Recording method and recording device
By using water-based inks for both white and non-white ink adhesion processes and processing solutions, the speed and image quality issues in serial inkjet recording methods have been resolved, achieving efficient ink adhesion and stable ink ejection, thus improving the visual effect of color images.
Patent Information
- Application Number
- CN202410352721.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-28
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-03-26
AI Technical Summary
Existing serial inkjet recording methods suffer from slow recording speed, reduced ink ejection stability due to condensation on the nozzle surface, and image quality degradation caused by mixing of white and colored inks and ink droplet bleeding.
The process involves applying white and non-white inks using water-based inks. The ink is applied to the recording medium by scanning. A treatment liquid containing a coagulant is used to promote ink coagulation. The amount and temperature of ink application are controlled, and heating drying or low-temperature treatment is avoided to suppress condensation. The nozzle surface temperature difference is optimized.
It improves recording speed, suppresses condensation, enhances image quality, and ensures ink ejection stability and visual recognizability of color images.
Smart Images

Figure HDA0004760345280000011 
Figure HDA0004760345280000021 
Figure HDA0004760345280000031
Abstract
Description
Technical Field
[0001] The present invention relates to a recording method and a recording device. Background Art
[0002] The inkjet recording method can record high-definition images with a relatively simple device, and has achieved rapid development in various fields. Among them, the following research has been conducted: recording (printing) using water-based ink on a recording medium including a film such as PET by a so-called serial recording method, wherein the recording is performed by performing a plurality of main scans while moving the inkjet head and ejecting the ink to adhere to the medium.
[0003] In particular, films such as PET are transparent or semi-transparent, and in order to improve the visibility of color images, a layer formed of white ink called a base layer to conceal the background and a layer formed of color ink on which a predetermined image is formed are sometimes laminated for printing.
[0004] For example, Patent Document 1 describes an inkjet recording method in which a process of forming an image layer using white ink and a process of forming an image layer using color ink are performed by performing a plurality of main scans in a serial recording method.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent document 1: Japanese Patent Application Publication No. 2018-15968.
[0008] However, the serial recording method has a problem of slow recording speed.
[0009] In addition, there are problems such as condensation on the nozzle surface, which reduces ink ejection stability, and / or white ink and color ink mixing and / or ink droplet bleeding, which deteriorates image quality (uneven light and dark).
[0010] Therefore, there is a demand for a recording method that has an excellent recording speed, suppresses condensation, and has excellent image quality (uneven shading). Summary of the invention
[0011] One embodiment of the recording method according to the present invention comprises:
[0012] a treatment liquid attachment step of attaching the treatment liquid containing the coagulant to the recording medium;
[0013] A white ink attaching step of ejecting a white ink composition containing a white color material from an inkjet head and attaching the composition to the recording medium; and
[0014] a non-white ink attaching step of ejecting a non-white ink composition containing a non-white color material from the inkjet head and attaching the non-white ink composition to the recording medium;
[0015] The white ink composition and the non-white ink composition are water-based inks,
[0016] The white ink attaching step and the non-white ink attaching step are respectively performed by scanning, in which the ink composition is ejected from the inkjet head to attach to the recording medium while the inkjet head is moved relative to the recording medium in a fixed position.
[0017] The white ink attaching step attaches the white ink composition to a scanning area of a single scan by a single scan.
[0018] The non-white ink attaching step attaches the non-white ink composition to the scanning area of the scanning by scanning once,
[0019] For a scan area in which one of the scanning in the white ink attaching step and the scanning in the non-white ink attaching step has been performed, the other scanning is performed by another scanning.
[0020] The surface temperature of the recording medium in the white ink attaching step and the non-white ink attaching step is 35° C. or less.
[0021] One embodiment of the recording device according to the present invention is:
[0022] A recording device for recording using the recording method of one of the above schemes,
[0023] The recording device includes the processing liquid, the white ink composition, the non-white ink composition, and the inkjet head. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a front view schematically showing an example of the recording device according to the present embodiment.
[0025] Figure 2 It is a bottom view partially showing the structure of the recording unit.
[0026] Figure 3 It is a figure which shows the composition example of ink and a process liquid (Table 1).
[0027] Figure 4 It is a figure which shows the example of a recording method and an evaluation result (Table 2).
[0028] Figure 5 It is a figure which shows the example of a recording method and an evaluation result (Table 3).
[0029] Figure 6 (a), (b), (c), and (d) are schematic diagrams showing the use of Figure 1 A diagram showing an example of recording performed by a recording device according to the present embodiment.
[0030] Figure 7 It is a perspective view schematically showing another example of the recording device according to the present embodiment.
[0031] Figure 8 (a), (b), (c), and (d) are schematic diagrams showing the use of Figure 7 A diagram showing an example of recording performed by a recording device according to the present embodiment.
[0032] Fig. 9 (a), (b), and (c) are schematic diagrams showing the use of Figure 7 A diagram showing another example of recording of this embodiment performed by a recording device.
[0033] Explanation of symbols
[0034] 100, 500, recording device; 200, main device; 210, printer driver; 230, communication control unit; 240, monitor; 300, printer unit; 400, printer control unit; 1, main body shell; 2, unwinding unit; 9, housing of slide; 12, main body of slide; 13, slide moving mechanism; 14, conveying unit; 21, unwinding shaft; 3, printing room; 30, 11, paper plate; 31, recording unit; 32, slide; 33, support plate; 34, 35, 510, inkjet head; 37, X-axis guide; 38, suction unit; 39, heater; 4, drying unit; 5, winding unit; 51, winding shaft; 6, base; 71-77, rollers; 8, box mounting unit; 81, processing liquid box; 82, ink cartridge; R1, R2, rollers; S, sheet. DETAILED DESCRIPTION
[0035] Hereinafter, the embodiments of the present invention will be described. The embodiments described below are merely examples of the present invention. The present invention is not limited to the following embodiments, and also includes various modifications implemented within the scope of not changing the gist of the present invention. In addition, all the structures described below are not necessarily the necessary structures of the present invention.
[0036] 1. Recording method
[0037] The recording method according to one embodiment of the present invention comprises: a treatment liquid attachment step of attaching a treatment liquid containing a coagulant to a recording medium; a white ink attachment step of ejecting a white ink composition containing a white color material from an inkjet head and attaching it to the recording medium; and a non-white ink attachment step of ejecting a non-white ink composition containing a non-white color material from the inkjet head and attaching it to the recording medium, wherein the white ink composition and the non-white ink composition are water-based inks, and the white ink attachment step and the non-white ink attachment step are respectively performed by scanning, and during the scanning, the inkjet head is moved relative to a position where the ink is being moved. The recording medium in a fixed state moves while the ink composition is ejected from the inkjet head and attached to the recording medium. The white ink attachment process attaches the white ink composition to a scanning area scanned once by a single scan, and the non-white ink attachment process attaches the non-white ink composition to a scanning area scanned once by a single scan. For a scanning area scanned by either the white ink attachment process or the non-white ink attachment process, the other scanning is performed by another scanning. The surface temperature of the recording medium in the white ink attachment process and the non-white ink attachment process is below 35°C.
[0038] The following research has been conducted: recording (printing) using aqueous ink on a recording medium including a film such as PET by a so-called serial recording method, in which recording is performed by performing a plurality of main scans while moving an inkjet head and ejecting ink to adhere to the medium.
[0039] In particular, films such as PET are transparent (including semi-transparent ones), and in order to improve the visibility of color images, a layer formed of white ink called a base layer to conceal the background and a layer formed of color ink to form a predetermined image are sometimes stacked for printing.
[0040] Here, the serial recording method has the advantage of easily ensuring nozzle reliability because the inkjet head comes to a position deviated from the medium during the interval between main scans, so the ink can be flushed from the nozzle at a position not on the medium. In addition, since the position of the medium is fixed during the main scan, image degradation caused by changes in the conveying speed associated with the medium conveying can be prevented. Moreover, by performing multiple main scans, a wider image can be recorded, which is useful in that the length of the nozzle column of the inkjet head (the width of the ink that can be attached in one main scan) can be shortened.
[0041] However, in the serial recording method, when one ink is separately attached to the scanning area of the medium to which the ink can be attached in one main scan by two or more main scans, the number of main scans required for recording increases, and the recording speed becomes slower. Therefore, by completely attaching one ink to the scanning area of the medium to which the ink can be attached in one main scan by one main scan (one ink is not attached to the same scanning area by two or more main scans), the recording speed is increased.
[0042] On the other hand, when a color image is formed at a position overlapping with a white image by such recording, that is, when recording is performed in which white ink is attached by one main scan and color ink is attached by one main scan in a scanning area of a medium to which ink can be attached by one main scan, condensation occurs on the nozzle surface, and a new problem of reduced ink ejection stability due to condensation occurs. This is presumably because all inks are attached by one main scan in the scanning area of the medium, so the amount of ink attached in one main scan is large, and a large amount of solvent components of the ink attached to the medium evaporate at one time, thereby increasing the vapor concentration on the recording medium, and in the main scan for attaching the next ink, the solvent components of the evaporated ink condense on the nozzle surface.
[0043] After verification, it was found that when a primary drying process is performed to heat the medium near the paper plate, the evaporation of the ink is promoted by the heating, and the temperature difference between the nozzle surface and the vicinity of the paper plate becomes large, so condensation is likely to occur. Therefore, in the process of attaching each ink, by not performing a primary drying process based on heating or by setting the medium temperature to a low temperature below a predetermined temperature even if the process is performed, the evaporation of the solvent component of the ink can be suppressed, and the temperature difference between the nozzle surface and the vicinity of the paper plate can be suppressed to a low level, thereby reducing condensation.
[0044] However, when the primary drying process based on heating is not performed or low-temperature heating is performed, since the drying of the ink is not accelerated, there is a new problem of deterioration of image quality (uneven light and dark) due to mixing of white ink and color ink and bleeding of ink droplets. In addition, when ink is attached to the scanning area of the medium to which ink can be attached in one main scan by one main scan, the amount of ink attached in one scan is large, and image quality degradation due to bleeding of ink droplets is likely to occur.
[0045] Therefore, by using a treatment liquid containing a coagulant for aggregating the components of the ink, the ink droplets can be fixed on the medium as soon as possible, and the image quality (uneven density) can be improved.
[0046] Therefore, according to the recording method according to the present embodiment, it is possible to provide a recording method that has an excellent recording speed, suppresses condensation, and has excellent image quality (uneven shading).
[0047] Hereinafter, each step and the like of the recording method according to the present embodiment will be described. In addition, when a white ink composition and a non-white ink composition are not particularly distinguished, they may be referred to as an ink composition or ink.
[0048] 1.1 Treatment liquid attachment process
[0049] The recording method according to the present embodiment includes a processing liquid attaching step of attaching a processing liquid containing an aggregating agent to a recording medium.
[0050] 1.1.1 Attachment method
[0051] As a method for attaching the treatment liquid to the recording medium, any of non-contact and contact methods or a combination of methods such as an inkjet method, a method of applying the treatment liquid using a roller or a scraper, a method of applying the treatment liquid to the recording medium using various sprayers, a method of immersing the recording medium in the treatment liquid, and a method of applying the treatment liquid to the recording medium using a brush, etc. can be used. Among them, the inkjet method is preferred.
[0052] The recording method involved in this embodiment preferably performs a treatment liquid attachment process by scanning, in which the treatment liquid is ejected from the inkjet head while the inkjet head is moved and attached to the recording medium. In this case, it is easy to control the amount of treatment liquid attached and the position of attachment. Moreover, the white ink attachment process and the non-white ink attachment process described later are preferably scanned to attach the treatment liquid to the same scanning area in the same scanning as the scanning for attaching the ink composition. If it is such an attachment method (simultaneous injection), the treatment liquid and each ink composition are easy to mix and react. In this case, the viscosity and coagulation of the ink are further promoted, and the ink droplets can be fixed on the medium as soon as possible, so there is a tendency for the image quality (uneven light and dark) to be better.
[0053] The above-mentioned attachment method, for example, in the case of a nozzle array composed of a plurality of nozzles arranged along a direction (hereinafter also referred to as "nozzle array direction") intersecting the direction in which the inkjet head moves (hereinafter also referred to as "nozzle moving direction") on the nozzle surface of the inkjet head along the nozzle moving direction, can be configured so that when the nozzle array that ejects the processing liquid is projected along the nozzle moving direction, at least a portion of it overlaps with the nozzle array that ejects the white ink composition and the nozzle array that ejects the non-white ink composition in the nozzle array direction.
[0054] In the above-mentioned attachment method, the timing of landing of the white ink composition and the treatment liquid and the timing of landing of the non-white ink composition and the treatment liquid may be different, but the time difference is very small. Therefore, the order of landing of the ink composition and the treatment liquid is not particularly limited. However, from the viewpoint of better reactivity, it is preferred that the treatment liquid lands before the ink composition lands.
[0055] When the process liquid attaching step is performed together with the white ink attaching step, the maximum attachment amount of the process liquid is preferably in the range of 0.1 to 5.0 mg / inch per unit area of the recording medium. 2 , more preferably 0.2 to 4.0 mg / inch 2 , more preferably 0.3 to 3.0 mg / inch 2 , particularly preferably 0.4 to 2.0 mg / inch 2 , more preferably 0.5 to 1.5 mg / inch 2 , particularly preferably 0.8 to 1.5 mg / inch 2 When the maximum deposition amount of the treatment liquid is within the above range, there is a tendency that a better image quality (uneven density) can be obtained and a better ink filling property can be obtained.
[0056] Furthermore, “concurrently performed” means that the treatment liquid is attached to the recording medium in the treatment liquid attaching step before or simultaneously with the white ink composition being attached to the recording medium in the white ink attaching step.
[0057] When the process liquid attaching step is performed together with the non-white ink attaching step, the maximum amount of the process liquid attached is preferably within a range of 0.01 to 3.0 mg / inch per unit area of the recording medium. 2 , more preferably 0.05 to 2.0 mg / inch 2 , more preferably 0.1 to 1.0 mg / inch 2 , particularly preferably 0.2 to 0.8 mg / inch 2 , more preferably 0.3 to 0.7 mg / inch 2 When the maximum deposition amount of the treatment liquid is within the above range, there is a tendency to obtain better image quality (uneven density) and better ink filling properties.
[0058] In addition, the maximum total amount of treatment liquid deposited in each treatment liquid depositing step performed in conjunction with the white ink depositing step and the non-white ink depositing step is preferably within a range of 4.0 mg / inch. 2 Below, more preferably 0.1 mg / inch 2 Above 3.8mg / inch 2More preferably, it is 0.5 mg / inch 2 Above 3.5mg / inch 2 Below, more preferably 0.8 mg / inch 2 Above 2.5mg / inch 2 Below, more preferably 1.0 mg / inch 2 Above 2.0mg / inch 2 When the total maximum deposition amount of the processing liquid is within the above range, there is a tendency to obtain a more excellent image quality (uneven density) and a more excellent ink filling property.
[0059] In addition, in the area where the white ink composition and the non-white ink composition are attached, the amount of the treatment liquid attached to the recording medium can be set to be constant or different according to the position. In particular, the amount of the treatment liquid attached can also be made different according to the amount of the non-white ink composition attached. However, it is preferred that in any position (recording area) where recording is performed in the recording method, the following method is used: the amount of the treatment liquid in the treatment liquid attachment process (hereinafter also referred to as the "second treatment liquid attachment process") performed in the same recording area in conjunction with the non-white ink attachment process is smaller than the amount of the treatment liquid in the treatment liquid attachment process (hereinafter also referred to as the "first treatment liquid attachment process") performed in conjunction with the white ink attachment process.
[0060] For example, even in a recording area where the amount of treatment liquid attached in the second treatment liquid attachment process is the largest, it is preferable to perform the process in such a manner that the amount of treatment liquid attached in the second treatment liquid attachment process is smaller than the amount of treatment liquid attached in the first treatment liquid attachment process. That is, even in a recording area where the amount of treatment liquid attached in the second treatment liquid attachment process is the largest and the amount of treatment liquid attached in the first treatment liquid attachment process is the smallest, it is preferable to perform the process in such a manner that the amount of treatment liquid attached in the second treatment liquid attachment process is smaller than the amount of treatment liquid attached in the first treatment liquid attachment process in the same recording area.
[0061] The ratio (mass ratio) of the amount of treatment liquid deposited in the second treatment liquid depositing step to the amount of treatment liquid deposited in the first treatment liquid depositing step is preferably less than 1, more preferably 0.1 to 0.9, further preferably 0.2 to 0.5, further preferably 0.3 to 0.49, and particularly preferably 0.4 to 0.47. In this case, image quality is better, so it is preferred.
[0062] The ratio (mass ratio) of the amount of the white ink composition deposited in the white ink depositing step to the amount of the treatment liquid deposited in the first treatment liquid depositing step is preferably 5 to 20, more preferably 7 to 17, and still more preferably 10 to 15. In this case, image quality and the like are further improved, which is preferred.
[0063] The ratio (mass ratio) of the amount of the non-white ink composition deposited in the non-white ink depositing step to the amount of the treatment liquid deposited in the second treatment liquid depositing step is preferably 8 to 18, more preferably 10 to 16, and even more preferably 11 to 15. In this case, image quality and the like are further improved, so this is preferred.
[0064] When droplets of the treatment liquid are attached to the recording medium by coating using an inkjet method or a sprayer, the maximum weight of each drop of the treatment liquid is preferably in the range of 0.5 to 8 ng, more preferably 1 to 6 ng, further preferably 1.5 to 5 ng, and particularly preferably 2 to 4 ng. This can increase the contact opportunities between the treatment liquid and the ink on the recording medium, thereby tending to obtain better image quality (uneven light and dark) and better ink filling properties.
[0065] 1.1.2. Recording medium
[0066] The recording medium used in the recording method according to the present embodiment is not particularly limited, and examples thereof include absorptive recording media such as paper and cloth; low-absorptive recording media such as printing paper; and non-absorptive recording media such as metal, glass, and polymers.
[0067] Here, the low-absorption or non-absorption recording medium refers to a recording medium having the property of not absorbing liquid at all or hardly absorbing liquid. Quantitatively, the low-absorption or non-absorption recording medium refers to "the recording medium having a low absorption rate from the start of contact to 30 msec in the Bristow method". 1 / 2 The water absorption is 10mL / m 2 The Bristow method is the most popular method for measuring the amount of liquid absorbed in a short period of time, and is also adopted by the Japan Pulp and Paper Technology Association (JAPAN TAPPI). Details of the test method are described in Standard No. 51 "Paper and Board - Liquid Absorption Test Method - Bristow Method" of "JAPAN TAPPI Pulp and Paper Test Method 2000 Edition". In contrast, an absorbent recording medium refers to a recording medium that does not conform to a low-absorbency or non-absorbent recording medium.
[0068] As low-absorption recording media, for example, there can be mentioned recording media having a low-absorption coating layer on the surface, which is called coated paper. For example, as recording media whose substrate is paper, there can be mentioned: art paper, coated paper, matte paper and other printing papers. When the substrate is a plastic film, there can be mentioned: recording media whose surfaces are coated with polymers such as polyvinyl chloride, polyethylene terephthalate, polycarbonate, polystyrene, polyurethane, polyethylene, polypropylene and the like; and recording media whose surfaces are coated with particles of silica, titanium and the like together with an adhesive.
[0069] Examples of non-absorbent recording media include recording media in which a substrate such as paper is coated with plastic, recording media in which a plastic film is bonded to a substrate such as paper, and plastic films having no absorbing layer (receiving layer). Examples of the plastic include polyvinyl chloride, polyethylene terephthalate, polycarbonate, polystyrene, polyurethane, polyethylene, and polypropylene.
[0070] The absorbent recording medium is not particularly limited, and examples thereof include plain paper, thick paper, and liner paper. Examples of liner paper include paper made of kraft pulp, waste paper, and the like.
[0071] Furthermore, the recording medium may be colorless and transparent, semi-transparent, colored and transparent, colored and opaque, colorless and opaque, etc. Furthermore, the recording medium itself may be colored, semi-transparent, or transparent.
[0072] 1.1.3 Treatment fluid
[0073] Hereinafter, each component contained in the treatment liquid used in the treatment liquid attachment process is described. In addition, the treatment liquid is not an ink composition used for coloring the recording medium, but an auxiliary liquid used together with the ink composition used for coloring. In addition, the treatment liquid may contain a coloring material such as a pigment, but preferably 0.2% by mass or less, more preferably 0.1% by mass or less, and further preferably 0.05% by mass or less relative to the total mass of the treatment liquid, and the lower limit is 0% by mass. The treatment liquid preferably does not contain a coloring material.
[0074] Coagulant
[0075] The processing liquid used in the recording method involved in this embodiment contains a coagulant that causes the components of the ink to condense. The coagulant has the function of condensing the color material and the resin particles by reacting with the color material contained in the ink, the resin particles that may be contained in the ink, and the like. However, the degree of condensation of the color material or the resin particles caused by the coagulant varies depending on the types of the coagulant, the color material, and the resin particles, and can be adjusted. In addition, the coagulant can condense the color material and the resin particles by reacting with the color material and the resin particles contained in the ink. Through such condensation, for example, the color development of the color material can be improved, the fixability of the resin particles can be improved, and / or the viscosity of the ink can be increased.
[0076] The coagulant is not particularly limited, and metal salts, organic acids, inorganic acids, cationic compounds, etc. can be cited. As the cationic compound, cationic resins (cationic polymers), etc. can be used. Among them, as the metal salt, a polyvalent metal salt is preferred, and as the cationic compound, a cationic resin is preferred. Therefore, as the coagulant, it is preferably selected from cationic resins, organic acids, and polyvalent metal salts in terms of particularly excellent image quality, abrasion resistance, gloss, etc.
[0077] Metal Salts
[0078] As the metal salt, a polyvalent metal salt is preferred, but metal salts other than polyvalent metal salts may also be used. Among these coagulants, at least one selected from metal salts and organic acids is preferably used from the point of view of excellent reactivity with the components contained in the ink. In addition, among cationic compounds, cationic resins are preferably used from the point of view of easy dissolution in the treatment liquid. In addition, multiple coagulants may be used simultaneously.
[0079] The polyvalent metal salt refers to a compound composed of a divalent or higher metal ion and an anion. Examples of divalent or higher metal ions include ions of calcium, magnesium, copper, nickel, zinc, barium, aluminum, titanium, strontium, chromium, cobalt, and iron. Among the metal ions constituting the polyvalent metal salt, at least one of calcium ions and magnesium ions is preferred from the perspective of excellent cohesion of the components of the ink.
[0080] Anions constituting the polyvalent metal salt are inorganic ions or organic ions. That is, the polyvalent metal salt in the present invention refers to a salt consisting of an inorganic ion or an organic ion and a polyvalent metal. Examples of such inorganic ions include chloride ions, bromide ions, iodide ions, nitrate ions, sulfate ions, hydroxide ions, and the like. Examples of organic ions include organic acid ions, such as carboxylic acid ions and formate ions.
[0081] In addition, the polyvalent metal compound is preferably an ionic polyvalent metal salt, and in particular, when the polyvalent metal salt is a magnesium salt or a calcium salt, the stability of the treatment solution is better. In addition, the counter ion of the polyvalent metal may be any one of an inorganic acid ion and an organic acid ion.
[0082] As the specific example of the above-mentioned polyvalent metal salt, calcium carbonate, calcium nitrate, calcium chloride, calcium sulfate, magnesium sulfate, calcium hydroxide, magnesium chloride, magnesium carbonate, barium sulfate, barium chloride, zinc carbonate, zinc sulfide, aluminum silicate, calcium silicate, magnesium silicate, copper nitrate, calcium formate, calcium acetate, magnesium acetate, aluminum acetate, etc. such as heavy calcium carbonate and light calcium carbonate can be enumerated. These polyvalent metal salts can be used alone or in combination. Wherein, owing to can ensure sufficient solubility to water and the trace of treatment solution is reduced (trace is not obvious), therefore preferably at least any one of calcium formate, magnesium sulfate, calcium nitrate and calcium chloride, more preferably calcium formate, calcium nitrate. In addition, these metal salts can also have hydration water under raw material form.
[0083] Examples of the metal salt other than the polyvalent metal salt include monovalent metal salts such as sodium salts and potassium salts, and examples thereof include sodium sulfate and potassium sulfate.
[0084] Organic Acid
[0085] As organic acid, for example, preferably include: poly (meth) acrylic acid, acetic acid, glycolic acid, malonic acid, malic acid, maleic acid, ascorbic acid, succinic acid, glutaric acid, fumaric acid, citric acid, tartaric acid, lactic acid, sulfonic acid, orthophosphoric acid, pyrrolidonecarboxylic acid, pyranonecarboxylic acid, pyrrolecarboxylic acid, furancarboxylic acid, pyridinecarboxylic acid, coumaric acid, thiophenecarboxylic acid, nicotinic acid or derivatives of these compounds, or their salts, etc. The organic acid can be used alone or in combination of two or more. The salt of the metal salt in the salt of the organic acid is included in the above-mentioned metal salt.
[0086] Inorganic acid
[0087] Examples of the inorganic acid include sulfuric acid, hydrochloric acid, nitric acid, phosphoric acid, etc. The inorganic acid may be used alone or in combination of two or more.
[0088] Cationic resin
[0089] Examples of the cationic resin (cationic polymer) include cationic urethane resins, cationic olefin resins, cationic amine resins, etc. The cationic polymer is preferably water-soluble.
[0090] As the cationic urethane resin, commercially available products can be used, for example, Hydran CP-7010, CP-7020, CP-7030, CP-7040, CP-7050, CP-7060, CP-7610 (trade names, manufactured by Dainippon Ink & Chemicals Co., Ltd.), Superflex 600, 610, 620, 630, 640, 650 (trade names, manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.), polyurethane emulsions WBR-2120C, WBR-2122C (trade names, manufactured by Daisei Fine Chemicals Co., Ltd.), etc. can be used.
[0091] Cationic olefin resin is a resin having olefins such as ethylene and propylene in the structural skeleton, and well-known olefin resins can be appropriately selected for use. In addition, cationic olefin resins can also be an emulsion state dispersed in a solvent including water, an organic solvent, etc. As cationic olefin resins, commercially available products can be used, for example, ArrowBase CB-1200, CD-1200 (trade name, Japan Unitika Co., Ltd. system) etc. can be cited.
[0092] As cationic amine resin (cationic polymer), as long as it has an amino group in the structure, well-known amine resins can be appropriately selected for use. For example, polyamine resins, polyamide resins, polyallylamine resins, etc. can be cited. Polyamine resins are resins having amino groups in the main skeleton of the resin. Polyamide resins are resins having amide groups in the main skeleton of the resin. Polyallylamine resins are resins having a structure derived from allyl groups in the main skeleton of the resin.
[0093] In addition, examples of cationic polyamine resins include Unisense KHE103L (hexamethylenediamine / epichlorohydrin resin, a 1% aqueous solution having a pH of about 5.0, a viscosity of 20 to 50 (mPa·s), and a solid content concentration of 50% by mass) and Unisense KHE 104L (dimethylamine / epichlorohydrin resin, a 1% aqueous solution having a pH of about 7.0, a viscosity of 1 to 10 (mPa·s), and a solid content concentration of 20% by mass) manufactured by Senka Co., Ltd. Specific examples of commercially available cationic polyamine resins include FL-14 (manufactured by SNF), Arafix 100, 251S, 255, 255LOX (manufactured by Arakawa Chemical Co., Ltd.), DK-6810, 6853, 6885; WS-4010, 4011, 4020, 4024, 4027, 4030 (manufactured by Seiko PMC Co., Ltd.), Papiogen P-105 (manufactured by Senka Co., Ltd.), Sumirez Resin 650 (30), 675A, 6615, SLX-1 (manufactured by Taoka Chemical Industry Co., Ltd.), CatioMaster (registered trademark) PD-1, 7 (epichlorohydrin-amine derivative resin), 30, A, PDT-2, PE-10, PE-30, DT-EH, EPA-SK01, TMHMDA-E (manufactured by Yokkaichi Synthetic Co., Ltd.), JetFix 36N, 38A, 5052 (manufactured by Satoda Chemical Co., Ltd.).
[0094] As the polyamine resin, polyallylamine resin can also be mentioned. Examples of the polyallylamine resin include: polyallylamine hydrochloride, polyallylamine amide sulfate, allylamine hydrochloride-diallylamine hydrochloride copolymer, allylamine acetate-diallylamine acetate copolymer, allylamine hydrochloride-dimethylallylamine hydrochloride copolymer, allylamine-dimethylallylamine copolymer, polydiallylamine hydrochloride, polymethyldiallylamine hydrochloride, polymethyldiallylamine amide sulfate, polymethyldiallylamine acetate, polydiallyldimethylammonium chloride, diallylamine acetate-sulfur dioxide copolymer, diallylmethylethylammonium ethyl sulfate-sulfur dioxide copolymer, methyldiallylamine hydrochloride-sulfur dioxide copolymer, diallyldimethylammonium chloride-sulfur dioxide copolymer, diallyldimethylammonium chloride-acrylamide copolymer, and the like.
[0095] These flocculating agents can also be used in a variety of ways. In addition, among these flocculating agents, if at least one of a polyvalent metal salt, an organic acid, and a cationic resin is selected, the flocculation effect is better, and therefore a higher quality image (particularly a good color development property) can be formed.
[0096] The total content of the coagulant in the treatment liquid is preferably, for example, 1% by mass or more and 30% by mass or less relative to the total mass of the treatment liquid. The lower limit of the content is preferably 2% by mass or more, more preferably 3% by mass or more. In addition, the upper limit of the content is preferably 20% by mass or less, more preferably 15% by mass or less, further preferably 12% by mass or less, further preferably 10% by mass or less, and particularly preferably 8% by mass or less.
[0097] In addition, when the coagulant is shared by the solution and / or the dispersion, the content as the solid component is also preferably within the above range. If the content of the coagulant is 1% by mass or more, there is a tendency that the coagulant has a sufficient ability to coagulate the components contained in the ink. In addition, by making the content of the coagulant 30% by mass or less, the solubility and dispersibility of the coagulant in the treatment liquid become better, and there is a tendency that the storage stability of the treatment liquid can be improved.
[0098] Since the solubility of the coagulant in the treatment liquid is good even when the hydrophobicity of the organic solvent that can be contained in the treatment liquid is high, it is preferred to use a coagulant having a solubility of 1 g or more in 100 g of water at 25°C, and it is more preferred to use a coagulant having a solubility of 3 g or more and 80 g or less.
[0099] water
[0100] The treatment liquid used in the recording method according to the present embodiment preferably contains water. The type and content of water can be the same as those of the white ink composition described below. An aqueous treatment liquid is preferred.
[0101] Organic solvents
[0102] The processing liquid used in the recording method according to the present embodiment preferably contains an organic solvent. The type and content of the organic solvent may be the same as those of the white ink composition described below.
[0103] The treatment liquid preferably contains an alkane polyol organic solvent having a normal boiling point exceeding 280° C. in an amount not exceeding 2% by mass, more preferably not exceeding 1.5% by mass, further preferably not exceeding 1.0% by mass, still further preferably not exceeding 0.5% by mass, and particularly preferably not exceeding 0.1% by mass, relative to the total mass of the treatment liquid. The lower limit of the content of the alkane polyol organic solvent having a normal boiling point exceeding 280° C. may be 0% by mass.
[0104] The treatment liquid preferably contains an organic solvent having a normal boiling point of 150 to 280° C. The normal boiling point of the organic solvent is more preferably 160 to 270° C., further preferably 170 to 260° C., and particularly preferably 180 to 250° C. In addition, the content of the organic solvent is preferably 10 to 50% by mass, more preferably 20 to 40% by mass, and further preferably 25 to 35% by mass relative to the total mass of the treatment liquid.
[0105] In this way, the drying of the formed image becomes good, faster recording can be performed, and there is a tendency that the close contact with the recording medium can also be improved. In addition, the processing liquid is more preferably an organic solvent (not limited to polyols) with a standard boiling point exceeding 280.0°C within the above range. Examples of organic solvents with a standard boiling point exceeding 280°C include glycerin and polyethylene glycol monomethyl ether.
[0106] Surfactants
[0107] The processing liquid used in the recording method according to the present embodiment preferably contains a surfactant. The type and content of the surfactant may be the same as those of the white ink composition described below.
[0108] Other ingredients
[0109] The processing liquid used in the recording method of this embodiment may contain resin particles, wax, additives, resin dispersants, preservatives / mildewproof agents, rust inhibitors, chelating agents, viscosity modifiers, antioxidants, etc. in addition to the above-mentioned components as long as the function is not impaired. These components may be the same as those of the white ink composition described later.
[0110] Physical properties of treatment fluid
[0111] From the viewpoint of making the wettability and spreadability to the recording medium appropriate, the surface tension of the treatment liquid used in the recording method involved in this embodiment at 25° C. is preferably 40 mN / m or less, more preferably 38 mN / m or less, further preferably 35 mN / m or less, further preferably 30 mN / m or less, and particularly preferably 25 mN / m or less. In addition, the surface tension can be measured by using an automatic surface tensiometer CBVP-Z (manufactured by Kyowa Interface Science Co., Ltd.) and confirming the surface tension when a platinum plate is wetted with the composition under an environment of 25° C.
[0112] The processing liquid used in the recording method involved in this embodiment is more preferably attached to the recording medium by an inkjet method. In this case, the viscosity at 20°C is preferably set to 1.5 mPa·s to 15 mPa·s, more preferably 1.5 mPa·s to 7 mPa·s, and further preferably 1.5 mPa·s to 5.5 mPa·s. In the case where the processing liquid is attached to the recording medium by an inkjet method, it is easy to effectively form a predetermined processing liquid attachment area on the recording medium. In addition, the viscosity is measured, for example, using a rheometer (MCR302 / manufactured by Anton Paar) at 25°C and a shear rate of 200 s -1 The measurement was carried out under the conditions of .
[0113] 1.2 White ink adhesion process
[0114] The recording method according to the present embodiment includes a white ink attaching step of discharging a white ink composition containing a white color material from an inkjet head and attaching the composition to the recording medium.
[0115] 1.2.1 Attachment method
[0116] The white ink adhesion process of the recording method involved in this embodiment is performed by scanning (hereinafter also referred to as "main scanning"), in which the white ink composition is ejected from the inkjet head and adhered to the recording medium while the inkjet head is moved relative to the recording medium in a fixed position.
[0117] Such scanning refers to, for example, Figure 1 In the recording device 100 shown, the carriage 32 is moved in a direction parallel to the X-axis direction relative to the sheet S stopped on the upper surface of the paper plate 30, while the white ink composition is ejected from the nozzle N of the inkjet head 35 onto the surface of the sheet S. The position of the sheet S can be moved by conveying the sheet S when the inkjet head is not scanning, but the position of the sheet S does not move during scanning, so the position is fixed. The position being fixed means that the position does not move as described above.
[0118] Furthermore, the recording medium whose position is fixed may be further sucked onto a platen or held by a roller or the like in order to prevent it from floating.
[0119] In addition, the white ink attachment process of the recording method involved in the present embodiment is a process of attaching a white ink composition to a scanning area of a single scan by a single scan. In a serial recording method, it is also possible to attach one ink separately in a scanning area of a medium to which ink can be attached in a single main scan by two or more main scans, but in this case, the number of main scans required for recording increases and the recording speed slows down. In contrast, in the white ink attachment process of the recording method involved in the present embodiment, the white ink composition is completely attached to the scanning area of the medium to which the white ink composition can be attached in a single main scan by a single main scan (the white ink composition is not attached to the same scanning area by two or more main scans), thereby increasing the recording speed. In addition, the scanning area of a single scan refers to the area on the recording medium where the inkjet head moves when the inkjet head performs a single scan. It is a rectangular area with a longitudinal length of the length of the inkjet head and a lateral length of the scanning distance. The length of the inkjet head is the length of the nozzle array of the inkjet head.
[0120] For the scanning area of this one scan, the scanning of the white ink adhesion process is performed only once, and the scanning of the non-white ink adhesion process is performed only once.
[0121] In addition, when one ink is attached separately by two or more main scans, the vapor concentration on the recording medium is low, and the vapor diffuses between two or more main scans, so it is difficult to cause condensation on the nozzle surface. In addition, the so-called line recording method in which the ink attachment process is performed while the recording medium is transported is a method in which the ink is attached by a single scan, but in the line recording method, the recording medium is continuously transported without stopping, and the ink attached part immediately moves to the downstream side of the inkjet head, so the vapor does not stay near the inkjet head, and it is difficult to cause condensation.
[0122] In the recording method according to the present embodiment, the distance that the inkjet head moves relative to the recording medium in the above-mentioned one scan in the white ink attaching step and the non-white ink attaching step described later is preferably 0.3 m or more, more preferably 0.5 m or more, further preferably 1.0 m or more, further preferably 1.5 m or more, and particularly preferably 2.0 m or more. When the distance is greater than the above range, it is useful because it is possible to record a wide recorded object.
[0123] On the other hand, in the case of condensation on the nozzle surface, the longer the distance for the main scan, the more opportunities the nozzle surface is exposed to the steam, so condensation is more likely to occur. According to the recording method involved in this embodiment, the distance is particularly greater than 0.5 m, so there is a tendency that condensation can be well suppressed even in the case where the nozzle surface is more likely to be exposed to the steam and condensation is more likely to occur.
[0124] On the other hand, the upper limit of the distance is preferably 7.0 m or less, preferably 5.0 m or less, more preferably 4.0 m or less, and further preferably 3.0 m or less. Furthermore, it is preferably 2.0 m or less, further preferably 1.8 m or less, and further preferably 1.0 m or less. When the upper limit of the distance is below the above range, condensation reduction is more excellent, which is preferred.
[0125] In addition, "the distance that the inkjet head moves relative to the recording medium in one scan" is, for example, the distance when scanning from end to end (from one end to the other end) of the recording medium in one scan. Or, it is the distance when scanning from end to end (from one end to the other end) of the maximum recordable area of the recording medium in one scan.
[0126] The process order of the white ink attachment process and the non-white ink attachment process described later is not particularly limited. The white ink attachment process may be performed first and then the non-white ink attachment process, or the non-white ink attachment process may be performed first and then the white ink attachment process. Printing based on the former order (front white printing) is suitable for observing the printed matter from the side where the image is printed. In addition, printing based on the latter order (back white printing) is suitable for observing the printed matter from the back side of the recording medium (especially transparent film, etc.). In addition, condensation on the nozzle surface is a problem that occurs regardless of the above process order.
[0127] In the recording method involved in this embodiment, for the scanning area where the scanning of either one of the white ink attachment process and the non-white ink attachment process described later is performed, the scanning of the other side is performed by another scanning. In this way, the subsequent ink composition can be attached by the scanning of the other side so as to overlap with the previous ink composition attached by the scanning of one side. In this way, a layer formed by white ink called a base layer that conceals the background and a layer formed by color ink that forms a predetermined image can be printed in a stacked manner, so that even if the recording medium is transparent, the visual recognition of the color image can be improved.
[0128] In the recording method according to the present embodiment, the maximum adhesion amount of the ink composition in the first step of the white ink adhesion step and the non-white ink adhesion step described later is preferably within a range of 5 mg / inch.2 More preferably 8 mg / inch 2 More preferably, 10 mg / inch 2 More preferably, 12 mg / inch 2 Above, particularly preferably 14 mg / inch 2 In this case, the color development property of the image produced by the ink is particularly excellent, which is preferable.
[0129] The upper limit of the maximum adhesion amount is not particularly limited, but is preferably 25 mg / inch 2 Below, more preferably 23 mg / inch 2 Below, more preferably 20 mg / inch 2 Below, particularly preferably 18 mg / inch 2 In addition, regardless of the order of the steps, it is also preferred that the range of the maximum adhesion amount of the white ink composition in the white ink adhesion step is set to the above range. In addition, the range of the maximum adhesion amount of the ink composition in the subsequent steps of the white ink adhesion step and the non-white ink adhesion step may also be set to the above range.
[0130] It is speculated that the condensation on the nozzle surface is caused by the fact that the solvent component of the ink attached to the recording medium in the previous process evaporates in large quantities at once, and the vapor concentration on the recording medium becomes high, and the solvent component of the previous ink after evaporation is affected during the main scan for attaching the next ink. According to the recording method involved in this embodiment, the range of the maximum attachment amount is particularly 8 mg / inch 2 As described above, there is a tendency that condensation can be suppressed well even when the vapor concentration becomes higher and condensation is more likely to occur.
[0131] In addition, the maximum adhesion amount of the ink composition in the subsequent step of the white ink adhesion step and the non-white ink adhesion step described later is preferably smaller than the maximum adhesion amount of the ink composition in the previous step, and more preferably 1 mg / inch smaller. 2 More than, preferably less than 5mg / inch 2 Above, preferably less than 8mg / inch 2 Above, especially preferably less than 11 mg / inch 2 above.
[0132] In the recording method according to the present embodiment, in the white ink attaching step and the non-white ink attaching step described later, the maximum weight range of each droplet of the white ink composition and the non-white ink composition is preferably 0.5 to 20 ng, preferably 0.5 to 15 ng, more preferably 1 to 15 ng, further preferably 3 to 15 ng, further preferably 5 to 15 ng, and particularly preferably 6 to 13 ng. When the maximum weight range of each droplet of each ink composition is within the above range, the droplets are relatively small and thus easily evaporated and condensation is more likely to occur. However, according to the recording method according to the present embodiment, there is a tendency that condensation can be well suppressed even in such a case.
[0133] From the same viewpoint, the maximum weight of each droplet of the white ink composition in the white ink attaching step is preferably in the range of 5 to 20 ng, more preferably 7 to 18 ng, further preferably 9 to 16 ng, and particularly preferably 10 to 15 ng.
[0134] In addition, the maximum weight range of each drop of the ink composition of the first step in the white ink attachment step and the non-white ink attachment step described later may be set to the above range. Due to the vapor generated by the ink composition of the first attachment step, there is a tendency for condensation to occur in the attachment step performed later. When the maximum weight range of each drop of the ink composition of the first step is set to the above range, the recording method of this embodiment is particularly useful.
[0135] In general, if the maximum weight range of each drop of ink droplet is small, the density of ink droplets per recording unit area increases, so the recording resolution becomes higher. In addition, the recording resolution is proportional to the nozzle density. That is, if the amount of ink attached is the same, the side with a higher nozzle density is more likely to produce condensation.
[0136] Therefore, from the viewpoint of being able to further enjoy the effect of the present invention that condensation can be well suppressed, the nozzle density of the inkjet head used in the recording method involved in this embodiment is preferably 600 dpi or more, more preferably 800 dpi or more, more preferably 1000 dpi or more, and particularly preferably 1200 dpi or more. The upper limit of the nozzle density is preferably 2400 dpi or less, more preferably 2000 dpi or less, and even more preferably 1600 dpi or less.
[0137] The recording resolution is preferably 600×600 dpi or higher, more preferably 800×800 dpi or higher, further preferably 1000×1000 dpi or higher, and particularly preferably 1200×1200 dpi or higher.
[0138] In the recording method according to the present embodiment, the surface temperature of the recording medium in the white ink attaching step and the non-white ink attaching step described later is 35° C. or less. When recording is performed by attaching white ink and color ink by one main scan in a scanning area of the medium to which ink can be attached in one main scan, condensation occurs on the nozzle surface and the ink ejection stability is reduced due to the condensation. Therefore, in the process of attaching each ink, by setting the medium temperature to a low temperature below a predetermined temperature, the evaporation of the solvent component of the ink can be suppressed, and the temperature difference between the nozzle surface and the vicinity of the platen can be suppressed to be low, thereby reducing condensation.
[0139] The surface temperature of the recording medium in the white ink attachment process and the non-white ink attachment process described later is 35°C or less, but preferably 33°C or less, more preferably 31°C or less, further preferably 29°C or less, and particularly preferably 27°C or less. The lower limit of the surface temperature is not particularly limited, but is preferably 5°C or more, more preferably 10°C or more. It is further preferably 15°C or more, and particularly preferably 20°C or more. If the surface temperature is below the above range, condensation can be further reduced, which is preferred. In addition, if the surface temperature is above the above range, the image quality is better, which is preferred.
[0140] This temperature is the surface temperature of the portion of the recording surface of the recording medium to which the liquid adheres during the adhesion process, and is the highest temperature in the adhesion process in the recording area.
[0141] In the white ink attaching step and the non-white ink attaching step, a primary heating step may or may not be performed. The primary heating step is a step of heating the recording medium by a primary heating mechanism at a position to which the ink composition is attached in the white ink attaching step and the non-white ink attaching step. The primary heating mechanism is a heating mechanism for heating the recording medium, a heating mechanism for heating the recording medium from above, etc., which is provided on a member supporting the recording medium at a position to which the ink composition is attached.
[0142] Even when the heating step is performed once, the surface temperature of the recording medium in the white ink attaching step and the non-white ink attaching step is set to 35° C. or less.
[0143] Regardless of whether the primary heating step is not performed or the recording medium is heated by heat generated by recording device components other than the primary heating mechanism, the surface temperature at the location to which the ink composition adheres is set to 35° C. or less.
[0144] 1.2.2 White ink composition
[0145] Hereinafter, each component contained in the white ink composition used in the white ink adhesion step will be described.
[0146] White color material
[0147] The white ink composition used in the recording method according to the present embodiment contains a white color material. Examples of the white color material include metal compounds such as metal oxides, barium sulfate, and calcium carbonate. Examples of the metal oxide include titanium dioxide, zinc oxide, silicon dioxide, aluminum oxide, and magnesium oxide. In addition, the white color material may also include particles having a hollow structure, and known particles may be used as the particles having a hollow structure.
[0148] As the white color material, titanium dioxide is particularly preferably used from the viewpoint of good whiteness and abrasion resistance among the above examples. The white color material may be used alone or in combination of two or more.
[0149] The volume-based average particle size (D50) of the white color material (also referred to as "volume average particle size") is preferably 30.0 nm to 600.0 nm, more preferably 100.0 nm to 500.0 nm, and further preferably 150.0 nm to 400.0 nm. If the volume average particle size of the white color material is within the above range, the particles are difficult to settle, and the dispersion stability can be good. In addition, when applied to an inkjet recording device, it is not easy to cause nozzle clogging, etc. In addition, if the volume average particle size of the white color material is within the range, it can be very helpful to improve the visual recognition of the image.
[0150] The volume average particle size of the white color material can be measured by a particle size distribution measuring device. As a particle size distribution measuring device, for example, a particle size distribution meter (for example, "Nanotrac series", manufactured by Microtrac BEL) based on the dynamic light scattering method can be cited. The volume average particle size is set to D50 value.
[0151] In addition, in this specification, the term "white" when referring to a white ink composition, a white color material, etc. does not refer only to pure white, but also includes colors colored with chromatic or achromatic colors, and glossy colors as long as they can be visually recognized as white. In addition, it includes the names of inks and pigments that make it appear that they are white, the names of white pigments, and compositions sold.
[0152] More quantitatively, “white” includes not only a color having an L* of 100 in a recorded matter, for example, CIELAB, but also a color having an L* of 60 or more and 100 or less, and a* and b* of ±10 or less, respectively.
[0153] More specifically, for example, the white ink composition is preferably a composition that, when recording is performed on the surface of a transparent film recording medium with the ink in an amount sufficient to cover the surface, the lightness (L*) and chromaticity (a*, b*) of the recorded portion of the recorded object are within the above ranges when the color is measured using a spectrophotometer based on CIELAB. The recorded object recorded in an amount sufficient to cover the surface of the transparent film recording medium is, for example, 15 mg / inch. 2 The adhesion amount is preferably 80≤L*≤100, -4.5≤a*≤2, -10≤b*≤2.5. As a recording medium made of a transparent film, for example, LAGJet E-1000ZC (manufactured by Lintec) can be cited. As a spectrophotometer based on CIELAB, for example, Spectrolino (trade name, manufactured by GretagMacbeth) can be cited, and the measurement conditions are set to D50 light source, the observation field is set to 2°, the concentration is set to DIN NB, the white reference is set to Abs, the filter is set to No, and the measurement mode is set to Reflectance for measurement.
[0154] Typical examples of white colorants include titanium dioxide, such as Tipaque CR-50-2, CR-57, CR-58-2, CR-60-2, CR-60-3, CR-Super-70, CR-90-2, CR-95, CR953, PC-3, PF-690, PF-691, PF-699, PF-711, PF-728, PF-736, PF-737, PF-739, PF-740, PF-742, R-980, UT-717 (all manufactured by Ishihara Sangyo Co., Ltd.), etc.
[0155] The content (solid content) of the white color material in the white ink composition is preferably 0.5% by mass or more and 20.0% by mass or less, more preferably 1.0% by mass or more and 20.0% by mass or less, further preferably 3.0% by mass or more and 15.0% by mass or less, and further preferably 7.0% by mass or more and 12.0% by mass or less, relative to the total mass of the white ink composition. If the content of the white color material is within the above range, a sufficiently visually recognizable image can be obtained.
[0156] In the recording method involved in the present embodiment, the white color material has the function of concealing the background of the image and improving the visual recognition of the obtained image. When the content of the white color material in the white ink composition is used for the purpose of improving the visual recognition of the image, it can be reduced compared with the case where the background is concealed. Therefore, when the white ink composition is used for the purpose of improving the visual recognition of the image, sufficient visual recognition of the image can be obtained, and it is easy to make the dispersion stability of the white color material good and difficult to settle. From such a viewpoint, the upper limit of the content of the white color material in the white ink composition is preferably the above range, preferably 10.0 mass % or less.
[0157] The white color material is preferably able to be stably dispersed in the dispersion medium, and a dispersant can be used to disperse it. As the dispersant, a resin dispersant can be cited, and it is selected from dispersants that can make the dispersion stability of the white color material in the white ink composition containing the above-mentioned white color material good. In addition, the white color material can also be used as a self-dispersible pigment by oxidizing or sulfonating the pigment surface with, for example, ozone, hypochlorous acid, fuming sulfuric acid, etc. to modify the surface of the pigment particles.
[0158] Examples of the resin dispersant (dispersant resin) include (meth)acrylic acid resins and salts thereof such as poly(meth)acrylic acid, (meth)acrylic acid-acrylonitrile copolymers, (meth)acrylic acid-(meth)acrylic ester copolymers, vinyl acetate-(meth)acrylic ester copolymers, vinyl acetate-(meth)acrylic acid copolymers, and vinylnaphthalene-(meth)acrylic acid copolymers; styrene resins and salts thereof such as styrene-(meth)acrylic acid copolymers, styrene-(meth)acrylic acid-(meth)acrylic ester copolymers, styrene-α-methylstyrene-(meth)acrylic acid copolymers, styrene-α-methylstyrene-(meth)acrylic acid-(meth)acrylic ester copolymers, styrene-maleic acid copolymers, and styrene-maleic anhydride copolymers; urethane resins and salts thereof, which are polymer compounds (resins) containing urethane bonds formed by the reaction of an isocyanate group and a hydroxyl group, and may be linear and / or branched, and may or may not have a crosslinked structure; polyvinyl alcohols; vinylnaphthalene-maleic acid copolymers and salts thereof; vinyl acetate-maleic acid ester copolymers and salts thereof; and water-soluble resins such as vinyl acetate-crotonic acid copolymers and salts thereof. Among them, copolymers of monomers having hydrophobic functional groups and monomers having hydrophilic functional groups, and polymers composed of monomers having both hydrophobic functional groups and hydrophilic functional groups are preferred. As the form of the copolymer, any form among random copolymers, block copolymers, alternating copolymers, and graft copolymers can be used.
[0159] Commercially available products of styrene-based resin dispersants include, for example, X-200, X-1, X-205, X-220, and X-228 (manufactured by Seikyo PMC Co., Ltd.); Nopcosperse (registered trademark) 6100 and 6110 (manufactured by San Nopco Co., Ltd.); Joncryl 67, 586, 611, 678, 680, 682, and 819 (manufactured by BASF); DISPERBYK-190 (manufactured by BYK Chemie Japan Co., Ltd.); N-EA137, N-EA157, N-EA167, N-EA177, N-EA197D, N-EA207D, and E-EN10 (manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.);
[0160] In addition, commercially available products of acrylic resin dispersants include BYK-187, BYK-190, BYK-191, BYK-194N, BYK-199 (manufactured by BYK Chemie Co., Ltd.); Aron A-210, A6114, AS-1100, AS-1800, A-30SL, A-7250, CL-2 (manufactured by Toagosei Co., Ltd.), etc.
[0161] Further, commercially available products of the urethane resin dispersant include BYK-182, BYK-183, BYK-184, BYK-185 (manufactured by BYK Chemie Co., Ltd.), TEGO Disperse 710 (manufactured by Evonic Tego Chemi Co., Ltd.), and Borchi (registered trademark) Gen 1350 (manufactured by OMG Borschers Co., Ltd.).
[0162] Dispersant can be used alone or in combination of two or more. The total content of the dispersant is preferably 0.2 mass parts or more and 60 mass parts or less relative to 100 mass parts of white color material, more preferably 1 mass parts or more and 50 mass parts or less, further preferably 5 mass parts or more and 55 mass parts or less, further preferably 10 mass parts or more and 50 mass parts or less, particularly preferably 20 mass parts or more and 40 mass parts or less. By making the content of the dispersant 0.2 mass parts or more relative to 100 mass parts of white color material, the dispersion stability of the white color material can be further improved. In addition, if the content of the dispersant is 60 mass parts or less relative to 100 mass parts of white color material, the viscosity of the obtained dispersion can be suppressed to be smaller.
[0163] Among the dispersants exemplified above, at least one selected from anionic dispersant resins is more preferred. In this case, the weight average molecular weight of the dispersant is more preferably 500 or more. Further, it is preferably 5000 or more and 100000 or less, and more preferably 10000 or more and 50000 or less.
[0164] By using such a resin dispersant as a dispersant, the dispersion and aggregation of the white pigment are improved, and an image with better dispersion stability and better image quality can be obtained. In addition, it is easy to increase the viscosity increase rate of the white ink composition to 5 times or more, which is preferred.
[0165] Anionic dispersant resins are resins having anionic functional groups and exhibiting anionic properties. Examples of anionic functional groups include carboxyl groups, sulfonyl groups, and phosphoric acid groups. Among these groups, carboxyl groups are more preferred.
[0166] The dispersant resin preferably has an acid value, and the acid value is preferably 5 mgKOH / g or more, more preferably 10 to 200 mgKOH / g, and further preferably 15 to 150 mgKOH / g. Also, it is preferably 20 to 100 mgKOH / g, and further preferably 25 to 70 mgKOH / g. In this case, it is easy to make the viscosity increase rate of the white ink composition described later 5 times or more, so it is preferred.
[0167] The acid value can be measured by neutralization potentiometric titration in accordance with JIS K 0070. As a titration apparatus, for example, "AT610" manufactured by Kyoto Electronics Industry Co., Ltd. can be used.
[0168] water
[0169] The white ink composition used in the recording method of the present embodiment is an aqueous ink, preferably containing water. "Aqueous" means containing at least water as a solvent component, and may also contain water as a main solvent component. As water, for example, pure water such as ion exchange water, ultrafiltration water, reverse osmosis water, and distilled water, and water with reduced ionic impurities such as ultrapure water can be cited. In addition, when water sterilized by ultraviolet irradiation or addition of hydrogen peroxide is used, the generation of bacteria and fungi can be suppressed when the white ink composition is stored for a long time.
[0170] The content of water in the liquid medium component is preferably 30% by mass or more, more preferably 30 to 99% by mass. Further, it is preferably 30 to 95% by mass, more preferably 40 to 90% by mass, and even more preferably 50 to 80% by mass. In addition, the liquid medium refers to a solvent component such as water or an organic solvent.
[0171] In addition, the water content is preferably 30% by mass or more, more preferably 40% by mass or more, more preferably 45% by mass or more, and particularly preferably 50% by mass or more, relative to the total mass of the white ink composition. The upper limit of the water content is not particularly limited, but, for example, is preferably 99% by mass or less, further preferably 90% by mass or less, more preferably 80% by mass or less, and further preferably 70% by mass or less, relative to the total mass of the ink composition.
[0172] When the water content is below the above range, condensation reduction is more excellent, which is preferred. On the other hand, when the water content is above the above range, the freedom of ink design is high. Even in this case, the recording method according to this embodiment can achieve excellent condensation reduction, which is useful.
[0173] Furthermore, from the above viewpoint, it is also preferred that the water content of the ink composition to be deposited first in the white ink composition and the non-white ink composition described later be within the above range.
[0174] Organic solvents
[0175] The white ink composition used in the recording method of the present embodiment may contain an organic solvent. The organic solvent is preferably water-soluble. One of the functions of the organic solvent is to increase the wettability of the white ink composition to the recording medium or to increase the moisture retention of the white ink composition. In addition, the organic solvent can also function as a penetrant.
[0176] Examples of organic solvents include esters, alkylene glycol ethers, cyclic esters, nitrogen-containing solvents, polyhydric alcohols, etc. Examples of nitrogen-containing solvents include cyclic amides, non-cyclic amides, etc. Examples of non-cyclic amides include alkoxyalkylamides, etc.
[0177] Examples of the esters include glycol monoacetates such as ethylene glycol monomethyl ether acetate, ethylene glycol monoethyl ether acetate, and ethylene glycol monobutyl ether acetate; and glycol diesters such as ethylene glycol diacetate, diethylene glycol diacetate, and propylene glycol diacetate.
[0178] The alkylene glycol ethers may be monoethers or diethers of alkylene glycol, and alkyl ethers are preferred. Specific examples include alkylene glycol monoalkyl ethers such as ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, ethylene glycol monoisopropyl ether, ethylene glycol monobutyl ether, and diethylene glycol monomethyl ether, and alkylene glycol dialkyl ethers such as ethylene glycol dimethyl ether, ethylene glycol diethyl ether, ethylene glycol dibutyl ether, diethylene glycol dimethyl ether, and diethylene glycol diethyl ether.
[0179] Examples of the cyclic esters include cyclic esters (lactones) such as β-propiolactone, γ-butyrolactone, δ-valerolactone, ε-caprolactone, and β-butyrolactone, and compounds in which the hydrogen atoms of the methylene groups adjacent to the carbonyl groups thereof are substituted with alkyl groups having 1 to 4 carbon atoms.
[0180] Examples of the alkoxyalkylamides include 3-methoxy-N,N-dimethylpropionamide, 3-methoxy-N,N-diethylpropionamide, 3-methoxy-N,N-methylethylpropionamide, 3-ethoxy-N,N-dimethylpropionamide, 3-ethoxy-N,N-diethylpropionamide, 3-ethoxy-N,N-methylethylpropionamide, 3-n-butoxy-N,N-dimethylpropionamide, 3-n-butoxy-N,N-diethylpropionamide, and 3-n-butoxy-N,N-methylethylpropionamide.
[0181] Examples of cyclic amides include lactams, such as pyrrolidones such as 2-pyrrolidone, 1-methyl-2-pyrrolidone, 1-ethyl-2-pyrrolidone, 1-propyl-2-pyrrolidone, and 1-butyl-2-pyrrolidone. These are preferred in terms of promoting the solubility of the coagulant and the film formation of the resin particles described later. 2-pyrrolidone is particularly preferred.
[0182] As the alkoxyalkylamides, compounds represented by the following general formula (1) are also preferably used.
[0183] R 1 -O-CH2CH2-(C=O)-NR 2 R 3 ……(1)
[0184] In the above formula (1), R 1 represents an alkyl group having 1 to 4 carbon atoms, R 2 and R 3 Each independently represents a methyl group or an ethyl group. The "alkyl group having a carbon number of 1 or more and 4 or less" can be a linear or branched alkyl group, for example, a methyl group, an ethyl group, an n-propyl group, an isopropyl group, an n-butyl group, a sec-butyl group, an isobutyl group, or a tert-butyl group. The compound represented by the above formula (1) can be used alone or in combination of two or more.
[0185] As a function of the nitrogen-containing solvent, for example, it is possible to improve the surface drying and fixing properties of the white ink composition attached to the low-absorption recording medium. In particular, the compound represented by the above formula (1) is excellent in the effect of moderately softening and dissolving the vinyl chloride resin. Therefore, the compound represented by the above formula (1) can soften and dissolve the recording surface containing the vinyl chloride resin, so that the white ink composition can penetrate into the interior of the low-absorption recording medium. By the white ink composition penetrating into the low-absorption recording medium in this way, the white ink composition is firmly fixed, and the surface of the white ink composition becomes easy to dry. Therefore, the obtained image is easy to become an image with excellent surface drying and fixing properties.
[0186] The content of the nitrogen-containing solvent is not particularly limited to about 5% by mass and about 50% by mass, preferably about 10% by mass and about 30% by mass, relative to the total mass of the white ink composition. By making the content within the above range, the fixability and surface drying property of the image (especially the surface drying property when recording under a high temperature and high humidity environment) can sometimes be further improved.
[0187] Examples of the polyhydric alcohol include 1,2-alkanediols (e.g., ethylene glycol, propylene glycol (also known as propane-1,2-diol), 1,2-butanediol, 1,2-pentanediol, 1,2-hexanediol, 1,2-heptanediol, 1,2-octanediol and other alkanediols), polyhydric alcohols other than 1,2-alkanediol (polyhydric alcohols) (e.g., diethylene glycol, dipropylene glycol, 1,3-propanediol, 1,3-butanediol (also known as 1,3-butylene glycol) , 1,4-butanediol, 1,5-pentanediol, 1,6-hexanediol, 2-ethyl-2-methyl-1,3-propanediol, 2-methyl-2-propyl-1,3-propanediol, 2-methyl-1,3-propanediol, 2,2-dimethyl-1,3-propanediol, 3-methyl-1,3-butanediol, 2-ethyl-1,3-hexanediol, 3-methyl-1,5-pentanediol, 2-methylpentane-2,4-diol, trimethylolpropane, glycerol, etc.) and the like.
[0188] Examples of polyhydric alcohols include alkanediols and polyols. Alkanediols are diols of alkanes having 5 or more carbon atoms. The carbon number of the alkane is preferably 5 to 15, more preferably 6 to 10, and even more preferably 6 to 8. 1,2-alkanediol is preferred.
[0189] The polyol is an intermolecular condensate between hydroxyl groups of a polyol of an alkane having 4 or less carbon atoms or a polyol of an alkane having 4 or less carbon atoms. The carbon number of the alkane is preferably 2 to 3. The number of hydroxyl groups in the molecule of the polyol is 2 or more, preferably 5 or less, and more preferably 3 or less. When the polyol is the above-mentioned intermolecular condensate, the number of intermolecular condensation is 2 or more, preferably 4 or less, and more preferably 3 or less. The polyhydric alcohols can be used alone or in combination of two or more.
[0190] Alkanediols and polyols can function mainly as penetrating solvents and / or moisturizing solvents. However, alkanediols tend to have a strong property as penetrating solvents, and polyols tend to have a strong property as moisturizing solvents.
[0191] When the white ink composition contains an organic solvent, one organic solvent may be used alone or two or more organic solvents may be used in combination. In addition, the total content of the organic solvent relative to the total mass of the white ink composition is, for example, 5% by mass or more and 50% by mass or less, preferably 10% by mass or more and 45% by mass or less, more preferably 15% by mass or more and 40% by mass or less, and further preferably 20% by mass or more and 40% by mass or less. By making the content of the organic solvent within the above range, the balance between the wettability and the drying property is further improved, and it is easy to form a higher-quality image.
[0192] The white ink composition preferably contains an organic solvent having a normal boiling point of 150 to 280° C. among the organic solvents exemplified above. The normal boiling point of the organic solvent is more preferably 160 to 270° C., further preferably 170 to 260° C., and particularly preferably 180 to 250° C. In addition, the content of the organic solvent is preferably 10 to 50% by mass, more preferably 20 to 40% by mass, and further preferably 25 to 35% by mass relative to the total mass of the white ink composition.
[0193] The white ink composition preferably contains an alkane polyol organic solvent having a normal boiling point exceeding 280° C. in an amount of not more than 2% by mass, more preferably not more than 1.5% by mass, further preferably not more than 1.0% by mass, still further preferably not more than 0.5% by mass, and particularly preferably not more than 0.1% by mass, relative to the total mass of the white ink composition. The lower limit of the content of the alkane polyol organic solvent having a normal boiling point exceeding 280° C. may be 0% by mass.
[0194] This improves drying of the formed image, enables faster recording, and improves adhesion to the recording medium. In addition, the white ink composition preferably contains an organic solvent (not limited to polyols) having a normal boiling point exceeding 280.0°C within the above range.
[0195] Resin particles
[0196] The white ink composition used in the recording method of the present embodiment may contain resin particles. The resin particles can further improve the adhesion of the image formed by the white ink composition attached to the recording medium. As resin particles, for example, resin particles composed of urethane resins, acrylic resins (including styrene acrylic resins), fluorene resins, polyolefin resins, rosin-modified resins, terpene resins, polyester resins, polyamide resins, epoxy resins, vinyl chloride resins, vinyl chloride-vinyl acetate copolymers, ethylene vinyl acetate resins, etc. can be cited. Among them, urethane resins, acrylic resins, polyolefin resins, and polyester resins are preferred. These resin particles are mostly processed in the form of emulsions, but can also be in the form of powders. In addition, the resin particles can be used alone or in combination of two or more.
[0197] Urethane resin is a general term for resins having urethane bonds. As urethane resins, polyether urethane resins having ether bonds in the main chain in addition to urethane bonds, polyester urethane resins having ester bonds in the main chain in addition to urethane bonds, polycarbonate urethane resins having carbonate bonds in the main chain in addition to urethane bonds, etc. can be used. In addition, as the urethane resin, commercially available products can be used, for example, SUPERFLEX 460, 460s, 840, E-4000 (trade names, manufactured by Dai-ichi Kogyo Seiyaku Co., Ltd.), Resamine D-1060, D-2020, D-4080, D-4200, D-6300, D-6455 (trade names, manufactured by Dainichi Seika Industries, Ltd.), Takelac WS-6021, W-512-A-6 (trade names, manufactured by Mitsui Chemicals Polyurethanes, Ltd.), SunCure 2710 (trade name, manufactured by LUBRIZOL), Permarin UA-150 (trade name, manufactured by Sanyo Chemical Industries, Ltd.) and the like can be used.
[0198] Acrylic resin is a general term for polymers obtained by polymerizing at least acrylic monomers such as (meth)acrylic acid and (meth)acrylate as one component, and examples thereof include resins obtained from acrylic monomers, copolymers of acrylic monomers and other monomers, etc. For example, acrylic-vinyl resins, which are copolymers of acrylic monomers and vinyl monomers, etc., can be mentioned. In addition, for example, as vinyl monomers, styrene, etc. can be mentioned.
[0199] As acrylic monomers, acrylamide, acrylonitrile, etc. can also be used. For the resin emulsion using acrylic resin as raw material, commercial products can be used, for example, FK-854 (trade name, manufactured by Chuo Rika Kogyo Co., Ltd.), Mowinyl 952B, 718A (trade name, manufactured by Nippon Synthetic Chemical Industry Co., Ltd.), Nipol LX852, LX874 (trade name, manufactured by Nippon Zeon Co., Ltd.), etc. can be selected for use.
[0200] In addition, in this specification, the acrylic resin may be a styrene-acrylic resin described later. In addition, in this specification, the expression "(meth)acrylic group" means an acrylic group or a methacrylic group.
[0201] Styrene acrylic resins are copolymers obtained from styrene monomers and (meth)acrylic monomers, and examples thereof include styrene-acrylic acid copolymers, styrene-methacrylic acid copolymers, styrene-methacrylic acid-acrylate copolymers, styrene-α-methylstyrene-acrylic acid copolymers, and styrene-α-methylstyrene-acrylic acid-acrylate copolymers. As the styrene-acrylic resin, commercially available products can be used, for example, Joncryl 62J, 7100, 390, 711, 511, 7001, 632, 741, 450, 840, 74J, HRC-1645J, 734, 852, 7600, 775, 537J, 1535, PDX-7630A, 352J, 352D, PDX-7145, 538J, 7640, 7641, 631, 790, 780, 7610 (trade names, manufactured by BASF), Mowinyl 966A, 975N (trade names, manufactured by Nippon Synthetic Chemical Industry Co., Ltd.), Vinyblan 2586 (manufactured by Nissin Chemical Industry Co., Ltd.), etc. can be used.
[0202] The polyolefin resin is a resin having olefins such as ethylene, propylene, and butene in the structural skeleton, and known resins can be appropriately selected for use. As the olefin resin, commercially available products can be used, for example, ArrowBase CB-1200 and CD-1200 (trade names, manufactured by Unitika Co., Ltd.) can be used.
[0203] The glass transition temperature (Tg) of the resin particles is preferably above -50°C and below 200°C, more preferably above 0°C and below 150°C, and further preferably above 50°C and below 100°C. In addition, it is particularly preferably above 50°C and below 80°C. By making the glass transition temperature (Tg) of the resin particles within the above range, there is a tendency for better durability and clogging resistance. The glass transition temperature is measured, for example, using a differential scanning calorimeter "DSC7000" manufactured by Hitachi High-Tech Sciences, Ltd. in accordance with JIS K7121 (Method for Determination of Transition Temperature of Plastics).
[0204] The volume average particle size of the resin particles is preferably 10 nm to 300 nm, more preferably 30 nm to 300 nm, further preferably 30 nm to 250 nm, particularly preferably 40 nm to 220 nm. The volume average particle size can be measured by the above-mentioned method.
[0205] The acid value of the resin of the resin particles is preferably 50 mgKOH / g or less, more preferably 30 mgKOH / g or less, further preferably 20 mgKOH / g or less, and particularly preferably 10 mgKOH / g or less. In addition, the lower limit of the acid value is 0 mgKOH / g or more, preferably 5 mgKOH / g or more, and more preferably 10 mgKOH / g or more. In this case, the image quality is excellent and preferred. The acid value can be measured by the above method.
[0206] When the resin particles are contained in the white ink composition, the content thereof is 0.1% by mass to 20% by mass, preferably 1% by mass to 15% by mass, more preferably 2% by mass to 10% by mass, and particularly preferably 3% by mass to 7% by mass, based on the solid content of the total mass of the white ink composition.
[0207] wax
[0208] The white ink composition used in the recording method according to the present embodiment may contain wax. The wax has a function of providing lubrication to the image formed by the white ink composition, and thus can reduce peeling of the image formed by the white ink composition.
[0209] As the components constituting the wax, for example, plant and animal waxes such as carnauba wax, candelilla wax, beeswax, rice bran wax, and lanolin can be used alone or in combination of multiple types; petroleum waxes such as paraffin wax, microcrystalline wax, polyethylene wax, oxidized polyethylene wax, and petrolatum; mineral waxes such as montan wax and ozokerite; synthetic waxes such as carbowax, Hoechst wax, polyolefin wax, and stearic acid amide; natural and synthetic wax emulsions or composite waxes such as α-olefin maleic anhydride copolymers, etc. Among them, polyolefin waxes (particularly polyethylene wax and polypropylene wax) and paraffin wax are preferably used from the viewpoint of having a more excellent effect of improving the fixing property of the ink.
[0210] As the wax, commercially available products may be used, for example, Nopcote PEM-17 (trade name, manufactured by San Nopco Co., Ltd.), Chemipearl W4005 (trade name, manufactured by Mitsui Chemicals, Inc.), AQUACER 515, 539, 593 (these are trade names, manufactured by BYK Chemie Japan Co., Ltd.), etc.
[0211] In addition, when the recording method includes a heating step, etc., from the viewpoint of suppressing excessive melting of the wax and deterioration of its performance, it is preferred to use a wax having a melting point of preferably 50°C to 200°C, more preferably 70°C to 180°C, and further preferably 90°C to 150°C.
[0212] The wax may be supplied in the form of an emulsion or a suspension. The wax content is 0.1% by mass or more and 10% by mass or less, more preferably 0.5% by mass or more and 5% by mass or less, and further preferably 0.5% by mass or more and 2% by mass or less, relative to the total mass of the white ink composition, in terms of solid content. If the wax content is within the above range, the function of the wax can be well exerted. In addition, if one or both of the white ink composition and the non-white ink composition described later contain wax, the function of providing lubrication to the image can be fully obtained.
[0213] Surfactants
[0214] The white ink composition used in the recording method according to the present embodiment may contain a surfactant. The surfactant has the function of adjusting the surface tension of the white ink composition and adjusting, for example, wettability with the recording medium. Among the surfactants, for example, acetylene glycol surfactants, silicone surfactants, and fluorine surfactants can be preferably used.
[0215] The acetylene glycol surfactant is not particularly limited, and examples thereof include Surfynol 104, 104E, 104H, 104A, 104BC, 104DPM, 104PA, 104PG-50, 104S, 420, 440, 465, 485, SE, SE-F, 504, 61, DF37, CT111, CT121, CT131, CT136, TG, GA, and DF110D (all of the above are trade names, manufactured by Air Products & Chemicals Co., Ltd.); Olfine B, Y, P, A, STG, SPC, E1004, E1010, PD-001, PD-002W, PD-003, PD-004, EXP.4001, EXP.4036, EXP.4051, AF-103, AF-104, AK-02, SK-14, AE-3 (all of the above are trade names, manufactured by Nissin Chemical Industry Co., Ltd.); Acetylenol E00, E00P, E40, E100 (all of the above are trade names, manufactured by Kawakami Fine Chemical Co., Ltd.).
[0216] The silicone surfactant is not particularly limited, but preferably a polysiloxane compound. The polysiloxane compound is not particularly limited, and examples thereof include polyether-modified silicone. Commercially available products of the polyether-modified silicone include BYK-306, BYK-307, BYK-333, BYK-341, BYK-345, BYK-346, and BYK-348 (these are trade names, BYK Chemie·Japan Co., Ltd.); KF-351A, KF-352A, KF-353, KF-354L, KF-355A, KF-615A, KF-945, KF-640, KF-642, KF-643, KF-6020, X-22-4515, KF-6011, KF-6012, KF-6015, KF-6017 (the above are trade names, manufactured by Shin-Etsu Chemical Co., Ltd.); Silface SAG002, 005, 503A, 008 (the above are trade names, manufactured by Nissin Chemical Industry Co., Ltd.), etc.
[0217] As the fluorine-based surfactant, a fluorine-modified polymer is preferably used. Specific examples thereof include BYK-3440 (manufactured by BYK Chemie Japan Co., Ltd.), Surflon S-241, S-242, S-243 (these are trade names, manufactured by AGC Seimi Chemical Co., Ltd.), and Ftergent 215M (manufactured by neos Co., Ltd.).
[0218] When the white ink composition contains a surfactant, it may contain multiple types. When the white ink composition contains a surfactant, the content thereof can be set to 0.1% by mass or more and 2% by mass or less, preferably 0.4% by mass or more and 1.5% by mass or less, and more preferably 0.5% by mass or more and 1.0% by mass or less, relative to the total mass of the white ink composition.
[0219] Other ingredients
[0220] The white ink composition used in the recording method according to the present embodiment may contain additives, resin dispersants, preservatives / mildew preventers, rust preventers, chelating agents, viscosity modifiers, antioxidants, and other components in addition to the above components unless the function is impaired.
[0221] Examples of the additive include ureas, amines, sugars, and the like.
[0222] Examples of ureas include urea, ethylene urea, tetramethyl urea, thiourea, 1,3-dimethyl-2-imidazolidinone, and betaines (trimethylglycine, triethylglycine, tripropylglycine, triisopropylglycine, N,N,N-trimethylalanine, N,N,N-triethylalanine, N,N,N-triisopropylalanine, N,N,N-trimethylmethylalanine, carnitine, acetylcarnitine, and the like).
[0223] Examples of the amines include diethanolamine, triethanolamine, triisopropanolamine, etc. Ureas and amines can also function as pH adjusters.
[0224] Examples of the sugar include glucose, mannose, fructose, ribose, xylose, arabinose, galactose, aldonic acid, glucitol (sorbitol), maltose, cellobiose, lactose, sucrose, trehalose, and maltotriose.
[0225] Physical properties of white ink composition
[0226] The viscosity of the white ink composition is preferably 1.5 mPa·s to 15 mPa·s at 20° C., more preferably 1.5 mPa·s to 7 mPa·s, and even more preferably 1.5 mPa·s to 5.5 mPa·s. Within the above viscosity range, a predetermined image can be easily and efficiently formed on a recording medium.
[0227] From the viewpoint of making the wettability and spreadability of the white ink composition on the recording medium appropriate, the surface tension of the white ink composition at 25° C. is preferably 40 mN / m or less, more preferably 38 mN / m or less, further preferably 35 mN / m or less, further preferably 30 mN / m or less, and particularly preferably 25 mN / m or less. In addition, the surface tension is preferably 20 mN / m or more, more preferably 25 mN / m or more.
[0228] The viscosity and the surface tension can be measured as described above as the measurement of the physical properties of the treatment liquid.
[0229] The viscosity of the treatment fluid increases when mixed
[0230] The viscosity increase of the above-mentioned treatment liquid in the white ink composition when mixed with the white ink composition at a mass ratio of 1:10 is preferably 5 times or more. By having such a thickening property, there is a tendency that the cohesion of the components of the white ink composition is fully obtained when in contact with the above-mentioned treatment liquid, and the image quality of the image formed by the white ink composition and the image quality of the non-white ink composition used together are excellent. In particular, the thinning of thin lines used for text, etc. can be reduced. In addition, the treatment liquid used in the measurement of the viscosity increase preferably contains 7% by mass of calcium formate relative to the total mass of the treatment liquid.
[0231] Here, regarding the increase in the viscosity of the ink when mixed with the processing liquid, "viscosity increase" is defined as follows. That is, the viscosity increase refers to the ratio (ratio) of the viscosity of the mixed liquid after mixing relative to the viscosity of the ink before mixing, using the processing liquid and the ink used in the recording method, and mixing and stirring the processing liquid and the ink at a mass ratio of 1:10. The viscosity is measured at 20°C. Therefore, the viscosity increase is the ratio of the viscosity after mixing based on the viscosity before mixing. The viscosity increase is, for example, about 0.5 times or more and 10.0 times or less. In addition, depending on the composition of the ink, there is also a case where the viscosity increase is less than 1.0 times and the viscosity decreases, but it is called viscosity increase as a name. In addition, the measurement of viscosity can be carried out as described above as the measurement of physical properties in the processing liquid.
[0232] The lower limit of the viscosity increase of the white ink composition is preferably 5 times or more, more preferably more than 5 times, more preferably 5.5 times or more, further preferably 6 times or more, particularly preferably 7 times or more, and further preferably 10 times or more.
[0233] On the other hand, the upper limit of the viscosity increase of the white ink composition is not limited, but is preferably 20 times or less, more preferably 10 times or less, more preferably 9 times or less, more preferably 8.5 times or less, and even more preferably 8 times or less. When the viscosity of the white ink composition increases to the above range, the image quality, crack resistance, abrasion resistance, ejection stability, etc. are more excellent, which is preferred. In addition, there is a tendency that the image quality of the non-white ink composition used together is also excellent, especially the thinning of fine lines used for text, etc. can be reduced. In addition, the image quality is excellent even when the amount of ink attached is large, so the amount of ink attached can be increased, and there is a tendency that the background concealment of the white image is excellent.
[0234] The viscosity increase of the white ink composition can be adjusted mainly by adjusting the type and content of the white color material (including the resin dispersant) and / or the resin particles. In particular, it is easy to adjust by adjusting the type and content of the white color material (including the resin dispersant), which is preferred.
[0235] 1.3 Non-white ink adhesion process
[0236] The recording method according to the present embodiment includes a non-white ink attaching step of discharging a non-white ink composition containing a non-white color material from the inkjet head and attaching the non-white ink composition to the recording medium.
[0237] 1.3.1 Attachment method
[0238] The non-white ink attaching process of the recording method according to the present embodiment is performed by scanning, in which the inkjet head is moved relative to the recording medium in a fixed position, while the non-white ink composition is ejected from the inkjet head and attached to the recording medium, and the non-white ink composition is attached to the scanning area of one scan by one scan, and the surface temperature of the recording medium in the non-white ink attaching process is 35° C. or less. Since such an attaching method is the same as the above-mentioned white ink attaching process, a detailed description thereof will be omitted.
[0239] In addition, regarding the attachment method other than the above, it can also be set to the same as the above-mentioned white ink attachment step.
[0240] In the recording method according to the present embodiment, the maximum adhesion amount of the ink composition in the subsequent step of the above-mentioned white ink adhesion step and the non-white ink adhesion step is preferably within a range of 1 mg / inch. 2 More than 3 mg / inch 2 More preferably, 5 mg / inch 2The upper limit of the maximum adhesion amount is not particularly limited, but is preferably 20 mg / inch 2 Below, more preferably 15mg / inch 2 Below, more preferably 10 mg / inch 2 Below, particularly preferably 8 mg / inch 2 In addition, regardless of the order of the steps, it is also preferable that the range of the maximum adhesion amount of the non-white ink composition in the non-white ink adhesion step be within the above range.
[0241] From the viewpoint of being able to effectively suppress condensation, the maximum weight range of each droplet of the non-white ink composition in the non-white ink attachment step is preferably 1 to 15 ng, more preferably 2 to 14 ng, further preferably 3 to 13 ng, and particularly preferably 4 to 10 ng.
[0242] 1.3.2 Non-white ink composition
[0243] The following describes the components contained in the non-white ink composition used in the non-white ink attachment process. In addition, the components other than the colorant in the non-white ink composition can be the same as those of the white ink composition described above and can be selected independently of the white ink composition. These components can all be the same as those of the white ink composition described above, and the "white ink composition" can be renamed as the "non-white ink composition".
[0244] Non-white color materials
[0245] The non-white ink composition contains a non-white color material. The non-white color material contained in the non-white ink composition refers to a color material other than the above-mentioned white color material. The non-white color material is preferably a color material such as cyan, yellow, magenta, black, etc. As the non-white color material, for example, dyes, pigments, etc. can be cited.
[0246] The non-white color material may be any one of a dye and a pigment, or a mixture. However, among dyes and pigments, it is more preferred to include a pigment. The pigment is excellent in storage stability such as light resistance, weather resistance, and gas resistance, and is further preferably an organic pigment from this viewpoint.
[0247] Specifically, the pigment can use azo pigments such as insoluble azo pigments, condensed azo pigments, azo lakes, chelated azo pigments, phthalocyanine pigments, perylene and pyrene pigments, anthraquinone pigments, quinacridone pigments, dioxane pigments, thioindigo pigments, isoindolinone pigments, quinophthalone pigments and other polycyclic pigments, dye chelates, dyeing lakes, nitro pigments, nitroso pigments, aniline black, daylight fluorescent pigments, carbon black, etc. The above-mentioned pigments can be used alone or in combination of two or more. Further, as a non-white color material, a bright pigment can also be used.
[0248] Specific examples of the pigment are not particularly limited, and examples thereof include the following pigments.
[0249] Examples of the black pigment include No. 2300, No. 900, MCF88, No. 33, No. 40, No. 45, No. 52, MA7, MA8, MA100, and No. 2200B (all manufactured by Mitsubishi Chemical Corporation); Raven 5750, Raven 5250, Raven 5000, Raven 3500, Raven 1255, and Raven 700 (all manufactured by Carbon Columbia Corporation); Regal 400R, Regal 330R, Regal 660R, Mogul L, Monarch 700, Monarch 800, Monarch 880, Monarch 900, Monarch 1000, Monarch 1100, Monarch 1300, and Monarch 1400 (all manufactured by CABOT Corporation); JAPAN KK); Pigment Black FW1, Pigment Black FW2, Pigment Black FW2V, Pigment Black FW18, Pigment Black FW200, Pigment Black S150, Pigment Black S160, Pigment Black S170, Printex 35, Printex U, Printex V, Printex 140U, Extra Black 6, Extra Black 5, Extra Black 4A, Extra Black 4 (all manufactured by Degussa).
[0250] Examples of the yellow pigment include CI Pigment Yellow 1, 2, 3, 4, 5, 6, 7, 10, 11, 12, 13, 14, 16, 17, 24, 34, 35, 37, 53, 55, 65, 73, 74, 75, 81, 83, 93, 94, 95, 97, 98, 99, 108, 109, 110, 113, 114, 117, 120, 124, 128, 129, 133, 138, 139, 147, 151, 153, 154, 167, 172, and 180.
[0251] Examples of the magenta pigment include CI Pigment Red 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 14, 15, 16, 17, 18, 19, 21, 22, 23, 30, 31, 32, 37, 38, 40, 41, 42, 48 (Ca), 48 (Mn), 57 (Ca), 57:1, 88, 112, 114, 122, 123, 144, 146, 149, 150, 166, 168, 170, 171, 175, 176, 177, 178, 179, 184, 185, 187, 202, 209, 219, 224, and 245; and CI Pigment Violet 19, 23, 32, 33, 36, 38, 43, and 50.
[0252] Examples of the cyan pigment include CI Pigment Blue 1, 2, 3, 15, 15:1, 15:2, 15:3, 15:34, 15:4, 16, 18, 22, 25, 60, 65, and 66; and CI Vat Blue 4 and 60.
[0253] Pigments other than magenta, cyan, and yellow are not particularly limited, and examples thereof include CI Pigment Green 7, 10, CI Pigment Brown 3, 5, 25, 26, and CI Pigment Orange 1, 2, 5, 7, 13, 14, 15, 16, 24, 34, 36, 38, 40, 43, and 63.
[0254] The pearlescent pigment is not particularly limited, and examples thereof include pigments having pearl luster or interference luster, such as titanium dioxide-coated mica, fish scale foil, and bismuth oxychloride.
[0255] The metal pigment is not particularly limited, and examples thereof include particles composed of a single substance or an alloy of aluminum, silver, gold, platinum, nickel, chromium, tin, zinc, indium, titanium, copper, and the like.
[0256] As dyes, various dyes generally used in inkjet recording such as direct dyes, acid dyes, food dyes, basic dyes, reactive dyes, disperse dyes, vat dyes, soluble vat dyes, and reactive disperse dyes can be used.
[0257] The non-white color material is preferably stably dispersed or dissolved in a dispersion medium, and may be dispersed using a dispersant as needed. As the dispersant, the same dispersant used to improve the dispersibility of the white color material of the above-mentioned white ink composition can be cited. As the dispersant, a dispersant resin is preferred.
[0258] The acid value of the dispersant resin of the non-white color material can be set to the same value as the acid value of the dispersant resin of the above-mentioned white color material, and is particularly preferably 30 mgKOH / g or more. The acid value of the dispersant resin of the non-white color material is preferably higher than the acid value of the dispersant resin of the white color material, more preferably 5 mgKOH / g or more, and further preferably 10 to 30 mgKOH / g higher. In this case, the image quality is better, which is preferred.
[0259] The content of the non-white colorant is preferably 0.3% by mass or more and 20% by mass or less, more preferably 0.5% by mass or more and 15% by mass or less, relative to the total mass of the non-white ink composition. Further, it is preferably 1% by mass or more and 10% by mass or less, more preferably 2% by mass or more and 7% by mass or less.
[0260] The volume average particle size of the pigment particles when using pigment in the non-white color material is preferably 10nm or more and 300nm or less, more preferably 30nm or more and 250nm or less, further preferably 50nm or more and 250nm or less, and particularly preferably 70nm or more and 200nm or less. Further, preferably 80nm or more and 150nm or less. The volume average particle size of the non-white color material is measured as an initial state using the above-mentioned method for confirming the volume average particle size. When the volume average particle size is in the above-mentioned range, it is preferred in that it is easy to obtain the desired color material and it is easy to make the characteristics of the color material good.
[0261] water
[0262] The non-white ink composition used in the recording method according to the present embodiment is an aqueous ink and preferably contains water. The type and content of water that can be used are the same as those of the white ink composition described above, and thus detailed descriptions thereof are omitted.
[0263] Organic solvents
[0264] The non-white ink composition used in the recording method according to the present embodiment may contain an organic solvent. The types and content of the organic solvent that can be used are the same as those of the white ink composition described above, and thus detailed descriptions thereof are omitted.
[0265] The non-white ink composition preferably contains an organic solvent having a normal boiling point of 150 to 280° C. The normal boiling point of the organic solvent is more preferably 160 to 270° C., further preferably 170 to 260° C., and particularly preferably 180 to 250° C. In addition, the content of the organic solvent is preferably 10 to 50% by mass, more preferably 20 to 40% by mass, and further preferably 25 to 35% by mass relative to the total mass of the non-white ink composition.
[0266] The non-white ink composition preferably contains an alkane polyol organic solvent having a normal boiling point exceeding 280° C. in an amount not exceeding 2% by mass, more preferably not exceeding 1.5% by mass, further preferably not exceeding 1.0% by mass, still further preferably not exceeding 0.5% by mass, and particularly preferably not exceeding 0.1% by mass, relative to the total mass of the non-white ink composition. The lower limit of the content of the alkane polyol organic solvent having a normal boiling point exceeding 280° C. may be 0% by mass.
[0267] Resin particles
[0268] The non-white ink composition used in the recording method according to the present embodiment may contain resin particles. The types and content of the resin particles that can be used are the same as those of the white ink composition described above, and therefore detailed descriptions thereof will be omitted.
[0269] wax
[0270] The non-white ink composition used in the recording method according to the present embodiment may contain wax. The types and content of the wax that can be used are the same as those of the white ink composition described above, and thus detailed descriptions thereof are omitted.
[0271] Surfactants
[0272] The non-white ink composition used in the recording method according to the present embodiment may contain a surfactant. The types and contents of the surfactant that can be used are the same as those of the white ink composition described above, and thus detailed descriptions thereof are omitted.
[0273] Other ingredients
[0274] The non-white ink composition used in the recording method involved in this embodiment may contain additives, resin dispersants, preservatives / mildewproof agents, rust inhibitors, chelating agents, viscosity modifiers, antioxidants and other components in addition to the above-mentioned components, as long as the functions are not impaired, similar to the above-mentioned white ink composition.
[0275] Physical properties of non-white ink composition
[0276] The viscosity and surface tension of the non-white ink composition are the same as those of the white ink composition described above, and thus detailed description thereof will be omitted.
[0277] The viscosity of the treatment fluid increases when mixed
[0278] The viscosity increase of the non-white ink composition when the above-mentioned treatment liquid and the non-white ink composition are mixed at a mass ratio of 1:10 is preferably 5 times or more. By having such a thickening property, there is a tendency that the cohesion of the components of the non-white ink composition is fully obtained when in contact with the above-mentioned treatment liquid, and the image quality of the image formed by the non-white ink composition and the image quality of the white ink composition used together are excellent. In particular, the thinning of thin lines used for text, etc. can be reduced. In addition, the treatment liquid used in the measurement of the viscosity increase preferably contains 7% by mass of calcium formate relative to the total mass of the treatment liquid.
[0279] The lower limit of the viscosity increase of the non-white ink composition is preferably 5 times or more, more preferably more than 5 times, more preferably 5.5 times or more, further preferably 6 times or more, particularly preferably 7 times or more, and further preferably 10 times or more.
[0280] On the other hand, the upper limit of the viscosity increase of the non-white ink composition is not limited, but is preferably 20 times or less, more preferably 10 times or less, more preferably 9 times or less, more preferably 8.5 times or less, and even more preferably 8 times or less. When the viscosity of the non-white ink composition increases within the above range, the image quality, crack resistance, abrasion resistance, ejection stability, etc. are more excellent, which is preferred. In particular, there is a tendency to reduce the thinning of thin lines used for text, etc., and there is a tendency that the image quality of the white ink composition used together is also excellent.
[0281] The viscosity increase of the non-white ink composition can be adjusted mainly by adjusting the type and content of the non-white color material (including the resin dispersant) and the resin particles. In particular, it is easy to adjust by adjusting the type and content of the non-white color material (including the resin dispersant), which is preferred.
[0282] 1.4 Conveying process
[0283] The recording method according to the present embodiment may include a conveying step of conveying the recording medium, but the recording medium is not conveyed while scanning is being performed.
[0284] In addition, it is preferable that the conveying process is not performed for the scanning area where one of the scanning of the white ink attaching process and the non-white ink attaching process is performed, and the other scanning is performed. In other words, it is preferable that the position of the recording medium is fixed during the period from when the scanning of the white ink attaching process and the non-white ink attaching process is performed until the scanning area where the one of the scanning is performed is scanned by the other.
[0285] Furthermore, in the above case, it is preferable to perform the conveying step after the other scanning is completed and / or before performing one scanning.
[0286] The transport step transports the portion of the recording medium where ink has not been deposited to a position where the ink depositing step is performed, or moves the portion of the recording medium where ink has been deposited from the position where the ink depositing step is performed.
[0287] More specifically, if Figure 1 For example, the recording unit 31 moves the carriage 32 in a direction parallel to the X-axis direction, and ejects the white ink composition or the non-white ink composition from the nozzle N of the inkjet head 35 onto the surface of the sheet S, so that the ink is attached to the scanning area of the first scan by one scan. Then, preferably, the carriage 32 is moved again in a direction parallel to the X-axis direction without conveying the sheet S, and the non-white ink composition or the white ink composition is ejected from the nozzle N of the inkjet head 35 onto the surface of the sheet S, so that the ink is attached to the scanning area of the first scan by one scan.
[0288] If this method is adopted, recording can be performed at a higher speed, but during the main scan of the other side to which the next ink is attached, the vapor concentration on the recording medium is higher, so condensation on the nozzle surface is more likely to occur. Even in such a case, the recording method according to this embodiment can well suppress condensation.
[0289] The conveying direction of the recording medium in the conveying process may be a direction along the axis of the scanning direction of the main scan, or may be a direction along the axis intersecting the axis of the scanning direction of the main scan. Here, if the scanning area of the medium to which ink can be attached is wider in one main scan, the printing area per unit time becomes larger, and therefore, the recording speed can be further increased. By increasing the number of nozzles arranged in the inkjet head to extend the length of the inkjet head, the scanning area of the medium to which ink can be attached can be expanded, but the length that can be extended is limited from the perspective of cost. Therefore, in order to efficiently utilize the length of the inkjet head, it is preferred to set the inkjet head in parallel with the width direction of the recording medium. In this case, the plurality of nozzles in the inkjet head are arranged in parallel in the direction along the axis intersecting the axis of the scanning direction of the main scan. That is, the conveying direction of the recording medium becomes the direction along the axis of the scanning direction of the main scan. That is, the conveying direction may be Figure 1 In any direction, right or left. Figure 1 In this example, it is the right direction.
[0290] As described above, in the recording method involved in the present embodiment, from the viewpoint of being able to easily increase the recording speed, it is preferred that a conveying process for conveying the recording medium is provided after the scanning of the white ink attachment process and the scanning of the non-white ink attachment process, and the conveying direction of the conveying process is the direction of the axis along the scanning direction of the scanning.
[0291] In addition, similarly, from the perspective of being able to easily increase the recording speed, it is preferred that the inkjet head has a nozzle array consisting of a plurality of nozzles that eject the ink composition, and the length of the nozzle array in the longitudinal direction is greater than the length of the area in that direction where recording can be performed on the recording medium.
[0292] From the viewpoint of being able to further improve the recording speed, the length of the length direction of the nozzle array of the inkjet head is preferably more than 10 cm, more preferably more than 20 cm, further preferably more than 30 cm, and particularly preferably more than 33 cm. The upper limit of this length is not limited, but is preferably less than 100 cm, more preferably less than 80 cm, and further preferably less than 50 cm.
[0293] 1.5 Post-heating process
[0294] The recording method involved in this embodiment may also include a post-heating process for heating the recording medium after each of the above-mentioned attachment processes. The post-heating process can be performed, for example, using appropriate heating means. The post-heating process is performed, for example, by a post-heater (equivalent to the drying section 4 in the example of the recording device 100 described later. It is also called a secondary heater.). In addition, the heating means is not limited to the heating means possessed by the recording device, and other drying means may also be used. In this way, the obtained image can be dried and fixed more fully, so that, for example, the recorded object can be put into a state that can be used as soon as possible. The post-heating process is also called a secondary heating process.
[0295] The temperature of the recording medium in this case is not particularly limited, and can be set, for example, in consideration of the Tg of the resin component constituting the resin particles contained in the recorded material, etc. In consideration of the Tg of the resin component constituting the resin particles or the wax, the temperature can be set to be 5.0°C or higher, preferably 10.0°C or higher than the Tg of the resin component constituting the resin particles.
[0296] The surface temperature of the recording medium reached by heating in the post-heating process is 30.0°C or higher and 120.0°C or lower, preferably 40.0°C or higher and 100.0°C or lower, more preferably 50.0°C or higher and 95°C or lower, and further preferably 70°C or higher and 90°C or lower. The surface temperature of the recording medium reached by heating in the post-heating process is particularly preferably 70°C or higher. If the temperature of the recording medium is within this range, there is a tendency that the resin particles or wax that may be contained in the recorded material can be coated and flattened, and the obtained image can be dried and fixed more fully.
[0297] 1.6 Other processes
[0298] The recording method of the present embodiment may have a primary drying process. The primary drying process is a process for drying the recording medium before or during the process of attaching the treatment liquid or ink composition. In addition to the method of stopping recording and placing, the primary drying process can also be performed by using a drying mechanism to dry it. As a method for drying using a drying mechanism, there can be cited: a method of supplying air at room temperature or warm air to the recording medium (air supply type), and a method of irradiating the recording medium with radiation (infrared rays, etc.) that generates heat (radiation type), a component that contacts the recording medium and transfers heat to the recording medium (conduction type), and a combination of two or more of these methods. In the case of having a primary drying process, among these methods, it is more preferable to perform it in an air supply type.
[0299] In the primary drying process, a drying mechanism that heats the recording medium is used as a drying mechanism, which is specifically referred to as a primary heating process. For example, among the above-mentioned drying mechanisms, a conduction type, a radiation type, and a warm air blowing type are considered as heating processes. A drying process that blows air at room temperature is not considered as a heating process.
[0300] In the case of having a primary drying step other than a heating step, it is preferred because excellent image quality can be obtained by accelerating drying and the surface temperature of the recording medium can be easily made 35° C. or less.
[0301] The drying process can be performed simultaneously with one or more of the above-mentioned treatment liquid adhesion process and ink adhesion process. When the drying process and the ink adhesion process are performed simultaneously, the surface temperature of the recording medium is 35°C or less, preferably 33°C or less, more preferably 31°C or less, further preferably 29°C or less, and particularly preferably 27°C or less.
[0302] In addition, each attachment process may not be accompanied by a primary heating process. That is, in the recording method of this embodiment, it is preferred that the recording medium is not heated by a heating mechanism for heating the recording medium provided by a member supporting the recording medium at a position to which the ink composition is attached, and the recording medium is not heated by a heating mechanism for heating the recording medium from above. In such a case, it is easy to set the surface temperature of the recording medium in the ink attachment process to a low temperature below a predetermined temperature, further suppress the evaporation of the solvent component of the ink, and the temperature difference between the nozzle surface and the vicinity of the platen can be suppressed to a lower level, so there is a tendency to further reduce condensation.
[0303] 2. Recording device
[0304] A recording device according to one embodiment of the present invention is a recording device that performs recording using the above-mentioned recording method, and includes the above-mentioned processing liquid, the above-mentioned white ink composition, the above-mentioned non-white ink composition, and an inkjet head.
[0305] According to the recording device of the present embodiment, since recording is performed by the above-mentioned recording method, it is possible to achieve an excellent recording speed, suppress condensation, and achieve excellent image quality (uneven shading).
[0306] Figure 1 Schematically shows a front view of an example of a recording device according to the present embodiment. Figure 1 and Figure 2 In order to clarify the configuration relationship of each part of the device, the XYZ orthogonal coordinates with the Z axis as the vertical axis are recorded. In addition, in the following description, the direction of each coordinate axis (arrow) is appropriately regarded as the positive direction, and the opposite direction is appropriately regarded as the negative direction. In addition, Figure 1 The recording device shown is a serial recording device, but because the recording medium is transported in the direction along the axis of the scanning direction, it is also particularly called a transverse recording device.
[0307] The recording device 100 includes a host device 200 that generates print data based on image data (bitmap data) received from an external device such as a personal computer, and a printer unit 300 that prints an image based on the print data received from the host device 200. The printer unit 300 prints an image on the surface of a long sheet S using an inkjet method while conveying the long sheet S in a roll-to-roll manner.
[0308] like Figure 1As shown, the printer unit 300 includes a main body housing 1 having a substantially rectangular parallelepiped shape. The main body housing 1 includes: a reel 2 for reeling out a sheet S from a roll R1 on which the sheet S is wound; a printing chamber 3 for printing by ejecting ink onto the surface of the reeled sheet S; a drying unit 4 for drying the sheet S to which the ink is attached; and a reel 5 for reeling the dried sheet S into a roll R2.
[0309] More specifically, the main body housing 1 is divided into upper and lower parts in the Z-axis direction by a flat base 6 arranged parallel to the XY plane (i.e., horizontally), and the upper side of the base 6 serves as the printing chamber 3. A paper press 30 is fixed to the upper surface of the base 6 in a substantially central portion of the printing chamber 3. The paper press 30 has a rectangular shape, and supports the sheet S from the lower side by its upper surface parallel to the XY plane. Then, the recording unit 31 prints on the surface of the sheet S supported on the paper press 30.
[0310] On the other hand, the unwinding section 2, the drying section 4, and the winding section 5 are arranged on the lower side of the base 6. The unwinding section 2 is arranged on the lower side of the negative direction of the X axis relative to the paperboard 30 ( Figure 1 The reel 21 is provided with a rotatable unwinding shaft 21. The sheet S is wound on the unwinding shaft 21, thereby supporting the reel R1. On the other hand, the reeling section 5 is arranged on the lower side of the X-axis positive direction relative to the paperboard 30 ( Figure 1 The drying section 4 is disposed directly below the paper pressing plate 30 between the unwinding section 2 and the winding section 5 in the X-axis direction and has a rotatable winding shaft 51. The sheet S is wound on the winding shaft 51, thereby supporting the roll R2.
[0311] Then, the sheet S unwound from the unwinding shaft 21 of the unwinding section 2 passes through the printing chamber 3 and the drying section 4 in sequence while being guided by the rollers 71 to 77, and then is wound around the winding shaft 51 of the winding section 5. In addition, the rollers 72 and 73 are arranged straightly (i.e., horizontally) in the X-axis direction in such a manner as to sandwich the paper pressing plate 30, and the positions are adjusted so that the tops of the rollers 72 are at the same height as the upper surface of the paper pressing plate 30 (the surface supporting the sheet S). Therefore, the sheet S hung on the roller 72 moves horizontally (in the X-axis direction) while being in sliding contact with the upper surface of the paper pressing plate 30 until it reaches the roller 73.
[0312] In the printing room 3, the printing process on the sheet S is performed by the recording unit 31 arranged on the upper side of the platen 30. The recording unit 31 prints an image on the surface of the sheet S by ejecting the processing liquid and the white ink composition and the non-white ink composition onto the surface of the sheet S. Here, at the end ( Figure 1A cartridge mounting portion 8 is provided at the left end portion of the sheet S, and a treatment liquid cartridge 81 storing the treatment liquid and a plurality of ink cartridges 82 storing the white ink composition and the non-white ink composition are detachably mounted on the cartridge mounting portion 8. The recording unit 31 can eject the treatment liquid supplied from the treatment liquid cartridge 81 and the ink composition supplied from the ink cartridge 82 onto the surface of the sheet S by inkjet method.
[0313] Figure 2 FIG. 1 is a bottom view partially showing the structure of the recording unit. Figure 1 as well as Figure 2 The recording unit 31 is described in detail. The recording unit 31 includes a carriage 32, a flat support plate 33 mounted on the lower surface of the carriage 32, and inkjet heads 34 and 35 mounted on the lower surface of the support plate 33. On the lower surface of the support plate 33, four inkjet heads 35 and one inkjet head 34 are arranged at equal pitches in the X-axis direction, and in each of the inkjet heads 34 and 35, a plurality of nozzles N are arranged parallel to the Y-axis direction. The inkjet head 34 ejects a processing liquid from the nozzles N, and the four inkjet heads 35 eject inks of different colors, that is, a white ink composition and a non-white ink composition, from the nozzles N, respectively.
[0314] Back to Figure 1 The description will be continued. The carriage 32 of the recording unit 31 constructed as described above can move integrally with the support plate 33 and the inkjet heads 34 and 35. That is, an X-axis guide rail 37 extending parallel to the X-axis direction is provided in the printing chamber 3, and when the carriage 32 receives the driving force of the X-axis motor, it moves in the X-axis direction along the X-axis guide rail 37.
[0315] See also Figure 6 right Figure 1 The inkjet head H is mounted on the carriage 32. Figure 6 In the embodiment, the inkjet head H has: a nozzle row W, in which a plurality of nozzles N for ejecting white ink are arranged in the nozzle row direction; four nozzle rows C, in which a plurality of nozzles N for ejecting non-white ink are arranged in the nozzle row direction; and a nozzle row R, in which a plurality of nozzles N for ejecting treatment liquid are arranged in the nozzle row direction. In addition, Figure 6 The figure is viewed from the recording surface side of the recording medium where recording is performed, and the nozzle row is shown on the front side of the figure. However, in reality, the nozzle row is located on the back side of the figure and faces the recording medium.
[0316] exist Figure 6 In FIG. 1 , the sheet S is described as a recording medium M. The sheet S is unrolled from the roll R1 and conveyed onto the platen P. As shown in FIG.
[0317] exist Figure 6In (a), the recording device moves the carriage 32 in the outward direction (scanning direction MS, right direction in the figure) parallel to the X-axis direction, while ejecting the white ink composition from the nozzle array W of the inkjet head H to the surface of the sheet S, so that the white ink composition is attached to the scanning area of one scan through one scan. In addition, in the figure, the inkjet head H is in a state where it advances to about half of the scanning distance in the scanning direction, but the inkjet head H scans the scanning distance in the scanning direction to the end.
[0318] At this time, the sheet S stops on the upper surface of the platen P. By the same scan as the first scan, the processing liquid is ejected from the nozzle array R of the inkjet head H onto the surface of the sheet S in the same scan area.
[0319] Then, in Figure 6 In (b), the carriage 32 returns to the initial position, and while the carriage 32 is moved again in the outward direction parallel to the X-axis direction, the non-white ink composition is ejected from the nozzle array C onto the surface of the sheet S, so that the non-white ink composition is attached to the scanning area of the single scan by the single scan. In this way, the non-white ink is attached to the scanning area to which the white ink composition is attached.
[0320] By the same scan as the one scan, the processing liquid is ejected from the nozzle row R onto the surface of the sheet S in the same scan area.
[0321] Alternatively, instead of returning the recording unit 31 to the initial position, similar scanning may be performed by depositing the non-white ink composition while moving the carriage 32 in the return direction (left direction in the figure) parallel to the X-axis direction.
[0322] Thus, a two-dimensional image of one frame is printed in the X-axis direction by the length of the nozzle array in the Y-axis direction on the surface of the sheet S. In addition, the color material of the ink constituting the two-dimensional image is condensed by the processing liquid and fixed on the surface of the sheet S.
[0323] Next, the sheet S is conveyed in the conveying direction SS (right direction in the figure) by a length of one frame in the X-axis direction, and the sheet S of one frame is moved from the platen P.
[0324] Then, in Figure 6 In (c), the sheet S is scanned so that the white ink composition adheres to a new portion of the sheet S that has stopped on the upper surface of the paper plate P. Figure 6 In (d), scanning is performed to allow the non-white ink composition to adhere. Figure 6 (c) scanning, Figure 6 The scanned contents of (d) are respectively Figure 6 (a) scanning, Figure 6The scanning contents of the scanning of (b) are the same. Thus, the image of the next frame is printed. In the case of further continuing the recording, the scanning of (b) is repeated. Figure 6 The process after the sheet S is conveyed in (b) is sufficient.
[0325] As another embodiment, the recording device may print an image on the surface of the sheet S stopped on the upper surface of the paper platen 30 by ejecting the processing liquid and the ink composition from the inkjet heads 34 and 35 while the carriage 32 is reciprocated in the Y-axis direction above the paper platen 30. In this case, the following structure is adopted: a Y-axis guide (not shown) extending parallel to the Y-axis direction is provided in the printing chamber 3, and the carriage 32 moves in the Y-axis direction along the Y-axis guide when receiving the driving force of the Y-axis motor (not shown). In addition, the inkjet heads 35 and 34 are arranged at equal pitches in the Y-axis direction, and in each of the inkjet heads 34 and 35, a plurality of nozzles N are arranged in parallel in the X-axis direction.
[0326] The printing of one frame as described above is repeatedly performed while the sheet S is intermittently moved in the X-axis direction. Specifically, a predetermined range covering substantially the entire area of the upper surface of the paper press 30 becomes the printing area. Moreover, the sheet S is intermittently conveyed in the X-axis direction in units of a distance (intermittent conveying distance) corresponding to the length of the printing area in the X-axis direction, and one frame of printing is performed on the sheet S stopped on the upper surface of the paper press 30 during the intermittent conveying. In other words, when the printing of one frame on the sheet S stopped on the paper press 30 is completed, the sheet S is conveyed in the X-axis direction by the intermittent conveying distance, so that the unprinted surface of the sheet S stops on the paper press 30. Then, one frame of printing is re-executed on the unprinted surface, and when the printing is completed, the sheet S is again conveyed in the X-axis direction by the intermittent conveying distance. Then, these series of actions are repeated.
[0327] Furthermore, in order to keep the sheet S stopped on the upper surface of the paper press 30 during intermittent conveyance flat, the paper press 30 may also be provided with a mechanism for sucking the sheet S stopped on its upper surface. Specifically, a plurality of suction holes, not shown, are provided on the upper surface of the paper press 30, and a suction unit 38 is installed on the lower surface of the paper press 30. Then, by the operation of the suction unit 38, negative pressure is generated in the suction holes on the upper surface of the paper press 30, so that the sheet S is sucked to the upper surface of the paper press 30. Furthermore, while the sheet S is stopped on the paper press 30 for printing, the suction unit 38 sucks the sheet S, thereby keeping the sheet S flat. On the other hand, when printing is finished, the suction unit 38 stops sucking the sheet S, thereby enabling the sheet S to be smoothly conveyed.
[0328] In addition, a heater 39 may be installed on the lower surface of the paper press 30. The heater 39 can heat the paper press 30 to a predetermined temperature (for example, 30° C.) as needed. Thus, the following structure can be set: the sheet S is dried once by the heat of the paper press 30 while receiving the printing process of the inkjet heads 34 and 35.
[0329] However, in the recording device according to the present embodiment, the recording medium may be heated by a heating mechanism (e.g., heater 39) provided in a member supporting the recording medium or a heating mechanism (not shown) for heating the recording medium from above at a position to which the ink composition is attached, such as on the platen 30. Examples of the heating mechanism for heating the recording medium from above include a blower fan and an IR heater.
[0330] However, even when the process is performed, the surface temperature of the recording medium when the ink is attached is 35° C. or lower, and it is preferable to adopt a structure in which the process is not performed.
[0331] This makes it easy to set the surface temperature of the recording medium at 35° C. or less when the ink is attached, thereby further suppressing evaporation of the solvent component of the ink and further suppressing the temperature difference between the nozzle surface and the vicinity of the platen, which tends to further reduce condensation.
[0332] Thus, the sheet S having received one frame of printing moves from the platen 30 to the drying section 4 as the sheet S is intermittently conveyed. The drying section 4 is a member capable of performing a post-heating process for completely drying the processing liquid or ink composition landed on the sheet S using air heated for drying.
[0333] In the drying section 4 , the sheet S is preferably heated to a surface temperature of 30.0° C. to 120.0° C., preferably 40.0° C. to 100.0° C., more preferably 50.0° C. to 95° C., and further preferably 70° C. to 90° C.
[0334] Then, the sheet S subjected to the drying process reaches the winding section 5 as the sheet S is intermittently conveyed, and is wound into a roll R2.
[0335] Figure 7 It is a schematic perspective view schematically showing another example of the recording device according to the present embodiment. Figure 7 The recording device 500 is also an example of a serial recording device. The recording device 500 includes an inkjet head 510, a carriage housing 9, a carriage body 12, a paper plate 11, a carriage moving mechanism 13, a conveying unit 14, and a control unit CONT. The overall operation of the inkjet recording device 500 is controlled by the control unit CONT.
[0336] The inkjet head 510 performs scanning by ejecting ink from the nozzles of the inkjet head 510 while moving in the scanning direction MS. The recording medium M is transported in the transport direction SS by the transport unit 14. The inkjet head 510 is attached to the lower surface of the carriage.
[0337] Figure 8 It is shown that the use Figure 7 An example of recording performed by a recording device of this embodiment is shown in FIG. The inkjet head H is mounted on a carriage and Figure 6 Similarly, nozzle row W, nozzle row C, and nozzle row R are provided.
[0338] The recording medium M is transported from Figure 8 The material is transported to the press board from above.
[0339] exist Figure 8 In (a), the recording device ejects the white ink composition from the nozzle array W of the inkjet head H onto the surface of the recording medium M while moving the carriage in the forward direction (scanning direction MS), thereby attaching the white ink composition to the scanning area of the single scan through a single scan. At this time, the recording medium M stops on the upper surface of the paper platen P. Through the same scan as the single scan, the processing liquid is ejected from the nozzle array R onto the surface of the recording medium M for the same scanning area.
[0340] Then, in Figure 8 In (b), the carriage returns to the initial position, and while the carriage is moved again in the scanning direction MS, the non-white ink composition is ejected from the nozzle array C onto the surface of the recording medium M, so that the non-white ink composition is attached to the scanning area of the single scan by the single scan. In this way, the non-white ink is attached to the scanning area to which the white ink composition is attached.
[0341] By the same scan as this one scan, the processing liquid is ejected from the nozzle row R onto the surface of the recording medium M with respect to the same scan area.
[0342] Instead of returning the carriage to the initial position, scanning may be performed in the same manner such that the non-white ink composition is deposited while the carriage is moved in the return direction (left direction in the figure) parallel to the MS axis direction.
[0343] Thus, an image corresponding to one frame of the scanning distance in the scanning direction MS is printed on the surface of the recording medium M by the length of the nozzle row in the conveying direction SS. In addition, the color material of the ink constituting the image is aggregated by the processing liquid and fixed on the surface of the recording medium M.
[0344] Next, the recording medium M is conveyed in the conveying direction SS by a length corresponding to one frame, and the recording medium M corresponding to one frame is moved from the platen P.
[0345] Then, in Figure 8 In (c), scanning is performed to make the white ink composition adhere to a new portion of the recording medium M stopped on the upper surface of the paper plate P. Next, Figure 8 In (d), scanning is performed to allow the non-white ink composition to adhere. Figure 8 (c) scanning, Figure 8 The scanned contents of (d) are respectively Figure 8 (a) scanning, Figure 8 The scanning contents of the scanning of (b) are the same. Thus, the image of the next frame is printed. In the case of further continuing the recording, the scanning of (b) is repeated. Figure 8 The process after the recording medium M is transported in (b) is sufficient.
[0346] Fig. 9 It is shown that the use Figure 7 FIG. 1 is a diagram showing another example of recording performed by a recording device of the present embodiment. The inkjet head H is mounted on a carriage and has a nozzle row W arranged on the upstream side and a nozzle row C arranged on the downstream side along the conveying direction SS. The nozzle row R is arranged on the upstream side and the downstream side. The nozzle rows can be arranged in such a positional relationship or can be arranged in a Figure 8 Similarly, each nozzle row is arranged from the upstream side to the downstream side along the conveying direction SS. Fig. 9 The recorded part is used for recording. Fig. 9 The unrecorded parts are not used for recording. Fig. 9 The nozzle row is a nozzle row used for recording.
[0347] exist Fig. 9 In (a), the recording device ejects the white ink composition from the nozzle array W of the inkjet head H onto the surface of the recording medium M while moving the carriage in the forward direction (scanning direction MS), thereby attaching the white ink composition to the scanning area of the single scan through a single scan. At this time, the recording medium M stops on the upper surface of the paper platen P. Through the same scan as the single scan, the processing liquid is ejected from the nozzle array R onto the surface of the recording medium M for the same scanning area.
[0348] Next, the recording medium M is transported along the transport direction SS by a distance corresponding to the length of the nozzle row W.
[0349] Then, in Fig. 9In (b), the carriage returns to the initial position, and while the carriage is moved again in the scanning direction MS, the non-white ink composition is ejected from the nozzle array C onto the surface of the recording medium M, so that the non-white ink composition is attached to the scanning area of the first scan by one scan. In this way, the non-white ink is attached to the scanning area to which the white ink composition is attached. At this time, at the same time, the nozzle array W attaches the white ink composition to a new part of the recording medium M by one scan.
[0350] By the same scan as this one scan, the processing liquid is ejected from the nozzle row R onto the surface of the recording medium M with respect to the same scan area.
[0351] Instead of returning the carriage to the initial position, scanning may be performed in the same manner such that the non-white ink composition is deposited while the carriage is moved in the return direction (left direction in the figure) parallel to the MS axis direction.
[0352] Thus, an image corresponding to one frame of the scanning distance in the scanning direction MS is printed on the surface of the recording medium M by the length of the nozzle row C in the conveying direction SS. In addition, the color material of the ink constituting the image is aggregated by the processing liquid and fixed on the surface of the recording medium M.
[0353] Next, the recording medium M is transported in the transport direction SS by a distance corresponding to the length of the nozzle row W. The length of the nozzle row W and the length of the nozzle row C along the transport direction SS are equal.
[0354] Then, with Fig. 9 The recording medium M is conveyed in the same manner as in step (a). Thus, one frame of the recording medium M is moved from the platen P.
[0355] Then, in Fig. 9 In (c), a scan is performed to make the white ink and the non-white ink adhere. The scanning content of this scan is the same as Fig. 9 The scanning contents of (b) are the same. In case of further continuing recording, repeat Fig. 9 The process after the recording medium M is transported in (b) is sufficient.
[0356] Fig. 9 An example of recording is a method in which the recording medium is conveyed between a scan that is performed earlier and a scan that is performed later in the scan that causes the white ink to adhere and the scan that causes the non-white ink to adhere.
[0357] 3. Example
[0358] The present invention is described in more detail below by way of examples, but the present invention is not limited to these examples. In the following, "%" is a mass reference unless otherwise specified. In addition, unless otherwise specified, the evaluation is performed under an environment of a temperature of 25.0°C and a relative humidity of 40.0%.
[0359] 3.1. Preparation of ink and treatment solution
[0360] According to Table 1 ( Figure 3 ) were placed in a container, mixed and stirred for 2 hours with a magnetic stirrer, and then dispersed using a bead mill filled with zirconia beads with a diameter of 0.3 mm to fully mix. After stirring for 1 hour, the mixture was filtered using a 5.0 μm PTFE membrane filter to obtain white ink compositions (W1 to W4), non-white ink compositions (C1 to C3), and treatment liquids (R1 to R3). Table 1 ( Figure 3 ) represent mass %. Pure water was used as water and was added so that the mass of each ink and the treatment liquid was 100 mass %. In addition, the pigment and the dispersant resin were prepared into a dispersion liquid described later and used.
[0361] For Table 1( Figure 3 ) The components other than the compound names shown in the formula are supplemented as follows:
[0362] Cationic polymer: "CatioMaster-PD-7, polyamine resin (epichlorohydrin-amine derivative resin)" manufactured by Yokkaichi Synthetic Co., Ltd.
[0363] Dispersant resin, resin A (anionic): acrylic acid-acrylate copolymer (weight average molecular weight: 25,000, acid value: 25)
[0364] Dispersant resin, resin C (anionic): acrylic acid-acrylate copolymer (weight average molecular weight: 25,000, acid value: 35)
[0365] Carbon black: No. 33 (Mitsubishi Chemical Corporation)
[0366] Resin particles, styrene acrylic A: see below (high cohesion)
[0367] Resin particles, styrene acrylic B: see below (low cohesion)
[0368] Wax: Polyethylene: "Nopcoat PEM-17" (trade name, manufactured by SanNopco Co., Ltd.)
[0369] Surfactant, Silicone: Silicone surfactant "BYK348" manufactured by BYK Resin particles: Preparation of styrene acrylic B
[0370] Resin emulsion B (acid value 7 mgKOH / g) was obtained by emulsion copolymerization of 75 parts by mass of styrene, 0.8 parts by mass of acrylic acid, 14.2 parts by mass of methyl methacrylate and 10 parts by mass of cyclohexyl methacrylate. In addition, as a surfactant for emulsion polymerization, Newcol NT-30 (manufactured by Nippon Emulsifier Co., Ltd.) was used in an amount of 2 parts by mass based on 100 parts by mass of the total monomer amount.
[0371] Resin particles: Preparation of styrene acrylic A
[0372] Except for changing the monomer composition, the same operation as above was carried out to obtain a resin emulsion A (acid value: 30 mgKOH / g). The amount of the surfactant for emulsion polymerization was 1 part by mass based on 100 parts by mass of the total amount of the monomers.
[0373] Preparation of pigment dispersion
[0374] White pigment dispersion based on resin A
[0375] First, 12 parts by mass of anionic acrylic acid-acrylate copolymer (weight average molecular weight: 25,000, acid value: 25) was added to 155 parts by mass of ion exchange water in which 0.1 parts by mass of 30% ammonia solution (neutralizer) was dissolved as a resin dispersant and dissolved. 40 parts by mass of titanium dioxide (CI pigment white 6) as a white pigment was added thereto, and a zirconia bead mill was used for 10 hours of dispersion treatment. Then, impurities such as coarse particles and garbage were removed by centrifugal filtration by a centrifuge, thereby adjusting the concentration of the white pigment to 20% by mass to obtain a white color material dispersion. The particle size of the white pigment is 350nm in terms of average particle size.
[0376] Non-white pigment dispersion based on resin C
[0377] An acrylic acid-acrylate copolymer (weight average molecular weight: 25,000, acid value: 35) was used as a resin dispersant, and carbon black was used as a color material. The amount of the resin dispersant added was such that the mass ratio of the resin dispersant to the pigment was as shown in Table 1 ( Figure 3 ) by mass ratio, and a non-white color material dispersion liquid (black) was obtained in the same manner except that the above-mentioned conditions were changed to 0.1 wt. % by mass. The particle size of the pigment was 60 nm in average particle size.
[0378] 3.2 Evaluation methods
[0379] 3.2.1 Viscosity increase rate
[0380] Table 1 Figure 3 ) is the viscosity increase ratio when mixed with the test solution of R1 under the same conditions as R1, after each ink and the treatment solution of R1 were mixed at a mass ratio of 10:1 and stirred for 1 minute, and then the viscosity was measured using a rheometer (MCR302 / made by Anton-Paar) at 25°C and a shear rate of 200 s -1 When the viscosity is measured under the conditions of, the ratio of the viscosity of the mixed liquid after mixing to the viscosity of the ink before mixing.
[0381] 3.2.2 Recording test
[0382] We prepared a modified L-4733AW made by Epson, which has an inkjet head with a length equal to the width of the recording medium, and can record in the width of the recording medium in one pass. Figure 1 The structure shown. Figure 6 Such recording. For the recording medium (PET 50A, manufactured by Lintec) fixed on the printing table (pressboard), each ink is recorded in 1 pass (1 pass for white ink, 1 pass for color ink, 2 passes in total). The pass is scanning. The attachment of the treatment liquid is performed by simultaneous impact in the process of attaching the white ink and each process of attaching the color ink. After the above-mentioned 2 passes of recording in total, the recording medium is transported by the length of the printing table and the new part is moved to the printing table to perform the next recording. At this time, the transport direction and scanning direction of the recording medium are the same axial direction (for example Figure 1 in the X-axis direction).
[0383] In addition, Table 3 ( Figure 5 ) are examples of recording by a line recording method in which each ink attachment process is performed while conveying the recording medium. In this line recording, the inkjet head of the modified machine is fixed near the center of the X-axis direction on the platen, and the recording is performed by ejecting ink from the inkjet head while the modified machine conveys the recording medium in the conveying direction. Except for recording in a line manner, Reference Example 3 is the same as Comparative Example 1, and Reference Example 4 is the same as Example 1.
[0384] In Tables 2 and 3 ( Figure 4 , 5 ) in the example where the surface temperature of the medium is 25°C, the platen heater is turned off and the platen is not heated. On the other hand, in the example where the surface temperature of the medium is 28°C or higher, the platen heater is turned on and adjusted to the temperature in Tables 2 and 3 ( Figure 4 , 5 ) is the medium surface temperature.
[0385] Table 2, 3 ( Figure 4 , 5 ) in which the head movement distance is the length of the recording medium on the stage (e.g. Figure 1 In addition, as an example of changing the head moving distance from 0.5 m, an example of changing the length of the printing table in the main scanning direction is prepared.
[0386] The width of the recording medium used (e.g. Figure 1 In this case, the length of the inkjet head (the length of the recording medium in the Y-axis direction) is 30 cm. In this case, the length of the inkjet head (nozzle array) exceeds 30 cm.
[0387] The test pattern is entirely a recording pattern except for the 5 mm blanks on the four sides of the recording medium on the stage.
[0388] The nozzle density of the inkjet head was set to 1200 dpi. In addition, the basic resolution in 1-pass recording was set to 1200 × 1200 dip, and the number of ink droplets actually attached to each pixel was adjusted to adjust the ink attachment amount [mg / inch 2 ] is Table 2, 3 ( Figure 4 , 5 ) In addition, the weight of each drop of ink (Iw [ng / dot]) is set to the value in Tables 2 and 3 ( Figure 4 , 5 ) in the .
[0389] The secondary heating was performed by heating the recording medium to 70° C. using a secondary heater located downstream in the conveyance direction of the recording medium.
[0390] 3.2.3 Evaluation of landfill and pinholes
[0391] The solid image area of the recorded object was visually observed under a fluorescent lamp and evaluated according to the following criteria. In addition, the evaluation of white ink was performed on the portion of the recorded pattern where the white ink composition and the treatment liquid were attached but the non-white ink composition and the treatment liquid were not attached. The evaluation of non-white ink was performed on the portion of the recorded pattern where the white ink composition and the treatment liquid were attached and the non-white ink composition and the treatment liquid were attached in an overlapping manner.
[0392] A: There are no unfilled areas or pinholes.
[0393] B: Unfilled areas or pinholes are slightly visible.
[0394] C: Unfilled areas or pinholes are clearly seen.
[0395] 3.2.4 Evaluation of uneven shades
[0396] The solid image area of the recorded material was visually observed under a fluorescent light and evaluated according to the following criteria.
[0397] The recording pattern used in the evaluation of the white ink and the recording pattern used in the evaluation of the non-white ink are the same as those in the evaluation of the buried pinholes.
[0398] A: There is no color bleeding (unevenness of light and dark).
[0399] B: Bleeding (unevenness in light and dark) is slightly observed.
[0400] C: Bleeding (unevenness in light and dark) is clearly observed.
[0401] 3.2.5 Evaluation of 3pt text
[0402] blank text
[0403] A non-white full-print image was made on a white full-print image, and white text (3pt) was formed in the non-white full-print image in the portion without non-white ink. Then, the boundary bleeding between the white ink and the non-white ink was observed. The evaluation was performed according to the following evaluation criteria. The results were recorded in the white position in the table.
[0404] A: There is no color bleeding at the borders of blank text.
[0405] B: There is slight color bleeding at the border between blank characters.
[0406] C: There is bleeding of color at the border between blank characters.
[0407] Non-white text
[0408] The text (3 pt) was recorded with non-white ink on the solid white image. Then, the thinning and interruption of the line of the non-white text was evaluated. The non-white text was evaluated according to the following evaluation criteria. The results were recorded in the non-white position of the table.
[0409] A: Non-white text on a solid white page can be clearly read.
[0410] B: There is a slight interruption of the non-white text on the solid white page.
[0411] C: There is a break in the non-white text on the solid white page.
[0412] 3.2.6 Condensation evaluation
[0413] In Tables 2 and 3 ( Figure 4 , 5 ) for 1 hour, and after recording, the nozzles of the ejection nozzle group were inspected and the nozzle surface was observed, and the evaluation was performed according to the following evaluation criteria. In addition, the situation where no ejection or flight bending of more than half of the distance between adjacent nozzles occurred was considered as ejection failure. It should be noted that the ink may come into contact with condensation and cause flight bending, etc.
[0414] A: There is no condensation on the nozzle surface. There are no defective nozzles.
[0415] B: There is no condensation on the nozzle surface. The number of nozzles with defective ejection is less than 1%.
[0416] C: Condensation slightly occurs on the nozzle surface. The number of nozzles with defective ejection exceeds 1% and is less than 3%.
[0417] D: Considerable condensation occurs on the nozzle surface. More than 3% of nozzles have defective ejection.
[0418] 3.2.7 Evaluation of recording speed
[0419] The number of passes recorded at one time is evaluated according to the following evaluation criteria.
[0420] A: The number of trips recorded at one time is less than 2 trips.
[0421] B: The number of trips recorded at one time is more than 3.
[0422] 3.3 Evaluation results
[0423] The evaluation results are shown in Tables 2 and 3. Figure 4 , 5 ).
[0424] From Tables 2 and 3 ( Figure 4 , 5 ) It was found that according to the recording method of each embodiment, an excellent recording speed is set, and condensation is suppressed and the image quality (uneven light and dark) is excellent, wherein the recording method comprises: a treatment liquid adhesion step, in which a treatment liquid containing a coagulant is adhered to a recording medium; a white ink adhesion step, in which a white ink composition containing a white color material is ejected from an inkjet head and adhered to the recording medium; and a non-white ink adhesion step, in which a non-white ink composition containing a non-white color material is ejected from the inkjet head and adhered to the recording medium, wherein the white ink composition and the non-white ink composition are water-based inks, and the white ink adhesion step and the non-white ink adhesion step are performed by scanning, respectively, in the During scanning, the inkjet head is moved relative to the recording medium in a fixed position, while the ink composition is ejected from the inkjet head and attached to the recording medium. The white ink attachment process attaches the white ink composition to the scanning area of the first scan by a single scan, and the non-white ink attachment process attaches the non-white ink composition to the scanning area of the first scan by a single scan. For the scanning area that has been scanned by either the white ink attachment process or the non-white ink attachment process, the other scanning is performed by another scanning. The surface temperature of the recording medium in the white ink attachment process and the non-white ink attachment process is below 35°C.
[0425] In contrast, the recording methods of the comparative examples other than the above recording methods were inferior in any of the recording speed, suppression of condensation, and image quality (uneven shading). The recording methods of the reference examples other than the above recording methods did not cause the problem of the present invention.
[0426] According to the comparison between Example 1 and Comparative Example 1, when the surface temperature of the recording medium was not 35° C. or lower, the condensation evaluation was poor.
[0427] According to the comparison between Example 1 and Comparative Example 2, when the processing liquid attachment step is not provided, the image quality (uneven density) is poor.
[0428] According to the comparison between Example 1 and Comparative Examples 3 to 5, when the white ink attaching step does not attach the white ink composition to the scanning area of one scanning by one scanning, the recording speed is different.
[0429] With reference to Reference Examples 1 and 2, when the white ink attaching step is not provided, there are no problems with the recording speed, suppression of condensation, and image quality (uneven density).
[0430] Referring to Reference Examples 3 and 4, in printing based on the line-based recording method, there is no problem of condensation, etc. However, during recording, there is no time when the inkjet head is not facing the recording medium.
[0431] From the results of Example 1 and Examples 2 and 3, it is clear that if the reactivity of the processing liquid is within a predetermined range, it is possible to achieve good filling and pinholes, uneven shading, and text 3pt in a well-balanced manner.
[0432] According to the results of Example 1, Example 4, Example 5, Example 13, Example 17, and Example 1, Example 9, and Example 10, if the water content of the white ink composition and the non-white ink composition is within a predetermined range, the filling of pinholes and unevenness in light and dark can be well balanced.
[0433] From the results of Example 1 and Example 6, when the reactivity of the white ink composition is within a predetermined range, the unevenness of light and dark and the 3 pt of characters can be well balanced.
[0434] The results of Examples 1, 7, and 16 show that when the amount of the white ink composition deposited is within a predetermined range, the evaluations of buried pinholes, uneven density, text 3 pt, and condensation can be well balanced.
[0435] According to the results of Example 1 and Example 8, if the weight of each drop of the treatment liquid is within a predetermined range, the pinhole filling and the text 3pt can be well balanced.
[0436] According to the results of Example 1 and Example 11, and Example 13 and Examples 14 and 15, even in a case where the head movement distance is long and condensation is likely to occur, condensation can be suppressed well.
[0437] According to the results of Example 1 and Examples 12 and 13, the closer the medium surface temperature is to the ambient temperature, the better the image quality and the suppression of condensation are.
[0438] According to the results of Example 13 and Example 18, regardless of the order of the ink attachment process, good suppression of condensation and image quality (uneven density) were achieved.
[0439] According to the results of Example 13 and Example 19, if the weight per drop of the white ink composition is within a predetermined range, condensation is more excellently suppressed.
[0440] Although not shown in the table, the ink and recording conditions of each example were used. Figure 7 The recording device Figure 8 , Fig. 9 When recording, the recording speed, condensation suppression and image quality are excellent.
[0441] The following contents are derived from the above-mentioned embodiments.
[0442] One embodiment of the recording method comprises:
[0443] a treatment liquid attachment step of attaching the treatment liquid containing the coagulant to the recording medium;
[0444] a white ink attaching step of ejecting a white ink composition containing a white color material from an inkjet head and attaching the composition to the recording medium; and
[0445] a non-white ink attaching step of ejecting a non-white ink composition containing a non-white color material from the inkjet head and attaching the non-white ink composition to the recording medium;
[0446] The white ink composition and the non-white ink composition are water-based inks,
[0447] The white ink attaching step and the non-white ink attaching step are respectively performed by scanning, in which the ink composition is ejected from the inkjet head to attach to the recording medium while the inkjet head is moved relative to the recording medium in a fixed position.
[0448] The white ink attaching step attaches the white ink composition to a scanning area of a single scan by a single scan.
[0449] The non-white ink attaching step attaches the non-white ink composition to the scanning area of the scanning by scanning once,
[0450] For a scan area in which one of the scanning in the white ink attaching step and the scanning in the non-white ink attaching step has been performed, the other scanning is performed by another scanning.
[0451] The surface temperature of the recording medium in the white ink attaching step and the non-white ink attaching step is 35° C. or less.
[0452] In one embodiment of the above recording method, it may also be that,
[0453] The maximum adhesion amount of the ink composition in the first step of the white ink adhesion step and the non-white ink adhesion step is in the range of 8 mg / inch 2 above.
[0454] In any of the above recording methods, it may also be that,
[0455] The viscosity increase when the treatment liquid and the white ink composition are mixed at a mass ratio of 1:10 in the white ink composition and the viscosity increase when the treatment liquid and the non-white ink composition are mixed at a mass ratio of 1:10 are each 5 times or more.
[0456] In any of the above recording methods, it may also be that,
[0457] The distance that the inkjet head moves relative to the recording medium in the one scan is 0.5 m or more.
[0458] In any of the above recording methods, it may also be that,
[0459] In the white ink attaching step and the non-white ink attaching step, the maximum weight of each droplet of the white ink composition and the non-white ink composition is in the range of 0.5 ng to 15 ng, respectively.
[0460] In any of the above recording methods, it may also be that,
[0461] For the scanning area where the scanning in either the white ink attaching step or the non-white ink attaching step is performed, the other scanning is performed without performing the conveying step of conveying the recording medium.
[0462] In any of the above recording methods, it may also be that,
[0463] The inkjet head has a nozzle array composed of a plurality of nozzles that eject an ink composition, and the length of the nozzle array in a longitudinal direction is equal to or longer than the length of a region in the direction where recording can be performed on the recording medium.
[0464] In any of the above recording methods, it may also be that,
[0465] After the scanning in the white ink attaching step and the scanning in the non-white ink attaching step, a conveying step of conveying the recording medium is provided, wherein the conveying direction of the conveying step is a direction along an axis of the scanning direction of the scanning.
[0466] In any of the above recording methods, it may also be that,
[0467] The process liquid attaching step is performed by scanning, in which the process liquid is ejected from the inkjet head while the inkjet head is moved, and the process liquid is attached to the recording medium.
[0468] The white ink attaching step and the non-white ink attaching step are each performed by scanning the same scanning area as the scanning for attaching the ink composition, so as to attach the processing liquid.
[0469] In any of the above recording methods, it may also be that,
[0470] The nozzle density of the inkjet head is greater than 600 dpi.
[0471] In any of the above recording methods, it may also be that,
[0472] At the position receiving the adhesion of the ink composition, the recording medium is not heated by a heating mechanism for heating the recording medium provided in a member supporting the recording medium, and the recording medium is not heated by a heating mechanism for heating the recording medium from above.
[0473] One embodiment of the recording device is a recording device that uses the recording method of any of the above embodiments to perform recording, wherein:
[0474] The invention comprises the treatment liquid, the white ink composition, the non-white ink composition, and the inkjet head.
[0475] The present invention is not limited to the above-mentioned embodiments, and various modifications are possible. For example, the present invention includes a configuration substantially the same as the configuration described in the embodiments, such as a configuration with the same function, method, and result, or a configuration with the same purpose and effect. In addition, the present invention includes a configuration in which a non-essential part of the configuration described in the embodiments is replaced. In addition, the present invention includes a configuration that has the same effect as the configuration described in the embodiments, or a configuration that can achieve the same purpose. In addition, the present invention includes a configuration in which a known technology is added to the configuration described in the embodiments.
Claims
1. A recording method, characterized in that: have: a treatment liquid attachment step of attaching the treatment liquid containing the coagulant to the recording medium; a white ink attaching step of ejecting a white ink composition containing a white color material from an inkjet head and attaching it to the recording medium; as well as a non-white ink attaching step of ejecting a non-white ink composition containing a non-white color material from the inkjet head and attaching the non-white ink composition to the recording medium; The white ink composition and the non-white ink composition are water-based inks, The white ink attaching step and the non-white ink attaching step are respectively performed by scanning, in which the ink composition is ejected from the inkjet head to attach to the recording medium while the inkjet head is moved relative to the recording medium in a fixed position. The white ink attaching step attaches the white ink composition to a scanning area of a single scan by a single scan. The non-white ink attaching step attaches the non-white ink composition to the scanning area of the scanning by scanning once, For a scan area in which one of the scanning in the white ink attaching step and the scanning in the non-white ink attaching step has been performed, the other scanning is performed by another scanning. The surface temperature of the recording medium in the white ink attaching step and the non-white ink attaching step is 35° C. or less.
2. The recording method according to claim 1, characterized in that The maximum adhesion amount of the ink composition in the first step of the white ink adhesion step and the non-white ink adhesion step is in the range of 8 mg / inch 2 above.
3. The recording method according to claim 1, characterized in that The viscosity increase when the treatment liquid and the white ink composition are mixed at a mass ratio of 1:10 in the white ink composition and the viscosity increase when the treatment liquid and the non-white ink composition are mixed at a mass ratio of 1:10 are each 5 times or more.
4. The recording method according to claim 1, characterized in that: The distance that the inkjet head moves relative to the recording medium in the one scan is 0.5 m or more.
5. The recording method according to claim 1, characterized in that In the white ink attaching step and the non-white ink attaching step, the maximum weight of each droplet of the white ink composition and the non-white ink composition is in the range of 0.5 ng to 15 ng, respectively.
6. The recording method according to claim 1, characterized in that: For the scanning area where the scanning in either the white ink attaching step or the non-white ink attaching step is performed, the other scanning is performed without performing the conveying step of conveying the recording medium.
7. The recording method according to claim 1, characterized in that: The inkjet head has a nozzle array composed of a plurality of nozzles that eject an ink composition, and the length of the nozzle array in a longitudinal direction is equal to or longer than the length of a region in the direction where recording can be performed on the recording medium.
8. The recording method according to claim 7, characterized in that: After the scanning in the white ink attaching step and the scanning in the non-white ink attaching step, a conveying step of conveying the recording medium is provided, wherein the conveying direction of the conveying step is a direction along an axis of the scanning direction of the scanning.
9. The recording method according to claim 1, characterized in that: The process liquid attaching step is performed by scanning, in which the process liquid is ejected from the inkjet head while the inkjet head is moved, and the process liquid is attached to the recording medium. The white ink attaching step and the non-white ink attaching step are each performed by scanning the same scanning area as the scanning for attaching the ink composition, so as to attach the processing liquid.
10. The recording method according to claim 1, characterized in that: The nozzle density of the inkjet head is above 600 dpi.
11. The recording method according to claim 1, characterized in that: At the position receiving the adhesion of the ink composition, the recording medium is not heated by a heating mechanism for heating the recording medium provided in a member supporting the recording medium, and the recording medium is not heated by a heating mechanism for heating the recording medium from above.
12. A recording device, characterized in that: A recording device for recording using the recording method according to any one of claims 1 to 11, The recording device includes the processing liquid, the white ink composition, the non-white ink composition, and the inkjet head.
Citation Information
Patent Citations
Scalpel blade extractor
EP0005052A1
Inkjet recording method, inkjet ink composition and ink set
JP2018015968A
Ink jet recording method and recording apparatus
CN110194005A
Media advance
US20110311290A1
Ink Set, Printing Method, And Printing Apparatus
US20210062027A1