A screening method and test device for foaming agent for carbon dioxide flooding
By using microfluidic chips to simulate the reservoir structure in a supercritical environment of carbon dioxide, analyzing the fluidity and stability of foam agents, the problems of long-term screening of foam agents, large sample volume and high cost in the prior art are solved, and rapid , economical foam screening and better reservoir simulation.
Patent Information
- Application Number
- CN202410596054.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-14
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-05-14
AI Technical Summary
The existing foam agent screening method for carbon dioxide oil flooding is long, has a large sample volume and is costly, making it difficult to quickly and effectively screen suitable foam agents under different reservoir conditions.
Microfluidic chips are used to simulate the porous structure of the reservoir reservoir. In the supercritical environment of carbon dioxide, the fluidity and stability of the foam agent are quickly evaluated by analyzing the foam quantity, pressure difference, half-life and mobility reduction factors, shortening the test time and reducing the Sample volume, reduce costs.
The foaming agent screening time is significantly shortened, the sample volume is reduced, the test cost is reduced, and the reservoir structure can be better simulated, and foam stability analysis at the pore scale is carried out, which improves screening efficiency and representativeness.
Smart Images

Figure CN118465186B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oilfield exploitation, and in particular to a screening method and a test device for a foaming agent used for carbon dioxide oil recovery. Background Art
[0002] CO 2 Oil flooding is an oil recovery technology that improves oil fluidity and increases oil recovery by injecting carbon dioxide foam. 2 The viscosity and density are low, and it is easy to bypass potential oil resources. When applied to reservoirs composed of different permeabilities, the above defects are more obvious. 2 It will preferentially flow through areas of higher permeability and bypass areas of lower permeability.
[0003] To alleviate the above problems, technicians in this field add foaming agents to the water phase of the porous rock structure of the reservoir to react with the injected CO 2 Formation of CO 2 Foam, this method can effectively increase its viscosity and reduce the overall CO 2 Since different reservoirs have different mineralogy, depth, temperature, water salinity and other characteristics, different CO2-based 2 Foaming agent. Screening for efficient foaming agents is a very expensive process that requires a large number of tests under the conditions of reservoir pressure and temperature and other parameter variables. The traditional method is to use core displacement and foam rheometer tests for screening, which usually takes days or even weeks and requires a large number of fluid samples, resulting in high test costs. Summary of the invention
[0004] In view of the technical problems of the existing carbon dioxide oil recovery foaming agent screening method, such as long time consumption, large sample amount and high cost, the present invention provides a carbon dioxide oil recovery foaming agent screening method and test device, which utilizes the small sample amount required by microfluidic chips to simulate the porous structure in the reservoir, and visualizes the entire test process, so as to quickly evaluate the CO generated by different foaming agents. 2 The foam fluidity and stability greatly shortened the entire test time.
[0005] In a first aspect, the present invention provides a method for screening a foaming agent for carbon dioxide oil recovery, comprising the following steps:
[0006] The microfluidic chip was placed in a supercritical carbon dioxide environment. A porous medium area simulating the porous structure of the reservoir was set in the microfluidic chip. Foaming agent and CO were injected into the microfluidic chip. 2 , foaming agent and CO 2 The mixing produces supercritical carbon dioxide foam;
[0007] Screening is performed by analyzing the foam quantity, foam pressure difference, foam half-life and / or mobility reduction factor of the foaming agent in the porous medium area, wherein the foam quantity is analyzed visually, the foam pressure difference is measured by the pressure sensor on the chip, the foam half-life is the time it takes for the foam quantity to decrease to half of its initial quantity, and the mobility reduction factor is calculated as follows:
[0008] ,
[0009] Where, MRF represents the mobility reduction factor of the foaming agent;
[0010] Indicates CO 2 The pressure difference of the foam in the microfluidic chip, in MPa, can be measured by the pressure sensor at the entrance of the foaming agent connected to the microfluidic chip. 1 and the pressure P at the outlet of the microfluidic chip 3 , by P 1 -P 3 get;
[0011] Indicates CO 2 The pressure difference in the microfluidic chip, in MPa, can be measured by pressure sensors, respectively, for CO 2 Connect the pressure P at the inlet of the microfluidic chip 2 and the pressure P at the outlet of the microfluidic chip 3 , by P 2 -P 3 get;
[0012] Indicates CO 2 The volume flow rate of the foaming agent injected into the microfluidic chip, in mL / min;
[0013] Indicates CO 2 The volume flow rate injected into the microfluidic chip, in mL / min.
[0014] Furthermore, the carbon dioxide supercritical environment is an environment of 100° C. and 13.8 MPa.
[0015] Furthermore, the microfluidic chip is divided into a mixing zone, a foam generating zone and a porous medium zone. The mixing zone is provided with a foaming agent inlet channel and a CO 2 The foam agent inlet channel is connected to the foam agent container arranged outside the microfluidic chip through a first pipeline, and a syringe pump, a first pressure sensor and a valve are arranged on the first pipeline. 2 The inlet channel is connected to the CO2-containing gas flowmeter outside the microfluidic chip through a second pipeline. 2The gas source, the second pipeline is provided with a high-pressure regulating pump, a second pressure sensor and a valve; the foaming agent inlet channel and the CO 2 The inlet channels are connected with the inlet of the foam generating area after merging. The foam generating area includes several annular channels and a main line channel connecting the annular channels in sequence. The outlet of the foam generating area is connected with the inlet of the porous medium area. The porous medium area is used to simulate the porous structure of the reservoir. The outlet of the porous medium area is connected with the outside of the microfluidic chip through a third pipeline. The third pipeline is provided with a valve and a third pressure sensor.
[0016] Furthermore, more than two foaming agents are screened. A large number of foams in the porous medium zone, a high pressure difference, a long half-life and / or a large mobility reduction factor value indicate a good foaming agent effect; a small number of foams in the porous medium zone, a low pressure difference, a short half-life and / or a small mobility reduction factor value indicate a poor foaming agent effect.
[0017] Further, the specific steps for screening two or more foaming agents are:
[0018] (1) n microfluidic chips were placed in the same supercritical carbon dioxide environment. A porous medium area simulating the porous structure of the reservoir was set in the microfluidic chip. Different foaming agents and CO were injected into the n microfluidic chips. 2 , foaming agent and CO 2 Mixing to produce supercritical carbon dioxide foam, n is the same as the number of foaming agents to be screened;
[0019] (2) visually analyzing the amount of foam in the porous media area of multiple microfluidic chips, and selecting the top m foaming agents in descending order of the amount of foam, where m is an integer less than n;
[0020] (3) measuring and comparing the foam pressure differences of the foaming agents screened in step (2) under different foam quality conditions, and screening out the top x foaming agents and their corresponding foam qualities in descending order of pressure difference, where x is an integer less than or equal to m;
[0021] The foam quality calculation formula is:
[0022] ,
[0023] Wherein, M represents the foam mass, unit is %; and has the same meaning as above;
[0024] (4) measuring the foam half-life of the foaming agents screened in step (3) under the conditions of corresponding foam mass and different concentrations, and screening out the first y foaming agents and their corresponding concentrations in the order of half-life from longest to shortest, where y is an integer less than or equal to x;
[0025] (5) Calculate the mobility reduction factor of the foaming agent screened in step (4) under the conditions of corresponding foam mass and concentration, determine the foaming agent with the largest mobility reduction factor and the corresponding foam mass and concentration, and obtain.
[0026] In a second aspect, the present invention provides a test device for screening foaming agents for carbon dioxide oil recovery, comprising a microfluidic chip, wherein the interior of the microfluidic chip is divided into a mixing zone, a foam generating zone and a porous medium zone, wherein the mixing zone is provided with a foaming agent inlet channel and a CO 2 The foam agent inlet channel is connected to the foam agent container arranged outside the microfluidic chip through a first pipeline, and a syringe pump, a first pressure sensor and a valve are arranged on the first pipeline. 2 The inlet channel is connected to the CO2-containing gas flowmeter outside the microfluidic chip through a second pipeline. 2 The gas source, the second pipeline is provided with a high-pressure regulating pump, a second pressure sensor and a valve; the foaming agent inlet channel and the CO 2 The inlet channels are connected with the inlet of the foam generating area after merging. The foam generating area includes several annular channels and a main line channel connecting the annular channels in sequence. The outlet of the foam generating area is connected with the inlet of the porous medium area. The porous medium area is used to simulate the porous structure of the reservoir. The outlet of the porous medium area is connected with the outside of the microfluidic chip through a third pipeline. The third pipeline is provided with a valve and a third pressure sensor.
[0027] Furthermore, the test device also includes a microscope and a camera installed above the microfluidic chip, the microscope is used to observe the amount of foam inside the microfluidic chip in the screening test, and the camera is used to take time-lapse images of the microfluidic chip in the screening test.
[0028] Furthermore, the foam inlet channel and CO 2 A diverter block is provided at the confluence of the inlet channels, and a diverter block is provided near the inlet of the porous medium area. The diverter block is used to separate the foaming agent and the formed CO 2 The foam diverts the flow and has a buffering effect.
[0029] Furthermore, a grid-like channel is provided in the porous medium region;
[0030] Alternatively, the porous medium area can also be designed and engraved according to the pore structure of the reservoir rock to be analyzed. For example, the internal and external structures of the reservoir rock sample are obtained by micro-CT scanning, and then the pore structure model of the sample is established by computer software (such as avizo, etc.) and converted into editable drawings (such as CAD drawings, etc.), and finally the corresponding structure is engraved on the chip by a laser engraving machine.
[0031] The beneficial effects of the present invention are:
[0032] The method of the present invention can complete the screening in just a few hours, which is shorter than the existing technology that takes several days or weeks; the method of the present invention requires a smaller sample volume, and only a few milliliters of sample can complete the test, while the existing technical solution requires hundreds of milliliters of sample, so the method of the present invention can achieve safer and more cost-effective operation. In addition, technicians can also directly observe the damage mechanism of solid precipitation and deposition to the formation during the test, and analyze the fluid behavior at the pore scale through microscopes, cameras and other equipment.
[0033] The microfluidic-based carbon dioxide flooding foam screening method provided by the present invention has a good effect in the preliminary screening of foaming agents, saving time and cost. Compared with traditional tests, it can also better simulate the reservoir structure and conduct more representative pore-scale foam stability analysis by modifying the pore structure in the porous medium area. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0035] Figure 1 1 is a top view of the microfluidic chip in Example 1.
[0036] Figure 2 It is a schematic diagram of the structure of the test device used for screening foaming agents for carbon dioxide oil recovery in Example 1.
[0037] Figure 3 It is a line graph of the pressure difference of the foams formed by various surfactants under different foam qualities in Example 4.
[0038] Figure 4 It is a line graph of the half-life of foams formed by surfactants of different concentrations at 70% foam mass in Example 3.
[0039] Figure 5 It is a bar chart comparing the MRFs of different surfactants in Example 2.
[0040] Figure 1: microfluidic chip, 2: foaming agent inlet channel, 3: CO 2 Inlet channel, 4-foaming agent container, 5-syringe pump, 6-CO 2Gas source, 7-high pressure regulating pump, 8-foam generating area, 9-first diverter block, 10-annular channel, 11-porous medium area, 12-second diverter block, 13-outlet of porous medium area, 14-back pressure regulator, 15-image observation and acquisition equipment, 16-first pressure sensor, 17-second pressure sensor, 18-third pressure sensor. DETAILED DESCRIPTION
[0041] In order to enable those skilled in the art to better understand the technical solutions in the present invention, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0042] Example 1
[0043] A test device for screening foaming agents for carbon dioxide flooding comprises a microfluidic chip 1, wherein the microfluidic chip 1 is internally divided into a mixing zone, a foam generating zone 8 and a porous medium zone 11, wherein the mixing zone is provided with a foaming agent inlet channel 2 and a CO 2 The inlet channel 3 and the foaming agent inlet channel 2 are connected to the foaming agent container 4 arranged outside the microfluidic chip 1 through the first pipeline, and the first pipeline is provided with a syringe pump 5, a first pressure sensor 16 and a valve; CO 2 The inlet channel 3 is connected to the CO2-containing gas outlet outside the microfluidic chip 1 through a second pipeline. 2 Gas source 6, a high pressure regulating pump 7, a second pressure sensor 17 and a valve are arranged on the second pipeline;
[0044] Foam agent inlet channel 2 and CO 2 The inlet channel 3 is connected to the inlet of the foam generating area 8 after merging, and the foaming agent inlet channel 2 and CO 2 A plurality of first flow dividing blocks 9 are arranged at the confluence of the inlet channels 3, and the foam generating area 8 includes a plurality of annular channels 10 and a main line channel connecting the annular channels 10 in sequence;
[0045] The outlet of the foam generating zone is connected to the inlet of the porous medium zone 11. A grid-like channel is arranged in the porous medium zone 11 to simulate the porous structure of the reservoir. A plurality of second flow dividing blocks 12 are arranged near the inlet of the porous medium zone 11. The outlet 13 of the porous medium zone is connected to the back pressure regulator 14 outside the microfluidic chip 1 through a third pipeline. A valve and a third pressure sensor 18 are arranged on the third pipeline.
[0046] The first pressure sensor 16, the second pressure sensor 17, and the third pressure sensor 18 are all of the Omega Engineering PX409-3.5KGUSBH type. The first pressure sensor 16 is used to measure the pressure of the first pipeline, that is, the pressure P at the inlet of the foaming agent connected to the microfluidic chip 1. 1 The second pressure sensor 17 is used to measure the pressure P of the second pipeline 2 , i.e. CO 2 The third pressure sensor 18 is used to measure the pressure P of the third pipeline. 3 , i.e., the pressure at the outlet of the microfluidic chip 1;
[0047] The test device also includes an image observation and acquisition device 15 installed above the microfluidic chip 1. The image observation and acquisition device 15 includes a microscope and a camera. The microscope is used to observe the foam inside the microfluidic chip 1 during the screening test, and the camera is used to take a time-lapse image of the foam changes inside the microfluidic chip during the screening test.
[0048] Example 2
[0049] On the basis of Example 1, in the test device for screening foaming agents for carbon dioxide oil recovery, the porous medium area of the microfluidic chip can also be designed and engraved according to the pore structure of the reservoir rock to be analyzed. For example, the internal and external structures of the reservoir rock sample are obtained by micro-CT scanning, and then the pore structure model of the sample is established by computer software (such as avizo, etc.) and converted into an editable drawing (such as CAD drawing, etc.), and finally the corresponding structure is engraved on the chip by a laser engraving machine.
[0050] Example 3
[0051] A method for screening a foaming agent for carbon dioxide oil recovery using the test device of Example 1 or Example 2, firstly placing a microfluidic chip in a carbon dioxide supercritical environment (100°C, 13.8Mpa), injecting a foaming agent and CO into the microfluidic chip 2 , foaming agent and CO 2 The mixing produces supercritical carbon dioxide foam;
[0052] Then, choose one of the following four aspects to judge the effect of the foaming agent, or choose several of them to comprehensively evaluate the effect of the foaming agent.
[0053] (1) Foam quantity
[0054] When comparing two or more foaming agents, observe the amount of foam in the porous medium area. A large amount of foam indicates that the foaming agent is relatively more effective, while a small amount of foam indicates that the foaming agent is relatively less effective.
[0055] (2) Foam pressure difference
[0056] Smaller bubble size, i.e., higher bubble density, can increase gas viscosity, form a higher pressure difference, and reduce CO 2 Fluidity, therefore the performance of the foaming agent can be judged by measuring the foam pressure difference.
[0057] The foam pressure difference is measured by measuring CO 2 The pressure change of the foam in the microfluidic chip is recorded by recording the pressure value P at the inlet of the microfluidic chip connected to the foam agent. 1 and the pressure value P at the outlet of the microfluidic chip 3 , then according to the formula =P 1 -P 3 To calculate CO 2 The pressure difference of the foam in the microfluidic chip should be continuously recorded for analysis during the experiment.
[0058] When comparing two or more foamers, a high pressure differential indicates a relatively more effective foamer, and a low pressure differential indicates a relatively less effective foamer.
[0059] (3) Bubble Half-Life
[0060] Traditional tests for measuring foam stability are conducted in vertical columns, and the foam decay rate is evaluated by measuring the foam height, but it cannot reflect the foam decay changes under different pore conditions in actual reservoir rocks. This method can simulate the pore size in actual rocks through the porous medium area of the microfluidic chip and use cameras and microscopes to visualize the entire test process. The number of foam layers and the foam half-life (i.e. the time it takes for the amount of foam to decrease to half of its initial amount) are analyzed by taking time-lapse images of the microfluidic chip.
[0061] When comparing two or more foaming agents, a longer foam half-life indicates a relatively more effective foaming agent, and a shorter foam half-life indicates a relatively less effective foaming agent.
[0062] (4) Foaming agent mobility reduction factor
[0063] When comparing two or more foaming agents, calculate the mobility reduction factor of the foaming agent and use the mobility reduction factor to quantify the CO 2 The flow resistance and mobility reduction factor are calculated as follows:
[0064] ,
[0065] Where, MRF represents the mobility reduction factor of the foaming agent;
[0066] Indicates CO 2The pressure difference of the foam in the microfluidic chip, in MPa, =P 1 -P 3 , P 1 is the pressure value at the inlet of the foaming agent connected to the microfluidic chip, P 3 is the pressure value at the outlet of the microfluidic chip;
[0067] Indicates CO 2 The pressure difference in the microfluidic chip, in MPa, =P 2 -P 3 , P 2 For CO 2 The pressure value at the inlet of the microfluidic chip, P 3 is the pressure value at the outlet of the microfluidic chip;
[0068] Indicates CO 2 The volume flow rate of the foaming agent injected into the microfluidic chip, in mL / min;
[0069] Indicates CO 2 The volume flow rate injected into the microfluidic chip, in mL / min.
[0070] A large foam mobility reduction factor value indicates that the foaming agent is relatively effective, and a small foam mobility reduction factor value indicates that the foaming agent is relatively ineffective.
[0071] Example 4
[0072] Ten surfactants commonly used in laboratories, including polyethylene glycol PEG, polyvinyl alcohol PVA, alkyl polysaccharide APG, perfluorooctanoic acid PFOA, perfluorooctane sulfonate PFOS, sodium dodecyl sulfate SDS, sodium dodecyl ether sulfate SLES, octanol polyoxyethylene ether OEO, sodium dodecylbenzene sulfonate SDBS, and sodium octylbenzene sulfonate OBS, were selected as screening objects to analyze and compare the foam size, pressure difference, half-life and its mobility reduction factor to determine the most suitable surfactant as a carbon dioxide oil recovery foam agent.
[0073] The structure of the experimental device used is the same as that of Example 1, wherein the annular channel in the foam generating zone has a depth of 10 μm, an outer diameter of 1.2 mm, and an inner diameter of 0.7 mm, and the main line channel has a depth of 10 μm and a width of 300 μm; the grid-like channel in the porous medium zone is formed by staggered transverse channels and vertical channels, and the size of the pore formed by the intersection of a transverse channel and a vertical channel is 20 μm (width) × 20 μm (depth); the injection pump model for injecting the foaming agent is Chemyx Fusion 6000, which is used to inject CO 2The high-pressure regulating pump model for adjusting the outlet pressure of the microfluidic chip is Teledyne ISCO 260D.
[0074] The specific screening steps are as follows:
[0075] Step 1: Combine surfactant and CO 2 The CO was injected into the microfluidic chip through the inlet at a constant flow rate, and the test environment was adjusted to 100°C and 13.8MPa. 2 The supercritical state was maintained and the amount of foam generated at the entrance of the porous medium zone by different surfactant formulations was observed under an optical microscope. The observed foam amounts were in the following order: OBS>SLES>SDS>APG>SDBS>PEG>PVA>PFOA>OEO>PFOS. The top five surfactants with the best foam amounts, OBS, SLES, SDS, APG and SDBS, were screened for subsequent experiments.
[0076] Step 2: Under the conditions of foam quality of 30%, 50%, 60%, 70%, 80%, 90% and 95%, measure the pressure difference of the foam formed by each surfactant, and screen out the surfactant solution that produces the largest pressure difference.
[0077] The foam quality calculation formula is:
[0078] ,
[0079] Wherein, M represents the foam mass, unit is %;
[0080] Indicates CO 2 The volume flow rate of the foaming agent injected into the microfluidic chip, in mL / min;
[0081] Indicates CO 2 The volume flow rate injected into the microfluidic chip, in mL / min;
[0082] The results are as follows Figure 3 As shown in the figure, when the foam quality is 70%, the pressure difference generated by SLES and OBS is relatively high, that is, the foam performance is better. When the foam quality is greater than 80%, the foam pressure difference of all surfactants is significantly reduced, which will lead to CO 2 The fluidity of the aqueous phase increased, indicating that the ability of the surfactant to form stable strong foam under this condition was poor. Therefore, the two surfactants SLES and OBS with better foam stability were selected for the next screening, and the optimal foam quality corresponding to the two surfactants was determined to be 70%.
[0083] Step 3: Under the condition of 70% foam mass, the half-life of the foam generated by different concentrations of SLES and OBS surfactants was measured to determine the optimal concentration of the corresponding surfactant.
[0084] Depend on Figure 4 It can be seen that when the concentration of SLES is 0.4wt%, the half-life time exceeds 300min, while when the concentration of OBS is 0.5wt%, the half-life time is the longest, and the effects are both good. Therefore, 0.4wt% SLES and 0.5wt% OBS were selected for subsequent screening.
[0085] Step 4: Calculate the mobility reduction factor MRF of the two surfactants at the optimal foam quality and concentration, given by Figure 5 It can be seen that the result of MRF is SLES>OBS.
[0086] Through the above four stages of experiments, it can be concluded that SLES surfactant with a foam mass of 70% and a concentration of 0.4wt% can produce a more stable and better performing supercritical CO 2 Foam.
[0087] To ensure that the initial conditions were the same for all experiments, a new microfluidic chip was used for each experiment.
[0088] Although the present invention has been described in detail with reference to the accompanying drawings and in combination with the preferred embodiments, the present invention is not limited thereto. Without departing from the spirit and essence of the present invention, a person of ordinary skill in the art may make various equivalent modifications or substitutions to the embodiments of the present invention, and these modifications or substitutions shall be within the scope of the present invention. Any person of ordinary skill in the art may easily think of changes or substitutions within the technical scope disclosed by the present invention, and these shall be within the scope of protection of the present invention.
Claims
1. A method for screening a foaming agent for carbon dioxide flooding, It is characterized in that Screening two or more foaming agents, a large number of foams in the porous medium area, a high pressure difference, a long half-life and / or a large mobility reduction factor value indicates a good foaming agent effect; a small number of foams in the porous medium area, a low pressure difference, a short half-life and / or a small mobility reduction factor value indicates a poor foaming agent effect; The specific steps are: (1) Place n microfluidic chips in the same supercritical carbon dioxide environment and inject different foaming agents and CO into the n microfluidic chips. 2 , foaming agent and CO 2 Mixing to produce supercritical carbon dioxide foam, n is the same as the number of foaming agents to be screened; The microfluidic chip is divided into a mixing zone, a foam generation zone, and a porous medium zone simulating the porous structure of the reservoir. The mixing zone is equipped with a foaming agent inlet channel and a CO 2 The foam agent inlet channel is connected to the foam agent container arranged outside the microfluidic chip through a first pipeline, and a syringe pump, a first pressure sensor and a valve are arranged on the first pipeline. 2 The inlet channel is connected to the CO2-containing gas flowmeter outside the microfluidic chip through a second pipeline. 2 The gas source, the second pipeline is provided with a high-pressure regulating pump, a second pressure sensor and a valve; the foaming agent inlet channel and the CO 2 The inlet channels are connected with the inlet of the foam generating area after merging, the foam generating area includes a plurality of annular channels and a main line channel connecting the annular channels in sequence, the outlet of the foam generating area is connected with the inlet of the porous medium area, the porous medium area is used to simulate the porous structure of the reservoir, the outlet of the porous medium area is connected with the outside of the microfluidic chip through a third pipeline, and a valve and a third pressure sensor are arranged on the third pipeline; (2) visually analyzing the amount of foam in the porous media area of multiple microfluidic chips, and selecting the top m foaming agents in descending order of the amount of foam, where m is an integer less than n; (3) measuring and comparing the foam pressure differences of the foaming agents screened in step (2) under different foam quality conditions, wherein the foam pressure difference is measured by a pressure sensor on the chip, and the top x foaming agents and their corresponding foam qualities are screened out in descending order of pressure difference, where x is an integer less than or equal to m; The foam quality calculation formula is: , Wherein, M represents the foam mass, unit is %; Indicates CO 2 The volume flow rate of the foaming agent injected into the microfluidic chip, in mL / min; Indicates CO 2 The volume flow rate injected into the microfluidic chip, in mL / min; (4) measuring the foam half-life of the foaming agents screened in step (3) under the conditions of corresponding foam mass and different concentrations. The foam half-life is the time it takes for the amount of foam to decrease to half of its initial amount. The first y foaming agents and their corresponding concentrations are screened in descending order of half-life, where y is an integer less than or equal to x; (5) Calculate the mobility reduction factor of the foaming agent screened in step (4) under the corresponding foam mass and concentration conditions, determine the foaming agent with the largest mobility reduction factor and the corresponding foam mass and concentration, and obtain; The calculation formula of mobility reduction factor is: , Where, MRF represents the mobility reduction factor of the foaming agent; Indicates CO 2 The pressure difference of the foam in the microfluidic chip, in MPa; Indicates CO 2 The pressure difference in the microfluidic chip, in MPa; Indicates CO 2 The volume flow rate of the foaming agent injected into the microfluidic chip, in mL / min; Indicates CO 2 The volume flow rate injected into the microfluidic chip, in mL / min.
2. The screening method according to claim 1, It is characterized in that The supercritical environment of carbon dioxide is 100°C and 13.8Mpa.
3. The screening method according to claim 1, It is characterized in that It also includes a microscope and camera mounted above the microfluidic chip.
4. The screening method according to claim 1, It is characterized in that The foaming agent inlet channel is connected to the foaming agent container arranged outside the microfluidic chip through a pipeline, and a syringe pump, a pressure sensor and a valve are arranged on the pipeline; CO 2 The inlet channel is connected to the CO2-containing gas flowmeter outside the microfluidic chip through a pipeline. 2 Gas source, with injection pump, pressure sensor and valve on the pipeline.
5. The screening method according to claim 1, It is characterized in that Foam inlet channel and CO 2 A flow dividing block is arranged at the confluence of the inlet channels, and a flow dividing block is arranged near the inlet of the porous medium area.
6. The screening method according to claim 1, It is characterized in that A grid-like channel is arranged in the porous medium area; Alternatively, the porous media zone is designed and carved according to the pore structure of the reservoir rock to be analyzed.
Citation Information
Patent Citations
Foam flooding micro-nano chemical chip device and method
CN116087097A
Micro-fluidic chip for research on oil-water seepage mechanism of carbonate reservoir and manufacturing method of micro-fluidic chip
CN116920971A
Enhanced oil recovery with janus nanoparticles
WO2022020719A1