A tempering tool for achieving damage-free ultra-thin flexible glass surface
By designing the tempering tooling of the multi-layer flexible glass placement unit and the jagged edge fixing rope, the problem of invisible friction lines on the flexible glass surface caused by the contact of the support strips in the existing technology has been solved, and the damage-free tempering of the flexible glass surface has been achieved, improving product quality.
Patent Information
- Application Number
- CN202210730634.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-24
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-06-24
AI Technical Summary
In mass production of existing ultra-thin flexible glass tempering tooling, invisible friction lines are caused by the contact between the support bar and the glass surface, which increases the defective rate of the product.
A tempered tooling including an outer frame, a multi-layer flexible glass placement unit, an edge fixing rope and a tooling limiter is designed. A point contact space is formed through a multi-strand bottom limiter rope and a zigzag edge fixing rope to reduce the contact between the flexible glass and the tooling stopper. The contact area of the tooling.
It minimizes the occurrence of friction marks on the surface of flexible glass and improves product quality and production efficiency.
Smart Images

Figure CN117923772B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of flexible glass preparation, and in particular to a tempering tool for achieving surface damage-free ultra-thin flexible glass. Background Art
[0002] In order to improve the scratch resistance and impact resistance of the ultra-thin flexible glass surface, it is usually necessary to place the ultra-thin flexible glass in a tempered tank to enhance the strength of the glass surface. Before the glass is placed in the tempered tank, special tooling is required to fix it.
[0003] The applicant has applied for patent CN214299866 U, which discloses a tooling for tempering ultra-thin flexible glass (UTG), including: an installation frame, which is formed by connecting multiple support surfaces end to end; a support bar, which is detachably installed in the installation frame, and a plurality of the support bars are arranged in a horizontal and vertical interval to form an independent chamber for storage. The tooling is placed in the tempering tank to temper the glass. The installation frame and the support bar are made of high-temperature resistant materials. The support bar is detachably installed in the installation frame. A plurality of the support bars are arranged in a horizontal and vertical interval to form an independent chamber for storage. The size of the independent chamber is determined according to the size specifications of the foldable glass. When it is necessary to temper glass similar to the size of a mobile phone screen, the horizontal and vertical intervals between the plurality of the support bars are relatively small. When it is necessary to temper glass similar to the size of a tablet screen, the horizontal and vertical intervals between the plurality of the support bars are relatively large. The applicant discovered in actual production that since the independent chambers are formed by support strips arranged vertically and horizontally, when visually inspecting the flexible glass in batches, it was found that invisible friction lines would appear on the surface of the flexible glass due to contact with the support strips, which increased the defective rate of the product to a certain extent. Summary of the invention
[0004] The present invention provides a tempering tool for preventing the surface of ultra-thin flexible glass from being damaged, so as to solve the problems raised in the above-mentioned background technology.
[0005] In order to solve the above technical problems, the present invention discloses a tempering tool for preventing the surface of ultra-thin flexible glass from being damaged, comprising: an outer frame, a multi-strand bottom limiting rope for placing the flexible glass is installed at the bottom end of the outer frame;
[0006] A flexible glass placement unit, which is composed of a multi-layer flexible glass tooling assembly and is installed in the outer frame from top to bottom;
[0007] The edge fixing rope is zigzag-shaped and wound around the flexible glass tooling assembly, and a point contact space for limiting the flexible glass is formed in the groove of the edge fixing rope.
[0008] Preferably, the flexible glass tooling assembly is composed of two tooling limiters arranged opposite to each other, and both ends of the tooling limiters can be slidably mounted on the outer frame.
[0009] Preferably, a strip-shaped locking screw hole is provided on the outer frame, and two ends of the tooling limiter can be slidably installed in the strip-shaped locking screw hole by screws.
[0010] Preferably, the tooling limit piece is arranged in a sawtooth shape, and a fixing groove is provided on the back of the tooling limit piece for facilitating the winding of the edge fixing rope, and the groove of the edge fixing rope is formed between the tooth blocks of adjacent tooling limit pieces.
[0011] Preferably, the tooling limit piece is arranged in a comb-teeth shape, and fixing columns for facilitating the winding of the edge fixing rope are arranged at equal intervals on the tooling limit piece, and the fixing columns are arranged close to the groove of each of the tooling limit pieces, and the groove of the edge fixing rope is formed between the tooth columns of adjacent tooling limit pieces.
[0012] Preferably, it also includes:
[0013] The side limiting rope is provided on the fixing column with a groove for passing the side limiting rope, and the two ends of the flexible glass in the width direction are placed on the side limiting rope.
[0014] Preferably, the bottom limiting rope, the side fixing rope and the side limiting rope are all made of metal ropes or corrosion-resistant fiber ropes. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0016] Figure 1 It is a structural schematic diagram of the present invention;
[0017] Figure 2 For the top view of the present invention Figure 1 ;
[0018] Figure 3 For the top view of the present invention Figure 2 .
[0019] In the figure: 11, outer frame; 12, flexible glass tooling group; 13, side fixing rope; 14, bottom limiting rope; 15, fixing column; 16, side limiting rope. DETAILED DESCRIPTION
[0020] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0021] In addition, in the present invention, the descriptions of "first", "second", etc. are only used for descriptive purposes, and do not specifically refer to the order or sequence, nor are they used to limit the present invention. They are only used to distinguish components or operations described with the same technical terms, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions and technical features between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0022] Example 1
[0023] The embodiment of the present invention provides a tool for tempering ultra-thin flexible glass to prevent damage to the surface. Figure 1 As shown, including:
[0024] An outer frame 11, wherein a plurality of bottom limiting ropes 14 for placing flexible glass are installed at the bottom end of the outer frame 11;
[0025] Flexible glass placement unit: a multi-layer flexible glass tooling set 12 constitutes the flexible glass placement unit 1 and is installed in the outer frame 11 from top to bottom;
[0026] The edge fixing rope 13 is zigzag-shaped and wound around the flexible glass tooling assembly 12 . A point contact space for limiting the position of the flexible glass is formed in the groove of the edge fixing rope 13 .
[0027] The flexible glass tooling set 12 is composed of two tooling limiters arranged opposite to each other, and both ends of the tooling limiters can be slidably installed on the outer frame 11.
[0028] The flexible glass tooling set 12 is composed of two tooling limiters arranged opposite to each other, and both ends of the tooling limiters can be slidably installed on the outer frame 11.
[0029] The working principle of the above technical solution is as follows: the present invention provides a tempering tooling for achieving damage-free surface of ultra-thin flexible glass. The flexible glass is placed into the flexible glass placement unit from the top of the outer frame 11, and the edge end of the flexible glass is placed in the point contact space formed by the bottom limiting rope 14 and the side fixing rope 13. The tooling is placed in the tempering groove to complete the tempering process of the flexible glass.
[0030] The beneficial effects of the above technical solution are as follows: the present invention provides a tempering tooling for achieving damage-free surface of ultra-thin flexible glass, which minimizes the contact area between the flexible glass and the tooling, and does not produce invisible friction lines on the surface of the flexible glass during the tempering process.
[0031] Example 2
[0032] On the basis of the above-mentioned embodiment 1, Figure 2 As shown, the tooling limiter is serrated, and a fixing groove is provided on the back of the tooling limiter for facilitating the winding of the edge fixing rope 13 , and the groove of the edge fixing rope 13 is formed between the tooth blocks of adjacent tooling limiters.
[0033] The working principle and beneficial effects of the above technical solution are:
[0034] The tooling limiter is arranged in a serrated shape, and the groove of the edge fixing rope 13 is formed between the tooth blocks of the adjacent tooling limiter. The edge end of the flexible glass is placed in the groove of the edge fixing rope 13 to form a point contact space for limiting the edge end of the flexible glass.
[0035] Example 3
[0036] On the basis of the above-mentioned embodiment 1, Figure 3 As shown, the tooling limit piece is arranged in a comb-teeth shape, and the tooling limit piece is provided with fixed columns 15 at equal intervals for facilitating the winding of the edge fixing rope 13. The fixed columns 15 are arranged close to the groove of each of the tooling limit pieces, and the groove of the edge fixing rope 13 is formed between the tooth columns of adjacent tooling limit pieces.
[0037] Among them, it also includes:
[0038] The side limiting rope 16 is provided on the fixing column 15 with a groove for passing the side limiting rope 16 , and the two ends of the flexible glass in the width direction are placed on the side limiting rope 16 .
[0039] The working principle and beneficial effects of the above technical solution are:
[0040] The tooling limit piece is arranged in a comb-teeth shape, and the groove of the edge fixing rope 13 is formed between the tooth columns of adjacent tooling limit pieces. The edge end of the flexible glass in the width direction is located between the two edge limiting ropes 16 and can be movably located in the groove of the fixing rope 13, so that the flexible glass has a small range of displacement in its thickness direction.
[0041] Example 4
[0042] On the basis of the above-mentioned embodiments 1-3, the bottom limiting rope 14, the side fixing rope 13 and the side limiting rope 16 are all made of metal ropes or corrosion-resistant fiber ropes.
[0043] The working principle and beneficial effects of the above technical solution are as follows: when it is necessary to temper glasses of different sizes, the placement plate 7 is moved to drive the rotating rod 21 to move, drive the roller 13 to roll in the hole groove 18, and change the distance between the placement plates 7; by setting the roller 13, the distance between the placement plates 7 can be effectively adjusted, and the friction is small, and glasses of different sizes can also be placed, which effectively improves the functionality of the device.
[0044] Example 5
[0045] On the basis of any one of the above embodiments 1-4, the tooling for tempering the ultra-thin flexible glass surface to prevent damage further includes:
[0046] Thermometer: The thermometer is installed in the tempering tank to detect the temperature in the tempering tank;
[0047] Timer: The timer is installed on the outer wall of the tempered glass tank and is used to detect the working time of the tempered glass tank;
[0048] The second controller and the alarm are respectively installed on the outside of the tempering tank, the second controller is electrically connected to the thermometer, the timer and the alarm, and the second controller controls the alarm to work based on the thermometer and the timer, including the following steps:
[0049] Step 1: The second controller obtains the tempering degree index of the tempering tank based on the thermometer, the timer and formula (1):
[0050]
[0051] Among them, K is the tempering degree index of the tempering tank; C is the specific heat capacity of the glass; ρ is the density of the glass; V is the volume of a single piece of glass; T1 is the thermometer detection value; P is the rated power of the tempering tank; ε is the heating efficiency of the tempering tank; t is the timer detection value; is the time change coefficient of the tempering tank; T2 is the normal temperature setting value of the glass to be processed;
[0052] Step 2: Compare the tempering degree index of the tempered glass tank calculated by formula (1) with the preset tempering degree index range. When the tempering degree index of the tempered glass tank calculated by formula (1) is not within the preset tempering degree index range, the second controller controls the alarm to sound an alarm.
[0053] Among them, specific heat capacity is also called specific heat capacity, or specific heat for short. It is the heat capacity of a substance per unit mass, that is, the internal energy absorbed or released when a unit mass object changes unit temperature. Specific heat capacity is a physical quantity that represents the thermal properties of a substance;
[0054] The time change coefficient is the ratio of temperature to time when the horizontal tempering tank uses different furnace temperature setting values.
[0055] In the formula, CρVT1 is used to represent the energy required to heat the tempered tank to T1 during operation. It is used to indicate the time required for the tempering tank to be heated to the actual temperature. The time required to heat to the actual temperature and the preset temperature during heating;
[0056] Assume that the specific heat capacity of glass C = 0.64 kJ / kg·℃; the density of glass ρ = 2.5 kg / m3; the volume of a single glass piece V = 2 m3; the temperature in the tempering tank T1 = 690℃; the rated power of the tempering tank P = 10 kW; the heating efficiency of the tempering tank ε = 0.86; the working time of the tempering tank t = 1 h; the time change coefficient of the tempering tank The normal temperature setting value of the glass to be processed is T2=650°C; the tempering degree index K of the tempering tank can be calculated as K=1.64. If the corresponding preset tempering degree index range is 0.6-3, the alarm will not sound at this time.
[0057] The working principle and beneficial effects of the above calculation scheme are as follows: first, the tempering degree index of the tempering tank is calculated using formula (1), and the controller compares the tempering degree index of the tempering tank calculated by formula (1) with the preset tempering degree index range. When the tempering degree index of the tempering tank calculated by formula (1) is not within the preset tempering degree index range of 0.6-3, the controller controls the alarm to alarm, reminding personnel that the furnace temperature in the tempering tank is too high or too low, and timely checking the situation in the tempering tank. By setting the alarm to realize abnormal alarm and remind personnel to check the problem, the safety and service life of the tempered glass can be effectively improved, and the quality of the tempered glass can be improved.
[0058] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. If these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A tempering tool for achieving surface damage-free ultra-thin flexible glass, characterized in that: include: An outer frame (11), wherein a plurality of bottom limit ropes (14) for placing flexible glass are installed at the bottom end of the outer frame (11); A flexible glass placement unit, wherein a multi-layer flexible glass tooling set (12) constitutes the flexible glass placement unit (1) and is installed from top to bottom in the outer frame (11); An edge fixing rope (13), the edge fixing rope (13) being wound around the flexible glass tooling assembly (12) in a zigzag shape, and a point contact space for limiting the position of the flexible glass is formed in a groove of the edge fixing rope (13); The tooling is placed in the tempered tank; The tooling also includes: Thermometer: The thermometer is installed in the tempering tank to detect the temperature in the tempering tank; Timer: The timer is installed on the outer wall of the tempered glass tank and is used to detect the working time of the tempered glass tank; The second controller and the alarm are respectively installed on the outside of the tempering tank, the second controller is electrically connected to the thermometer, the timer and the alarm, and the second controller controls the alarm to work based on the thermometer and the timer, including the following steps: Step 1: The second controller obtains the tempering degree index of the tempering tank based on the thermometer, the timer and formula (1): in, is the toughening degree index of the toughened tank; is the specific heat capacity of glass; is the density of glass; is the volume of a single piece of glass; is the thermometer detection value; is the rated power of the tempered tank; The heating efficiency of the tempering tank; Detect value for the timer; is the time change coefficient of the tempering tank; is the normal temperature setting value of the glass to be processed; wherein, the time change coefficient is the ratio of temperature to time when the horizontal tempering tank uses different furnace temperature setting values; Step 2: Compare the tempering degree index of the tempered glass tank calculated by formula (1) with a preset tempering degree index range. When the tempering degree index of the tempered glass tank calculated by formula (1) is not within the preset tempering degree index range, the second controller controls the alarm to sound an alarm. The flexible glass tooling assembly (12) is composed of two tooling limiters arranged opposite to each other, and both ends of the tooling limiters can be slidably mounted on the outer frame (11); The tooling limiting member is arranged in a comb-tooth shape, and fixing columns (15) are arranged at equal intervals on the tooling limiting member to facilitate the winding of the edge fixing rope (13), and the fixing columns (15) are arranged close to the groove of each tooling limiting member, and the groove of the edge fixing rope (13) is formed between the tooth columns of adjacent tooling limiting members; Also includes: A side limiting rope (16), wherein a groove for passing the side limiting rope (16) is provided on the fixing column (15), and both ends of the flexible glass in the width direction are placed on the side limiting rope (16).
2. The tooling for tempering ultra-thin flexible glass to prevent damage to the surface according to claim 1, characterized in that: The outer frame (11) is provided with a strip-shaped locking screw hole, and the two ends of the tooling limiter can be slidably mounted in the strip-shaped locking screw hole by means of screws.
3. The tooling for tempering ultra-thin flexible glass to prevent damage to the surface according to claim 1, characterized in that: The bottom limiting rope (14), the side fixing rope (13) and the side limiting rope (16) are all made of metal ropes or corrosion-resistant fiber ropes.
Citation Information
Patent Citations
Tool for ultra-thin flexible glass (UTG) tempering
CN214299866U
Ultrathin glass toughened frame
CN114031276A
Production tempering frame for mobile phone film
CN204916453U