Semiconductor device and method of forming high crystalline quality magnetic layer for shielding low frequency magnetic fields
By using laser spike annealing technology to process magnetic film materials in a magnetic field, the problem of poor shielding effect of semiconductor devices on low-frequency magnetic fields is solved, the crystal quality and magnetic permeability of the magnetic film are improved, and more effective low-frequency magnetic field shielding is achieved.
Patent Information
- Application Number
- CN202311775497.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2023-12-21
- Publication Date
- 2024-10-01
AI Technical Summary
Existing semiconductor devices are inefficient in shielding low-frequency magnetic fields in high-frequency applications, and due to low magnetic permeability and magnetic film peeling problems caused by crystal defects, it is difficult to effectively suppress low-frequency magnetic field interference.
Laser spike annealing technology is used to process magnetic film materials in a magnetic field, reducing crystal defects through alignment of magnetic spin directions, improving the crystal quality and magnetic permeability of the magnetic film, and forming a high crystal quality magnetic film layer to shield low-frequency magnetic fields.
It significantly improves the magnetic permeability and crystal quality of the magnetic film, enhances the shielding effect on low-frequency magnetic fields, reduces crystal defects and avoids peeling problems caused by lamination processing, achieving more effective electromagnetic shielding.
Smart Images

Figure CN118737844A_ABST
Abstract
Description
Technical Field
[0001] The present invention generally relates to semiconductor devices, and more particularly, to a semiconductor device and method for forming a high crystal quality magnetic film layer for shielding a low frequency magnetic field. Background Art
[0002] Semiconductor devices are commonly found in modern electronic products. Semiconductor devices perform a wide range of functions, such as signal processing, high-speed computing, transmitting and receiving electromagnetic signals, controlling electronic devices, optoelectronics, and creating visual images for television displays. Semiconductor devices are found in the fields of communications, power conversion, networking, computers, entertainment, and consumer products. Semiconductor devices are also found in military applications, aviation, automobiles, industrial controllers, and office equipment.
[0003] Semiconductor devices, especially in high-frequency applications such as radio frequency (RF) wireless communications, often contain one or more integrated passive devices (IPDs) to perform the necessary electrical functions. Multiple semiconductor dies and IPDs can be integrated into a system-in-package (SiP) module for higher density and expanded electrical functions in a small space. In a SIP module, the semiconductor die and IPD are deployed on a substrate for structural support and electrical interconnection. The encapsulant is deposited over the semiconductor die, IPD, and substrate.
[0004] The SiP module includes high-speed digital and RF electrical components that are highly integrated for small size and low height, and operate at high clock frequencies and high power ratings. Electromagnetic shielding materials are typically conformally applied over the encapsulation. The electromagnetic shielding materials reduce or suppress electromagnetic interference (EMI), radio frequency interference (RFI), and other inter-device interference (e.g., as radiated by high-speed digital devices) from affecting adjacent devices within or adjacent to the SiP module.
[0005] The electrical components within the SiP module may also be susceptible to or generate low-frequency magnetic fields from sources such as wireless power charging (Qi-WPC), near field communication (NFC), radio frequency identification (RFID), power management adapter (PMA), wireless charging transmitter (WCT), switching power supply, inductor module and magnetic RAM, as well as being susceptible to or generating electromagnetic noise interference radiated by SiP or circuits with high frequency and density. High-frequency shielding is often inefficient for low-frequency magnetic fields. Magnetic films can reduce the impact of low-frequency magnetic fields. However, due to crystallization defects, magnetic films produced by PVD typically exhibit low magnetic permeability. In addition, applying magnetic films using a lamination process may result in peeling at the interface magnetic film and EMC or shielding layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figure 1a-Figure 1c A semiconductor wafer having a plurality of semiconductor dies separated by saw streets is shown;
[0007] Figure 2a-2h Figure 1 shows a process of forming a high crystal quality magnetic film layer for shielding low frequency magnetic fields using laser spike annealing in a magnetic field;
[0008] Figure 3a-Figure 3b The diagram shows the orientation of the magnetic spin direction;
[0009] Figure 4a-4e A second embodiment of forming a high crystal quality magnetic film layer for shielding low frequency magnetic field by using laser spike annealing in a magnetic field is shown;
[0010] Figure 5a-Figure 5e A third embodiment of forming a high crystal quality magnetic film layer for shielding low frequency magnetic field by using laser spike annealing in a magnetic field is shown;
[0011] Figure 6a-6c A fourth embodiment of forming a high crystal quality magnetic film layer for shielding low frequency magnetic fields by using laser spike annealing in a magnetic field is shown;
[0012] Figure 7 The M and H magnetic fields applied to the magnetic film layer before laser annealing are shown;
[0013] Figure 8 illustrates additional M and H magnetic fields applied to the magnetic film layer prior to laser annealing; and
[0014] Fig. 9 A printed circuit board (PCB) is illustrated with different types of packages deployed on a surface of the PCB. DETAILED DESCRIPTION
[0015] The present invention is described in one or more embodiments in the following description with reference to the figures, wherein the same numerals represent the same or similar elements. Although the present invention is described with respect to the best mode for achieving the objectives of the present invention, it will be appreciated by those skilled in the art that it is intended to cover alternatives, modifications and equivalents that may be included in the spirit and scope of the present invention as defined by the appended claims and their equivalents (supported by the following disclosure and drawings). The features shown in the figures are not necessarily drawn to scale. Elements with similar functions are assigned the same reference numerals in the figures. The term "semiconductor die" as used herein refers to both singular terms and plural terms, and therefore, may refer to both a single semiconductor device and a plurality of semiconductor devices.
[0016] Semiconductor devices are generally manufactured using two complex manufacturing processes: front-end manufacturing and back-end manufacturing. Front-end manufacturing involves forming multiple dies on the surface of a semiconductor wafer. Each die on the wafer contains active and passive electrical components that are electrically connected to form a functional circuit. Active electrical components (such as transistors and diodes) have the ability to control the flow of electrical current. Passive electrical components (such as capacitors, inductors, and resistors) create the relationship between voltage and current necessary to perform the circuit function.
[0017] Back-end manufacturing refers to cutting or singulating the completed wafer into individual semiconductor die and packaging the semiconductor die for structural support, electrical interconnection and environmental isolation. In order to singulate the semiconductor die, the wafer is scribed along the non-functional area of the wafer (referred to as saw road or scratch (scribe)) and the wafer is broken. The wafer is singulated using a laser cutting tool or saw blade. After singulation, the individual semiconductor die is deployed on a package substrate including pins or contact pads for interconnection with other system components. The contact pads formed above the semiconductor die are then connected to the contact pads in the package. Electrical connections can be made using conductive layers, bumps, columnar bumps, conductive solder paste or wiring bonding. Encapsulants or other molding materials are deposited above the package to provide physical support and electrical isolation. The completed package is then inserted into the electrical system, and the functions of the semiconductor device are made available to other system components.
[0018] Figure 1a A semiconductor wafer 100 is shown having a base substrate material 102 (such as silicon, germanium, aluminum phosphide, aluminum arsenide, gallium arsenide, gallium nitride, indium phosphide, silicon carbide, or other bulk material) for structural support. A plurality of semiconductor dies or electrical components 104 are formed on the wafer 100, separated by non-active inter-die wafer regions or saw streets 106. The saw streets 106 provide dicing areas to singulate the semiconductor wafer 100 into individual semiconductor dies 104. In one embodiment, the semiconductor wafer 100 has a width or diameter of 100-450 millimeters (mm).
[0019] Figure 1bA cross-sectional view of a portion of a semiconductor wafer 100 is shown. Each semiconductor die 104 has a backside or inactive surface 108 and an active surface 110, which contains analog or digital circuits implemented as active devices, passive devices, conductive layers, and dielectric layers formed within the die and electrically interconnected according to the electrical design and function of the die. For example, the circuit may include one or more transistors, diodes, and other circuit elements formed within the active surface 110 to implement analog or digital circuits, such as a digital signal processor (DSP), an application specific integrated circuit (ASIC), memory, or other signal processing circuits. The semiconductor die 104 may also include IPDs for RF signal processing, such as inductors, capacitors, and resistors.
[0020] Conductive layer 112 is formed over active surface 110 using physical vapor deposition (PVD), chemical vapor deposition (CVD), electrolytic plating, electroless plating, or other suitable metal deposition processes. Conductive layer 112 may be one or more layers of aluminum (Al), copper (Cu), tin (Sn), nickel (Ni), gold (Au), silver (Ag), or other suitable conductive materials. Conductive layer 112 operates as contact pads 110 that are electrically connected to the circuit on active surface 110.
[0021] Conductive bump material is deposited on the conductive layer 112 using evaporation, electrolytic plating, electroless plating, ball drop or screen printing. The bump material can be Al, Sn, Ni, Au, Ag, Pb, Bi, Cu, solder and combinations thereof with an optional flux solution. For example, the bump material can be eutectic Sn / Pb, high lead solder or lead-free solder. The bump material is bonded to the conductive layer 112 using a suitable attachment or bonding process. In one embodiment, the bump material is reflowed by heating the material above its melting point to form a ball or bump 114. In one embodiment, the bump 114 is formed above the under-bump metallization (UBM) having a wetting layer, a barrier layer and an adhesive layer. The bump 114 can also be compression bonded or thermally compressed bonded to the conductive layer 112. The bump 114 represents a type of interconnect structure that can be formed above the conductive layer 112. The interconnect structure can also use bonding wiring, conductive solder paste, columnar bumps, microbumps or other electrical interconnects.
[0022] exist Figure 1c In the process, semiconductor wafer 100 is singulated into individual semiconductor die 104 through saw streets 106 using a saw blade or laser cutting tool 118. Individual semiconductor die 104 may be inspected and electrically tested for identifying known good dies or known good units (KGD / KGU) after singulation.
[0023] Figure 2a-2hThe diagram shows a process of forming a high crystal quality magnetic film layer for shielding low frequency magnetic fields using laser spike annealing in a magnetic field. Figure 2a A cross-sectional view of a multilayer interconnect substrate 120 including a conductive layer 122 and an insulating layer 124 is shown. The conductive layer 122 may be one or more layers of Al, Cu, Sn, Ni, Au, Ag or other suitable conductive materials. The conductive layer 112 may be formed using PVD, CVD, electrolytic plating, electroless plating or other suitable metal deposition processes. The conductive layer 122 provides horizontal electrical interconnections across the substrate 120 and vertical electrical interconnections between the top surface 126 and the bottom surface 128 of the substrate 120. Depending on the design and function of the semiconductor die 104 and other electrical components, portions of the conductive layer 122 may be electrically shared or electrically isolated. The insulating layer 124 includes one or more layers of silicon dioxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), tantalum pentoxide (Ta2O5), aluminum oxide (Al2O3), solder resist, polyimide, benzocyclobutene (BCB), polybenzoxazole (PBO) and other materials having similar insulating and structural properties. The insulating layer 124 may be formed using PVD, CVD, printing, lamination, spin coating, spray coating, sintering, or thermal oxidation. The insulating layer 124 provides isolation between the conductive layers 122 .
[0024] exist Figure 2b In the embodiment, electrical components 130a-130f are disposed on the surface 126 of the interconnect substrate 120 and are electrically and mechanically connected to the conductive layer 122. For example, electrical components 130a, 130b, 130d, and 130e may be discrete electrical devices or IPDs, such as diodes, transistors, resistors, capacitors, and inductors. Electrical components 130 and 130f may be or may be made similar to those from Figure 1c The semiconductor die 104 is provided with the bumps 114 oriented toward the surface 126 of the substrate 120. Alternatively, the electrical components 130a-130f may include other semiconductor dies, semiconductor packages, surface mount devices, RF components, discrete electrical devices, or integrated passive devices (IPDs).
[0025] The electrical components 130a-130f are positioned over the substrate 120 using a pick and place operation. The electrical components 130a-130f are brought into contact with the conductive layer 122 on the surface 126 of the substrate 120. The terminals 134 of the electrical components 130a, 130b, 130d, and 130e are electrically and mechanically connected to the conductive layer 122 using solder or conductive paste 136. The electrical components 130a and 130f are electrically and mechanically connected to the conductive layer 122 by reflowing the bumps 114. Figure 2c Electrical components 130 a - 130 f are shown electrically and mechanically connected to the conductive layer 122 of the substrate 120 .
[0026] exist Figure 2d In the process, an encapsulant or molding compound 140 is deposited over and around the electrical components 130a-130f and the substrate 120 using solder paste printing, compression molding, transfer molding, liquid encapsulant molding, vacuum lamination, spin coating, or other suitable applicators. The encapsulant 140 can be a liquid or granular polymer composite material, such as an epoxy resin with filler, an epoxy acrylate with filler, or a polymer with an appropriate filler. The encapsulant 140 is non-conductive, provides structural support, and environmentally protects the semiconductor device from external elements and contaminants.
[0027] Conductive bump material is deposited on the conductive layer 122 on the surface 128 of substrate 120 using evaporation, electrolytic plating, electroless plating, ball drop or screen printing process. The bump material can be Al, Sn, Ni, Au, Ag, Pb, Bi, Cu, solder and combinations thereof with optional flux solution. For example, the bump material can be eutectic Sn / Pb, high lead solder or lead-free solder. The bump material is bonded to the conductive layer 122 using a suitable attachment or bonding process. In one embodiment, the bump material is reflowed to form a ball or bump 144 by heating the material above its melting point. In one embodiment, bump 144 is formed above the UBM having a wetting layer, a barrier layer and an adhesive layer. Bump 144 can also be compression bonded or thermally compressed bonded to the conductive layer 122. In one embodiment, bump 144 is a copper core bump for durability and to maintain its height. Bump 144 represents a type of interconnect structure that can be formed above the conductive layer 122. The interconnect structure may also use bonding wires, conductive solder paste, stud bumps, micro bumps, or other electrical interconnects.
[0028] The electrical components 130a-130f may include IPDs that are susceptible to or generate EMI, RFI, harmonic distortion, and inter-device interference. For example, the IPDs included in the electrical components 130a-130f provide electrical characteristics required for high-frequency applications (such as resonators, high-pass filters, low-pass filters, band-pass filters, symmetrical Hi-Q resonant transformers, and tuning capacitors). In another embodiment, the electrical components 130a-130f include digital circuits that switch at high frequencies, which may interfere with the operation of other IPDs. Alternatively or in addition, the electrical components 130a-130f may be susceptible to or generate low-frequency magnetic fields from sources such as Qi-WPC, NFC, RFID, PMA, WCT, switching power supplies, inductor modules, and magnetic RAM, as well as being susceptible to or generating electromagnetic noise interference radiated by SiP or circuits with high frequencies and density.
[0029] To cope with low frequency magnetic fields, a magnetic film material or layer 150 is formed over the surface 146 of the encapsulant 140, such as in Figure 2e In one embodiment, the magnetic film material 150 is a quasi-amorphous material made of nickel-iron (Ni-Fe), Ni-Fe-based alloys, ferrites, and other ferromagnetic materials and alloys, and is deposited by sputtering, PVD, spraying, plating, and other suitable deposition processes. The magnetic film material 150 may contain crystalline defects due to the random orientation of the magnetic spin directions. Figure 3a is a graph showing the random orientation of the magnetic spin directions 156 from Figure 2e An enlargement of the box or area 152.
[0030] exist Figure 2f In the embodiment of the present invention, the magnetic film material 150 is subjected to laser spike annealing by scanning a laser 160 across the entire surface 164 of the magnetic film material or moving in the direction of arrow 162. At the same time, the magnetic film material 150 is subjected to a magnetic field 165 between an N-pole magnet 166 and an S-pole magnet 168. The N-pole magnet 166 is disposed on a first side of the substrate 120, and the S-pole magnet 168 is disposed on a second side of the substrate opposite to the first side of the substrate. The random magnetic spin directions 156 are aligned in one direction in the magnetic field 165 to achieve optimal magnetic properties, such as Figure 3b As shown in FIG. By performing laser spike annealing in a magnetic field 165, Figure 3a The magnetic film material is thus transformed into Figure 3b The alignment of the magnetic spin directions 156 increases the magnetic properties of the magnetic film material 150. The combined laser spike annealing in the magnetic field 165 reduces crystal defects and increases grain size. Figure 3b The size of the magnetic domains 158 is shown to increase to enhance the crystal quality of the magnetic film material 150. The magnetic film material 150 becomes a laser spike annealed magnetic film material.
[0031] exist Figure 2g In the process, the substrate 120 is singulated into individual semiconductor packages 180 using a saw blade or laser cutting tool 182 .
[0032] Figure 2hThe semiconductor package 180 after singulation is shown. In order to deal with EMI, RFI, harmonic distortion and interference between devices, a shielding layer 184 is formed above the surface 186 of the magnetic film material 150 to reduce or suppress the influence of EMI, RFI and other interference between devices. The shielding layer 184 extends further downward on the side surface 188 of the semiconductor package 180 to be electrically connected to the conductive layer 122 of the substrate 120. The shielding layer 184 can be carbonyl iron, stainless steel, nickel silver, low carbon steel, silicon iron steel, foil, conductive resin, carbon black, aluminum flakes, Cu, Sn, Ni, Au, Ag and other metals, composites and conductive materials capable of dissipating charged particles to the ground. The shielding layer 184 can be formed by sputtering. The shielding layer 184 is grounded through the interconnection substrate 120. The combination of the substrate 120, the electrical components 130a-130c, the encapsulation 140, the magnetic film material 150 and the shielding layer 184 constitutes SiP189.
[0033] In another embodiment, from Figure 2d Initially, shielding layer 190 is formed over surface 146 of encapsulant 140 to reduce or suppress the effects of EMI, RFI, and other inter-device interference, such as in Figure 4a Shielding layer 190 may be carbonyl iron, stainless steel, nickel silver, low carbon steel, ferrosilicon steel, foil, conductive resin, carbon black, aluminum flakes, Cu, Sn, Ni, Au, Ag and other metals, composites and conductive materials capable of dissipating charged particles to the ground. Shielding layer 190 may be formed by sputtering.
[0034] exist Figure 4b In the process, a saw blade or laser cutting tool 192 is used to singulate the substrate 120 into individual semiconductor packages 194 .
[0035] Figure 4c The semiconductor package 194 after singulation is shown. In order to cope with low-frequency magnetic fields, a magnetic film material or layer 196 is formed above a surface 197 of the shielding layer 190. The magnetic film material 196 further extends downward on a side surface 198 of the semiconductor package 194 to be electrically connected to the conductive layer 122 of the substrate 120. In one embodiment, the magnetic film material 196 is a quasi-amorphous material made of Ni-Fe, Ni-Fe-based alloys, ferrites, and other ferromagnetic materials and alloys, and is deposited by sputtering, PVD, spraying, plating, and other suitable deposition processes. The magnetic film material 196 may contain crystalline defects due to the random orientation of the magnetic spin directions. The magnetic film material 196 may exhibit a random orientation of the magnetic spin directions, similar to Figure 3a .
[0036] exist Figure 4dIn the embodiment, the magnetic film material 196 is subjected to laser spike annealing by scanning a laser 200 across the entire surface of the magnetic film material or moving in the direction of arrow 202. At the same time, the magnetic film material 196 is subjected to a magnetic field 204 between an N-pole magnet 206 and an S-pole magnet 207. The N-pole magnet 204 is disposed on a first side of the semiconductor package 194, and the S-pole magnet 206 is disposed on a second side of the semiconductor package opposite to the first side of the semiconductor package. Figure 3a The random magnetic spin directions 156 in the magnetic field 204 are aligned in one direction to achieve optimal magnetic properties, such as Figure 3b As shown in FIG. 2 . By performing laser spike annealing in a magnetic field 204, Figure 3a The magnetic film material is thus transformed into Figure 3b The alignment of the magnetic spin directions 156 increases the magnetic properties of the magnetic film material 196. Combining laser spike annealing in a magnetic field 204 reduces crystal defects and increases grain size. Figure 3b The size of the magnetic domains 158 is shown to increase to enhance the crystal quality of the magnetic film material 196. The magnetic film material 196 becomes a laser spike annealed magnetic film material. The combination of the substrate 120, the electrical components 130a-130c, the encapsulant 140, the shielding layer 190, and the magnetic film material 196 constitutes the SiP 208, as shown in FIG. Figure 4e Like in.
[0037] In another embodiment, from Figure 2d Continuing, the substrate 120 is singulated into individual semiconductor packages 212 using a saw blade or laser cutting tool 210, as in Figure 5a As shown in.
[0038] Figure 5b The semiconductor package 212 after singulation is shown. In order to deal with EMI, RFI, harmonic distortion and interference between devices, a shielding layer 214 is formed above the surface 146 of the encapsulant 140 to reduce or suppress the effects of EMI, RFI and other interference between devices. The shielding layer 214 further extends downward on the side surface 216 of the semiconductor package 212 to be electrically connected to the conductive layer 122 of the substrate 120. The shielding layer 214 can be carbonyl iron, stainless steel, nickel silver, low carbon steel, silicon iron steel, foil, conductive resin, carbon black, aluminum flakes, Cu, Sn, Ni, Au, Ag and other metals, composites and conductive materials capable of dissipating charged particles to the ground. The shielding layer 214 is grounded through the interconnect substrate 120.
[0039] To cope with low frequency magnetic fields, a magnetic film material or layer 218 is formed over a surface 219 of the shielding layer 214, such as Figure 5c. The magnetic film material 218 further extends downwardly from the side surface 220 of the shielding layer 214. In one embodiment, the magnetic film material 218 is a quasi-amorphous material made of Ni-Fe, Ni-Fe based alloys, ferrites, and other ferromagnetic materials and alloys, and is deposited by sputtering, PVD, spraying, plating, and other suitable deposition processes. The magnetic film material 218 may contain crystalline defects due to the random orientation of the magnetic spin directions. The magnetic film material 218 may exhibit random orientation of the magnetic spin directions, similar to Figure 3a .
[0040] exist Figure 5d In the embodiment, the magnetic film material 218 is subjected to laser spike annealing by scanning a laser 224 across the entire surface of the magnetic film material or moving in the direction of arrow 225. At the same time, the magnetic film material 218 is subjected to a magnetic field 227 between an N-pole magnet 226 and an S-pole magnet 228. The N-pole magnet 226 is disposed on a first side of the semiconductor package 212, and the S-pole magnet 228 is disposed on a second side of the semiconductor package opposite to the first side of the semiconductor package. Figure 3a The random magnetic spin directions 156 in the magnetic field 227 are aligned in one direction to achieve optimal magnetic properties, such as Figure 3b As shown in FIG. By performing laser spike annealing in a magnetic field 227, Figure 3a The magnetic film material is thus transformed into Figure 3b The alignment of the magnetic spin directions 156 increases the magnetic properties of the magnetic film material 218. The combined laser spike annealing in the magnetic field 227 reduces crystal defects and increases grain size. Figure 3b The size of the magnetic domains 158 is shown to increase to enhance the crystal quality of the magnetic film material 218. The magnetic film material 218 becomes a laser spike annealed magnetic film material. The combination of the substrate 120, the electrical components 130a-130c, the encapsulant 140, the shielding layer 214, and the magnetic film material 218 constitutes a SiP 230, as shown in FIG. Figure 5e Like in.
[0041] In another embodiment, from Figure 5a Continuing, and in order to cope with low frequency magnetic fields, a magnetic film material or layer 232 is formed over the surface 146 of the encapsulant 140, as in Figure 6a. The magnetic film material 232 further extends downward on the side surface 233 of the semiconductor package 212 to be electrically connected to the conductive layer 122 of the substrate 120. In one embodiment, the magnetic film material 232 is a quasi-amorphous material made of Ni-Fe, Ni-Fe alloys, ferrites, and other ferromagnetic materials and alloys, and is deposited by sputtering, PVD, spraying, plating, and other suitable deposition processes. The magnetic film material 232 may contain crystalline defects due to the random orientation of the magnetic spin directions. The magnetic film material 232 may exhibit random orientation of the magnetic spin directions, similar to Figure 3a .
[0042] exist Figure 6b In the embodiment, the magnetic film material 232 is subjected to laser spike annealing by scanning a laser 234 across the entire surface 236 of the magnetic film material or moving in the direction of arrow 235. At the same time, the magnetic film material 232 is subjected to a magnetic field 240 between an N-pole magnet 242 and an S-pole magnet 244. The N-pole magnet 242 is disposed on a first side of the semiconductor package 212, and the S-pole magnet 244 is disposed on a second side of the semiconductor package opposite to the first side of the semiconductor package. Figure 3a The random magnetic spin directions 156 in the magnetic field 240 are aligned in one direction to achieve optimal magnetic properties, such as Figure 3b As shown in FIG. By performing laser spike annealing in a magnetic field 240, Figure 3a The magnetic film material is thus transformed into Figure 3b The alignment of the magnetic spin directions 156 increases the magnetic properties of the magnetic film material 232. The combined laser spike annealing in the magnetic field 240 reduces crystal defects and increases grain size. Figure 3b The size of the magnetic domains 158 is shown to increase to enhance the crystal quality of the magnetic film material 232. The magnetic film material 232 becomes a laser spike annealed magnetic film material.
[0043] In order to deal with EMI, RFI, harmonic distortion and interference between devices, a shielding layer 246 is formed above the surface 236 of the magnetic film material 232 to reduce or suppress the effects of EMI, RFI and other interference between devices. The shielding layer 246 further extends downward on the side surface 248 of the semiconductor package 212 to be electrically connected to the conductive layer 122 of the substrate 120. The shielding layer 246 can be carbonyl iron, stainless steel, nickel silver, low carbon steel, silicon iron steel, foil, conductive resin, carbon black, aluminum flakes, Cu, Sn, Ni, Au, Ag and other metals, composites and conductive materials capable of dissipating charged particles to the ground. The shielding layer 248 is grounded through the interconnect substrate 120. The combination of the substrate 120, the electrical components 130a-130c, the encapsulant 140, the magnetic film material 232 and the shielding layer 248 constitutes a SiP 250, as shown in Figure 6b Like in.
[0044] Figure 7 and Figure 8 The figure shows the state before laser annealing (i.e., as in Figure 2e and Figure 3a 2 and 3.0 μm). As the thickness of the magnetic film material 150 increases to several microns, the material exhibits low magnetic permeability due to the perpendicular anisotropy in the stripe domains. As the coercive force increases, the magnetic permeability decreases. The coercive force is related to the magnetic permeability in the magnetic field. Plot 260 shows the behavior of the magnetic film material 150 having a thickness of 0.15 μm. Plots 262 and 264 show the behavior of the magnetic film material 150 having a thickness of 0.2 μm. After a thickness of 0.15 μm of the magnetic film material 150, the coercive force increases rapidly. Therefore, after a thickness of 0.15 μm of the magnetic film material 150, a decrease in magnetic permeability is expected. The hysteresis loop of the 0.20 μm magnetic film material 150 shows the typical behavior of a film with stripe domains caused by perpendicular anisotropy, thereby degrading the magnetic properties. In one embodiment, the magnetic film material 150 should be deposited to a thickness below 0.15 μm in order to reduce the coercivity and thereby increase the magnetic permeability. In other words, sputtering alone cannot deposit a high crystal quality magnetic thick film with high magnetic permeability. The same behavior is also true for the magnetic film materials 196 and 218.
[0045] To improve the magnetic permeability, laser spike annealing as described herein enables the sputtered several micron thick magnetic film to achieve high magnetic permeability and high crystal quality on the surface of the SiP module. Laser spike annealing is a fast, high energy process that does not leave encapsulation defects such as cracks or thermal deformations.
[0046] Fig. 9 An electrical device 400 is shown having a chip carrier substrate or PCB 402 with multiple semiconductor packages (including SiPs 189, 208, 230, and 250) disposed on a surface of the PCB 402. The electrical device 400 may have one type of semiconductor package or multiple types of semiconductor packages depending on the application.
[0047] The electrical device 400 can be an independent system that uses a semiconductor package to perform one or more electrical functions. Alternatively, the electrical device 400 can be a subcomponent of a larger system. For example, the electrical device 400 can be part of a tablet, a cellular phone, a digital camera, a communication system, or other electrical devices. Alternatively, the electrical device 400 can be a graphics card, a network interface card, or other signal processing cards that can be inserted into a computer. The semiconductor package can include a microprocessor, a memory, an ASIC, a logic circuit, an analog circuit, an RF circuit, a discrete device, or other semiconductor die or electrical components. Miniaturization and lightweight are crucial for products to be accepted by the market. The distance between semiconductor devices can be reduced to achieve higher density.
[0048] exist Fig. 9 4, PCB 402 provides a general substrate for structural support and electrical interconnection of semiconductor packages deployed on the PCB. Conductive signal traces 404 are formed over the surface of PCB 402 or within the layers of PCB 402 using evaporation, electrolytic plating, electroless plating, screen printing or other suitable metal deposition processes. Signal traces 404 provide electrical communication between each of the semiconductor packages, the mounted components and other external system components. Traces 404 also provide power and ground connections to each of the semiconductor packages.
[0049] In some embodiments, the semiconductor device has two packaging levels. The first level packaging is a technology for mechanically and electrically attaching a semiconductor die to an intermediate substrate. The second level packaging involves mechanically and electrically attaching an intermediate substrate to a PCB. In other embodiments, the semiconductor device may only have a first level packaging, in which the die is directly mechanically and electrically deployed on the PCB. For the purpose of illustration, several types of first level packaging are shown on PCB 402, including bonding wiring packages 406 and flip chips 408. Additionally, several types of second level packaging (including ball grid arrays (BGA) 410, bump chip carriers (BCC) 412, planar grid arrays (LGA) 416, multi-chip modules (MCM) or SIP modules 418, quad flat no-wire packages (QFN) 420, quad flat packages 422, embedded wafer-level ball grid arrays (eWLB) 424, and wafer-level chip scale packages (WLCSP) 426) are shown as being deployed on PCB 402. In one embodiment, eWLB 424 is a fan-out wafer level package (Fo-WLP), and WLCSP 426 is a fan-in wafer level package (Fi-WLP). Depending on the system requirements, any combination of semiconductor packages configured with any combination of first-level and second-level packaging styles and other electrical components can be connected to PCB 402. In some embodiments, electrical device 400 includes a single attached semiconductor package, while other embodiments require multiple interconnected packages. By combining one or more semiconductor packages on a single substrate, manufacturers can incorporate prefabricated components into electrical devices and systems. Because semiconductor packages include complex functions, electrical devices can be manufactured using less expensive components and streamlined manufacturing processes. The resulting devices are less likely to fail and less expensive to manufacture, resulting in lower costs for consumers.
[0050] While one or more embodiments of the present invention have been illustrated in detail, those skilled in the art will appreciate that modifications and adaptations to these embodiments may be made without departing from the scope of the invention as set forth in the following claims.
Claims
1. A method for manufacturing a semiconductor device, include: providing a substrate; disposing electrical components above the substrate; depositing an encapsulant over the electrical component and the substrate; forming a magnetic film material over the encapsulant; as well as Laser spike annealing of magnetic film materials is performed in a magnetic field.
2. The method of claim 1, further comprising: include: A shielding layer is formed over the magnetic film material.
3. The method of claim 1, further comprising: include: forming a shielding layer over the encapsulation; forming a magnetic film material over the shielding layer; as well as After forming the shielding layer, the magnetic film material is subjected to laser spike annealing in a magnetic field.
4. The method of claim 1, wherein the magnetic film material extends downwardly on a side surface of the semiconductor device.
5. The method of claim 1, further comprising: include: disposing a first magnet on a first side of the semiconductor device; as well as A second magnet is disposed on a second side of the semiconductor device opposite the first side of the semiconductor device, wherein the first magnet has a first pole and the second magnet has a second pole opposite the first pole.
6. A method for manufacturing a semiconductor device, include: providing a substrate; forming a magnetic film material over the substrate; as well as Laser spike annealing of magnetic film materials is performed in a magnetic field.
7. The method of claim 6, further comprising: include: disposing electrical components above the substrate; as well as An encapsulant is deposited over the electrical components and the substrate.
8. The method of claim 6, further comprising: include: A shielding layer is formed over the magnetic film material.
9. The method of claim 6, further comprising: include: forming a shielding layer over the encapsulation; forming a magnetic film material over the shielding layer; as well as After forming the shielding layer, the magnetic film material is subjected to laser spike annealing in a magnetic field.
10. The method of claim 6, further comprising: include: disposing a first magnet on a first side of the semiconductor device; as well as A second magnet is disposed on a second side of the semiconductor device opposite the first side of the semiconductor device, wherein the first magnet has a first pole and the second magnet has a second pole opposite the first pole.
11. A semiconductor device, include: substrate; an electrical component disposed over the substrate; an encapsulant deposited over the electrical components and the substrate; and A magnetic film material is formed over the encapsulant, wherein the magnetic film material is annealed by a laser spike in a magnetic field. 12 . The semiconductor device of claim 11 , further comprising a shielding layer formed over the magnetic film material.
13. The semiconductor device according to claim 11, further comprising: include: a shielding layer formed over the encapsulant; and Magnetic film material on top of the shield.
14. The semiconductor device of claim 11, wherein the magnetic film material extends downwardly on a side surface of the semiconductor device.
15. The semiconductor device according to claim 11, further comprising: include: a first magnet disposed on a first side of the semiconductor device; and A second magnet is disposed on a second side of the semiconductor device opposite the first side of the semiconductor device, wherein the first magnet has a first pole and the second magnet has a second pole opposite the first pole.