Polarizing plate

By using a (meth)acrylic resin film and a multi-layer adhesive layer combination in the polarizing plate, the problems of warping and insufficient solvent resistance of the existing polarizing plate in a high temperature and high humidity environment are solved, and a newer polarizing plate is achieved. High stability and durability.

CN118732136APending Publication Date: 2024-10-01SUMITOMO CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410376630.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-29
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing polarizing plates are prone to warping in high-temperature and high-humidity environments and have insufficient solvent resistance, making it difficult to meet the long-term storage needs of base films such as display panels.

Method used

A polarizing plate composed of a (meth)acrylic resin film, an adhesive layer, a polarizing plate, a protective film and an adhesive layer is used. By adjusting the structure and hierarchy of the resin, the Martens hardness and energy storage mode of the resin are improved. quantity to ensure stability in high temperature and high humidity environments.

Benefits of technology

Significantly improves the solvent resistance and anti-warping performance of the polarizing plate, ensuring that it is not easy to warp in high temperature and high humidity environments, and meets the long-term use needs of applications such as display panels.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732136A_ABST
    Figure CN118732136A_ABST
Patent Text Reader

Abstract

Provided is a polarizing plate which has excellent solvent resistance and is capable of reducing warpage in a high-temperature, high-humidity environment. A polarizing plate (100) is provided with a (meth) acrylic resin film (10), a first adhesive layer (12), a polarizer (20), a second adhesive layer (14), a protective film (30), and an adhesive layer (40) in this order. The Martens hardness of the (meth) acrylic resin film (10) is 140 N / mm2 or more, and the storage modulus of the adhesive layer (40) at 25 DEG C and a measurement frequency of 1 Hz is 1.5 * 105 Pa or less.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present invention relates to a polarizing plate. Background Art A polarizing plate having a structure of acrylic resin film / polarizer / cycloolefin resin film is known. Prior art literature Patent Literature Patent Document 1: Japanese Patent Application Publication No. 2018-200339 Patent Document 2: Japanese Patent Application Publication No. 2017-204007 Summary of the invention Problems to be solved by the invention However, this polarizing plate has problems such as warping when stored in a high-temperature and high-humidity environment in a state of being attached to a base film such as a display panel, and insufficient solvent resistance. An object of the present invention is to provide a polarizing plate which has excellent solvent resistance and can reduce warping in a high-temperature and high-humidity environment. Means for solving problems

[0001] A polarizing plate comprising, in order, a (meth)acrylic resin film, a first adhesive layer, a polarizer, a second adhesive layer, a protective film, and an adhesive layer. The Martens hardness of the (meth)acrylic resin film is 140 N / mm 2 above, The storage modulus of the adhesive layer at 25°C and a measurement frequency of 1 Hz is 1.5×10 5 Below Pa.

[0002] The polarizing plate according to [1], wherein the (meth)acrylic resin film The tensile modulus in the MD direction at 25°C is defined as T MD (25°C), the tensile modulus in the MD direction at 80°C is defined as T MD (80℃), The tensile modulus in the TD direction at 25°C is defined as T TD (25°C), the tensile modulus in the TD direction at 80°C is defined as T TD (80℃), T MD (25℃) / T MD (80℃) and T TD (25℃) / T TD (80℃) are all less than 2.0.

[0003] The polarizing plate according to [1] or [2], wherein the (meth)acrylic resin film has a storage modulus G′ in the MD direction at 80° C. and a measurement frequency of 10 Hz. MD (80℃) and tensile modulus T in MD direction at 80℃ MD (80℃) ratio G' MD (80℃) / T MD (80℃) less than 1.2.

[0004] The polarizing plate according to any one of [1] to [3], wherein the (meth)acrylic resin film has a storage modulus in the MD direction at 80° C. and a measurement frequency of 10 Hz, G′ MD The storage modulus in the TD direction at 80°C and a measurement frequency of 10 Hz is G' TD (80℃), G' MD (80℃) / G' TD (80°C) is 1.05 or less.

[0005] The polarizing plate according to any one of [1] to [4], wherein the product of the moisture permeability and the thickness of the (meth)acrylic resin film is 2500 (g / m 2 ·24hr·μm) or less.

[0006] The polarizing plate according to any one of [1] to [5], wherein the polarizer is a polyvinyl alcohol-based resin film and contains a boron compound, and the boron content is 4.0 wt % or less.

[0007] The polarizing plate according to any one of [1] to [6], wherein the first adhesive layer is a cured product of a (meth)acrylic adhesive.

[0008] The polarizing plate according to any one of [1] to [7], wherein the protective film is a cyclic polyolefin-based resin film. Effects of the Invention According to the present invention, a polarizing plate can be provided which has excellent solvent resistance and can reduce warping in a high-temperature and high-humidity environment. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 It is a schematic diagram of a cross section of a polarizing plate according to one embodiment. Figure 2 It is a schematic diagram explaining the measurement position of the warpage amount in the wet heat warpage test. Description of Reference Numerals 10 ... (meth)acrylic resin film, 12 ... first adhesive layer, 20 ... polarizer, 14 ... second adhesive layer, 30 ... protective film, 40 ... adhesive layer, 100 ... polarizing plate. DETAILED DESCRIPTION (Polarizing Plate) like Figure 1 As shown, a polarizing plate 100 according to one embodiment of the present invention includes a (meth)acrylic resin film 10 , a first adhesive layer 12 , a polarizer 20 , a second adhesive layer 14 , a protective film 30 , and a pressure-sensitive adhesive layer 40 in this order. ((Meth) acrylic resin film 10) The (meth)acrylic resin film 10 is a film containing a (meth)acrylic resin, and functions as a protective film of the polarizing plate 20 . (Meth) acrylic resin is a polymer with (meth) acrylic acid ester, especially (meth) acrylic acid alkyl ester as the main structural unit (50% by mass or more relative to all structural units). The resin can be a homopolymer of (meth) acrylic acid ester, a copolymer using two or more (meth) acrylic acid esters, or a copolymer of (meth) acrylic acid ester and a monomer copolymerizable therewith. It should be noted that in this specification, (meth) acrylic acid refers to acrylic acid and / or methacrylic acid. Similarly, (meth) acrylic acid ester refers to acrylic acid ester and / or methacrylic acid ester. Specific examples of (meth)acrylates include alkyl acrylates such as methyl acrylate, ethyl acrylate, propyl acrylate, isopropyl acrylate, butyl acrylate, isobutyl acrylate, sec-butyl acrylate, tert-butyl acrylate, hexyl acrylate, cyclohexyl acrylate, octyl acrylate, 2-ethylhexyl acrylate, decyl acrylate and dodecyl acrylate; alkyl methacrylates such as methyl methacrylate, ethyl methacrylate, propyl methacrylate, isopropyl methacrylate, butyl methacrylate, isobutyl methacrylate, sec-butyl methacrylate, tert-butyl methacrylate, hexyl methacrylate, octyl methacrylate, 2-ethylhexyl methacrylate, decyl methacrylate and dodecyl methacrylate; and the like. These alkyl (meth)acrylates may have an arbitrary substituent such as a hydroxyl group or a halogen atom at the alkyl portion. Examples of alkyl (meth)acrylates having such a substituent include 2-hydroxyethyl acrylate, 2-hydroxypropyl acrylate, 4-hydroxybutyl acrylate, 2-hydroxyethyl methacrylate, 2-hydroxypropyl methacrylate, 4-hydroxybutyl methacrylate, 3-chloro-2-hydroxypropyl methacrylate, glycidyl methacrylate, and the like. Among these (meth)acrylates, methyl methacrylate is preferably used as the main raw material of the acrylic resin. That is, as described in detail below, a homopolymer of methyl methacrylate, a copolymer of methyl methacrylate as a main constituent monomer and other (meth)acrylates, a copolymer of methyl methacrylate as a main constituent monomer and other monomers other than (meth)acrylates, or a copolymer of methyl methacrylate as a main constituent monomer and other (meth)acrylates and other monomers other than (meth)acrylates is preferably used as the (meth)acrylic resin. Examples of monomers copolymerizable with (meth)acrylates include α,β-ethylenically unsaturated carboxylates other than the above-mentioned (meth)acrylates, α,β-ethylenically unsaturated carboxylates, alkenyl aromatic compounds, conjugated dienes, non-conjugated dienes, vinyl cyanide, α,β-ethylenically unsaturated carboxylic acid amides, carboxylic acid unsaturated alcohol esters, olefins, and the like. Specific examples of α,β-ethylenically unsaturated carboxylic acid esters other than (meth)acrylates include dimethyl fumarate, diethyl fumarate, dimethyl maleate, diethyl maleate, dimethyl itaconate, monoethyl maleate, monobutyl fumarate, etc. In addition, the α,β-ethylenically unsaturated carboxylic acid may be any of a monocarboxylic acid, a polycarboxylic acid, and a polycarboxylic acid anhydride, and specific examples thereof include acrylic acid, methacrylic acid, crotonic acid, maleic acid, fumaric acid, itaconic acid, maleic anhydride, itaconic anhydride, etc. Specific examples of alkenyl aromatic compounds include styrene, α-methylstyrene, α-methyl-2-, -3- or -4-methylstyrene, vinyltoluene, divinylbenzene, etc. Specific examples of conjugated dienes include 1,3-butadiene, 2-methyl-1,3-butadiene, 1,3-pentadiene, 2,3-dimethyl-1,3-butadiene, 2-chloro-1,3-butadiene, cyclopentadiene, etc. Specific examples of non-conjugated dienes include 1,4-hexadiene, dicyclopentadiene, ethylidene norbornene, etc. Specific examples of vinyl cyanide include acrylonitrile, methacrylonitrile, α-chloroacrylonitrile, α-ethylacrylonitrile, etc. Specific examples of α,β-ethylenically unsaturated carboxylic acid amides include acrylamide, methacrylamide, N-methylol acrylamide, N-methylol methacrylamide, N,N-dimethyl acrylamide, etc. Specific examples of carboxylic acid unsaturated alcohol esters include vinyl acetate, etc. Specific examples of olefins include ethylene, propylene, butene, pentene, etc. When a monomer other than (meth)acrylate is copolymerized, the monomer other than (meth)acrylate may be only one kind, or two or more kinds may be copolymerized. When such a monomer other than (meth)acrylate is copolymerized, the content of the structural units derived from these monomers in the (meth)acrylic resin is preferably 50% by weight or less, more preferably 15% by weight or less, and further preferably 10% by weight or less in all the structural units. Specific examples of (meth) acrylic resins preferably used in the present invention include poly(methyl methacrylate), copolymers of methyl methacrylate / methyl acrylate, copolymers of methyl methacrylate / methyl acrylate / butyl acrylate / styrene, copolymers of methyl methacrylate / styrene / butyl acrylate, copolymers of methyl methacrylate / ethylene, etc. Among them, preferably, the polymer in which the structural unit derived from methyl methacrylate is 70% by weight or more, further 80% by weight or more, and especially 90% by weight or more in all structural units. One (meth) acrylic resin may be used alone, or two or more may be used in combination. The molecular weight of the (meth) acrylic resin is, for example, about 50,000 to 500,000 in terms of the weight average molecular weight converted to polystyrene. If the weight average molecular weight is within this range, it is easy to obtain a homogeneous film when forming a film by a melt extrusion method. When the (meth) acrylic resin has a ring structure in its main chain, the heat resistance and hardness of the (meth) acrylic resin film finally obtained can be improved. When the (meth) acrylic resin has a ring structure in the main chain, the content of the ring structure in the resin can usually be in the range of 0.1 to 99 mass%, 1 to 95 mass%, 2 to 93 mass%, or 5 to 90 mass%, but from the perspective of appropriately maintaining the stretchability and handling properties of the (meth) acrylic resin film and improving the above-mentioned heat resistance and hardness, it is preferably 10 to 70 weight%, more preferably 10 to 60 weight%, and particularly preferably in the range of 10 to 50 mass%. If the content of the ring structure is too large, the stretchability and handling properties of the (meth) acrylic resin film are reduced. Examples of the ring structure that the (meth)acrylic resin may have in the main chain include a glutarimide structure, a lactone ring structure, a succinic anhydride structure, and a succinimide structure. The glutarimide structure is preferably represented by the following general formula (1): [Chemical formula 1] In the general formula (1), R 11 and R 12 Each independently represents hydrogen or an alkyl group having 1 to 8 carbon atoms, R 13represents an alkyl group having 1 to 18 carbon atoms, a cycloalkyl group having 3 to 12 carbon atoms, or an aryl group having 6 to 10 carbon atoms. 11 and R 12 are each independently hydrogen or methyl, R 13 is hydrogen, methyl, butyl or cyclohexyl. 11 is methyl, R 12 is hydrogen, R 13 The acrylic resin may contain only a single glutarimide unit, or may contain R in the above general formula (1). 11 , R 12 and R 13 Different multiple glutarimide structures. Acrylic resins having a glutarimide structure are described in, for example, Japanese Patent Application Laid-Open Nos. 2006-309033, 2006-317560, 2006-328334, 2006-337491, 2006-337492, 2006-337493, and 2006-337569. The glutarimide ring content in the (meth)acrylic resin may be 0.1 to 20% by mass, or 1 to 10% by mass. The (meth)acrylic resin having a ring structure in the main chain is commercially available and can be produced by a known method. In the (meth)acrylic resin film, in addition to the (meth)acrylic resin, rubber particles can also be used. As the rubber particles that can be used, rubber-like polymers with acrylate as the main monomer, rubber-like polymers with butadiene as the main monomer, ethylene-vinyl acetate copolymers, etc. can be cited. Among them, acrylic rubber particles as rubber-like polymers with acrylate as the main monomer are preferred. Of course, acrylic rubber particles and other rubber particles can also be used in combination. The acrylic rubber particles may be acrylic rubber particles whose main constituent monomers are acrylic acid alkyl esters having a large number of carbon atoms in the alkyl group such as butyl acrylate and 2-ethylhexyl acrylate, for example, 4 to 8 carbon atoms. Among them, elastic polymers whose main constituent monomers are butyl acrylate are preferred. Rubber particles having a single-layer structure including an elastic polymer whose main constituent monomer is an alkyl acrylate, and rubber particles having a multi-layer structure including a layer of the elastic polymer are also effective. As a representative example of the latter, there are rubber particles in which a layer of an acrylic elastic polymer and a hard polymer layer whose main constituent monomer is methyl methacrylate are formed in a core-shell structure, such as a grafted elastic polymer of an alkyl acrylate such as butyl acrylate and styrene. More specifically, there are rubber particles having a two-layer structure in which a layer of the hard polymer is formed on the outside of the acrylic elastomer, and rubber particles having a three-layer structure in which a layer of the hard polymer is formed on the inside of the acrylic elastomer and a layer of the hard polymer is also formed on the outside of the acrylic elastomer. In particular, as a suitable example, an example of acrylic rubber particles having such a multilayer structure can be cited. If acrylic rubber particles having a multilayer structure are used, the value of tensile fracture strain can be adjusted without excessively lowering the Vicat softening point of the (meth)acrylic resin, and fracture during film molding can be prevented without lowering heat resistance. The number average particle size of the rubber particles dispersed in the (meth)acrylic base resin is preferably 1,000 nm or less, more preferably in the range of 100 to 1,000 nm, and particularly preferably in the range of 100 to 500 nm. If the number average particle size of the rubber particles is large, the haze (turbidity) of the film becomes too large and the light transmittance becomes low. On the other hand, if the number average particle size is too small, there is a tendency for the flexibility of the film to decrease. The average particle size of acrylic rubber particles containing acrylic elastic polymers is measured as follows. That is, such rubber particles are mixed with acrylic base resins to form films. If the cross section is dyed with an aqueous solution of ruthenium oxide, only the layer of acrylic elastic polymer is colored and observed to be roughly circular, and the acrylic resin of the parent layer is not dyed. Therefore, a slice is prepared from the cross section of the film after such dyeing using a slicer, and it is observed with an electron microscope. Then, 100 dyed elastic polymer particles are randomly selected, and after calculating their respective particle sizes, the number average value is used as the average particle size. Since the measurement is performed by such a method, the average particle size of the rubber particles specified here is the number average particle size. In the case of using rubber particles whose outermost layer is a hard polymer mainly composed of methyl methacrylate and in which an acrylic elastic polymer is enclosed, if the rubber particles are mixed into an acrylic matrix resin, the outermost layer of the rubber particles is mixed with the acrylic matrix resin. Therefore, if the cross section is stained with ruthenium oxide and observed with an electron microscope, the rubber particles are observed in the form of particles with the outermost layer removed. Specifically, in the case of using rubber particles with a two-layer structure in which the inner layer is an acrylic elastic polymer and the outer layer is a hard polymer mainly composed of methyl methacrylate, the acrylic elastic polymer part of the inner layer is stained and observed in the form of particles with a single-layer structure. In addition, in the case of using rubber particles with a three-layer structure in which the innermost layer is a hard polymer mainly composed of methyl methacrylate, the middle layer is an acrylic elastic polymer, and the outermost layer is a hard polymer mainly composed of methyl methacrylate, the center part of the innermost particle is not stained, but is observed in the form of particles with a two-layer structure in which only the acrylic elastic polymer part of the middle layer is stained. The amount of rubber particles added to the (meth)acrylic base resin is preferably 10 to 50% by weight, more preferably 10 to 40% by weight, based on the total amount of the (meth)acrylic resin composition containing the rubber particles. If the amount of rubber particles is too small, the slip and flexibility of the film are insufficient, whereas if it is too large, it is difficult to achieve sufficient heat resistance of the film. In the (meth)acrylic resin film, the amount of the (meth)acrylic resin may be 10% by mass or more, 20% by mass or more, 40% by mass or more, 50% by mass or more, 80% by mass or more, 90% by mass or more, or 100% by mass relative to the whole. The (meth) acrylic resin film may contain an ultraviolet absorber. The ultraviolet absorber may be selected from ultraviolet absorbers commonly used in resins, such as hydroxybenzophenone compounds, benzotriazole compounds, triazine compounds, salicylate compounds, and the like. The film can be produced by a known method, that is, a thermoplastic composition containing a (meth)acrylic resin is melt-kneaded, extruded from a T-die to form a film, and then cooled. The (meth)acrylic resin film may be a non-stretched film, a uniaxially stretched film, or a biaxially stretched film. The stretching ratio may be 1.5 to 3.5. (thickness) The thickness of the (meth)acrylic resin film is not particularly limited, and may be 15 μm or more, preferably 30 μm or more, or 65 μm or less, preferably 50 μm or less. (Martens hardness) The Martens hardness of the (meth)acrylic resin film is 140 N / mm 2 Above, it can be 145N / mm 2 Above, can also be 150N / mm 2 Above, in addition, 300N / mm 2 Below, it can be 280N / mm 2 Below, can also be 250N / mm 2 Below, can also be 200N / mm 2 the following. By adjusting the type of (meth) acrylic resin constituting the (meth) acrylic resin film (the type of structural unit constituting the (meth) acrylic resin, and their mixing ratio in the case of having multiple structural units), glass transition temperature, and stereoregularity, a film with a desired Martens hardness can be obtained. For example, by making the (meth) acrylic resin have a ring structure in its main chain and making the content of the ring structure in the resin 5% by mass or more, or increasing the glass transition temperature of the (meth) acrylic resin, or increasing the stereoregularity of the (meth) acrylic resin (syndiotacticity represented by a triad), there is a tendency to increase the Martens hardness. In addition, in the case of containing multiple (meth) acrylic resins, by adjusting their mixing ratio, a film with a desired Martens hardness can be obtained. In addition, the Martens hardness can also be adjusted according to the type and amount of additives contained in the (meth) acrylic resin film. For example, in the case where the additive is rubber particles, there is a tendency to increase the Martens hardness by reducing its mixing amount. (Product of moisture permeability and thickness) The product of the moisture permeability and thickness of the (meth) acrylic resin film is preferably 2500 (g / m 2 ·24hr·μm) or less, can be 2400 (g / m 2 ·24hr·μm) or less, and can also be 1800 (g / m 2 ·24hr·μm) or more, and may be 2000(g / m 2 ·24hr·μm) or more. The (meth)acrylic resin film has a tensile elastic modulus in the MD direction at 25° C. as T MD (25°C), the tensile modulus in the MD direction at 80°C is defined as T MD (80°C), the tensile modulus in the TD direction at 25°C is defined as T TD (25℃), T at 80℃ TD The tensile elastic modulus in the direction is set as T TD (80℃), T MD (25℃) / TMD (80℃) and T TD (25℃) / T TD (80°C) is preferably less than 2.0, and may be less than 1.9, less than 1.85, or not less than 1.5. When the ratio is low, the hardness of the (meth)acrylic resin film at high temperatures is maintained, which contributes to the reduction of wet heat warpage. For the (meth)acrylic resin film, the storage modulus G′ in the MD direction at 80° C. and a measurement frequency of 10 Hz is MD (80℃) and tensile modulus T in MD direction at 80℃ MD (80℃) ratio G' MD (80℃) / T MD (80°C) is preferably less than 1.2, may be less than 1.1, or may be 0.7 or more. When this ratio is low, there is an effect of reducing wet heat warpage. The storage modulus of the (meth)acrylic resin film in the MD direction at 80° C. and a measurement frequency of 10 Hz is defined as G′. MD The storage modulus in the TD direction at 80°C and a measurement frequency of 10 Hz is G' TD (80℃), G' MD (80℃) / G' TD (80°C) is preferably 1.05 or less, and may be 1.00 or less, or 0.7 or more. When this ratio is low, there is an effect of reducing wet heat warpage. The MD direction of the (meth)acrylic resin film refers to a machine flow direction from a die during film formation, and the TD direction refers to a width direction perpendicular to the machine flow direction from a die during film formation. The relationship between the MD direction of the (meth)acrylic resin film 10 and the absorption axis direction of the polarizing plate 20 is not particularly limited, but it is preferable that they are parallel to each other. (Polarizing Plate) In the present invention, the polarizing plate is formed by adsorbing and aligning a dichroic pigment (iodine, dichroic dye) on a uniaxially stretched polyvinyl alcohol-based resin film and cross-linking the film with a boron compound such as boric acid or borax. The boron content in the polarizer can be below 5.0 mass %, can be below 4.2 mass %, and is suitable below 4.0 mass %. In addition, the boron content in the polarizer can be above 0.5 mass %, can be above 1.0 mass %, can be above 1.5 mass %, and is suitable above 2.0 mass %. The boron content (mass %) of the polarizer can be calculated as follows: 0.2 g of the polarizer is dissolved in 200 g of a 1.9 wt % mannitol aqueous solution to prepare a measurement sample solution, and a sodium hydroxide aqueous solution (1 mol / L) is added dropwise until the measurement sample solution reaches the neutralization point, and the boron content (mass %) is calculated based on the amount added. Examples of the polyvinyl alcohol resin constituting the polyvinyl alcohol resin film include resins obtained by saponifying polyvinyl acetate resins. Examples of the polyvinyl acetate resins include copolymers of vinyl acetate and other monomers copolymerizable therewith, in addition to polyvinyl acetate which is a homopolymer of vinyl acetate. Examples of other monomers copolymerizable with vinyl acetate include unsaturated carboxylic acids, olefins, vinyl ethers, unsaturated sulfonic acids, and (meth)acrylamides having an ammonium group. The degree of saponification of the polyvinyl alcohol-based resin is usually about 85 mol % or more, preferably about 90 mol % or more, and more preferably about 99 mol % or more. The polyvinyl alcohol-based resin may be modified. For example, polyvinyl formal, polyvinyl acetal, polyvinyl butyral, etc. modified with aldehydes may be used. The average degree of polymerization of the polyvinyl alcohol resin is preferably 100 or more and 10000 or less, more preferably 1500 or more and 8000 or less, and further preferably 2000 or more and 5000 or less. The average degree of polymerization of the polyvinyl alcohol resin can be obtained according to JIS K 6726 (1994). When the average degree of polymerization is within the above range, there is a tendency for excellent polarization performance and film processability. The polarizer can be manufactured by a process (hereinafter also referred to as a "treatment process") of contacting a raw material polyvinyl alcohol-based resin film (raw material film) with a treatment liquid. The method of contacting with the treatment liquid can be a method of immersing the film in a treatment liquid (hereinafter also referred to as a "treatment bath") contained in a treatment tank, or a method of treating the film by attaching the treatment liquid to the surface of the film by spraying, flowing down, dripping, etc. In the case of performing the treatment process by immersing the film in a treatment bath, the treatment bath for one treatment process is not limited to one, and the film can also be immersed in two or more treatment baths in sequence to complete one treatment process. As the above-mentioned treatment liquid, swelling liquid, dyeing liquid, cross-linking liquid, cleaning liquid, etc. can be exemplified. In addition, as the above-mentioned treatment process, a swelling process in which the swelling liquid is brought into contact with the original material film for swelling treatment, a dyeing process in which the dyeing liquid is brought into contact with the film after swelling treatment for dyeing treatment, a cross-linking process in which the cross-linking liquid is brought into contact with the film after dyeing treatment for cross-linking treatment, and a cleaning process in which the cleaning liquid is brought into contact with the film after cross-linking treatment for cleaning treatment can be exemplified. In addition, between these series of treatment processes (i.e., before and after any one or more treatment processes and / or in any one or more treatment processes), uniaxial stretching treatment is performed in a wet or dry manner. Other treatment processes may also be added as needed. The swelling step is performed for the purpose of removing foreign matter on the surface of the original film, removing plasticizers in the original film, imparting dyeability, plasticizing the original film, etc. As the swelling liquid, a medium mainly composed of water, such as water, distilled water, or pure water, is generally used. The cross-linking process is a treatment for the purpose of water resistance and color adjustment based on cross-linking. As a cross-linking liquid, a solution obtained by dissolving a cross-linking agent in a solvent can be used. As a cross-linking agent, boron compounds such as boric acid and borax can be mentioned. They can be one or more. As a solvent, water can be used, and an organic solvent compatible with water can also be included. The concentration of the cross-linking agent in the cross-linking liquid, the temperature of the cross-linking bath, the immersion time of the film, and the number of cross-linking baths in which the film is immersed are not particularly limited. By appropriately selecting them, a polarizing film with a boron content of 5.0% by mass or less can be obtained. In the case where the dichroic pigment used in the dyeing treatment is iodine, the cross-linking liquid preferably contains iodide in addition to boric acid, and the amount of iodide can be set to 1 to 30 parts by weight relative to 100 parts by weight of water, for example. As iodide, potassium iodide, zinc iodide, etc. can be mentioned. In addition, compounds other than iodide, such as zinc chloride, cobalt chloride, zirconium chloride, sodium thiosulfate, potassium sulfite, sodium sulfate, etc., can also coexist. The cross-linking treatment can be performed multiple times, usually 2 to 5 times. In this case, the composition and temperature of each cross-linking bath used may be the same or different. The cleaning process is carried out for the purpose of removing excess boric acid, iodine and other chemical reagents attached to the polyvinyl alcohol resin film. The cleaning process is carried out, for example, by immersing the cross-linked polyvinyl alcohol resin film in a cleaning bath containing a cleaning solution. It should be noted that the cleaning process can also be carried out by spraying the cleaning solution on the film in the form of a spray, or by using both immersion in the cleaning bath and spraying the cleaning solution, instead of the process of immersing the film in the cleaning bath. By adjusting the conditions of the cleaning process (such as the contact time with the cleaning solution, the temperature of the cleaning solution), the boron content of the polarizer finally obtained can be adjusted. As described above, the raw material film is subjected to a uniaxial stretching treatment in a wet or dry manner between the above series of treatment steps (i.e., before or after any one or more treatment steps and / or during any one or more treatment steps). The uniaxial stretching step can be performed multiple times during the period from the raw material film to obtaining a polarizing plate. The thickness of the polarizer is usually 65 μm or less, preferably 50 μm or less, more preferably 35 μm or less, further preferably 30 μm or less, and particularly preferably 20 μm or less. The thickness of the polarizer is usually 2 μm or more, preferably 5 μm or more, more preferably 10 μm or more, and further preferably 15 μm or more. The thickness of the polarizer can be controlled, for example, by the selection of the polyvinyl alcohol resin film, the adjustment of the stretching ratio, etc. (First Adhesive Layer and Second Adhesive Layer) The first adhesive layer 12 bonds the (meth) acrylic resin film 10 to the polarizer 20, and the second adhesive layer 14 bonds the protective film 30 to the polarizer 20. The first adhesive layer 12 and the second adhesive layer 14 are preferably a cured product of a curable adhesive containing a curable (polymerizable) compound. The curable compound is preferably an active energy ray-curable adhesive that is cured by heating or irradiation with active energy rays such as ultraviolet rays, visible light, electron beams, and X-rays. The polymerizable compound refers to a compound or oligomer that undergoes a polymerization reaction and cures by irradiation or heating with active energy rays such as ultraviolet rays, visible light, electron beams, and X-rays. Examples of the curable adhesive include epoxy adhesives and (meth)acrylic adhesives. The first adhesive layer and the second adhesive layer may be cured products of the same adhesive or cured products of different adhesives. (Epoxy adhesive) The epoxy adhesive contains an epoxy compound as a polymerizable compound. An epoxy compound refers to a compound having one or more, preferably two or more epoxy groups in a molecule. The epoxy compound may be used alone or in combination of two or more. The epoxy adhesive may further contain an oxetane compound, a vinyl compound, etc. as a polymerizable compound. Examples of the epoxy compound include alicyclic epoxy compounds, aromatic epoxy compounds, hydrogenated epoxy compounds, aliphatic epoxy compounds, etc. Among them, from the viewpoints of weather resistance, curing speed and adhesion, the epoxy compound preferably includes an alicyclic epoxy compound and an aliphatic epoxy compound, and more preferably includes an alicyclic epoxy compound. The alicyclic epoxy compound is a compound having one or more epoxy groups bonded to an alicyclic ring in the molecule. The "epoxy group bonded to an alicyclic ring" refers to the bridging oxygen atom -O- in the structure represented by the following formula (2). In the following formula (2), m is an integer of 2 to 5. [Chemical formula 2] The (CH2) in the above formula (2) is removed. m Compounds in which one or more hydrogen atoms are bonded to other chemical structures can become alicyclic epoxy compounds. (CH2) m One or more hydrogen atoms in the group may be appropriately substituted with a straight-chain alkyl group such as a methyl group or an ethyl group. Among them, the cured products of alicyclic epoxy compounds having a cyclopentane oxide structure (structure in which m=3 in the above formula (2)) and a cyclohexane oxide structure (structure in which m=4 in the above formula (2)) have a high glass transition temperature and are also advantageous in terms of adhesion between the polarizing film and the protective film. Specific examples of alicyclic epoxy compounds are listed below. Here, first, the compound names are listed, and then the chemical formulas corresponding to each are shown, and the same symbols are marked on the compound names and the chemical formulas corresponding to them. A: 3,4-epoxycyclohexylmethyl ester, B: 3,4-epoxy-6-methylcyclohexyl methyl ester, C: Ethylene bis(3,4-epoxycyclohexanecarboxylate), D: Bis(3,4-epoxycyclohexylmethyl) adipate, E: Bis(3,4-epoxy-6-methylcyclohexylmethyl) adipate, F: Diethylene glycol bis(3,4-epoxycyclohexyl methyl ether), G: Ethylene glycol bis(3,4-epoxycyclohexyl methyl ether), H: 2,3,14,15-diepoxy-7,11,18,21-tetraoxatrispiro[5.2.2.5.2.2]heneicosane, I: 3-(3,4-epoxycyclohexyl)-8,9-epoxy-1,5-dioxaspiro[5.5]undecane, J: 4-vinylcyclohexene dioxide, K: Limonene dioxide, L: Bis(2,3-epoxycyclopentyl) ether, M: dicyclopentadiene dioxide. [Chemical formula 3] [Chemical formula 4] Aromatic epoxy compounds are compounds having an aromatic ring and an epoxy group in the molecule. Specific examples thereof include: bisphenol-type epoxy compounds or oligomers thereof such as diglycidyl ether of bisphenol A, diglycidyl ether of bisphenol F, and diglycidyl ether of bisphenol S; phenol-formaldehyde epoxy resins such as phenol novolac epoxy resin, cresol novolac epoxy resin, and hydroxybenzaldehyde phenol novolac epoxy resin; polyfunctional epoxy compounds such as glycidyl ether of 2,2',4,4'-tetrahydroxydiphenylmethane and glycidyl ether of 2,2',4,4'-tetrahydroxybenzophenone; and polyfunctional epoxy resins such as epoxidized polyvinylphenol. The hydrogenated epoxy compound is a glycidyl ether of a polyol having an alicyclic ring, and may be a compound obtained by glycidyl etherifying a core hydrogenated polyol (Japanese: core water added polyol) obtained by selectively hydrogenating the aromatic ring of an aromatic polyol in the presence of a catalyst and under pressure. Specific examples of aromatic polyols include bisphenol-type compounds such as bisphenol A, bisphenol F, and bisphenol S; phenolic resins such as phenol novolac, cresol novolac, and hydroxybenzaldehyde phenol novolac; and polyfunctional compounds such as tetrahydroxydiphenylmethane, tetrahydroxybenzophenone, and polyvinylphenol. Glycidyl ethers can be prepared by reacting epichlorohydrin with an alicyclic polyol obtained by hydrogenating the aromatic ring of an aromatic polyol. As a preferred compound among hydrogenated epoxy compounds, diglycidyl ether of hydrogenated bisphenol A can be cited. Aliphatic epoxy compounds are compounds having at least one oxirane ring (three-membered cyclic ether) bonded to an aliphatic carbon atom in the molecule. For example, there are monofunctional epoxy compounds such as butyl glycidyl ether and 2-ethylhexyl glycidyl ether; bifunctional epoxy compounds such as 1,4-butanediol diglycidyl ether, 1,6-hexanediol diglycidyl ether, and neopentyl glycol diglycidyl ether; trifunctional or higher epoxy compounds such as trimethylolpropane triglycidyl ether and pentaerythritol tetraglycidyl ether; 4-vinylcyclohexene dioxide, limonene dioxide, and other epoxy compounds having one epoxy group directly bonded to an alicyclic ring and an oxirane ring bonded to an aliphatic carbon atom. Among them, from the viewpoint of adhesion between the polarizing film and the protective film, a bifunctional epoxy compound (also called an aliphatic diepoxy compound) having two oxirane rings bonded to an aliphatic carbon atom in the molecule is preferred. The above-mentioned suitable aliphatic diepoxy compound can be represented by the following formula (3), for example. [Chemical formula 5] In the above formula (3), Y is an alkylene group having 2 to 9 carbon atoms, an alkylene group having 4 to 9 carbon atoms in total with an ether bond interposed therebetween, or a divalent hydrocarbon group having 6 to 18 carbon atoms having an alicyclic structure. The aliphatic diepoxy compound represented by the formula (3) is specifically a diglycidyl ether of an alkanediol, a diglycidyl ether of an oligoalkylene glycol having a repeating number of about 4, or a diglycidyl ether of an alicyclic diol. Specific examples of glycols that can form the aliphatic diepoxy compound represented by the above formula (3) are shown below. Examples of alkanediols include ethylene glycol, propylene glycol, 1,3-propylene glycol, 2-methyl-1,3-propylene glycol, 2-butyl-2-ethyl-1,3-propylene glycol, 1,4-butanediol, neopentyl glycol, 3-methyl-2,4-pentanediol, 2,4-pentanediol, 1,5-pentanediol, 3-methyl-1,5-pentanediol, 2-methyl-2,4-pentanediol, 2,4-diethyl-1,5-pentanediol, 1,6-hexanediol, 1,7-heptanediol, 3,5-heptanediol, 1,8-octanediol, 2-methyl-1,8-octanediol, and 1,9-nonanediol. Examples of oligoalkylene glycols include diethylene glycol, triethylene glycol, tetraethylene glycol, and dipropylene glycol. Examples of the alicyclic diol include cyclohexanediol and cyclohexanedimethanol. Oxetane compounds, which are one of the cationic polymerizable compounds, are compounds containing one or more oxetane rings (oxetane groups) in the molecule, and specific examples thereof include 3-ethyl-3-hydroxymethyloxetane (also known as oxetane alcohol), 2-ethylhexyloxetane, 1,4-bis[{(3-ethyloxetane-3-yl)methoxy}methyl]benzene (also known as xylylenebisoxetane), 3-ethyl-3[{(3-ethyloxetane-3-yl)methoxy}methyl]oxetane, 3-ethyl-3-(phenoxymethyl)oxetane, and 3-(cyclohexyloxy)methyl-3-ethyloxetane. Oxetane compounds can be used as the main component of cationic polymerizable compounds, or they can be used in combination with epoxy compounds. By using oxetane compounds in combination, the curing speed and adhesion can sometimes be improved. Examples of the vinyl compound that can become a cationically polymerizable compound include aliphatic or alicyclic vinyl ether compounds, and specific examples thereof include vinyl ethers of alkyl alcohols or alkenyl alcohols having 5 to 20 carbon atoms, such as n-pentyl vinyl ether, isopentyl vinyl ether, n-hexyl vinyl ether, n-octyl vinyl ether, 2-ethylhexyl vinyl ether, n-dodecyl vinyl ether, stearyl vinyl ether, and oleyl vinyl ether; vinyl ethers containing a hydroxyl group, such as 2-hydroxyethyl vinyl ether, 3-hydroxypropyl vinyl ether, and 4-hydroxybutyl vinyl ether; vinyl ethers of monoalcohols having an aliphatic ring or an aromatic ring, such as cyclohexyl vinyl ether, 2-methylcyclohexyl vinyl ether, cyclohexyl methyl vinyl ether, and benzyl vinyl ether; glycerol monovinyl ether, 1,4-butanediol, and the like. Monovinyl ethers to polyvinyl ethers of polyhydric alcohols such as alcohol monovinyl ether, 1,4-butanediol divinyl ether, 1,6-hexanediol divinyl ether, neopentyl glycol divinyl ether, pentaerythritol divinyl ether, pentaerythritol tetravinyl ether, trimethylolpropane divinyl ether, trimethylolpropane trivinyl ether, 1,4-dihydroxycyclohexane monovinyl ether, 1,4-dihydroxycyclohexane divinyl ether, 1,4-dihydroxymethylcyclohexane monovinyl ether, and 1,4-dihydroxymethylcyclohexane divinyl ether; polyalkylene glycol monovinyl ethers to divinyl ethers such as diethylene glycol divinyl ether, triethylene glycol divinyl ether, and diethylene glycol monobutyl monovinyl ether; other vinyl ethers such as glycidyl vinyl ether and ethylene glycol vinyl ether methacrylate. The vinyl compound may be used as the main component of the cationically polymerizable compound, or may be used in combination with an epoxy compound, or an epoxy compound and an oxetane compound. By using a vinyl compound in combination, the curing speed may be increased or the viscosity of the adhesive may be reduced. The cationically polymerizable adhesive may further contain other curable compounds other than those described above. Specific examples of other curable compounds include other cationically polymerizable compounds other than those described above, such as lactone compounds, cyclic acetal compounds, cyclic sulfide compounds, and spiroorthoester compounds. In epoxy adhesives, from the viewpoint of suppressing the outflow of dichroic pigments such as iodine from the polarizer 20, when the total amount of curable compounds contained in the adhesive is set to 100% by weight, the content of all polymerizable compounds is preferably 80% by weight or more, more preferably 90% by weight or more, and even more preferably 100% by weight. Epoxy adhesives can be active energy ray curable or heat curable, preferably active energy ray curable. In the case of imparting active energy ray curability to the adhesive, it is preferred to incorporate a photocationic polymerization initiator in the adhesive. The photocationic polymerization initiator generates cationic species or Lewis acids by irradiation with active energy rays such as visible light, ultraviolet rays, X-rays or electron beams, and initiates the polymerization reaction of cationic curable compounds. The photocationic polymerization initiator exerts a catalytic effect through light, so even if it is mixed into a photocationic curable compound, the storage stability and workability are also excellent. As compounds that generate cationic species or Lewis acids by irradiation with active energy rays, for example, onium salts such as aromatic iodonium salts and aromatic sulfonium salts, aromatic diazonium salts, iron-arene complexes, etc. can be cited. The photocationic polymerization initiator may be used alone or in combination of two or more. Among them, aromatic sulfonium salts have ultraviolet absorption properties even in the wavelength region near 300 nm, so they are excellent in curability and can provide a cured product with good mechanical strength and bonding strength, so they are preferably used. The amount of the photocationic polymerization initiator is usually 0.5 to 10 parts by weight, preferably 6 parts by weight or less, relative to 100 parts by weight of the cationic polymerizable compound. By adding 0.5 parts by weight or more of the photocationic polymerization initiator, the cationic polymerizable compound can be fully cured, and the obtained optical laminate can be given high mechanical strength and bonding strength. On the other hand, if the amount is too much, the hygroscopicity of the cured product may increase due to the increase of the ionic substance in the cured product, and the durability of the polarizer may be reduced. ((Meth)acrylic adhesive) The (meth)acrylic adhesive contains a (meth)acrylate compound as a polymerizable compound. ((Meth)acrylate compound) The (meth)acrylate compound is a radical polymerizable compound having one or more (meth)acryloyloxy groups in the molecule. The adhesive composition may contain one or more (meth)acrylate compounds. Examples of the (meth)acrylate compound include a monofunctional (meth)acrylate compound having one (meth)acryloyloxy group in the molecule, a bifunctional (meth)acrylate compound having two (meth)acryloyloxy groups in the molecule, and a polyfunctional (meth)acrylate compound having three or more (meth)acryloyloxy groups in the molecule. The (meth)acrylate compound may contain one or more monofunctional (meth)acrylate compounds, bifunctional (meth)acrylate compounds, and polyfunctional (meth)acrylate compounds. An example of a monofunctional (meth)acrylate compound is an alkyl (meth)acrylate. Examples of the alkyl (meth)acrylate include methyl (meth)acrylate, ethyl (meth)acrylate, n-propyl (meth)acrylate, isopropyl (meth)acrylate, n-butyl (meth)acrylate, isobutyl (meth)acrylate, tert-butyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, isostearyl (meth)acrylate, and stearyl acrylate. Another example of the monofunctional (meth)acrylate compound includes an aromatic (meth)acrylate compound in which the group bonded to -O- of the ester bond (-C(=O)-O-) includes an aromatic ring, such as aralkyl (meth)acrylates such as benzyl (meth)acrylate, and phenoxy (meth)acrylates such as 2-phenoxyethyl (meth)acrylate, phenoxyethylene glycol (meth)acrylate, 2-hydroxy-3-phenoxypropyl (meth)acrylate, and ethoxylated o-phenylphenol (meth)acrylate. Alicyclic alkyl (meth)acrylate compounds containing an alicyclic ring in the group bonded to the -O- of the ester bond (-C(=O)-O-), such as cyclohexyl (meth)acrylate, cyclohexylmethyl (meth)acrylate, dicyclopentyl (meth)acrylate, 1,4-cyclohexanedimethanol mono(meth)acrylate, and isobornyl (meth)acrylate; (Meth)acrylic acid aminoalkyl ester compounds such as N,N-dimethylaminoethyl acrylate; (meth)acrylate compounds including an ether bond in the -O- bonded group of the ester bond (-C(=O)-O-) such as dicyclopentenyloxyethyl (meth)acrylate, ethyl carbitol (meth)acrylate, and tetrahydrofurfuryl (meth)acrylate, and other compounds other than those listed above. As another example of the monofunctional (meth)acrylate compound, for example, there can be mentioned (meth)acrylate compounds in which the group bonded to -O- of the ester bond (-C(=O)-O-) such as 2-hydroxyethyl (meth)acrylate, 2- or 3-hydroxypropyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, 2-hydroxy-3-phenoxypropyl (meth)acrylate, trimethylolpropane mono(meth)acrylate, and pentaerythritol mono(meth)acrylate contains a hydroxyl group; 2-carboxyethyl (meth)acrylate, ω-carboxy-poly(meth)acrylate, (Meth)acrylate compounds containing a carboxyl group in the -O-bonded group of an ester bond (-C(=O)-O-) such as caprolactone (n≈2) mono(meth)acrylate, 1-[2-(meth)acryloyloxyethyl]phthalate, 1-[2-(meth)acryloyloxyethyl]hexahydrophthalate, 1-[2-(meth)acryloyloxyethyl]succinate, 4-[2-(meth)acryloyloxyethyl]trimellitate, and N-(meth)acryloyloxy-N',N'-dicarboxymethyl-p-phenylenediamine. Examples of the bifunctional (meth)acrylate compound include alkylene glycol di(meth)acrylates, polyoxyalkylene glycol di(meth)acrylates, halogen-substituted alkylene glycol di(meth)acrylates, di(meth)acrylates of aliphatic polyols, di(meth)acrylates of hydrogenated dicyclopentadiene or tricyclodecanediol, di(meth)acrylates of dioxanediol or dioxanediol, di(meth)acrylates of alkylene oxide adducts of bisphenol A or bisphenol F, and epoxy di(meth)acrylates of bisphenol A or bisphenol F. More specific examples of the bifunctional (meth)acrylate compound include ethylene glycol di(meth)acrylate, 1,3-butanediol di(meth)acrylate, 1,4-butanediol di(meth)acrylate, 1,6-hexanediol di(meth)acrylate, 1,9-nonanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, trimethylolpropane di(meth)acrylate, pentaerythritol di(meth)acrylate, ditrimethylolpropane di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, dipropylene glycol di(meth)acrylate, tripropylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, polypropylene glycol di(meth)acrylate, polytetramethylene glycol di(meth)acrylate, silicone di(meth)acrylate, di(meth)acrylate of hydroxypivalic acid neopentyl glycol ester, 2 ,2-bis[4-(meth)acryloyloxyethoxyethoxyphenyl]propane, 2,2-bis[4-(meth)acryloyloxyethoxyethoxycyclohexyl]propane, hydrogenated dicyclopentadienyl di(meth)acrylate, tricyclodecane dimethanol di(meth)acrylate, 1,3-dioxane-2,5-diyl di(meth)acrylate [alias: dioxanediol di(meth)acrylate], acetal compound of hydroxypivalaldehyde and trimethylolpropane [chemical name: 2-(2-hydroxy-1,1-dimethylethyl)-5-ethyl-5-hydroxymethyl-1,3-dioxane] di(meth)acrylate, tri(hydroxyethyl)isocyanurate di(meth)acrylate, ethoxylated bisphenol A di(meth)acrylate, propoxylated bisphenol A di(meth)acrylate, ethoxylated bisphenol F di(meth)acrylate, propoxylated bisphenol F di(meth)acrylate, etc. The bifunctional (meth)acrylate preferably has at least one alicyclic skeleton or at least one aromatic ring in the molecule, and more preferably has at least one aromatic ring. From the viewpoint of moisture permeability of the cured product, compatibility with the maleic anhydride-modified compound described below, and adhesion to a resin film (particularly a (meth)acrylic resin film), the bifunctional (meth)acrylate preferably contains a compound represented by the following formula (4). [Chemical formula 6] (Where R 1 and R 2 Each independently represents a hydrogen atom or a methyl group, X represents ethylene oxide (-C2H4O-) or propylene oxide (-C3H6O-), n represents an integer of 1 to 20, and m represents an integer of 1 to 20. X is preferably ethylene oxide. The average of the total of m and n is preferably 2-20, more preferably 3-15, and particularly preferably 4-13. Examples of the polyfunctional (meth)acrylate compound having three or more (meth)acryloyloxy groups in the molecule include poly(meth)acrylates of trifunctional or higher aliphatic polyols such as glycerol tri(meth)acrylate, alkoxylated glycerol tri(meth)acrylate, trimethylolpropane tri(meth)acrylate, ditrimethylolpropane tri(meth)acrylate, ditrimethylolpropane tetra(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol tetra(meth)acrylate, dipentaerythritol penta(meth)acrylate and dipentaerythritol hexa(meth)acrylate; Poly(meth)acrylates of halogen-substituted polyols having three or more functional groups; Alkylene oxide adducts of glycerol tri(meth)acrylates; Tri(meth)acrylate of an alkylene oxide adduct of trimethylolpropane; 1,1,1-Tris[(meth)acryloyloxyethoxyethoxy]propane; Tris(hydroxyethyl)isocyanurate tri(meth)acrylate, etc. From the viewpoint of reducing the viscosity of the acrylic adhesive and the viewpoint of the adhesiveness of the acrylic adhesive to the polarizer 20 and the films 10 and 30 , the (meth)acrylate compound preferably contains a monofunctional (meth)acrylate compound. From the viewpoint of reducing the viscosity of the acrylic adhesive and the adhesive ability of the adhesive to the polarizer 20 and the films 10 and 30, the monofunctional (meth)acrylate compound preferably includes at least one compound selected from the group consisting of alicyclic alkyl (meth)acrylate compounds and aromatic (meth)acrylate compounds. Among them, from the viewpoint of reducing the moisture permeability (hereinafter sometimes referred to as low moisture permeability) of the cured film formed by the acrylic adhesive, alicyclic alkyl (meth)acrylate compounds are more preferred. When the total amount of the (meth)acrylic adhesive is set to 100 mass %, the content of the (meth)acrylate compound is generally 15 mass % to 75 mass %, and from the viewpoint of the bonding ability to the polarizer 20 and the films 10 and 30, it is preferably 15 mass % to 70 mass %, more preferably 20 mass % to 60 mass %, and further preferably 30 mass % to 55 mass %. When the total amount of the (meth)acrylate compound is set to 100 mass %, the content of the monofunctional (meth)acrylate compound is usually 60 mass % or more, and from the viewpoint of the adhesion between the polarizer 20 and the films 10 and 30, it is preferably 70 mass % or more, and more preferably 80 mass % or more. When the total amount of the (meth)acrylate compound is set to 100 mass %, the content of the monofunctional (meth)acrylate compound can be 100 mass %, and from the viewpoint of the mechanical strength of the cured product of the (meth)acrylic adhesive and the mechanical strength of the polarizing plate produced using the adhesive, it is preferably 99 mass % or less, more preferably 98 mass % or less, and can be 90 mass % or less. When the content of the monofunctional (meth)acrylate compound is less than 100% by mass, the remainder of the (meth)acrylate compound is a bifunctional (meth)acrylate compound and / or a polyfunctional (meth)acrylate compound, and preferably contains a bifunctional (meth)acrylate compound. When the total amount of the (meth)acrylate compounds is 100 mass %, the content of the bifunctional (meth)acrylate compound is preferably 0.5 mass % or more, more preferably 1 mass % or more, and preferably 10 mass % or less, more preferably 5 mass % or less. (Maleic anhydride modified compound) The (meth)acrylic adhesive is suitable for further comprising a maleic anhydride-modified compound. A maleic anhydride-modified compound is a compound containing a maleic anhydride structure in the molecule. The (meth)acrylic adhesive may comprise one maleic anhydride-modified compound, or may comprise two or more maleic anhydride-modified compounds. Examples of the maleic anhydride-modified compound include maleic anhydride-modified polymers. The maleic anhydride-modified polymer is a polymer modified by introducing a maleic anhydride structure as a side chain of the polymer. The adhesive composition may contain one maleic anhydride-modified polymer or may contain two or more maleic anhydride-modified polymers. The maleic anhydride structure is a structure represented by the following formula (5). [Chemical formula 7] (* indicates the bond to the main chain.) Among maleic anhydride-modified polymers, polymers modified by maleic anhydride include diene polymers, polyolefin polymers, (meth)acrylic polymers, polyester polymers, polystyrene polymers, polyether polymers, etc. These polymers may be homopolymers composed of one monomer or copolymers composed of two or more monomers. In the present specification, "(meth)acrylic" means at least one selected from acrylic and methacrylic groups. The same applies to expressions such as "(meth)acryloyl" and "(meth)acrylate". The maleic anhydride-modified polymer is preferably in a liquid state from the viewpoint of being able to prepare a solvent-free adhesive composition having good adhesiveness. The liquid state means that the polymer exhibits fluidity at a temperature of 25°C. From the viewpoint of obtaining an adhesive composition with good coating properties, the viscosity of the liquid maleic anhydride-modified polymer at 25°C is preferably from 10 Pa·sec to 10,000 Pa·sec, more preferably from 15 Pa·sec to 7,000 Pa·sec, further preferably from 15 Pa·sec to 300 Pa·sec, and particularly preferably from 15 Pa·sec to 100 Pa·sec. A preferred example of a liquid maleic anhydride-modified polymer is maleic anhydride-modified polybutadiene. These polymers may be either homopolymers or copolymers, and are preferably homopolymers. The number average molecular weight of the maleic anhydride-modified polymer is usually 500 to 15,000, preferably 600 to 12,000, more preferably 700 to 10,000, further preferably 2,000 to 10,000, and particularly preferably 3,500 to 10,000, from the viewpoint of viscosity and coating properties. The number average molecular weight of the maleic anhydride-modified polymer can be measured as a standard polystyrene conversion value based on gel permeation chromatography (GPC). The acid value of the maleic anhydride modified polymer is usually 10KOHmg / g or more and 200KOHmg / g or less. From the viewpoint of the adhesive ability of the adhesive composition to the protective film, it is preferably 15KOHmg / g or more and 150KOHmg / g or less, more preferably 20KOHmg / g or more and 100KOHmg / g or less, further preferably 30KOHmg / g or more and 100KOHmg / g or less, and particularly preferably 45KOHmg / g or more and 100KOHmg / g or less. Using a maleic anhydride modified polymer having an acid value in this range is advantageous in improving the adhesive ability of the adhesive composition to the protective film, and is particularly advantageous in providing an adhesive composition having high adhesion between the polyvinyl alcohol-based polarizer and the thermoplastic resin film when a polyvinyl alcohol-based polarizer is used as the polarizer. The acid value of the maleic anhydride-modified polymer is measured by a neutralization titration method using phenolphthalein as an indicator in accordance with JIS K 0070:1992. When the total amount of the (meth)acrylic adhesive is set to 100 mass %, the content of the maleic anhydride modified compound is usually 3 mass % or more and 40 mass % or less. From the viewpoint of bonding ability, especially when a polyvinyl alcohol polarizer is used as a polarizer, from the viewpoint of improving the adhesion between the polyvinyl alcohol polarizer and the films 10 and 30, it is preferably 5 mass % or more and 35 mass % or less, and more preferably 10 mass % or more and 30 mass % or less. (Photopolymerization Initiator) The (meth)acrylic adhesive preferably contains a photopolymerization initiator. The photopolymerization initiator is not particularly limited as long as it is a compound that generates active radicals, acids, etc. by the action of light and can initiate polymerization of a (meth)acrylate compound. The adhesive composition may contain only one photopolymerization initiator or two or more photopolymerization initiators. The photopolymerization initiator is not particularly limited, and examples thereof include oxime compounds such as O-acyl oxime compounds, alkyl phenone compounds, and acyl phosphine oxide compounds. The O-acyl oxime compound is a compound having a structure represented by the following formula (6): Hereinafter, * represents a connecting bond. [Chemical formula 8] Examples of the O-acyl oxime compound include N-benzoyloxy-1-(4-phenylsulfanylphenyl)butane-1-one-2-imine, N-benzoyloxy-1-(4-phenylsulfanylphenyl)octane-1-one-2-imine, N-benzoyloxy-1-(4-phenylsulfanylphenyl)-3-cyclopentylpropane-1-one-2-imine, N-acetoxy-1-[9-ethyl-6-(2-methylbenzoyl)-9H-carbazole-3-yl]ethane-1-imine, N-acetoxy-1-[9-ethyl-6-{2-methyl-4-(3,3-dimethyl-2,4-dioxolanylmethoxy)benzoyl}-9H-carbazole-3-

[0013] N-acetoxy-1-[4-(2-hydroxyethoxy)phenylsulfanylphenyl]propane-1-one-2-imine, N-acetoxy-1-[4-(1-methyl-2-methoxyethoxy)-2-methylphenyl]-1-(9-ethyl-6-nitro-9H-carbazole-3-yl)methane-1-imine, and the like. Commercially available products such as Irgacure (trade name) OXE01, Irgacure OXE02, Irgacure OXE03 (all manufactured by BASF), N-1919, NCI-930, and NCI-831 (all manufactured by ADEKA) can be used. The alkylphenone compound is a compound having a partial structure represented by the following formula (6a) or a partial structure represented by the following formula (6b). In these partial structures, the benzene ring may have a substituent. [Chemical formula 9] Examples of the compound having a structure represented by formula (6a) include 2-methyl-2-morpholino-1-(4-methylsulfanylphenyl)propane-1-one, 2-dimethylamino-1-(4-morpholinophenyl)-2-benzylbutane-1-one, and 2-(dimethylamino)-2-[(4-methylphenyl)methyl]-1-[4-(4-morpholinyl)phenyl]butane-1-one. Commercially available products such as Omnirad (trade name) 369, Omnirad 907, and Omnirad 379 (all manufactured by IGM Resins B.V.) can be used. Examples of the compound having a structure represented by formula (6b) include 2-hydroxy-2-methyl-1-phenylpropane-1-one, 2-hydroxy-2-methyl-1-[4-(2-hydroxyethoxy)phenyl]propane-1-one, 1-hydroxycyclohexyl phenyl ketone, oligomers of 2-hydroxy-2-methyl-1-(4-isopropenylphenyl)propane-1-one, α,α-diethoxyacetophenone, and benzil dimethyl ketal. Commercially available products such as Omnirad (trade name) 184 (manufactured by IGM Resins BV) can be used. Examples of the acylphosphine oxide compound include phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide (for example, trade name “Omnirad 819” (manufactured by IGM Resins BV)) and 2,4,6-trimethylbenzoyldiphenylphosphine oxide. Further examples of the photopolymerization initiator (C) include benzoin compounds such as benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, and benzoin isobutyl ether; benzophenone compounds such as benzophenone, methyl o-benzoylbenzoate, 4-phenylbenzophenone, 4-benzoyl-4'-methyldiphenyl sulfide, 3,3',4,4'-tetrakis(tert-butylperoxycarbonyl)benzophenone, 2,4,6-trimethylbenzophenone, and 4,4'-bis(N,N'-dimethylamino)-benzophenone; Xanthone compounds such as 2-isopropylthioxanthone and 2,4-diethylthioxanthone; Anthracene compounds such as 9,10-dimethoxyanthracene, 2-ethyl-9,10-dimethoxyanthracene, 9,10-diethoxyanthracene, and 2-ethyl-9,10-diethoxyanthracene; Quinone compounds such as 9,10-phenanthrenequinone, 2-ethylanthraquinone, and camphorquinone; Benzil, methyl phenylglyoxylate, titanocene compounds, etc. When the total amount of the (meth)acrylic adhesive composition is set to 100 mass %, the content of the photopolymerization initiator is usually 0.1 mass % to 20 mass %, and is preferably 0.5 mass % to 15 mass % from the viewpoint of the curability of the (meth)acrylic adhesive and the bonding ability to the polarizer 20 and the films 10 and 30, and is more preferably 1 mass % to 10 mass % (for example, 8 mass % or less). When the total amount of the (meth)acrylate compound is set to 100 parts by mass, the content of the photopolymerization initiator is usually 0.1 parts by mass or more and 30 parts by mass or less. From the viewpoint of the curability of the (meth)acrylic adhesive and the bonding ability to the polarizer 20 and the films 10 and 30, it is preferably 0.5 parts by mass or more and 20 parts by mass or less, and more preferably 1 part by mass or more and 10 parts by mass or less. (Petroleum resin) The acrylic adhesive may further contain a petroleum resin. By making the (meth) acrylic adhesive composition further contain a petroleum resin, the moisture permeability of the cured film can be reduced. The adhesive capable of forming a cured film with low moisture permeability is suitable for applications requiring the suppression of the entry and exit of moisture through the cured film. For example, in a polarizing plate having a protective film laminated on at least one surface of a polarizer by means of an adhesive layer or an image display panel including the polarizing plate, if the adhesive layer has low moisture permeability, the curling (warping) of the polarizing plate or the image display panel caused by the entry and exit of moisture can be suppressed. The (meth)acrylic adhesive further containing a petroleum resin may be advantageous in terms of improving the adhesion between the polarizer and the thermoplastic resin film. Examples of the petroleum resin include aromatic petroleum resins, aliphatic petroleum resins, cycloaliphatic petroleum resins, aliphatic / aromatic petroleum resins, and coumarone-based resins, and examples thereof include hydrogenated petroleum resins of these resins. The aromatic petroleum resin is a resin containing one or two or more structural units derived from aromatic hydrocarbons, and may be a resin obtained by hydrogenating the resin or a resin obtained by modifying the resin. The aromatic petroleum resin is preferably a C9 petroleum resin. The C9 petroleum resin is a resin obtained by copolymerizing a C9 fraction, and may be a resin obtained by hydrogenating the resin or a resin obtained by modifying the resin. The C9 petroleum resin may be a resin obtained by copolymerizing a C9 fraction with other monomer components, a resin obtained by hydrogenating the resin, or a resin obtained by modifying the resin. As other monomer components, a C5 fraction may be mentioned. Examples of the C9 fraction include petroleum fractions having about 8 to 10 carbon atoms, such as styrene, alkylstyrene, vinyltoluene, 1-methyl-1-phenylethylene, indene, and methylindene. Examples of the C5 fraction include petroleum fractions having about 4 to 5 carbon atoms, such as cyclopentadiene, pentene, pentadiene, and piperylene. In addition, the petroleum resin may be a C5-based petroleum resin obtained by copolymerizing the above-mentioned C5 fraction, a resin obtained by hydrogenating the C5-based petroleum resin, or a resin obtained by modifying the resin. In addition, it may be an alicyclic hydrocarbon resin obtained by polymerizing the C5 fraction after cyclodimerization. Examples of the alicyclic hydrocarbon resin include polymers containing structural units derived from dicyclopentadiene. The weight average molecular weight of the petroleum resin is usually 500 to 10,000, preferably 500 to 7,000, more preferably 600 to 5,000, further preferably 60 to 3,000, and particularly preferably 600 to 1,500, from the viewpoint of reducing the moisture permeability of the cured film formed by the adhesive composition and the adhesion of the adhesive composition to the protective film (or layer). The weight average molecular weight of the petroleum resin can be measured as a standard polystyrene conversion value based on gel permeation chromatography (GPC). In the case where the acrylic adhesive composition contains a petroleum resin, when the total amount of the adhesive is set to 100 mass%, from the viewpoint of reducing the moisture permeability of the cured film, from the viewpoint of the adhesion ability of the adhesive composition to the protective film, and especially from the viewpoint of improving the adhesion between the polyvinyl alcohol polarizer and the protective film when a polyvinyl alcohol polarizer is used as the polarizer, the content of the petroleum resin is preferably from 20 mass% to 70 mass%, and more preferably from 30 mass% to 65 mass%. When the acrylic adhesive contains a monofunctional (meth)acrylate compound and a petroleum resin, the mass ratio thereof (monofunctional (meth)acrylate compound / petroleum resin) is preferably 0.5 or more and 3.0 or less, more preferably 0.7 or more and 2.0 or less, further preferably 0.9 or more and 1.5 or less, and even more preferably 1.0 or more and 1.3 or less, from the viewpoint of reducing the moisture permeability of a cured film formed from the adhesive composition, from the viewpoint of the adhesion ability of the adhesive composition to the protective film, and especially from the viewpoint of improving the adhesion between the polyvinyl alcohol polarizer and the protective film when a polyvinyl alcohol polarizer is used as the polarizer. (additive) The first adhesive and / or the second adhesive may contain other additives as needed. Specific examples of additives include ion traps, antioxidants, chain transfer agents, polymerization accelerators (polyols, etc.), sensitizers, sensitizing aids, light stabilizers, tackifiers, thermoplastic resins, fillers, flow regulators, plasticizers, defoamers, leveling agents, silane coupling agents, pigments, antistatic agents, ultraviolet absorbers, and thermal polymerization initiators. It should be noted that in the case of preparing a thermosetting adhesive, a thermal polymerization initiator is used instead of a photopolymerization initiator. As ion traps, powdered bismuth, antimony, magnesium, aluminum, calcium, titanium, and mixed inorganic compounds thereof can be cited, and as antioxidants, hindered phenol antioxidants can be cited. The thickness of the first adhesive layer 150 and the second adhesive layer 160 is preferably 20 μm or less, more preferably 15 μm or less, further preferably 10 μm or less, and may be 5 μm or less, and may be 0.05 μm or more, and may be 0.5 μm or more. (Protective film 30) The protective film 30 is not particularly limited as long as it is a transparent optical film. For example, the protective film may be a film of a polyolefin resin such as polyethylene, polypropylene, or cyclic polyolefin; a cellulose acetate resin such as triacetyl cellulose or diacetyl cellulose; a polyester resin such as polyethylene terephthalate, polyethylene naphthalate, or polybutylene terephthalate; a polycarbonate resin, a (meth)acrylic resin, or a polypropylene resin. In particular, the protective film 30 is preferably a cyclic polyolefin-based resin film. Cyclic polyolefin resin is a general term for resins obtained by polymerizing cyclic olefins as polymerization units, and examples thereof include resins described in JP-A-1-240517, JP-A-3-14882, JP-A-3-122137, and the like. Specific examples of cyclic polyolefin resins include ring-opening (co)polymers of cyclic olefins, addition polymers of cyclic olefins, copolymers of cyclic olefins with chain olefins such as ethylene and propylene (representatively random copolymers), graft polymers formed by modifying them with unsaturated carboxylic acids and their derivatives, and their hydrogenated products. Among them, it is preferable to use a norbornene-based resin obtained by polymerizing a norbornene-based monomer such as norbornene, which is a cyclic olefin, or a polycyclic norbornene-based monomer. From the viewpoint of thinning, the thickness of the protective film 30 is usually 100 μm or less, preferably 80 μm or less, more preferably 65 μm or less, and is usually 15 μm or more, preferably 20 μm or more. The protective film 30 may have a phase difference. When the protective film 30 is a retardation film, the machine flow direction (MD direction) from the die during film formation of the protective film 30 and the direction of the absorption axis of the polarizer 20 are not particularly limited, but are preferably parallel to each other. (Adhesive layer 40) The adhesive layer 40 is attached to the outer surface of the protective film 30. The adhesive layer 40 can be used to bond the polarizing plate 100 to a display element (eg, a liquid crystal cell) or other optical members. A release film is preferably laminated on the lower surface of the adhesive layer 40. The material of the adhesive layer 40 is not particularly limited. The adhesive layer can be composed of an adhesive composition having a resin such as (meth) acrylic acid, rubber, urethane, ester, silicone, or polyvinyl ether as a main component. Among them, an adhesive composition having a (meth) acrylic acid resin having excellent transparency, weather resistance, heat resistance, etc. as a base polymer is suitable. The adhesive composition can be an active energy ray curable type or a heat curable type. As the (meth)acrylic resin (base polymer) used in the adhesive composition, for example, a polymer or copolymer using one or more of (meth)acrylates such as butyl (meth)acrylate, ethyl (meth)acrylate, isooctyl (meth)acrylate, and 2-ethylhexyl (meth)acrylate as monomers is preferably used. Preferably, a polar monomer is copolymerized with the base polymer. Examples of the polar monomer include monomers having a carboxyl group, a hydroxyl group, an amide group, an amino group, an epoxy group, and the like, such as (meth)acrylic acid, 2-hydroxypropyl (meth)acrylate, hydroxyethyl (meth)acrylate, (meth)acrylamide, N,N-dimethylaminoethyl (meth)acrylate, and glycidyl (meth)acrylate. The adhesive composition may contain only the above-mentioned base polymer, but usually further contains a crosslinking agent. Examples of the crosslinking agent include a crosslinking agent that is a divalent or higher metal ion and forms a carboxylic acid metal salt with a carboxyl group; a crosslinking agent that is a polyamine compound and forms an amide bond with a carboxyl group; a crosslinking agent that is a polyepoxide compound or a polyol and forms an ester bond with a carboxyl group; and a crosslinking agent that is a polyisocyanate compound and forms an amide bond with a carboxyl group. Among them, polyisocyanate compounds are preferred. The active energy ray-curable adhesive composition refers to an adhesive composition that has the property of being cured by being irradiated with active energy rays such as ultraviolet rays and electron beams, and has the property of being adhesive before being irradiated with active energy rays and being able to be closely attached to adherends such as films, and being cured by being irradiated with active energy rays so as to adjust the close adhesion. The active energy ray-curable adhesive composition is preferably an ultraviolet curable adhesive composition. The active energy ray-curable adhesive composition contains an active energy ray polymerizable compound in addition to a base polymer and a crosslinking agent. In addition, a photopolymerization initiator, a photosensitizer, etc. may also be contained as needed. The adhesive composition may contain additives such as microparticles, microbeads (resin microbeads, glass microbeads, etc.), glass fibers, resins other than base polymers, antistatic agents, thickeners, fillers (metal powders, other inorganic powders, etc.), antioxidants, ultraviolet absorbers, dyes, pigments, colorants, defoaming agents, anticorrosive agents, photopolymerization initiators, etc., for imparting light scattering properties. The thickness of the adhesive layer 40 is usually 1 to 40 μm, and preferably 3 to 25 μm (eg 3 to 20 μm, more preferably 3 to 15 μm) from the viewpoint of thinning the optical sheet and suppressing dimensional changes of the polarizing plate 100 while maintaining good processability. (Storage modulus) The storage modulus of the adhesive layer 40 at 25°C and a measurement frequency of 1 Hz is 1.5×10 5 Pa or less, it can be 1.3×105 Pa or less, and can also be 1.0×10 5 Pa or less, and can also be 5.0×10 4 Pa or less. In addition, the storage modulus of the adhesive layer 40 at 25°C and a measurement frequency of 1 Hz can be 5.0×10 3 Pa or more, and can also be 1.0×10 4 Pa or more. The storage modulus of the adhesive layer at 25°C and a measurement frequency of 1 Hz can be measured using a rheometer. For example, the adhesive layer is stacked in a manner of 200 μm to prepare a measurement sample, and a rheometer ("MCR-301" (trade name) manufactured by Anton Parr Co., Ltd., PP25 is used for parallel plates) is used to measure the storage modulus at a strain of 1% and a frequency of 1 Hz at a temperature of 10°C / min, and the value of the storage modulus at 25°C is read, thereby obtaining the storage modulus. The storage modulus of the adhesive layer 40 at 25°C and a measurement frequency of 1 Hz can be set to a desired value by adjusting, for example, the type of resin of the main component of the adhesive composition (e.g., the type of the constituent monomer of the resin, and the mixing ratio thereof in the case of multiple constituent monomers), molecular weight (weight average molecular weight, number average molecular weight), glass transition temperature, type and mixing amount of the crosslinking agent in the adhesive composition, etc. In addition, when the adhesive layer 40 is formed of an active energy ray-curable adhesive composition, in addition to adjusting the above-mentioned resin and crosslinking agent, the desired storage modulus can also be obtained by adjusting the type and mixing amount of the active energy ray-polymerizable compound. (Effect) It is believed that if the (meth) acrylic resin film 10 is hard to a certain extent, the structure of the (meth) acrylic resin film 10 becomes dense, and thus the solvent resistance becomes excellent. In addition, if the (meth) acrylic resin protective film 10 is hard to a certain extent and the adhesive layer 40 is soft to a certain extent, when the polarizing plate 100 attached to the substrate is placed in a high temperature and high humidity environment, even if the polarizer 20 shrinks, the adhesive layer 40 will deform and absorb the stress, so the device including the polarizing plate 100 and the substrate (liquid crystal panel, etc.) is not easy to warp as a whole. Such a polarizing plate can be applied not only to a general liquid crystal display device but also to various image display devices such as an electroluminescent display device, a plasma display device, and a field emission display device. Example [Preparation of (meth)acrylic resin film I] Polymethyl methacrylate (Mw = 48 × 10 3, Mw / Mn=2.0) were melt-kneaded at 245° C. by an extruder and supplied to a T-die set at 245° C. The film-shaped molten resin extruded from the T-die was sandwiched between the first and second cooling rolls arranged opposite to each other, and wound around the third cooling roll for molding and cooling to obtain a resin film. The glass transition temperature of this film was measured and found to be 115.0°C. The film was subjected to sequential biaxial stretching. The film was stretched longitudinally to 1.8 times at a temperature 20°C higher than the glass transition temperature to obtain a longitudinally stretched film. Subsequently, the film was stretched transversely to 1.8 times at a temperature 20°C higher than the glass transition temperature to obtain a biaxially stretched film having a thickness of 40 μm. [Preparation of (meth)acrylic resin film II] Polymethyl methacrylate (Mw = 48 × 10 3 , Mw / Mn=2.0) were melt-kneaded at 245° C. by an extruder and supplied to a T-die set at 245° C. The film-shaped molten resin extruded from the T-die was sandwiched between the first and second cooling rolls arranged opposite to each other, and wound around the third cooling roll for molding and cooling to obtain a resin film. The glass transition temperature of this film was measured and found to be 115.4°C. The film was subjected to sequential biaxial stretching. The film was stretched to 2.0 times in the longitudinal direction at a temperature 20°C higher than the glass transition temperature to obtain a longitudinally stretched film. Then, the film was stretched to 2.0 times in the transverse direction at a temperature 20°C higher than the glass transition temperature to obtain a biaxially stretched film having a thickness of 40 μm. [Preparation of (meth)acrylic resin film III] A (meth)acrylic resin (Mw = 107 × 10 3, Mw / Mn=2.6), 72 parts by mass of a copolymer (SMA700, manufactured by Jiaxing Huawen Chemical Co.) of styrene / maleic anhydride=18 / 82 (mass ratio), and 20 parts by mass of (meth)acrylic rubber particles as a (meth)acrylic multilayer polymer consisting of a three-layer structure (first layer (innermost layer): a copolymer of methyl methacrylate and methyl acrylate and allyl methacrylate (mass ratio 93.8 / 6.0 / 0.2) / second layer: a copolymer of butyl acrylate and styrene and allyl methacrylate (mass ratio 80.6 / 17.4 / 2.0) / third layer (outermost layer): a copolymer of methyl methacrylate and methyl acrylate (mass ratio 94 / 6)) were melt-kneaded at 245°C using an extruder and supplied to a T-die set at 245°C. The film-shaped molten resin extruded from the T-die was sandwiched between the first cooling roll and the second cooling roll disposed opposite to each other, and was wound around the third cooling roll to be shaped and cooled, thereby obtaining an unstretched film having a thickness of 70 μm. The glass transition temperature of this film was measured and found to be 102.8°C. [Preparation of (meth)acrylic resin film IV] A (meth)acrylic resin (Mw = 107 × 10 3 , Mw / Mn=2.6) 64 parts by mass of a methacrylic resin (homopolymer of methyl methacrylate, Mw=69×10 3 , Mw / Mn=1.1) and 20 parts by mass of (meth)acrylic rubber particles as a (meth)acrylic multilayer polymer consisting of a three-layer structure (first layer (innermost layer): copolymer of methyl methacrylate and methyl acrylate and allyl methacrylate (mass ratio 93.8 / 6.0 / 0.2) / second layer: copolymer of butyl acrylate and styrene and allyl methacrylate (mass ratio 80.6 / 17.4 / 2.0) / third layer (outermost layer): copolymer of methyl methacrylate and methyl acrylate (mass ratio 94 / 6)) were melt-kneaded at 245°C by an extruder and supplied to a T-die set at a temperature of 245°C. The film-like molten resin extruded from the T-die was sandwiched between the first cooling roll and the second cooling roll arranged opposite to each other, and was wound around the third cooling roll for molding and cooling to obtain an unstretched film with a thickness of 60μm. The glass transition temperature of this film was measured and found to be 104.0°C. [Preparation of (meth)acrylic resin film V] A (meth)acrylic resin (Mw = 111 × 10 3 , Mw / Mn=2.0) and 30 parts by mass of (meth)acrylic rubber particles as a (meth)acrylic multilayer polymer consisting of a three-layer structure (first layer (innermost layer): copolymer of methyl methacrylate and methyl acrylate and allyl methacrylate (mass ratio 93.8 / 6.0 / 0.2) / second layer: copolymer of butyl acrylate and styrene and allyl methacrylate (mass ratio 80.6 / 17.4 / 2.0) / third layer (outermost layer): copolymer of methyl methacrylate and methyl acrylate (mass ratio 94 / 6)) were melt-kneaded at 245°C by an extruder and supplied to a T-die set at a temperature of 245°C. The film-like molten resin extruded from the T-die was sandwiched between the first cooling roll and the second cooling roll arranged opposite to each other, and was wound around the third cooling roll for molding and cooling to obtain an unstretched film with a thickness of 60μm. The glass transition temperature of this film was measured and found to be 98.9°C. [Curable Adhesive Composition A (Epoxy-based)] The curable adhesive composition A is prepared by mixing 20 parts by mass of 3',4'-epoxycyclohexylmethyl 3,4-epoxycyclohexanecarboxylate (trade name "Celloxide 2021P" manufactured by Daicel Co., Ltd.), 70 parts by mass of neopentyl glycol diglycidyl ether (trade name "EX-211L" manufactured by Nagase ChemteX Co., Ltd.), 2 parts by mass of 4-hydroxybutyl vinyl ether (trade name "HBVE" manufactured by NIPPON CARBIDE INDUSTRIES), 8 parts by mass of methyl methacrylate-methacrylic acid glycidyl ether copolymer (cationic polymerizable polymer) (trade name "MARPROOF G-01100" manufactured by NOF Corporation), and 2.25 parts by mass of a solid content of a photopolymerization initiator (trade name "CPI-100P" manufactured by San-Apro Co., Ltd.), and degassing. [Curable Adhesive Composition B (Epoxy-based)] The curable adhesive composition B is prepared by mixing 70 parts by mass of 3',4'-epoxycyclohexylmethyl 3,4-epoxycyclohexanecarboxylate (trade name "Celloxide 2021P" manufactured by Daicel Co., Ltd.), 20 parts by mass of neopentyl glycol diglycidyl ether (trade name "EX-211" manufactured by Nagase ChemteX Co., Ltd.), 10 parts by mass of 2-ethylhexyl glycidyl ether (trade name "EX-121" manufactured by Nagase ChemteX Co., Ltd.) and 2.8 parts by mass of a solid content of a photopolymerization initiator (trade name "CPI-100P" manufactured by San-Apro Co., Ltd.), and degassing. [Curable Adhesive Composition C ((Meth) Acrylic)] Curable adhesive composition C is composed of 17 parts by mass of maleic anhydride-modified liquid polybutadiene (trade name "Lithene ultra N4-5000-10MA" manufactured by Synthomer Co., Ltd., number average molecular weight: 5500, viscosity at 25°C: 25 to 60 Pa·sec, acid value: 54 KOHmg / g), 34 parts by mass of dicyclopentanyl acrylate (trade name "FA-513AS" manufactured by Hitachi Chemical Co., Ltd.), 12 parts by mass of stearyl acrylate (trade name "STA" manufactured by Osaka Organic Chemical Co., Ltd.), 2 parts by mass of ethoxylated bisphenol A diacrylate (trade name "A-BPE-10" manufactured by Shin-Nakamura Chemical Co., Ltd., EO 10 mol), 5.0 parts by mass of tricyclodecane dimethanol diacrylate (trade name (A-DCP) manufactured by Shin-Nakamura Chemical Co., Ltd.), and petroleum resin (trade name "T-REZ HA105", a hydrogenated resin (alicyclic saturated hydrocarbon resin with dicyclopentadiene as a monomer component), softening point (nominal value): 104.5°C, weight average molecular weight (nominal value): 610) 30 parts by mass are mixed, 3.0 parts by mass of phenylbis(2,4,6-trimethylbenzoyl)phosphine oxide (trade name "Omnirad 819" manufactured by IGM Resins BV) is added to 100 parts by mass of the total weight, and the mixture is degassed to prepare the product. Example 1 [Production of polarizing plate] The surface (inside of the roll) of the (meth) acrylic resin film I was subjected to a corona treatment, and a curable adhesive composition A was applied to the corona treated surface using an adhesive coating device. The obtained coating layer was laminated with a polyvinyl alcohol-iodine polarizer I having a thickness of 23 μm and a boron content of 4.2% by mass using a nip roller to obtain a polarizer with a (meth) acrylic resin film I. In the polarizer with a (meth) acrylic resin film I, the mechanical flow direction (MD direction) of the (meth) acrylic resin film I was parallel to the absorption axis of the polarizer. Next, a 50 μm thick phase difference film (trade name "ZEONOR" manufactured by ZEON Co., Ltd., Japan) formed of a cyclic polyolefin resin was subjected to a corona treatment, and a curable adhesive composition B was applied to the corona treated surface using an adhesive coating device. The obtained coating layer was laminated with the polarizer surface of the polarizer with a (meth) acrylic resin film I using a clamping roller to obtain a laminate. In the laminate, the mechanical flow direction (MD direction) of the phase difference film is parallel to the absorption axis of the polarizer. The total integrated light intensity (integrated intensity of light irradiation in the wavelength range of 320 to 400 nm) was about 200 mJ / cm by irradiating from the retardation film side of the laminate. 2 The polarizing plate was prepared by curing the layer of curable adhesive composition B and the layer of curable adhesive composition A with ultraviolet light (UVB) (measurement device: measured value based on UV Power Puck II manufactured by FusionUV). It should be noted that the thickness of the cured layer of curable adhesive composition A was about 3 μm, and the thickness of the cured layer of curable adhesive composition B was about 3 μm. The storage modulus of the cyclic polyolefin film side of the produced polarizing plate at 25 μm and 25° C. was 2.5×10 4 Pa (measurement frequency 1 Hz) of the (meth)acrylic adhesive layer A. The adhesive layer side of the produced polarizing plate with an adhesive layer was cut into a size of 150 mm×90 mm and bonded to an alkali-free glass substrate (thickness: 0.7 mm) on the adhesive layer side to obtain a laminate. Example 2 A polarizing plate was produced in the same manner as in Example 1, except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Example 3 A polarizing plate was produced in the same manner as in Example 1 except that a polyvinyl alcohol-iodine polarizer II having a thickness of 18 μm and a boron content of 3.9 mass % was used instead of the polyvinyl alcohol-iodine polarizer I. Example 4 A polarizing plate was produced in the same manner as in Example 3 except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Example 5 A polarizing plate was produced in the same manner as in Example 1, except that the (meth)acrylic resin film II was used instead of the (meth)acrylic resin film I. Example 6 A polarizing plate was produced in the same manner as in Example 5, except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Example 7 A polarizing plate was produced in the same manner as in Example 5 except that a polyvinyl alcohol-iodine polarizer II having a thickness of 18 μm and a boron content of 3.9 mass % was used instead of the polyvinyl alcohol-iodine polarizer I. Example 8 A polarizing plate was produced in the same manner as in Example 7 except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Example 9 A polarizing plate was produced in the same manner as in Example 3 except that the (meth)acrylic resin film III was used instead of the (meth)acrylic resin film I. Example 10 A polarizing plate was produced in the same manner as in Example 9, except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Embodiment 11 A polarizing plate was produced in the same manner as in Example 3 except that the (meth)acrylic resin film IV was used instead of the (meth)acrylic resin film I. Example 12 A polarizing plate was produced in the same manner as in Example 11 except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Example 13 to Example 20 Storage modulus at 20 μm thickness and 25°C: 1.5×10 4 A polarizing plate was produced in the same manner as in Examples 1 to 8 except that the (meth)acrylic pressure-sensitive adhesive layer B having a value of Pa (measurement frequency: 1 Hz) was used instead of the (meth)acrylic pressure-sensitive adhesive layer A. Example 21 to Example 28 Use thickness 5μm, storage modulus 1.1×10 5 A polarizing plate was produced in the same manner as in Examples 1 to 8 except that the (meth)acrylic pressure-sensitive adhesive layer C with a relative humidity of 1 Hz was used instead of the (meth)acrylic pressure-sensitive adhesive layer A. Comparative Example 1 A polarizing plate was produced in the same manner as in Example 1, except that the (meth)acrylic resin film V was used instead of the (meth)acrylic resin film I. Comparative Example 2 A polarizing plate was produced in the same manner as in Comparative Example 1, except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. Comparative Example 3 A polarizing plate was produced in the same manner as in Comparative Example 1 except that a polyvinyl alcohol-iodine polarizer II having a thickness of 18 μm and a boron content of 3.9 mass % was used instead of the polyvinyl alcohol-iodine polarizer I. Comparative Example 4 A polarizing plate was produced in the same manner as in Comparative Example 3 except that curable adhesive composition C was used instead of curable adhesive composition A and the thickness of the cured layer of curable adhesive composition C was set to 10 μm. [Table 1] [Table 2] [Table 3] [Table 4] <Measurement and evaluation> Martens hardness The (meth)acrylic resin film was cut into 30 mm × 30 mm pieces and used as the film. The film had a thickness of 25 μm and a storage modulus of 2.5 × 10 4 An acrylic adhesive of 1000 Pa (measurement frequency 1 Hz) was attached to an alkali-free glass substrate (thickness: 0.7 mm) to obtain a sample for measurement. In an atmosphere of temperature 23°C and relative humidity 55%, an ultra-microhardness tester (FISCHERSCOPE HM2000: manufactured by Fischer Instruments Co., Ltd.) was used to apply a load to the surface of the sample for measurement at a pressure rate of 10 mN / 5 s, and the creep time (the time for maintaining a load of 10 mN) was set to 5 s to measure the Martens hardness HM (N / mm 2 ). Glass transition temperature (Tg) Using a DSC device (EXSTAR6000, manufactured by Seiko Instruments Co., Ltd.), according to the differential scanning calorimetry analysis method based on JIS K7121: 1987, the (meth) acrylic film was cooled to -80°C at a cooling rate of 10°C / min at a nitrogen flow rate of 40 mL / min, and after holding for 10 minutes, the temperature was increased to 160°C at a heating rate of 10°C / min and held for 10 minutes. Next, the temperature was decreased from 160°C to -80°C at a cooling rate of 10°C / min, and after holding for 10 minutes, the temperature was increased to 160°C at a heating rate of 10°C / min, and the starting point glass transition temperature (Tg) was obtained and used as the glass transition temperature. The larger the value, the higher the heat resistance. Tensile elastic modulus in MD direction T MD (25℃ and 80℃) Cut the (meth) acrylic resin film into a rectangle of 70 mm in length and 10 mm in width. The length direction of the test piece is the MD direction of the resin film, and the width direction is the TD direction of the resin film (the direction perpendicular to the MD direction). Next, use the upper and lower clamps of a tensile testing machine (Autograph AG-1S testing machine, manufactured by Shimadzu Corporation) to clamp the two ends of the length direction (MD direction of the resin film) of the above-mentioned test piece in a manner that the interval between the clamps becomes 5 cm. Under the environment of 80°C and 25°C, the test piece is stretched along the length direction (MD direction of the resin film) at a stretching speed of 50 mm / min. According to the slope of the initial straight line in the obtained stress-strain curve, the tensile elastic modulus (MPa) of the resin film in the MD direction at 80°C and 25°C is calculated. Tensile elastic modulus in TD direction T TD (25℃ and 80℃) The (meth) acrylic resin film was cut into a rectangle of 70 mm in length and 10 mm in width. The length direction of the test piece was the TD direction of the resin film, and the width direction was the MD direction of the resin film (the direction orthogonal to the TD direction). Next, the upper and lower clamps of a tensile testing machine (Autograph AG-1S testing machine, manufactured by Shimadzu Corporation) were used to clamp the two ends of the length direction (TD direction of the resin film) of the test piece in a manner such that the interval between the clamps was 5 cm. The test piece was stretched along the length direction (TD direction of the resin film) at a stretching speed of 50 mm / min under an environment of 80°C and 25°C. Based on the slope of the initial straight line in the obtained stress-strain curve, the tensile elastic modulus (MPa) of the resin film in the TD direction at 80°C and 25°C was calculated. Storage modulus G' in MD direction MD (80℃) Cut the (meth) acrylic resin film into a rectangle of 30 mm in length and 5 mm in width. The length direction of the test piece is the MD direction of the resin film, and the width direction is the TD direction (the direction perpendicular to the MD direction) of the resin film. Next, use the clamp of the dynamic viscoelasticity measuring device "DVA-220" manufactured by IT Measurement and Control Co., Ltd. to clamp the two ends of the length direction (MD direction of the resin film) of the above test piece in a manner that the interval between the clamps becomes 2 cm, set the frequency of stretching and shrinking to 10 Hz, set the heating rate to 10°C / min, and find the storage modulus of the resin film in the MD direction at a temperature of 80°C. Storage modulus G' in TD direction TD (80℃) Cut the (meth) acrylic resin film into a rectangle of 30 mm in length and 5 mm in width. The length direction of the test piece is the TD direction of the resin film, and the width direction is the MD direction of the resin film (the direction orthogonal to the TD direction). Next, use the clamp of the dynamic viscoelasticity measuring device "DVA-220" manufactured by IT Measurement and Control Co., Ltd. to clamp the two ends of the length direction (TD direction of the resin film) of the above test piece in a manner that the interval between the clamps becomes 2 cm, set the frequency of stretching and shrinking to 10 Hz, set the heating rate to 10°C / min, and find the storage modulus of the resin film in the TD direction at a temperature of 80°C. Moisture Permeability The water vapor permeability (g / (m 2 ·24hr)). Internal haze Dimethyl phthalate was dropped onto the front and back surfaces of a (meth)acrylic resin film cut into 30 mm×30 mm, and the film was sandwiched between PMMA plates (SUMIPEX E00 1.0 mm) and measured using a haze meter (HM-150N, manufactured by Murakami Color Research Laboratory Co., Ltd.) in accordance with JIS K7136. Sample preparation for chemical resistance test The (meth) acrylic resin film was cut into a square of 80 mm in length and 80 mm in width, and the resin film was attached to an alkali-free glass substrate (thickness: 0.7 mm) using an acrylic adhesive having a thickness of 25 μm, and a sample for chemical resistance test (sample before chemical resistance test) was prepared. The sample was allowed to stand at 80°C for 5 minutes, and immediately after being taken out to 23°C / 55% RH, 1.5 mL of a mixed solvent of ethanol and water (99.5% ethanol manufactured by Fujifilm Wako Pure Chemical Industries, Ltd. / pure water = 9 / 1, weight ratio) was dripped onto the surface of the resin film. Then, a cylindrical weight of 0.6 kg and 5.5 cm in diameter covered with a cleaning wiper (CFW8009L, manufactured by Chang-Fong Textile Technology Co., Ltd.) was placed on the resin film in such a way that the bottom of the cylinder was in contact with the droplets of the mixed solvent, and allowed to stand for 30 seconds. Next, the weight behind the cylinder was removed from the film to obtain a sample after the chemical resistance test. The following evaluations were performed on the sample before the chemical resistance test and the sample after the chemical resistance test. Chemical resistance test (1) Appearance evaluation The appearance of the samples before and after the chemical resistance test was visually observed and evaluated based on the following criteria. ○: No change in appearance before and after the chemical resistance test ×: After the chemical resistance test, the film surface was cloudy and cracks appeared (2) ΔHaze (chemical resistance) evaluation The haze value of the sample before and after the chemical resistance test was measured using a haze meter (HM-150N, manufactured by Murakami Color Research Laboratory Co., Ltd.) in accordance with JIS K7136. The value obtained by subtracting the haze value of the sample before the chemical resistance test from the haze value of the sample after the chemical resistance test was taken as ΔHaze (chemical resistance), which was used as an indicator of chemical resistance. The smaller the value of ΔHaze (chemical resistance), the smaller the change caused by alcohol contact, and the better the chemical resistance. (3) Sa (after test) / Sa (before test) evaluation The surface roughness of the samples before and after the chemical resistance test was evaluated using a laser microscope (LEXT OLS5000, manufactured by OLYMPUS). The value of the arithmetic mean height Sa was used as an index of surface roughness. The ratio of the Sa value of the sample before the chemical resistance test (Sa (before the test)) to the Sa value of the sample after the chemical resistance test (Sa (after the test)), i.e., Sa (after the test) / Sa (before the test), was used as an index of chemical resistance. The smaller the value of Sa (after the test) / Sa (before the test), the smaller the change caused by alcohol contact, and the better the chemical resistance. Wet Heat Warpage The polarizing plate with an adhesive layer is cut into a rectangle with a length of 150 mm (in a direction parallel to the absorption axis of the polarizer) and a width of 90 mm (in a direction perpendicular to the absorption axis of the polarizer), and is attached in a manner that it is located in the center of an alkali-free glass substrate (thickness: 0.2 mm) with a length of 160 mm and a width of 102 mm to prepare a sample for a wet heat warpage test. The sample is allowed to stand for 75 hours in an environment of 30°C and 95% humidity. The laminate is taken out of the test tank, and after standing for 2 hours in an environment of 25°C and 50% relative humidity, it is placed on the measuring table of a two-dimensional measuring instrument (manufactured by Nikon Corporation, NEXIV (registered trademark) MR-12072) with the front polarizing plate on the upper side. Next, the focus is aligned with the surface of the measuring table, and based on this, the focus is aligned with 25 points on the glass sample surface, and the height from the focus as the reference is measured. The difference between the maximum and minimum values ​​of the height at the 25 measuring points is taken as the amount of warpage. Specifically, Figure 2 Point 50 is shown as the measurement point. Figure 2 The 25 points shown are points in a region 5 mm inside the end of the polarizing plate, and are arranged at intervals of about 20 mm in the short-side direction and about 35 mm in the long-side direction. GPC analysis conditions ·Measurement device: HLC-8320GPC manufactured by Tosoh Corporation Column composition: Sample column: 2 TSKgel SuperMultipore HZ-M and 1 TSKguardColmn SuperMP(HZ)-M connected in series Reference column: 2 TSKgel Super H-RC connected in series Detector: RI (differential refractometer) detector Calculation method: Molecular weight calculation Internal standard: Chloroform was used as the internal standard. · Allowable time for internal standard peak: 0.15 minutes Internal standard peak elution time: Set the elution time of chloroform when measuring the standard sample for the standard curve. Reference sample: THF (special grade, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) Measurement sample: 25 mg of a (meth)acrylic resin was fully dissolved in 5 mL of a THF / chloroform solution in which chloroform (manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) as an internal standard was dissolved in THF (special grade, manufactured by Fujifilm Wako Pure Chemical Industries, Ltd.) to give 0.04 vol %, thereby preparing a measurement sample. Column temperature: 40℃ Injection volume: 10μL Sample side pump flow rate: 0.35ml / min Reference side pump flow rate: 0.60ml / min Under the above GPC analysis conditions, the RI detection intensity relative to the elution time of the (meth)acrylic resin was measured. As standard samples for the calibration curve, the following 7 types of monodisperse methacrylic resins with known mass average molecular weight and different molecular weights (Shodex STANDARD M-75 manufactured by Showa Denko K.K.) were used. Peak molecular weight Standard sample 1: 1,050,000 Standard sample 2: 569,000 Standard sample 3: 211,000 Standard sample 4: 68,800 Standard sample 5: 18,500 Standard sample 6: 7,360 Standard sample 7: 3,070 The standard samples for the calibration curve were measured under the same conditions as for the (meth)acrylic resin, and the elution time of the peak top of each standard sample was obtained. Based on the obtained elution time and peak molecular weight, the following third-order approximate formula was obtained as the calibration formula for analyzing the measurement results of the (meth)acrylic resin. Log M (molecular weight) = At3 + Bt2 + Ct + D A, B, C, D: variables t: dissolution time The (meth)acrylic resin was analyzed by the above-mentioned GPC measurement to obtain Mw and Mn.

Claims

1. A polarizing plate comprising, in order, a (meth)acrylic resin film, a first adhesive layer, a polarizer, a second adhesive layer, a protective film, and an adhesive layer, The Martens hardness of the (meth)acrylic resin film is 140 N / mm 2 above, The storage modulus of the adhesive layer at 25°C and a measurement frequency of 1 Hz is 1.5×10 5 Below Pa.

2. The polarizing plate according to claim 1, wherein For the (meth)acrylic resin film, The tensile modulus in the MD direction at 25°C is defined as T MD (25°C), the tensile modulus in the MD direction at 80°C is defined as T MD (80℃), The tensile modulus in the TD direction at 25°C is defined as T TD (25°C), the tensile modulus in the TD direction at 80°C is defined as T TD (80℃), T MD (25℃) / T MD (80℃) and T TD (25℃) / T TD (80℃) are all less than 2.

0.

3. The polarizing plate according to claim 1 or 2, wherein For the (meth)acrylic resin film, Storage modulus G' in MD direction at 80°C and measurement frequency 10 Hz MD (80℃) and tensile modulus T in MD direction at 80℃ MD (80℃) ratio G' MD (80℃) / T MD (80℃) less than 1.

2.

4. The polarizing plate according to claim 1 or 2, wherein For the (meth)acrylic resin film, The storage modulus in the MD direction at 80°C and a measurement frequency of 10 Hz is defined as G'. MD The storage modulus in the TD direction at 80°C and a measurement frequency of 10 Hz is G' TD (80℃), G' MD (80℃) / G' TD (80°C) is 1.05 or less.

5. The polarizing plate according to claim 1 or 2, wherein The product of the moisture permeability and thickness of the (meth) acrylic resin film is 2500 (g / m 2 ·24hr·μm) or less.

6. The polarizing plate according to claim 1 or 2, wherein: The polarizer is a polyvinyl alcohol-based resin film and contains a boron compound, wherein the boron content is 4.0 wt % or less.

7. The polarizing plate according to claim 1 or 2, wherein: The first adhesive layer is a cured product of a (meth)acrylic adhesive.

8. The polarizing plate according to claim 1 or 2, wherein The protective film is a cyclic polyolefin resin film.