A method for determining the collapsibility coefficient of loess based on the proportion of large and medium porosity and water content

By measuring the proportion of large and medium pores and water content, and combining the Origin software to fit a three-dimensional surface model, the problem of insufficient accuracy in measuring the loess collapsibility coefficient in traditional methods has been solved, and more accurate assessment and prevention of collapsibility has been achieved.

CN117849313BActive Publication Date: 2026-11-10XIJING UNIV
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410026608.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-01-08
Publication Date
2026-11-10
Estimated Expiration
2044-01-08

AI Technical Summary

Technical Problem

Traditional methods fail to consider the microstructural characteristics of loess and the differences in collapsibility coefficients under different moisture contents when determining the collapsibility coefficient of loess, resulting in insufficient measurement accuracy and affecting engineering construction in collapsible loess areas.

Method used

By measuring the proportion of large and medium pores and water content, and combining Origin software to fit a three-dimensional surface model, the collapsibility coefficient of loess was accurately determined, and the collapsibility potential of loess under different water contents and pore proportions was considered.

Benefits of technology

It improves the precision and accuracy of loess collapsibility determination, and forms an intuitive three-dimensional model diagram, which can better evaluate and prevent loess collapsibility.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117849313B_ABST
    Figure CN117849313B_ABST
Patent Text Reader

Abstract

A method for determining the collapsibility coefficient of loess based on the proportion of large and medium porosity and water content is proposed. First, undisturbed soil samples are taken and their basic physical properties are measured. Then, two groups of soil samples with different water contents are prepared. Indoor consolidation tests are conducted on both groups of soil samples. The water content w` of the first group of soil samples after consolidation is measured. The second group of soil samples undergoes further collapsibility tests, and the collapsibility coefficient δ of each soil sample is determined. s Then, mercury intrusion porosimetry was performed on the undisturbed soil samples in their initial state, and the pore sizes were classified into large, medium, small, and micro pores according to the fractal volume model. Mercury intrusion porosimetry was also performed on the first group of soil samples with the measured consolidated water content, and the proportion of large and medium pores (n) of each soil sample under different water contents (w`) and different pressures was measured. Finally, in Origin, the water content (w`), the proportion of large and medium pores (n), and the collapsibility coefficient (δ) were used to... s A three-dimensional surface model is fitted, and the fitting formula is output. Finally, the fitting formula is verified. This invention requires less work, produces more intuitive data graphs, and provides a more accurate evaluation of the collapsibility of loess.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of loess collapsibility determination technology in geotechnical engineering, and particularly to a method for determining the loess collapsibility coefficient based on the proportion of large and medium porosity and water content. Background Technology

[0002] Collapsible loess is a special type of soil that undergoes significant collapsing deformation after being soaked in water, under the stress of its overlying soil layer or under the combined effects of its own weight and additional stress. Collapsible loess poses a significant threat to human engineering activities. When the foundation soil of a project is subjected to the combined effects of external pressure and water immersion, its original structure will be rapidly destroyed, leading to significant soil subsidence, deformation of buildings, and even collapse, causing enormous damage.

[0003] The traditional method for determining the collapsibility of loess in soil mechanics involves immersing the soil under external loads and measuring its collapsibility coefficient (GB50025-2018 "Standard for Construction in Collapsible Loess Areas"). However, this method has certain shortcomings in calculating the collapsibility coefficient. The test is conducted under macroscopic external forces, and loess has a unique structure; this method does not consider the influence of its microstructural characteristics on the collapsibility coefficient. Furthermore, loess has higher strength in a dry state and lower strength in a wet state. Although the traditional method divides the applied load into several stages (gradually loading to the specified pressure of the soil sample), it does not consider that the collapsibility coefficient value of the same soil sample varies at different moisture contents. This inevitably affects the accuracy of the loess collapsibility coefficient calculation, and consequently, the prevention and control of soil collapse in construction projects in collapsible loess areas. Summary of the Invention

[0004] In order to overcome the shortcomings of the prior art, the present invention aims to provide a method for determining the loess collapsibility coefficient based on the proportion of large and medium porosity and water content. This method requires less work, produces more intuitive data graphs, and provides a more accurate evaluation of the loess's collapsibility, thereby enabling better prevention and control work.

[0005] To achieve the above objectives, the technical solution adopted by the present invention is as follows:

[0006] A method for determining the collapsibility coefficient of loess based on the proportion of large and medium porosity and water content includes the following steps:

[0007] Step 1: Take undisturbed soil samples and determine basic physical properties;

[0008] Step 2: Prepare two groups of soil samples with different moisture contents;

[0009] Step 3: Conduct indoor consolidation tests on the two groups of soil samples with different moisture contents. The moisture content w` of the first group of soil samples after consolidation is measured. For the second group of soil samples, further collapsibility tests are conducted, and the collapsibility coefficient δ of each soil sample is determined. s;

[0010] Step 4: Perform mercury intrusion porosimetry on the undisturbed soil samples in their initial state, and classify the pore sizes into large, medium, small, and micro pores according to the fractal volume model; perform mercury intrusion porosimetry on the first group of soil samples with the measured water content after consolidation, and measure the proportion of large and medium pores n of each soil sample under different water contents w` and different pressures.

[0011] Step 5: In Origin, utilize the water content w`, the proportion of large and medium porosity n, and the collapsibility coefficient δ s A 3D surface model is fitted, and the fitting formula δ is output. s = f(w`, n);

[0012] Step Six: Fit the formula δ s =f(w`, n) is used for testing.

[0013] Step one specifically involves: taking soil samples from the collapsible loess layer at the target site, cutting off the entire undisturbed soil sample, tightly wrapping it, marking the top and bottom surfaces, as well as the time and location of the soil sampling, transporting it back to the laboratory, and placing it in a dry and ventilated place; conducting water content, density, and particle size distribution tests on the soil sample according to GB / T50123-2019 "Standard for Geotechnical Testing Methods", and determining the proportion of large and medium porosity in the undisturbed soil sample according to step four.

[0014] Step two specifically involves preparing the collected soil samples into ring soil samples and dividing them into two groups according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods"; reducing or increasing the moisture content by air drying and water film transfer methods, thereby setting the target moisture content of the ring soil samples to 5%, 10%, 15%, 20%, and 25% respectively.

[0015] Step three specifically involves: conducting consolidation tests on the two prepared soil samples according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods"; for general collapsible loess, vertical loads of 200 kPa, 400 kPa, and 800 kPa are taken sequentially; for newly deposited loess, vertical loads of 100 kPa, 200 kPa, 400 kPa, and 800 kPa are taken sequentially; after the consolidation tests, the water content w` of each soil sample in the first group is measured, and the proportion of large and medium pores is measured according to step four; the collapsibility test is conducted on the second group of soil samples according to GB50025-2018 "Standard for Construction in Collapsible Loess Areas", and the collapsibility coefficient δ of each soil sample is measured. s .

[0016] The step 4 is specifically as follows: perform a mercury intrusion test on the undisturbed soil sample in the initial state, according to the fractal volume model method, that is, V(d<D) / Vt∝D^k, where V(d<D) represents the cumulative volume of pores with a diameter less than D, Vt is the total pore volume of the soil sample, and k is the linear fitting slope of the relationship between lg(V(d<D) / Vt) and lgD. Since the curve of the fractal volume model method does not have a unique slope but presents piecewise linear characteristics, the pore size at the turning point on the curve is taken as the demarcation point to divide it into 4 parts, and each part has a fixed slope. Therefore, the sections corresponding to these 4 parts are named as micropores, small pores, mesopores and macropores respectively in the way of relative pore size; perform a mercury intrusion test on the first group of soil samples that have passed the consolidation test, measure the pore volume and pore size distribution of each soil sample after consolidation under different moisture contents w' and different pressures, calculate the proportions of macropores, mesopores, small pores and micropores according to the pore size, so as to further determine the proportion n of macropores and mesopores in each soil sample, as shown in formula (1),

[0017]

[0018] In the formula: n — the proportion of macropores and mesopores of the soil sample after consolidation stabilization;

[0019] v' — the total volume of macropores and mesopores of the soil sample after consolidation stabilization;

[0020] v — the total pore volume of the soil sample after consolidation stabilization.

[0021] The step 5 is specifically as follows: in the Origin software, set the X-axis, Y-axis and Z-axis as the moisture content w', the proportion n of macropores and mesopores, and the collapsibility coefficient δ in sequence s , input all the data obtained from the test into the Origin software, establish a three-dimensional surface model through the fitting function of the software, and output the fitting formula δ s =f(w', n), as shown in formula (2), so as to establish a method for determining the collapsibility coefficient based on the proportion of macropores and mesopores and the moisture content;

[0022] f(w', n)=aw' 2 +bw'+cn 2 +dn+e (2)

[0023] In the formula: w' — the moisture content of the soil sample after consolidation stabilization (%);

[0024] a, b, c, d, e — model fitting parameters.

[0025] The step 6 is specifically as follows: prepare at least two groups of soil samples with arbitrary moisture contents, repeat the above steps 3 and 4 for one group, substitute the measured moisture content w' and the proportion n of macropores and mesopores into the fitting formula δ s =f(w', n) to obtain δ s1 Another group determined the collapsibility coefficient δ according to GB50025-2018 "Standard for Building Construction in Collapsible Loess Areas". s The measured collapsibility coefficient δ s Comparative test δ s 1 If the collapsibility coefficient δ after substituting into the fitting formula s 1 With the collapsibility coefficient δ s If the data error is within 3%, the verification is successful, and the fitted model is accurate and usable; if the data error exceeds 3%, the verification fails, and the experiment needs to be repeated and the model fitted again.

[0026] Compared with the prior art, the present invention has the following advantages:

[0027] 1. Compared with traditional methods for determining the collapsibility coefficient, this invention can quickly determine the collapsibility coefficient by measuring the water content and the proportion of large and medium porosity in the soil sample. The method is simple and easy to operate.

[0028] 2. Compared with traditional methods for macroscopically determining the collapsibility coefficient, this invention essentially considers the two determinants of loess collapsibility: water content and the proportion of large and medium porosity. The collapsibility of soil samples is determined by these two key indicators, making the measured results more accurate. This is a major innovation in loess mechanics.

[0029] 3. Compared with the two-dimensional planar diagram drawn by traditional collapsibility tests, the present invention finally forms a three-dimensional curved surface model diagram, which can be used to more intuitively, vividly and accurately determine the collapsibility potential of loess under different water contents and the proportion of large and medium porosity. Attached Figure Description

[0030] Figure 1 This is a flowchart of an embodiment of the present invention.

[0031] Figure 2 The following is a sampling diagram of loess in the study area of ​​the example; where (a) is the location of a sampling point at a foundation pit, and (b) is the original soil sample packaging.

[0032] Figure 3 This is a diagram illustrating the preparation of undisturbed soil samples for an example.

[0033] Figure 4 This is a diagram of the consolidation apparatus for an example.

[0034] Figure 5 The graph shows the mercury intrusion porosimetry results of undisturbed loess in its initial state, as an example.

[0035] Figure 6 The figure shows the deformation pore volume curves of undisturbed loess under different pressures in the example.

[0036] Figure 7The figure shows the pore size distribution curves of undisturbed loess under different pressures in the example.

[0037] Figure 8 The diagram shows the distribution of pore volume content of undisturbed loess under different pressures in the example.

[0038] Figure 9 The example shows a three-dimensional scatter plot and model of the proportion of large and medium pores, water content and collapsibility coefficient of undisturbed loess under different pressures. Detailed Implementation

[0039] The present invention will be further described in detail below with reference to the embodiments.

[0040] like Figure 1 As shown, a method for determining the collapsibility coefficient of loess based on the proportion of large and medium porosity and water content includes the following steps:

[0041] Step 1: Take undisturbed soil samples and measure basic physical properties;

[0042] like Figure 2 As shown, the loess in this embodiment was taken from Weiyang District, Xi'an City, Shaanxi Province. The soil depth was between 2.0m and 3.0m. The soil was yellowish-brown and uniform in texture. When taking the soil, the soil sample was cut into a whole piece of approximately 40cm*40cm*40cm and tightly wrapped with black plastic bags and tape. The upper and lower parts of the soil were marked. During transportation, the disturbance of the soil was strictly controlled. After being transported back to the laboratory, the soil was placed in a dry and ventilated place. The moisture content and density of the soil were tested according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods" (5.2) and (6.2). The specific gravity of the soil particles was taken as 2.70. After conversion of the three ratios, the void ratio was calculated to be 1.07. The basic physical properties of the soil sample are shown in Table 1.

[0043] (1) The natural moisture content was measured by the drying method, and the moisture content ω was calculated according to equation (3):

[0044]

[0045] Where: m—total mass of soil sample (g);

[0046] m s —Total mass of solid particles in the soil sample (g);

[0047] w—Natural moisture content (%);

[0048] (2) The natural density was measured using the ring cutter method. The natural density ρ of the soil sample was calculated according to equation (4):

[0049]

[0050] Where: v—total volume of soil sample (cm³) 3 The volume of the large ring cutter is 100 cm³. 3 ;

[0051] ρ — Natural density (g / cm³) 3 );

[0052] Three sets of parallel experiments were conducted, and the average value was taken to obtain the final natural density ρ.

[0053] The calculated natural water content w is 15.84%, and the natural density ρ is 1.51 g·cm³. -3 ;

[0054] Table 1 Basic physical properties of soil samples

[0055] <![CDATA[Specific gravity of soil particles G s > Natural moisture content ω (%) <![CDATA[Natural density ρ (g / cm 3 )]]> Porosity e 2.70 15.84 1.51 1.07

[0056] Step two: Prepare two groups of soil samples with different moisture contents;

[0057] like Figure 3 As shown, in this embodiment, the collected soil samples were prepared into ring soil samples with a diameter of 79.8 mm and a height of 20 mm according to GB / T50123-2019 "Standard for Geotechnical Testing Methods" (4.5). The designed moisture content w1 of the soil samples was controlled by air drying and water film transfer method. Soil samples with target moisture contents of 5%, 10%, and 15% were dehydrated by natural air drying in a dehydration dish, while soil samples with target moisture contents of 20% and 25% were dehydrated by water film transfer method. The soil samples were prepared as follows: For general collapsible loess, 6 identical soil samples were prepared at each moisture content (according to step 3, 2 sets of consolidation tests under 3 different pressures were required), for a total of 30 soil samples; For newly deposited loess with high compressibility, 8 identical soil samples were prepared at each moisture content (according to step 3, 2 sets of consolidation tests under 4 different pressures were required), for a total of 40 soil samples; The newly deposited loess can be judged according to Appendix D of GB50025-2018 "Standard for Building Construction in Collapsible Loess Areas";

[0058] Fill a spray bottle with the predetermined amount of distilled water and spray it gently and evenly onto the upper and lower surfaces of the soil sample in several applications; wrap all soil samples that have reached the target moisture content with plastic wrap and place them in a humidifying dish for at least 48 hours to achieve uniform internal moisture content before conducting an indoor consolidation test; cover with plastic film for sealed curing to prevent moisture evaporation; the amount of water that needs to be reduced or increased is calculated according to formula (5):

[0059]

[0060] Where: m w —The amount of water that needs to be increased or decreased (g);

[0061] w1—Design moisture content (%);

[0062] w0—Target moisture content (%);

[0063] m0—the current mass (g) of the soil sample;

[0064] Step 3: Conduct indoor consolidation tests on the two groups of soil samples with different moisture contents. The moisture content w` of the first group of soil samples after consolidation is measured. For the second group of soil samples, further collapsibility tests are conducted, and the collapsibility coefficient δ of each soil sample is determined. s ;

[0065] In this embodiment, consolidation tests were conducted on three soil samples (four for newly deposited loess) at five different moisture contents in two groups, according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods". For general collapsible loess, vertical loads were taken as 200 kPa, 400 kPa, and 800 kPa respectively; for newly deposited loess, vertical loads were taken as 100 kPa, 200 kPa, 400 kPa, and 800 kPa respectively. After the consolidation tests, the moisture content w` of each soil sample in the first group was measured, and the proportion of large and medium pores was determined according to step four. The collapsibility test was carried out on the second group of soil samples according to GB50025-2018 "Standard for Building Construction in Collapsible Loess Areas" (4.3), and the collapsibility coefficient δ of each soil sample was determined. s .

[0066] First, in this embodiment, standard consolidation tests were simultaneously conducted on two groups of soil samples using a consolidation apparatus. The consolidation tests were performed in the laboratory using a standard consolidation apparatus (see...). Figure 4 To complete the test, the prepared soil sample is placed in a consolidation apparatus, and vertical loads are applied sequentially at 200 kPa, 400 kPa, and 800 kPa. Consolidation continues for one day after each load application until the soil sample deformation is less than 0.01 mm per hour. The specific test procedures are as follows:

[0067] 3.1) Place the permeable stone 5 and filter paper 4 in container 1. Carefully place the soil sample 9 with the ring cutter and the ring cutter 3 together with the blades facing down into the lower protective ring 2. Then place the filter paper 4 and permeable stone 5 on the soil sample 9 with the ring cutter. Install the pressure cap 6. Connect the gauge sleeve 7 to the pressure cap 6. The gauge sleeve 7 and the gauge holder 8 are matched. Finally, place the pressure piston and install the pressure device and dial gauge.

[0068] 3.2) Apply preload to make the soil sample contact with the upper and lower parts of the instrument, adjust the dial gauge or sensor to zero or take the initial reading. Usually, the dial gauge distance is adjusted to be greater than 8 mm.

[0069] 3.3) Determine the pressure levels to be applied, with pressure levels of 200 kPa, 400 kPa, and 800 kPa respectively;

[0070] 3.4) The four soil samples in each group were tested under different pressures. The height of the soil sample was measured after 24 hours of each applied pressure as the stability standard. When the deformation was less than 0.01 mm every hour, it was taken as the stability degree until the end of the test.

[0071] Secondly, after the experiment, the instruments used to measure the first group of soil samples were removed, the soil samples were taken out, and the water content w` after consolidation was measured. The test results are shown in Table 2 below.

[0072] Table 2. Calculation of Moisture Content After Consolidation under Various Pressure Preloading Levels (%)

[0073]

[0074] Finally, the second group of consolidated soil samples underwent a loess collapsibility test using the following method.

[0075] 3.5) Take the second set of soil samples after consolidation and stabilization;

[0076] 3.6) Unload the soil samples under each pressure, and then uniformly load them to 200 kPa (for newly deposited highly compressible soil, the test pressure should be loaded to 100 kPa). Measure the height h1 of the soil sample after deformation stabilization under 200 kPa pressure. After deformation stabilization under 200 kPa immersion pressure, pour pure water into container 1 from bottom to top or from top to bottom. The water level should be higher than the top surface of the soil sample. Measure the degree of deformation every 1 hour until the soil sample deformation stabilizes. Measure the height h2 of the soil sample after immersion deformation stabilization.

[0077] 3.7) Determine the stability reading of soil sample immersion deformation, and calculate the collapsibility coefficient of each soil sample according to formula (6). The calculation results are shown in Table 3 below.

[0078]

[0079] Where: δ s --------- Collapse coefficient;

[0080] h1----------The height (mm) of the soil sample after deformation stabilization under a certain pressure level;

[0081] h2----------The height (mm) of a soil sample after stabilization following water immersion and subsidence deformation under a certain pressure level;

[0082] h0----------Original height of soil sample (mm);

[0083] Table 3. Calculation of Loess Collapsibility Coefficient at 200 kPa after Preloading at Various Pressure Levels

[0084]

[0085] Step 4: Perform a mercury intrusion test on the undisturbed soil sample in the initial state, and classify the pore sizes into large, medium, small, and micro pores according to the fractal volume model; perform a mercury intrusion test on the first group of soil samples whose water content after consolidation has been measured, and measure the large and medium pore proportion n of each soil sample under different water contents w' and different pressures;

[0086] Perform a mercury intrusion test on the undisturbed soil sample in the initial state, according to the fractal volume model method, that is, V(d<D) / Vt∝D^k, where V(d<D) represents the cumulative volume of pores with a diameter less than D, Vt is the total pore volume of the soil sample, k is the slope of the straight line fit for the relationship between lg(V(d<D) / Vt) and lgD. Since the curve of the fractal volume model method does not have a unique slope but presents piecewise linear characteristics, the pore size with an obvious turning point on the curve is taken as the demarcation point to divide it into 4 parts, each part has a fixed slope. Therefore, the sections corresponding to these 4 parts are named as micropores, small pores, medium pores, and large pores respectively in the manner of relative pore size; perform a mercury intrusion test on the first group of soil samples that have undergone the consolidation test, measure the pore volume and pore size distribution of each soil sample after consolidation under different water contents w' and different pressures, calculate the proportions of large, medium, small, and micro pores according to the pore sizes, so as to further determine the large and medium pore proportion n of each soil sample, as shown in formula (1),

[0087]

[0088] In the formula: n — the large and medium pore proportion of the soil sample after consolidation and stabilization;

[0089] v' — the total volume of large and medium pores of the soil sample after consolidation and stabilization;

[0090] v — the total pore volume of the soil sample after consolidation and stabilization;

[0091] With reference to Figure 5 , based on the pore size distribution curve of the undisturbed loess in the study area in the initial state obtained from the mercury intrusion test (excluding a few minimum points in the low-high pressure conversion interval), this curve characterizes the pore volume density (dV / dlogD, mL / g) within a certain pore size range per unit mass of soil sample. It can be found that there are three peaks on the loess pore size distribution curve: the first peak with a medium peak point is located in the medium pores, and its dominant pore size is about 0.57μm; the second relatively sharp peak with a higher peak point and the gentle areas on both sides represent the inter-particle pore group (mosaic pores, overhead pores and secondary pores), and its dominant pore size is about 6.58μm; the third relatively gentle peak with a lower peak point is located in the large pores, and its dominant pore size is about 118.47μm.

[0092] As can be seen from the cumulative pore volume curve, the curve does not have a unique slope, but rather exhibits a segmented linear characteristic. There are three obvious inflection points on the curve: 0.02 μm, 0.21 μm, and 13.5 μm. Dividing the curve into four parts, each part has a fixed slope. This indicates that the pores within each interval (scale-free region) have self-similarity, that is, the pore size distribution of loess has multifractal characteristics. Therefore, these three dividing points can be used as the boundary pore sizes to distinguish similar pores within each interval. The corresponding segments are named micropores, small pores, mesopores, and macropores respectively, based on their relative pore size. These four types of pores have their corresponding material structure characteristics and formation mechanisms in natural sedimentary loess. Micropores correspond to intragranular pores, small pores correspond to embedded pores, mesopores correspond to ventral pores, and macropores correspond to a small number of large-sized ventral pores and visible secondary pores.

[0093] Reference Figure 6 The deformation pore volume curves of undisturbed loess under different pressures show that: under the same pressure, as the water content increases, the variation range of the cumulative pore volume of the soil sample gradually increases significantly. Within the medium pore size range (0.21–13.5 μm), the cumulative volume of the soil sample shows obvious changes. When P ≤ 400 kPa, the relative changes of undisturbed loess with different water contents are obvious in the micro, small, and medium pore size ranges, while the cumulative pore volume curves basically overlap in the large pore size range. When P = 800 kPa, the relative changes of the cumulative pore volume curves of undisturbed loess with different water contents in the micro, small, and medium pore size ranges are relatively small, while the cumulative pore volume curves for the large pore size basically overlap.

[0094] Reference Figure 7 The pore size distribution curves of undisturbed loess deformation under different pressures show that the overall trend of the pore size distribution density curves is relatively consistent. From the perspective of the boundary pore size, the pore size distribution density of mesopores varies more and is dominant, followed by the pore size distribution density of macropores, and the pore size distribution density of micro and small pores is the lowest. As the pressure increases, the distribution density of micro and small pores increases slightly, while the distribution density of macro and mesopores shows a decreasing trend. Under the same pressure, as the water content increases, the distribution density curve shows a decreasing trend.

[0095] Reference Figure 8 According to mercury porosimetry test data ( Figure 6 and Figure 7 The percentage of large and medium pores in the total pores of soil samples with different water contents was measured under vertical loads of 200 kPa, 400 kPa and 800 kPa, respectively, so as to determine the percentage of large and medium pores n in each soil sample. The calculation results are shown in Table 4 below.

[0096] Table 4. Calculation of the proportion of large and medium porosity in loess soil samples at 200 kPa after preloading at various pressure levels.

[0097]

[0098]

[0099] Step 5: In Origin, utilize the water content w`, the proportion of large and medium porosity n, and the collapsibility coefficient δ s A 3D surface model is fitted, and the fitting formula δ is output. s =f(w`, n).

[0100] Reference Figure 9 The X-axis, Y-axis, and Z-axis are respectively set as water content w`, the proportion of large and medium porosity n, and the collapsibility coefficient δ. s All experimental data were input into Origin software. A three-dimensional surface model was built using the software's fitting function, and the fitting formula δ was output. s =f(w`, n); where the proportion of large and medium porosity, water content, and collapsibility coefficient of undisturbed loess are used as indicators to construct a nonlinear surface fitting model under different pressures, with fitting factor R. 2 The value is 0.98, and the quantization equation is as follows:

[0101] δ s =0.0000378w` 2 -0.00141w`+3.11035n 2 -3.96739n+1.27544 (7) Where:

[0102] w`—Moisture content (%) of the soil sample after consolidation and stabilization;

[0103] n—The proportion of large and medium porosity in the soil sample after consolidation and stabilization;

[0104] δ s — Collapse coefficient;

[0105] Step 6, fit the formula δ s =f(w`, n) is used for testing;

[0106] In this embodiment, two groups of soil samples with a moisture content of 7% were prepared. Steps three and four were repeated. Experiments showed that, under vertical loads of 150 kPa, 250 kPa, and 500 kPa, the consolidated moisture content w` of the soil samples was 6.82%, 6.54%, and 6.26%, respectively; the proportion of large and medium porosity n was 80.86%, 76.94%, and 71.58%, respectively; and the collapsibility coefficient δ... s The values ​​were 0.091, 0.057, and 0.022, respectively. The water content w` and the proportion of large and medium porosity n after consolidation of the soil samples under different pressures were substituted into the fitting formula δ. s In f(w`, n), we obtain δs 1 As shown in Table 5 below; compare the experimental values ​​δ of the soil samples. s and calculated value δ s 1 It can be observed that the fitting error is 2.4% at 150 kPa, 0.71% at 250 kPa, and 0.5% at 500 kPa. All four data errors are within the allowable range, so the fitting formula is obtained.

[0107] Table 5 Calculation of Collapse Coefficient

[0108] Pressure (kPa) 150 250 500 Moisture content w` (%) after consolidation 6.82 6.54 6.26 The percentage of large and medium porosity n (%) 0.8086 0.7694 0.7158 <![CDATA[Collapsibility coefficient δ s 1 > 0.0932 0.0566 0.02189

[0109] In summary, the advantages of this embodiment are:

[0110] 1. Compared with traditional methods for determining the collapsibility coefficient, this invention can quickly determine the collapsibility coefficient by measuring the water content and the proportion of large and medium porosity in the soil sample. The method is simple and easy to operate.

[0111] 2. Compared with traditional methods for macroscopically determining the collapsibility coefficient, this invention essentially considers the two determinants of loess collapsibility: water content and the proportion of large and medium porosity. The collapsibility of soil samples is determined by these two key indicators, making the measured results more accurate. This is a major innovation in loess mechanics.

[0112] 3. Compared with the two-dimensional planar diagram drawn by traditional collapsibility tests, the present invention finally forms a three-dimensional curved surface model diagram, which can be used to more intuitively, vividly and accurately determine the collapsibility potential of loess under different water contents and the proportion of large and medium porosity.

Claims

1. A method for determining the collapsibility coefficient of loess based on the proportion of large and medium porosity and water content, characterized in that, Includes the following steps: Step 1: Take undisturbed soil samples and determine basic physical properties; Step 2: Prepare two groups of soil samples with different moisture contents; Step 3: Conduct indoor consolidation tests on the two groups of soil samples with different moisture contents. Measure the moisture content of the first group of soil samples after consolidation. w` The second group of soil samples underwent collapsibility tests, and the collapsibility coefficient of each soil sample was determined. δ s ; Step 4: Perform mercury intrusion porosimetry on the undisturbed soil samples, and classify them into large, medium, small, and micro pore sizes according to the fractal volume model; perform mercury intrusion porosimetry on the first group of soil samples with the measured consolidated moisture content, and determine the different moisture contents. w` The proportion of large and medium porosity in various soil samples under different pressures n Specifically: Mercury intrusion porosimetry was performed on undisturbed soil samples, based on the fractal volume model method, i.e. V(d <D) / Vt ∞ DkV ( d <D ),in, V ( d <D ) indicates that the diameter is less than D The cumulative volume of pores, V t is the total pore volume of the soil sample. k yes lg ( V ( d <D ) / Vt )and lgD The slope of the linear fitting of the relationship between them; since the curve of the fractal volume model method does not have a unique slope, but rather exhibits piecewise linear characteristics, the pore size at the inflection point on the curve is used as the dividing point, dividing it into 4 parts, each with a fixed slope. The segments corresponding to the 4 parts are named micropores, small pores, medium pores, and large pores respectively according to the relative size of the pore size; mercury intrusion porosimetry is performed on the first group of soil samples that have passed the consolidation test to measure different water contents. w` The pore volume and pore size distribution of each soil sample after consolidation under different pressures were analyzed. Based on the pore size, the proportions of large, medium, small, and micro pores were calculated, thereby further determining the proportion of large and medium pores in each soil sample. n As shown in equation (1), (1) In the formula: n —The proportion of large and medium porosity in the soil sample after consolidation and stabilization; —The total volume of large and medium pores in the soil sample after consolidation and stabilization; v —Total pore volume of the soil sample after consolidation and stabilization; Step 5: Utilize moisture content in Origin w` Large and medium porosity n and collapsibility coefficient δ s Fit a 3D surface model and output the fitting formula. δ s = f ( w` , n Specifically: In Origin software, set the X-axis, Y-axis, and Z-axis to moisture content in sequence. w` Large and medium porosity n and collapsibility coefficient δ s All the data obtained from the experiment were input into Origin software. The software then used fitting to build a three-dimensional surface model and output the fitting formula. δ s = f ( w` , n As shown in equation (2), a method for determining the collapsibility coefficient based on the proportion of large and medium pores and water content is established. f ( w` , n )=a w` 2 +bw`+cn 2 +dn+e (2) In the formula: w` —Moisture content (%) of the soil sample after consolidation and stabilization; a , b , c , d , e — Model fitting parameters; Step Six: Fitting the Formula δ s = f ( w` , n The following steps are performed: Prepare at least two soil samples with arbitrary moisture content. Repeat steps three and four above for each sample, and measure the moisture content. w` Large and medium porosity n Substitute into the fitting formula δ s = f ( w` , n From ), we obtain δ s 1 Another group determined the collapsibility coefficient according to GB50025-2018 "Standard for Building Construction in Collapsible Loess Areas". δ s Using the measured collapsibility coefficient δ s Comparative test δ s 1 If the collapsibility coefficient after substituting into the fitting formula δ s 1 With the collapsibility coefficient δ s If the data error is within 3%, the verification is successful, and the fitted model is accurate and usable; if the data error exceeds 3%, the verification fails, and the experiment needs to be repeated and the model fitted again.

2. The method according to claim 1, characterized in that, Step one specifically involves: taking soil samples from the collapsible loess layer at the target site, cutting off the entire undisturbed soil sample, tightly wrapping it, marking the top and bottom surfaces, as well as the time and location of the soil sampling, transporting it back to the laboratory, and placing it in a dry and ventilated place; conducting water content, density, and particle size distribution tests on the soil sample according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods", and determining the large and medium void ratio of the undisturbed soil sample according to step four.

3. The method according to claim 1, characterized in that, The second step is as follows: the collected soil samples are prepared into ring soil samples and divided into two groups according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods"; the water content is reduced or increased by air drying method and water film transfer method, so that the target water content of the ring soil samples is set to 5%, 10%, 15%, 20%, and 25% respectively.

4. The method according to claim 1, characterized in that, Step three specifically involves conducting consolidation tests on the two prepared soil samples according to GB / T 50123-2019 "Standard for Geotechnical Testing Methods". For general collapsible loess, vertical loads are taken as follows: 200 kPa, 400 kPa, and 800 kPa. For newly deposited loess, vertical loads are taken as follows: 100 kPa, 200 kPa, 400 kPa, and 800 kPa. After the consolidation tests are completed, the water content of each soil sample in the first group is measured. w`, And determine the proportion of large and medium porosity according to step four; The second group of soil samples underwent collapsibility testing according to GB50025-2018 "Standard for Building Construction in Collapsible Loess Areas", and the collapsibility coefficient of each soil sample was determined. δ s .

Citation Information

Patent Citations

  • Loess collapsibility coefficient calculation method

    CN106485057A