Display panel and display device

By filling the cracks in the encapsulation layer of the OLED display panel with fluid materials for repair, the problem of water vapor ingress caused by cracks at the edge is solved, extending the service life of the panel and improving the sealing effect.

CN117794323BActive Publication Date: 2024-10-11HKC CORP LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311835010.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-10-11
Estimated Expiration
2043-12-27

AI Technical Summary

Technical Problem

In high-temperature and high-humidity environments, OLED display panels are prone to cracks in the packaging layer at the edges, causing water vapor to enter, resulting in device failure and shortened service life.

Method used

When there is a crack in the packaging layer of the display panel, a fluid filling material is filled into the receiving groove and heated to turn it into a liquid state, thereby filling the crack into the crack, repairing the packaging layer, and improving the sealing effect.

Benefits of technology

It effectively extends the service life of the display panel, avoids failure problems caused by cracks, and improves the sealing effect of the packaging layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117794323B_ABST
    Figure CN117794323B_ABST
Patent Text Reader

Abstract

The present application discloses a display panel and a display device, wherein the display panel further comprises a substrate, a light-emitting unit layer, an encapsulation layer, an encapsulation cover plate and a sealant; the light-emitting unit layer is arranged on the substrate and is located in the display area; the encapsulation layer is arranged on the light-emitting unit layer and extends from the display area to the non-display area; the encapsulation cover plate is arranged on the encapsulation layer; the sealant is arranged on the outer side of the encapsulation layer, and its two ends are respectively bonded to the substrate and the encapsulation cover plate; wherein a receiving groove is arranged on a side of the encapsulation cover plate close to the substrate, the receiving groove is arranged in the non-display area, and extends from the junction of the encapsulation layer and the sealant to the display area, and a filling material is arranged in the receiving groove, and the filling material is used to have fluidity in a heated state to fill cracks generated on a side of the encapsulation layer close to the sealant, thereby effectively extending the service life of the display panel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a display device. Background Art

[0002] Organic light emitting diode (OLED) has the advantages of surface light source, cold light, energy saving, fast response, flexibility, ultra-light and low cost, and its mass production technology is becoming more and more mature. Since OLED has poor stability and is extremely sensitive to water and oxygen, packaging technology is particularly critical. The purpose of packaging is mainly to prevent water vapor and oxygen from entering OLED. The current mainstream technologies are cover packaging technology and thin film packaging technology. Cover packaging technology is mainly divided into Frit (glass glue packaging), Dam (isolation dam packaging) and Face seal (surface packaging).

[0003] In the cover packaging technology, the edge position is the weakest position of the package. It is easily affected by water vapor in a high temperature and high humidity environment, and the edge position is subjected to greater force. The film layer at this position is more likely to crack. When the film layer cracks, water vapor can easily pass through the film layer to reach the device, causing the device to fail. Summary of the invention

[0004] The purpose of the present application is to provide a display panel and a display device, which can repair cracks in the encapsulation layer when they exist, thereby avoiding display panel failure problems caused by the cracks, and can effectively extend the service life of the display panel to a certain extent.

[0005] The present application discloses a display panel, which includes a display area and a non-display area, and the display panel also includes a substrate, a light-emitting unit layer, a packaging layer, a packaging cover plate and a sealant; the light-emitting unit layer is arranged on the substrate and is located in the display area; the packaging layer is arranged on the light-emitting unit layer and extends from the display area to the non-display area; the packaging cover plate is arranged on the packaging layer; the sealant is arranged on the outer side of the packaging layer, and the two ends are respectively bonded to the substrate and the packaging cover plate; wherein, a receiving groove is arranged on a side of the packaging cover plate close to the substrate, the receiving groove is arranged in the non-display area, and extends from the junction of the packaging layer and the sealant to the display area, and a filling material is arranged in the receiving groove, and the filling material is used to have fluidity in a heated state to fill cracks generated on a side of the packaging layer close to the sealant.

[0006] Optionally, the filling material includes one or more materials selected from the group consisting of polyethylene wax, bismuth-based alloy, lead-based alloy, and lead-tin-antimony-copper quaternary alloy; and the melting temperature of the filling material is between 100°C and 200°C.

[0007] Optionally, the accommodating groove includes a plurality of first accommodating holes, the plurality of first accommodating holes are arranged at intervals, and the filling material is disposed in the first accommodating holes.

[0008] Optionally, the depth of the first accommodating hole is between 10um and 50um, the diameter of the hole is between 5um and 10um, and the spacing between adjacent first accommodating holes is between 8um and 10um.

[0009] Optionally, the encapsulation layer includes a first inorganic insulating layer and a second inorganic insulating layer, the first inorganic insulating layer is arranged on one side of the substrate to wrap the light-emitting unit layer, and the second inorganic insulating layer is arranged on one side of the substrate to wrap the first inorganic insulating layer; the second inorganic insulating layer includes a main body and an extension part, the main body is arranged on the first inorganic insulating layer, and on the orthographic projection of the substrate, the main body and the first inorganic insulating layer completely overlap; the extension part is arranged on the outside of the main body, the extension part is connected to the main body and extends to the substrate, and the extension part is arranged between the frame glue and the first inorganic insulating layer; on the orthographic projection of the substrate, the accommodating groove is located within the projection range of the extension part.

[0010] Optionally, a plurality of second accommodating holes are further provided at the bottom of the accommodating groove, and the plurality of second accommodating holes are arranged at intervals, and the filling material is provided in the accommodating groove and fills the second accommodating holes.

[0011] Optionally, the display panel also includes a detection structure, which is arranged on the substrate and located in the non-display area, and on the orthographic projection of the substrate, the detection structure overlaps with the receiving groove; the detection structure is used to emit light toward the receiving groove and receive light reflected by the receiving groove; when a crack appears in the encapsulation layer at the position of the receiving groove, the detection structure cannot receive the light reflected by the receiving groove.

[0012] Optionally, a semi-reflective coating is provided on the encapsulation layer, and the semi-reflective coating is provided corresponding to the groove and is located in the non-display area.

[0013] Optionally, an infrared emitter is further provided in the detection structure, and the infrared emitter is used to emit an infrared laser to the filling material to melt the filling material.

[0014] The present application also discloses a display device, comprising a driving circuit and the above-mentioned display panel, wherein the driving circuit is used to drive the display panel to display.

[0015] The present application sets a receiving groove on the packaging cover plate near the edge of the packaging, and the receiving groove is filled with a filling material. When cracks are found in the packaging layer near the frame glue area, the filling material in the receiving groove is heated to change from solid to liquid and flow out of the receiving groove under the action of gravity, thereby filling the corresponding cracks to repair the cracks in the packaging layer and improve the sealing effect of the packaging layer. Specifically, in a rigid package, the packaging layer at the junction of the frame glue and the packaging layer is easily affected by external forces on the one hand, and the stress between the film layers on the other hand easily causes the packaging layer in this area to be damaged and cracked, and the cracks will gradually develop and extend inward, and eventually water vapor will enter the display area through the cracks. In this regard, the present application provides a packaging repair solution, which repairs the cracks in the packaging layer before they are aggravated, thereby avoiding the problem of display panel failure caused by cracks, and can effectively extend the service life of the display panel to a certain extent. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The included drawings are used to provide a further understanding of the embodiments of the present application, which constitute a part of the specification, are used to illustrate the implementation methods of the present application, and together with the text description, explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. In the drawings:

[0017] Figure 1 is a schematic diagram of a display panel of the present application;

[0018] Figure 2 is a schematic top view of a display panel of the present application;

[0019] Figure 3 is a schematic diagram of another receiving groove of the first embodiment of the present application;

[0020] Figure 4 is a cross-sectional schematic diagram of a receiving tank according to a second embodiment of the present application;

[0021] Figure 5 is a schematic top view of a receiving tank according to a second embodiment of the present application;

[0022] Figure 6 is a schematic diagram of a receiving tank according to a third embodiment of the present application;

[0023] Figure 7 is a schematic diagram of a display panel according to a fourth embodiment of the present application;

[0024] Figure 8 It is a schematic diagram of light detection showing that the encapsulation layer of the present application has no cracks;

[0025] Fig. 9 It is a schematic diagram of light detection of cracks in the encapsulation layer of the present application;

[0026] Fig.10 is a schematic diagram of a display device of the present application.

[0027] Among them, 100, display panel; 101, display area; 102, non-display area; 103, substrate; 104, light-emitting unit layer; 110, encapsulation layer; 111, first inorganic insulating layer; 112, second inorganic insulating layer; 113, main body; 114, extension part; 120, encapsulation cover; 121, receiving groove; 122, first receiving hole; 123, second receiving hole; 130, frame glue; 140, filling material; 150, detection structure; 160, semi-reflective coating; 200, display device; 210, driving circuit. DETAILED DESCRIPTION

[0028] It should be understood that the terms used herein, the specific structures and functional details disclosed are only for describing specific embodiments and are representative, but the present application can be implemented in many alternative forms and should not be construed as being limited to only the embodiments described herein.

[0029] In the description of the present application, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating relative importance or implicitly indicating the number of technical features indicated. Therefore, unless otherwise specified, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features; "multiple" means two or more. In addition, the terms "upper", "lower", "left", "right", "vertical", "horizontal", etc. indicating orientation or positional relationships are described based on the orientation or relative positional relationships shown in the accompanying drawings, and are only for the convenience of describing the simplified description of the present application, rather than indicating that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to the specific circumstances.

[0030] The present application is described in detail below with reference to the accompanying drawings and optional embodiments.

[0031] Figure 1 is a schematic diagram of the display panel of the present application, see Figure 1As shown, the present application discloses a display panel 100, the display panel 100 includes a display area 101 and a non-display area 102, the display panel 100 also includes a substrate 103, a light-emitting unit layer 104, an encapsulation layer 110, an encapsulation cover plate 120 and a sealant 130; the light-emitting unit layer 104 is arranged on the substrate 103 and is located in the display area 101; the encapsulation layer 110 is arranged on the light-emitting unit layer 104 and extends from the display area 101 to the non-display area 102; the encapsulation cover plate 120 is arranged on the encapsulation layer 110; the sealant 130 It is arranged on the outer side of the packaging layer 110, and its two ends are respectively bonded to the substrate 103 and the packaging cover plate 120; wherein, a receiving groove 121 is arranged on the side of the packaging cover plate 120 close to the substrate 103, and the receiving groove 121 is arranged in the non-display area 102, and extends from the junction of the packaging layer 110 and the frame glue 130 to the display area 101, and a filling material 140 is arranged in the receiving groove 121, and the filling material 140 is used to have fluidity in a heated state to fill the cracks generated on the side of the packaging layer 110 close to the frame glue 130.

[0032] The present application sets a receiving groove 121 on the packaging cover plate 120 near the edge of the packaging, and fills the receiving groove 121 with a filling material 140. When cracks are found in the packaging layer 110 near the sealant 130 area, the filling material 140 in the receiving groove 121 is heated to change from solid to liquid and flow out of the receiving groove 121 under the action of gravity, thereby filling the corresponding cracks to repair the cracks in the packaging layer 110 and improve the sealing effect of the packaging layer 110. Specifically, in a rigid package, the packaging layer 110 at the junction of the sealant 130 and the packaging layer 110 is easily affected by external forces on the one hand, and on the other hand, the stress between the film layers easily causes the packaging layer 110 in this area to be damaged and cracked, and the cracks will gradually develop and extend inward, and eventually water vapor will enter the display area 101 through the cracks. In this regard, the present application provides a packaging repair solution, which repairs cracks in the packaging layer 110 before they become more severe, thereby avoiding malfunctions of the display panel 100 caused by the cracks and effectively extending the service life of the display panel 100 to a certain extent.

[0033] Specifically, the filling material 140 in the receiving groove 121 is a solid material, which may include one or more materials selected from polyethylene wax, bismuth-based alloy, lead-based alloy, and lead-tin-antimony-copper quaternary alloy. The above materials have the characteristics of low melting point, high strength, good fluidity, small expansion and contraction rate, and non-toxicity. The filling material 140 has the characteristics of being dissolved into liquid when heated and solid after cooling, and no gas is generated in the process of being heated to liquid, and has good fluidity, and what occurs is a physical change.

[0034] Specifically, the melting temperature of the filling material 140 is between 100°C and 200°C. Generally speaking, even if the display panel 100 generates heat or is used in a hot environment, it is difficult to reach about 100°C. In order to prevent the filling material 140 from becoming liquid during normal use of the display panel 100, the melting temperature of the filling material 140 can be set above 100°C. Since the OLED display panel 100 is not easy to withstand high temperatures, the melting temperature of the filling material 140 can be less than or equal to 200°C. Relatively speaking, the filling material 140 with the required melting point can be achieved by adjusting the ratio of materials with different melting points.

[0035] In one embodiment, the filling material 140 can be heated and melted by laser, so that the filling material 140 is converted from solid to liquid. The laser heating method can be used for fixed-point heating to achieve directional repair. Of course, other heating methods can also be used to convert the filling material 140 into liquid and then flow into the crack for repair.

[0036] Continue to see Figure 1 As shown, the encapsulation layer 110 includes a first inorganic insulating layer 111 and a second inorganic insulating layer 112, wherein the first inorganic insulating layer 111 is disposed on one side of the substrate 103 to wrap the light-emitting unit layer 104, and the second inorganic insulating layer 112 is disposed on one side of the substrate 103 to wrap the first inorganic insulating layer 111; the second inorganic insulating layer 112 is disposed on the outside of the first inorganic insulating layer 111. In the orthographic projection of the substrate 103, the first inorganic insulating layer 111 is completely located within the projection range of the second inorganic insulating layer 112; and the second inorganic insulating layer 112 is directly in contact with the substrate 103 at a portion not located above the first inorganic insulating layer 111.

[0037] The first inorganic insulating layer 111 is formed of silicon oxynitride material, and the second inorganic insulating layer 112 is formed of silicon nitride material. The thickness of the first inorganic insulating layer 111 may be about 1.5um, and the thickness of the second inorganic insulating layer 112 may be between 2um and 5um (including the end value). The first inorganic insulating layer 111 and the second inorganic insulating layer 112 extend from the display area 101 to the non-display area 102 respectively, and the receiving groove 121 is mainly located in the non-display area 102 and is arranged corresponding to the second inorganic insulating layer 112 to repair cracks generated in the second inorganic insulating layer 112.

[0038] The second inorganic insulating layer 112 includes a main body portion 113 and an extending portion 114. The main body portion 113 is disposed on the first inorganic insulating layer 111, and in the orthographic projection of the substrate 103, the main body portion 113 and the first inorganic insulating layer 111 completely overlap; the extending portion 114 is disposed outside the main body portion 113, the extending portion 114 is connected to the main body portion 113 and extends towards the substrate 103, and the extending portion 114 is disposed between the frame adhesive 130 and the first inorganic insulating layer 111. In the orthographic projection of the substrate 103, the extending portion 114 is annular, and the inner side of the annulus contacts the first inorganic insulating layer 111, the outer side contacts the frame adhesive 130, the lower side contacts the substrate 103, and the upper side contacts the encapsulation cover plate 120. In the orthographic projection of the substrate 103, the receiving groove 121 is located within the projection range of the extending portion 114.

[0039] What this application mainly considers is that the encapsulation layer 110 near the position of the frame adhesive 130 is vulnerable to external forces and is prone to breakage, while the position of the main body portion 113 of the second inorganic insulating layer 112 will not crack relatively. Therefore, for the receiving groove 121, it can be set corresponding to the position of the extending portion 114 to fully repair the second inorganic insulating layer 112.

[0040] Generally, the encapsulation layer 110 is mostly encapsulated by a stack of multiple inorganic insulating layers and organic insulating layers. However, considering the good passivation effect of the inorganic insulating layer, therefore, regardless of how many layers of inorganic insulating layers and organic insulating layers are stacked, the outermost layer of the encapsulation layer 110 close to the encapsulation cover plate 120 is an inorganic insulating layer. In this application, it is the second inorganic insulating layer 112. Specifically, the organic insulating layer can be designed according to actual situations between the first inorganic insulating layer 111 and the second inorganic insulating layer 112.

[0041] Figure 2 is a top view schematic diagram of the display panel of this application. Refer to Figure 2 As shown, the frame adhesive 130 is in a square shape with a hole in the middle. The frame adhesive 130 surrounds the display area 101, and the extending portion 114 is also annular and is disposed inside the frame adhesive 130. In an embodiment, the receiving groove 121 of this application is also an annular structure in the orthographic projection of the substrate 103. In this solution, in the projection of the substrate 103, the maximum width of the receiving groove 121 does not exceed the maximum width of the extending portion 114, and at least a corresponding filling material 140 is provided at each position of the extending portion 114 so that when cracks appear at different positions of the extending portion 114, there is a filling material 140 to repair it.

[0042] In this solution, the amount of the filling material 140 can be controlled by controlling the depth of the receiving groove 121, so that the filling material 140 can cover as large an area as possible to fill the crack while using as little filling material 140 as possible, and relatively speaking, a large amount of filling material 140 is not required to repair the crack.

[0043] Figure 3 is a schematic diagram of another receiving groove of the first embodiment of the present application, see Figure 3 As shown, in the direction from the package cover plate 120 to the substrate 103, the opening of the receiving groove 121 is gradually reduced. By gradually reducing the opening of the receiving groove 121, the solid filling material 140 disposed inside the receiving groove 121 is not easy to leak from the receiving groove 121 even when the package cover plate is inverted, causing inconvenience in the transportation of the package cover plate 120. When the filling material 140 on the package cover plate 120 is specifically made, a liquid filling material 140 can be selected to be filled into the above-mentioned receiving groove 121, and after curing, the package cover plate 120 is disposed on the packaging layer 110. The minimum opening of the receiving groove 121 is 10um. Compared with the receiving groove 121 with a square cross-section, when the filling material 140 flows out more, it is easy to make the opening position of the receiving groove 121 not have enough filling material 140 to seal. The opening of the receiving groove 121 is gradually reduced, so that when the filling material 140 flows out more, even if a small amount of filling material 140 remains, the receiving groove 121 can still be sealed.

[0044] In another embodiment, the receiving groove 121 includes a first annular groove and a second annular groove, the first annular groove is arranged around the second annular groove, and the second annular groove is arranged around the display area 101. In other words, the receiving groove 121 includes at least two annular grooves arranged in an arranged manner. This solution can further reduce the use of the filling material 140. In actual use, multiple annular grooves can be arranged at intervals, and the multiple annular grooves can be used to repair the extension portion 114 of the area covered by them.

[0045] Furthermore, in each annular groove, a plurality of intermittently arranged square grooves may be provided, and the intermittently arranged square grooves are arranged to form an annularly arranged receiving groove 121. In this solution, by further providing a plurality of unconnected square grooves in each annular groove, when repairing a specific area, only the filling material 140 in the receiving groove 121 corresponding to the specific area moves, while the filling material 140 in the receiving groove 121 in other areas remains the same.

[0046] Figure 4 is a cross-sectional schematic diagram of a receiving tank according to a second embodiment of the present application, Figure 5 is a top view of the receiving tank of the second embodiment of the present application, see Figure 4-5As shown, the receiving groove 121 includes a plurality of first receiving holes 122 , the plurality of first receiving holes 122 are arranged at intervals, and the filling material 140 is disposed in the first receiving holes 122 .

[0047] On the basis of the above-mentioned embodiment, the present solution further sets the receiving groove 121 as a plurality of first receiving holes 122, and the plurality of first receiving holes 122 are arranged at a preset interval. The present solution sets a plurality of arranged first receiving holes 122, on the one hand, which can be controlled at a fixed point, and in the corresponding area where cracks appear, a first receiving hole 122 or a plurality of first receiving holes 122 are selected for repair, and the control method is more precise. Another solution is that quantitative control can be achieved, and the amount of filling material 140 can be accurately controlled, for example, by the number of first receiving holes 122 heated, to achieve more refined control.

[0048] Specifically, the hole depth of the first receiving hole 122 is between 10um and 50um, the hole diameter is between 5um and 10um, and the interval between adjacent first receiving holes 122 is between 8um and 10um.

[0049] In this solution, the depth and diameter of the receiving hole are required to ensure that the contained filling material 140 can repair the cracks, and since the receiving holes are all located in the non-display area 102, the display effect is basically not affected. Specifically, the first receiving hole 122 can be extended from the extension part 114 to the main body 113, but the first receiving hole 122 should not exceed the area of ​​the non-display area 102, specifically, the distance from the edge of the display area 101 is at least greater than 0.5um.

[0050] Figure 6 is a schematic diagram of the receiving tank of the third embodiment of the present application, see Figure 6 As shown, a plurality of second accommodating holes 123 are further provided at the bottom of the accommodating groove 121 , and the plurality of second accommodating holes 123 are arranged at intervals. The filling material 140 is provided in the accommodating groove 121 and fills the second accommodating holes 123 .

[0051] In this solution, the purpose of setting the second receiving hole 123 at the bottom of the receiving groove 121 is mainly to ensure that during the actual repair process, only the filling material 140 in the second receiving hole 123 flows out for repair, and the receiving groove 121 does not need to be set deeper, and a larger area can be set, thereby avoiding the filling material 140 at a corresponding position of the receiving groove 121 being insufficient to repair the crack.

[0052] Figure 7 is a schematic diagram of a display panel of the fourth embodiment of the present application, see Figure 7As shown, the present application also discloses a display panel 100, the display panel 100 further comprising a substrate 103, a light-emitting unit layer 104, an encapsulation layer 110, an encapsulation cover plate 120, a sealant 130 and a detection structure 150; the light-emitting unit layer 104 is disposed on the substrate 103 and is located in the display area 101; the encapsulation layer 110 is disposed on the light-emitting unit layer 104 and extends from the display area 101 to the non-display area 102; the encapsulation cover plate 120 is disposed on the encapsulation layer 110; the sealant 130 is disposed on the encapsulation layer 1 10, and the two ends are respectively bonded to the substrate 103 and the packaging cover plate 120; wherein, a receiving groove 121 is provided on the side of the packaging cover plate 120 close to the substrate 103, and the receiving groove 121 is provided in the non-display area 102, and extends from the junction of the packaging layer 110 and the frame glue 130 to the display area 101, and a filling material 140 is provided in the receiving groove 121, and the filling material 140 is used to have fluidity in a heated state to fill the cracks generated on the side of the packaging layer 110 close to the frame glue 130. The detection structure 150 is arranged on the substrate 103 and is located in the non-display area 102. On the orthographic projection of the substrate 103, the detection structure 150 overlaps with the receiving groove 121; the detection structure 150 is used to emit light toward the receiving groove 121 and receive light reflected by the receiving groove 121; when a crack appears in the encapsulation layer 110 at the position of the receiving groove 121, the detection structure 150 cannot receive the light reflected by the receiving groove 121.

[0053] In this solution, a detection structure 150 is provided on the substrate 103 of the display panel 100. The detection structure 150 mainly includes a light emitting end and a light receiving end. A cold light source is emitted by the light emitting end. When there is no crack on the extension part 114, the light receiving end receives reflected light of a first intensity. When there is a crack on the extension part 114, the light receiving end receives reflected light of a second intensity. According to the reflected light intensity information collected by the light receiving end, it is determined whether a crack occurs at the corresponding position. When there is a crack, a heating operation is performed to repair the crack using the filling material 140.

[0054] Furthermore, an infrared emitter is also disposed in the detection structure 150 , and the infrared emitter is used to emit an infrared laser to the filling material 140 to melt the filling material 140 .

[0055] The present solution provides a solution that can perform detection and repair in real time. Specifically, the packaging of the display panel 100 is detected by controlling the detection structure 150 when the display panel 100 is turned on or off or at other preset times. When a crack is detected, the infrared emitter in the detection structure 150 that detects the crack is controlled to emit a laser, and the laser is irradiated onto the filling material 140, so that the filling material 140 is melted by heat and flows toward the crack, thereby filling the crack.

[0056] Of course, the solution of using an external detection device and using an external heating source to heat the filling material 140 is also applicable. Relatively speaking, the use of an external detection device requires detection before the display panel 100 leaves the factory, and cannot be detected after leaving the factory, but there is no need to integrate the detection structure 150 inside the display panel 100, so that the cost of the display panel 100 can be reduced.

[0057] In another embodiment, the detection device may not be used. Before the display panel 100 leaves the factory, the cracks may be directly repaired by the filling material 140 through a heating process. When there is no crack at a position corresponding to a certain receiving groove 121, even if the filling material 140 is heated, the filling material 140 will not flow out of the receiving groove 121.

[0058] Specifically, in order to further increase the detection structure 150 set up as above, the present application sets a semi-reflective coating 160 on the encapsulation layer 110 , and the semi-reflective coating 160 is set corresponding to the groove and is located in the non-display area 102 .

[0059] Figure 8 This is a schematic diagram of light detection showing that the encapsulation layer of the present application has no cracks. Fig. 9 This is a schematic diagram of light detection of cracks in the packaging layer of this application, see Figure 8-9 As shown, in the initial state, when there is no crack in the film layer, the light emitting end below emits vertical light, and after being reflected by the semi-reflective coating, most of the light enters the light receiving end as reverse vertical light. Of course, due to the slight unevenness of the film surface, the received light will have some oblique reflection, which can be used as noise filter. After a large crack occurs in the film layer, the semi-reflective coating will also break along with the inorganic insulating layer. At this time, the light emitted by the light emitting end will be reflected or transmitted by the corresponding interface, causing the light at the light receiving end to change, thereby locating the location of the crack in the film layer.

[0060] The detection structure 150 may have a plurality of light emitting ends, and the density or number of the light emitting ends may be consistent with the density or number of the first receiving holes 122, or greater than the density or number of the first receiving holes 122. Relatively speaking, the greater the density of the light emitting ends, the higher the detection accuracy. After the crack position is detected, the infrared emitter at the corresponding position emits an infrared laser to the crack position, so that the filling material 140 at the crack position can be melted and filled into the crack, and the cross section of the crack can be repaired.

[0061] In this solution, a receiving groove 121 or a receiving hole is arranged near the edge of the package, and a filling material 140 is filled in the receiving groove 121 or the receiving hole. By setting a detection structure 150, when the packaging layer 110 of the display panel 100 has cracks, the filling material 140 at the corresponding position is controlled to be repaired, so as to repair the packaging isolation effect of the packaging layer 110, so as to improve the strength and service life of the packaging layer 110.

[0062] Fig.10 is a schematic diagram of the display device of the present application, see Fig.10 As shown, the present application discloses a display device 200, which includes the above-mentioned display panel 100 and a driving circuit 210, wherein the driving circuit 210 is used to drive the display panel 100 to display. The display panel 100 in this embodiment is an organic light emitting display panel 100.

[0063] The present application sets a receiving groove 121 on the packaging cover plate 120 near the edge of the packaging, and fills the receiving groove 121 with a filling material 140. When cracks are found in the packaging layer 110 near the sealant 130 area, the filling material 140 in the receiving groove 121 is heated to change from solid to liquid and flow out of the receiving groove 121 under the action of gravity, thereby filling the corresponding cracks to repair the cracks in the packaging layer 110 and improve the sealing effect of the packaging layer 110. Specifically, in a rigid package, the packaging layer 110 at the junction of the sealant 130 and the packaging layer 110 is easily affected by external forces on the one hand, and on the other hand, the stress between the film layers easily causes the packaging layer 110 in this area to be damaged and cracked, and the cracks will gradually develop and extend inward, and eventually water vapor will enter the display area 101 through the cracks. In this regard, the present application provides a packaging repair solution, which repairs cracks in the packaging layer 110 before they become more severe, thereby avoiding malfunctions of the display panel 100 caused by the cracks and effectively extending the service life of the display panel 100 to a certain extent.

[0064] It should be noted that the inventive concept of the present application can form a large number of embodiments, but the length of the application document is limited and it is impossible to list them one by one. Therefore, under the premise of no conflict, the embodiments or technical features described above can be arbitrarily combined to form new embodiments. After the embodiments or technical features are combined, the original technical effects will be enhanced.

[0065] The above content is a further detailed description of the present application in combination with specific optional implementation methods, and it cannot be determined that the specific implementation of the present application is limited to these descriptions. For ordinary technicians in the technical field to which the present application belongs, several simple deductions or substitutions can be made without departing from the concept of the present application, which should be deemed to fall within the scope of protection of the present application.

Claims

1. A display panel comprising a display area and a non-display area, It is characterized in that The display panel comprises: substrate; A light-emitting unit layer, disposed on the substrate and located in the display area; An encapsulation layer, disposed on the light-emitting unit layer and extending from the display area to the non-display area; a packaging cover plate, disposed on the packaging layer; and A frame glue is arranged on the outer side of the packaging layer, and the two ends thereof are respectively bonded to the substrate and the packaging cover plate; Among them, a receiving groove is arranged on the side of the packaging cover plate close to the substrate, the receiving groove is arranged in the non-display area, and extends from the junction of the packaging layer and the frame glue to the display area, and a filling material is arranged in the receiving groove. The filling material is used to have fluidity under heating state so as to fill the cracks generated on the side of the packaging layer close to the frame glue.

2. The display panel according to claim 1, It is characterized in that The filling material includes one or more materials selected from polyethylene wax, bismuth-based alloy, and lead-based alloy; The melting temperature of the filling material is between 100°C and 200°C.

3. The display panel according to claim 1, It is characterized in that The receiving groove includes a plurality of first receiving holes, the plurality of first receiving holes are arranged at intervals, and the filling material is disposed in the first receiving holes.

4. The display panel according to claim 3, It is characterized in that The depth of the first accommodating hole is between 10um and 50um, the diameter of the hole is between 5um and 10um, and the spacing between adjacent first accommodating holes is between 8um and 10um.

5. The display panel according to claim 1, It is characterized in that The encapsulation layer includes a first inorganic insulating layer and a second inorganic insulating layer, wherein the first inorganic insulating layer is disposed on one side of the substrate to wrap the light-emitting unit layer, and the second inorganic insulating layer is disposed on one side of the substrate to wrap the first inorganic insulating layer; The second inorganic insulating layer comprises a main body and an extension, the main body is disposed on the first inorganic insulating layer, and in an orthographic projection of the substrate, the main body and the first inorganic insulating layer completely overlap; The extension portion is arranged outside the main body portion, the extension portion is connected to the main body portion and extends to the substrate, and the extension portion is arranged between the sealant and the first inorganic insulating layer; On the orthographic projection of the substrate, the receiving groove is located within the projection range of the extending portion.

6. The display panel according to claim 1, It is characterized in that A plurality of second accommodating holes are also arranged at the bottom of the accommodating groove, and the plurality of second accommodating holes are arranged at intervals. The filling material is arranged in the accommodating groove and fills the second accommodating holes.

7. The display panel according to claim 1, It is characterized in that The display panel further includes a detection structure, which is disposed on the substrate and located in the non-display area, and in an orthographic projection of the substrate, the detection structure overlaps with the receiving groove; The detection structure is used to emit light toward the receiving groove and receive the light reflected by the receiving groove; when cracks appear in the packaging layer at the position of the receiving groove, the detection structure cannot receive the light reflected by the receiving groove.

8. The display panel according to claim 7, It is characterized in that A semi-reflective coating is arranged on the encapsulation layer, the semi-reflective coating is arranged corresponding to the receiving groove and is located in the non-display area.

9. The display panel according to claim 7, It is characterized in that An infrared emitter is also arranged in the detection structure, and the infrared emitter is used to emit infrared laser to the filling material to melt the filling material.

10. A display device, It is characterized in that It comprises a driving circuit and the display panel according to any one of claims 1 to 9, wherein the driving circuit is used to drive the display panel to display.