A method for fabricating a saddle-shaped superconducting coil

By winding multi-layer saddle-shaped coils with a single superconducting wire and using a copper wire model and vacuum-impregnated paraffin to fix the shape, the problems of complex winding of saddle-shaped coils and the influence of joints on the magnetic field were solved, achieving efficient, stable magnetic field uniformity and low-cost production.

CN117577441BActive Publication Date: 2026-11-17INST OF ELECTRICAL ENG CHINESE ACAD OF SCI
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311719262.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-14
Publication Date
2026-11-17
Estimated Expiration
2043-12-14

AI Technical Summary

Technical Problem

Existing saddle-shaped superconducting coils are complex to wind, and multi-layered coil joints cause magnetic field instability. The heating of the joint resistance affects the uniformity of the magnetic field, and the joints are difficult to manufacture, which affects the overall performance.

Method used

A multi-layer saddle-shaped coil is wound using a single superconducting wire. The first saddle-shaped coil wound with copper wire is used as a model. The shape is fixed by vacuum impregnation with paraffin wax. The coil is wound from the inside out, using the previous turn of wire to provide mechanical support. The copper wire is replaced layer by layer to form a compact overall structure.

Benefits of technology

It eliminates safety hazards in joint manufacturing, reduces the impact of joints on the magnetic field, improves magnetic field uniformity and manufacturing efficiency, reduces costs, and is easy to industrialize.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117577441B_ABST
    Figure CN117577441B_ABST
Patent Text Reader

Abstract

This invention provides a saddle-shaped superconducting coil and its manufacturing method. A single-layer first saddle-shaped coil is wound with copper wire, serving as a model coil with the same dimensions as a second saddle-shaped coil actually wound with superconducting wire. The first saddle-shaped coil, wound with copper wire, acts as a winding mold, guiding the even-numbered layers of the actual second saddle-shaped coil from the outside in. By using an inside-out winding method for odd-numbered layers and a first saddle-shaped coil as the winding trajectory to guide the superconducting wire from the outside in for even-numbered layers, the winding of all second saddle-shaped coils is completed. After the second saddle-shaped coils are wound, the entire coil is vacuum-pressure impregnated with paraffin wax, making the second saddle-shaped coil 4 a single unit. This overcomes the problem of multiple joints generated by existing multi-layer patch-type saddle-shaped coils. It avoids the problem of joint pre-reserved wires affecting magnetic field uniformity when multiple saddle-shaped coils are stacked, resulting in a more compact coil structure and reduced impact of joints on the magnetic field.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of superconducting coils and relates to a method for manufacturing a saddle-shaped superconducting coil. Background Technology

[0002] Since their discovery, superconducting materials have been widely used in people's lives, such as in nuclear magnetic resonance spectrometers, nuclear magnetic resonance imaging equipment, high-magnetic-field scientific instruments, controlled nuclear fusion devices, and magnetically pulled single-crystal equipment for the manufacture of single-crystal silicon.

[0003] The most common shape for a superconducting coil is a central solenoid, which serves as the main coil and provides a strong central magnetic field. Solenoid coils manufactured using precision wiring can ensure a certain degree of magnetic field uniformity at the center. To further improve the uniformity of the central magnetic field, shimming coils and other devices are needed to regulate the central magnetic field, thus creating equipment with a highly uniform central magnetic field.

[0004] Due to their unique shape, saddle-shaped superconducting coils offer optimized structures and higher magnetic field efficiency in some applications compared to other shapes, providing a significant advantage in terms of the amount of expensive superconducting wire used. For example, in magnetohydrodynamic (MHD) power generation devices, saddle-shaped superconducting coils offer the advantage of saving materials. Furthermore, as a common form of active shielding and shimming coil, saddle-shaped superconducting coils can effectively shield and compensate for stray fields, improving the uniformity of the magnetic field. However, the winding process of saddle-shaped superconducting coils is relatively complex. The anisotropic shape of the coil, including circular arcs, straight sections, and corners, along with varying radii of curvature, increases the difficulty of winding.

[0005] Furthermore, the even-numbered layers of the saddle coil need to be wound from the outside in. The previous turn cannot provide mechanical support for the next turn, making it difficult for the next turn to be tightly arranged, which can easily lead to gaps. This affects the uniformity of the magnetic field of the saddle coil, and the gaps can easily cause the conductor to move during the excitation process due to the lack of mechanical support, thus causing the saddle coil to lose quench. Summary of the Invention

[0006] To overcome the problems of multiple joints generated by multi-layer patch saddle coils in existing technologies, which cause current changes due to joint resistance heating and thus affect magnetic field quality, leading to magnetic field instability, and requiring the joint's current-carrying capacity to be comparable to that of the saddle coil (otherwise, quenching failure may occur due to low joint current-carrying capacity), and to address the challenges of fabricating joints between multi-layer coils (requiring sufficient superconducting wire to house the joint fabrication equipment outside each layer), which inevitably affects magnetic field uniformity, this invention provides a method for manufacturing saddle-shaped superconducting coils. This method uses a single superconducting wire to wind multiple layers of saddle-shaped coils, eliminating the need for internal joint connections, thus avoiding safety hazards associated with joint fabrication, reducing the impact of joints on the magnetic field, saving space, and improving manufacturing efficiency. Furthermore, this invention results in a simple saddle-shaped coil structure, low manufacturing cost, and ease of industrialization.

[0007] The objective of this invention is achieved through the following technical solution.

[0008] This invention involves winding copper wire onto a cylindrical surface with a specific number of ampere-turns according to an electromagnetic design. A single-layer first saddle-shaped coil is then wound using this copper wire, serving as a model coil with the same dimensions as the actual superconducting coil. This first saddle-shaped coil is then used as a winding mold to guide the even-numbered layers of the actual saddle-shaped coil as it is wound from the outside in. Due to the shape of the saddle-shaped coil, each previous turn provides mechanical support for the next adjacent turn during winding from the inside out, allowing the winding to be completed under a certain tension.

[0009] The method for fabricating the saddle-shaped superconducting coil of the present invention includes the following steps:

[0010] Step 1: Install an epoxy resin board on a cylindrical frame. The epoxy resin board is in close contact with the outer surface of the cylindrical frame. Using the epoxy resin board as the base, a single-layer first saddle-shaped coil is wound on the epoxy resin board using copper wire. The winding process is from the inside to the outside. The two sides of the first saddle-shaped coil are parallel to the axis of the cylindrical frame, and the two top edges are perpendicular to the two sides.

[0011] Step 2: The wound first saddle-shaped coil is vacuum impregnated to fill the spaces between the turns with paraffin wax. The shape of the first saddle-shaped coil is then maintained by the adhesion of the cured paraffin wax to the wires. The first saddle-shaped coil and the epoxy resin plate at its bottom are then removed from the cylindrical frame.

[0012] Step 3: Repeat steps 1 and 2 to prepare multiple first saddle-shaped coils.

[0013] Step 4: The first layer of the second saddle-shaped coil is wound on the cylindrical frame using superconducting wire. An epoxy resin board is installed on the cylindrical frame, with the epoxy resin board closely attached to the outer surface of the cylindrical frame. Using the epoxy resin board as the base plate, the first layer of the second saddle-shaped coil is wound on the epoxy resin board using superconducting wire. The winding process is from the inside to the outside. The two sides of the second saddle-shaped coil are parallel to the axis of the cylindrical frame, and the two top edges are perpendicular to the two sides.

[0014] Step 5: After the first layer of the second saddle coil is wound, place the first saddle coil, which has been impregnated with paraffin, on the upper surface of the second saddle coil, and use an epoxy resin plate to accurately position and fix the first and second saddle coils.

[0015] Step 6: Wind the second layer of the second saddle coil from the outside in. The winding trajectory of the superconducting wire coincides with the trajectory of the first saddle coil. Strip the copper wire lead from the outermost layer of the first saddle coil. As the copper wire is stripped from each turn of the first saddle coil, the superconducting wire of the second layer of the second saddle coil gradually replaces the position of the copper wire of the first saddle coil. Finally, the winding of the second layer of the second saddle coil ends when the innermost layer is reached.

[0016] Step 7: Heat the surface of the second saddle-shaped coil with a hot air gun to remelt the residual paraffin wax. After the paraffin wax solidifies, it plays a shaping role for the second layer of the second saddle-shaped coil.

[0017] Step 8: Continue winding the third layer of the second saddle-shaped coil, winding from the inside out.

[0018] Step 9: Repeat steps 6 and 7 to complete the winding of the fourth layer of superconducting wire for the second saddle-shaped coil.

[0019] Step 10: Repeat steps 4 to 9, using the method of winding from the inside out for odd-numbered layers and using the first saddle-shaped coil as the winding trajectory to guide the superconducting wire to wind from the outside in for even-numbered layers, to complete the winding of all second saddle-shaped coils.

[0020] Step 11: After the second saddle-shaped coil is wound, the entire second saddle-shaped coil is vacuum pressure impregnated with paraffin wax to make the second saddle-shaped coil impregnated into a whole.

[0021] The epoxy resin board has a thickness of 0.05-0.2mm and serves as an insulating layer between the second saddle-shaped coil layers. Holes with a diameter of 1-3mm are made in the epoxy board to allow the paraffin wax to flow, ensuring the overall impregnation of the second saddle-shaped coil.

[0022] Beneficial effects:

[0023] The saddle-shaped coil manufactured in this invention is wound with a single superconducting wire, eliminating the problem of pre-existing joint wires affecting magnetic field uniformity that occurs when multiple saddle-shaped coils are stacked. This results in a more compact coil structure, reducing the impact of joints on the magnetic field and minimizing their vulnerability to damage during the overall coil excitation process. The first saddle-shaped coil wound with copper wire, used as a model coil, ensures dimensional accuracy and allows for reuse of the copper wire, thus reducing manufacturing costs. Attached Figure Description

[0024] Figure 1 Schematic diagram of the first saddle-shaped coil of the present invention;

[0025] Figure 2 Schematic diagram of the first saddle-shaped coil and frame of the present invention;

[0026] Figure 3 Schematic diagram of the second saddle-shaped coil winding process of the present invention;

[0027] Figure 4 A schematic diagram of the second saddle-shaped coil of the present invention. Detailed Implementation

[0028] The present invention will be further described below with reference to the accompanying drawings and specific embodiments.

[0029] like Figures 1-4 As shown, the saddle-shaped superconducting coil of the present invention is formed by a first saddle-shaped coil 1, an epoxy resin plate 2, a cylindrical frame 3, and a second saddle-shaped coil 4. The first saddle-shaped coil 1 is made of copper wire wound on the cylindrical frame 3, and its shape is fixed by vacuum pressure impregnation with paraffin wax. An epoxy resin plate 2 is installed between the first saddle-shaped coil 1 and the cylindrical frame 3. The epoxy resin plate 2 has holes for the flow channels of the paraffin wax. The first layer of the second saddle-shaped coil 4 is wound on the cylindrical frame 3 using superconducting wire. The paraffin-impregnated first saddle-shaped coil 1 is placed on the upper surface of the second saddle-shaped coil 4, and the epoxy resin plate 2 is used to precisely position and fix the coil. The second layer of the second saddle-shaped coil 4 is wound from the outside to the inside, and the winding trajectory of the superconducting wire coincides with the trajectory of the first saddle-shaped coil 1, gradually replacing the first saddle-shaped coil 1. Repeat the above steps, using the method of winding from the inside out for odd-numbered layers and using the first saddle-shaped coil 1 as the winding trajectory to guide the superconducting wire to wind from the outside in for even-numbered layers, to complete the winding of all second saddle-shaped coils 4. Finally, after the second saddle-shaped coils 4 are wound, they are impregnated by vacuum pressure to allow the paraffin wax to re-enter the interior of the second saddle-shaped coils 4, forming a single, integral second saddle-shaped coil 4 wound with a single superconducting wire.

[0030] Example 1

[0031] An epoxy resin board 2 is mounted on a cylindrical frame 3, with the epoxy resin board 2 tightly attached to the outer surface of the cylindrical frame 3. Using the epoxy resin board 2 as a base, a single-layer first saddle-shaped coil 1 is wound on the epoxy resin board 2 using copper wire. The winding process proceeds from the inside out. The two sides of the first saddle-shaped coil 1 are parallel to the axial direction of the cylindrical frame 3, and the two top edges are parallel to the arcuate weft direction of the cylindrical frame 3. The wound first saddle-shaped coil 1 is then vacuum impregnated to fill the inter-turn spaces with paraffin wax. The shape of the first saddle-shaped coil 1 is maintained by the adhesion of the cured paraffin wax to the wire. The first saddle-shaped coil 1 and the epoxy resin board 2 at its bottom are then removed from the cylindrical frame 3. Multiple first saddle-shaped coils 1 are prepared. The first layer of a second saddle-shaped coil 4 is wound on the cylindrical frame 3 using superconducting wire. After the first layer of the second saddle coil 4 is wound, the paraffin-impregnated first saddle coil 1 is placed on the upper surface of the second saddle coil 4. The epoxy resin board 2 is used for precise positioning and fixation of the first saddle coil 1 and the second saddle coil 4. The second layer of the second saddle coil 4 is wound from the outside in, with the winding trajectory of the superconducting wire coinciding with that of the first saddle coil 1. Copper wire leads are stripped from the outermost layer of the first saddle coil 1. As copper wire is stripped from each turn of the first saddle coil 1, the superconducting wire of the second layer of the second saddle coil 4 gradually replaces the position of the copper wire in the first saddle coil 1, finally winding to the innermost layer to complete the second layer winding of the second saddle coil 4. The surface of the second saddle coil 4 is heated with a hot air gun to remelt the remaining paraffin. The solidified paraffin serves to shape the second layer of the second saddle coil 4. The third layer of the second saddle coil 4 is then wound, from the inside out. The fourth layer of superconducting wire winding of the second saddle coil 4 is then completed. Repeat the above steps, using the method of winding from the inside out for odd-numbered layers and winding the superconducting wire from the outside in for even-numbered layers with the first saddle-shaped coil 1 as the winding trajectory guide, to complete the winding of all second saddle-shaped coils 4. After the second saddle-shaped coils 4 are wound, the entire second saddle-shaped coil 4 is vacuum pressure impregnated with paraffin wax to make the second saddle-shaped coil 4 impregnated into a whole.

Claims

1. A method of making a saddle-shaped superconducting coil, characterized by, Includes the following steps: Step 1: Install an epoxy resin board on a cylindrical frame. The epoxy resin board is in close contact with the outer surface of the cylindrical frame. Using the epoxy resin board as the base, a single-layer first saddle-shaped coil is wound on the epoxy resin board with copper wire. The winding process is from the inside to the outside. Step 2: The wound first saddle-shaped coil is vacuum impregnated to fill the inter-turn spaces of the first saddle-shaped coil with paraffin wax. The shape of the first saddle-shaped coil is maintained by the adhesion of the cured paraffin wax to the wire. The first saddle-shaped coil and the epoxy resin plate at the bottom of the first saddle-shaped coil are removed from the cylindrical frame. Step 3: Repeat steps 1 and 2 to prepare multiple first saddle-shaped coils and epoxy resin plates at the bottom of the first saddle-shaped coils; Step 4: Install an epoxy resin board on a cylindrical frame. The epoxy resin board is in close contact with the outer surface of the cylindrical frame. Using the epoxy resin board as the base, wind the first layer of the second saddle-shaped coil on the epoxy resin board using superconducting wire. The winding process is from the inside to the outside. Step 5: After the first layer of the second saddle coil is wound, place the first saddle coil impregnated with paraffin and the epoxy resin plate at the bottom of the first saddle coil on the upper surface of the second saddle coil. Use the epoxy resin plate to accurately position and fix the first saddle coil and the second saddle coil. Step 6: Wind the second layer of the second saddle coil from the outside in. The winding trajectory of the superconducting wire coincides with the trajectory of the first saddle coil. Strip the copper wire lead from the outermost layer of the first saddle coil. As the copper wire is stripped from each turn of the first saddle coil, the superconducting wire of the second layer of the second saddle coil gradually replaces the position of the copper wire of the first saddle coil. Finally, the winding of the second layer of the second saddle coil ends when the innermost layer is reached. Step 7: Heat the surface of the second saddle coil with a hot air gun to remelt the residual paraffin wax. After the paraffin wax solidifies, it plays a shaping role on the second layer of the second saddle coil. Step 8: Continue winding the third layer of the second saddle-shaped coil, winding from the inside out; Step 9: Repeat steps 6 and 7 to complete the winding of the fourth layer of superconducting wire for the second saddle-shaped coil. Step 10: Repeat steps 4 to 9 above, using the method of winding from the inside out for odd-numbered layers and using the first saddle-shaped coil as the winding trajectory to guide the superconducting wire to wind from the outside in for even-numbered layers, to complete the winding of the second saddle-shaped coil. Step 11: After the second saddle-shaped coil is wound, the entire second saddle-shaped coil is vacuum pressure impregnated with paraffin wax to make the second saddle-shaped coil impregnated into a whole. The second saddle-shaped coil is made by winding a single superconducting wire; The epoxy resin board has a thickness of 0.05-0.2mm and serves as an insulating layer between the second saddle-shaped coil layers. Holes with a diameter of 1-3mm are made in the epoxy resin board to facilitate the flow of paraffin wax and ensure the overall impregnation of the second saddle-shaped coil.

2. The method for fabricating a saddle-shaped superconducting coil according to claim 1, characterized in that, The two sides of the first saddle-shaped coil are parallel to the axis of the cylindrical frame, and the two top edges are perpendicular to the two sides; the two sides of the second saddle-shaped coil are parallel to the axis of the cylindrical frame, and the two top edges are perpendicular to the two sides.

Citation Information

Patent Citations

  • Manufacturing method for skeleton-free niobium-tri-tin superconducting coil

    CN109545539A

  • Solenoid type high-temperature superconducting coil and curing method thereof

    CN110957100A