Photovoltaic cell, photovoltaic cell assembly and method for manufacturing photovoltaic cell
By providing a groove on the backlight surface of the photovoltaic cell and covering the groove wall with a tunnel oxide layer and a polysilicon layer, combined with the staggered arrangement of the tunnel oxide layer and polysilicon layer in the anti-reflection layer, the conversion efficiency of TBC cells is solved. It reduces the problem and achieves the effect of improving the electron migration rate and battery efficiency.
Patent Information
- Application Number
- CN202311819755.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-27
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2043-12-27
AI Technical Summary
The cell conversion efficiency in the tunnel layer passivated back contact cell (TBC) is low, and the electron migration rate needs to be increased to increase the short-circuit current.
A first groove is provided on the base backlight surface of the photovoltaic cell. The first passivation structure includes a first tunnel oxide layer and a first polysilicon layer covering the groove wall. The second passivation structure is provided in the anti-reflection layer. In the layer, the second tunnel oxide layer and the second polysilicon layer are stacked, and the first and second passivation structures are projected to be staggered along the first direction to increase the area of the tunnel oxide layer to accelerate electron migration.
By increasing the tunnel oxide layer area, the electron migration rate is increased, thereby increasing the short-circuit current and battery conversion efficiency.
Smart Images

Figure CN117766598B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of photovoltaic cells, and in particular to a photovoltaic cell, a photovoltaic cell assembly and a method for manufacturing a photovoltaic cell. Background Art
[0002] When non-renewable energy sources such as coal and oil are frequently in short supply, energy issues have gradually become a bottleneck restricting social and economic development. Therefore, more and more countries have begun to develop solar energy resources to seek new impetus for economic development. In this environment, photovoltaic cells have a broader development prospect. Among various types of photovoltaic cells, the all-back contact cell (IBC) has a higher light absorption efficiency because both the positive and negative electrodes are located on the backlight side and there is no component blocking the light-facing side of the cell. On this basis, the tunneling layer passivated contact back contact cell (TBC) combines the advantages of the tunneling oxide passivation cell (TOPCon) tunneling oxide passivation cell (TOPCon) tunneling oxide passivation cell (TBC) and the advantage of no grid lines on the front of the all-back contact cell (IBC). However, in the related technology, the cell conversion efficiency of some tunneling layer passivation contact back contact cells (TBC) still needs to be improved. Summary of the invention
[0003] Based on this, it is necessary to provide a photovoltaic cell, a photovoltaic cell assembly and a method for manufacturing a photovoltaic cell, which can accelerate the electron migration rate to increase the short-circuit current and improve the cell conversion efficiency.
[0004] A photovoltaic cell, comprising:
[0005] A substrate, the substrate having a light-facing surface and a backlight surface arranged opposite to each other along a first direction, the backlight surface being provided with a first groove, wherein the first direction is a thickness direction of the substrate;
[0006] A first passivation structure is disposed in the first groove, wherein the first passivation structure includes a first tunneling oxide layer covering a groove wall of the first groove, and a first polysilicon layer stacked on the first tunneling oxide layer;
[0007] an anti-reflection layer, disposed on one side of the backlight surface of the substrate to cover the backlight surface and the first passivation structure; and
[0008] A second passivation structure is disposed in the anti-reflection layer; the second passivation structure comprises a second tunneling oxide layer and a second polysilicon layer which are stacked;
[0009] The first polysilicon layer and the second polysilicon layer have different doping types; and the projections of the first passivation structure and the second passivation structure in the first direction are staggered with each other.
[0010] In one embodiment, the first tunneling oxide layer covers the groove wall of the first groove to define a first accommodating cavity;
[0011] The first polysilicon layer fills the first receiving cavity.
[0012] In one embodiment, the anti-reflection layer comprises:
[0013] a first anti-reflection film, covering the backlight surface and the first passivation structure; the first anti-reflection film is provided with a second groove, and the second passivation structure is at least partially provided in the second groove; and
[0014] A second anti-reflection film covers a side of the first anti-reflection film away from the substrate and the second passivation structure.
[0015] In one of the embodiments, a side of the second passivation structure along the first direction away from the second anti-reflection film is flush with the backlight surface.
[0016] In one embodiment, the second tunneling oxide layer covers the groove wall of the second groove to define a second accommodating cavity;
[0017] The second polysilicon layer fills the second receiving cavity.
[0018] In one embodiment, the photovoltaic cell further includes a first electrode and a second electrode;
[0019] The first electrode is in ohmic contact with the first passivation structure through the anti-reflection layer;
[0020] The second electrode is in ohmic contact with the second passivation structure through the anti-reflection layer.
[0021] In one embodiment, the photovoltaic cell includes a plurality of the first passivation structures and a plurality of the second passivation structures;
[0022] The first passivation structure and the second passivation structure are alternately distributed along the second direction;
[0023] The second direction is perpendicular to the first direction and perpendicular to the longitudinal extension direction of the first groove.
[0024] A photovoltaic cell assembly comprises a plurality of the above-mentioned photovoltaic cells and a frame. The plurality of photovoltaic cells are spliced and installed in the frame.
[0025] A method for manufacturing a photovoltaic cell, the method comprising the following steps:
[0026] The first groove is formed on the backlight surface of the substrate;
[0027] Depositing the first tunneling oxide layer and the first polysilicon layer in sequence on the backlight side of the substrate;
[0028] The second passivation structure and the anti-reflection layer are deposited.
[0029] In one embodiment, depositing the first tunneling oxide layer and the first polysilicon layer in sequence on the backlight side of the substrate comprises:
[0030] Depositing the first tunneling oxide layer on the backlight side of the substrate so that the first tunneling oxide layer covers the backlight surface and the groove wall of the first groove;
[0031] Depositing the first polysilicon layer on a side of the first tunnel oxide layer facing away from the substrate;
[0032] Portions of the first tunnel oxide layer and the first polysilicon layer protruding from the backlight surface are removed.
[0033] In one embodiment, the first polysilicon layer is deposited by a solution method so that an end surface of the first polysilicon layer facing away from the first tunnel oxide layer is parallel to the backlight surface.
[0034] In one embodiment, depositing the second passivation structure and the anti-reflection layer comprises:
[0035] Depositing a first anti-reflection film on the backlight side of the substrate so that the first anti-reflection film covers the backlight surface and the first passivation structure;
[0036] A second groove is formed on the first anti-reflection film, wherein the second groove is staggered from the projection of the first groove along the first direction, and the depth of the second groove is not less than the thickness of the first anti-reflection film;
[0037] sequentially depositing the second tunneling oxide layer and the second polysilicon layer in the second groove;
[0038] A second anti-reflection film is deposited on a side of the first anti-reflection film and the second passivation structure facing away from the substrate.
[0039] In one embodiment, the sequentially depositing the second tunneling oxide layer and the second polysilicon layer in the second groove includes:
[0040] Depositing the second tunneling oxide layer so that the second tunneling oxide layer covers a side of the first anti-reflection film away from the substrate and a groove wall of the second groove;
[0041] Depositing the second polysilicon layer on a side of the second tunnel oxide layer facing away from the substrate;
[0042] Portions of the second tunneling oxide layer and the second polysilicon layer protruding from the first anti-reflection film are removed.
[0043] In the photovoltaic cell, photovoltaic cell assembly and photovoltaic cell manufacturing method, the backlight surface of the substrate is provided with a first groove, and in the first passivation structure, the first tunneling oxide layer covers the groove wall of the first groove, and the first polysilicon layer is stacked on the first tunneling oxide layer. The second passivation structure is staggered from the projection of the first passivation structure along the first direction so that the battery will not leak. Compared with the structure of depositing a flat first tunneling oxide layer directly on the backlight surface in the related art, in the embodiment of the present application, the first tunneling oxide layer is located in the first groove and covers the groove wall of the first groove, which can increase the area of the first tunneling oxide layer (compared with direct deposition on the backlight surface, it is equivalent to increasing the part of the first tunneling oxide layer covered on the groove wall extending along the first direction). The larger area of the first tunneling oxide layer is conducive to accelerating the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] FIG. 1 is a schematic diagram of the structure of a photovoltaic cell in an embodiment of the present application.
[0045] FIG. 2 is a schematic diagram of the structure after step S100 in one embodiment of the present application.
[0046] FIG. 3 is a schematic diagram of the structure after step S220 in one embodiment of the present application.
[0047] FIG. 4 is a schematic diagram of the structure after step S230 in one embodiment of the present application.
[0048] FIG. 5 is a schematic diagram of the structure after step S310 in one embodiment of the present application.
[0049] FIG. 6 is a schematic diagram of the structure after step S320 in one embodiment of the present application.
[0050] FIG. 7 is a schematic diagram of the structure after step S332 in one embodiment of the present application.
[0051] FIG. 8 is a schematic diagram of the structure after step S333 in one embodiment of the present application.
[0052] Reference numerals:
[0053] 100, substrate; 110, light-facing surface; 120, backlight surface; 121, first groove; 200, first passivation structure; 210, first tunneling oxide layer; 211, third extension portion; 212, fourth extension portion; 220, first polysilicon layer; 300, second passivation structure; 310, second tunneling oxide layer; 311, first extension portion; 312, second extension portion; 320, second polysilicon layer; 400, anti-reflection layer; 410, first anti-reflection film; 411, second groove; 420, second anti-reflection film. DETAILED DESCRIPTION
[0054] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.
[0055] In the description of the present application, it should be understood that if the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc. appear, the orientation or position relationship indicated by these terms is based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.
[0056] In addition, if the terms "first" or "second" appear, these terms are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of this application, if the term "plurality" appears, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0057] In this application, unless otherwise clearly specified and limited, if the terms "installed", "connected", "connected", "fixed" and the like appear, these terms should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.
[0058] In the present application, unless otherwise clearly specified and limited, if there is a description that a first feature is "above" or "below" a second feature, etc., or similar descriptions appear, it may mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, the first feature being "above", "above" and "above" the second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. The first feature being "below", "below" and "below" the second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0059] It should be noted that if an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. If an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. If any, the terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used in this application are for illustrative purposes only and do not represent the only implementation method.
[0060] Referring to FIG. 1 and FIG. 2 , a photovoltaic cell provided in an embodiment of the present application includes a substrate 100, a first passivation structure 200, a second passivation structure 300 and an anti-reflection layer 400. The substrate 100 has a light-facing surface 110 and a backlight surface 120 arranged opposite to each other along a first direction, and the backlight surface 120 is provided with a first groove 121, wherein the first direction is the thickness direction of the substrate 100. The first passivation structure 200 is arranged in the first groove 121, and includes a first tunneling oxide layer 210 covering the groove wall of the first groove 121, and a first polysilicon layer 220 stacked on the first tunneling oxide layer 210. The anti-reflection layer 400 is arranged on the backlight surface 120 side of the substrate 100 to cover the backlight surface 120 and the first passivation structure 200. The second passivation structure 300 is arranged in the anti-reflection layer 400, and includes a second tunneling oxide layer 310 and a second polysilicon layer 320 stacked. The first polysilicon layer 220 and the second polysilicon layer 320 have different doping types, and the projections of the second passivation structure 300 and the first passivation structure 200 in the first direction are staggered with each other.
[0061] In the photovoltaic cell, the backlight surface 120 of the substrate 100 is provided with a first groove 121, and in the first passivation structure 200, the first tunneling oxide layer 210 covers the groove wall of the first groove 121, and the first polysilicon layer 300 is stacked on the first tunneling oxide layer 200. The projection of the second passivation structure 300 and the first passivation structure 200 along the first direction is staggered so that the battery will not leak. Compared with the structure of directly depositing a flat first tunneling oxide layer 210 on the backlight surface 120 in the related art, in the embodiment of the present application, the first tunneling oxide layer 210 is located in the first groove 121 and covers the groove wall of the first groove 121, which can increase the area of the first tunneling oxide layer 210 (compared with directly depositing a flat first tunneling oxide layer 210 on the backlight surface 120, it is equivalent to adding the part of the first tunneling oxide layer 210 covering the groove wall extending along the first direction, that is, the third extension portion 211 shown in FIG. 4). The first tunnel oxide layer 210 has a larger area, which is beneficial to accelerating the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency.
[0062] Specifically, in some embodiments, the first tunneling oxide layer 210 covers the groove wall of the first groove 121 to define a first accommodating cavity, and the first polysilicon layer 220 fills the first accommodating cavity so that the side of the entire first passivation structure 200 facing away from the light-facing surface 110 is flush with the backlight surface 120 of the substrate 100.
[0063] In the embodiment shown in the drawings, the doping type of the substrate 100 is n-type, the doping type of the first polysilicon layer 220 is p-type, and the doping type of the second polysilicon layer 320 is n-type.
[0064] In other embodiments, the doping type of the substrate 100 may also be p-type, the doping type of the first polysilicon layer 220 may be n-type, and the doping type of the second polysilicon layer 320 may be p-type.
[0065] 1 and 6 , in some embodiments, the anti-reflection layer includes a first anti-reflection film 410 and a second anti-reflection film 420. The first anti-reflection film 410 covers the backlight surface 120 and the first passivation structure 200. The first anti-reflection film 410 is provided with a second groove 411. The second passivation structure 300 is at least partially provided in the second groove 411. The second anti-reflection film 420 covers the side of the first anti-reflection film 410 away from the substrate 100 and the second passivation structure 300.
[0066] Referring to FIG. 1 and FIG. 8 , in some embodiments, the side of the second passivation structure 300 away from the second anti-reflection film 420 along the first direction is flush with the backlight surface 120. That is, the entire second passivation structure 300 is located entirely within the second groove 411. As described above, the projections of the second passivation structure 300 and the first passivation structure 200 along the first direction are staggered so that the battery will not leak electricity. In the above embodiment, the side of the second passivation structure 300 away from the second anti-reflection film 420 along the first direction is flush with the backlight surface 120, so that the projections of the second passivation structure 300 and the first passivation structure 200 along the second direction (the second direction is perpendicular to the first direction and perpendicular to the longitudinal extension direction of the first groove 121) have no overlapping parts, and the isolation effect is better, which can further ensure that the battery will not leak electricity and has higher safety. In addition, the second passivation structure 300 is flush with the backlight surface 120 and does not extend into the interior of the substrate 100, so as not to cause damage to the substrate 100.
[0067] In other embodiments, the second passivation structure 300 may also extend into the interior of the substrate 100 , that is, a portion of the second passivation structure 300 is disposed in the anti-reflection layer 400 , and another portion is disposed in the substrate 100 .
[0068] Referring to FIG. 1 and FIG. 6 , in some embodiments, the second tunneling oxide layer 310 covers the groove wall of the second groove 411 to define a second receiving cavity, and the second polysilicon layer 320 is filled in the second receiving cavity.
[0069] Compared with the structure of directly depositing the flat second tunnel oxide layer 310 in the related art, the above embodiment is equivalent to adding the second tunnel oxide layer 310 extending along the first direction. In this way, the area of the second tunnel oxide layer 310 can be made larger, which is conducive to further accelerating the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency.
[0070] Referring to Figures 1 and 8, specifically, in some embodiments, the second tunneling oxide layer 310 includes a first extension portion 311 extending along a first direction, and a second extension portion 312 extending along a second direction, the first extension portion 311 extends from the second extension portion 312 toward a side away from the light-facing surface 110, the first extension portion 311 and the second extension portion 312 enclose a second accommodating cavity, and the second polysilicon layer 320 is filled in the second accommodating cavity.
[0071] Specifically, the first extension part 311 is connected to the edge of the second extension part 312 so that the annular first extension part 311 surrounds the edge of the second extension part 312. The second extension part 312 and the annular first extension part 311 enclose a second accommodating cavity that is open on the side facing away from the light-facing surface 110, and the second polysilicon layer 320 is filled in the second accommodating cavity. Compared with the structure of directly depositing a flat second tunneling oxide layer 310 in the related art, the above embodiment is equivalent to adding a first extension part 311 extending along the first direction. In this way, the area of the second tunneling oxide layer 310 can be made larger, which is conducive to further accelerating the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency.
[0072] In other embodiments, the first extension portion 311 may be provided only at the edge of the second extension portion 312 , which can also increase the area of the second tunnel oxide layer 310 to a certain extent, thereby improving the battery conversion efficiency.
[0073] Referring to Figures 1, 2 and 4, similarly, in some embodiments, the first tunnel oxide layer 210 includes a third extension portion 211 extending along the first direction, and a fourth extension portion 212 extending along the second direction, the third extension portion 211 extends from the fourth extension portion 212 toward a side away from the light surface 110, and the third extension portion 211 and the fourth extension portion 212 enclose a first accommodating cavity.
[0074] Specifically, the third extension portion 211 covers the groove wall of the first groove 121 extending along the first direction, and the fourth extension portion 212 covers the groove wall of the first groove 121 extending along the second direction. In the embodiment shown in the drawings, all areas of the groove wall of the first groove 121 extending along the first direction are covered with the third extension portion 211, that is, the edge of the fourth extension portion 212 is connected to the third extension portion 211, so that the annular third extension portion 211 surrounds the edge of the fourth extension portion 212. The fourth extension portion 212 and the annular third extension portion 211 surround a first accommodating cavity with an opening on the side away from the light-facing surface 110, and the first polysilicon layer 220 is filled in the first accommodating cavity. Compared with the structure of depositing a flat first tunneling oxide layer 210 directly on the backlight surface 120 in the related art, the above embodiment is equivalent to adding this part of the first tunneling oxide layer 210 extending along the first direction, that is, adding the third extension portion 211. In this way, the area of the first tunnel oxide layer 210 can be made larger, which is beneficial to further accelerate the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency.
[0075] In other embodiments, the third extension portion 211 may be covered only on a partial area of the groove wall extending along the first direction of the first groove 121, that is, the third extension portion 211 is connected only to the edge portion of the fourth extension portion 212, which can also increase the area of the first tunneling oxide layer 210 to a certain extent, thereby improving the battery conversion efficiency.
[0076] In some embodiments, the photovoltaic cell further includes a first electrode and a second electrode; the first electrode is in ohmic contact with the first passivation structure 200 through the anti-reflection layer 400; and the second electrode is in ohmic contact with the second passivation structure 300 through the anti-reflection layer 400.
[0077] 1 , in some embodiments, the photovoltaic cell includes a plurality of first passivation structures 200 and a plurality of second passivation structures 300 , and the first passivation structures 200 and the second passivation structures 300 are alternately spaced and distributed along a second direction, wherein the second direction is perpendicular to the first direction and perpendicular to the longitudinal extension direction of the first groove 121 .
[0078] In some embodiments, the photovoltaic cell assembly includes a plurality of photovoltaic cells according to any one of the aforementioned embodiments, and also includes a frame, and the plurality of photovoltaic cells are spliced and arranged and are all installed in the frame.
[0079] Referring to FIG. 1 and FIG. 2 , in some embodiments, the method for manufacturing the photovoltaic cell in any of the above embodiments comprises the following steps:
[0080] S100, forming a first groove 121 on the backlight surface 120 of the substrate 100;
[0081] S200, depositing a first tunneling oxide layer 210 and a first polysilicon layer 220 in sequence on the backlight side of the substrate 100;
[0082] S300 , depositing a second passivation structure 300 and an anti-reflection layer 400 .
[0083] Specifically, the first groove 121 is recessed from the backlight surface 120 along the first direction toward the inside of the substrate 100. In step S200, when depositing the first tunnel oxide layer 210, it usually follows the morphology of the backlight side of the substrate 100, so that the first tunnel oxide layer 210 is deposited on the backlight surface 120 and the groove wall of the first groove 121, thereby increasing the area of the first tunnel oxide layer 210, which is conducive to accelerating the electron migration rate, thereby increasing the short-circuit current and improving the battery conversion efficiency.
[0084] In some embodiments, before step S100 , the method further includes: performing a texturing treatment on the surface of the substrate 100 .
[0085] Specifically, the n-type substrate 100 is immersed in a KOH or NaOH solution with a temperature of 60° C. to 80° C. and a mass fraction of 1% to 3% to perform double-sided texturing for a texturing time of 15 to 25 minutes.
[0086] In some embodiments, in step S100, the first groove 121 is formed by laser grooving. The depth of the first groove 121 is 30-60 nm, and the width is 1.5 times that of the positive electrode grid line.
[0087] Referring to FIG. 2 to FIG. 4 , in some embodiments, step S200 includes:
[0088] S210, depositing a first tunnel oxide layer 210 on the backlight side of the substrate 100, so that the first tunnel oxide layer 210 covers the backlight surface 120 and the groove wall of the first groove 121;
[0089] S220, depositing a first polysilicon layer 220 on a side of the first tunnel oxide layer 210 facing away from the substrate 100;
[0090] S230 , removing the portions of the first tunnel oxide layer 210 and the first polysilicon layer 220 protruding from the backlight surface 120 .
[0091] Specifically, in step S210, a thermal oxidation method or CVD method is used to deposit and form a first tunnel oxide layer 210. The material of the first tunnel oxide layer 210 is silicon dioxide. The specific process can directly adopt the existing technology, which will not be repeated here. When the first tunnel oxide layer 210 is deposited, since the first groove 121 is provided on the backlight surface 120, the first tunnel oxide layer 210 can be covered on the backlight surface 120 and the groove wall of the first groove 121 during deposition.
[0092] In step S220 , after the first tunnel oxide layer 210 is deposited, a boron-doped first polysilicon layer 220 is deposited on its surface. The deposition thickness of the first polysilicon layer 220 is large so that the end face away from the first tunnel oxide layer 210 can exceed the depth range of the first groove 121 .
[0093] In step S230, the first tunnel oxide layer 210 and the first polysilicon layer 220 are removed, and the portion protruding from the backlight surface 120 can be obtained, and the structure shown in FIG. 4 can be obtained. The first tunnel oxide layer 210 and the first polysilicon layer 220 are only distributed in the first groove 121. Usually, when the first polysilicon layer 220 is formed, a borosilicate glass layer is also formed on its surface away from the first tunnel oxide layer 210. Therefore, in step S230, the borosilicate glass layer is first removed by chain cleaning, and then the first tunnel oxide layer 210 and the first polysilicon layer 220 outside the range of the first groove 121 are etched and removed by an alkaline etchant (including one of KOH, NaOH and TMAH, etc.), that is, the portion of the first tunnel oxide layer 210 and the first polysilicon layer 220 protruding from the backlight surface 120 is removed.
[0094] In the above embodiment, the first tunnel oxide layer 210 and the first polysilicon layer 220 are first deposited in sequence on the entire backlight surface 120 and the groove wall of the first groove 121, and then the portions of the two protruding from the backlight surface 120 are removed, so that the two are only distributed in the first groove 121. Compared with direct deposition in the first groove 121, there is no need to shield the area outside the first groove 121, and the operation difficulty is lower.
[0095] 2 to 4 , in some embodiments, the first polysilicon layer 220 is deposited by a solution process, so that the end surface of the first polysilicon layer 220 facing away from the first tunnel oxide layer 210 is parallel to the backlight surface 120 .
[0096] Specifically, the solution method may be a sol-gel method, chemical plating, etc. When the solution method is used for deposition, the end surface of the first polysilicon layer 220 away from the first tunnel oxide layer 210 may be a flat shape protruding from the backlight surface 120, rather than a curved surface following the shape of the first tunnel oxide layer 210 (the portion corresponding to the range of the first groove 121 may not protrude from the backlight surface 120, and the portion corresponding to the outside of the range of the first groove 121 protrudes from the backlight surface 120). In this way, in step S230, it is only necessary to remove all the structures protruding from the surface of the backlight surface 120, which makes the operation less difficult.
[0097] Further, a certain proportion of silicate (such as tetraethyl orthosilicate) or silicon tetrachloride, ethanol and distilled water mixture (N-type doping source can be phosphorus oxychloride, phosphine, etc., P-type doping source can be boron trichloride, borane, etc.), and then hydrochloric acid, sodium hydroxide, ammonia and other catalysts are added to accelerate the sol-gel reaction, magnetic stirring for 5-12 hours, standing for 12-48 hours, and then using spin coating to prepare a thin film on the substrate 100. Finally, the thin film is dried at 200-300°C, and then annealed at 1000-1200°C to obtain the first polysilicon layer 220.
[0098] In a specific embodiment, the ratio of tetraethyl orthosilicate, ethanol, and distilled water is 1:4:4 (the N-type doping source can be phosphorus oxychloride, phosphine, etc., and the P-type doping source can be boron trichloride, borane, etc.), and then 5%-15% of sodium hydroxide is added to accelerate the reaction, magnetic stirring is performed for 5 hours, and the film is allowed to stand for 24 hours, and then a spin coating method is used to prepare a thin film on the substrate 100. Finally, the film is dried at 250°C and then annealed at 1000°C to obtain the first polysilicon layer 220.
[0099] Referring to FIGS. 5 to 8 and FIG. 1 , in some embodiments, step S300 includes:
[0100] S310, depositing a first anti-reflection film 410 on the backlight side of the substrate 100, so that the first anti-reflection film 410 covers the backlight surface 120 and the first passivation structure 200;
[0101] S320, opening a second groove 411 on the first anti-reflection film 410, wherein the second groove 411 is staggered from the projection of the first groove 121 along the first direction, and the depth of the second groove 411 is not less than the thickness of the first anti-reflection film 410;
[0102] S330, depositing the second tunneling oxide layer 310 and the second polysilicon layer 320 in the second groove 411 in sequence, so that the second tunneling oxide layer 310 covers the groove wall of the second groove 411, and the second polysilicon layer 320 fills the second accommodation cavity surrounded by the second tunneling oxide layer 310;
[0103] S340 , depositing a second anti-reflection film 420 on the side of the first anti-reflection film 410 and the second passivation structure 300 facing away from the substrate 100 .
[0104] Specifically, the first anti-reflection film 410 and the second anti-reflection film 420 together constitute the aforementioned anti-reflection layer 400, and the anti-reflection layer 400 can optimize the passivation characteristics of the photovoltaic cell surface and the light absorption characteristics. The first anti-reflection film 410 and the second anti-reflection film 420 are made of the same material, for example, both are SiNx, or the two materials can also be different.
[0105] In some embodiments, the thickness of the first anti-reflection film 410 is in a range of 40-80 nm, and the thickness of the second anti-reflection film 420 is in a range of 30-50 nm.
[0106] In some embodiments, a second groove 411 is formed in the first anti-reflection film 410 by laser grooving. When the second groove 411 is formed, it is ensured that the projection of the second groove 411 along the first direction is staggered with the projection of the first groove 121, so that the first passivation structure 200 and the second passivation structure 300 are separated in the second direction, so that the battery is not easy to leak electricity. The depth of the second groove 411 ranges from 40 to 100 nm, and the width is 1.5 times that of the negative electrode grid line.
[0107] Preferably, in some embodiments, the depth of the second groove 411 is equal to the thickness of the first anti-reflection film 410. In this way, in the second tunneling oxide layer 310 formed in step S330, the end of the second extension portion 312 away from the first extension portion 311 is flush with the backlight surface 120, so that the projections of the second passivation structure 300 and the first passivation structure 200 along the second direction have no overlapping parts, the isolation effect is better, and the battery can be further guaranteed not to leak electricity, and the safety is higher.
[0108] In other embodiments, the depth of the second groove 411 may also be greater than the thickness of the first anti-reflection film 410. At this time, the second passivation structure 300 extends into the substrate 100, that is, part of the second passivation structure 300 is embedded in the anti-reflection layer 400, and the other part is embedded in the substrate 100.
[0109] In the above embodiment of step S300, the first anti-reflection film 410 is formed in step S310. In addition to being a part of the anti-reflection layer 400 to optimize the anti-reflection performance of the cell, the area outside the second groove 411 can also serve as a mask in step S330 to protect the first tunneling oxide layer 210 and the first polysilicon layer 220, and when forming the phosphorus-doped second polysilicon layer 320, phosphorus is inhibited from passing through the first tunneling oxide layer 210 and the first polysilicon layer 220 to diffuse to the substrate 100. In this way, there is no need to set up a mask separately, which can simplify the process and make the operation easier.
[0110] Referring to FIGS. 6 to 8 and FIG. 1 , in some embodiments, step S330 includes:
[0111] S331, depositing a second tunneling oxide layer 310, so that the second tunneling oxide layer 310 covers a side of the first anti-reflection film 410 away from the substrate 100 and a groove wall of the second groove 411;
[0112] S332, depositing a second polysilicon layer 320 on a side of the second tunnel oxide layer 310 facing away from the substrate 100;
[0113] S333 , removing the portions of the second tunnel oxide layer 310 and the second polysilicon layer 320 protruding from the first anti-reflection film 410 .
[0114] Specifically, in step S331, a thermal oxidation method or CVD method is used to deposit and form the second tunnel oxide layer 310. The material of the second tunnel oxide layer 310 is silicon dioxide. The specific process can directly adopt the existing technology, which will not be repeated here. When the second tunnel oxide layer 310 is deposited, since the first anti-reflection film 410 is provided with a second groove 411, when deposition is performed, the second tunnel oxide layer 310 can be covered on the side of the first anti-reflection film 410 away from the substrate 100 and the groove wall of the second groove 411.
[0115] In step S332 , after the second tunnel oxide layer 310 is deposited, a phosphorus-doped second polysilicon layer 320 is deposited on its surface. The deposition thickness of the second polysilicon layer 320 is large so that the end face away from the second tunnel oxide layer 310 can exceed the depth range of the second groove 411 .
[0116] In step S333 , the portions of the second tunneling oxide layer 310 and the second polysilicon layer 320 protruding from the first anti-reflection film 410 are removed to obtain the structure shown in FIG. 8 . The second tunneling oxide layer 310 and the second polysilicon layer 320 are only distributed in the second groove 411 .
[0117] Generally, when the second polysilicon layer 320 is formed, a phosphosilicate glass layer is also formed on its surface away from the second tunnel oxide layer 310. Therefore, in step S333, the phosphosilicate glass layer is first removed by chain cleaning, and then the second tunnel oxide layer 310 and the second polysilicon layer 320 outside the second groove 411 are etched away by an alkaline etchant (including one of KOH, NaOH and TMAH, etc.), that is, the second tunnel oxide layer 310 and the second polysilicon layer 320 protruding from the first anti-reflection film 410 are removed.
[0118] In the above embodiment, the second tunnel oxide layer 310 and the second polysilicon layer 320 are first deposited in sequence on the entire first anti-reflection film 410 and the groove wall of the second groove 411, and then the portions of the second and second polysilicon layers 320 protruding from the first anti-reflection film 410 are removed, so that the second and second polysilicon layers are only distributed in the second groove 411. Compared with direct deposition in the second groove 411, there is no need to shield the area outside the second groove 411, and the operation is less difficult.
[0119] In some embodiments, the second polysilicon layer 320 is deposited by a solution method so that the end surface of the second polysilicon layer 320 away from the second tunnel oxide layer 310 is parallel to the backlight surface 120. In this way, in step S333, it is only necessary to remove all structures protruding from the first anti-reflection film 410 along the surface of the first anti-reflection film 410 away from the substrate 100, which is less difficult to operate. The specific process is similar to the above-mentioned deposition to form the first polysilicon layer 220, and will not be repeated here.
[0120] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0121] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.
Claims
1. A photovoltaic cell, characterized in that: The photovoltaic cell comprises: A substrate, the substrate having a light-facing surface and a backlight surface arranged opposite to each other along a first direction, the backlight surface being provided with a first groove, wherein the first direction is a thickness direction of the substrate; A first passivation structure is disposed in the first groove, the first passivation structure comprising a first tunneling oxide layer covering the groove wall of the first groove, and a first polysilicon layer stacked on the first tunneling oxide layer; the first tunneling oxide layer covers the groove wall of the first groove to define a first accommodating cavity, and the first polysilicon layer fills the first accommodating cavity; an anti-reflection layer, continuously disposed on one side of the backlight surface of the substrate, the anti-reflection layer comprising a first anti-reflection film and a second anti-reflection film, the first anti-reflection film covers the backlight surface and the first passivation structure, and the first anti-reflection film is provided with a second groove; and a second passivation structure, at least partially disposed in the second groove, the second anti-reflection film covering the side of the first anti-reflection film away from the substrate and the second passivation structure; the second passivation structure comprises a second tunneling oxide layer and a second polysilicon layer stacked, the second tunneling oxide layer covers the groove wall of the second groove to define a second accommodating cavity, and the second polysilicon layer fills the second accommodating cavity; The first polysilicon layer and the second polysilicon layer have different doping types; and the projections of the first passivation structure and the second passivation structure in the first direction are staggered with each other.
2. The photovoltaic cell according to claim 1, characterized in that: A side of the second passivation structure that is away from the second anti-reflection film along the first direction is flush with the backlight surface.
3. The photovoltaic cell according to claim 1, characterized in that: The photovoltaic cell further comprises a first electrode and a second electrode; The first electrode is in ohmic contact with the first passivation structure through the anti-reflection layer; The second electrode is in ohmic contact with the second passivation structure through the anti-reflection layer.
4. The photovoltaic cell according to any one of claims 1 to 3, characterized in that The photovoltaic cell comprises a plurality of the first passivation structures and a plurality of the second passivation structures; The first passivation structure and the second passivation structure are alternately distributed along the second direction; The second direction is perpendicular to the first direction and perpendicular to the longitudinal extension direction of the first groove.
5. A photovoltaic cell assembly, characterized in that: The photovoltaic cell assembly comprises a plurality of photovoltaic cells as described in any one of claims 1 to 4; The photovoltaic cell assembly also includes a frame, and a plurality of the photovoltaic cells are spliced and arranged and are all installed in the frame.
6. A method for manufacturing a photovoltaic cell according to any one of claims 1 to 4, characterized in that: The manufacturing method comprises the following steps: The first groove is formed on the backlight surface of the substrate; Depositing the first tunneling oxide layer and the first polysilicon layer in sequence on the backlight side of the substrate; The second passivation structure and the anti-reflection layer are deposited.
7. The manufacturing method according to claim 6, characterized in that: The sequentially depositing the first tunneling oxide layer and the first polysilicon layer on the backlight side of the substrate comprises: Depositing the first tunneling oxide layer on the backlight side of the substrate so that the first tunneling oxide layer covers the backlight surface and the groove wall of the first groove; Depositing the first polysilicon layer on a side of the first tunnel oxide layer facing away from the substrate; Portions of the first tunnel oxide layer and the first polysilicon layer protruding from the backlight surface are removed.
8. The manufacturing method according to claim 7, characterized in that: The first polysilicon layer is deposited by a solution method so that an end surface of the first polysilicon layer facing away from the first tunnel oxide layer is parallel to the backlight surface.
9. The manufacturing method according to claim 7, characterized in that: The depositing of the second passivation structure and the anti-reflection layer comprises: Depositing a first anti-reflection film on the backlight side of the substrate so that the first anti-reflection film covers the backlight surface and the first passivation structure; A second groove is formed on the first anti-reflection film, wherein the second groove is staggered from the projection of the first groove along the first direction, and the depth of the second groove is not less than the thickness of the first anti-reflection film; sequentially depositing the second tunneling oxide layer and the second polysilicon layer in the second groove; A second anti-reflection film is deposited on a side of the first anti-reflection film and the second passivation structure facing away from the substrate.
10. The manufacturing method according to claim 9, characterized in that: The sequentially depositing the second tunneling oxide layer and the second polysilicon layer in the second groove comprises: Depositing the second tunneling oxide layer so that the second tunneling oxide layer covers a side of the first anti-reflection film away from the substrate and a groove wall of the second groove; Depositing the second polysilicon layer on a side of the second tunnel oxide layer facing away from the substrate; Portions of the second tunneling oxide layer and the second polysilicon layer protruding from the first anti-reflection film are removed.