Method and device for improving solid core optical fiber-hollow core optical fiber coupling efficiency

By pulling the solid core optical fiber and thermally expanding the solid core optical fiber, the mode field matches the hollow core optical fiber, and corrosion of the cladding to reduce backlight, the problem of low coupling efficiency between the hollow core optical fiber and the solid core optical fiber is solved, and the problem of low coupling efficiency between the hollow core optical fiber and the solid core optical fiber is achieved Efficient and stable fiber coupling, suitable for high-power laser transmission and miniaturization integration.

CN118732170BActive Publication Date: 2024-11-01NAT UNIV OF DEFENSE TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411229567.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-01
Estimated Expiration
2044-09-03

AI Technical Summary

Technical Problem

The coupling efficiency of the prior art hollow core optical fiber and solid core optical fiber is low, and the system is large and unstable, and there are problems such as mode field matching, return light and poor mechanical intensity during the welding process.

Method used

By drawing or thermal expansion of the solid core optical fiber, the mode field matches the hollow core optical fiber, and corrosion of the cladding makes its diameter smaller than the hollow core optical fiber core, preventing light back, and finally the corrosion of the solid core The core fiber is inserted into the hollow core fiber for coupling, and a multi-dimensional adjustment table is used to achieve accurate alignment.

Benefits of technology

It improves coupling efficiency, reduces Fresnel reflection, enhances mechanical strength and system stability, is suitable for high-power laser transmission, and realizes miniaturization and full fiber integration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118732170B_ABST
    Figure CN118732170B_ABST
Patent Text Reader

Abstract

A method and device for improving the coupling efficiency of solid-core fiber and hollow-core fiber, comprising: preparing a solid-core fiber and confirming the application wavelength; using FDTD to confirm the mode field diameters of the solid-core fiber and the hollow-core fiber, comparing the mode field diameters of the solid-core fiber and the hollow-core fiber, and if there is a mismatch, taper or expand the solid-core fiber until the mode fields of the solid-core fiber and the hollow-core fiber are similar, corroding the cladding of the solid-core fiber, and using FDTD software to simulate the insertion of the corroded solid-core fiber into the hollow-core fiber, and selecting the solid-core fiber with the highest coupling efficiency according to the simulation results; cutting the selected corroded solid-core fiber and the hollow-core fiber, and coating the end face of the solid-core fiber with a high-transmittance film after grinding; inserting the corroded section of the solid-core fiber after coating into the core of the hollow-core fiber, and performing integrated packaging processing on the connection between the solid-core fiber and the hollow-core fiber. The present invention can be applied to hollow-core fibers of various core sizes and can withstand high-power laser transmission.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention mainly relates to the technical field of optical fiber coupling, in particular to a method and a device for improving the coupling efficiency of a solid core optical fiber and a hollow core optical fiber. Background Art

[0002] Hollow-core optical fiber has broad prospects in the fields of high-power laser beam transmission, optical fiber sensing, hollow-core optical fiber gas laser, etc. due to its advantages such as low nonlinear effect, ultra-low group velocity dispersion, low material absorption loss and high material damage threshold. In the application of hollow-core optical fiber, it is inevitable to prepare all-fiber devices, among which the low-loss coupling between hollow-core optical fiber and solid-core optical fiber is the key issue.

[0003] The commonly used methods to achieve coupling between hollow-core fiber and solid-core fiber are spatial optical path coupling and fiber fusion splicing. The spatial optical path coupling scheme is to convert the output light of the solid-core fiber into parallel light through a lens, and then use another lens to focus and couple it into the hollow-core fiber. The lens needs to select a suitable numerical aperture and focal length so that the mode field diameter of the output light of the solid-core fiber matches the mode field diameter of the hollow-core fiber. In order to achieve precise adjustment of the coupling, the lens system needs to be fixed on a three-dimensional motion platform. The problems with this method are: the spatial optical path contains lenses, and a three-dimensional motion platform is required for adjustment. The system is bulky and difficult to achieve miniaturization and all-fiber integration; due to the adjustment of the spatial optical path, it is subject to greater external interference and the system is unstable; in addition, the optical lens and the optical fiber surface will cause Fresnel reflection, resulting in reduced coupling efficiency.

[0004] Fiber fusion splicing is another commonly used method. A major difficulty faced by fusion splicing is mode field matching. Tapering and core expansion can solve this problem, but the fusion splicing process also faces the following problems: (1) collapse of the internal structure of the fiber; (2) inability to prevent light return; (3) poor mechanical strength of the melting point and easy damage; (4) inability to withstand high-power lasers. Summary of the invention

[0005] In view of the technical problems existing in the prior art, the present invention proposes a method and device for improving the coupling efficiency of solid-core optical fiber and hollow-core optical fiber, which tapers or thermally expands the solid-core optical fiber to match the mode field of the solid-core optical fiber and the hollow-core optical fiber, and then etches the cladding of the solid-core optical fiber to make its cladding diameter smaller than the core diameter of the hollow-core optical fiber; the end face of the corroded solid-core optical fiber is cut at a flat angle and then coated to prevent light return; finally, the corroded section of the solid-core optical fiber is inserted into the hollow-core optical fiber for coupling connection; the coupled optical fiber can have a higher coupling efficiency due to mode field matching. Coating the end face of the solid-core optical fiber effectively restrains Fresnel reflection, suppresses light return, and protects the safety of front-end components. At the same time, because there is no thermal welding process, there is no collapse inside the hollow-core optical fiber and no welding loss. Therefore, this coupling method is suitable for low-loss, high-mechanical-strength welding applications and can withstand high-power laser transmission.

[0006] To achieve the above purpose, the technical solution adopted by the present invention is as follows:

[0007] In one aspect, the present invention provides a method for improving solid core fiber-hollow core fiber coupling efficiency, comprising:

[0008] S1. Prepare solid core optical fiber and confirm the wavelength to be used;

[0009] S2. Use FDTD software to simulate solid-core optical fiber and hollow-core optical fiber, input the core size of solid-core optical fiber and hollow-core optical fiber, the cladding size of optical fiber, the refractive index of optical fiber material, the wavelength to be applied, set the light source and monitor, and confirm the mode field diameter of solid-core optical fiber and hollow-core optical fiber;

[0010] S3. Construct a mode field mismatch loss function, and judge whether the mode fields of the solid core fiber and the hollow core fiber are similar or mismatched according to the mode field mismatch loss function:

[0011] ;

[0012] in is the mode field mismatch loss, is the hollow core fiber mode field diameter, is the mode field diameter of the solid core optical fiber;

[0013] when When , it is determined that the mode fields of the solid core fiber and the hollow core fiber are similar, and the process goes to step S4;

[0014] when When , it is determined that the solid core fiber and the hollow core fiber mode field are mismatched, and the process goes to step S5;

[0015] S4. The solid core optical fiber cladding is corroded, and the diameter of the solid core optical fiber cladding after corrosion is smaller than the diameter of the hollow core optical fiber core, so that the solid core optical fiber can be inserted into the hollow core optical fiber core, and then go to step S6;

[0016] S5. Taper or expand the solid core optical fiber to change the mode field diameter of the solid core optical fiber, and return to S2 until the mode field of the solid core optical fiber is close to the mode field of the hollow core optical fiber;

[0017] S6. Confirm the core size of the solid-core optical fiber after corrosion, the cladding size of the optical fiber, the refractive index of the optical fiber material, the core size of the hollow-core optical fiber, the cladding size of the optical fiber, the refractive index of the optical fiber material, and the wavelength to be applied, and use FDTD software to simulate the insertion of the corroded solid-core optical fiber into the hollow-core optical fiber. According to the simulation results, select the solid-core optical fiber with the highest coupling efficiency, that is, the solid-core optical fiber with the highest light transmission rate;

[0018] S7. Cutting the selected corroded solid core optical fiber and hollow core optical fiber;

[0019] S8. Grind the end face of the cut solid core optical fiber and then coat it with a high-transmittance film to prevent light return;

[0020] S9. Inserting the coated corroded section of the solid core optical fiber into the core of the hollow core optical fiber;

[0021] S10. Perform integrated packaging processing on the connection between the solid core optical fiber and the hollow core optical fiber.

[0022] Furthermore, the taper method described in S5 is to fix the solid core optical fiber in a taper machine, and reduce the size of the cladding and the core and the mode field by controlling the parameters of the taper, wherein the taper parameters include: the size and length of the taper waist and the taper region of the taper, and the length of the taper region is controlled between 3-5 cm;

[0023] The core expansion method is to discharge the end face of the optical fiber through the electrode of the fusion splicer or heat it with hydrogen-oxygen flame, so that the doping in the optical fiber core diffuses into the cladding, thereby expanding the mode field.

[0024] Furthermore, in S4, the etching of the cladding of the solid core optical fiber with a chemical etching solution requires precise control of the etching time to control the size of the cladding after etching, so that the cladding diameter of the solid core optical fiber is 1-2µm larger than the core, close to exposing the core.

[0025] Furthermore, the end faces of the solid core optical fiber and the hollow core optical fiber after cutting in S7 are flat angles.

[0026] Furthermore, in S8, the end face of the cut solid core optical fiber is polished to ensure that the end face is flat and has no obvious scratches.

[0027] Furthermore, in S9, the corroded section of the solid core optical fiber is inserted into the core of the hollow core optical fiber, and the solid core optical fiber and the hollow core optical fiber are made coaxial by moving and rotating.

[0028] Furthermore, in S9, the solid core optical fiber and the hollow core optical fiber are respectively arranged on a multi-dimensional adjustment table, and the accuracy of the multi-dimensional adjustment table is controlled at the μm level. The movement and rotation of the solid core optical fiber and the hollow core optical fiber are controlled by the two multi-dimensional adjustment tables. The corroded section of the solid core optical fiber is inserted into the core of the hollow core optical fiber, and the solid core optical fiber is made coaxial with the hollow core optical fiber.

[0029] Furthermore, S9 also includes performing coaxial detection on the corroded section of the solid core optical fiber after being inserted into the core of the hollow core optical fiber. The method is: connecting a laser to one end of the solid core optical fiber, and placing a power meter at the output end of the hollow core optical fiber to detect the power. According to the power information detected by the power meter, it is determined whether the solid core optical fiber and the hollow core optical fiber meet the coaxial requirements. When the power information detected by the power meter is maximized by finely adjusting the movement and rotation of the solid core optical fiber and the hollow core optical fiber, it means that the current coupling efficiency is the highest. It is believed that the solid core optical fiber and the hollow core optical fiber are precisely aligned at this time, and the solid core optical fiber and the hollow core optical fiber are coaxial.

[0030] Furthermore, in S10, the integrated packaging process is completed by coating glue at the contact point between the solid core optical fiber and the hollow core optical fiber end face.

[0031] On the other hand, the present invention provides a device for improving the coupling efficiency of a solid core fiber and a hollow core fiber based on the above-mentioned method for improving the coupling efficiency of a solid core fiber and a hollow core fiber.

[0032] Compared with the prior art, the technical effects that the present invention can produce are:

[0033] 1. Compared with the method of directly inserting the hollow-core fiber after taper, the scheme of the present invention has the following advantages: (1) It can make the mode fields of the solid-core fiber and the hollow-core fiber more matched, so as to make the coupling efficiency higher. The scheme of inserting the hollow-core fiber after taper requires that the cladding of the solid-core fiber be tapered to a size smaller than the core size of the hollow-core fiber. At this time, the mode field of the solid-core fiber will be smaller than that of the hollow-core fiber, and the mode field mismatch loss of the two increases. In this scheme, for the solid-core fiber and the hollow-core fiber with similar mode fields, the solid-core fiber is directly corroded and then inserted; for the two cases of mode field mismatch, the solid-core fiber is respectively tapered and expanded to make its mode field diameter basically match that of the hollow-core fiber, and then the cladding is reduced by corrosion to make it smaller than the core of the hollow-core fiber. (2) It can withstand high power. The method of directly inserting the hollow-core fiber after taper makes the cone head of the optical fiber too small, which is more likely to heat up and be damaged under high power. The core of the method of the present invention is relatively larger and can withstand higher power.

[0034] 2. Compared with the traditional spatial optical path coupling, the scheme of the present invention adopts the method of inserting the hollow core optical fiber core after optical fiber corrosion to form a fully integrated solid core optical fiber and hollow core optical fiber coupling device, which does not require any spatial optical path components and adjustment devices, making the coupling device small and compact, greatly improving the system integration and mechanical stability.

[0035] 3. The scheme of the present invention can achieve precise alignment through power feedback, and proposes a method of inserting the optical fiber into the core of the hollow-core optical fiber after etching, so that the light of the solid-core optical fiber can completely enter the cladding. It can be applied to hollow-core optical fibers of various core sizes, thereby promoting the application of hollow-core optical fibers.

[0036] 4. The invention scheme completely seals the entire device through glue sealing, so that it has high practical value and broad application prospects in the fields of optical fiber gas laser, ultra-high sensitivity gas sensing, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0038] Figure 1 is a flow chart of a method for improving solid core fiber-hollow core fiber coupling efficiency provided by an embodiment;

[0039] Figure 2 Schematic diagram of a device for improving the coupling efficiency of solid core optical fiber and hollow core optical fiber provided by an embodiment, wherein: Figure 2 (a) is a schematic diagram of the coupling device for corroding a solid core optical fiber and inserting it into a hollow core optical fiber. Figure 2 (b) is a schematic diagram of the coupling device in which the solid-core optical fiber is tapered and then corroded to insert into the hollow-core optical fiber. Figure 2 (c) is a schematic diagram of the coupling device for the hollow-core optical fiber after core expansion by corrosion. Figure 2 (d) is a schematic diagram of the structure of a hollow core optical fiber. Figure 2 (e) is a schematic diagram of the structure of a solid core optical fiber;

[0040] Figure 3 is a schematic diagram of a device for corroding a solid core optical fiber provided by an embodiment;

[0041] Figure 4 This is an FDTD simulation diagram and simulation result diagram of inserting a solid core optical fiber into a hollow core optical fiber after corrosion provided by an embodiment, wherein: Figure 4 (a) is the FDTD simulation diagram, Figure 4 (b) is the simulation result diagram;

[0042] Figure 5 The FDTD simulation diagram and simulation result diagram of inserting a solid core optical fiber into a hollow core optical fiber after taper and corrosion provided by an embodiment, wherein: Figure 5 (a) is the FDTD simulation diagram, Figure 5 (b) is the simulation result diagram.

[0043] Figure annotation:

[0044] 1. Solid core optical fiber; 2. Hollow core optical fiber; 3. High transmittance film; 4. Contact surface between solid core optical fiber and hollow core optical fiber; 101. Corrosion section of solid core optical fiber; 102. Waist region; 103. Taper region; 104. Core expansion gradient region of solid core optical fiber; 105. Core expansion region of solid core optical fiber; 106. Cladding of solid core optical fiber; 107. Core of solid core optical fiber; 201. Cladding of hollow core optical fiber; 202. Core of hollow core optical fiber. DETAILED DESCRIPTION

[0045] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0046] Reference Figure 1 In one embodiment, a method for improving the coupling efficiency of a solid core fiber to a hollow core fiber is provided, comprising:

[0047] S1. Prepare solid core optical fiber and confirm the wavelength to be used;

[0048] S2. Use FDTD software to simulate solid-core optical fiber and hollow-core optical fiber, input the core size of solid-core optical fiber and hollow-core optical fiber, the cladding size of optical fiber, the refractive index of optical fiber material, and the wavelength to be applied, and confirm the mode field diameter of solid-core optical fiber and hollow-core optical fiber;

[0049] S3. Construct a mode field mismatch loss function, and judge whether the mode fields of the solid core fiber and the hollow core fiber are similar or mismatched according to the mode field mismatch loss function:

[0050] ;

[0051] in is the mode field mismatch loss, is the hollow core fiber mode field diameter, is the mode field diameter of the solid core optical fiber;

[0052] when When , it is determined that the mode fields of the solid core fiber and the hollow core fiber are similar, and the process goes to step S4;

[0053] when When , it is determined that the solid core fiber and the hollow core fiber mode field are mismatched, and the process goes to step S5;

[0054] S4. The solid core optical fiber cladding is corroded, and the diameter of the solid core optical fiber cladding after corrosion is smaller than the diameter of the hollow core optical fiber core, so that the solid core optical fiber can be inserted into the hollow core optical fiber core, and then go to step S6;

[0055] S5. Taper or expand the solid core optical fiber to change the mode field diameter of the solid core optical fiber, and return to S2 until the mode field of the solid core optical fiber is close to the mode field of the hollow core optical fiber;

[0056] S6. Confirm the core size of the solid-core optical fiber after corrosion, the cladding size of the optical fiber, the refractive index of the optical fiber material, the core size of the hollow-core optical fiber, the cladding size of the optical fiber, the refractive index of the optical fiber material, and the wavelength to be applied, and use FDTD software to simulate the insertion of the corroded solid-core optical fiber into the hollow-core optical fiber. According to the simulation results, select the solid-core optical fiber with the highest coupling efficiency, that is, the solid-core optical fiber with the highest light transmission rate;

[0057] S7. Cutting the selected corroded solid core optical fiber and hollow core optical fiber;

[0058] S8. Grind the end face of the cut solid core optical fiber and then coat it with a high-transmittance film to prevent light return;

[0059] S9. Inserting the coated corroded section of the solid core optical fiber into the core of the hollow core optical fiber;

[0060] S10. Perform integrated packaging processing on the connection between the solid core optical fiber and the hollow core optical fiber.

[0061] The hollow core optical fiber includes one of an antiresonant optical fiber, a kagome optical fiber, a nested antiresonant optical fiber, a hollow core photonic bandgap optical fiber, a capillary optical fiber, and a multi-hollow optical fiber.

[0062] In S2, FDTD software is used to confirm the mode field diameters of solid core fiber 1 and hollow core fiber 2. Specifically, a Gaussian light source with a wavelength to be applied is incident from the end face of the optical fiber. By controlling the waist size of the Gaussian light source, the mode field diameter of the Gaussian light transmitted in the optical fiber can be controlled. By comparing Gaussian light fields with different mode field diameters, the Gaussian light field that can be stably transmitted in the optical fiber is found, and the light intensity of the light field is calculated to decay to 1 / e 2 The diameter at this time is the mode field diameter of the optical fiber.

[0063] Reference Figure 2 , Figure 2 (d) Figure 2 (e) are schematic diagrams of the structure of hollow-core optical fiber and solid-core optical fiber, respectively. In S2, it is necessary to determine the mode field diameters of solid-core optical fiber 1 and hollow-core optical fiber 2. Figure 2 As shown in (a), if the mode field diameter of the hollow core fiber 2 is similar to that of the solid core fiber 1, the cladding 106 of the solid core fiber is directly corroded; Figure 2 As shown in (b), if the mode field diameter of the hollow core fiber 2 is smaller than that of the solid core fiber 1, the solid core fiber 1 is tapered; Figure 2 As shown in (c), if the mode field diameter of the hollow core fiber 2 is larger than that of the solid core fiber 1, the solid core fiber 1 is expanded to match the mode field of the solid core fiber 1 with that of the hollow core fiber 2. Through the above treatment, the present invention is applicable to hollow core fibers and solid core fibers of almost any mode field.

[0064] Furthermore, the taper means fixing the optical fiber on the taper machine, heating it with a flame, pushing the optical fiber at a speed lower than the speed of pulling out the optical fiber, and setting the taper parameters, the size and length of the taper region 103 and the waist region 102 to accurately control the size of the optical fiber cladding after taper. The core expansion means discharging the end face of the optical fiber with the electrode of the fusion splicer or heating it with a hydrogen-oxygen flame, so that the doping in the optical fiber core diffuses into the cladding, thereby expanding the mode field; the doping in the core 107 of the solid core optical fiber diffuses into the cladding to form the core expansion region 105 of the solid core optical fiber and the core expansion gradient region 104 of the solid core optical fiber. In the process of core expansion, the size of the core increases, and the size of the cladding remains almost unchanged.

[0065] Reference Figure 3 In S4, the cladding 106 of the solid core optical fiber is corroded with a chemical corrosion solution. The corrosion time needs to be precisely controlled to control the size of the cladding after corrosion. After corrosion, it is rinsed with a solution neutralized with acidity and alkalinity. The time is precisely controlled so that the diameter of the cladding of the solid core optical fiber after corrosion is smaller than the diameter of the core 202 of the hollow core optical fiber. The diameter of the cladding 106 of the solid core optical fiber is 1-2 μm larger than the core, close to the exposed core. The chemical corrosion solution includes corrosive solutions such as hydrofluoric acid, concentrated strong alkali, concentrated phosphoric acid, borate and boric anhydride.

[0066] Specifically, Figure 4 and Figure 5 As shown, FDTD software is used in S6 to simulate the insertion of the corroded solid core fiber into the hollow core fiber 2; solid core fiber 1 and hollow core fiber 2 are modeled in solidworks and imported into FDTD, the light source is set to a Gaussian light source with a wavelength of 1080nm, the core diameter of the solid core fiber is 25μm, and the core diameter of the hollow core fiber is 35μm. At this wavelength, the mode field diameter of the solid core fiber 1 is larger than the mode field diameter of the hollow core fiber 2.

[0067] Further, Figure 4 FDTD simulation diagram and simulation result diagram of directly corroding the solid core fiber and inserting it into the hollow core fiber. Figure 4 (a) is the FDTD simulation diagram, Figure 4 (b) is a simulation result diagram, showing the light transmission rate when the cladding is corroded to different radii. The results show that when the cladding radius is corroded to 15um, the light transmission rate is the largest, 91.6%, which is 2.5μm larger than the core.

[0068] Further, Figure 5 FDTD simulation diagram and simulation result diagram of inserting solid core optical fiber into hollow core optical fiber after taper and corrosion. Figure 5 (a) is the FDTD simulation diagram, Figure 5(b) is a simulation result diagram, which shows the light transmission rate when the cladding of the tapered area is corroded to different sizes after taper. The core radius of the solid core fiber after taper is 10μm, and the core radius of the hollow core fiber is 35μm. A monitor is set at 2 of the hollow core fiber to record the light transmission rate. The results show that when the cladding is smaller and closer to the exposed core, the light transmission rate is the largest and the coupling efficiency is the highest. The simulation shows that when the cladding is corroded to a radius of 10.5μm, the coupling efficiency is about 93.3% at its maximum. This simulation also proves the feasibility of this method.

[0069] Furthermore, when a Gaussian light source with a wavelength of 1084nm is used as the incident light, the mode field diameter of the solid-core optical fiber 1 is larger than that of the hollow-core optical fiber 2. By comparison, the coupling efficiency of the hollow-core optical fiber 2 inserted after taper corrosion is greater than the coupling efficiency of the solid-core optical fiber 1 directly corroded, which proves the effectiveness of this method.

[0070] Furthermore, in S7, a large core diameter cutting knife is used to cut the hollow core optical fiber, and a cutting knife is selected for the solid core optical fiber 1 according to the cladding size.

[0071] Furthermore, the end faces of the solid core optical fiber 1 and the hollow core optical fiber 2 after cutting in S7 are flat angles, and the end faces of the solid core optical fiber 1 and the hollow core optical fiber 2 are flat angles and are both planes perpendicular to the central axis of the optical fiber.

[0072] Specifically, in S8, grinding is performed before coating the end face of the solid core optical fiber in order to make the end face of the optical fiber smoother and free of obvious scratches, so as to effectively realize the anti-reflection film effect. The end face of the solid core optical fiber is coated with a high-transmittance film mainly to prevent Fresnel reflection, suppress return light, protect the front-end components, and reduce coupling loss. Currently, bevel cutting is commonly used to prevent return light. The disadvantage is that it is difficult to achieve reliable and precise angle cutting on the delicate hollow core optical fiber structure, and the direction of the output light beam of the solid core optical fiber after angle cutting deviates from the optical fiber axis, which may lead to higher coupling loss. Flat-angle coating can solve this problem.

[0073] Furthermore, in S9, the corroded section 101 of the solid core optical fiber is inserted into the core 202 of the hollow core optical fiber, and the solid core optical fiber 1 is made coaxial with the hollow core optical fiber 2 by moving, rotating, etc. The corroded section 101 of the solid core optical fiber is surrounded by the capillary wall of the hollow core optical fiber 2, so that the output light beam of the optical fiber is confined in the core.

[0074] Furthermore, the solid core optical fiber 1 and the hollow core optical fiber 2 are respectively arranged on a multi-dimensional adjustment table, and the accuracy of the multi-dimensional adjustment table is controlled at the μm level. The movement and rotation of the solid core optical fiber 1 and the hollow core optical fiber 2 are controlled by the two multi-dimensional adjustment tables. The etched section 101 of the solid core optical fiber is inserted into the core 202 of the hollow core optical fiber, and the solid core optical fiber 1 is made coaxial with the hollow core optical fiber 2.

[0075] Furthermore, S9 also includes performing a coaxial detection on the corroded section 101 of the solid core optical fiber after it is inserted into the core 202 of the hollow core optical fiber. The method is as follows: a laser is connected to one end of the solid core optical fiber 1, and a power meter is placed at the output end of the hollow core optical fiber 2 to detect the power. The power information detected by the power meter is used to determine whether the solid core optical fiber 1 and the hollow core optical fiber 2 meet the coaxial requirements. When the power information detected by the power meter is maximized by finely adjusting the movement and rotation of the solid core optical fiber 1 and the hollow core optical fiber 2, it indicates that the current coupling efficiency is the highest. It is believed that the solid core optical fiber 1 and the hollow core optical fiber 2 are precisely aligned at this time, and the cone region 103 where the solid core optical fiber 1 is inserted is located at the center of the hollow core optical fiber core, and the solid core optical fiber 1 is coaxial with the hollow core optical fiber 2.

[0076] Furthermore, in order to increase the mechanical stability, glue is applied to the connection between the taper region 103 of the solid core optical fiber 1 and the end face of the hollow core optical fiber 2 for integrated packaging, so that the stability of the system is improved. The sealed gas cavity can be used in the fields of optical fiber gas laser, ultra-high sensitivity gas sensing, etc.

[0077] In another embodiment, a device for improving the coupling efficiency between a solid core fiber and a hollow core fiber is provided based on the method for improving the coupling efficiency between a solid core fiber and a hollow core fiber.

[0078] Matters not covered by the present invention are known technologies.

[0079] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0080] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent of the present application shall be subject to the attached claims.

[0081] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for improving the coupling efficiency of a solid core fiber and a hollow core fiber, characterized in that: include: S1. Prepare solid core optical fiber and confirm the wavelength to be used; S2. Use FDTD software to simulate solid-core optical fiber and hollow-core optical fiber, input the core size of solid-core optical fiber and hollow-core optical fiber, the cladding size of optical fiber, the refractive index of optical fiber material, the wavelength to be applied, set the light source and monitor, and confirm the mode field diameter of solid-core optical fiber and hollow-core optical fiber; S3. Construct a mode field mismatch loss function, and judge whether the mode fields of the solid core fiber and the hollow core fiber are similar or mismatched according to the mode field mismatch loss function: ; in is the mode field mismatch loss, is the hollow core fiber mode field diameter, is the mode field diameter of the solid core optical fiber; when When , it is determined that the mode fields of the solid core fiber and the hollow core fiber are similar, and the process goes to step S4; when When , it is determined that the solid core fiber and the hollow core fiber mode field are mismatched, and the process goes to step S5; S4. The solid core optical fiber cladding is corroded, and the diameter of the solid core optical fiber cladding after corrosion is smaller than the diameter of the hollow core optical fiber core, so that the solid core optical fiber can be inserted into the hollow core optical fiber core, and then go to step S6; S5. Taper or expand the solid core optical fiber to change the mode field diameter of the solid core optical fiber, and return to S2 until the mode field of the solid core optical fiber is close to the mode field of the hollow core optical fiber; S6. Confirm the core size of the solid-core optical fiber after corrosion, the cladding size of the optical fiber, the refractive index of the optical fiber material, the core size of the hollow-core optical fiber, the cladding size of the optical fiber, the refractive index of the optical fiber material, and the wavelength to be applied, and use FDTD software to simulate the insertion of the corroded solid-core optical fiber into the hollow-core optical fiber. According to the simulation results, select the solid-core optical fiber with the highest coupling efficiency, that is, the solid-core optical fiber with the highest light transmission rate; S7. Cutting the selected corroded solid core optical fiber and hollow core optical fiber; S8. Grind the end face of the cut solid core optical fiber and then coat it with a high-transmittance film to prevent light return; S9. Inserting the coated corroded section of the solid core optical fiber into the core of the hollow core optical fiber; S10. Perform integrated packaging processing on the connection between the solid core optical fiber and the hollow core optical fiber.

2. The method for improving the coupling efficiency of solid core fiber and hollow core fiber according to claim 1, characterized in that: The taper method described in S5 is to fix the solid core optical fiber in a taper machine, and reduce the size of the cladding and the core and the mode field by controlling the taper parameters, wherein the taper parameters include: the size and length of the taper waist and the taper region, and the length of the taper region is controlled between 3-5 cm; The core expansion method is to discharge the end face of the optical fiber through the electrode of the fusion splicer or heat it with hydrogen-oxygen flame, so that the doping in the optical fiber core diffuses into the cladding, thereby expanding the mode field.

3. The method for improving the coupling efficiency of solid core fiber and hollow core fiber according to claim 1, characterized in that: In S4, the cladding of the solid core optical fiber is corroded with a chemical etching solution. It is necessary to precisely control the etching time to control the size of the cladding after etching, so that the cladding diameter of the solid core optical fiber is 1-2µm larger than the core, close to exposing the core.

4. The method for improving the coupling efficiency of solid core fiber and hollow core fiber according to claim 1, characterized in that: The end faces of the solid core fiber and the hollow core fiber after cutting in S7 are flat angles.

5. The method for improving the coupling efficiency of solid core fiber and hollow core fiber according to claim 1, characterized in that: In S8, the end face of the cut solid core optical fiber is polished to ensure that the end face is flat and has no obvious scratches.

6. The method for improving the coupling efficiency of solid core fiber and hollow core fiber according to claim 1, characterized in that: In S9, the corroded section of the solid core optical fiber is inserted into the core of the hollow core optical fiber, and the solid core optical fiber and the hollow core optical fiber are made coaxial by moving and rotating.

7. The method for improving the solid core fiber-hollow core fiber coupling efficiency according to claim 6, characterized in that: In S9, the solid core optical fiber and the hollow core optical fiber are respectively arranged on a multi-dimensional adjustment table, the accuracy of which is controlled at the μm level. The movement and rotation of the solid core optical fiber and the hollow core optical fiber are controlled by two multi-dimensional adjustment tables. The etched section of the solid core optical fiber is inserted into the core of the hollow core optical fiber, and the solid core optical fiber is made coaxial with the hollow core optical fiber.

8. The method for improving the coupling efficiency between solid core fiber and hollow core fiber according to claim 7, characterized in that: S9 also includes the step of inserting the corroded section of the solid-core optical fiber into the core of the hollow-core optical fiber and performing a coaxial detection, wherein a laser is connected to one end of the solid-core optical fiber, and a power meter is placed at the output end of the hollow-core optical fiber to detect the power, and the power information detected by the power meter is used to determine whether the solid-core optical fiber and the hollow-core optical fiber meet the coaxial requirements. When the power information detected by the power meter is maximized by finely adjusting the movement and rotation of the solid-core optical fiber and the hollow-core optical fiber, it indicates that the current coupling efficiency is the highest, and it is considered that the solid-core optical fiber and the hollow-core optical fiber are precisely aligned and are coaxial.

9. The method for improving the coupling efficiency between solid core fiber and hollow core fiber according to claim 1, characterized in that: In S10, the integrated packaging process is completed by coating glue at the contact point between the solid core optical fiber and the hollow core optical fiber end face.

10. A device for improving the coupling efficiency of solid core optical fiber and hollow core optical fiber, characterized in that: The method for improving the coupling efficiency between solid core optical fiber and hollow core optical fiber as described in any one of claims 1 to 9 is used to prepare the optical fiber.