A method, device, equipment and medium for detecting oxidation wear of cutting tools

By determining the detection time point based on the wear curve of similar tools, and combining a variety of microscopes and analysis techniques to gradually detect tool oxidation wear, the problem of inaccurate detection results in the existing technology is solved, and more accurate oxidation wear detection and workpiece processing quality are achieved. promote.

CN118417947BActive Publication Date: 2024-10-11四川工程职业技术大学
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410892045.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-04
Publication Date
2024-10-11
Estimated Expiration
2044-07-04

AI Technical Summary

Technical Problem

The detection results of tool oxidation wear in the existing technology are inaccurate, resulting in problems with workpiece processing accuracy and surface quality, and the occurrence time and degree of tool oxidation wear cannot be effectively predicted.

Method used

By determining multiple inspection time points of the tool to be inspected based on the wear curves of similar tools, and using optical microscopes, scanning electron microscopes, energy spectrometers and X-ray diffraction technology to gradually conduct inspections, obtain detailed information on the tool wear area and improve inspection results. accuracy.

Benefits of technology

It improves the accuracy of tool oxidation wear detection, can predict the occurrence time and degree of oxidation wear, guide tool design and improve workpiece processing quality, and avoid early tool failure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118417947B_ABST
    Figure CN118417947B_ABST
Patent Text Reader

Abstract

The present application provides a tool oxidation wear detection method, device, equipment and medium, which relates to the field of tool detection technology, and is used to solve the problem of poor accuracy of tool oxidation wear detection results. The method includes: determining multiple detection time points of the tool to be detected according to the tool wear curve of the same type of tool; the tool information and processing information of the tool to be detected and the same type of tool are the same; the multiple detection time points include a first time point; during the processing of the tool to be detected on the machine tool, at the first time point, the tool to be detected is obtained from the machine tool, and the first image of the tool to be detected under the first optical microscope is obtained; the first image is compared with the optical microscope image of the new tool to obtain the first detection result of the tool to be detected. The present application determines the detection time point according to the wear curve of the same type of tool, detects the tool to be detected at the determined detection time point, and improves the accuracy of the detection result of tool oxidation wear.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of tool wear detection, and provides a tool oxidation wear detection method, device, equipment and medium. Background Art

[0002] Different tool wear mechanisms have different effects on workpiece machining accuracy and surface quality, which can easily cause workpiece dimensional deviation and surface quality deterioration in the semi-finishing and finishing stages, and even cause the workpiece to be scrapped. Tool oxidation wear seriously damages the tool coating and substrate, and has a significant impact on the workpiece surface machining quality. The detection results of tool oxidation wear have a promoting effect on tool design, tool coating improvement and workpiece surface quality improvement.

[0003] In the prior art, tool oxidation wear detection is performed based on data or images. Since the tool wear process is a slowly changing process, when tools of different materials cut different workpiece materials, the tool wear rates and tool lives are different. Tool oxidation wear randomly appears at different stages of tool wear. Tool wear is detected at different stages, and the test results obtained are different, resulting in inaccurate tool oxidation wear detection results obtained by the prior art. Summary of the invention

[0004] The present application provides a tool oxidation wear detection method, device, equipment and medium, which are used to solve the problem of poor accuracy of tool oxidation wear detection results.

[0005] In a first aspect, a method for detecting oxidation wear of a tool is provided, comprising:

[0006] Determine multiple detection time points of the tool to be detected according to the tool wear curve of the same type of tool; wherein the tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time; the tool information and processing information of the tool to be detected and the tool of the same type are the same; the multiple detection time points include the first time point;

[0007] During the machining process of the tool to be detected on the machine tool, at the first time point, the tool to be detected is obtained from the machine tool, and a first image of the tool to be detected under a first optical microscope is obtained;

[0008] The first image is compared with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected; the optical microscope image of the new tool is an image of the new tool just out of the factory under a second optical microscope, and the first detection result is used to indicate information about the tool wear area of ​​the tool to be detected.

[0009] Optionally, multiple detection time points of the tool to be detected are determined based on the tool wear curve of the same type of tool, including:

[0010] According to the tool wear curve of the same type of tool, determine the normal wear start time and the processing scrap time; wherein the normal wear start time refers to the time point when the same type of tool begins to show normal wear during the processing; the processing scrap time refers to the time point when the same type of tool has quality problems during the processing;

[0011] The time period from the start time of normal wear to the processing scrap time is divided into equal intervals to determine a plurality of detection time points of the tool to be detected.

[0012] Optionally, the multiple detection time points further include a second time point later than the first time point; after comparing the first image with the optical microscope image of the new tool to obtain the first detection result of the tool to be detected, the tool oxidation wear detection method further includes:

[0013] If the first detection result does not meet the preset condition, the tool to be detected is returned to the machine tool for further processing; the preset condition is used to indicate that the tool to be detected has undergone oxidation wear;

[0014] At the second time point, acquiring the tool to be detected from the machine tool, and acquiring a second image of the tool to be detected under the first optical microscope;

[0015] The second image is compared with the optical microscope image of the new tool to obtain a second detection result of the tool to be detected; the second detection result is used to indicate information about the tool wear area of ​​the tool to be detected.

[0016] Optionally, the preset conditions include at least one of the following conditions: the area ratio of the tool wear area is greater than a preset ratio, the grayscale value of the tool wear area is within a preset grayscale value range, the length of the adhesive in the tool wear area is greater than a preset length, and the number of adhesives in the tool wear area is greater than a preset number.

[0017] Optionally, after comparing the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected, the tool oxidation wear detection method further includes:

[0018] If the first detection result meets the preset condition, a third image of the tool to be detected under the first scanning electron microscope is obtained, and an energy spectrum of the electron beam scanning the tool to be detected is obtained; the energy spectrum is used to indicate the distribution of each element in the tool to be detected and / or the surface workpiece material; the surface workpiece material refers to the workpiece material bonded to the surface of the tool to be detected;

[0019] Compare the third image with the electron microscope image of the new tool to obtain a third detection result of the tool to be detected; the electron microscope image of the new tool is an image of the new tool just produced by the factory under the second scanning electron microscope; the third detection result is used to indicate information about the tool wear area of ​​the tool to be detected;

[0020] The energy spectrum is analyzed to obtain an energy spectrum analysis result; the energy spectrum analysis result is used to indicate the content percentage of each element.

[0021] Optionally, after analyzing the energy spectrum to obtain the energy spectrum analysis result, the tool oxidation wear detection method further includes:

[0022] If the third detection result meets the preset condition and the percentage of oxygen content in the energy spectrum analysis result is greater than the preset percentage, X-ray diffraction (XRD) detection is performed on the tool to be detected to obtain the XRD conventional detection result of the tool to be detected; the XRD conventional detection result is used to indicate the crystal structure information of the tool to be detected and / or the surface workpiece material.

[0023] Optionally, after performing X-ray diffraction (XRD) detection on the tool to be detected to obtain a conventional XRD detection result of the tool to be detected, the tool oxidation wear detection method further includes:

[0024] If the peak distribution in the conventional XRD test result coincides with the oxide distribution of the tool material and / or the workpiece material in the parameter library, the oxidation area of ​​the tool to be tested and / or the surface workpiece material is determined according to the bright spot area of ​​the oxygen distribution in the energy spectrum analysis result;

[0025] Performing XRD detection on the oxidized area to obtain an XRD micro-area detection result of the tool to be detected; the XRD micro-area detection result is used to indicate the crystal structure information of the oxidized area.

[0026] In a second aspect, a tool oxidation wear detection device is provided, comprising:

[0027] A detection time determination module, used to determine a plurality of detection time points of the tool to be detected according to a tool wear curve of a similar tool; wherein the tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time; the tool information and processing information of the tool to be detected and the similar tool are the same; the plurality of detection time points include the first time point;

[0028] An image acquisition module, used to acquire the tool to be detected from the machine tool at the first time point during the processing of the tool to be detected on the machine tool, and acquire a first image of the tool to be detected under a first optical microscope;

[0029] The detection module is used to compare the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected; the optical microscope image of the new tool is an image of the new tool just out of the factory under a second optical microscope, and the first detection result is used to indicate information about the tool wear area of ​​the tool to be detected.

[0030] In a third aspect, the present application provides a computer device, which includes a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the tool oxidation wear detection method described in the first aspect.

[0031] In a fourth aspect, the present application provides a computer-readable storage medium having a computer program stored thereon, and a processor executes the computer program to implement the tool oxidation wear detection method described in the first aspect.

[0032] Compared with the prior art, the beneficial effects of the embodiments of the present application are as follows:

[0033] The present application provides a tool oxidation wear detection method, which determines multiple detection time points of the tool to be detected based on the tool wear curve of similar tools, that is, the relationship between the wear degree and the processing time during the processing, and the multiple detection time points include a first time point. During the processing of the tool to be detected, the image of the tool to be detected at the first time point is compared with the image of a new tool just produced by the factory under an optical microscope to obtain information on the tool wear area of ​​the tool to be detected. The method can predict the time point when the tool to be detected starts to oxidize and wear based on the tool wear curve of similar tools, and then detect the tool to be detected at the determined detection time point, which can improve the accuracy of the detection result of tool oxidation wear. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] In order to more clearly illustrate the technical solutions in the embodiments of the present application or the related technologies, the drawings required for use in the embodiments or the related technical descriptions are briefly introduced below. Obviously, the drawings described below are only the embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.

[0035] Attached Figure 1 A schematic diagram of an application scenario provided for an embodiment of the present application;

[0036] Attached Figure 2 A schematic diagram of a process flow of a tool oxidation wear detection method provided in an embodiment of the present application;

[0037] Attached Figure 3 A schematic diagram of a tool wear curve provided in an embodiment of the present application;

[0038] Attached Figure 4 A schematic diagram of five tool wear curves provided in an embodiment of the present application;

[0039] Attached Figure 5 A schematic diagram of the conventional XRD test results provided in the embodiments of the present application;

[0040] Attached Figure 6 A schematic diagram of the XRD micro-area detection results provided in the embodiments of the present application;

[0041] Attached Figure 7 A schematic diagram of the overall process of the tool oxidation wear detection method provided in an embodiment of the present application;

[0042] Attached Figure 8 This is a schematic diagram of the structure of a tool oxidation wear detection device provided in an embodiment of the present application.

[0043] Markings in the figure: 101 - processor, 102 - communication bus, 103 - user interface, 104 - network interface, 105 - memory. DETAILED DESCRIPTION

[0044] In order to make the purpose, technical scheme and advantages of the present application clearer, the technical scheme in the embodiment of the present application will be clearly and completely described below in conjunction with the drawings in the embodiment of the present application. Obviously, the described embodiment is only a part of the embodiment of the present application, rather than all the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application. In the absence of conflict, the embodiments in the present application and the features in the embodiments can be combined with each other arbitrarily. In addition, although the logical order is shown in the flow chart, in some cases, the steps shown or described can be performed in an order different from that here.

[0045] In order to solve the problem of poor accuracy of tool oxidation wear detection results, the present application provides a tool oxidation wear detection method, which is applied to computer equipment. Before introducing the specific technical solution of the present application, the hardware operating environment involved in the embodiment of the present application is first introduced.

[0046] See attached Figure 1 , attached Figure 1 A schematic diagram of the computer device structure of the hardware operating environment involved in the embodiment of the present application.

[0047] As attached Figure 1As shown, the computer device may include: a processor 101, such as a central processing unit (CPU), a communication bus 102, a user interface 103, a network interface 104, and a memory 105. Among them, the communication bus 102 is used to realize the connection and communication between these components. The user interface 103 may include a display screen (Display), an input unit such as a keyboard (Keyboard), and the optional user interface 103 may also include a standard wired interface and a wireless interface. The network interface 104 may optionally include a standard wired interface and a wireless interface (such as a wireless fidelity (WIreless-FIdelity, WI-FI) interface). The memory 105 may be a high-speed random access memory (Random Access Memory, RAM) memory, or a stable non-volatile memory (Non-Volatile Memory, NVM), such as a disk memory. The memory 105 may also be a storage device independent of the aforementioned processor 101.

[0048] Those skilled in the art will appreciate that Figure 1 The structure shown in the figure does not constitute a limitation on the computer device, and may include more or less components than shown in the figure, or combine some components, or arrange the components differently.

[0049] As attached Figure 1 As shown, the memory 105 as a storage medium may include an operating system, a network communication module, a user interface module, and a tool oxidation wear detection device.

[0050] In the attached Figure 1 In the computer device shown, the network interface 104 is mainly used for data communication with the network server; the user interface 103 is mainly used for data interaction with the user; the processor 101 and the memory 105 in the computer device of the present invention can be set in the computer device, and the computer device calls the tool oxidation wear detection device stored in the memory 105 through the processor 101, and executes the tool oxidation wear detection method provided in the embodiment of the present application.

[0051] Based on the computer device of the aforementioned embodiment, refer to the attached Figure 2 The present invention provides a method for detecting oxidation wear of a tool, comprising the following steps:

[0052] S201. Determine multiple detection time points of a tool to be detected according to a tool wear curve of a similar tool.

[0053] In the specific implementation process, the computer device can pre-store in the database the tool wear curves of different tools in the process of processing different materials. The tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time. The tool to be tested refers to the tool that has not been tested for oxidation wear. The tool to be tested can be a tool that processes the target material on a machine tool.

[0054] After determining the tool information and processing information of the tool to be detected, the tool wear curve of the same type of tool is obtained from the database. The tool information and processing information of the tool to be detected and the same type of tool are the same. Then, based on the tool wear curve, multiple detection time points of the tool to be detected are determined. The multiple detection time points include a first time point and a second time point that is later than the first time point. The first time point can be any one of the multiple detection time points, and can also be the earliest time point of the multiple detection time points.

[0055] Among them, tool information and processing information are involved, which are introduced below respectively.

[0056] 1. Tool information:

[0057] Tool information is used to describe relevant information of the tool, such as tool material, tool type, etc.

[0058] 1. Tool material: such as high-speed steel, carbide, ceramic, diamond, etc.

[0059] 2. Types of tools: such as turning tools, milling cutters, drills, boring tools and grinding tools, etc.

[0060] 2. Processing information:

[0061] Processing information is used to describe relevant information during the tool processing process, such as processing methods, process parameters, workpiece material type, etc.

[0062] 1. Processing methods: such as turning, milling, drilling, boring, grinding, etc.

[0063] 2. Process parameters: such as cutting speed, feed per tooth, cutting depth, cutting width, etc.

[0064] 3. Workpiece material type: such as aluminum, iron, steel, titanium alloy, high temperature alloy, composite material, carbon fiber, etc.

[0065] The following uses the same type of tool as an example to introduce how to obtain the tool wear curve.

[0066] During the process of processing the target material by the same type of tool, the average wear width of the flank face of the same type of tool is detected at preset time intervals. The average wear width of the flank face refers to the average width of the wear area of ​​the flank face, and the corresponding processing time points are recorded until the average wear width of the flank face of the same type of tool reaches a preset width, for example, 300 μm. The detection is stopped, and multiple processing time points and the average wear width of the flank face corresponding to each processing time point are obtained. The tool wear curve of the same type of tool is drawn with multiple processing times t as the horizontal axis and the average wear width VB of the flank face corresponding to each processing time point as the vertical axis.

[0067] In a possible embodiment, after obtaining the tool wear curve of the same type of tool, the normal wear start time and the processing scrap time can be determined according to the tool wear curve of the same type of tool, and the time period from the normal wear start time to the processing scrap time can be divided into equal intervals to determine multiple detection time points for the tool to be detected.

[0068] In the specific implementation process, the normal wear start time refers to the time point when the same type of tool begins to show normal wear during the processing, specifically the start time of the straight line approaching the horizontal in the tool wear curve. The processing scrap time refers to the time point when the same type of tool has quality problems during the processing, specifically the time point corresponding to the preset width in the tool wear curve.

[0069] For example, the ten equal points from the start time of normal wear to the processing scrap time can be determined as multiple detection time points of the tool to be detected. The multiple detection time points are sorted in order from early to late, including the first time point, the second time point, ..., the Nth time point, the difference between two adjacent time points is the same, the first time point is the start time of normal wear, the second time point is later than the first time, and the Nth time point is the processing scrap time, N represents the total number of the multiple detection time points, and N is a positive integer greater than 1.

[0070] Please refer to the attached Figure 3 , is a schematic diagram of a tool wear curve provided in an embodiment of the present application, which is generated during the turning process of a coated cemented carbide tool on a nickel-based high-temperature alloy. Figure 3 The horizontal axis t is the processing time in seconds, and the vertical axis VB is the average wear width of the flank in μm. The first time point is t=600s, and the Nth time point is the time point t=2400 corresponding to the preset width of 300μm.

[0071] Please refer to the attached Figure 4 , which is a schematic diagram of five tool wear curves provided in the embodiment of the present application. These five tool wear curves are obtained when the coated cemented carbide tool is milling a nickel-based high-temperature alloy at different cutting speeds. v c Produced under, attached Figure 4 The horizontal axis is the cutting time, i.e., the processing time, in seconds, and the vertical axis is the average wear width VB of the flank, in μm. The normal wear start time (i.e., the first time point) of the five tool wear curves is different. The first time point corresponding to the cutting speed of 25 m / min is t=500s, the first time point corresponding to the cutting speed of 30 m / min is 800s, the first time point corresponding to the cutting speed of 35 m / min is 1000s, the first time point corresponding to the cutting speed of 40 m / min is 1200s, and the first time point corresponding to the cutting speed of 45 m / min is 2000s.

[0072] S202 . While the tool to be inspected is being processed on a machine tool, at a first time point, the tool to be inspected is obtained from the machine tool, and a first image of the tool to be inspected under a first optical microscope is obtained.

[0073] In a specific implementation process, when the tool to be detected starts to process the target material on the machine tool, the target material is, for example, a nickel-based high-temperature alloy. At a first time point, the machine tool is stopped, and the tool to be detected is removed from the machine tool, and the tool to be detected is placed on the workbench of the first optical microscope, and the magnification of the first optical microscope is adjusted. After the camera device captures the first image of the tool to be detected under the first optical microscope, the first image is sent to the computer device, or the computer device itself captures the first image of the tool to be detected under the first optical microscope.

[0074] S203: Compare the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected.

[0075] In the specific implementation process, the computer device can pre-store the optical microscope image of the new tool in the database in advance, wherein the optical microscope image of the new tool is the image of the new tool just produced under the second optical microscope, and the new tool can be the tool to be tested or a similar tool. The second optical microscope and the first optical microscope can be the same optical microscope. If the second optical microscope and the first optical microscope are different optical microscopes, then the second optical microscope and the first optical microscope have the same model and the same magnification. The optical microscope image of the new tool can be sent to the computer device after being collected by the camera device, or it can be collected by the computer device itself, or it can be input by the user, or it can be downloaded from the Internet.

[0076] After obtaining the first image, the first image is compared with the new tool optical microscope image to determine the tool wear area in the first image. For example, the first image and the new tool optical microscope image can be imported into image processing software, the two images are superimposed together, the two images are placed in different layers, and their transparency is adjusted so that the first image and the new tool optical microscope image can be displayed at the same time, and then the contrast and brightness are adjusted to highlight the tool wear area in the first image. Finally, the tool wear area in the first image is marked, and then the first detection result of the tool to be detected is obtained based on the tool wear area in the first image. The first detection result is used to indicate the information of the tool wear area of ​​the tool to be detected. The information of the tool wear area is introduced in detail below.

[0077] The information of the tool wear area includes the area ratio, color, length of adhesive, number of adhesives, etc. of the tool wear area, wherein the area ratio of the tool wear area refers to the ratio of the area of ​​the tool wear area to the total area of ​​the tool, and the color of the tool wear area can be represented by a grayscale value, and the grayscale value generally ranges from 0 to 255. The larger the grayscale value, the closer the color is to white, and the smaller the grayscale value, the closer the color is to black. Since the tool wear area may contain multiple pixels, the grayscale value of each pixel may be different, so the grayscale value of the tool wear area can be the maximum value or average value of the grayscale values ​​of multiple pixels. The adhesive in the tool wear area refers to a layer of deposits formed on the surface or blade of the tool, such as residues, oxides or other chemicals of the cutting material. The length of the adhesive refers to the size of the adhesive in a preset direction. Since the tool wear area may contain multiple adhesives, the length of the adhesive can be the maximum value or average value of the lengths of multiple adhesives.

[0078] In the embodiment of the present application, taking into account that different tools have different oxidation wear rates when processing different workpiece materials, the time point when the tool to be tested begins to undergo oxidation wear is predicted based on the tool wear curve of similar tools. Then, at the predicted time point, the tool to be tested is tested through an optical microscope, which can improve the accuracy of the tool oxidation wear test results.

[0079] In a possible embodiment, after comparing the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be inspected, if the first detection result does not meet the preset conditions, the tool to be inspected is returned to the machine tool for further processing; at a second time point, the tool to be inspected is obtained from the machine tool, and a second image of the tool to be inspected under the first optical microscope is obtained; the second image is compared with the optical microscope image of the new tool to obtain a second detection result of the tool to be inspected.

[0080] In the specific implementation process, the preset condition is used to indicate that the tool to be detected has undergone oxidation wear. If the first detection result does not meet the preset condition, it means that the tool to be detected has not undergone oxidation wear. The tool to be detected is put back into the machine tool for further processing. The machine tool is stopped at a second time point, and the tool to be detected is taken out from the machine tool. The tool to be detected is placed on the workbench of the first optical microscope, and the magnification of the first optical microscope is adjusted. After the computer device obtains the second image of the tool to be detected under the first optical microscope, the second image is compared with the optical microscope image of the new tool to obtain the second detection result of the tool to be detected. The second detection result is used to indicate the information of the tool wear area of ​​the tool to be detected. The process of obtaining the second detection result is the same as the process of obtaining the first detection result, which will not be repeated here.

[0081] In an embodiment of the present application, when oxidation wear has not yet occurred on the tool to be tested, the tool to be tested is placed back into the machine tool, and the tool to be tested is taken out again for oxidation wear testing at the next testing time point. By continuously searching for the time point when the oxidation reaction occurs, the oxides generated during the processing process can be detected, and then the oxidation wear can be determined, thereby ensuring the accuracy of the oxidation wear test results.

[0082] In a possible embodiment, after comparing the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected, if the first detection result meets a preset condition, a third image of the tool to be detected under a first scanning electron microscope is obtained, and an energy spectrum of the electron beam scanning the tool to be detected is obtained; the third image is compared with the electron microscope image of the new tool to obtain a third detection result of the tool to be detected; and the energy spectrum is analyzed to obtain an energy spectrum analysis result.

[0083] In the specific implementation process, the preset condition is used to indicate that the tool to be tested has undergone oxidation wear. If the first test result meets the preset condition, it means that the tool to be tested has undergone oxidation wear. Then, the tool to be tested is placed on the workbench of the first scanning electron microscope, and the magnification of the first scanning electron microscope is adjusted. The scanning electron microscope is a microscope that uses an electron beam to observe the sample. The surface of the tool to be tested is scanned by the electron beam, and the electron beam reflected from the surface of the tool to be tested is measured to form a third image, and the energy spectrum of the electron beam is measured. The energy spectrum is used to indicate the distribution of each element in the tool to be tested and / or the surface workpiece material. The surface workpiece material refers to the workpiece material bonded to the surface of the tool to be tested. The energy spectrum can indicate the distribution of each element in the tool to be tested, and can also indicate the distribution of each element in the workpiece material bonded to the surface of the tool to be tested.

[0084] After obtaining the third image and the energy spectrum, the third image is compared with the electron microscope image of the new tool to determine the tool wear area in the third image. The electron microscope image of the new tool is an image of a new tool that has just left the factory under the second scanning electron microscope. The second scanning electron microscope and the first scanning electron microscope can be the same scanning electron microscope. If the second scanning electron microscope and the first scanning electron microscope are different scanning electron microscopes, then the second scanning electron microscope and the first scanning electron microscope have the same model and the same magnification. Then, according to the tool wear area in the third image, the third detection result of the tool to be detected is obtained, and the third detection result is used to indicate the information of the tool wear area of ​​the tool to be detected. And by analyzing the energy spectrum, the energy spectrum analysis result can be obtained, and the energy spectrum analysis result is used to indicate the content percentage of each element, and the content percentage can be weight percentage or atomic percentage.

[0085] In an embodiment of the present application, an optical microscope is used to inspect the tool to be inspected. After determining that the tool to be inspected is likely to have oxidation wear, a scanning electron microscope is used to further inspect the tool to be inspected to obtain more detailed oxidation wear detection results for the tool to be inspected.

[0086] As described above, two situations are introduced: the first detection result meets the preset condition and the first detection result does not meet the preset condition. The preset condition is involved and is introduced below.

[0087] In a possible embodiment, the preset conditions include at least one of the following conditions: the area ratio of the tool wear area is greater than the preset ratio, the grayscale value of the tool wear area is within the preset grayscale value range, the length of the adhesive in the tool wear area is greater than the preset length, and the number of adhesives in the tool wear area is greater than the preset number.

[0088] Among them, the preset proportion is, for example, one-fifth, the preset gray value range is the gray value range corresponding to dark gray, black, blue, purple and other colors, the preset length is, for example, 20μm or 50μm, and the preset number is, for example, 3.

[0089] It should be noted that there are multiple combinations of preset conditions, and the preset proportions, preset gray value ranges, preset lengths, and preset numbers may be different in different combinations. For example, if the preset condition is that the length of the adhesive in the tool wear area is greater than the preset length, then the preset length is 50 μm. If the length of the adhesive exceeds 50 μm, it means that the first detection result meets the preset condition. If the length of the adhesive is less than 50 μm, it means that the first detection result does not meet the preset condition. Or for example, if the preset condition is that the length of the adhesive in the tool wear area is greater than the preset length and the number of adhesives is greater than the preset number, then the preset length is 20 μm and the number of adhesives is 3. If the length of the adhesive exceeds 20 μm and the number of adhesives exceeds 3, it means that the first detection result meets the preset condition. If the length of the adhesive is less than 20 μm and / or the number of adhesives is less than 3, it means that the first detection result does not meet the preset condition.

[0090] In the embodiment of the present application, the preset conditions are determined by combining different conditions to meet the actual needs of the tools to be detected in different situations. The accuracy of the judgment can be improved according to a variety of conditions, thereby improving the accuracy of whether to perform further detection.

[0091] In a possible embodiment, after analyzing the energy spectrum and obtaining the energy spectrum analysis result, if the third detection result meets the preset conditions and the oxygen content percentage in the energy spectrum analysis result is greater than the preset percentage, an X-ray diffraction (XRD) test is performed on the tool to be detected to obtain the XRD conventional test result of the tool to be detected; the XRD conventional test result is used to indicate the crystal structure information of the tool to be detected and / or the surface workpiece material.

[0092] In the specific implementation process, it is determined whether the third test result meets the preset conditions and the percentage of oxygen content in the energy spectrum analysis result is greater than the preset percentage. The preset conditions are used to indicate that oxidation wear has occurred on the tool to be tested. If the third test result meets the preset conditions and the percentage of oxygen content in the energy spectrum analysis result is greater than the preset percentage, for example, 5%, the tool to be tested is further subjected to conventional XRD testing, and the entire area of ​​the tool to be tested is irradiated with X-rays, and the angle and intensity of diffraction of the tool to be tested are measured. According to the diffraction intensity at different diffraction angles, the conventional XRD test result of the tool to be tested, that is, the overall diffraction spectrum, can be obtained. By analyzing the position, intensity, shape and other characteristics of the diffraction peak in the diffraction spectrum, the overall crystal structure information of the tool to be tested and / or the overall crystal structure information of the workpiece material bonded to the surface of the tool to be tested can be inferred.

[0093] Please refer to the attached Figure 5 , is a schematic diagram of the conventional XRD test results provided in the embodiments of the present application, and Figure 5The horizontal axis is the XRD angle, that is, the angle between the X-ray and the normal line of the tool surface, in degrees, and the vertical axis Intensity is the intensity of the XRD peak, in counts. The oxidation reaction of the tool to be tested is as follows:

[0094]

[0095] in, Indicates gas.

[0096] In an embodiment of the present application, based on the detection results of the scanning electron microscope, on the basis that the information of the tool wear area meets the preset conditions and the oxygen content percentage is greater than the preset percentage, the tool to be tested is further subjected to conventional XRD testing, and the entire tool can be analyzed to obtain an overall diffraction spectrum, so as to fully understand the overall situation of the tool to be tested.

[0097] In a possible embodiment, after analyzing the energy spectrum and obtaining the energy spectrum analysis result, if the third detection result meets the non-preset condition, or the oxygen content percentage in the energy spectrum analysis result is less than the preset percentage, the tool to be detected is returned to the machine tool for further processing; at a second time point, the tool to be detected is obtained from the machine tool, and a third image of the tool to be detected under a first scanning electron microscope is obtained, and the energy spectrum of the electron beam scanning the tool to be detected is obtained; the third image is compared with the electron microscope image of the new tool to obtain the third detection result of the tool to be detected, and the energy spectrum is analyzed to obtain the energy spectrum analysis result.

[0098] In a possible embodiment, after performing X-ray diffraction (XRD) detection on the tool to be detected and obtaining the XRD conventional detection result of the tool to be detected, if the distribution of peaks in the XRD conventional detection result coincides with the oxide distribution of the tool material and / or the workpiece material in the parameter library, the oxidation area of ​​the tool to be detected and / or the surface workpiece material is determined based on the bright spot area of ​​the oxygen distribution in the energy spectrum analysis result; the XRD micro-area detection is performed on the oxidation area to obtain the XRD micro-area detection result of the tool to be detected; the XRD micro-area detection result is used to indicate the crystal structure information of the oxidation area.

[0099] In the specific implementation process, if the XRD conventional test result coincides with the oxide distribution of the tool material in the parameter library, it means that the tool to be tested has indeed undergone an oxidation reaction, or, if the XRD conventional test result coincides with the oxide distribution of the workpiece material in the parameter library, it means that the surface workpiece material, that is, the workpiece material bonded to the surface of the tool to be tested, has indeed undergone an oxidation reaction. For the key areas of tool oxidation wear, including the oxidation area of ​​the tool to be tested, and / or the oxidation area of ​​the surface workpiece material, micro-area detection is performed using XRD with a voltage of 45KV, a current of 40mA, and a spot diameter of 0.5mm to 1.0mm, and the extremely small oxidation area is accurately analyzed to obtain the XRD micro-area detection result of the oxidation area, that is, the local diffraction spectrum. By analyzing the position, intensity, shape and other characteristics of the diffraction peak in the local diffraction spectrum, the crystal structure information of the oxidation area can be inferred, providing more detailed crystal structure information of the tool to be tested.

[0100] Please refer to the attached Figure 6 , is a schematic diagram of the XRD micro-area detection results provided in the embodiments of the present application, and Figure 6 The two curves in the figure represent the XRD conventional test results of the two oxidation areas. The horizontal coordinate Two-Theta represents the 2 times angle of XRD, the unit is deg, and the vertical coordinate Intensity represents the intensity of the XRD peak, the unit is Counts. The oxidation reaction in the oxidation area is as follows:

[0101]

[0102] in, Indicates gas.

[0103] In a possible embodiment, after performing X-ray diffraction (XRD) testing on the tool to be tested and obtaining the XRD conventional test result of the tool to be tested, if the distribution of peaks in the XRD conventional test result does not coincide with the oxide distribution of the tool material and the workpiece material in the parameter library, the tool to be tested is returned to the machine tool for further processing; at a second time point, the tool to be tested is obtained from the machine tool, and an XRD test is performed on the tool to be tested to obtain the XRD conventional test result of the tool to be tested.

[0104] Please refer to the attached Figure 7 , is a schematic diagram of the overall process of the tool oxidation wear detection method provided in the embodiment of the present application, and the following is combined with the attached Figure 7 The overall process of tool oxidation wear detection method is introduced.

[0105] First, according to the tool wear curve of similar tools, multiple detection time points of the tool to be detected are determined, and the multiple detection time points are sorted in order from early to late, including the first time point, the second time point, ..., the i-th time point. Initialize i=1, at the i-th time point, remove the tool to be detected from the machine tool, and use an optical microscope to detect the tool to be detected to obtain the first detection result.

[0106] Secondly, determine whether the first test result meets the preset conditions. If not, put the tool to be tested back into the machine tool, remove the tool to be tested from the machine tool at the i+1th time point, and continue to test the tool to be tested using an optical microscope. If yes, use a scanning electron microscope and an energy spectrometer to test the tool to be tested to obtain a third test result and an energy spectrum analysis result.

[0107] Then, it is determined whether the third test result meets the preset conditions and whether the oxygen content percentage in the energy spectrum analysis result is greater than the preset percentage. If not, the tool to be tested is put back into the machine tool, and at the i+1th time point, the tool to be tested is removed from the machine tool, and the tool to be tested is continuously tested using a scanning electron microscope and an energy spectrometer. If yes, the tool to be tested is routinely tested using XRD to obtain a conventional XRD test result.

[0108] Finally, determine whether the peak distribution in the XRD conventional test result coincides with the oxide distribution of the tool material and / or workpiece material in the parameter library. If so, use XRD to perform micro-area detection on the oxidized area to obtain the XRD micro-area detection result, and the process ends. If not, put the tool to be detected back into the machine tool, remove the tool to be detected from the machine tool at the i+1th time point, perform conventional detection on the tool to be detected using XRD, obtain the XRD conventional detection result, and the process ends until the last detection time point.

[0109] In summary, tool oxidation wear is a microscopic physical and chemical change that is not easy to observe. It requires the use of high-resolution ultra-depth optical microscopes, scanning electron microscopes, energy spectrometers, XRD and other equipment to detect tool oxidation wear. The existing technology usually uses one of these devices to detect tool oxidation wear, but the optical microscope cannot detect the detailed oxidation of the tool, and the scanning electron microscope, energy spectrometer and XRD equipment are expensive and have high requirements for the detection environment. In the case of uncertainty as to whether the tool has undergone oxidation wear, if the tool has not undergone oxidation wear or the degree of oxidation wear of the tool is low, blindly using scanning electron microscopes, energy spectrometers and XRD equipment for detection is not only costly, but may also obtain invalid test results, resulting in low detection efficiency.

[0110] The embodiment of the present application provides a tool oxidation wear detection method. According to the tool wear curve of similar tools, the detection time point of the tool to be detected is predicted, and the detection is performed at an appropriate detection time point. Through the judgment after each detection, the detection is performed step by step. With the help of optical microscopes, scanning electron microscopes, energy spectrometers and XRD and other equipment, the oxidation wear caused by the oxidation reaction of the tool material during the tool wear process is detected, thereby realizing the tool oxidation wear detection. According to the subsequent detection results of tool oxidation wear, it can promote the improvement of the tool matrix and coating, and the improvement of the workpiece processing surface quality, which is conducive to guiding the selection of appropriate cutting process parameters, avoiding the rapid oxidation reaction in the tool wear area, aggravating the tool wear and causing tool failure.

[0111] Based on the same inventive concept, as shown in the attached Figure 8 As shown, the embodiment of the present application also provides a tool oxidation wear detection device, comprising:

[0112] A detection time determination module is used to determine multiple detection time points of the tool to be detected according to a tool wear curve of a similar tool; wherein the tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time; the tool information and processing information of the tool to be detected and the similar tool are the same; the multiple detection time points include the first time point;

[0113] An image acquisition module is used to acquire the tool to be detected from the machine tool at a first time point during the processing of the tool to be detected on the machine tool, and to acquire a first image of the tool to be detected under a first optical microscope;

[0114] The detection module is used to compare the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected; the optical microscope image of the new tool is an image of the new tool just out of the factory under the second optical microscope, and the first detection result is used to indicate information about the tool wear area of ​​the tool to be detected.

[0115] Optionally, the detection time determination module is specifically used for:

[0116] According to the tool wear curve of similar tools, determine the normal wear start time and processing scrap time; the normal wear start time refers to the time point when similar tools begin to show normal wear during the processing; the processing scrap time refers to the time point when similar tools have quality problems during the processing;

[0117] The time period from the start time of normal wear to the processing scrap time is divided into equal intervals to determine multiple detection time points of the tool to be detected.

[0118] Optionally, the multiple detection time points further include a second time point later than the first time point; and the detection module is further used for:

[0119] After the first image is compared with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected, if the first detection result does not meet a preset condition, the tool to be detected is returned to the machine tool to continue processing the target material; the preset condition is used to indicate that the tool to be detected has been oxidized and worn;

[0120] At a second time point, obtaining a tool to be inspected from a machine tool, and obtaining a second image of the tool to be inspected under a first optical microscope;

[0121] The second image is compared with the optical microscope image of the new tool to obtain a second detection result of the tool to be detected; the second detection result is used to indicate information about the tool wear area of ​​the tool to be detected.

[0122] Optionally, the preset conditions include at least one of the following conditions: the area ratio of the tool wear area is greater than a preset ratio, the grayscale value of the tool wear area is within a preset grayscale value range, the length of the adhesive in the tool wear area is greater than a preset length, and the number of adhesives in the tool wear area is greater than a preset number.

[0123] Optionally, the detection module is also used to:

[0124] After the first image is compared with the optical microscope image of the new tool to obtain the first detection result of the tool to be detected, if the first detection result meets the preset condition, a third image of the tool to be detected under the first scanning electron microscope is obtained, and an energy spectrum of the electron beam scanning the tool to be detected is obtained; the energy spectrum is used to indicate the distribution of each element in the tool to be detected and / or the surface workpiece material; the surface workpiece material refers to the workpiece material bonded to the surface of the tool to be detected;

[0125] Compare the third image with the electron microscope image of the new tool to obtain a third detection result of the tool to be detected; the electron microscope image of the new tool is an image of the new tool just produced by the factory under the second scanning electron microscope; the third detection result is used to indicate information about the tool wear area of ​​the tool to be detected;

[0126] The energy spectrum is analyzed to obtain an energy spectrum analysis result; the energy spectrum analysis result is used to indicate the content percentage of each element.

[0127] Optionally, the detection module is also used to:

[0128] After analyzing the energy spectrum and obtaining the energy spectrum analysis result, if the third detection result meets the preset conditions and the oxygen content percentage in the energy spectrum analysis result is greater than the preset percentage, X-ray diffraction XRD detection is performed on the tool to be detected to obtain the XRD conventional detection result of the tool to be detected; the XRD conventional detection result is used to indicate the overall crystal structure information of the tool to be detected and / or the surface workpiece material.

[0129] Optionally, the detection module is also used to:

[0130] After performing X-ray diffraction (XRD) detection on the tool to be detected and obtaining the XRD conventional detection result of the tool to be detected, if the distribution of peaks in the XRD conventional detection result coincides with the oxide distribution of the tool material and / or the workpiece material in the parameter library, then determining the oxidation area of ​​the tool to be detected and / or the surface workpiece material according to the bright spot area of ​​oxygen distribution in the energy spectrum analysis result;

[0131] The oxidized area is subjected to XRD detection to obtain an XRD micro-area detection result of the tool to be detected; the XRD micro-area detection result is used to indicate the crystal structure information of the oxidized area.

[0132] It should be noted that each module in the tool oxidation wear detection device in this embodiment corresponds one-to-one to each step in the tool oxidation wear detection method in the aforementioned embodiment. Therefore, the specific implementation of this embodiment can refer to the implementation of the aforementioned tool oxidation wear detection method, which will not be repeated here.

[0133] In addition, in one embodiment, the present application also provides a computer device, which includes a processor, a memory, and a computer program stored in the memory, and the computer program implements the aforementioned tool oxidation wear detection method when executed by the processor.

[0134] In addition, in one embodiment, the present application also provides a computer storage medium, on which a computer program is stored, and when the computer program is executed by a processor, the aforementioned tool oxidation wear detection method is implemented.

[0135] In some embodiments, the computer readable storage medium may be a memory such as FRAM, ROM, PROM, EPROM, EEPROM, flash memory, magnetic surface memory, optical disk, or CD-ROM; or various devices including one or any combination of the above memories. The computer may be various computing devices including intelligent terminals and servers.

[0136] In some embodiments, executable instructions may be in the form of a program, software, software module, script or code, written in any form of programming language (including compiled or interpreted languages, or declarative or procedural languages), and may be deployed in any form, including as a stand-alone program or as a module, component, subroutine or other unit suitable for use in a computing environment.

[0137] As an example, executable instructions may, but need not, correspond to a file in a file system, may be stored as part of a file storing other programs or data, such as in one or more scripts in a HyperText Markup Language (HTML) document, in a single file dedicated to the program in question, or in multiple coordinated files (e.g., files storing one or more modules, subroutines, or code portions).

[0138] By way of example, executable instructions may be deployed to be executed on one computing device, or on multiple computing devices located at one site, or on multiple computing devices distributed across multiple sites and interconnected by a communication network.

[0139] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or system including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or system. In the absence of further restrictions, an element defined by the sentence "comprises a ..." does not exclude the existence of other identical elements in the process, method, article or system including the element.

[0140] The serial numbers of the above-mentioned embodiments of the present application are for description only and do not represent the advantages or disadvantages of the embodiments.

[0141] Through the description of the above implementation methods, those skilled in the art can clearly understand that the above-mentioned embodiment methods can be implemented by means of software plus a necessary general hardware platform, and of course by hardware, but in many cases the former is a better implementation method. Based on such an understanding, the technical solution of the present application, or the part that contributes to the prior art, can be embodied in the form of a software product, which is stored in a storage medium (such as a read-only memory / random access memory, a magnetic disk, or an optical disk), and includes a number of instructions for enabling a multimedia terminal device (which can be a mobile phone, a computer, a television receiver, or a network device, etc.) to execute the methods described in each embodiment of the present application.

[0142] The above are only preferred embodiments of the present application, and are not intended to limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.

Claims

1. A method for detecting oxidation wear of a tool, characterized in that: The method comprises: According to the tool wear curve of the same type of tool, multiple detection time points of the tool to be detected are determined; wherein the tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time; the tool information and processing information of the tool to be detected and the same type of tool are the same; the multiple detection time points include a first time point and a second time point later than the first time point; the first time point is any one of the multiple detection time points or the earliest time point of the multiple detection time points; During the machining process of the tool to be detected on the machine tool, at the first time point, the tool to be detected is obtained from the machine tool, and a first image of the tool to be detected under a first optical microscope is obtained; Compare the first image with the optical microscope image of the new tool to obtain a first detection result of the tool to be detected; the optical microscope image of the new tool is an image of the new tool just produced by the factory under the second optical microscope, and the first detection result is used to indicate information about the tool wear area of ​​the tool to be detected; If the first detection result does not meet the preset condition, the tool to be detected is returned to the machine tool for further processing; the preset condition is used to indicate that the tool to be detected has undergone oxidation wear; the preset condition includes at least one of the following conditions: the area ratio of the tool wear area is greater than the preset ratio, the gray value of the tool wear area is within the preset gray value range, the length of the adhesive in the tool wear area is greater than the preset length, and the number of adhesives in the tool wear area is greater than the preset number; At the second time point, acquiring the tool to be detected from the machine tool, and acquiring a second image of the tool to be detected under the first optical microscope; Comparing the second image with the optical microscope image of the new tool to obtain a second detection result of the tool to be detected; the second detection result is used to indicate information about the tool wear area of ​​the tool to be detected; If the first detection result meets the preset condition, a third image of the tool to be detected under the first scanning electron microscope is obtained, and an energy spectrum of the electron beam scanning the tool to be detected is obtained; the energy spectrum is used to indicate the distribution of each element in the tool to be detected and / or the surface workpiece material; the surface workpiece material refers to the workpiece material bonded to the surface of the tool to be detected; Compare the third image with the electron microscope image of the new tool to obtain a third detection result of the tool to be detected; the electron microscope image of the new tool is an image of the new tool just produced by the factory under the second scanning electron microscope; the third detection result is used to indicate information about the tool wear area of ​​the tool to be detected; The energy spectrum is analyzed to obtain an energy spectrum analysis result; the energy spectrum analysis result is used to indicate the content percentage of each element.

2. The tool oxidation wear detection method according to claim 1, characterized in that: According to the tool wear curve of similar tools, determine multiple detection time points for the tool to be tested, including: According to the tool wear curve of the same type of tool, determine the normal wear start time and the processing scrap time; wherein the normal wear start time refers to the time point when the same type of tool begins to show normal wear during the processing; the processing scrap time refers to the time point when the same type of tool has quality problems during the processing; The time period from the start time of normal wear to the processing scrap time is divided into equal intervals to determine a plurality of detection time points of the tool to be detected.

3. The tool oxidation wear detection method according to claim 1, characterized in that: After analyzing the energy spectrum and obtaining the energy spectrum analysis result, the tool oxidation wear detection method further includes: If the third detection result meets the preset condition and the percentage of oxygen content in the energy spectrum analysis result is greater than the preset percentage, X-ray diffraction (XRD) detection is performed on the tool to be detected to obtain the XRD conventional detection result of the tool to be detected; the XRD conventional detection result is used to indicate the crystal structure information of the tool to be detected and / or the surface workpiece material.

4. The tool oxidation wear detection method according to claim 3, characterized in that: After performing X-ray diffraction (XRD) detection on the tool to be detected and obtaining the XRD conventional detection result of the tool to be detected, the tool oxidation wear detection method further includes: If the peak distribution in the conventional XRD test result coincides with the oxide distribution of the tool material and / or the workpiece material in the parameter library, the oxidation area of ​​the tool to be tested and / or the surface workpiece material is determined according to the bright spot area of ​​the oxygen distribution in the energy spectrum analysis result; Performing XRD detection on the oxidized area to obtain an XRD micro-area detection result of the tool to be detected; the XRD micro-area detection result is used to indicate the crystal structure information of the oxidized area.

5. A tool oxidation wear detection device, characterized in that: include: A detection time determination module, used to determine multiple detection time points of a tool to be detected according to a tool wear curve of a similar tool; wherein the tool wear curve is used to indicate the relationship between the wear degree of the tool during the processing and the processing time; the tool information and processing information of the tool to be detected and the similar tool are the same; the multiple detection time points include a first time point and a second time point later than the first time point; the first time point is any one of the multiple detection time points or the earliest time point of the multiple detection time points; An image acquisition module, used to acquire the tool to be detected from the machine tool at the first time point during the processing of the tool to be detected on the machine tool, and acquire a first image of the tool to be detected under a first optical microscope; A detection module, used for comparing the first image with an optical microscope image of a new tool to obtain a first detection result of the tool to be detected; the optical microscope image of the new tool is an image of a new tool just produced from the factory under a second optical microscope, and the first detection result is used to indicate information about a tool wear area of ​​the tool to be detected; The detection module is further used for returning the tool to be detected to the machine tool for further processing if the first detection result does not meet a preset condition; the preset condition is used to indicate that the tool to be detected has undergone oxidation wear; the preset condition includes at least one of the following conditions: the area ratio of the tool wear region is greater than a preset ratio, the gray value of the tool wear region is within a preset gray value range, the length of the adhesive in the tool wear region is greater than a preset length, and the number of adhesives in the tool wear region is greater than a preset number; at the second time point, obtaining the tool to be detected from the machine tool, and obtaining a second image of the tool to be detected under the first optical microscope; comparing the second image with the optical microscope image of the new tool to obtain a second detection result of the tool to be detected; the second detection result is used to indicate information about the tool wear region of the tool to be detected; The detection module is also used to obtain a third image of the tool to be detected under the first scanning electron microscope and an energy spectrum of the electron beam scanning the tool to be detected if the first detection result meets the preset condition; the energy spectrum is used to indicate the distribution of each element in the tool to be detected and / or the surface workpiece material; the surface workpiece material refers to the workpiece material bonded to the surface of the tool to be detected; the third image is compared with the electron microscope image of the new tool to obtain the third detection result of the tool to be detected; the electron microscope image of the new tool is the image of the new tool just produced from the factory under the second scanning electron microscope; the third detection result is used to indicate the information of the tool wear area of ​​the tool to be detected; the energy spectrum is analyzed to obtain the energy spectrum analysis result; the energy spectrum analysis result is used to indicate the content percentage of each element.

6. A computer device, characterized in that: The computer device comprises a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the tool oxidation wear detection method according to any one of claims 1 to 4.