.g., a protective layer) (e.g., as a conformal coating over the entire structured surface) can be deposited using any suitable deposition technique. Various coating methods that can be used include, for example, layer-by-layer (LbL) coating, chemical vapor deposition (CVD), sputtering, reactive sputtering, and atomic layer deposition (ALD). Subsequently, at least some of the deposited layers (e.g., all layers, or all layers except the optional inorganic optically transparent layer) can be substantially removed from the optical facet (e.g., to the extent that any material removed from at least some of the remaining deposited layers on the optical facet does not significantly affect the optical performance).

[0064] In some embodiments, at least one of the first layer and the optical absorption layer comprises at least two bilayers deposited by a process commonly referred to as a “layer-by-layer self-assembly process.” This process is typically used for the electrostatic assembly of membranes or coatings of polymeric electrolytes with opposite charges, but other functionalities such as hydrogen bond donors / acceptors, metal ion / ligands, and covalent moieties can be driving forces for membrane assembly. Some examples of suitable processes include those described in U.S. Patent Nos. 8,234,998 (Krogman et al.) and 8,313,798 (Nogueira et al.); U.S. Patent Application Publication No. 2011 / 0064936 (Hammond-Cunningham et al.); and International Patent Application No. WO 2019 / 118685 (Schmidt et al.). For example, layer-by-layer dip coating can be performed using a StratoSequence VI dip coating robot (nanoStrata Inc., Tallahassee, FL).

[0065] In some embodiments, the multiple bilayers deposited by layer-by-layer self-assembly are stacks of polymeric electrolytes comprising organic polymeric polyions (e.g., cationic) and counterions (e.g., anionic) containing light-absorbing materials (e.g., pigments). At least a portion of the cationic layer, at least a portion of the anionic layer, or at least a combination thereof may comprise light-absorbing materials (e.g., pigments) ionically bonded to the polymeric electrolyte. The light-absorbing compound may be dispersed within at least a portion of the polymeric electrolyte layer. A variety of polymeric electrolytes may be used, including inorganic compounds such as silica or silicates, and various phosphonocarboxylic acids and their salts (some of which are described in U.S. Patent 10,365,415 (Schmidt)).

[0066] The thickness and number of bilayers can be selected to achieve desired optical properties (e.g., light absorption in the case of an optical absorption layer, or reduced reflection between the sidewalls and the optical absorption layer in the case of a first layer). In some embodiments, the thickness and / or number of bilayers are selected to achieve the desired optical properties using a self-assembled layer with the minimum total thickness and / or a minimum number of layer-by-layer deposition steps. The thickness of each bilayer is typically in the range of about 5 nm to 350 nm. The number of bilayers is typically at least 5, 6, 7, 8, 9, or 10. In some embodiments, the number of bilayers in each stack is no more than 150 or 100. It should be understood that the individual bilayers in the final article may not be distinguishable from each other by methods common in the art such as scanning electron microscopy (SEM) or transmission electron microscopy (TEM). In some embodiments, the thickness and total number of bilayers are selected such that the total thickness of the first layer and the optical absorption layer is less than 2 micrometers.

[0067] After the optical absorption layer and optional first and / or second and / or inorganic optically transparent layers are applied to the (e.g., the entire) microstructured surface of the film and dried, the optical absorption layer and the first and second layers (if present) can be removed from the optical facets and also from the plateau regions between adjacent Fresnel elements (if any). The inorganic optically transparent layers, which can be used as etch barrier layers, are typically not removed but may optionally be removed in subsequent etch steps.

[0068] Any suitable method can be used to selectively remove layers from optical facets. In some implementations, layers are removed by reactive ion etching (RIE). Reactive ion etching (RIE) is a directional etching process that uses ion bombardment to remove material. RIE systems are used to remove organic or inorganic materials by etching surfaces in the direction of ion bombardment. The most significant difference between reactive ion etching and isotropic plasma etching is the etching direction. Reactive ion etching is characterized by a ratio of vertical etching rate to lateral etching rate greater than 1. Systems used for reactive ion etching are typically built around a robust vacuum chamber. Before starting the etching process, the chamber is typically evacuated to a base pressure below 1 Torr, 100 mTorr, 20 mTorr, 10 mTorr, or 1 mTorr. Typically, the electrodes hold the material to be processed and are electrically isolated from the vacuum chamber. The electrodes may be cylindrical, rotatable electrodes. Counter electrodes are also typically located within the chamber and may include the vacuum reactor wall. A gas containing the etchant is typically introduced into the chamber through a control valve. The process pressure can be maintained by continuously evacuating the chamber gas using a vacuum pump. The type of gas used depends on the etching process. For example, etchants may include one or more of oxygen, fluorinated gases, or other halogenated gases. Carbon tetrafluoride (CF4), sulfur hexafluoride (SF6), octafluoropropane (C3F8), perfluorohexane (C6F8) are examples. 14 Trifluoromethane (CHF3), boron trichloride (BCl3), hydrogen bromide (HBr), nitrogen trifluoride (NF3), chlorine, argon, and oxygen are commonly used for etching. Radio frequency (RF) power is applied to the electrodes to generate plasma. Reactive ion etching is known in the art and is further described, for example, in U.S. Patent No. 8,460,568 (David et al.) and International Patent Application No. WO 2019 / 118685 (Schmidt et al.).

[0069] Samples can be transported across electrodes via plasma over a controlled time period to achieve specific etching depths or limit etching so that the etching does not penetrate below the layer to be removed. For example, if the goal is to remove an optical absorption layer, and excluding an inorganic optically transparent layer, the time period can be adjusted to minimize the time the optical facets are exposed to plasma. As described elsewhere, this reduces the surface roughness of the optical facets (e.g., making Ra < 250 nm).

[0070] In some implementations, optically absorbing layers (and / or other layers) are removed by laser ablation (e.g., pulsed laser ablation). Pulsed laser ablation (PLA) is a directional ablation process that utilizes photon flux to generate sufficient photon energy density to remove material by oxidation and / or sputtering. PLA systems are used to remove organic or inorganic materials by etching a surface in the direction of photon energy density, which can evaporate the target when a plasma plume is generated. PLA depends on the wavelength of the laser and the amount of absorption present in the light-absorbing material at that wavelength. The absorption of the laser pulse generates energy for thermal, chemical, or mechanical evaporation, ablation, and / or plasma formation. The presence of oxidizing gases at the laser pulse location may alter the amount of chemical oxidation that occurs during the PLA process. The energy density can be varied by optical configuration to change the size and location of the focal spot, and the energy density can be varied by the power setting of the laser system. The relative orientation of the laser energy density and the sample allows those skilled in the art to ablate optically absorbing layers coated at an angle on a structured surface.

[0071] Examples of optical films including microstructures (each microstructure having an optical facet and a sidewall intersecting the optical facet at the ridge of the microstructure, wherein an optical absorption layer is disposed on the sidewall instead of on the optical facet) are described in U.S. Application No. 62 / 932578, filed November 8, 2019, entitled “Optical Film” and International Patent Application No. PCT / IB2020 / 060184.

[0072] For example Figure 1 Optical models are performed for the optical system described in general and the contrast optical system, where a Fresnel lens is placed on the light-controlling film, and the Fresnel facets are 130° away from the light source. The surface of the light source is obtained having a parabolic shape in a cross-section orthogonal to the z-axis, where the reference... Figure 1 The xyz coordinate system has a shape determined by y = ½ 0.00645 x 2 Given that y and x are in mm. The radius of curvature at x=0 is approximately 155 mm. The Fresnel lens is designed such that light rays emitted perpendicular to the surface of the light source are refracted by the Fresnel lens in the y-direction. Calculate the brightness distribution for various viewing angles (90 degrees on the axis) and various positions (x-coordinate) along the surface of the light source. Figure 22 The results of the comparison optical system are shown. Figure 23 It shows no optical absorption layer on the sidewalls. Figure 1 The result of the optical system. Figure 24 This illustrates an optical absorption layer (e.g., as shown) on the sidewalls. Figure 11 shown) Figure 1 The results of the optical system are shown. A bright band is observed at a contrasting optical system for a viewing angle of approximately 60 degrees and an x-coordinate of approximately -40 mm. Figure 1 and Figure 23 In the optical system, this bright band is essentially eliminated. However, light leakage exists at a viewing angle of approximately 50 degrees and an x-coordinate of approximately 55 mm, which can be undesirable in some applications. This can be addressed by... Figure 24 As shown, an optical absorption layer is included on the sidewall, which effectively eliminates this light leakage.

[0073] Figure 25 This is a schematic cross-sectional view of a structured (e.g., microstructured) layer 320 according to some embodiments, which may be included in an optical film or disposed between an optical film and a light-controlling film. The structured layer 320 may include particles or beads 332 in an adhesive 338. In some embodiments, the structured layer 320 is an optically diffuser layer. In some embodiments, the optically diffuser layer 320 includes a coating comprising beads 332 defining a structured (e.g., microstructured) main surface 331 of the coating. The structured layer 320 may be a coating applied to, for example, the main surface 114 of optical films 110, 210, or 310 or another optical film described elsewhere herein, or it may be a coating applied to, for example, a light-controlling film 120 and bonded to, for example, a second layer 148. For example, the structured layer 320 may be formed by coating a layer of particles in an adhesive and a solvent, and then drying off the solvent. Alternatively, for example, an adhesive 338 layer may be applied to a surface, and then beads may be applied to the adhesive. Suitable methods for manufacturing the structured layer 320 are described, for example, in U.S. Patent Application Publication No. 2008 / 0002256 (Sasagawa et al.).

[0074] Figure 26 This is a schematic cross-sectional view of an optically diffused layer 420 comprising particles or beads 432 dispersed in an adhesive 438, according to some embodiments. Any of layers 164, 191, 148, or 144 may correspond, for example, to the optically diffused layer 420 and may include beads 432 dispersed in the adhesive 438. The optically diffused layer 420 can be formed by mixing the beads 432 into the adhesive 438 and then optionally curing the adhesive 438. Alternatively, the beads 432 may be mixed into the adhesive 438 at a temperature above their melting point, and then the adhesive may be cooled to form layer 420.

[0075] Beads 332 and 432 may be, for example, glass beads or polymethyl methacrylate beads, and adhesives 338 and 438 may include, for example, silicone or optically transparent adhesives. For example, the beads may have an average diameter in the range of 1 micrometer to 10 micrometers or 2 micrometers to 5 micrometers.

[0076] Figure 27This is a schematic cross-sectional view of a structured (e.g., microstructured) surface or interface 824 according to some implementation schemes. Surfaces or interfaces 114, 222, 223, 225, 226 (see example...) Figure 6 Any of these can correspond, for example, to structured surface or interface 824. Structured surface or interface 824 can be formed by embossing or micro-replication (e.g., casting and curing), as is known in the art. Suitable micro-replication techniques are described in U.S. Patent Nos. 7,510,462 (Bryan et al.); 8,657,472 (Aronson et al.); and 10,605,965 (Pham et al.).

[0077] Figures 28 to 36 This is a schematic cross-sectional view of an optical system or optical stack according to some embodiments of this specification. Each of the optical systems or optical stacks shown includes an optical film (510, 610, 710, 810, 910, 1010, 1110, or 1210) and a light-controlling film (220 or 520), which may be bent about an axis, as further described elsewhere herein. For example, optical films 510, 610, 710, 810, 910, 1010, 1110, or 1210 may correspond to optical films 110, 210, or 310. For example, light-controlling film 220 or 520 may correspond to light-controlling film 120.

[0078] The light control film 220 includes a structured (e.g., microstructured) layer 121 formed on a substrate 123, wherein the structured layer 121 includes a plurality of spaced-apart optical absorption regions 124. The substrate 123 may be disposed between the optical film and the structured layer 121, or the structured layer 121 may be disposed between the optical film and the substrate 123. The light control film 520 includes a structured (e.g., microstructured) layer 121 formed on a substrate 523, wherein the substrate 523 has a structured (e.g., microstructured) main surface facing the optical film. Alternatively, the substrate 523 may be considered as a layer of the optical film or as a layer disposed between the optical film and the light control film 121.

[0079] Figures 30 to 36 This schematically illustrates what can be included Figures 28 to 29 Various reflection mitigation elements in the implementation scheme. Figure 28 In the middle, any one of layers 164, 191, 148, and 123 can be an optically diffused layer (e.g., as shown in the image). Figure 26 The schematically illustrated volume diffuser (which may include beads in the adhesive) and / or any of the surfaces or interfaces 114, 222, 223, and 324 may be structured or include an anti-reflective coating. Figure 29 In the middle, any one of layers 164, 191, 148, and 123 can be an optically diffused layer (e.g., as shown in the image). Figure 26The schematically illustrated surfaces or interfaces (including beads in the adhesive) and / or surfaces or interfaces 114, 222, 223, and 325 may be structured or include an anti-reflective coating. Such a structured surface or interface or optically diffused layer may be a reflection-mitigating element suitable for mitigating the undesirable reflection effects of ambient light 654. Figure 28 The image is schematically shown as a reflection from the interface between layer 148 and layer 123. The interfaces 229 and / or the main surfaces 241, 341 of the optical film facing away from the optical film may optionally be microstructured (e.g., as shown in the image). Figure 27 (Surface or interface 824 is schematically shown in the diagram). Such structured surfaces or interfaces can be used, for example, for defect concealment. For example, the main surfaces 241, 341 of the light-control film may include a hard coating for scratch resistance (e.g., a hard coating with a matte finish). Similarly, a hard coating may optionally be included on the main surface 114.

[0080] In some embodiments, the optical film includes a second layer 148 disposed on and in contact with at least a majority of the first main surfaces of the first layers 191, 291, 391. In some embodiments, at least a majority of the first main surfaces comprises at least 80%, at least 90%, or at least 95% of the total area of ​​the first main surfaces. In some embodiments, the second layer 148 is disposed on the first main surfaces of the first layers 191, 291, 391 and has a main surface 149 facing the first main surfaces of the first layers and substantially conforming to the first main surfaces of the first layers (see, for example...). Figure 6 In some embodiments, the second layer 148 bonds the optical film to the light-controlling film. In some embodiments, for at least one wavelength in the range of about 400 nm to about 700 nm, or about 420 nm to about 680 nm, or about 450 nm to about 650 nm (e.g., 532 nm, 550 nm, or 633 nm), the second layer 148 has a lower refractive index than the first layer (e.g., at least 0.05, or at least 0.1, or at least 0.15 lower, and in some embodiments, up to 0.5, or up to 0.4). For example, the wavelength range may be λ1 to λ2 (see example...). Figure 28 ), where λ1 can be about 400nm, about 420nm or about 450nm, and λ2 can be about 700nm, or about 680nm or about 650nm.

[0081] Optical film 610 includes a structured layer 320 disposed between the second layer 148 and the light control film 220. Alternatively, the structured layer 320 may be considered to be disposed between the optical film and the light control film. Optical film 710 includes a structured surface 424 at the interface between the second layer 248 (e.g., corresponding to the second layer 148 but having a structured surface) and the light control film 520. Optical film 810 includes a structured interface 322 between the first layer 291 and the substrate 264. Optical film 910 includes an optical diffuser layer 644 disposed between the second layer 148 and the light control film 220. Alternatively, the optical diffuser layer 644 may be considered to be disposed between the optical film and the light control film 220. Optical film 1010 includes an antireflective coating 744 disposed between the second layer 148 and the light control film 220. Alternatively, the antireflective coating 744 may be considered to be disposed between the optical film and the light control film 220. Figures 35 to 36 As shown, for example, an optical system may include more than one reflection mitigation element. Optical film 1110 includes a first layer 191 disposed on optically diffuser layer 364. Optical film 1110 also includes an optically diffuser second layer 348, which may correspond to second layer 148 but may include, for example, beads dispersed in an adhesive. Optical film 1110 also includes an anti-reflective coating 744. Alternatively, the anti-reflective coating 744 may be considered disposed between the optical film and the light-controlling film 220. Optical film 1210 includes an optically diffuser first layer 391 (e.g., corresponding to first layer 191 but including beads in an adhesive), and includes a structured surface 466 of substrate 464 and a structured surface 424 of second layer 248. Alternatively, layers 248 and 523 may be considered disposed between the optical film (including layers 391, 464) and the light-controlling film 121. In some embodiments, at least one reflection mitigation element includes a plurality of beads dispersed in the first layer 391, such as… Figure 36 As illustrated in the diagram. In embodiments where the first layer 391 includes beads, the amount (e.g., concentration) of the beads may be limited to avoid interfering with the desired refractive properties of the layer.

[0082] The antireflective coating 744 may include one or more layers (e.g., one or more ¼-wave layers or a combination of ¼ and ½-wave layers), which may be vapor-deposited, for example, as known in the art.

[0083] In some embodiments, at least one reflection mitigation element includes a microstructured interface (e.g., 322, 424, 431). In some embodiments, the optical film further includes: a second layer (e.g., 148, 248, 348) disposed on a first main surface of the first layer, wherein the second layer has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm; and a third layer (e.g., 320, 523) disposed between the second layer and the photocontrol film, wherein the interface between the second and third layers (e.g., 424, 431) includes a microstructured interface. In some embodiments, the second layer contacts at least a majority of the first main surface of the first layer and / or has a main surface facing the first main surface of the first layer and substantially conforming to the first main surface of the first layer. In some embodiments, the third layer is an optical adhesive for bonding the second layer to the photocontrol film. In some embodiments, the third layer includes a structured layer bonded to the photocontrol film, wherein the second layer includes an adhesive bonded to the first main surface of the first layer and the structured main surface of the structured layer. In some embodiments, the adhesive is or includes a silicone adhesive. In some embodiments, the optical film further includes a second layer disposed on a first main surface of the first layer, wherein the second layer bonds the optical film to the photocontrol film, and has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm. The interface between the second layer and the photocontrol film may include a microstructured interface (e.g., 424), and / or at least one reflection mitigation element may include the microstructured main surface 424 of the second layer facing the photocontrol film 520. In some embodiments, the photocontrol film includes a structured layer 121 formed on substrates 123, 523, wherein the structured layer 121 includes a plurality of spaced-apart optical absorption regions 224, and the substrate 523 is disposed between the optical film and the structured layer 121. In some embodiments, the photocontrol film includes a structured layer 121 formed on substrates 123, 523, wherein the structured layer 121 includes a plurality of spaced-apart optical absorption regions 224, and the structured layer 121 is disposed between the optical film and the substrate. In some implementations, the interface between the microstructured layer and the substrate is structured (e.g., Figures 28 to 29 Interface 229 in the middle can be like Figure 27 It is structured as shown in interface 824.

[0084] In some embodiments, at least one reflection mitigation element includes a microstructured interface 322, wherein the optical film includes a substrate 264, a first layer 291 is disposed on the substrate, wherein a first main surface 312 of the first layer faces away from the substrate, and the interface 322 between the first layer 291 and the substrate 264 includes a microstructured interface.

[0085] In some implementations, optical films (e.g., Figure 36The optical film 1210 shown schematically includes a substrate, wherein a first layer is disposed on the substrate, wherein a first main surface of the first layer faces away from the substrate, and wherein at least one reflection mitigation element includes a microstructured main surface 466 of the substrate facing away from the first layer.

[0086] In some embodiments, at least one reflection mitigation element includes an optically diffuser layer. In some embodiments, the optically diffuser layer includes beads (e.g., 432) dispersed in an adhesive (e.g., 438). In some embodiments, the optically diffuser layer includes a coating 320 that includes beads 332 defining a structured main surface 331 of the coating. In some embodiments, the optically diffuser layer includes microstructured main surfaces 331, 824. In some embodiments, the optically diffuser layer (e.g., layer 348) is disposed on and in contact with at least a majority of a first main surface of the optical film. In some embodiments, the optically diffuser layer is disposed on a first main surface of the first layer and has a main surface facing and substantially conforming to the first main surface of the first layer. In some embodiments, a first layer 191 is disposed on a substrate 364, wherein the substrate is or includes the optically diffuser layer. In some embodiments, the optical film further includes a second layer disposed on the first main surface of the first layer, wherein the second layer has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm, and wherein optical diffuser layers 320, 644 are disposed between the second layer and the photocontrol film. The second layer may contact at least a majority of the first main surface of the optical film, and / or the second layer may have a main surface facing the first main surface of the optical film and substantially conforming to the first main surface of the optical film.

[0087] In some embodiments, at least one reflection mitigation element includes an antireflective coating 744. In some embodiments, the optical film further includes a second layer disposed on a first main surface of the first layer, wherein the second layer has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm; and a third layer disposed between the second layer and the photocontrol film, wherein the antireflective coating is disposed between the second and third layers (e.g., Figure 35The substrate 123 in the light control film can be considered as the third layer of the optical film 1110, or the substrate layer can be omitted and layer 123 can be an adhesive layer. In some embodiments, the third layer is an optical adhesive that bonds the second layer to the light control film. For example, the adhesive can be or includes silicone adhesive. In some embodiments, the optical film further includes a second layer disposed on the first main surface of the first layer, wherein the second layer bonds the optical film to the light control film, wherein the second layer has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm, and wherein an anti-reflective coating 744 is disposed between the second layer and the light control film. The second layer may contact at least a majority of the first main surface of the optical film, and / or the second layer may have a main surface facing the first main surface of the optical film and substantially conforming to the first main surface of the optical film. The anti-reflective coating 744 may be disposed on the main surface of the light control film facing the optical film and substantially conforming to the main surface of the light control film facing the optical film.

[0088] In some implementations, optical films (e.g., Figure 30 The schematic diagram (610) further includes: a second layer 148 disposed on the first main surface 412 of the first layer 191, wherein the second layer 148 has a lower refractive index than the first layer for at least one wavelength in the range of about 400 nm to about 700 nm; and a third layer disposed between the second layer and the photocontrol film, wherein the third layer includes a structured layer 320 bonded to the photocontrol film 220, and wherein the second layer 148 includes an adhesive bonded to the first main surface of the first layer 191 and the structured main surface 431 of the structured layer 320. As further described elsewhere herein, the second layer may be in contact with at least a majority of the first main surface of the optical film, and / or the second layer may have a main surface facing the first main surface of the optical film and substantially conforming to the first main surface of the optical film.

[0089] In some embodiments, at least one reflection mitigation element is disposed on the side of the light-control film facing the optical film. For example, Figure 35 An embodiment can be described as including an optical film comprising layers 191 and 364 disposed on a light-controlling film, the light-controlling film comprising layers 123 and 121, wherein layers 348 and 744 are disposed between the optical film and the light-controlling film. As another example, Figure 36 An embodiment can be described as including an optical film comprising layers 464 and 391 disposed on a light control film including layer 121, wherein layers 248 and 523 are disposed between the optical film and the light control film.

[0090] Terms such as “about” will be understood in the context in which they are used and described by those skilled in the art. If it is unclear to those skilled in the art in the context of their use and description of “about” to express quantities of characteristic size, quantity, and physical properties, then “about” will be understood to mean within 10% of the specified value. A quantity given a specified value as “about” can be precisely the specified value. For example, if it is unclear to those skilled in the art in the context of their use and description of this specification, a quantity having a value of about 1 means that the quantity has a value between 0.9 and 1.1, and that the value can be 1.

[0091] All cited references, patents, and patent applications are incorporated herein by reference in their entirety in a consistent manner. In the event of any inconsistency or contradiction between the incorporated references and this application, the information in the foregoing description shall prevail.

[0092] Unless otherwise indicated, the description of elements in the accompanying drawings should be understood to apply equally to corresponding elements in the other drawings. While specific embodiments have been illustrated and described herein, those skilled in the art will recognize that various alternative and / or equivalent embodiments may be used instead of the illustrated and described embodiments without departing from the scope of this disclosure. This application is intended to cover any modifications or variations of the specific embodiments discussed herein. Therefore, this disclosure is intended to be limited only by the claims and their equivalents.

Claims

1. An optical system, comprising: a light source; an optical film, which is curved around a first axis and comprises a first layer, the first layer comprising a microstructured first major surface, the microstructured first major surface defining a linear Fresnel lens, the linear Fresnel lens comprising a plurality of Fresnel elements extending along the first axis; and a light control film, which is curved around the first axis and substantially coextensive with the optical film, the light control film being disposed between the light source and the optical film, the first major surface of the optical film facing the light control film, the light control film comprising a plurality of spaced apart light absorbing regions extending along the first axis and along a direction substantially perpendicular to the major surface of the light control film, wherein at least one of the optical film or at least one layer disposed between the optical film and the light control film comprises at least one reflection mitigating element.

2. The optical system according to claim 1, wherein each Fresnel element comprises an optical facet and a sidewall intersecting the optical facet at the ridge of the Fresnel element, wherein for each of at least a majority of the Fresnel elements, a light absorbing layer is disposed on and substantially covers the sidewall, the light absorbing layer having an average thickness t, 100 nm < t < 1 micrometer.

3. An optical system, comprising: an optical film, which is curved around a first axis and comprises a first layer, the first layer comprising a microstructured first major surface, the microstructured first major surface defining a linear Fresnel lens, the linear Fresnel lens comprising a plurality of Fresnel elements extending along the first axis, each Fresnel element comprising an optical facet and a sidewall intersecting the optical facet at the ridge of the Fresnel element, wherein for each of at least a majority of the Fresnel elements, a light absorbing layer is disposed on and substantially covers the sidewall, the light absorbing layer having an average thickness t, 100 nm < t < 1 micrometer; and a light control film, which is disposed adjacent to the optical film, the light control film being curved around the first axis and substantially coextensive with the optical film, the first major surface of the optical film facing the light control film, the light control film comprising a plurality of spaced apart light absorbing regions extending along the first axis and along a direction substantially perpendicular to the major surface of the light control film, wherein at least one of the optical film or at least one layer disposed between the optical film and the light control film comprises at least one reflection mitigating element.

4. The optical system according to any one of claims 1 to 3, wherein the at least one reflection mitigating element comprises at least one of a structured surface other than the microstructured first major surface, an anti-reflective coating, or a bulk diffuser.

5. The optical system according to any one of claims 1 to 3, wherein the at least one reflection mitigating element comprises a microstructured interface.

6. The optical system according to claim 5, wherein the optical film further comprises: A second layer, disposed on the first main surface of the first layer and having a main surface facing and substantially conforming to the first main surface of the first layer, having a lower refractive index than the first layer for at least one wavelength in the range of 400 nm to 700 nm; and The third layer is disposed between the second layer and the light-control film. The interface between the second layer and the third layer includes the microstructured interface.

7. The optical system of claim 5, wherein the optical film comprises a substrate and a first layer disposed on the substrate, the first main surface of the first layer facing away from the substrate, wherein the interface between the first layer and the substrate comprises the microstructured interface.

8. The optical system according to any one of claims 1 to 3, wherein the optical film further comprises: A second layer is disposed on the first main surface of the first layer and has a main surface facing and substantially conforming to the first main surface of the first layer. The second layer bonds the optical film to the light-controlling film. For at least one wavelength in the range of 400 nm to 700 nm, the second layer has a lower refractive index than the first layer. The at least one of the reflection mitigation elements includes a microstructured main surface of the second layer facing the light control film.

9. The optical system according to any one of claims 1 to 3, wherein the optical film comprises a substrate and a first layer disposed on the substrate, the first main surface of the first layer facing away from the substrate, wherein the at least one reflection mitigation element comprises a microstructured main surface of the substrate facing away from the first layer.

10. The optical system according to any one of claims 1 to 3, wherein the at least one reflection mitigation element comprises an optical diffuser layer.

11. The optical system of claim 10, wherein the optical diffuser layer is disposed on the first main surface of the first layer and has a main surface facing the first main surface of the first layer and substantially conforming to the first main surface of the first layer.

12. The optical system of claim 10, wherein the first layer is disposed on a substrate, the substrate including the optical diffuser layer.

13. The optical system of claim 10, wherein the optical diffuser layer comprises a plurality of beads dispersed in the binder.

14. The optical system according to any one of claims 1 to 3, wherein the at least one reflection mitigation element comprises an anti-reflection coating.

15. The optical system of claim 14, wherein the optical film further comprises: A second layer is disposed on the first main surface of the first layer and has a main surface facing and substantially conforming to the first main surface of the first layer. The second layer bonds the optical film to the light-controlling film. For at least one wavelength in the range of 400 nm to 700 nm, the second layer has a lower refractive index than the first layer. The anti-reflective coating is disposed between the second layer and the light control film.

Citation Information

Patent Citations

  • Articles comprising self-assembled layers comprising nanoparticles with a phosphorous surface treatment

    US10365415B2

  • Optical diffusing films and methods of making same

    US10605965B2

  • Brightness enhancement film, and methods of making and using the same

    US20060114569A1

  • Optical article including a beaded layer

    US20080002256A1

  • Method of Asymmetrically Functionalizing Porous Materials