Additive manufacturing method for thrust chamber body containing variable-dip-angle spiral regenerative cooling channel
By performing macroscopic scaling design and process compensation on the three-dimensional model of the thrust chamber body, optimizing laser scanning parameters, and combining with temperature control preheating, the accuracy problem of the variable-inclination spiral regeneration cooling channel of the thrust chamber body was solved, and high precision was achieved Shaping meets the requirements for precision transportation and efficient cooling of propellant.
Patent Information
- Application Number
- CN202410860330.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-01
AI Technical Summary
The existing technology has problems in manufacturing the variable-inclination spiral regeneration cooling channel in the thrust chamber body. The dimensional accuracy and shape accuracy caused by uneven stress, structural shrinkage, and deformation cannot meet the requirements for precise propellant transportation and efficient cooling.
By establishing a three-dimensional model of the thrust chamber body, determining the growth direction, carrying out macro scaling design, anti-deformation process design, process compensation for structural mutation areas, optimizing laser type, scanning strategy and scanning parameters, combined with temperature control preheating, to achieve high precision taking shape.
It improves the forming accuracy and dimensional accuracy of the thrust chamber body, solves the accuracy problem of the variable inclination spiral regeneration cooling channel of the thrust chamber body in additive manufacturing, and meets the development needs of high-performance thrust chambers.
Smart Images

Figure CN118720165A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of additive manufacturing, and in particular relates to an additive manufacturing method for a thrust chamber body including a variable-inclination spiral regenerative cooling channel. Background Art
[0002] The thrust chamber body is the core component of aerospace liquid rocket engines. Its function is to convert the chemical energy of liquid propellant into jet kinetic energy and generate thrust. During the operation of the thrust chamber body, it is accompanied by the erosion and ablation of high-temperature, high-pressure and high-speed combustion gases. The maximum combustion gas temperature can reach 3500K and the heat flux density can reach 160MW / m 2 , far exceeding the temperature limit that metal materials can withstand at present. In order to prevent the thrust chamber from overheating, oxidation corrosion, and erosion, efficient cooling must be achieved through a variable-angle spiral regenerative cooling channel. At present, the thrust chamber body is usually manufactured by machining a split forging blank and then brazing it. There are problems such as poor performance stability, low pass rate, and long processing cycle, which makes it difficult to meet the overall manufacturing needs of a high-performance, complex variable-angle spiral regenerative cooling channel thrust chamber.
[0003] Laser additive manufacturing technology is not limited by product structure and can realize integrated manufacturing of complex products. It has significant advantages in improving product quality, reducing production costs, and shortening production cycles. It has become the preferred solution for the overall manufacturing of such complex regenerative cooling channel components. However, the regenerative cooling channel of the thrust chamber body is responsible for the precise fuel delivery and efficient cooling functions, and the accuracy requirements of the channel are extremely high (tolerance requirement: ≤±0.05mm). At present, the laser additive manufacturing of the high aspect ratio thrust chamber body has problems such as inconsistent thrust line shrinkage along the height direction, deformation edges at structural mutations, warping deformation during the forming process of the small inclination channel, and uneven stress. As a result, the dimensional accuracy of the variable inclination spiral regenerative cooling channel is poor, with a deviation of ≥0.2mm, which cannot meet the use requirements. It is urgent to break through the precision control technology of the variable inclination spiral regenerative cooling channel of the thrust chamber body in additive manufacturing. Summary of the invention
[0004] The purpose of the present invention is to overcome the above-mentioned defects and provide an additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel, which solves the technical problem that the channel size accuracy / shape accuracy caused by the uneven stress / structural shrinkage and deformation of the current additively manufactured thrust chamber body cannot meet the requirements of precise propellant delivery and efficient cooling. The present invention can effectively improve the forming accuracy and dimensional accuracy of the thrust chamber body, and has important guiding and application significance for the development of high-performance thrust chambers.
[0005] In order to achieve the above-mentioned object of the invention, the present invention provides the following technical solutions:
[0006] An additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel, comprising:
[0007] S1 establishes a three-dimensional model of the thrust chamber body;
[0008] S2 determines the growth direction of the thrust chamber body based on the principle of minimum stress, least support and removable support;
[0009] S3 obtains a macroscopically scaled three-dimensional model of the thrust chamber body according to the three-dimensional model and growth direction of the thrust chamber body;
[0010] S4 obtains the three-dimensional model of anti-deformation process design based on the macro-scaled three-dimensional model of the thrust chamber body;
[0011] S5 designs a three-dimensional model based on the anti-deformation process and performs process compensation in the model mutation area;
[0012] S6 optimizes the laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel;
[0013] S7 designs the process support and process powder cleaning port based on the model after process compensation to obtain the process 3D model of the thrust chamber body;
[0014] S8 uses the process 3D model of the thrust chamber body and the optimized laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel to complete the additive manufacturing of the thrust chamber body.
[0015] Furthermore, in step S2, the growth direction of the thrust chamber body is determined as:
[0016] The large end flange of the thrust chamber body is connected to the base plate, and the normal line of the thrust chamber body is perpendicular to the forming platform.
[0017] Furthermore, in step S3, according to the three-dimensional model and growth direction of the thrust chamber body, a method for obtaining a macro-scaled three-dimensional model of the thrust chamber body includes:
[0018] On the three-dimensional model of the thrust chamber body, local models of the cylindrical section, the contraction-expansion section, the throat section, and the expansion section are respectively cut out, and the height of the local model is 15 to 25 mm;
[0019] Set multiple groups of scaling ratios, scale each local model in three dimensions of X, Y, and Z, and obtain multiple groups of scaled local models; wherein the Z direction is the axial direction of the thrust chamber body, and the XY plane is perpendicular to the Z direction;
[0020] According to the scaled local model, the laser additive manufacturing process is used to prepare local test pieces of the cylindrical section, the contraction and expansion section, the throat, and the expansion section. The scaling ratio corresponding to the local test piece with the smallest diameter size deviation is taken as the optimal scaling ratio. The three-dimensional model of the thrust chamber body is scaled according to the optimal scaling ratio to obtain a macro-scaled three-dimensional model of the thrust chamber body.
[0021] Further, in step S3, the three-dimensional model of the thrust chamber body is scaled according to the scaling ratios of 1.004%, 1.004% and 1.001% in the X, Y and Z dimensions respectively, to obtain a macro-scaled three-dimensional model of the thrust chamber body; wherein the Z direction is the axial direction of the thrust chamber body, and the XY plane is perpendicular to the Z direction.
[0022] Furthermore, in step S4, the thrust line diameter d of the inverse deformation process design three-dimensional model and the thrust line diameter d0 of the macro-scaled three-dimensional model satisfy the following relationship:
[0023]
[0024] Wherein, H is the forming height.
[0025] Further, in step S5, the model mutation region includes the cylindrical section, the contraction-expansion section, and the region where the outer wall of the expansion section is connected to other components;
[0026] The method for performing process compensation in a model mutation area includes: adding a process compensation slice outside the mutation area of the reverse deformation process design three-dimensional model, and the process compensation slice smoothly transitions to the outer wall of the original reverse deformation process design three-dimensional model by chamfering and rounding.
[0027] Furthermore, the process compensation slice is annular, with a thickness of 0.2 to 0.3 mm and a width of 20 to 30 mm;
[0028] When the process compensation slice is smoothly transitioned to the outer wall of the original anti-deformation process design three-dimensional model by chamfering and rounding, the process compensation slice is first chamfered to ensure the maximum uniform transition, and then, on the basis of the chamfer, a large rounded corner of 50 to 100 mm is chamfered at the junction of the chamfer and the outer wall;
[0029] The bevel angle is an asymmetrical inclination angle.
[0030] Furthermore, in step S6, the optimization of the laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel includes:
[0031] The laser type of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel adopts flat-top laser.
[0032] The scanning strategy of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel includes: using the outer contour of the overhang feature as a reference to perform offset scanning path planning, and scanning from the core part close to the solid to the border part close to the powder in sequence;
[0033] The scanning parameters of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel include: a high scanning speed of 2000mm / s to 2600mm / s, a low laser power of 120w to 140w, and a wide scanning spacing of 0.11mm to 0.14mm.
[0034] Furthermore, the scanning parameters of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel of the contraction-expansion section, cylindrical section and expansion section are as follows:
[0035] The parameters of the lower surface of the spiral groove with an inclination angle of 35 to 45° in the expansion section are as follows: laser power 120w, scanning speed 2600mm / s, scanning spacing: 0.14mm;
[0036] Parameters of the lower epidermis of the spiral groove with an inclination angle of 45° in the cylindrical section: laser power 130w, scanning speed 2300mm / s, scanning spacing: 0.13mm;
[0037] The expansion section has an inclination angle of 45 to 60° and the lower surface parameters of the spiral groove are: laser power 140w, scanning speed 2000mm / s, scanning spacing: 0.11mm.
[0038] Further, in step S8, during the additive manufacturing process of the thrust chamber body, the temperature of the powder bed is controlled by using the temperature of the circulating airflow, and the temperature range is controlled to be 200-500° C. The specific method includes installing the PTC gas heating device at the circulating gas outlet position of the circulating system of the additive manufacturing equipment;
[0039] After the additive manufacturing of the thrust chamber body, the resulting workpiece is subjected to powder cleaning, heat treatment and stress relief processes, and wire cutting;
[0040] The heat treatment stress relief process is carried out by vacuum heat treatment, the temperature is 600-700℃, and the time is 6-8h;
[0041] Wire cutting adopts rectangular pulse wave, pulse width: 30 ~ 45μs, pulse interval: 200 ~ 220μs, current: 3 ~ 5A.
[0042] Compared with the prior art, the present invention has at least one of the following beneficial effects:
[0043] (1) The present invention comprehensively considers the influence of factors such as structural shrinkage and deformation during additive manufacturing on the forming accuracy of the thrust chamber body, and innovatively implements five control measures, namely, macro-scaling, thrust line anti-deformation process design, structural mutation area process compensation design, different inclination angle differentiated lower skin scanning strategy and process parameter control, and forming process temperature control preheating stress reduction, to achieve high-precision forming of the thrust chamber body with variable inclination angle spiral regenerative cooling channel;
[0044] (2) The present invention determines the optimal macro-scaling ratio of the thrust chamber body in the three dimensions of X, Y, and Z through the method of stress-strain simulation-process test iteration, establishes a thrust line anti-deformation process design calculation formula based on diameter and growth height, and obtains a method for controlling the dimensional uniformity and dimensional accuracy of the thrust chamber body with high aspect ratio through macro-scaling and thrust line anti-deformation process design, thereby solving the bottleneck problem of inconsistent shrinkage rules of additive manufacturing products in the height direction;
[0045] (3) The present invention designs a process compensation slice in the structural mutation area of the body three-dimensional model, and performs a combined smoothing process of "chamfering + rounding", thereby eliminating the step between the process compensation slice and the original model, compensating for the local shrinkage and dislocation edge of the thin wall of the body flow channel, and ensuring the flow channel size accuracy in the cross-sectional breakthrough area;
[0046] (4) The present invention separates the overhanging area of the lower surface of the flow channel by comparing the adjacent layers of the variable-angle spiral channel structure, and optimizes the laser energy distribution. It innovatively uses a flat-top laser to replace the energy Gaussian distribution laser, and utilizes the uniform energy density distribution characteristics of the flat-top laser to effectively suppress the collapse of the molten pool and control the shape and dimensional accuracy of the flow channel;
[0047] (5) The present invention adopts an offset profile scanning strategy of approaching the core first and then the frame, and provides high scanning speed, low laser power and wide scanning spacing to improve the uneven temperature gradient in the scanning layer caused by the difference in thermal conductivity between the powder and the solid, and control the warping deformation of the lower skin and the collapse of the molten pool; at the same time, for different inclination angles, a gradual lower skin process parameter is adopted to control the flow channel accuracy and realize high-precision forming of a variable inclination angle spiral channel structure;
[0048] (6) The present invention preheats the powder bed temperature by heating the circulating air flow temperature, so that the temperature of the forming chamber during the forming process is stabilized in a reasonable temperature range, reducing temperature difference stress and preventing body stress deformation. BRIEF DESCRIPTION OF THE DRAWINGS
[0049] Figure 1 This is a schematic diagram of the three-dimensional design structure of the thrust chamber body manufactured by additive manufacturing according to the present invention;
[0050] Figure 2 It is a schematic diagram of the characteristic area of the thrust chamber body structure mutation;
[0051] Figure 3 Schematic diagram of the original process compensation slice of the present invention; wherein (a) is a full circle slice; (b) is the slice cut wall thickness;
[0052] Figure 4 Schematic diagram of the process compensation slice after the "chamfer + rounded corner" smoothing of the present invention; wherein (a) is a full circle slice; (b) is the slice cut wall thickness;
[0053] Figure 5 It is a schematic cross-sectional view of two adjacent layers of the tilt structure of the present invention;
[0054] Figure 6 Schematic diagram of the scanning strategy for overhanging features of the present invention. DETAILED DESCRIPTION
[0055] The following detailed description of the present invention will make the features and advantages of the present invention more clear and explicit.
[0056] The word "exemplary" is used exclusively herein to mean "serving as an example, embodiment, or illustration." Any embodiment described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments. Although various aspects of the embodiments are shown in the drawings, the drawings are not necessarily drawn to scale unless otherwise noted.
[0057] An additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel comprises the following steps:
[0058] (1) Establish an integrated three-dimensional model of the thrust chamber body with a variable-angle spiral regenerative cooling channel based on additive manufacturing.
[0059] (2) Based on the stress distribution and support configuration of the integrated model obtained in step (1) during the forming process, the growth direction of the thrust chamber body is determined based on the principle of minimum stress, minimum support and removable support.
[0060] (3) According to the size, structure and growth direction of the three-dimensional model of the thrust chamber body, the macro-scaling coefficients of the three dimensions of X, Y and Z of the entire thrust chamber body are obtained through typical structural process tests, and the macro-scaled three-dimensional model of the thrust chamber body is obtained after adjustment according to the coefficients.
[0061] (4) Based on the macroscopic scaling three-dimensional model of the thrust chamber body, the dimensional deformation law of the thrust line of the high aspect ratio thrust chamber body in the height direction is obtained through the stress-strain simulation-process test iteration method, and the thrust line anti-deformation process design calculation formula based on diameter and growth height is established to obtain the anti-deformation process design three-dimensional model.
[0062] (5) The structural mutation characteristics of the thrust chamber body of the thin-walled regenerative cooling channel are extracted, and process compensation is designed in the structural mutation area of the body three-dimensional model to eliminate the shrinkage dislocation edges and ensure the dimensional accuracy of the flow channel in the cross-sectional breakthrough area.
[0063] (6) The variable-angle spiral regenerative cooling channel in the thrust chamber body model is extracted, and the shape accuracy and dimensional accuracy of the variable-angle spiral channel structure are optimized. By regulating the laser energy distribution, energy density, and scanning strategy, high-precision additive manufacturing of the spiral channel of the thrust chamber body is achieved.
[0064] (7) Based on the three-dimensional model determined in step (5) and the growth direction determined in step (2), the process support and the process powder cleaning port are designed to obtain the process three-dimensional model of the thrust chamber body.
[0065] (8) Using the process parameters and methods obtained in step (6), the process three-dimensional model obtained in step (7) is segmented and processed to obtain a program file containing the body structure feature slice section information and the laser scanning path and parameters of each slice section.
[0066] (9) Turn on the temperature control function of the additive manufacturing forming room to reduce the temperature difference stress during the forming process and prevent stress deformation of the body.
[0067] (10) Call the thrust chamber body program file and perform forming in the additive manufacturing equipment.
[0068] (11) The metal powder in the spiral channel of the thrust chamber body obtained in step (9) is removed, and after heat treatment to eliminate stress, the substrate and the product are separated by wire cutting. After removing the process support by grinding, a high-precision thrust chamber body product is obtained.
[0069] In step (1), the overall structure of the thrust chamber body manufactured by additive manufacturing is a double bell-shaped structure, including
[0070] The cylindrical section, the contraction and expansion section, the throat and the expansion section, in a specific embodiment, the large end diameter is 620mm, the small end diameter is 280mm, the throat diameter is 98mm, the total height is 660mm, and it contains three sections of variable inclination spiral regeneration cooling channels, the number of channels is 180, among which the cylindrical section spiral groove inclination angle is 45°, the groove width is 1.2mm, the groove depth is 1.8mm, the contraction and expansion section spiral groove inclination angle is 35-45°, the minimum groove width is 1mm, the groove depth is 1.4mm, the expansion section spiral groove inclination angle is 45-60°, the groove width is 1.6mm, the groove depth is 2.5mm, the wall thickness is 0.6mm, see Figure 1 .
[0071] In step (2), based on the stress distribution and support configuration during the forming process, the growth direction of the thrust chamber body is determined based on the principle of minimum stress, minimum support and removable support: the large end flange is connected to the base plate, and its normal is perpendicular to the forming platform.
[0072] In step (3), the whole circumference local component model of the small end of the cylindrical section, the throat of the expansion section, and the large end of the expansion section is cut out on the three-dimensional design model of the thrust chamber body, wherein the diameter of the small end of the cylindrical section is 280 mm, the diameter of the throat of the expansion section is 98 mm, the diameter of the large end of the expansion section is 620 mm, and the height of the local component is 20 mm. After obtaining the local component model, a laser additive manufacturing process test is carried out, and a macroscopic scaling study is conducted on it in the three dimensions of X, Y, and Z. Five groups of scaling ratios are set, which are (1.002, 1.002, 1.001)%, (1.003, 1.003, 1.001)%, (1.004, 1.004, 1.001)%, and (1.005, 1.005, 1.001)%. When the scaling ratios in the three directions of X, Y, and Z are (1.004, 1.004, 1.001)%, the diameter size of the test piece is consistent with that in the test piece. Figure 1 The deviation of the three-dimensional design model is the smallest, within 0.1mm, meeting the design requirements. Based on this, (1.004, 1.004, 1.001)% is determined as the macro-scaling ratio of the thrust chamber body. After scaling the three-dimensional model obtained in step (1) according to this ratio, the macro-scaling three-dimensional model of the thrust chamber body is obtained.
[0073] In step (4), the forming process of the additive manufacturing product is layer-by-layer forming, and its initial growth point is the substrate. In the area close to the substrate, the substrate has a large constraint on the product and its shrinkage is small. As the forming height increases, the constraint gradually decreases and the shrinkage gradually increases, resulting in inconsistent shrinkage rules in the height direction of the product. The farther away from the substrate, the larger the shrinkage size. This phenomenon is more obvious for the thrust chamber body with a high aspect ratio. To solve this problem, an anti-shrinkage deformation process design is carried out based on the macroscopic scaling three-dimensional model of the thrust chamber body to compensate for the shrinkage at different heights.
[0074] The anti-shrinkage deformation process design mainly includes three steps: the first step is to calculate the strain value of the thrust chamber body in the forming height direction through the Simufact simulation software, and add the strain values of different heights obtained by simulation to the three-dimensional model of the body to obtain the initial three-dimensional model of the thrust chamber body anti-shrinkage deformation; the second step is to cut one-eighth of the body model on the model, perform additive manufacturing to obtain the test piece, and perform three-dimensional scanning surface comparison measurement to obtain the deviation value between the contour size of the test piece and the theoretical requirement, and add the deviation value to the anti-shrinkage deformation three-dimensional model obtained in the first step, correct the simulation error, and obtain the final thrust chamber body anti-shrinkage deformation three-dimensional model. The third step is to statistically analyze the anti-shrinkage deformation of the thrust chamber body at different heights, obtain the dimensional deformation law of the thrust line of the thrust chamber body in the growth direction, and establish the thrust line anti-deformation process design calculation formula based on diameter and growth height:
[0075]
[0076] Where d is the thrust line diameter of the thrust chamber body after compensation, d0 is the initial thrust line diameter of the thrust chamber body, and H is the forming height.
[0077] In step (5), the structural mutation characteristics of the thrust chamber body of the thin-wall regenerative cooling channel are extracted, see Figure 2 , design process compensation slices with a thickness of 0.2-0.3mm and a width of 20-30mm in the structural mutation area of the three-dimensional model of the body, see Figure 3 , and sum it with the original model. On the three-dimensional model, a combination of "chamfer + rounding" is used to perform smooth processing to eliminate the steps between the process compensation slice and the original model. The "chamfer + rounding" method, in which the bevel angle is an asymmetric inclination angle, the distance 1 is the thickness of the compensation slice, and the distance 2 is 50 to 100 times the thickness of the compensation slice, ensures the maximum uniform transition, and the schematic diagram of distance 1 and distance 2 is shown in Figure 4 On the basis of chamfering, in order to further smooth the corners, a large rounded corner of 50 to 100 mm is added at the junction of the corner and the product. The schematic diagram of the compensation slice after smoothing is shown in Figure 4 .
[0078] In step (6), the variable-angle spiral regenerative cooling channel in the thrust chamber body model is extracted to optimize the shape accuracy and dimensional accuracy of the variable-angle spiral channel structure. For the angled channel structure, there is a cross-sectional change between the two adjacent layers of formed cross-sections. Figure 5 The figure shows the cross-section of two adjacent layers of the thrust chamber body with an inclination. Assuming that the solid line outline 1 in the figure is the cross-section of the nth layer of the part, and the dotted line outline 2 is the cross-section of the n+1th layer of the part, the red area in the figure will appear as the lower skin, and the cyan area will appear as the upper skin.
[0079] Since the area where the lower epidermis is located is a hanging feature, the powder below it is loose when there is no support, and its heat transfer efficiency is significantly lower than that of the non-hanging feature area (about 1 / 10 of the non-hanging feature entity), and it is easy to warp and deform slightly during the forming process; in addition, the growth support point of the lower epidermis is loose powder, and the existing conventional laser energy density is Gaussian distributed within the spot range, the energy density in the central area is high, and deep penetration of the laser is easy to cause the flow channel to collapse. The micro-deformation and collapse of the lower epidermis of the flow channel affect the dimensional accuracy of the flow channel. The growth support point of the upper epidermis is the solid part of the upper layer, without warping deformation and molten pool collapse protrusion, which does not affect the dimensional accuracy of the flow channel. In order to ensure high-precision forming of the flow channel, the present invention extracts the lower epidermis hanging feature area separately for laser type optimization, scanning strategy and scanning parameter planning. The laser type optimization adopts a flat-top laser to replace the energy Gaussian distribution laser, and utilizes the characteristics of the uniform energy density distribution of the flat-top laser in the circular area to effectively suppress the collapse of the molten pool and ensure the shape and dimensional accuracy of the flow channel. The scanning strategy and scanning parameter planning are based on the outer contour of the overhanging feature for biased scanning path planning, and the scanning is performed from the core part close to the solid to the border part close to the powder in sequence, such as Figure 6 The scanning parameters are specific parameters, and high scanning speed, low laser power and wide scanning spacing are used to reduce the warping deformation of the lower skin and the collapse of the molten pool.
[0080] High scanning speed, low laser power and wide scanning spacing reduce the warping deformation and molten pool collapse of the lower skin. The smaller the flow channel inclination angle and the larger the overhanging structure, the more likely it is to warp and collapse the molten pool. The present invention adopts gradual lower skin process parameters. Different process parameters are used for different inclination angles to control the flow channel accuracy. The lower skin parameters are as follows: the spiral groove lower skin parameters of the expansion section with an inclination angle of 35 to 45°: laser power 120w, scanning speed 2600mm / s, scanning spacing: 0.14mm; the spiral groove lower skin parameters of the cylindrical section with an inclination angle of 45°: laser power 130w, scanning speed 2300mm / s, scanning spacing: 0.13mm; the spiral groove lower skin parameters of the expansion section with an inclination angle of 45 to 60°: laser power 140w, scanning speed 2000mm / s, scanning spacing: 0.11mm.
[0081] In step (7), the process powder cleaning port and process support are designed to ensure smooth flow channel and additive manufacturing formability of the body.
[0082] In step (9), the additive manufacturing forming room temperature control system mainly relies on the temperature of the circulating airflow to control the temperature of the powder bed. Through the convection heat transfer principle, when the circulating airflow passes over the powder bed, it can preheat the powder bed, so that the forming room temperature during the forming process is stabilized in a reasonable temperature range, reducing the temperature difference stress. The temperature of the circulating airflow is heated by a PTC gas heating device, which is installed at the circulating air outlet of the circulating system of the additive manufacturing equipment, and the heating temperature range is 200 to 500°C.
[0083] In step (11), the metal powder in the spiral channel of the thrust chamber body is cleaned through the powder cleaning port by means of rotational vibration + high-pressure air blowing. After the powder cleaning is completed, an endoscope is used to confirm that there is no residual powder in the flow channel, and then a subsequent heat treatment stress relief process is performed. The heat treatment stress relief adopts vacuum heat treatment at a temperature of 600-700°C and a time of 6-8h. After the heat treatment is completed, the substrate and the product are separated by wire cutting. The wire cutting pulse waveform is rectangular, the pulse width is 30-45μs, the pulse interval is 200-220μs, and the current is 3-5A. The polishing and support removal adopts a pneumatic polishing gun to remove the body grid process support, and the support surface is refined and smoothly transitioned.
[0084] The present invention has been described in detail above in conjunction with specific implementations and exemplary examples, but these descriptions cannot be understood as limiting the present invention. Those skilled in the art understand that, without departing from the spirit and scope of the present invention, a variety of equivalent substitutions, modifications or improvements may be made to the technical solution of the present invention and its implementation methods, all of which fall within the scope of the present invention. The scope of protection of the present invention shall be subject to the attached claims.
[0085] The contents not described in detail in the specification of the present invention belong to the common knowledge of those skilled in the art.
Claims
1. An additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel, characterized in that: include: S1 establishes a three-dimensional model of the thrust chamber body; S2 determines the growth direction of the thrust chamber body based on the principle of minimum stress, least support and removable support; S3 obtains a macroscopically scaled three-dimensional model of the thrust chamber body according to the three-dimensional model and growth direction of the thrust chamber body; S4 obtains the three-dimensional model of anti-deformation process design based on the macro-scaled three-dimensional model of the thrust chamber body; S5 designs a three-dimensional model based on the anti-deformation process and performs process compensation in the model mutation area; S6 optimizes the laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel; S7 designs the process support and process powder cleaning port based on the model after process compensation to obtain the process 3D model of the thrust chamber body; S8 uses the process 3D model of the thrust chamber body and the optimized laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel to complete the additive manufacturing of the thrust chamber body.
2. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S2, the growth direction of the thrust chamber body is determined as: The large end flange of the thrust chamber body is connected to the base plate, and the normal line of the thrust chamber body is perpendicular to the forming platform.
3. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S3, according to the three-dimensional model and growth direction of the thrust chamber body, a method for obtaining a macro-scaled three-dimensional model of the thrust chamber body includes: On the three-dimensional model of the thrust chamber body, local models of the cylindrical section, the contraction-expansion section, the throat section, and the expansion section are respectively cut out, and the height of the local model is 15 to 25 mm; Set multiple groups of scaling ratios, scale each local model in three dimensions of X, Y, and Z, and obtain multiple groups of scaled local models; wherein the Z direction is the axial direction of the thrust chamber body, and the XY plane is perpendicular to the Z direction; According to the scaled local model, the laser additive manufacturing process is used to prepare local test pieces of the cylindrical section, the contraction and expansion section, the throat, and the expansion section. The scaling ratio corresponding to the local test piece with the smallest diameter size deviation is taken as the optimal scaling ratio. The three-dimensional model of the thrust chamber body is scaled according to the optimal scaling ratio to obtain a macro-scaled three-dimensional model of the thrust chamber body.
4. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S3, the three-dimensional model of the thrust chamber body is scaled according to the scaling ratios of 1.004%, 1.004% and 1.001% in the X, Y and Z dimensions respectively, to obtain a macro-scaled three-dimensional model of the thrust chamber body; wherein the Z direction is the axial direction of the thrust chamber body, and the XY plane is perpendicular to the Z direction.
5. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S4, the thrust line diameter d of the inverse deformation process design three-dimensional model and the thrust line diameter d0 of the macro-scaled three-dimensional model satisfy the following relationship: Wherein, H is the forming height.
6. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S5, the model mutation area includes the cylindrical section, the contraction and expansion section, and the area where the outer wall of the expansion section is connected to other components; The method for performing process compensation in a model mutation area includes: adding a process compensation slice outside the mutation area of the reverse deformation process design three-dimensional model, and the process compensation slice smoothly transitions to the outer wall of the original reverse deformation process design three-dimensional model by chamfering and rounding.
7. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 6, characterized in that: The process compensation slice is annular, with a thickness of 0.2-0.3mm and a width of 20-30mm; When the process compensation slice is smoothly transitioned to the outer wall of the original anti-deformation process design three-dimensional model by chamfering and rounding, the process compensation slice is first chamfered to ensure the maximum uniform transition, and then, on the basis of the chamfer, a large rounded corner of 50 to 100 mm is chamfered at the junction of the chamfer and the outer wall; The bevel angle is an asymmetrical inclination angle.
8. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S6, the optimization of the laser type, scanning strategy and scanning parameters of the variable-angle spiral regenerative cooling channel includes: The laser type of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel adopts flat-top laser. The scanning strategy of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel includes: using the outer contour of the overhang feature as a reference to perform offset scanning path planning, and scanning from the core part close to the solid to the border part close to the powder in sequence; The scanning parameters of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel include: a high scanning speed of 2000mm / s to 2600mm / s, a low laser power of 120w to 140w, and a wide scanning spacing of 0.11mm to 0.14mm.
9. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 8, characterized in that: The scanning parameters of the lower skin overhang feature area of the variable inclination spiral regenerative cooling channel in the contraction section, cylindrical section and expansion section are as follows: The parameters of the lower surface of the spiral groove with an inclination angle of 35 to 45° in the expansion section are as follows: laser power 120w, scanning speed 2600mm / s, scanning spacing: 0.14mm; Parameters of the lower epidermis of the spiral groove with an inclination angle of 45° in the cylindrical section: laser power 130w, scanning speed 2300mm / s, scanning spacing: 0.13mm; The expansion section has an inclination angle of 45 to 60° and the lower surface parameters of the spiral groove are: laser power 140w, scanning speed 2000mm / s, scanning spacing: 0.11mm.
10. The additive manufacturing method for a thrust chamber body including a variable-angle spiral regenerative cooling channel according to claim 1, characterized in that: In step S8, during the additive manufacturing process of the thrust chamber body, the temperature of the powder bed is controlled by using the temperature of the circulating airflow, and the temperature range is controlled to be 200-500° C. The specific method includes installing a PTC gas heating device at the circulating gas outlet position of the circulating system of the additive manufacturing equipment; After the additive manufacturing of the thrust chamber body, the resulting workpiece is subjected to powder cleaning, heat treatment and stress relief processes, and wire cutting; The heat treatment stress relief process is carried out by vacuum heat treatment, the temperature is 600-700℃, and the time is 6-8h; Wire cutting adopts rectangular pulse wave, pulse width: 30 ~ 45μs, pulse interval: 200 ~ 220μs, current: 3 ~ 5A.