Strength testing apparatus and strength testing method

By designing a strength testing device that utilizes the load-bearing surfaces and loading surfaces at both ends of a workpiece, the problem of tensile strength testing of thin-thickness CMC materials under high-temperature conditions was solved, and accurate strength testing of CMC materials with a thickness of less than 10 mm was achieved.

CN117740528BActive Publication Date: 2026-11-17AECC COMML AIRCRAFT ENGINE CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202211115885.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-09-14
Publication Date
2026-11-17
Estimated Expiration
2042-09-14

AI Technical Summary

Technical Problem

In the current technology, there is a lack of suitable thickness-direction strength testing devices and methods for small-thickness ceramic matrix composites (CMCs) under high-temperature environments, especially the out-of-plane tensile strength performance testing is difficult.

Method used

Design a strength testing device that uses the different load-bearing surfaces and corresponding loading surfaces at both ends of the workpiece to restrict its position, clamps the workpiece with a first fixture and a second fixture, and uses high-temperature resistant materials in a high-temperature environment to achieve clamping, fixing and tensile strength testing of the workpiece.

Benefits of technology

It enables tensile strength testing of thin-thickness workpieces under high-temperature conditions, ensuring the accuracy and reliability of the test, and is applicable to CMC materials with a thickness of no more than 10 mm.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117740528B_ABST
    Figure CN117740528B_ABST
Patent Text Reader

Abstract

This invention discloses a strength testing device and method for testing the tensile strength of a workpiece. The workpiece has a first load-bearing surface and a second load-bearing surface at both ends along the force direction, different from the force direction. These two load-bearing surfaces are located on opposite sides of the workpiece, extending inwards or outwards relative to the workpiece's outer surface. The strength testing device includes a first clamp and a second clamp, with the workpiece clamped between them. The surface of the first clamp relative to the workpiece includes a first loading surface that contacts and engages with the first load-bearing surface, and the surface of the second clamp relative to the workpiece includes a second loading surface that contacts and engages with the second load-bearing surface. This strength testing device and method cleverly utilize the workpiece's structural characteristics to achieve clamping and fixation at both ends of the workpiece through positional constraints, making it more suitable for strength testing of thin workpieces that are difficult to clamp.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of testing equipment technology, and in particular to a strength testing device and a strength testing method. Background Technology

[0002] Due to limitations in manufacturing processes, most ceramic matrix composites (CMCs) currently used in engineering are thin-walled, with relatively small thicknesses (3mm–10mm). This results in CMC specimens for out-of-plane tensile strength testing being mostly sheet-like, lacking sufficient area for clamping and applying test loads in the out-of-plane direction. This presents challenges for testing the out-of-plane tensile strength of CMCs. At room temperature, adhesive bonding is typically used to connect CMC specimens to metal loading fixtures and transfer test loads. However, due to the temperature limitations of adhesives, this method cannot be used at high temperatures. Currently, there is no suitable clamping and testing equipment for thin-thickness CMCs, and a mature testing method, especially for out-of-plane tensile strength testing at high temperatures, is lacking. Summary of the Invention

[0003] The technical problem to be solved by the present invention is to overcome the deficiency of the prior art in that there is no suitable thickness direction strength testing device for workpieces with small thickness, and to provide a strength testing device and a strength testing method.

[0004] The present invention solves the above-mentioned technical problems through the following technical solution:

[0005] A strength testing device is used to test the tensile strength of a workpiece. The workpiece has a first load-bearing surface and a second load-bearing surface at both ends along the force direction, which are different from the force direction. The first load-bearing surface and the second load-bearing surface are located on both sides of the workpiece. The first load-bearing surface and the second load-bearing surface extend inward or outward in a consistent manner relative to the outer surface of the workpiece.

[0006] The strength testing device includes a first clamp and a second clamp, and the workpiece is clamped between the first clamp and the second clamp;

[0007] The first fixture has a first loading surface that contacts and engages with the first load-bearing surface on the surface of the workpiece, and the second fixture has a second loading surface that contacts and engages with the second load-bearing surface on the surface of the workpiece.

[0008] In this scheme, the workpiece is clamped between a first fixture and a second fixture. Two load-bearing surfaces (the first and second load-bearing surfaces) in directions opposite to the force direction, along with two corresponding contacting loading surfaces (the first and second loading surfaces), are used to restrict the position of the two load-bearing surfaces of the workpiece. This cleverly utilizes the workpiece's structural characteristics (the orientation of the first and second load-bearing surfaces) to achieve clamping and fixation at both ends of the workpiece through positional constraints, without needing to clamp the workpiece at both ends for force-induced clamping. This allows for tensile strength testing of thin workpieces that are difficult to clamp. By applying pressure to the first fixture and / or the second fixture, the two loading surfaces are driven to compress the two load-bearing surfaces, causing tension at both ends of the workpiece, thus achieving the strength test. The force direction is the tensile direction of the workpiece.

[0009] Preferably, both the first loading surface and the second loading surface extend outward in a direction away from the workpiece.

[0010] In this scheme, since both the first loading surface and the second loading surface extend outward in a direction away from the workpiece, it is adapted to the situation where both load-bearing surfaces of the workpiece also extend outward in a direction away from the workpiece. This makes the compressive forces of the two clamps on the two load-bearing surfaces in opposite directions, thereby realizing the strength test by tensile method.

[0011] Preferably, the extension directions of the first loading surface and the second loading surface are parallel to each other.

[0012] In this scheme, the extension directions of the first loading surface and the second loading surface are set to be parallel to each other, so that equal force can be applied to the two load-bearing surfaces of the workpiece, which is conducive to the stable stress on the workpiece, avoids the displacement caused by uneven stress, and makes the strength test more stable.

[0013] Preferably, the workpiece further includes an intermediate test area, wherein the first load-bearing surface and the second load-bearing surface are respectively disposed at both ends of the intermediate test area along the force direction.

[0014] The first fixture also includes a third surface relative to the workpiece, the third surface being in clearance fit with the extended surface of the intermediate test area;

[0015] And / or, the second fixture further includes a fourth surface relative to the surface of the workpiece, the fourth surface being clearance-fitted with the extended surface of the intermediate test area.

[0016] In this scheme, the third surface and the extended surface of the intermediate test area are fitted with a clearance fit, so that the first fixture moves without resistance; the fourth surface and the extended surface of the intermediate test area are fitted with a clearance fit, so that the second fixture moves without resistance; thus ensuring that the external force applied to the first fixture and / or the second fixture is used for strength testing, and the force on the workpiece can be directly obtained without additional calculation, which is beneficial to the accuracy of strength testing and calculation.

[0017] Preferably, the third surface is parallel to the surface of the opposite workpiece.

[0018] And / or, the fourth surface is parallel to the surface of the opposite workpiece.

[0019] In this design, the third surface and the opposite workpiece surface are set in parallel, and / or the fourth surface and the opposite workpiece surface are set in parallel, so that the workpiece will not be obstructed by the fixture during the process of being stretched or compressed and moving, thus ensuring the accuracy of the strength test.

[0020] Preferably, the strength testing device further includes a heating chamber, the first clamp and the second clamp are both made of high-temperature resistant material, the workpiece, the first clamp and the second clamp are all disposed inside the heating chamber, and a portion of the first clamp or the second clamp extends out of the heating chamber.

[0021] In this scheme, the workpiece, the first fixture, and the second fixture are all placed inside the heating chamber, so that the workpiece is heated while it is clamped. A part of the first fixture or the second fixture extends out of the heating chamber, so that the workpiece can be loaded from outside the heating chamber. This avoids the loading tool that is in contact with the first fixture or the second fixture from being heated and softened, which would affect the magnitude of the force applied by the loading tool. This enables tensile strength testing of thin-thickness workpieces in a high-temperature environment.

[0022] Preferably, the thickness of the workpiece is no more than 10 mm.

[0023] In this solution, the strength testing device is applied to workpieces with a thickness of no more than 10 mm, which solves the technical problem that the workpiece is not easy to clamp due to its thinness and meets the need for strength testing of thin workpieces.

[0024] A strength testing method, wherein the strength testing method utilizes the strength testing device described above to perform a strength test on the workpiece, the strength testing method comprising:

[0025] The workpiece is clamped between the first fixture and the second fixture;

[0026] A first pressure is applied to either the first clamp or the second clamp along the direction of force to drive the first loading surface to pressurize the first load surface, and simultaneously drive the second loading surface to pressurize the second load surface, and the first pressure is continuously increased until the workpiece is destroyed;

[0027] Record the peak load;

[0028] The cross-sectional area of ​​the workpiece at failure is measured, and the strength of the workpiece is calculated based on the peak load and the cross-sectional area at failure.

[0029] In this scheme, the workpiece is clamped between the first fixture and the second fixture, and a first pressure is applied to either the first fixture or the second fixture in the direction of force, so that the two loading surfaces (the first loading surface and the second loading surface) contact the two load-bearing surfaces (the first load-bearing surface and the second load-bearing surface) respectively, generating compression. Thus, the workpiece is clamped and fixed by position restriction on both ends of the workpiece, and two tensile forces in opposite directions are formed on the workpiece, thereby realizing the tensile strength test.

[0030] Preferably, the strength testing method further includes:

[0031] A second pressure, opposite to the first pressure, is applied to the other of the first and second clamps, and the second pressure is continuously increased until the workpiece is destroyed.

[0032] In this solution, by applying a second pressure opposite to the first pressure to another of the first and second clamps, the workpiece is simultaneously subjected to two opposite external force sources, thereby improving the efficiency of external force loading.

[0033] Preferably, the strength testing method is further used for testing in a heated environment, and the strength testing method further includes:

[0034] The workpiece, the first fixture, or the second fixture is placed inside the heating chamber, and a portion of the first fixture or the second fixture extends outside the heating chamber;

[0035] The heating box heats the workpiece;

[0036] After the step of “recording load peak”, the heating of the heating chamber is stopped, and the workpiece is removed from the heating chamber after cooling.

[0037] In this scheme, the workpiece, the first fixture, and the second fixture are all placed inside the heating chamber, so that the workpiece is heated while it is clamped. A part of the first fixture or the second fixture extends out of the heating chamber, so that the workpiece can be loaded from outside the heating chamber. This avoids the loading tool that is in contact with the first fixture or the second fixture from being heated and softened, which would affect the magnitude of the force applied by the loading tool. This enables the tensile strength test of the workpiece to be performed in a high-temperature environment.

[0038] The positive and progressive effects of this invention are as follows: The strength testing device and method clamp the workpiece between the first clamp and the second clamp, and utilize two load-bearing surfaces (the first load-bearing surface and the second load-bearing surface) in directions different from the force direction, as well as two corresponding contacting loading surfaces (the first loading surface and the second loading surface), to achieve positional restriction of the two load-bearing surfaces of the workpiece. Thus, it cleverly utilizes the structural characteristics of the workpiece itself (the setting direction of the first load-bearing surface and the second load-bearing surface) to achieve clamping and fixing at both ends of the workpiece by positional restriction, without having to clamp the two ends of the workpiece to force clamping. This allows for tensile strength testing of workpieces with small thickness that are difficult to clamp, especially in high-temperature environments where adhesives cannot be used to bond small-thickness workpieces to be tested. Attached Figure Description

[0039] Figures 1a-1c This is a schematic diagram of the assembly structure of the strength testing device and the workpiece in Embodiment 1 of the present invention.

[0040] Figures 2a-2c These are, respectively, a three-dimensional structural diagram, a front view, and a half-sectional view of the workpiece in Embodiment 1 of the present invention.

[0041] Figure 2d This is a schematic diagram of the workpiece being loaded and subjected to load in Embodiment 1 of the present invention.

[0042] Figures 3a-3c These are, respectively, a three-dimensional structural diagram, a front view, and a half-sectional view of the first clamp in Embodiment 1 of the present invention.

[0043] Figures 4a-4c These are, respectively, a three-dimensional structural diagram, a front view, and a half-sectional view of the second clamp in Embodiment 1 of the present invention.

[0044] Figure 5a This is a schematic diagram of the structure of the workpiece after assembly with the first fixture and the second fixture in Embodiment 1 of the present invention.

[0045] Figure 5b for Figure 5a A magnified structural diagram of part B in the middle.

[0046] Figure 6 This is a schematic diagram of the strength testing device in Embodiment 2 of the present invention being tested under high temperature conditions.

[0047] Figure 7 This is a flowchart of the strength testing method in Embodiment 3 of the present invention.

[0048] Figure 8 This is a flowchart of the strength testing method in Embodiment 4 of the present invention.

[0049] Explanation of reference numerals in the attached figures:

[0050] Workpiece 1,

[0051] Upper loading area 15, lower loading area 16, middle test area 17.

[0052] Inner annular surface 13, first load-bearing surface 14,

[0053] Outer annular surface 11, second load-bearing surface 12,

[0054] First clamp 2,

[0055] First loading surface 22,

[0056] Third surface 21,

[0057] Second clamp 3,

[0058] Second loading surface 32,

[0059] Fourth surface 31,

[0060] Heating box 4,

[0061] Downward load F1,

[0062] Upward load F2,

[0063] The tensile load F on the workpiece

[0064] The direction of the force is A. Detailed Implementation

[0065] The present invention will be further illustrated by way of embodiments below, but the present invention is not limited to the scope of the embodiments described herein.

[0066] Example 1

[0067] As shown in Figures 1-5, this embodiment provides a strength testing device for testing the tensile strength of workpiece 1. Workpiece 1 is specifically a ceramic matrix composite material. The ceramic matrix composite material is thin-walled with a relatively small thickness, not exceeding 10 mm. Ceramic matrix composite material is a type of composite material with ceramic as the matrix and various fibers. It usually has excellent properties such as high temperature resistance, high strength and modulus, low density and strong corrosion resistance, and has broad application prospects in aerospace hot-end structural components.

[0068] like Figures 2a-2d As shown, the workpiece 1 has an overall annular structure, divided into an upper loading area 15, a lower loading area 16, and an intermediate test area 17. The inner side of the workpiece 1 includes an inner annular surface 13 and a first load-bearing surface 14, and the outer side of the workpiece 1 includes an outer annular surface 11 and a second load-bearing surface 12. The first load-bearing surface 14 is specifically an annular conical surface protruding inward from the lower loading area 16, and the second load-bearing surface 12 is specifically an annular conical surface protruding outward from the upper loading area 15. The two load-bearing surfaces (the first load-bearing surface 14 and the second load-bearing surface 12) are respectively located at both ends of the workpiece 1 along the force direction A and at an inclination angle different from the force direction A.

[0069] like Figures 1a-1c and Figures 5a-5b As shown, the strength testing device includes a first clamp 2 and a second clamp 3. The first clamp 2 is specifically a circular loading rod, and the second clamp 3 is specifically an annular support base. The workpiece 1 is clamped between the first clamp 2 and the second clamp 3.

[0070] The first clamp 2 has a first loading surface 22 at its lower edge relative to the surface of the workpiece 1, which is in contact with the first load-bearing surface 14. The first loading surface 22 is also an annular conical surface, used to transmit the test load by limiting contact with the workpiece 1. The second clamp 3 has a second loading surface 32 relative to the surface of the workpiece 1, which is in contact with the second load-bearing surface 12. The second loading surface 32 is also an annular conical surface, also used to provide support constraint load by limiting contact with the workpiece 1.

[0071] The workpiece 1 is clamped between the first clamp 2 and the second clamp 3. By using two load-bearing surfaces (the first load-bearing surface 14 and the second load-bearing surface 12) that are in a different direction from the force direction A (i.e. the thickness direction of the workpiece 1 under tension), and two corresponding loading surfaces (the first loading surface 22 and the second loading surface 32) that are in contact with each other, the position of the two load-bearing surfaces of the workpiece 1 is restricted. Thus, by cleverly utilizing the structural characteristics of the workpiece 1 itself (i.e. the first load-bearing surface 14 and the second load-bearing surface 12 of the annular structure workpiece are inclined outwards), the workpiece 1 is clamped and fixed by position restriction on the two ends of the workpiece 1, without having to clamp the two ends of the workpiece 1 under force. This allows the workpiece 1, which is thin and difficult to clamp, to achieve tensile strength testing in its thickness direction.

[0072] During testing, the second clamp 3 is first installed and fixed on the support platform of the strength testing device (not shown in the figure) and kept stationary. Then, the workpiece 1 is placed in the annular cavity of the second clamp 3 in a relatively coaxial position as shown in Figure 5, so that the second load-bearing surface 12 and the second loading surface 32 are well fitted. Then, the first clamp 2 is placed in the annular cavity of the workpiece 1 in a relatively coaxial position as shown in Figure 5, so that the first load-bearing surface 14 and the first loading surface 22 are well fitted. At this point, the workpiece 1 is clamped between the first clamp 2 and the second clamp 3, completing the installation of the workpiece 1, the first clamp 2, and the second clamp 3.

[0073] The compressive load F applied by the testing machine of the strength testing device is transmitted from the upper end face of the first clamp 2 to the first loading surface 22 through the first clamp 2, driving the first loading surface 22 to move. The first loading surface 22 and the first load-bearing surface 14 make limiting contact, so that the compressive load is transmitted from the first loading surface 22 to the first load-bearing surface 14 in the form of interaction force, generating a downward load F1 on the first load-bearing surface 14. At the same time, the second loading surface 32 on the second clamp 3 makes supporting limiting contact with the second load-bearing surface 12 on the test piece 1, and applies an upward load F2 to the second load-bearing surface 12. The resultant force of loads F1 and F2 is equal in magnitude and opposite in direction. Figure 2d As shown, loads F1 and F2 act on the lower loading zone 16 and upper loading zone 15 of the test workpiece 1, respectively, which are the areas belonging to the first loading surface 14 and the second loading surface 12. Between the lower loading zone 16 and the upper loading zone 15, the ceramic matrix composite material located in the intermediate test zone 17 will be subjected to a tensile load in the out-of-plane direction (i.e., the thickness direction, which is the direction of force A), with a magnitude equal to F (F = F1 = F2), and will eventually undergo tensile fracture failure under the action of continuously increasing tensile load. After the test, the stress value obtained by dividing the peak tensile load by the out-of-plane tensile failure cross-sectional area of ​​the test workpiece 1 can be used to characterize the out-of-plane tensile strength performance of the test workpiece 1.

[0074] In other embodiments, the shape and material of the test workpiece 1 can also be suitable for clamping by the strength testing device. The thickness of workpiece 1 can also be other, thicker or thinner dimensions, provided that the clamping effect and testing requirements are met. The load applied by the testing machine can also act on the second clamp 3, or simultaneously on the first clamp 2 and the second clamp 3, to improve the efficiency of the loading test.

[0075] Among them, such as Figure 2d As shown, the two load-bearing surfaces (first load-bearing surface 14 and second load-bearing surface 12) extend outward in a consistent manner relative to the inner annular surface 13 and outer annular surface 11 of the workpiece 1. Correspondingly, the two loading surfaces (first loading surface 22 and second loading surface 32) also extend outward in a direction away from the workpiece 1. This results in the two clamps exerting extrusive forces on the two load-bearing surfaces in opposite directions, thus achieving a tensile strength test. However, in other embodiments, the protruding directions of the first load-bearing surface 14 and the second load-bearing surface 12 can also extend inward in a consistent manner relative to the outer surface of the workpiece 1. In this case, the two clamps exert extrusive forces on the workpiece 1 in opposite directions, achieving a compressive strength test.

[0076] Among them, such as Figure 5b As shown, the extension directions of the first loading surface 22 and the second loading surface 32 are parallel to each other, which allows equal force to be applied to the two load-bearing surfaces of the workpiece 1. This is beneficial for the workpiece 1 to be subjected to stable force, avoids uneven force and displacement, and makes the strength test more stable.

[0077] Among them, such as Figures 3a-3c and Figures 4a-4c ,as well as Figures 5a-5b As shown, the inner ring surface 13 of the workpiece 1 includes the inner surface of the intermediate test area 17 and the inner surface of the extended upper loading area 15. The surface of the first fixture 2 relative to the workpiece 1 also includes a third surface 21, that is, the third surface 21 is relative to the inner ring surface 13, and the third surface 21 is in clearance fit with the inner ring surface 13.

[0078] The outer ring surface 11 of the workpiece 1 includes the outer surface of the intermediate test area 17 and the outer surface of the extended lower loading area 16. The surface of the second fixture 3 relative to the workpiece 1 also includes a fourth surface 31, that is, the fourth surface 31 is relative to the outer ring surface 11, and the fourth surface 31 is clearance-fitted with the outer ring surface 11.

[0079] In other embodiments, under sufficient tensile force, one of the third surface 21 and the fourth surface 31 can also be fitted with the corresponding inner ring surface 13 or outer ring surface 11, while the other of the third surface 21 and the fourth surface 31 can be in clearance fit with the corresponding inner ring surface 13 or outer ring surface 11, i.e., there is some frictional resistance, which can also achieve tensile strength testing. However, it is not as good as the clearance fit between the third surface 21 and the inner ring surface 13 in this embodiment, so that there is no resistance when the first clamp 2 moves; and the clearance fit between the fourth surface 31 and the outer ring surface 11, so that there is no resistance when the second clamp 3 moves; thereby ensuring the uniqueness of the load transfer path and the accuracy of the test results.

[0080] Among them, the inner ring surface 13 has a regular planar structure; the outer ring surface 11 also has a regular planar structure; the third surface 21 is parallel to the opposite inner ring surface 13, and the fourth surface 31 is parallel to the opposite outer ring surface 11, so that the workpiece 1 will not be hindered by the fixture during the process of being stretched or compressed, thus ensuring the accuracy of the strength test.

[0081] Example 2

[0082] like Figure 6 As shown, this embodiment provides another strength testing device that can be used for strength testing in high-temperature environments.

[0083] The strength testing device in this embodiment is largely the same as the strength testing device in Embodiment 1, except that:

[0084] The strength testing device also includes a heating chamber 4, which is specifically a high-temperature environment chamber. The first clamp 2 and the second clamp 3 are both made of high-temperature resistant materials, such as SiC ceramics or high-strength graphite.

[0085] During the test, workpiece 1, first fixture 2, and second fixture 3 are placed together inside a high-temperature environment chamber, with a portion of the first fixture 2 extending beyond the high-temperature zone through a connecting hole (not shown in the figure) in the chamber. The compressive load F applied by the testing machine acts on the portion of the first fixture 2 extending beyond the high-temperature environment chamber and transfers the test load to the test workpiece 1.

[0086] In this process, the workpiece 1, the first clamp 2, and the second clamp 3 are all placed inside the heating chamber 4, so that the workpiece 1 is heated while in a clamped state. A part of the first clamp 2 extends out of the heating chamber 4, so that the workpiece 1 can be loaded from outside the heating chamber 4. This avoids the loading tool that is in contact with the first clamp 2 being heated and softened, which would affect the magnitude of the force applied by the loading tool. This enables tensile strength testing of a thin-thickness workpiece 1 in a high-temperature environment.

[0087] In other embodiments, the load applied by the testing machine can also be applied to the second clamp 3, in which case a part of the second clamp 3 needs to extend outside the heating chamber 4 to apply the load from outside the heating chamber 4 and transfer it to the workpiece 1.

[0088] Example 3

[0089] like Figure 7 As shown, this embodiment provides a strength testing method. This strength testing method utilizes the strength testing device as described in Embodiment 1 or Embodiment 2 to perform a strength test on the workpiece 1. The strength testing method includes:

[0090] S10. Clamp the workpiece 1 between the first fixture 2 and the second fixture 3;

[0091] S20. Apply a first pressure to either the first clamp 2 or the second clamp 3 along the force direction A to drive the first loading surface 22 to press against the first load-bearing surface 14, and at the same time drive the second loading surface 32 to press against the second load-bearing surface 12, and continue to increase the first pressure until the workpiece 1 is destroyed.

[0092] S30, Record the peak load;

[0093] S40. Measure the cross-sectional area of ​​the workpiece 1 at failure, and calculate the strength of the workpiece 1 based on the peak load and the cross-sectional area at failure.

[0094] The workpiece 1 is clamped between the first clamp 2 and the second clamp 3, and a first pressure is applied to either the first clamp 2 or the second clamp 3 in the direction of force, so that the two loading surfaces (the first loading surface 22 and the second loading surface 32) contact the two load-bearing surfaces (the first load-bearing surface 14 and the second load-bearing surface 12) respectively, generating compression. Thus, the workpiece 1 is clamped and fixed by position restriction on both ends of the workpiece 1, and two tensile forces in opposite directions are formed on the workpiece 1, thereby realizing the tensile strength test.

[0095] Step S20 may further include:

[0096] A second pressure, opposite to the first pressure, is applied to another of the first clamp 2 and the second clamp 3, and the second pressure is continuously increased until the workpiece 1 is destroyed.

[0097] By applying a second pressure opposite to the first pressure to another of the first clamp 2 and the second clamp 3, the workpiece 1 is subjected to two opposite external force sources at the same time, thereby improving the efficiency of external force loading.

[0098] Example 4

[0099] like Figure 8As shown, this embodiment provides a strength testing method. This strength testing method uses the strength testing device as described in Embodiment 2 to perform a strength test on workpiece 1 in a high-temperature environment. The strength testing method includes:

[0100] S100. Clamp the workpiece 1 between the first fixture 2 and the second fixture 3;

[0101] S101. Place the workpiece 1, the first clamp 2, and the second clamp 3 into the heating box 4, and extend a portion of the first clamp 2 out of the heating box 4;

[0102] S102, Heating box 4 heats workpiece 1 and maintains the high-temperature environment temperature required by the design;

[0103] S200. The first pressure is applied to the first fixture 2 along the force direction by the testing machine, so as to drive the first loading surface 22 to press the first load-bearing surface 14, and at the same time drive the second loading surface 32 to press the second load-bearing surface 12, and continue to increase the first pressure until the workpiece 1 is destroyed.

[0104] S300, record peak load;

[0105] S301. Cut off the power supply to the heating box 4 and cool it down. After cooling is completed, take the workpiece 1 out of the heating box 4.

[0106] S400. Measure the cross-sectional area of ​​the workpiece 1 under out-of-plane tension failure, and calculate the strength of workpiece 1 based on the peak load and the cross-sectional area of ​​failure.

[0107] Workpiece 1, first clamp 2, and second clamp 3 are all placed inside heating chamber 4, so that workpiece 1 is heated in the clamped state; a part of the first clamp 2 extends out of heating chamber 4, so that workpiece 1 can be loaded from outside heating chamber 4, avoiding the loading tool that is in contact with the first clamp 2 from being heated and softened, which would affect the magnitude of the force applied by the loading tool, thus realizing the tensile strength test of workpiece 1 in a high temperature environment.

[0108] In other embodiments, the load applied by the testing machine can also be applied to the second clamp 3, in which case a part of the second clamp 3 needs to extend outside the heating chamber 4 to apply the load from outside the heating chamber 4 and transfer it to the workpiece 1.

[0109] While specific embodiments of the present invention have been described above, those skilled in the art should understand that these are merely illustrative examples, and the scope of protection of the present invention is defined by the appended claims. Those skilled in the art can make various changes or modifications to these embodiments without departing from the principles and essence of the present invention, but all such changes and modifications fall within the scope of protection of the present invention.

Claims

1. A strength testing device for testing the tensile strength of a workpiece, wherein the workpiece has a first load-bearing surface and a second load-bearing surface at both ends along the force direction, which are different from the force direction, and the first load-bearing surface and the second load-bearing surface are located on both sides of the workpiece, and the first load-bearing surface and the second load-bearing surface extend outward in a consistent manner relative to the outer surface of the workpiece. Its features are, The strength testing device includes a first clamp and a second clamp, and the workpiece is clamped between the first clamp and the second clamp; The first fixture has a first loading surface that contacts and engages with the first load-bearing surface on the surface of the workpiece, and the second fixture has a second loading surface that contacts and engages with the second load-bearing surface on the surface of the workpiece. The workpiece further includes an intermediate test area, with the first load-bearing surface and the second load-bearing surface respectively located at both ends of the intermediate test area along the force direction. The first fixture, relative to the surface of the workpiece, further includes a third surface, which is in clearance fit with the extended surface of the intermediate test area. And / or, the second fixture further includes a fourth surface relative to the surface of the workpiece, the fourth surface being clearance-fitted with the extended surface of the intermediate test area.

2. The strength testing device as described in claim 1, characterized in that, The extension directions of the first loading surface and the second loading surface are parallel to each other.

3. The strength testing device as described in claim 1, characterized in that, The third surface is parallel to the surface of the opposite workpiece. And / or, the fourth surface is parallel to the surface of the opposite workpiece.

4. The strength testing device as described in claim 1, characterized in that, The strength testing device also includes a heating chamber. The first fixture and the second fixture are both made of high-temperature resistant materials. The workpiece, the first fixture, and the second fixture are all disposed inside the heating chamber, and a portion of the first fixture or the second fixture extends out of the heating chamber.

5. The strength testing device as described in claim 1, characterized in that, The workpiece is made of ceramic matrix composite material.

6. The strength testing device as described in claim 1, characterized in that, The thickness of the workpiece is no more than 10 millimeters.

7. A strength testing method, characterized in that, The strength testing method utilizes the strength testing apparatus as described in any one of claims 1-6 to perform a strength test on the workpiece, and the strength testing method includes: The workpiece is clamped between the first fixture and the second fixture; A first pressure is applied to either the first clamp or the second clamp along the direction of force to drive the first loading surface to pressurize the first load surface, and simultaneously drive the second loading surface to pressurize the second load surface, and the first pressure is continuously increased until the workpiece is destroyed; Record the peak load; The cross-sectional area of ​​the workpiece at failure is measured, and the strength of the workpiece is calculated based on the peak load and the cross-sectional area at failure.

8. The strength testing method as described in claim 7, characterized in that, The strength testing method further includes: A second pressure, opposite to the first pressure, is applied to the other of the first and second clamps, and the second pressure is continuously increased until the workpiece is destroyed.

9. The strength testing method as described in claim 7, characterized in that, The strength testing method is also used for testing in a heated environment, and the strength testing method further includes: The workpiece, the first fixture, or the second fixture is placed inside the heating chamber, and a portion of the first fixture or the second fixture extends outside the heating chamber; The heating box heats the workpiece; After the step "record load peak", stop heating the heating chamber, and remove the workpiece from the heating chamber after cooling.

Citation Information

Patent Citations

  • Fiber reinforced composite material tube interlaminar shear strength testing device and testing method